Preparation method of cyclic carbonate
A cyclic carbonate and carbon atom technology is applied in the field of preparation of cyclic carbonate, and achieves the effects of simple catalytic system, mild and safe catalytic reaction conditions, and simple process
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2020-06-05
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention belongs to the technical field of green catalytic synthesis, and in particular relates to a preparation method of cyclic carbonate. Background technique
[0002] Currently, for carbon dioxide (CO 2 ) transformation and utilization has become the focus of global attention. What has been reported about CO 2 There are many conversion pathways, but due to CO 2 The molecule itself is very stable, and it is difficult to react with other substances, so CO 2 There are few technological routes for industrial production of raw materials. And by CO 2 The route to synthesize cyclic carbonates with epoxides is one of them.
[0003] Cyclic carbonates represented by propylene carbonate / ethylene carbonate are high-boiling polar organic solvents with excellent performance, and are widely used in textiles, batteries, cosmetics, gas separation, and carbon dioxide (CO 2 ) and hydrogen sulfide gas absorption and other fields. It is also an important o...
Examples
Embodiment 1
[0050] N-H catalysis: Add epoxide 13 (10 mmol) and ammonium halide catalyst 1 (0.2 mmol) into an autoclave equipped with mechanical stirring and temperature-controlled heating device. Seal the reactor with CO 2 Replace the air in the kettle 3 times, then fill the reactor with CO 2 When the initial pressure is 0.1 MPa, the reaction vessel is sealed, and the temperature is raised to 20° C., and the reaction time is 24 hours. After the reaction was completed, the reaction kettle was cooled to 0° C. with an ice-water mixture to release residual gas. Qualitative and quantitative analysis was carried out by gas chromatography, and a light yellow oily substance with a conversion rate of 86% and a selectivity of 97% was obtained.
Embodiment 2
[0052] N-H catalysis: Add epoxy 24 (10 mmol) and ammonium halide catalyst 2 (0.2 mmol) into an autoclave equipped with mechanical stirring and temperature-controlled heating device. Seal the reactor with CO 2 Replace the air in the kettle 3 times, then fill the reactor with CO 2 When the initial pressure is 0.2 MPa, the reactor is sealed, and the temperature is raised to 120° C., and the reaction time is 4 hours. After the reaction was completed, the reactor was cooled to 0° C. with an ice-water mixture to release residual gas, and qualitative and quantitative analysis was performed by gas chromatography to obtain a light yellow oily substance with a conversion rate of 91% and a selectivity of 99%.
Embodiment 3
[0054] N-H catalysis: Add epoxide 15 (10 mmol) and ammonium halide catalyst 3 (0.2 mmol) into an autoclave equipped with mechanical stirring and temperature-controlled heating device. Seal the reactor with CO 2 Replace the air in the kettle 3 times, then fill the reactor with CO 2 After the initial pressure is 0.2MPa, the reactor is sealed, and the temperature is raised to 90°C, and the reaction time is 2h. After the reaction was completed, the reactor was cooled to 0° C. with an ice-water mixture to release residual gas, and qualitative and quantitative analysis was performed by gas chromatography to obtain a light yellow oily substance with a conversion rate of 78% and a selectivity of 92%.