Power device and method for manufacturing power device

By introducing guide columns and isolation layers into superjunction power devices, and utilizing high-energy particle injection and redundant emitter structures, the problem of high forward voltage drop in the prior art is solved, achieving lower resistivity and faster Shutdown speed enhances device performance.

CN111370480BActive Publication Date: 2024-11-12WEEN SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010158090.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-03-09
Publication Date
2024-11-12
Estimated Expiration
2040-03-09

AI Technical Summary

Technical Problem

The forward voltage drop of existing superjunction power devices is high, resulting in the loss of the advantage of high current density, and it is impossible to effectively alleviate the contradiction between on-resistance and breakdown voltage.

Method used

A power device is designed, which includes a drift layer, a guide column, an isolation layer and a trench structure, and isolates the high-energy particle injection zone between the guide column and an isolation layer, and isolates the The doping concentration of the layer is greater than that of the drift layer, and a superjunction structure is formed to reduce the saturation voltage between the collector and the emitter, and to increase the carrier concentration through the shielding effect of the redundant emitter.

Benefits of technology

Lower resistivity and thinner drift layer thickness are achieved, shutdown speed and current density are improved, saturation voltage between collector and emitter are reduced, and device performance is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111370480B_ABST
    Figure CN111370480B_ABST
Patent Text Reader

Abstract

The present invention discloses a power device and a method for manufacturing the power device. The power device comprises: a substrate; an epitaxial layer located on the substrate, the epitaxial layer comprising a drift layer, the drift layer being configured as a first conductive type; a guide pillar configured as a second conductive type, the guide pillar being located in the epitaxial layer; a body region configured as the second conductive type, the body region being located on a surface of the epitaxial layer away from the substrate, and an isolation layer configured as the first conductive type, the isolation layer being located between the body region and the guide pillar, the doping concentration of the isolation layer being greater than the doping concentration of the drift layer. According to the power device of the embodiment of the present invention, the doping concentration of the isolation layer is greater than the doping concentration of the drift layer, which can reduce the saturation voltage between the collector and the emitter and improve the turn-off speed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor devices, and in particular to a power device and a method for manufacturing the power device. Background Art

[0002] Super junction power devices are a new type of power semiconductor devices that are developing rapidly and are widely used. Common super junction power devices are based on double-diffused MOSFET (DMOS), and introduce a super junction structure in its drift layer, which can alleviate the limitation of the contradictory relationship between the on-resistance and breakdown voltage of DMOS. At present, super junction DMOS has been widely used in terminals, lighting products, power supplies or adapters.

[0003] The superjunction structure usually uses P-type conductive pillars and N-type conductive pillars arranged alternately to form a drift layer. In the prior art, the P-type conductive pillars of the superjunction power device are directly connected to the emitter or source of the power device. Such a structure will result in a higher forward voltage drop of the superjunction power device, making the superjunction power device lose the advantage of high current density. Summary of the invention

[0004] The present invention provides a power device and a method for manufacturing the power device, thereby improving the performance of the power device.

[0005] On the one hand, an embodiment of the present invention provides a power device, which includes: a substrate; an epitaxial layer located on the substrate, the epitaxial layer including a drift layer, the drift layer being configured as a first conductivity type; a guide pillar configured as a second conductivity type, the guide pillar being located in the epitaxial layer; a body region configured as the second conductivity type, the body region being located on a surface of the epitaxial layer facing away from the substrate, and an isolation layer configured as the first conductivity type, the isolation layer being located between the body region and the guide pillar, the doping concentration of the isolation layer being greater than the doping concentration of the drift layer.

[0006] According to any of the aforementioned embodiments of one aspect of the present invention, the epitaxial layer is provided with a first groove, a second groove and a third groove, the first groove is located in the drift layer, and is used to accommodate a guide pillar, the second groove and the third groove are longitudinally recessed from the surface of the epitaxial layer away from the substrate side, and the second groove longitudinally runs through the body region, and the power device also includes: an insulating layer, covering the surface of the epitaxial layer away from the substrate side and the inner wall of the second groove and the inner wall of the third groove; a gate, located in the second groove; and a redundant emitter, located in the third trench.

[0007] According to any of the aforementioned embodiments of an aspect of the present invention, the second trench is recessed at least to the isolation layer in the longitudinal direction, so that the redundant emitter extends at least to the isolation layer in the longitudinal direction.

[0008] According to any of the aforementioned embodiments of one aspect of the present invention, a plurality of third grooves are arranged between laterally adjacent second grooves, and the lateral spacing dimension between the second grooves and adjacent third grooves is 1 micron to 3 microns; and / or the lateral spacing dimension between adjacent third grooves is 1 micron to 3 microns.

[0009] According to any of the aforementioned embodiments of an aspect of the present invention, a lateral spacing dimension between adjacent first trenches is 5 micrometers to 15 micrometers.

[0010] According to any of the aforementioned embodiments of an aspect of the present invention, the power device further includes: an emitter region configured as a heavily doped region of the first conductivity type, the emitter region being located on a surface of the body region facing away from the substrate and surrounding at least a portion of the lateral periphery of the second trench; a contact region configured as a heavily doped region of the second conductivity type, the contact region being located in the body region; and an emitter interconnection being located on the insulating layer, the emitter interconnection being coupled to the emitter region, the contact region and the redundant emitter via a contact hole penetrating the insulating layer.

[0011] According to any of the aforementioned implementations of an aspect of the present invention, the substrate is configured as a second conductivity type, and the power device further includes: a collector interconnect coupled to the substrate.

[0012] On the other hand, an embodiment of the present invention provides a method for manufacturing a power device, which includes: forming an epitaxial layer on a substrate, the epitaxial layer including a drift layer configured as a first conductivity type, the epitaxial layer including a first surface facing away from the substrate; patterning the epitaxial layer from the first surface to form a first groove; filling the first groove with a guide column having a second conductivity type; performing doping of the second conductivity type on the first surface to form a body region; performing high-energy particle injection on the side of the body region facing the substrate to form an isolation layer located between the body region and the guide column, the isolation layer being configured as the first conductivity type, and the doping concentration of the isolation layer being greater than the doping concentration of the drift layer.

[0013] According to any of the aforementioned embodiments of another aspect of the present invention, in the step of performing high energy particle implantation on the substrate side of the body region, the implantation dose of the high energy particle implantation is 1e12 atoms per square centimeter to 5e13 atoms per square centimeter.

[0014] According to any of the aforementioned embodiments of another aspect of the present invention, the lateral spacing between adjacent first grooves is 5 micrometers to 15 micrometers; and the longitudinal depth of the first grooves is 20 micrometers to 60 micrometers.

[0015] According to any of the aforementioned embodiments of another aspect of the present invention, the method for manufacturing a power device also includes: forming a second groove on the first surface; forming a first insulating layer on the inner wall of the second groove; forming a gate in the second groove, wherein the lateral groove width of the second groove is 0.3 microns to 1.0 microns; wherein the longitudinal depth of the second groove is 3 microns to 7 microns.

[0016] According to any of the aforementioned embodiments of another aspect of the present invention, while forming the second groove on the first surface, the method for manufacturing a power device further includes: forming a third groove on the first surface, while forming a first insulating layer on the inner wall of the second groove, the method for manufacturing a power device further includes: forming a second insulating layer on the inner wall of the third groove, while forming a gate in the second groove, the method for manufacturing a power device further includes: forming a redundant emitter in the third groove, wherein the lateral groove width of the third groove is 0.3 microns to 1.0 microns; wherein the longitudinal depth of the third groove is 3 microns to 7 microns.

[0017] According to any of the aforementioned embodiments of another aspect of the present invention, the lateral spacing dimension between the second groove and the adjacent third groove is 1 micron to 3 microns; and / or the lateral spacing dimension between adjacent third grooves is 1 micron to 3 microns.

[0018] According to any of the aforementioned embodiments of another aspect of the present invention, the method for manufacturing a power device also includes: performing heavy doping of a first conductivity type on a surface of a body region facing away from the substrate around at least a portion of the lateral periphery of the second trench to obtain an emitter region; forming a third insulating layer covering the first surface; patterning the third insulating layer to form contact holes penetrating the third insulating layer; performing heavy doping of a second conductivity type on a selective region of the body region to obtain a contact region; forming an emitter interconnect on the third insulating layer, wherein the emitter interconnect is coupled to the emitter region and the contact region through the contact hole.

[0019] According to any of the aforementioned embodiments of another aspect of the present invention, the substrate has a second surface away from the epitaxial layer, and the method for manufacturing the power device further includes: doping the second surface with a second conductivity type; and forming a collector interconnection on the second surface.

[0020] According to the power device of the embodiment of the present invention, the drift layer is configured as a first conductivity type, and has a conductive pillar of a second conductivity type penetrating the drift layer, so that the drift layer of the power device has a super junction structure, which can alleviate the limitation of the contradictory relationship between the on-resistance and the breakdown voltage of the traditional power device, and can accelerate the recombination of holes during the shutdown process of the super junction power device, thereby improving the shutdown speed. The power device includes an isolation layer located between the body region and the conductive pillar, so that the conductive pillar is floating. The doping concentration of the isolation layer is greater than the doping concentration of the drift layer, which can reduce the saturation voltage (Vcesat) between the collector and the emitter, and realize the design of a drift layer with a lower resistivity and a thinner drift layer thickness.

[0021] In some optional embodiments, the power device includes a redundant emitter, which extends longitudinally at least to the isolation layer. Due to the shielding effect of the redundant emitter in the third groove with a small pitch, the carrier concentration of the isolation layer of the first conductive type can be greatly increased, so that the power device can greatly reduce the saturation voltage between the collector and the emitter due to the carrier storage effect.

[0022] According to the method for manufacturing a power device in an embodiment of the present invention, high-energy particles are injected into the body region toward the substrate to form an isolation layer between the body region and the guide pillar, and the doping concentration of the isolation layer is made greater than the doping concentration of the drift layer, thereby reducing the saturation voltage between the collector and the emitter and increasing the turn-off speed. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Other features, objects and advantages of the present invention will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings, in which the same or similar reference numerals represent the same or similar features and the accompanying drawings are not drawn to scale.

[0024] Figure 1 is a schematic diagram of a cross-sectional structure of a power device provided according to an embodiment of the present invention;

[0025] Figure 2 yes Figure 1 A partial enlarged schematic diagram of the middle Q region;

[0026] Figures 3 to 17 It is a schematic diagram of the cross-sectional structure of each stage in the method for manufacturing a power device provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0027] The features and exemplary embodiments of various aspects of the present invention will be described in detail below. In order to make the purpose, technical solutions and advantages of the present invention clearer, the present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only configured to explain the present invention and are not configured to limit the present invention. For those skilled in the art, the present invention can be implemented without the need for some of these specific details. The following description of the embodiments is only to provide a better understanding of the present invention by illustrating examples of the present invention.

[0028] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "include..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0029] It should be understood that when describing the structure of a component, when a layer or a region is referred to as being "on" or "over" another layer or another region, it may mean that it is directly on the other layer or another region, or that other layers or regions are included between it and the other layer or another region. Moreover, if the component is turned over, the layer or a region will be "below" or "beneath" another layer or another region.

[0030] The embodiment of the present invention provides a power device. In the present application, the term "power device" refers to the general term for the entire power device formed in various steps of manufacturing the power device, including all layers or regions that have been formed.

[0031] The power device of the embodiment of the present invention may be a power metal oxide semiconductor field effect transistor (Metal-Oxide-Semiconductor Field-Effect Transistor, MOSFET), an insulated gate bipolar transistor (Insulated Gate Bipolar Transistor, IGBT), etc., and the power device will be described below using the structure of the IGBT as an example. It can be understood that the power device of the embodiment of the present invention may also be other types of semiconductor power devices with structures similar to the IGBT.

[0032] Figure 1 is a schematic diagram of a cross-sectional structure of a power device provided in an embodiment of the present invention. The power device 100 may include an active region and a terminal region surrounding at least a portion of the periphery of the active region. Figure 1 Schematic diagram of at least one unit cell (pitch) structure of the active region of the power device 100 is shown in FIG. Figure 2 yes Figure 1A partial enlarged schematic diagram of the middle Q region. In this article, the primitive cell structure refers to the smallest repeating unit of the conductive structure of the active area of ​​the power device. The structural schematic diagrams in this application are all schematic diagrams of the structural principles, and the actual size, detailed position, etc. of each component included in the power device can be adjusted according to actual conditions.

[0033] The power device 100 includes a substrate 110 and an epitaxial layer 120. The epitaxial layer 120 is located on the substrate 110. The epitaxial layer 120 includes a drift layer 121, and the drift layer 121 is configured as a first conductivity type, such as N-type. In some embodiments, the drift layer 121 is lightly N-type doped.

[0034] The power device 100 includes a pillar 130. The pillar 130 is configured as a second conductivity type, such as a P type. The pillar 130 is located in the epitaxial layer 120. In some embodiments, there are a plurality of pillars 130, and the plurality of pillars 130 are arranged at intervals from each other.

[0035] One of the first conductivity type and the second conductivity type is N-type, and the other is P-type. Herein, the first conductivity type is N-type and the second conductivity type is P-type as an example for explanation, and those skilled in the art should understand that the teachings here can be equally applied to devices with conductivity types opposite to the above examples.

[0036] The power device of the embodiment of the present invention further includes a body region 140 and an isolation layer. The body region 140 is configured as a second conductivity type, such as a P type. The body region 140 is located on a surface of the epitaxial layer 120 that is away from the substrate 110 .

[0037] The isolation layer 150 is configured as a first conductivity type, such as an N-type. The isolation layer 150 is located between the body region 140 and the guide pillar 130 , and the doping concentration of the isolation layer 150 is greater than the doping concentration of the drift layer 121 .

[0038] According to the power device 100 of the embodiment of the present invention, its drift layer 121 is configured as a first conductive type, and has a second conductive type guide column 130 penetrating the drift layer 121, so that the drift layer 121 of the power device 100 has a super junction structure, which can alleviate the limitations of the contradictory relationship between the on-resistance and the breakdown voltage of traditional power devices, and can accelerate the recombination of holes during the shutdown process of the super junction power device 100, thereby improving the shutdown speed.

[0039] The power device 100 includes an isolation layer 150 between the body region 140 and the guide pillar 130, so that the guide pillar 130 is floating. The doping concentration of the isolation layer 150 is greater than the doping concentration of the drift layer 121, which can reduce the saturation voltage (Vcesat) between the collector and the emitter, and realize the design of a drift layer with lower resistivity and thinner drift layer thickness.

[0040] In some embodiments, the epitaxial layer 120 is provided with a first trench T1, a second trench T2, and a third trench T3. The first trench T1 is located in the drift layer 121 and is used to accommodate the guide pillar 130. The second trench T2 and the third trench T3 are recessed longitudinally from the surface of the epitaxial layer 120 facing away from the substrate 110. The second trench T2 longitudinally penetrates the body region 140.

[0041] The power device 100 further includes an insulating layer 160, a gate 170, and a redundant emitter (emitter dummy) 181. The insulating layer 160 covers the surface of the epitaxial layer 120 away from the substrate 110 and the inner wall of the second trench T2 and the inner wall of the third trench T3. The gate 170 is located in the second trench T2. The redundant emitter 181 is located in the third trench T3.

[0042] In some embodiments, the second trench T2 is recessed at least to the isolation layer 150 along the longitudinal direction, so that the redundant emitter 181 extends at least to the isolation layer 150 along the longitudinal direction.

[0043] In some embodiments, the second trenches T2 and the third trenches T3 are formed in the same patterning process. A plurality of third trenches T3 are arranged between the laterally adjacent second trenches T2.

[0044] In some embodiments, the lateral spacing between the second trench T2 and the adjacent third trench T3 is 1 micron to 3 microns; and / or the lateral spacing between adjacent third trenches T3 is 1 micron to 3 microns. Due to the shielding effect of the redundant emitter 181 in the third trenches T3 with small spacing, the carrier concentration of the isolation layer 150 of the first conductivity type can be greatly increased, so that the power device 100 can greatly reduce the saturation voltage between the collector and the emitter due to the carrier storage effect.

[0045] Herein, the lateral spacing between trenches is referred to as the trench to trench size. In the primitive cell structure of the power device 100, the number of the second trenches T2 and the number of the third trenches T3 are adjusted accordingly according to the primitive cell size, product performance and parameters of the power device 100.

[0046] In some embodiments, the lateral spacing between adjacent first trenches T1 is 5 microns to 15 microns. In the process of forming the first trench T1, the second trench T2 and the third trench T3, the formation process of the second trench T2 and the third trench T3 can be performed separately and differently from the formation process of the first trench T1. The first trench T1 can adopt the conventional super junction structure guide pillar formation process, while the second trench T2 and the third trench T3 can be formed with a smaller size and spacing using a smaller precision trench process, so as to facilitate the formation of redundant emitters with smaller spacing and optimize the carrier concentration of the isolation layer.

[0047] The power device 100 further includes an emitter region 182 , a contact region 183 , and an emitter interconnect 191 .

[0048] The emitter region 182 is configured as a heavily doped region of the first conductivity type, such as an N-type heavily doped region. The emitter region 182 is located on a surface of the body region 140 facing away from the substrate 110 and surrounds at least a portion of the lateral periphery of the second trench T2.

[0049] The contact region 183 is configured as a heavily doped region of the second conductivity type, such as a P-type heavily doped region. The contact region 183 is located in the body region 140 .

[0050] The emitter interconnect 191 is located on the insulating layer 160. The emitter interconnect 191 is coupled to the emitter region 182, the contact region 183, and the redundant emitter 181 via a contact hole that penetrates the insulating layer 160. In some embodiments, the contact hole also extends into the body region 140; in some embodiments, the contact hole also penetrates the emitter region. The position of the contact region 183 in the body region 140 corresponds to the position of the contact hole. By providing the contact region 183 with a heavily doped conductive type, the latch effect can be improved.

[0051] In some embodiments, the substrate 110 is configured as a second conductivity type, such as a P-type. The power device 100 further includes a collector interconnect 192 coupled to the substrate 110 .

[0052] In some embodiments, the epitaxial layer 120 may further include a field stop (FS) layer 122, and the field stop layer 122 is located between the drift layer 121 and the substrate 110. In some embodiments, the field stop layer 122 is formed by ion implantation, so that it is configured as a first conductivity type, that is, N-type. In some other embodiments, a buffer layer may also be provided between the drift layer 121 and the substrate 110, and the buffer layer may be formed by epitaxial growth, so that it is configured as a first conductivity type, that is, N-type.

[0053] In the above embodiments, the power device is an IGBT as an example for explanation, however, according to the teaching of the embodiments of the present invention, its principle can be equally applied to devices with structures similar to the above examples. For example, in some embodiments, the power device is a power double-diffused metal-oxide-semiconductor field-effect transistor (DMOS), and its general structure is the same as the IGBT structure of the above embodiments, wherein the substrate 110 is configured as a first conductivity type, i.e., N-type. The source interconnection in the DMOS is the emitter interconnection of the above IGBT, and the drain interconnection in the DMOS is the collector interconnection of the above IGBT.

[0054] An embodiment of the present invention further provides a method for manufacturing a power device. The method for manufacturing a power device is, for example, applied in the process of forming the power device 100 of the above-mentioned embodiment of the present invention. The method for manufacturing a power device will be described below using the formation process of the above-mentioned power device 100 as an example.

[0055] Figures 3 to 17 The power device 100 may include an active region and a terminal region surrounding at least a portion of the periphery of the active region. The drawings herein mainly show a partial structure of the active region of the power device 100.

[0056] like Figure 3 , an epitaxial layer 120 is formed on the substrate 110 . The epitaxial layer 120 includes a drift layer 121 configured as a first conductivity type, such as an N-type, and the drift layer 121 is, for example, an N-type lightly doped layer. The epitaxial layer 120 includes a first surface S1 away from the substrate 110 .

[0057] The substrate 110 formed with the epitaxial layer 120 may be a first conductive type epitaxial wafer with sufficient thickness, such as a single crystal silicon wafer, and in some other embodiments, may also be a wafer with a field stop layer. The thickness of the epitaxial layer 120 or the drift layer 121 is determined by the withstand voltage value of the device design, for example, for a super junction IGBT (IGBT with a super junction structure) with a withstand voltage of 200V to 900V, the thickness of the epitaxial layer 120 is 20um to 70um, and the resistivity ranges from 0.5ohm to 5ohm according to the different lateral spacing dimensions of the pillars (e.g., 5um to 15um).

[0058] like Figure 4, the epitaxial layer 120 is patterned from the first surface S1 to form a first trench T1. The process of forming the first trench T1 can be dry etching, and the depth of the first trench T1 can be determined according to the breakdown voltage of the device. In some embodiments, the longitudinal depth of the first trench T1 is 20 microns to 60 microns.

[0059] In the process of forming the first trench T1, when dry etching is used to form the trench, an oxide or silicon nitride layer or a combination thereof may be used as a mask layer (hard mask). The mask layer is first patterned (eg, etched) and then etched to form the trench.

[0060] In some embodiments, there are a plurality of first trenches T1, which are arranged at intervals in the transverse direction. The transverse interval between adjacent first trenches T1 is 5 micrometers to 15 micrometers. In some embodiments, the longitudinal depth of the first trenches T1 is 20 micrometers to 60 micrometers.

[0061] like Figure 5 and Figure 6 , a guide pillar 130 having a second conductivity type is filled in the first trench T1. The guide pillar 130 may be formed by selective epitaxial filling, and P-type single crystal silicon is filled in the first trench T1 to form the guide pillar 130. Subsequently, the excess P-type single crystal silicon on the first surface S1 may be removed by a method such as chemical mechanical polishing (CMP). Thereafter, the mask layer on the first surface S1 is removed, and the first surface S1 is wet cleaned.

[0062] In some embodiments, the terminal region is insulated and covered on the structure obtained in the above steps. For example, an insulating layer such as silicon dioxide is grown by thermal oxidation, and the thickness of the insulating layer is 10 kilo-angstroms to 20 kilo-angstroms. Then, a mask layer is used to define the active region, and the insulating layer such as silicon dioxide is removed in the active region by dry etching or wet etching.

[0063] Afterwards, if Figure 7 , forming a second trench T2 on the first surface S1. In some embodiments, while forming the second trench T2 on the first surface S1, the method for manufacturing a power device further includes: forming a third trench T3 on the first surface S1. The second trench T2 is used to accommodate a gate. The third trench T3 is used to accommodate a redundant emitter.

[0064] In some embodiments, a mask layer is used to define the second trench T2 and the third trench T3. In one embodiment, the transverse trench width of the second trench T2 is 0.3 micrometers to 1.0 micrometers; in one embodiment, the longitudinal depth of the second trench T2 is 3 micrometers to 7 micrometers; in one embodiment, the transverse trench width of the third trench T3 is 0.3 micrometers to 1.0 micrometers; in one embodiment, the longitudinal depth of the third trench T3 is 3 micrometers to 7 micrometers.

[0065] In some embodiments, the lateral spacing between the second trench T2 and the adjacent third trench T3 is 1 micrometer to 3 micrometers; and / or the lateral spacing between the adjacent third trenches T3 is 1 micrometer to 3 micrometers.

[0066] like Figure 8 , a first insulating layer 161 is formed on the inner wall of the second trench T2. Thereafter, a gate 170 is formed in the second trench T2. In some embodiments, while the first insulating layer 161 is formed on the inner wall of the second trench T2, the method for manufacturing a power device further includes: forming a second insulating layer 162 on the inner wall of the third trench T3. In some embodiments, while the gate 170 is formed in the second trench T2, the method for manufacturing the power device 100 further includes: forming a redundant emitter 181 in the third trench T3.

[0067] The process of forming the first insulating layer 161 on the inner wall of the second trench T2 and the second insulating layer 162 on the inner wall of the third trench T3 may be: oxidizing the inner wall of the second trench T2 and the inner wall of the third trench T3 to form an oxide layer, wherein the thickness of the oxide layer is 500 angstroms to 1500 angstroms.

[0068] The process of forming the gate 170 in the second trench T2 and the redundant emitter 181 in the third trench T3 may be: filling the second trench T2 and the third trench T3 with polysilicon, and then etching back using dry etching to remove the polysilicon outside the second trench T2 and the third trench T3.

[0069] like Fig. 9 , doping of the second conductivity type is performed on the first surface S1 to form a body region 140. The second conductivity type is, for example, P-type. The process of forming the body region 140 is, for example, P-type conductive ion implantation and push-in junction. The push-in junction depth of the body region 140 is adjusted according to the longitudinal depth of the second trench T2, and the implantation dose of the P-type conductive ion is adjusted according to the threshold voltage requirement.

[0070] like Fig.10 High-energy particle implantation is performed on the body region 140 facing the substrate 110 to form an isolation layer 150 between the body region 140 and the guide pillar 130 . The isolation layer 150 is configured as a first conductivity type, and the doping concentration of the isolation layer 150 is greater than the doping concentration of the drift layer 121 .

[0071] In the step of high energy particle implantation on the side of the body region 140 facing the substrate 110, the implanted particles are, for example, N-type doping particles such as phosphorus and hydrogen. In some embodiments, high concentration N-type doping particles may be implanted only in the active region, and not in the terminal region.

[0072] In some embodiments, in the step of performing high energy particle implantation on the side of the body region 140 facing the substrate 110 , the implantation depth is 2 um to 6 um, which is within the longitudinal depth range of the second trench T2 and the third trench T3 below the body region 140 .

[0073] In some embodiments, in the step of performing high energy particle implantation on the side of the body region 140 facing the substrate 110, the implantation dose of the high energy particle implantation is 1e12 atoms per square centimeter to 5e13 atoms per square centimeter. After implantation, the N-type isolation layer 150 is annealed at a temperature of 800° C. to 1100° C. by rapid thermal annealing (RTA), rapid thermal processing (RTP) or furnace tube process.

[0074] like Fig.11 , the first conductive type is heavily doped around at least part of the lateral periphery of the second trench T2 and on the surface of the body region 140 away from the substrate 110 to obtain the emitter region 182. For example, N-type heavily doped is performed on the surface of the body region 140 away from the substrate 110 by ion implantation to obtain the N-type heavily doped emitter region 182.

[0075] like Fig.12 , forming a third insulating layer 163 covering the first surface S1. The third insulating layer 163 includes one or more oxide film layers, and the oxide film layers can be at least one of silicon dioxide (SiO2), phospho-silicate glass (PSG), borosilicate glass (BSG), or boro-phospho-silicate glass (BPSG). The total thickness of the third insulating layer 163 is 5 kilo-angstroms to 11 kilo-angstroms.

[0076] like Fig.13 , patterning the third insulating layer 163 to form a contact hole CH. In some embodiments, a mask layer is used to define the contact hole, and then dry etching or a combination of dry and wet etching is performed to obtain the contact hole CH. The contact hole CH exposes a portion of the surface of the emitter region 182 and the body region 140. In some embodiments, the contact hole CH also exposes a portion of the surface of the redundant emitter 181.

[0077] like Fig.14 In some embodiments, the second conductivity type is heavily doped in a selective region of the body region 140 to obtain the contact region 183. For example, the body region 140 in the region corresponding to the contact hole CH is heavily doped with P type by ion implantation to obtain the P type heavily doped contact region 183. In some other embodiments, selective ion implantation may also be performed before forming the contact hole CH to form the second conductivity type heavily doped contact region 183 to improve the latch effect.

[0078] Afterwards, if Fig.15 , an emitter interconnection 191 is formed on the third insulating layer 163. The emitter interconnection 191 is coupled to the emitter region 182 and the contact region 183 through the contact hole CH. In some embodiments, the emitter interconnection 191 is also coupled to the redundant emitter 181 through the contact hole CH.

[0079] The emitter interconnection 191 can be made of a conductive material such as metal. In one example, tungsten can be first deposited in the contact hole CH, followed by chemical mechanical polishing to form a tungsten plug, and then aluminum can be deposited to form the interconnection. In another example, aluminum can be directly deposited in the contact hole CH and on the third insulating layer 163 to form the interconnection.

[0080] In some embodiments, while forming the patterned emitter interconnect 191 , a gate interconnect and a terminal field plate structure may also be formed simultaneously.

[0081] In some embodiments, a patterned passivation layer may be formed on each of the conductive interconnect structures.

[0082] At this point, the general process on the first surface S1 side of the power device 100 is completed.

[0083] like Fig.16 , the substrate 110 has a second surface S2 away from the epitaxial layer 120, and the method for manufacturing the power device further includes thinning from the second surface S2 of the substrate 110, so that the total thickness of the substrate 110 and the epitaxial layer 120 is reduced. In some embodiments, the total thickness of the substrate 110 and the epitaxial layer 120 is 30 microns to 60 microns. For example, in a 600V super junction IGBT, the total thickness of the substrate 110 and the epitaxial layer 120 is 40 microns to 50 microns.

[0084] like Fig.17 The method for manufacturing a power device further includes performing a second conductivity type doping on the second surface S2, such as P-type doping. In some embodiments, ion implantation of P-type doping particles such as boron is performed on the second surface S2, and annealing is performed to configure the substrate 110 to be P-type doped.

[0085] Afterwards, a collector interconnection 192 is formed on the second surface S2 . The collector interconnection 192 is a patterned conductive material, covering the second surface S2 of the substrate 110 .

[0086] According to the method for manufacturing the power device 100 of an embodiment of the present invention, high-energy particle injection is performed on the side of the body region 140 facing the substrate 110 to form an isolation layer 150 located between the body region 140 and the guide pillar 130, and the doping concentration of the isolation layer 150 is made greater than the doping concentration of the drift layer 121, thereby reducing the saturation voltage between the collector and the emitter and increasing the turn-off speed.

[0087] According to the embodiments of the present invention as described above, these embodiments do not describe all the details in detail, nor do they limit the invention to the specific embodiments described. Obviously, many modifications and changes can be made based on the above description. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can make good use of the present invention and the modified use based on the present invention. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. A power device, characterized in that: include: substrate; An epitaxial layer is located on the substrate, the epitaxial layer includes a drift layer, the drift layer is configured as a first conductivity type, the epitaxial layer is provided with a first trench, a second trench and a third trench, the first trench is located in the drift layer, the second trench and the third trench are longitudinally recessed from a surface of the epitaxial layer away from the substrate side, and a plurality of the third trenches are spaced apart between the second trenches adjacent to each other in the transverse direction; an insulating layer, covering a surface of the epitaxial layer facing away from the substrate and an inner wall of the second trench and an inner wall of the third trench; a gate, located in the second trench; A redundant emitter, located in the third trench; A guide post, configured as a second conductivity type, the guide post being accommodated in the first groove; a body region configured as the second conductivity type, the body region being located on a surface of the epitaxial layer away from the substrate, and the second trench vertically penetrating the body region; an emitter region configured as a heavily doped region of the first conductivity type, the emitter region being located on a surface of the body region facing away from the substrate and surrounding at least a portion of a lateral periphery of the second trench; a contact region configured as a heavily doped region of the second conductivity type, the contact region being located in the body region; An emitter interconnection, located on the insulating layer, wherein the emitter interconnection is coupled with the emitter region, the contact region and the redundant emitter via a contact hole penetrating the insulating layer; as well as The isolation layer is configured as the first conductivity type, the isolation layer is located between the body region and the guide column, the doping concentration of the isolation layer is greater than the doping concentration of the drift layer, and the third grooves are all recessed at least to the isolation layer in the longitudinal direction, so that the redundant emitter extends at least to the isolation layer in the longitudinal direction.

2. The power device according to claim 1, characterized in that: The lateral spacing between the second groove and the adjacent third groove is 1 micron to 3 microns; and / or The lateral spacing between adjacent third grooves is 1 micron to 3 microns.

3. The power device according to claim 1, characterized in that: The lateral spacing between adjacent first grooves is 5 micrometers to 15 micrometers.

4. The power device according to claim 1, characterized in that: The substrate is configured as the second conductivity type, and the power device further includes: The collector is interconnected and coupled to the substrate.

5. A method for manufacturing a power device, characterized in that: include: forming an epitaxial layer on a substrate, the epitaxial layer comprising a drift layer configured as a first conductivity type, the epitaxial layer comprising a first surface facing away from the substrate; patterning the epitaxial layer from the first surface to form a first trench; Filling the first trench with a conductive column having a second conductivity type; forming a second groove and a third groove on the first surface, wherein a portion of the third groove is formed in the guide pillar; forming a first insulating layer on an inner wall of the second trench and forming a second insulating layer on an inner wall of the third trench; forming a gate in the second trench and forming a redundant emitter in the third trench; Doping the first surface with the second conductivity type to form a body region, wherein the second trench vertically penetrates the body region; High-energy particle implantation is performed on the side of the body region facing the substrate to form an isolation layer between the body region and the guide pillar, the isolation layer is configured as the first conductivity type, the doping concentration of the isolation layer is greater than the doping concentration of the drift layer, and the third trenches are longitudinally extended at least to the isolation layer, so that the redundant emitter is longitudinally extended at least to the isolation layer; Performing heavy doping of the first conductivity type on a surface of the body region away from the substrate around at least a portion of the lateral periphery of the second trench to obtain an emitter region; forming a third insulating layer covering the first surface; patterning the third insulating layer to form a contact hole penetrating the third insulating layer; Performing heavy doping of the second conductivity type in a selective region of the body region to obtain a contact region; An emitter interconnect is formed on the third insulating layer, and the emitter interconnect is coupled with the emitter region and the contact region through the contact hole.

6. The method for manufacturing a power device according to claim 5, characterized in that: In the step of performing high energy particle implantation on the side of the body region facing the substrate, an implantation dose of the high energy particle implantation is 1e12 atoms per square centimeter to 5e13 atoms per square centimeter.

7. The method for manufacturing a power device according to claim 5, characterized in that: The lateral spacing between adjacent first grooves is 5 microns to 15 microns; The longitudinal depth of the first groove is 20 micrometers to 60 micrometers.

8. The method for manufacturing a power device according to claim 5, characterized in that: The transverse groove width of the second groove is 0.3 micrometer to 1.0 micrometer; The second groove has a longitudinal depth of 3 micrometers to 7 micrometers.

9. The method for manufacturing a power device according to claim 5, characterized in that: The transverse groove width of the third groove is 0.3 micrometer to 1.0 micrometer; The third groove has a longitudinal depth of 3 micrometers to 7 micrometers.

10. The method for manufacturing a power device according to claim 5, characterized in that: The lateral spacing between the second groove and the adjacent third groove is 1 micron to 3 microns; and / or The lateral spacing between adjacent third grooves is 1 micron to 3 microns.

11. The method for manufacturing a power device according to claim 5, characterized in that: The substrate has a second surface away from the epitaxial layer, and the method for manufacturing the power device further includes: Performing doping of the second conductivity type on the second surface; A collector interconnect is formed on the second surface.