A FRP-wrapped cracked concrete structure

Through the synergy between the FRP plate and the FRP cloth, the concrete cracks are reinforced by three-way stress, which solves the problem of strain hysteresis of the FRP-reinforced concrete structure when under pressure and the prone to cracking of epoxy resin, and improves the compressive strength of the concrete column and durability, reducing prestressed tool requirements.

CN111379433BActive Publication Date: 2024-11-19NANJING INST OF TECH
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
CN201811607965.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-12-27
Publication Date
2024-11-19
Estimated Expiration
2038-12-27

AI Technical Summary

Technical Problem

The existing FRP reinforced concrete structures have strain hysteresis due to the influence of the bonding surface when under pressure, and the epoxy resin is prone to cracking and peeling, which reduces the durability of the concrete column, especially the high prestress magnitude requirement, which limits large-area application.

Method used

The synergistic effect of FRP sheet combination plate and FRP cloth is adopted to reinforce concrete cracks through three-way stress, and the compressive strength of FRP sheet and the deformation of FRP cloth are used to reduce prestress requirements, and the internal expansion and displacement of concrete are constrained through outsourcing structures. , improve overall strength.

Benefits of technology

It effectively solves the problem of strain hysteresis of FRP cloth, improves the compressive strength and durability of concrete columns, reduces the requirements of prestressed tools, and reduces the risk of late cracks of concrete cracks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111379433B_ABST
    Figure CN111379433B_ABST
Patent Text Reader

Abstract

An FRP-clad cracked concrete structure includes FRP fabric, FRP sheet assembly A, FRP sheet assembly B, and FRP sheet assembly C. FRP sheet assembly B, consisting of a resin layer, is attached to the cracked portion of the concrete column. FRP sheet assembly A, FRP sheet assembly B, and FRP sheet assembly C are bound to the fracture points of the concrete column via the FRP fabric. FRP sheet assembly A and FRP sheet assembly C are respectively attached to the two inclined surfaces of FRP sheet assembly B and simultaneously adhered to the surface of the concrete column. This external cladding structure constrains the expansion of the concrete's internal volume and the displacement of internal components, thereby improving the overall strength of the concrete. It also mitigates, to some extent, the adverse effects of epoxy resin's low toughness and poor crack resistance leading to subsequent re-cracking at concrete cracks.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of building concrete reinforcement, and in particular relates to an FRP-wrapped cracked concrete structure. Background Art

[0002] In the prior art, the fiber reinforced composite (FRP) reinforced concrete structure technology is to fix FRP on the surface of the concrete structure to form a composite body, and through the synergistic effect of the fiber reinforced composite material and the concrete structure, the purpose of strengthening the original structure and improving the structural stress performance is achieved. When the concrete is compressed, the FRP cloth is affected by the bonding surface and produces a hysteresis in the stress, and according to the flat section assumption, when the concrete in the compression zone reaches the ultimate strain, the fiber cloth only exerts about 20% of its strength. Although water-based epoxy resin repair concrete can restore or even improve the original strength of the concrete column in a short period of time, the cured epoxy resin is easy to crack and peel off, which will reduce the durability of the repaired concrete column to a certain extent. In particular, the general FRP cloth prestressed reinforcement of concrete columns cannot be used on a large scale due to the high requirements for the size of the prestress. Summary of the invention

[0003] 1. Technical issues to be solved

[0004] The object of the present invention is to provide a FRP-encased cracked concrete structure to solve the practical problems raised in the above background technology.

[0005] (II) Technical solution

[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: an FRP-wrapped cracked concrete structure, comprising an FRP cloth, an FRP plate composite board A, an FRP plate composite board B, and an FRP plate composite board C, wherein the FRP plate composite board B is attached to the cracked part of the concrete column by a resin layer, the FRP plate composite board A, the FRP plate composite board B, and the FRP plate composite board C are tied to the fracture of the concrete column by the FRP cloth, and the FRP plate composite board A and the FRP plate composite board C are respectively attached to the two inclined surfaces of the FRP plate composite board B and are simultaneously attached to the surface of the concrete column.

[0007] Preferably, the cross section of the FRP plate composite plate A is a parallelogram.

[0008] Preferably, the cross section of the FRP plate composite plate B is an isosceles trapezoid.

[0009] Preferably, the cross section of the FRP plate composite plate C is a parallelogram.

[0010] Preferably, the FRP cloth has different covering densities on the FRP plate assembly board A, the FRP plate assembly board B and the FRP plate assembly board C.

[0011] (III) Beneficial effects

[0012] The present invention provides a novel design structure of FRP outer-wrapped cracked concrete, which adopts a variety of FRP materials, improves the offset through the synergistic effect of FRP plates and FRP cloths, and further improves the centripetal force on the basis of centripetal prestress through the deformation of FRP cloths. The structural design adopts a three-dimensional stress method to reinforce the same crack, which can effectively solve the strain hysteresis problem caused by the transition buffer of the bonding surface of FRP cloth, and at the same time effectively exert the compressive strength of FRP plates, and solve several problems existing in the prior art. In particular, the structure has a certain reduction in the requirements for the size of prestress required for FRP cloth prestressed reinforcement of concrete columns, and effectively reduces the requirements for tools. Through the outer-wrapped structure, the expansion of the internal volume of concrete and the displacement of internal components are constrained to improve the overall strength of concrete, and to a certain extent solve the adverse effects of epoxy resin on the later re-cracking of concrete cracks due to low toughness and poor cracking resistance. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.

[0014] Figure 1 : Schematic diagram of the structure of the present invention.

[0015] Figure 2 : Schematic diagram of the position of the concrete column after being compressed and deformed according to the present invention.

[0016] Figure 3 : A schematic diagram of the side structure of the cracks in the concrete column and the position of the FRP composite plate of the present invention.

[0017] Figure 4 : Theoretical combination state of the FRP composite plate of the present invention and the analysis diagram of the stress conditions of each part.

[0018] Figure 5 : A schematic diagram of the force analysis of the FRP plate assembly A and the FRP plate assembly C after the FRP plate assembly B of the present invention has slipped;

[0019] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0020] 1-concrete column, 2-FRP cloth, 3-FRP plate composite board A, 4-FRP plate composite board B, 5-FRP plate composite board C. DETAILED DESCRIPTION

[0021] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] See also Figure 1-5 The present invention provides a technical solution: an FRP outer layer cracked concrete structure, comprising an FRP cloth 2, an FRP plate combination plate A3, an FRP plate combination plate B4, and an FRP plate combination plate C5, wherein the FRP plate combination plate A3 is arranged above the FRP plate combination plate B4, the FRP plate combination plate C5, the FRP plate combination plate B is attached to the cracked part of the concrete column by a resin layer, the FRP plate combination plate A3, the FRP plate combination plate B4, the FRP plate combination plate C5, the FRP plate combination plate B is attached to the cracked part of the concrete column by a resin layer, the FRP plate combination plate A3, the FRP plate combination plate The plate assembly board B4 and the FRP plate assembly board C5 are tied to the fracture of the concrete column 1 through the FRP cloth 2, and the FRP plate assembly board A3 and the FRP plate assembly board C5 are respectively bonded to the two inclined surfaces of the FRP plate assembly board B4 and are simultaneously bonded to the surface of the concrete column 1; the cross-section of the FRP plate assembly board A3 is a parallelogram; the cross-section of the FRP plate assembly board B4 is an isosceles trapezoid; the cross-section of the FRP plate assembly board C5 is a parallelogram; the covering density of the FRP cloth 2 on the FRP plate assembly board A3, the FRP plate assembly board B4 and the FRP plate assembly board C5 is different.

[0023] When the present invention is used in practice, firstly, the cracks of the concrete column and the surroundings are polished by the external reinforcement method, and then the concrete cracks are filled with water-based epoxy resin as a structural adhesive, and then the epoxy resin coating is added to paste the FRP plate composite plate on the damaged side of the concrete square column, and the cracked part of the concrete square column is pasted and reinforced, and finally the FRP cloth 2 is used to constrain the FRP plate to perform secondary structural reinforcement on the cracks and directly reinforce the concrete square column, and then the prestressed reinforcement method is used, and the sparse and dense interval circumferential column wrapping method is adopted, and the FRP cloth 2 is used to constrain the FRP plate outside the concrete. By improving the circumferential column wrapping method of the FRP cloth, a certain amount of slippage is provided while the effect of the FRP cloth 2 on improving the strength of the concrete column remains unchanged as much as possible, and the method is that the FRP cloths on both sides of the composite structure are denser and the FRP cloths in the middle of the composite structure are sparser, and are roughly parallel binding belts. That is, the FRP cloth in the outer concrete part is the tightest, followed by the FRP cloth at FRP plate A3 and FRP plate C5, and the FRP cloth at FRP plate B4 has almost no overlapping parts but also no gaps. Through the synergistic effect between the FRP plate and the FRP cloth, the FRP plate directly reinforces the cracked part of the concrete under the action of epoxy resin, and the crack is reinforced by secondary structure under the action of epoxy resin and FRP cloth. While reinforcing the FRP plate, the concrete outside the FRP plate is directly reinforced. Since the direct constraint of the FRP composite plate plays a major role in the reinforcement of concrete, reducing the FRP inclination angle as much as possible within the ultimate compressive strength can effectively enhance its constraint effect. The short side of the FRP plate in the vertical direction is the same length as the vertical side of FRP plate A3 and FRP plate C5. When the designed compressive strength of the FRP plate is 1000MPa, the optimal relationship between the theoretical inclination angle α of the FRP plate and the prestress F of the FRP cloth can be obtained through calculation, and the equation is obtained:

[0024]

[0025]

[0026]

[0027] Apparently

[0028]

[0029] σ1>σ2

[0030] therefore

[0031] [σ]>σ1>σ2

[0032]

[0033] Where: F——pressure of FRP cloth on FRP plate, N

[0034] α——Inclination angle of FRP plate, °

[0035] b——length of the short side of FRPⅡ plate, m

[0036] L——Thickness of FRP composite plate, m

[0037] d——Width of FRP composite slab, width of concrete square column, m

[0038] Under the corresponding design conditions, the theoretical working performance and durability of the combined structure of this design will have a better solution under this theoretical equation. The mechanical principle of amplifying the synergistic effect of the displacement of the FRP plate and the FRP cloth and increasing the centripetal force through the deformation of the FRP cloth, and three-way restraint and reinforcement of the same crack to improve the strength of the FRP plate:

[0039] like Figure 1 When the concrete block is not under pressure, the FRP plate is subjected to a uniform distribution of the annular centripetal compressive stress F of the FRP cloth, and the FRP plate itself is also relatively dispersed in reinforcing the concrete surface. Through the prestressed reinforcement method, the sparse and dense interval annular column wrapping method is adopted, and the FRP cloth is used to constrain the FRP plate outside the concrete. By improving the annular column wrapping method of the FRP cloth, a certain amount of slippage is provided while the effect of the FRP cloth on improving the strength of the concrete column is as unchanged as possible. The method is that the FRP cloth 2 on both sides of the composite structure is denser and the FRP cloth 2 in the middle of the composite structure is sparser, and is roughly parallel to the restraining belt. That is, the FRP cloth in the outer concrete part is the densest, followed by the FRP cloth at the FRP plate A3 and FRP plate C5, and the FRP cloth at the FRP plate B4 has almost no overlapping parts but also no gaps.

[0040] like Figure 2 Under compression, the existence of cracks in the concrete test block will cause the concrete of the FRP plate A3 corresponding to the concrete test block and the FRP plate A3 to slide downward. The extrusion between the FRP plate A3 and the FRP plate C5 will further constrain the stress concentration part, that is, the FRP plate B4. At the same time, the slippage of the FRP plate A3 will cause the deformation of the FRP cloth, resulting in greater tensile stress, which will become annular compressive stress.

[0041] like Figure 2, under further pressure, the concrete at the crack will expand slightly outward and be transmitted to the FRP cloth through the FRP plate B4. In this process, in addition to the tensile suppression of the concrete crack by the external bonding FRP plate, the deformation of the FRP plate B4 effectively amplifies the deformation of the concrete crack and acts on the FRP cloth. When the prestress of the FRP cloth reaches 200Mpa (ordinary prestressed wrapping), the theoretical strength of the overall working performance of the standard test block is greatly improved compared with the simple FRP cloth circumferential wrapping. In the above process, the FRP cloth 2 will further deform to produce greater tensile stress to effectively constrain the concrete test block and the FRP plate composite structure, which will better play the advantage of the high tensile strength of the FRP cloth. When the prestressed strength is further increased, the working performance of the composite structure will be further enhanced. If only FRP cloth is used for reinforcement, the strengthening effect on the concrete column is more inclined to two-way stress reinforcement. When the FRP composite plate is used as an auxiliary, the strengthening effect on the concrete column becomes three-way stress reinforcement. The effect of three-dimensional stress on the axial compressive strength of concrete columns is higher than that of two-dimensional stress. Due to the cracks in the concrete test block, the concrete of the FRP plate A3 corresponding to the concrete test block and the plate A3 slide downward. The FRP plate A3 and the FRP plate C5 squeeze the FRP plate B4. The concrete at the crack will expand slightly outward, causing the FRP plate B4 to arch outward and transmit to the FRP cloth 2, causing the deformation of the FRP cloth 2 to cause greater tensile stress and become circumferential compressive stress. In this process, in addition to the tensile suppression of the concrete cracks by the external bonding FRP plate, the deformation of the FRP plate B4 effectively amplifies the deformation of the concrete cracks and acts on the FRP cloth 2. When the prestress of the FRP cloth 2 reaches 200Mpa (ordinary prestressed wrapping), the theoretical strength of the overall working performance of the standard test block is greatly improved compared with the simple FRP cloth circumferential wrapping. In the above process, the FRP cloth 2 will further deform to produce greater tensile stress, which will effectively constrain the concrete test block and the FRP board composite plate, which will better play the advantage of the high tensile strength of the FRP cloth. When the prestressed strength is further increased, the working performance of the composite structure will be further enhanced.

[0042] like Figure 3 ,Through the force analysis, FRP plate A3 and FRP plate C5 will generate a torque when the load increases. Although the restraining capacity of the concrete around the crack is weakened to a certain extent, this will further increase the deformation of FRP cloth 2, thereby generating greater tensile stress in the concrete corresponding to FRP plate B4, i.e., the crack of the concrete;

[0043] like Figure 5As shown in the figure, through the force analysis, FRP plate A3 and FRP plate C5 will generate a torque when the load increases. Although the restraining capacity of the concrete around the crack is weakened to a certain extent, this will further increase the deformation of the FRP cloth, thereby generating greater tensile stress in the concrete corresponding to FRP plate B4, that is, the crack of the concrete.

[0044] After preliminary judgment, when the prestressed FRP cloth does not exceed the tensile strength of the FRP cloth under the action of the prestress F, it does not exceed the compressive strength of the FRP plate. It is assumed that the various parts of the FRP plate A3 and the FRP plate C5 are constrained by the same FRP cloth.

[0045] Under the above conditions:

[0046]

[0047]

[0048]

[0049] F'=0

[0050] 2bsin 3 α-2Lcos 3 α-L=0

[0051] Solved

[0052]

[0053]

[0054] Where:

[0055] σ——compressive stress of FRP plate, N

[0056] a——length of the long side of FRP plate II, m

[0057] F N ——The sum of the vertical compressive stresses on plate II, N

[0058] A——Cross-sectional area of ​​the side of plate II close to the crack, m 2

[0059] According to the above relationship formula, the reasonable length of the FRP composite plate can be selected according to the crack size on the concrete column, and the various parameters of the FRP plate composite plate can be designed and integrated to ensure the stability of the structure in the concrete column reinforcement and to avoid ineffective reinforcement to a certain extent to improve economic benefits.

[0060] The present invention provides a novel design structure of FRP outer-wrapped cracked concrete, which adopts a variety of FRP materials, improves the offset through the synergistic effect of FRP plates and FRP cloths, and further improves the centripetal force on the basis of centripetal prestress through the deformation of FRP cloths. The structural design adopts a three-dimensional stress method to reinforce the same crack, which can effectively solve the strain hysteresis problem caused by the transition buffer of the bonding surface of the FRP cloth, and at the same time effectively exert the compressive strength of the FRP plates, solving several problems existing in the prior art. In particular, the structure has a certain reduction in the requirements for the prestress of the FRP cloth, and effectively reduces the requirements for tools. Through the outer-wrapped structure, the expansion of the internal volume of the concrete and the displacement of the internal components are constrained to improve the overall strength of the concrete, and to a certain extent solve the adverse effects of the late re-cracking of the concrete cracks caused by the low toughness and poor cracking resistance of epoxy resin.

[0061] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0062] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. A FRP-encased cracked concrete structure, characterized in that: It comprises an FRP cloth (2), an FRP plate composite board A (3), an FRP plate composite board B (4), and an FRP plate composite board C (5), wherein the FRP plate composite board B (4) is attached to the cracked part of the concrete column (1) by a resin layer, and the FRP plate composite board C (5), the FRP plate composite board A (3), the FRP plate composite board B (4) and the FRP plate composite board C (5) are tied to the fractured part of the concrete column (1) through the FRP cloth (2), and the FRP plate composite board A (3) and the FRP plate composite board C (5) are attached to the two inclined surfaces of the FRP plate composite board B (4) respectively and attached to the surface of the concrete column (1) at the same time; The cross section of the FRP plate assembly board A (3) is a parallelogram; the cross section of the FRP plate assembly board B (4) is an isosceles trapezoid; the cross section of the FRP plate assembly board C (5) is a parallelogram; the covering density of the FRP cloth (2) on the FRP plate assembly board A (3), the FRP plate assembly board B (4) and the FRP plate assembly board C (5) is different, and the FRP cloth (2) on the FRP plate assembly board A (3) and the FRP plate assembly board C (5) is denser than the FRP cloth (2) on the FRP plate assembly board B (4).

Citation Information

Patent Citations

  • Construction method of prestress carbon fiber cloth reinforced reinforced-concrete square pillar

    CN106522577A

  • Construction method for additionally arranging cushion block outside carbon fiber cloth enhanced reinforced concrete square column

    CN106592997A

  • Anchoring device for concrete column

    CN107035158A

  • Method for reinforcing reinforced concrete pier stud through prestress FRP cloth

    CN107059665A

  • FRP section-steel composite pipe concrete combination column

    CN108240071A