A transparent back plate and production method thereof
By using PET film, hot melt adhesive layer, fluorine-containing film and POE or PE particles, combined with laminating process and UV or EB radiation technology, the problem of high price of transparent backsheet is solved, cost reduction and quality improvement are achieved, and it is suitable for Photovoltaic modules meet the demand for "affordable grid access" for photovoltaic modules.
Patent Information
- Application Number
- CN202010385549.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-05-09
- Publication Date
- 2024-10-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing transparent backsheet production processes and raw materials result in high prices, which cannot meet the "affordable grid" demand for photovoltaic modules, and the supply of production technology and raw materials is limited.
Using PET film as the base material, with hot melt adhesive layer and fluorine-containing film, adding POE or PE particles and additives, and cross-linking through laminating process and UV or EB radiation technology, avoiding the traditional coating process and chemical heat Cross-linking reduces costs and environmental risks.
The cost is significantly reduced without reducing quality, the weather resistance and mechanical properties of the transparent backsheet are improved, the optical loss problem is solved, the power gain is enhanced, and a green, environmentally friendly and efficient production process is achieved.
Smart Images

Figure CN111446320B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of photovoltaics, and in particular to a transparent backplane and a production method thereof. Background Art
[0002] With the increasing popularity of bifacial cells and the demand for cost reduction in both domestic and international markets, particularly the special exemption for bifacial modules under the US Section 201 Act, bifacial modules have been actively developed and tested by module manufacturers. Raw material manufacturers have also increased their investment in the development of transparent backsheets for bifacial modules. However, the current production process and raw material selection of transparent backsheets make them expensive, costing two to three times the price of conventional backsheets. This has hindered large-scale mass production. Furthermore, the production technology and raw material selection are limited to a few suppliers, failing to meet the original goal of achieving "grid parity" for photovoltaics. Summary of the Invention
[0003] The present invention aims to provide a transparent back plate and a production method thereof.
[0004] In order to achieve the above technical objectives, the present invention adopts the following technical scheme: a transparent backboard, the transparent backboard is based on PET film, the upper and lower layers of the PET film are hot melt adhesive layers, the upper layer is the outer hot melt adhesive layer, and the lower layer is the inner hot melt adhesive layer. The lower layer of the inner hot melt adhesive layer is compounded with a fluorine-containing film, and the upper and lower hot melt adhesive layers are added with plastic particles and additives, and the plastic particles are POE or PE particles.
[0005] Preferably, the thickness of the PET film is 250-300 μm, and the light transmittance is greater than 85%.
[0006] Preferably, the thickness of the fluorine-containing film is 20-50um, the fluorine content is not less than 10%, the transmittance is greater than 85%, and a white grid is affixed to the side of the fluorine-containing film that is attached to the inner hot melt adhesive layer. The reflectivity of the grid part is greater than 85%, and the grid part is made of glazed material.
[0007] Preferably, the grid pattern size error is 2 mm, and the thickness of the white grid is controlled at 5-25 μm.
[0008] Preferably, the auxiliary agents include photoinitiators, co-crosslinking agents, monomers, reactive diluents, antioxidants, light stabilizers, tackifiers, and wetting agents.
[0009] A method for producing a transparent backplane comprises the following steps:
[0010] S1. Select the film, choose PET (polyester film), thickness of 250-300um, light transmittance > 85%;
[0011] S2. Prepare hot melt adhesive and mix various additives, including photoinitiators, co-crosslinking agents, monomers, reactive diluents, antioxidants, light stabilizers, tackifiers, and wetting agents. The powdered additives are ground and mixed with other ground powdered additives. The powdered additives are ground to ≥200 mesh. The mass proportion of each additive in the adhesive is 0.5-5%, and the total proportion does not exceed 10%; S3. The flaky additives are melted and mixed with the liquid additives. The flaky additives are mixed at 100°C for half an hour before preparation. Then, the powdered additives processed in step S2 are added to the liquid additives for mixing and stirring;
[0012] S4. Add plastic particles into the stirring tank. The plastic particles are POE or PE particles. First, add the plastic particles into the stirring tank. The particle mixing temperature does not exceed 50° C. Then, add the additive stirred in step S3 and mix together until the additive is absorbed into the particles.
[0013] S5. After the mixing and stirring in step S4 is completed, the mixed particles are granulated, and the granulation temperature is controlled at 200±20°C;
[0014] S6. Using the mixed particles mentioned above to perform extrusion lamination, that is, uniformly coating the thermoplastic particles on a PET substrate under certain conditions, and coating both sides of the PET simultaneously or step by step according to different laminating equipment, and at the same time laminating one side with a fluorine-containing film, wherein the thickness of the fluorine-containing film is 20-50 μm, the fluorine content is not less than 10%, and the transmittance is greater than 85%. One side of the fluorine-containing film is provided with a white grid, and the side of the fluorine-containing film with the white grid is laminated with the PET substrate, the reflectivity of the grid portion is greater than 85%, and the grid portion is coated with a glaze material. Specifically, the fluorine-containing film adopts a grid coating process technology, and the inner side of the fluorine film is coated with a white reticulated glaze powder material;
[0015] S7. The semi-finished product is subjected to a cross-linking pretreatment by UV or EB radiation to improve the peeling force with PET and self-cross-linking.
[0016] Preferably, in step S7, when the semi-finished product is subjected to cross-linking pretreatment, the UV irradiation conditions are controlled at 800-2000 mj / cm2, and the EB irradiation conditions are controlled at 30-70 kGy.
[0017] Preferably, the POE or PE particles have a melt index of 3-20 g / 10 min, a melting temperature greater than 105° C., a light transmittance greater than 90%, and a haze less than 1%.
[0018] Preferably, POE or PE particles are used as the main particles, and EVA particles or PVB particles are selected as auxiliary particles. When EVA particles are selected as auxiliary particles, the melt index is required to be 3-20g / 10min, the melting temperature is greater than 45°C, the transmittance is greater than 90%, and the haze is less than 1%. When PVB particles are selected as auxiliary particles, the melt index is required to be 1-10g / 10min, the melting temperature is greater than 120°C, the transmittance is greater than 90%, and the haze is less than 1%. The mass ratio between the main particles and the auxiliary particles is ≥7:3.
[0019] Preferably, the adhesive is added with vinyl-terminated silicone resin with a vinyl content of 0.5% to 5%. Adding vinyl-terminated silicone to the hot melt adhesive can accelerate cross-linking and improve weather resistance, resulting in more excellent performance, simple and efficient production process, and significant innovation, which meets the country's demand for innovation.
[0020] The innovation of this invention is that it addresses the current high price of transparent backplanes and takes a different approach. It uses new equipment, processes and raw materials to significantly reduce costs without reducing quality. Based on this, a series of related products can be developed, including the development of transparent grid backplanes, which creates positive conditions for rapidly opening up the market. In addition, products can be customized according to customer needs. The development of grid fluorine films and grid transparent backplanes has practical significance and can be applied to photovoltaic modules. It not only solves the optical loss caused by transparency and enhances power gain, but also selects PET film as the base material of this backplane, which provides good mechanical properties and electrical insulation properties, and is not prone to shrinkage and deformation under certain high-temperature operations. The solvent-free thermoplastic hot melt adhesive used avoids the dangers and environmental problems of traditional adhesive solvents, complies with national environmental protection policy requirements, does not produce "three wastes", and is green, environmentally friendly, safe and efficient; the lamination process is used to avoid the traditional coating process, which is not only safe and environmentally friendly, but also highly efficient, reducing supporting requirements and investment funds; the use of UV or EB and other radiation technologies is stable and mature, avoiding traditional chemical thermal cross-linking technology. The entire process does not require the use and management of hazardous chemicals, and the operation is simple and safe, with no safety hazards in production. The textured fluorine film produced by the textured coating method can be customized in texture size and specifications according to the component layout design to prepare a textured transparent backplane and put it into production in the textured transparent backplane component.
[0021] The present invention abandons traditional liquid adhesives and adopts environmentally friendly and safe hot melt adhesive as the adhesive of the composite film. It also adopts a new process and new equipment, which saves energy consumption, eliminates the emission of "three wastes", and has the function of curing under UV or EB radiation. Therefore, the film coating and curing can be completed in one process, and it can be double-coated on one side or double-coated on both sides. It is different from traditional hot melt adhesives. Traditional hot melt adhesives are thermoplastic and cannot be converted into thermosetting types. Therefore, their usage conditions are limited and they cannot be used under high temperature conditions. This hot melt adhesive can be cross-linked and cured under UV or EB conditions after adding relevant additives. Moreover, traditional hot melt adhesives have poor weather resistance and are often used under mild conditions such as indoors. They cannot withstand the stringent weather resistance requirements of photovoltaic modules for adhesives.
[0022] The present invention selects EVA, PE, POE, and PVB particles with good weather resistance and transparency and combines them with other additives, so that the hot melt adhesive has cross-linking and curing functions under UV or EB conditions, enhances the bonding strength of the hot melt adhesive with the substrate and backing film, and also improves the heat and cold resistance and mechanical properties of the hot melt adhesive. The selection of suitable additives makes this hot melt adhesive have excellent weather resistance and anti-UV aging properties. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 is a flow chart of the production method of the present invention;
[0024] Figure 2 Schematic diagram of the transparent backplane of the present invention.
[0025] In the figure: 1. PET film; 2. Outer hot melt adhesive layer; 3. Inner hot melt adhesive layer; 4. Fluorine-containing film. DETAILED DESCRIPTION
[0026] The following describes embodiments of the present invention in detail. Examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended only to explain the present invention and are not to be construed as limiting the present invention.
[0027] In the description of the present invention, unless otherwise specified or limited, it should be noted that the terms "mounted," "connected," and "connected" should be understood broadly. For example, they may refer to mechanical or electrical connections, internal communication between two components, and direct or indirect connection through an intermediary. Those skilled in the art will understand the specific meanings of these terms based on specific circumstances.
[0028] A transparent backboard, which uses a PET film 1 as a base material. The upper and lower layers of the PET film are hot melt adhesive layers, respectively. The upper layer is an outer hot melt adhesive layer 2, and the lower layer is an inner hot melt adhesive layer 3. The lower layer of the inner hot melt adhesive layer 3 is compounded with a fluorine-containing film 4. Plastic particles and additives are added to the upper and lower hot melt adhesive layers. The plastic particles are POE or PE particles.
[0029] Preferably, the thickness of the PET film 1 is 250-300 μm, and the light transmittance is greater than 85%.
[0030] Preferably, the thickness of the fluorine-containing film 4 is 20-50um, the fluorine content is not less than 10%, and the transmittance is greater than 85%. A white grid is affixed to the side of the fluorine-containing film 4 that is attached to the inner hot melt adhesive layer. The reflectivity of the grid part is greater than 85%, and the grid part is made of glazed material.
[0031] Preferably, the grid pattern size error is 2 mm, and the thickness of the white grid is controlled at 5-25 μm.
[0032] Preferably, the auxiliary agents include photoinitiators, co-crosslinking agents, monomers, reactive diluents, antioxidants, light stabilizers, tackifiers, and wetting agents.
[0033] A method for producing a transparent backplane comprises the following steps:
[0034] S1. Select the film, choose PET (polyester film), thickness of 250-300um, light transmittance > 85%;
[0035] S2. Prepare hot melt adhesive and mix various additives, including photoinitiators, co-crosslinking agents, monomers, reactive diluents, antioxidants, light stabilizers, tackifiers, and wetting agents. The powdered additives are ground and mixed with other ground powdered additives. The powdered additives are ground to ≥200 mesh. The mass proportion of each additive in the adhesive is 0.5-5%, and the total proportion does not exceed 10%; S3. The flaky additives are melted and mixed with the liquid additives. The flaky additives are mixed at 100°C for half an hour before preparation. Then, the powdered additives processed in step S2 are added to the liquid additives for mixing and stirring;
[0036] S4. Add plastic particles into the stirring tank. The plastic particles are POE or PE particles. First, add the plastic particles into the stirring tank. The particle mixing temperature does not exceed 50° C. Then, add the additive stirred in step S3 and mix together until the additive is absorbed into the particles.
[0037] S5. After the mixing and stirring in step S4 is completed, the mixed particles are granulated, and the granulation temperature is controlled at 200±20°C;
[0038] S6. Using the mixed particles mentioned above to perform extrusion lamination, that is, uniformly coating the thermoplastic particles on a PET substrate under certain conditions, and coating both sides of the PET simultaneously or step by step according to different laminating equipment, and at the same time laminating one side with a fluorine-containing film, wherein the thickness of the fluorine-containing film is 20-50 μm, the fluorine content is not less than 10%, and the transmittance is greater than 85%. One side of the fluorine-containing film is provided with a white grid, and the side of the fluorine-containing film with the white grid is laminated with the PET substrate, the reflectivity of the grid portion is greater than 85%, and the grid portion is coated with a glaze material. Specifically, the fluorine-containing film adopts a grid coating process technology, and the inner side of the fluorine film is coated with a white reticulated glaze powder material;
[0039] S7. The semi-finished product is subjected to a cross-linking pretreatment by UV or EB radiation to improve the peeling force with PET and self-cross-linking.
[0040] Preferably, in step S7, when the semi-finished product is subjected to cross-linking pretreatment, the UV irradiation conditions are controlled at 800-2000 mj / cm2, and the EB irradiation conditions are controlled at 30-70 kGy.
[0041] Preferably, the POE or PE particles have a melt index of 3-20 g / 10 min, a melting temperature greater than 105° C., a light transmittance greater than 90%, and a haze less than 1%.
[0042] Preferably, POE or PE particles are used as the main particles, and EVA particles or PVB particles are selected as auxiliary particles. When EVA particles are selected as auxiliary particles, the melt index is required to be 3-20g / 10min, the melting temperature is greater than 45°C, the transmittance is greater than 90%, and the haze is less than 1%. When PVB particles are selected as auxiliary particles, the melt index is required to be 1-10g / 10min, the melting temperature is greater than 120°C, the transmittance is greater than 90%, and the haze is less than 1%. The mass ratio between the main particles and the auxiliary particles is ≥7:3.
[0043] Preferably, the adhesive is added with vinyl-terminated silicone resin with a vinyl content of 0.5% to 5%. Adding vinyl-terminated silicone to the hot melt adhesive can accelerate cross-linking and improve weather resistance, resulting in more excellent performance, simple and efficient production process, and significant innovation, which meets the country's demand for innovation.
[0044] The innovation of this invention is that it addresses the current high price of transparent backplanes and takes a different approach. It uses new equipment, processes and raw materials to significantly reduce costs without reducing quality. Based on this, a series of related products can be developed, including the development of transparent grid backplanes, which creates positive conditions for rapidly opening up the market. In addition, products can be customized according to customer needs. The development of grid fluorine films and grid transparent backplanes has practical significance and can be applied to photovoltaic modules. It not only solves the optical loss caused by transparency and enhances power gain, but also selects PET film as the base material of this backplane, which provides good mechanical properties and electrical insulation properties, and is not prone to shrinkage and deformation under certain high-temperature operations. The solvent-free thermoplastic hot melt adhesive used avoids the dangers and environmental problems of traditional adhesive solvents, complies with national environmental protection policy requirements, does not produce "three wastes", and is green, environmentally friendly, safe and efficient; the lamination process is used to avoid the traditional coating process, which is not only safe and environmentally friendly, but also highly efficient, reducing supporting requirements and investment funds; the use of UV or EB and other radiation technologies is stable and mature, avoiding traditional chemical thermal cross-linking technology. The entire process does not require the use and management of hazardous chemicals, and the operation is simple and safe, with no safety hazards in production. The textured fluorine film produced by the textured coating method can be customized in texture size and specifications according to the component layout design to prepare a textured transparent backplane and put it into production in the textured transparent backplane component.
[0045] The present invention abandons traditional liquid adhesives and adopts environmentally friendly and safe hot melt adhesive as the adhesive of the composite film. It also adopts a new process and new equipment, which saves energy consumption, eliminates the emission of "three wastes", and has the function of curing under UV or EB radiation. Therefore, the film coating and curing can be completed in one process, and it can be double-coated on one side or double-coated on both sides. It is different from traditional hot melt adhesives. Traditional hot melt adhesives are thermoplastic and cannot be converted into thermosetting types. Therefore, their usage conditions are limited and they cannot be used under high temperature conditions. This hot melt adhesive can be cross-linked and cured under UV or EB conditions after adding relevant additives. Moreover, traditional hot melt adhesives have poor weather resistance and are often used under mild conditions such as indoors. They cannot withstand the stringent weather resistance requirements of photovoltaic modules for adhesives.
[0046] The present invention selects EVA, PE, POE, and PVB particles with good weather resistance and transparency and combines them with other additives, so that the hot melt adhesive has cross-linking and curing functions under UV or EB conditions, enhances the bonding strength of the hot melt adhesive with the substrate and backing film, and also improves the heat and cold resistance and mechanical properties of the hot melt adhesive. The selection of suitable additives makes this hot melt adhesive have excellent weather resistance and anti-UV aging properties.
[0047] Throughout this specification, references to "one embodiment," "example," or "some examples" indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the present invention. In this specification, schematic representations of these terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in any one or more embodiments or examples.
[0048] While embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions, and variations may be made to the embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the claims and their equivalents.
Claims
1. A transparent backplane, characterized in that: The transparent back panel is based on PET film. The upper and lower layers of the PET film are hot melt adhesive layers respectively. The upper layer is the outer hot melt adhesive layer, and the lower layer is the inner hot melt adhesive layer. The lower layer of the inner hot melt adhesive layer is compounded with a fluorine-containing film. Plastic particles and additives are added to the upper and lower hot melt adhesive layers. The plastic particles are POE or PE particles.
2. The transparent backplane according to claim 1 is characterized in that the thickness of the PET film is 250-300 um and the transmittance is greater than 85%.
3. The transparent back panel according to claim 1 is characterized in that the thickness of the fluorine-containing film is 20-50um, the fluorine content is not less than 10%, the transmittance is greater than 85%, a white grid is attached to the side of the fluorine-containing film that is attached to the inner hot melt adhesive layer, the reflectivity of the grid part is greater than 85%, and the grid part is made of glazed material.
4. The transparent backplane according to claim 3 is characterized in that the grid pattern size error is 2 mm and the thickness of the white grid is controlled within 5-25 um.
5. The transparent back sheet according to claim 1 is characterized in that the auxiliary agent specifically includes a photoinitiator, a co-crosslinking agent, a monomer, a reactive diluent, an antioxidant, a light stabilizer, a tackifier, and a wetting agent.
6. A method for producing a transparent backplane, characterized in that: The following steps are involved: S1. Select the film, choose PET (polyester film), with a thickness of 250-300um and a light transmittance of >85%; S2, prepare hot melt adhesive, mix various additives, the additives specifically include photoinitiator, co-crosslinking agent, monomer, active diluent, antioxidant, light stabilizer, tackifier, wetting agent, the powdered additive is ground and mixed with other ground powdered additives, the powdered additive is ground to ≥200 mesh, the mass proportion of various additives in the adhesive is 0.5-5%, and the total proportion does not exceed 10%; S3, the flaky additive is melted and mixed with the liquid additive, the flaky additive is mixed at 100°C for half an hour before preparation, and then the powdered additive processed in step S2 is added to the liquid additive for mixing and stirring; S4, adding plastic particles into the stirring tank, the plastic particles are POE or PE particles, first adding the plastic particles into the stirring tank, the particle mixing temperature does not exceed 50° C., and then adding the additives stirred in step S3 and mixing together until the additives are absorbed into the particles; S5. After the mixing and stirring in step S4 is completed, the mixed particles are granulated, and the granulation temperature is controlled at 200±20°C; S6. Use the mixed particles to perform extrusion coating, that is, evenly coat the thermoplastic particles on the PET substrate under certain conditions, and coat both sides of the PET synchronously or step by step according to different coating equipment, and compound with a fluorine-containing film on one side at the same time. The thickness of the fluorine-containing film is 20-50um, the fluorine content is not less than 10%, and the light transmittance is greater than 85%. One side of the fluorine-containing film has a white grid, and the side of the fluorine-containing film with the white grid is compounded with the PET substrate, the reflectivity of the grid part is greater than 85%, and the grid part adopts glaze material. The fluorine-containing film specifically adopts the grid coating process technology, and the inner side of the fluorine film is coated with white mesh using glaze powder material; S7, the semi-finished product is subjected to cross-linking pretreatment by UV or EB radiation to improve the peeling force with PET and self-cross-linking.
7. The production method according to claim 6 is characterized in that, when the semi-finished product is subjected to cross-linking pretreatment in step S7, the UV irradiation condition is controlled at 800-2000 mj / cm2, and the EB irradiation condition is controlled at 30-70 kGy.
8. The production method according to claim 6, characterized in that: The melt index of POE or PE particles is 3-20g / 10min, the melting temperature is greater than 105°C, the light transmittance is greater than 90%, and the haze is less than 1%.
9. The production method according to claim 8, characterized in that: POE or PE particles are used as the main particles, and EVA particles or PVB particles are used as auxiliary particles. When EVA particles are used as auxiliary particles, the melt index is required to be 3-20g / 10min, the melting temperature is greater than 45°C, the transmittance is greater than 90%, and the haze is less than 1%. When PVB particles are used as auxiliary particles, the melt index is required to be 1-10g / 10min, the melting temperature is greater than 120°C, the transmittance is greater than 90%, and the haze is less than 1%. The mass ratio between the main particles and the auxiliary particles is ≥7:
3.
10. The production method according to claim 6, characterized in that: The adhesive contains vinyl-terminated silicone resin with a vinyl content of 0.5% to 5%.
Citation Information
Patent Citations
Transparent back plate
CN212571013U