Segmented air-breaking device and method for semiconductor thin film vacuum vapor deposition production

By introducing a segmented air-breaking device in the semiconductor thin film vacuum deposition production line, the vacuum degree control of the buffer transition zone is used to solve the problem of gasification or sublimation of the film in the slow-cooled zone, and high-quality thin film deposition and production line are achieved. Working normally.

CN111647868BActive Publication Date: 2024-11-26CHINA TRIUMPH INT ENG CO LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910160889.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-03-04
Publication Date
2024-11-26
Estimated Expiration
2039-03-04

AI Technical Summary

Technical Problem

During the vacuum deposition of semiconductor thin films, the vacuum environment of the thin film deposition zone and the slow-cooling zone in the existing production line devices is the same, resulting in the semiconductor thin film deposited on the substrate being vaporized or sublimated in the slow-cooling zone, resulting in waste and pollution of materials. Affects production.

Method used

Design a segmented air-breaking device, including a thin film deposition area, a buffer transition area and a slow cooling area, the vacuum degree of the slow cooling area is more than 10 times lower than that of the thin film deposition area, and is controlled in the buffer transition area through the conveying mechanism and vacuum system. The vacuum degree conversion prevents the semiconductor film from being vaporized or sublimated in the slow cooling zone.

Benefits of technology

Effectively prevent the gasification or sublimation of semiconductor films in the slow-cooled zone, ensure product quality, avoid material waste and pollution, and ensure the normal operation of the production line.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111647868B_ABST
    Figure CN111647868B_ABST
Patent Text Reader

Abstract

The present invention provides a segmented air-breaking device and method for semiconductor thin film vacuum vapor deposition production. The segmented air-breaking device includes a thin film deposition area, a buffer transition area, and a slow cooling area arranged in sequence along the moving direction of the substrate. The thin film deposition area, the buffer transition area, and the slow cooling area are all vacuum chambers. The vacuum degree in the slow cooling area is more than 10 times lower than the vacuum degree in the thin film deposition area. A conveying mechanism for transferring the substrate is arranged in the buffer transition area. In the present application, the thin film deposition area and the slow cooling area are separated by an additional buffer transition area, so that the vacuum degree in the slow cooling area is more than 10 times lower than the vacuum degree in the thin film deposition area; therefore, when the substrate removed from the thin film deposition area and deposited with the semiconductor thin film is slowly cooled in the slow cooling area, the semiconductor thin film deposited on the substrate no longer vaporizes or sublimates, thereby ensuring product quality, while also avoiding material waste and contamination of the slow cooling area and the mechanisms in the slow cooling area.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a semiconductor thin film deposition technology, in particular to a segmented air-breaking device and method for semiconductor thin film vacuum vapor deposition production. Background Art

[0002] In the process of vacuum vapor deposition of semiconductor thin films, in order to obtain high-performance semiconductor thin films, the substrate needs to be preheated to a certain temperature. For example, when cadmium telluride thin films are vapor deposited, the temperature of the substrate conductive glass needs to be preheated to above 550°C; when copper indium gallium selenide thin films are deposited by co-evaporation, the temperature of the conductive substrate needs to be preheated to above 550°C. Under vacuum conditions, such as <100Pa, when the semiconductor gas phase material reaches the substrate whose temperature is lower than that of the gas phase material, on the one hand, the gas phase material is deposited on the substrate to form a semiconductor thin film, and on the other hand, part of the semiconductor thin film is vaporized or sublimated due to the higher substrate temperature; but because the deposition rate is greater than the vaporization or sublimation rate, a semiconductor thin film is finally deposited on the substrate. The higher the substrate temperature, the fewer defects the obtained semiconductor thin film has.

[0003] In order to realize the large-scale vacuum vapor deposition production of semiconductor thin films, such as Figure 1 As shown, the current production line device includes a thin film deposition area 100 and a slow cooling area 200 which are arranged successively along the moving direction of the substrate. The substrate enters the thin film deposition area, completes the semiconductor thin film deposition, and then enters the slow cooling area, and stays in the slow cooling area for a period of time until the substrate temperature drops to a certain temperature, and then the substrate with the semiconductor material deposited is moved out of the slow cooling area. However, in the existing production line device, the thin film deposition area and the slow cooling area are arranged adjacent to each other, so that the vacuum environment of the thin film deposition area and the vacuum environment of the slow cooling area are the same. Combined with the fact that the substrate needs to stay in the slow cooling area for a period of time, this causes the semiconductor film deposited on the substrate in the slow cooling area to vaporize or sublimate, thereby causing the semiconductor film on the substrate to be thinned and waste materials, and the vaporized or sublimated semiconductor film will contaminate the cavity and the transmission roller of the slow cooling area, affecting normal production. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, the object of the present invention is to provide a segmented vapor-breaking device for semiconductor thin film vacuum vapor deposition production, which can prevent the semiconductor thin film deposited on the substrate from vaporizing or sublimating in the slow cooling zone.

[0005] To achieve the above-mentioned purpose, the present invention provides a segmented air-breaking device for semiconductor thin film vacuum vapor deposition production, comprising a thin film deposition zone, a buffer transition zone, and a slow cooling zone arranged in sequence along the moving direction of the substrate, wherein the thin film deposition zone, the buffer transition zone, and the slow cooling zone are all vacuum chambers, the vacuum degree in the slow cooling zone is more than 10 times lower than the vacuum degree in the thin film deposition zone, and a conveying mechanism for transferring the substrate is arranged in the buffer transition zone.

[0006] Furthermore, the vacuum degree in the slow cooling zone is 40-60 times lower than the vacuum degree in the thin film deposition zone.

[0007] Furthermore, the semiconductor material deposited on the substrate in the thin film deposition area is cadmium telluride; the vacuum degree of the thin film deposition area is 20Pa, and the vacuum degree of the slow cooling area is 1000Pa.

[0008] Furthermore, the conveying mechanism transfers the substrate in the buffer transition zone at a speed of 10-30 m / min.

[0009] Furthermore, the buffer transition zone is provided with an inlet portion connecting the thin film deposition zone and the buffer transition zone, an outlet portion connecting the buffer transition zone and the slow cooling zone, an inlet-end gate valve arranged at the inlet portion and capable of opening and closing the inlet portion, and an outlet-end gate valve arranged at the outlet portion and capable of opening and closing the outlet portion, and both ends of the conveying mechanism extend to the inlet portion and the outlet portion, respectively.

[0010] Furthermore, the segmented air-breaking device also includes a vacuum system connected to the buffer transition zone; when the inlet gate valve and the outlet gate valve are both closed, the vacuum system is opened so that the buffer transition zone has the same vacuum degree as the thin film deposition zone; when the inlet gate valve is opened or the outlet gate valve is opened, the vacuum system is closed.

[0011] Furthermore, the vacuum system is a separate vacuum pump set.

[0012] Furthermore, the conveying mechanism includes a plurality of conveying rollers arranged in the buffer transition area, the plurality of conveying rollers are arranged in sequence along the moving direction of the substrate, and each conveying roller extends in a direction perpendicular to the moving direction of the substrate.

[0013] Furthermore, the segmented air breaking device also includes an inlet chamber, a preheating zone and an outlet chamber. The inlet chamber, preheating zone, thin film deposition zone, buffer transition zone, slow cooling zone, and outlet chamber are arranged in sequence along the moving direction of the substrate. The vacuum degree in the preheating zone is the same as the vacuum degree in the thin film deposition zone.

[0014] Furthermore, the preheating zone and the buffer transition zone share a vacuum system.

[0015] The present invention also provides a segmented gas-breaking method for semiconductor thin film vacuum vapor deposition production, using the segmented gas-breaking device as described above, the segmented gas-breaking method sequentially comprises the following steps:

[0016] S1, cleaning substrate;

[0017] S2, preheating the substrate, and after the substrate temperature reaches the set preheating temperature, the substrate enters the thin film deposition area;

[0018] S3, depositing a semiconductor thin film on the surface of the substrate in the thin film deposition area;

[0019] S4, the substrate with the semiconductor thin film deposited thereon moves from the thin film deposition area to the buffer transition area, and the conveying mechanism in the buffer transition area moves the substrate to the slow cooling area; when the substrate enters the buffer transition area from the thin film deposition area, the thin film deposition area and the buffer transition area are connected, and the buffer transition area and the slow cooling area are not connected; when the substrate moves from the buffer transition area to the slow cooling area, the thin film deposition area and the buffer transition area are not connected, and the buffer transition area and the slow cooling area are connected;

[0020] S5. All substrates enter the slow cooling zone. After the substrate temperature drops to the set pre-cooling temperature, the substrates break through the air and leave the vacuum cavity in the segmented air-breaking device.

[0021] Furthermore, in step S2, the preheating temperature is 550°C.

[0022] Furthermore, in step S5, the precooling temperature is 200°C.

[0023] As described above, the segmented air-breaking device and method for semiconductor thin film vacuum vapor deposition production according to the present invention have the following beneficial effects:

[0024] In the present application, the thin film deposition area and the slow cooling area are separated by an additional buffer transition area, so that the thin film deposition area and the slow cooling area have different vacuum degrees, and in particular, the vacuum degree in the slow cooling area is more than 10 times lower than the vacuum degree in the thin film deposition area; therefore, when the substrate with the semiconductor thin film deposited thereon removed from the thin film deposition area is slowly cooled in the slow cooling area, the semiconductor thin film deposited on the substrate no longer vaporizes or sublimates, thereby ensuring product quality, while also avoiding material waste and pollution of the slow cooling area and the various mechanisms in the slow cooling area, thereby ensuring normal production of the production line. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a schematic diagram of the structure of a semiconductor thin film production line device in the prior art.

[0026] Figure 2 This is a schematic diagram of the structure of the segmented air-breaking device in this application.

[0027] Figure 3 for Figure 2 Schematic diagram of the structure of the middle buffer transition zone.

[0028] Component number description

[0029] 1. Entrance Room

[0030] 2 Preheating Zone

[0031] 3 Film deposition area

[0032] 4 Buffer transition zone

[0033] 41 Import Department

[0034] 42 Export Department

[0035] 5 Slow cooling area

[0036] 6 Exit Room

[0037] 7 Vacuum system

[0038] 8 Transmission mechanism

[0039] 81 conveyor roller

[0040] 9 substrate DETAILED DESCRIPTION

[0041] The following is a description of the implementation of the present invention by means of specific embodiments. Those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification.

[0042] It should be noted that the structures, proportions, sizes, etc. drawn in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the limiting conditions for the implementation of the present invention, so they have no substantial technical significance. Any modification of the structure, change of the proportional relationship or adjustment of the size should still fall within the scope of the technical content disclosed by the present invention without affecting the effects and purposes that can be achieved by the present invention. At the same time, the terms such as "upper", "lower", "left", "right", "middle" and "one" quoted in this specification are only for the convenience of description, and are not used to limit the scope of the implementation of the present invention. The change or adjustment of their relative relationship should also be regarded as the scope of the implementation of the present invention without substantially changing the technical content.

[0043] The present application provides a segmented air-breaking device and a segmented air-breaking method for semiconductor thin film vacuum vapor deposition production, wherein the segmented air-breaking device constitutes a semiconductor thin film vacuum vapor deposition production line, which can produce semiconductor thin films on a large scale. The preferred embodiment of the segmented air-breaking device is: Figure 2As shown, the segmented air-breaking device includes an inlet chamber 1, a preheating zone 2, a thin film deposition zone 3, a buffer transition zone 4, a slow cooling zone 5, and an outlet chamber 6, which are arranged in sequence along the moving direction of the substrate 9. The preheating zone 2, the thin film deposition zone 3, the buffer transition zone 4, and the slow cooling zone 5 are all vacuum chambers; in addition, the inlet chamber 1 is the transition of the substrate 9 from the atmospheric environment to the vacuum environment, and there are valves between the inlet chamber 1 and the preheating zone 2, and between the inlet chamber 1 and the outside atmosphere. The switch of the valve connected between the inlet chamber 1 and the outside atmosphere provides the conversion of the inlet chamber 1 from the atmosphere to the vacuum, and the movement of the substrate 9 from the atmosphere to the vacuum; and the outlet chamber 6 is the transition of the substrate 9 from the vacuum environment to the atmospheric environment, and there are valves between the outlet chamber 6 and the slow cooling zone 5, and between the outlet chamber 6 and the outside atmosphere. The switch of the valve connected between the outlet chamber 6 and the outside atmosphere provides the conversion of the outlet chamber 6 from the vacuum to the atmosphere, and the movement of the substrate 9 from the vacuum to the atmosphere. In particular, during the semiconductor thin film vapor deposition process, the vacuum degree in the slow cooling zone 5 is more than 10 times lower than the vacuum degree in the thin film deposition zone 3, that is, the vacuum degree in the slow cooling zone 5 is at least one order of magnitude lower than the vacuum degree in the thin film deposition zone 3; at the same time, a conveying mechanism 8 for transferring the substrate 9 is provided in the buffer transition zone 4, and the conveying mechanism 8 moves the substrate 9 toward the slow cooling zone 5; for the convenience of description, the moving direction of the substrate 9 is defined as the forward direction, therefore, Figure 2 In the illustrated views, the left side and the right side of the paper are the rear direction and the front direction, respectively.

[0044] The present application also provides a segmented air-breaking method for semiconductor thin film vacuum vapor deposition production, using the segmented air-breaking device as above, the segmented air-breaking method comprises the following steps in sequence:

[0045] S1 , cleaning the substrate 9 , the cleaned substrate 9 enters the inlet chamber 1 , and after the vacuum degree in the inlet chamber 1 reaches a pre-requirement, the substrate 9 enters the preheating zone 2 from the inlet chamber 1 .

[0046] S2 , preheating the substrate 9 . After the temperature of the substrate 9 reaches a set preheating temperature in the preheating zone 2 , the substrate 9 enters the thin film deposition zone 3 from the preheating zone 2 .

[0047] S3. In the thin film deposition area 3, a semiconductor thin film vacuum deposition technique is used to deposit the required semiconductor thin film on the surface of the substrate 9.

[0048] S4, the substrate 9 deposited with the semiconductor thin film is moved from the thin film deposition area 3 to the buffer transition area 4, and the conveying mechanism 8 in the buffer transition area 4 transfers the substrate 9 to the slow cooling area 5. In the process of transferring the substrate 9, the substrate 9 first enters the buffer transition area 4 from the thin film deposition area 3, that is, a part of the substrate 9 is in the thin film deposition area 3 and the other part is in the buffer transition area 4. At this time, the thin film deposition area 3 and the buffer transition area 4 are connected, and the buffer transition area 4 and the slow cooling area 5 are not connected, so that the vacuum degree of the thin film deposition area 3 and the buffer transition area 4 are the same; in this process, although the vacuum degree of the buffer transition area 4 is the same as that of the thin film deposition area 3, because the conveying mechanism 8 in the buffer transition area 4 transfers the substrate 9 forward, the substrate 9 stays in the vacuum environment with the same vacuum degree as that of the thin film deposition area 3 for a very short time, and only a trace amount of the semiconductor thin film deposited on the substrate 9 is vaporized or sublimated, which will not affect the semiconductor thin film deposited on the substrate 9. Afterwards, the entire substrate 9 enters the buffer transition zone 4. It is preferred that there is no connection between the thin film deposition zone 3 and the buffer transition zone 4, but there is communication between the buffer transition zone 4 and the slow cooling zone 5, so that the vacuum degree in the buffer transition zone 4 is the same as the vacuum degree in the slow cooling zone 5. Finally, the substrate 9 moves from the buffer transition zone 4 to the slow cooling zone 5, that is, a part of the substrate 9 is in the buffer transition zone 4 and the other part is in the slow cooling zone 5. At this time, there is no connection between the thin film deposition zone 3 and the buffer transition zone 4, and there is communication between the buffer transition zone 4 and the slow cooling zone 5, so that the vacuum degrees of the slow cooling zone 5 and the buffer transition zone 4 are the same, which are more than 10 times lower than the vacuum degree of the thin film deposition zone 3, so the semiconductor film deposited on the substrate 9 will not be vaporized or sublimated.

[0049] S5. All substrates 9 enter the slow cooling zone 5. After the temperature of the substrates 9 drops to the set pre-cooling temperature in the slow cooling zone 5, the substrates 9 enter the outlet chamber 6 from the slow cooling zone 5, break through the air and leave the vacuum cavity in the segmented air-breaking device, and enter the outside atmosphere through the outlet chamber 6 to be further cooled to room temperature.

[0050] The present application adds a buffer transition zone 4 between the thin film deposition zone 3 and the slow cooling zone 5, and separates the thin film deposition zone 3 and the slow cooling zone 5 through the buffer transition zone 4, so that the thin film deposition zone 3 and the slow cooling zone 5 have different vacuum degrees, and in particular, the vacuum degree in the slow cooling zone 5 is more than 10 times lower than the vacuum degree in the thin film deposition zone 3. The evaporation or sublimation rate of the semiconductor film deposited on the substrate 9 in the slow cooling zone 5 is reduced to zero by utilizing the characteristic that the evaporation or sublimation rate of the semiconductor material under certain temperature conditions is proportional to the vacuum degree; the higher the vacuum degree, the faster the evaporation or sublimation rate of the semiconductor material; the lower the vacuum degree, the slower the evaporation or sublimation rate of the semiconductor material; when the vacuum degree drops to a certain level, the evaporation or sublimation rate of the semiconductor material drops to zero. Therefore, when the substrate 9 with the semiconductor thin film deposited thereon, which is removed from the thin film deposition area 3, is slowly cooled in the slow cooling area 5, the semiconductor thin film deposited on the substrate 9 will no longer vaporize or sublime, thereby ensuring the integrity of the semiconductor thin film and thus ensuring the product quality. At the same time, it can also avoid material waste and pollution of the slow cooling area 5 and the various mechanisms in the slow cooling area 5, thereby ensuring the normal production of the production line.

[0051] Furthermore, the vacuum degree in the preheating zone 2 is the same as the vacuum degree in the thin film deposition zone 3, and the vacuum degree in the slow cooling zone 5 is 40-60 times, preferably 50 times, lower than the vacuum degree in the thin film deposition zone 3; preferably, the vacuum degree can be represented by a gas pressure value, and the larger the gas pressure value, the lower the vacuum degree, and the smaller the gas pressure value, the higher the vacuum degree. The conveying mechanism 8 transfers the substrate 9 in the buffer transition zone 4 at a transfer speed of 10-30m / min. In addition, the transfer speed of the substrate 9 in the preheating zone 2 is 1-5m / min, the transfer speed of the substrate 9 in the thin film deposition zone 3 is 1-5m / min, and the transfer speed of the substrate 9 in the slow cooling zone 5 is 1-5m / min.

[0052] Furthermore, the buffer transition zone 4 preferably adopts the following structure: Figure 3As shown, the rear end of the buffer transition zone 4 is provided with an inlet 41 connecting the thin film deposition zone 3 and the buffer transition zone 4, the front end is provided with an outlet 42 connecting the buffer transition zone 4 and the slow cooling zone 5, an inlet end gate valve is arranged at the inlet 41 and can open and close the inlet 41, and an outlet end gate valve is arranged at the outlet 42 and can open and close the outlet 42, and in the front and rear directions, the two ends of the conveying mechanism 8 extend to the inlet 41 and the outlet 42 respectively. The inlet end gate valve and the outlet end gate valve are both connected to the control system of the segmented air breaking device, and are both controlled to open or close by the control system. When the control system controls the inlet end gate valve to open, the inlet end gate valve opens the inlet 41, thereby connecting the thin film deposition zone 3 and the buffer transition zone 4; when the control system controls the inlet end gate valve to close, the inlet end gate valve closes the inlet 41, thereby blocking the thin film deposition zone 3 and the buffer transition zone 4. Similarly, when the control system controls the outlet gate valve to open, the outlet gate valve opens the outlet portion 42, thereby connecting the buffer transition zone 4 and the slow cooling zone 5; when the control system controls the outlet gate valve to close, the outlet gate valve closes the outlet portion 42, thereby blocking the buffer transition zone 4 and the slow cooling zone 5.

[0053] Furthermore, before the substrate 9 enters the buffer transition zone 4, the vacuum degree in the buffer transition zone 4 is the same as the vacuum degree in the thin film deposition zone 3. Based on this, Figure 3 As shown, the segmented air breaking device also includes a vacuum system 7 connected to the buffer transition zone 4, and the vacuum system 7 forms a vacuum environment in the buffer transition zone 4; the vacuum system 7 is also connected to the control system, and is controlled to be opened or closed by the control system. In particular, when the inlet end gate valve and the outlet end gate valve are both closed, the vacuum system 7 is opened, and before the substrate 9 enters the buffer transition zone 4, the vacuum degree in the buffer transition zone 4 is the same as the vacuum degree in the thin film deposition zone 3; when the inlet end gate valve is opened, or the outlet end gate valve is opened, the vacuum system 7 is closed, and the buffer transition zone 4 can have the same vacuum degree as the thin film deposition zone 3, or the buffer transition zone 4 can have the same vacuum degree as the slow cooling zone 5.

[0054] Preferably, the vacuum system 7 is implemented in the following two embodiments: Embodiment 1, the buffer transition zone 4 uses a vacuum system 7 alone, and the vacuum system 7 can be a separate vacuum pump set; Embodiment 2, the vacuum system 7 is a vacuum pump set for the preheating zone 2, that is, the preheating zone 2 and the buffer transition zone 4 share a vacuum system 7, and the buffer transition zone 4 is connected to the vacuum system 7 for the preheating zone 2 through a pipeline, and a valve is provided on the pipeline. In addition, the preferred structure of the conveying mechanism 8 is: Figure 3As shown, the conveying mechanism 8 includes a plurality of conveying rollers 81 arranged in the buffer transition zone 4, and the plurality of conveying rollers 81 are arranged front to back along the moving direction of the substrate 9, and the spacing between two adjacent conveying rollers 81 is smaller than the length of the substrate 9 in the front to back direction; each conveying roller 81 extends left to right in a direction perpendicular to the moving direction of the substrate 9; among the plurality of conveying rollers 81 arranged front to back, the conveying roller 81 arranged at the rearmost side is adjacent to the entrance 41 of the buffer transition zone 4, and the conveying roller 81 arranged at the frontmost side is adjacent to the exit 42 of the buffer transition zone 4, so that the conveying mechanism 8 transports the substrate 9 deposited with the semiconductor thin film from the entrance 41 to the exit 42 of the buffer transition zone 4.

[0055] Taking the production of cadmium telluride thin film as an example, the segmented air breaking method using the above-mentioned segmented air breaking device is as follows: 1. In the initial state, the vacuum degree of the preheating zone 2 is 20Pa; the vacuum degree of the thin film deposition zone 3 is 20Pa; the inlet end gate valve and the outlet end gate valve of the buffer transition zone 4 are closed, the vacuum system 7 of the buffer transition zone 4 is opened, and the vacuum degree of the buffer transition zone 4 is 20Pa; the vacuum degree of the slow cooling zone 5 is 1000Pa. 2. After cleaning, the substrate 9 enters the inlet chamber 1 through the conveying unit, and the conveying unit can also be composed of multiple conveying rollers; after the vacuum degree in the inlet chamber 1 reaches the pre-requirement, the substrate 9 enters the preheating zone 2 from the inlet chamber 1. 3. After the temperature of the substrate 9 reaches the preheating temperature of 550°C in the preheating zone 2, the substrate 9 enters the thin film deposition zone 3 from the preheating zone 2. 4. In the thin film deposition zone 3, the temperature of the substrate 9 is 550°C, and cadmium telluride is deposited on the substrate 9 to form a cadmium telluride thin film. 5. Open the inlet gate valve of the buffer transition zone 4 and close the vacuum system 7 of the buffer transition zone 4. The substrate 9 in the thin film deposition zone 3 enters the buffer transition zone 4 through the inlet 41. The buffer transition zone 4 is connected to the thin film deposition zone 3, and the vacuum degree of both is 20Pa. 6. After the substrate 9 completely enters the buffer transition zone 4, the inlet gate valve of the buffer transition zone 4 is closed, and the outlet gate valve of the buffer transition zone 4 is opened. The buffer transition zone 4 is connected to the slow cooling zone 5, and the vacuum degree of both is 1000Pa, and the substrate 9 in the buffer transition zone 4 enters the slow cooling zone 5 through the outlet portion 42. 7. After the substrate 9 completely enters the slow cooling zone 5, the outlet gate valve of the buffer transition zone 4 is closed, and the next substrate 9 deposited with a cadmium telluride thin film is waited for to enter the buffer transition zone 4. 8. In the slow cooling zone 5, after the temperature of the substrate 9 drops to the pre-cooling temperature of 200°C, the substrate 9 enters the outlet chamber 6 from the slow cooling zone 5, breaks through the air to leave the vacuum cavity in the segmented air breaking device, and enters the outside atmosphere through the outlet chamber 6, and is further cooled to room temperature.

[0056] In summary, the present invention effectively overcomes various shortcomings of the prior art and has high industrial utilization value.

[0057] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A segmented air-breaking method for semiconductor thin film vacuum vapor deposition production, using a segmented air-breaking device for semiconductor thin film vacuum vapor deposition production, Features: The segmented air-breaking device comprises a thin film deposition area (3), a buffer transition area (4), and a slow cooling area (5) which are arranged in sequence along the moving direction of the substrate (9); the semiconductor material deposited on the substrate (9) in the thin film deposition area (3) is cadmium telluride, and the evaporation or sublimation speed of cadmium telluride under certain temperature conditions is proportional to the vacuum degree; the thin film deposition area (3), the buffer transition area (4), and the slow cooling area (5) are all vacuum chambers, and the vacuum degree in the slow cooling area (5) is 40-60 times lower than the vacuum degree in the thin film deposition area (3), so that when the substrate (9) deposited with cadmium telluride removed from the thin film deposition area (3) is slowly cooled in the slow cooling area (5), the cadmium telluride thin film deposited on the substrate (9) no longer vaporizes or sublimates; the buffer transition area (4) is provided with a conveying mechanism (8) for conveying the substrate (9); The segmented air-breaking method comprises the following steps in sequence: S1, cleaning the substrate (9); S2, preheating the substrate (9), and after the temperature of the substrate (9) reaches a set preheating temperature, the substrate (9) enters the thin film deposition area (3); S3, depositing a semiconductor thin film on the surface of the substrate (9) in the thin film deposition area (3); S4, the substrate (9) deposited with the semiconductor thin film moves from the thin film deposition area (3) to the buffer transition area (4), and the conveying mechanism (8) in the buffer transition area (4) transfers the substrate (9) to the slow cooling area (5); when the substrate (9) enters the buffer transition area (4) from the thin film deposition area (3), the thin film deposition area (3) and the buffer transition area (4) are connected, and the buffer transition area (4) and the slow cooling area (5) are not connected; when the substrate (9) moves from the buffer transition area (4) to the slow cooling area (5), the thin film deposition area (3) and the buffer transition area (4) are not connected, and the buffer transition area (4) and the slow cooling area (5) are connected; S5, all substrates (9) enter the slow cooling zone (5), and after the temperature of the substrates (9) drops to the set pre-cooling temperature, the substrates (9) break through the air and leave the vacuum cavity in the segmented air-breaking device.

2. The segmented air-breaking method according to claim 1, Features: The conveying mechanism (8) conveys the substrate (9) in the buffer transition zone (4) at a conveying speed of 10-30 m / min.

3. The segmented air-breaking method according to claim 1, Features: The buffer transition zone (4) is provided with an inlet portion (41) connecting the thin film deposition zone (3) and the buffer transition zone (4), an outlet portion (42) connecting the buffer transition zone (4) and the slow cooling zone (5), an inlet-end gate valve arranged at the inlet portion (41) and capable of opening and closing the inlet portion (41), and an outlet-end gate valve arranged at the outlet portion (42) and capable of opening and closing the outlet portion (42), and both ends of the conveying mechanism (8) extend to the inlet portion (41) and the outlet portion (42), respectively.

4. The segmented air-breaking method according to claim 3, Features: It also includes a vacuum system (7) connected to the buffer transition zone (4); when the inlet end gate valve and the outlet end gate valve are both closed, the vacuum system (7) is opened so that the buffer transition zone (4) has the same vacuum degree as the thin film deposition zone (3); when the inlet end gate valve is opened or the outlet end gate valve is opened, the vacuum system (7) is closed.

5. The segmented air-breaking method according to claim 4, Features: The vacuum system (7) is a separate vacuum pump set.

6. The segmented air-breaking method according to claim 1, 2 or 3, Features: The conveying mechanism (8) comprises a plurality of conveying rollers (81) arranged in the buffer transition zone (4); the plurality of conveying rollers (81) are arranged in sequence along the conveying direction of the substrate (9); and each conveying roller (81) extends in a direction perpendicular to the conveying direction of the substrate (9).

7. The segmented air-breaking method according to claim 1, Features: It also includes an inlet chamber (1), a preheating zone (2) and an outlet chamber (6), wherein the inlet chamber (1), the preheating zone (2), the thin film deposition zone (3), the buffer transition zone (4), the slow cooling zone (5), and the outlet chamber (6) are arranged in sequence along the moving direction of the substrate (9), and the vacuum degree in the preheating zone (2) is the same as the vacuum degree in the thin film deposition zone (3).

8. The segmented air-breaking method according to claim 7, Features: The preheating zone (2) and the buffer transition zone (4) share a vacuum system (7).

9. The segmented air-breaking method according to claim 1, Features: In the step S2, the preheating temperature is 550°C.