Semiconductor device and method for forming the same
By using the photoresist layer perpendicular to the sidewall to form the sacrificial part and the upper electrode layer, the surface damage and dimensional control problems in semiconductor device preparation are solved, precise control of the suspended part is achieved, and device performance is improved.
Patent Information
- Application Number
- CN202011175964.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-29
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-10-29
AI Technical Summary
In the conventional semiconductor device preparation method, surface damage is easily caused to the upper electrode layer, and it is difficult to accurately control the size of the suspended portion, affecting device performance.
The first photoresist layer with a side wall vertical or nearly vertical formation with high accuracy is used to form a sacrificial portion, and the upper electrode layer is formed through a peeling process to avoid damage to the surface of the etching process to achieve the height of the suspended portion and the height of the suspended portion and Precise control of width dimensions.
The surface flatness of the upper electrode layer and the sacrificial part is improved, the dimensional accuracy of the suspended part is ensured, and the stability of device performance is guaranteed. It is suitable for different devices and multi-layer material structures.
Smart Images

Figure CN112104335B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for forming the same. Background Art
[0002] Semiconductor devices made using the inverse piezoelectric effect of piezoelectric materials are key components of crystal oscillators and filters, and are often used in bulk acoustic wave filters. Figure 1~Figure 2 is a schematic diagram of the structure of a semiconductor device during its preparation process, such as Figure 1~Figure 2 As shown, the method for forming the semiconductor device may include the following steps.
[0003] Step 1, specific reference Figure 1 As shown, a substrate 10 is provided, on which a lower electrode layer 20 and a piezoelectric material layer 30 are sequentially formed. Furthermore, an upper electrode material layer 40 a and a patterned passivation layer 50 are also formed on the lower electrode layer 20 and the piezoelectric material layer 30 .
[0004] Step 2, specific reference Figure 2 As shown, the upper electrode material layer 40a is etched by an etching process to form the upper electrode layer 40a. Also, when etching the upper electrode material layer 40a, the etchant will further laterally erode the portion of the upper electrode material layer 40a directly below the passivation layer 50, so that the end of the formed upper electrode layer 40 is retracted relative to the end of the passivation layer 50. At this time, the end of the passivation layer 50 is correspondingly extended relative to the upper electrode layer 40 to at least partially form a suspended portion 51, and the suspended portion 51 is suspended and covers the piezoelectric material layer 30.
[0005] It should be recognized that, for a BAW filter, forming the suspended portion 51 is beneficial to improving the quality factor (Q value) of the BAW resonator. The size of the suspended portion 51 has a great influence on the Q value of the device and is an important indicator of the product quality factor.
[0006] However, currently, etching the upper electrode material layer 40a while further eroding the suspended portion 51 laterally may easily cause etching damage to the surface of the formed upper electrode layer 400, and it is also difficult to accurately control the size of the suspended portion 51 formed. For example, for different devices, the thickness of the upper electrode layer 40 is usually different, which makes it difficult to unify the time for lateral erosion, and further makes it difficult to accurately control the width of the suspended portion of different devices. In addition, when the upper electrode layer 40 is composed of two or more conductive layers of different materials, due to the difference in etching rates of different conductive layers, the spatial size of the gap below the suspended portion will also be inconsistent at different heights, affecting the performance of the device. Summary of the invention
[0007] The object of the present invention is to provide a method for forming a semiconductor device to solve the problems in the existing preparation method that the upper electrode layer is easily damaged on the surface and the size of the suspended portion is difficult to be accurately controlled.
[0008] In order to solve the above technical problems, the present invention provides a method for forming a semiconductor device, comprising:
[0009] Providing a substrate, and sequentially forming a lower electrode layer and a piezoelectric material layer on the substrate;
[0010] Forming a sacrificial material layer on the piezoelectric material layer, and forming a patterned first photoresist layer on the sacrificial material layer, wherein the first photoresist layer at least exposes an upper electrode formation region, and the angle of the sidewall of the first photoresist layer relative to the horizontal direction is 90°+ / -5°;
[0011] Using the first photoresist layer as a mask, etching the sacrificial material layer, the remaining sacrificial material layer forming a sacrificial portion;
[0012] forming an upper electrode material layer, wherein the upper electrode material layer covers the first photoresist layer and the piezoelectric material layer;
[0013] Stripping the first photoresist layer to form an upper electrode layer, wherein an end of the upper electrode layer abuts against an end of the sacrificial portion;
[0014] forming a passivation layer, wherein the passivation layer covers the upper electrode layer and extends laterally to a portion of the sacrificial portion;
[0015] The sacrificial portion is removed, and the suspended and covered portion of the passivation layer constitutes a suspended portion.
[0016] Optionally, the first photoresist layer is formed by using positive photoresist.
[0017] Optionally, an anti-reflection layer is further formed between the first photoresist layer and the sacrificial material layer, and a method for forming the anti-reflection layer includes:
[0018] When performing the development process to form the patterned first photoresist layer, the developer also laterally etches the anti-reflection layer so that the end of the patterned anti-reflection layer is retracted relative to the end of the patterned first photoresist layer.
[0019] Optionally, the upper electrode material layer is formed by a sputtering process.
[0020] Optionally, the thickness of the upper electrode layer is not greater than the thickness of the sacrificial portion.
[0021] Optionally, the method of etching the sacrificial material layer using the first photoresist layer as a mask includes: etching the sacrificial material layer using a dry etching process.
[0022] Optionally, the method for forming the passivation layer includes: etching the passivation material layer using a dry etching process to form the passivation layer.
[0023] Optionally, the size of the suspended portion is between 0.7 μm and 3 μm.
[0024] Optionally, the semiconductor device includes a bulk acoustic wave filter
[0025] Another object of the present invention is to provide a semiconductor device manufactured by the above-mentioned forming method, comprising:
[0026] substrate;
[0027] A lower electrode layer formed on the substrate;
[0028] a piezoelectric material layer, covering the lower electrode layer;
[0029] an upper electrode layer formed on the piezoelectric material layer;
[0030] A passivation layer is formed on the upper electrode layer, and the passivation layer has a suspended portion extending from the upper electrode layer.
[0031] In the method for forming a semiconductor device provided by the present invention, a first photoresist layer with vertical or nearly vertical sidewalls is used to form a sacrificial portion with high precision, and the first photoresist layer is further used to perform a stripping process to form an upper electrode layer. At this time, the upper electrode layer does not need to be etched, which avoids surface damage to the upper electrode layer and the sacrificial portion, and correspondingly improves the surface flatness of the upper electrode layer and the sacrificial portion, so that the height dimension of the finally formed suspended portion can be accurately controlled in the height direction; and the formation of the sacrificial portion and the upper electrode layer based on the same photoresist layer is also conducive to achieving the end of the upper electrode layer can be self-aligned to the end of the sacrificial portion. In addition, in the present invention, the sidewalls of the first photoresist layer are formed as vertical sidewalls or nearly vertical sidewalls, so that the patterning accuracy of the sacrificial portion below it can be improved, and at this time, the width dimension of the finally formed suspended portion can be accurately controlled in the horizontal direction.
[0032] It should be recognized that based on the method provided by the present invention, even for upper electrode layers of different thicknesses in different devices, or for upper electrode layers with multiple layers of different materials in the same device, it is possible to accurately and stably control the size of the suspended portion in the passivation layer to ensure the performance of the prepared device. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1~Figure 2It is a structural schematic diagram of an existing method for forming a semiconductor device;
[0034] Figure 3 is a schematic flow chart of a method for forming a semiconductor device in one embodiment of the present invention;
[0035] Figure 4~Figure 11 The figure is a schematic structural diagram of a method for forming a semiconductor device in an embodiment of the present invention during its preparation process.
[0036] The reference numerals are as follows:
[0037] 10 / 100-substrate;
[0038] 20 / 200-lower electrode layer;
[0039] 30 / 300- piezoelectric material layer;
[0040] 40 / 400-upper electrode layer;
[0041] 40a / 400a-upper electrode material layer;
[0042] 50 / 500 - passivation layer;
[0043] 51- suspended part;
[0044] 500a-passivation material layer;
[0045] 600a-sacrificial material layer;
[0046] 600-Sacrificial Division;
[0047] 700-first photoresist layer;
[0048] 800-anti-reflective layer;
[0049] 900 - second photoresist layer. DETAILED DESCRIPTION
[0050] As described in the background art, in the current method for preparing semiconductor devices, a suspended portion of the passivation layer is usually formed by lateral etching of the upper electrode layer. This method not only easily causes surface damage to the upper electrode layer, but also makes it difficult to accurately control the size of the suspended portion formed.
[0051] To this end, the present invention provides a method for forming a semiconductor device to accurately and stably control the size of the formed overhanging portion. Figure 3 As shown, the method for forming the semiconductor device includes:
[0052] Step S100, providing a substrate, and sequentially forming a lower electrode layer and a piezoelectric material layer on the substrate;
[0053] Step S200, forming a sacrificial material layer on the piezoelectric material layer, and forming a patterned first photoresist layer on the sacrificial material layer, wherein the first photoresist layer at least exposes an upper electrode formation region, and an angle of a sidewall of the first photoresist layer relative to a horizontal direction is 90°+ / -5°;
[0054] Step S300, etching the sacrificial material layer using the first photoresist layer as a mask, and the remaining sacrificial material layer constitutes a sacrificial portion;
[0055] Step S400, forming an upper electrode material layer, wherein the upper electrode material layer covers the first photoresist layer and the piezoelectric material layer;
[0056] Step S500, peeling off the first photoresist layer to form an upper electrode layer, wherein an end of the upper electrode layer abuts against an end of the sacrificial portion;
[0057] Step S600, forming a passivation layer, wherein the passivation layer covers the upper electrode layer and extends laterally to a portion of the sacrificial portion;
[0058] Step S700, removing the sacrificial portion, and the suspended and covered portion of the passivation layer constitutes a suspended portion.
[0059] That is, in the formation method provided by the present invention, the sacrificial part is precisely defined based on the first photoresist layer with vertical or nearly vertical sidewalls, thereby improving the dimensional accuracy of the gap released by the subsequent removal of the sacrificial part. In addition, the first photoresist layer is further used to perform a stripping process to form the upper electrode layer, thereby avoiding the surface damage to the upper electrode layer and the sacrificial part caused by the etching process in the traditional process.
[0060] The following is combined with Figure 4~Figure 11 The semiconductor device and the method for forming the same according to the present invention are further described in detail with reference to the specific embodiments. Figure 4~Figure 11 The present invention is a schematic diagram of the structure of a method for forming a semiconductor device in an embodiment of the present invention during its preparation process. The advantages and features of the present invention will become more apparent from the following description. It should be noted that the drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.
[0061] In step S100, refer to Figure 4 As shown, a substrate 100 is provided, and a lower electrode layer 200 and a piezoelectric material layer 300 are sequentially formed on the substrate 100 .
[0062] The substrate 100 may be adjusted according to the specific application of the semiconductor device to be formed. For example, the semiconductor device may be a bulk acoustic wave (BAW) filter, in which case the substrate may include multiple Bragg reflection layers to further form a solid-state resonator (SMR); or the substrate may further include a cavity to further form a film bulk acoustic resonator (FBAR) filter.
[0063] Furthermore, the material of the lower electrode layer 200 may include a metal material, specifically, the metal material includes molybdenum (Mo), for example. Also, the material of the piezoelectric material layer 300 may include at least one of zinc oxide (ZnO), aluminum nitride (AlN), and lead zirconate titanate (PZT).
[0064] In step S200, refer to Figure 5 As shown, a sacrificial material layer 600 a is formed on the piezoelectric material layer 300 , and a patterned first photoresist layer 700 is formed on the sacrificial material layer 600 a , wherein the first photoresist layer 700 at least exposes an upper electrode forming region.
[0065] The material of the sacrificial material layer 600a includes, for example, an insulating material, and more specifically, the insulating material may include silicon oxide or silicon nitride, etc. Also, the upper electrode forming region is a region where an upper electrode layer is subsequently formed.
[0066] In this embodiment, the angle of the sidewall of the patterned first photoresist layer 700 relative to the horizontal direction is 90°+ / -5°. That is, the sidewall of the first photoresist layer 700 is a vertical sidewall or a nearly vertical sidewall. In this way, when the first photoresist layer 700 is subsequently used to pattern the sacrificial material layer, the patterning accuracy of the sacrificial material layer 600a can be improved. For example, the side boundary of the first photoresist layer 700 corresponds to the first position S1, and at this time, the side boundary of the sidewall of the etched sacrificial material layer can also correspond to the first position S1. In addition, since the sidewall of the first photoresist layer 700 is a vertical sidewall, it is also beneficial to realize that the sidewall of the sacrificial material layer after etching is also a vertical sidewall or a nearly vertical sidewall.
[0067] Furthermore, the first photoresist layer 700 may be formed by using positive photoresist. Compared with negative photoresist which easily forms an inverted trapezoidal photoresist layer, in this embodiment, using positive photoresist is more conducive to forming the first photoresist layer 700 with vertical sidewalls.
[0068] Continue to refer Figure 5As shown, in this embodiment, an anti-reflection layer 800 is further formed between the sacrificial material layer 600a and the first photoresist layer 700. By forming the anti-reflection layer 800, when preparing the patterned first photoresist layer 700, the patterning accuracy of the first photoresist layer 700 can be effectively improved, so that the first photoresist layer 700 is more likely to form a vertical sidewall.
[0069] Specifically, the method for forming the anti-reflection layer 800 includes: when performing a development process to form a patterned first photoresist layer 700, the developer also simultaneously laterally etches the anti-reflection layer 800 so that the end of the patterned anti-reflection layer 800 is retracted relative to the end of the patterned first photoresist layer 700. At this time, the end of the first photoresist layer 700 is correspondingly suspended.
[0070] It should be noted that, in this embodiment, a lift-off process is used to form an upper electrode layer based on the patterned first photoresist layer 700. That is, the first photoresist layer 700 is not only used to define the pattern of the sacrificial part, but also used to realize the preparation of the upper electrode layer. Since the sacrificial part and the upper electrode layer are patterned based on the same photoresist layer, the end of the sacrificial part and the end of the upper electrode layer can be self-aligned and abutted against each other. In addition, when performing the lift-off process, although the sidewall of the first photoresist layer 700 is a vertical sidewall, in this embodiment, an inward-retracted anti-reflection layer 800 is provided under the first photoresist layer 700. In this way, when the upper electrode material layer is subsequently formed, the electrode material covering the first photoresist layer 700 can still be more easily separated from the electrode material covering the piezoelectric material layer, so as to reduce the difficulty of stripping the first photoresist layer. Among them, the inward-retracted value of the end of the patterned anti-reflection layer 800 relative to the end of the patterned first photoresist layer 700 is, for example, between 0.5 μm and 2 μm.
[0071] In step S300, refer to Figure 6 As shown, the sacrificial material layer is etched using the first photoresist layer 700 as a mask to expose a portion of the piezoelectric material layer 300 corresponding to the upper electrode formation area, and the remaining sacrificial material layer constitutes a sacrificial portion 600 .
[0072] Based on the first photoresist layer 700 with vertical sidewalls, the sidewalls of the formed sacrificial part 600 are also more conducive to forming vertical sidewalls or nearly vertical sidewalls, thereby improving the control accuracy of the size of the sacrificial part 600. Furthermore, if the side boundary of the first photoresist layer 700 corresponds to the first position S1, then the side boundary of the sacrificial part 600 also corresponds to the first position S1 accordingly.
[0073] Specifically, the sacrificial material layer may be etched using a dry etching process to improve the etching accuracy of the sacrificial material layer, accurately control the size of the formed sacrificial portion 600 , and improve the verticality of the sidewall of the sacrificial portion 600 .
[0074] In step S400, refer to Figure 7 As shown, an upper electrode material layer 400 a is formed, and the upper electrode material layer 400 a covers the first photoresist layer 700 and the piezoelectric material layer 300 .
[0075] At this time, the end sidewall of the upper electrode material layer 400a covering the piezoelectric material layer 300 abuts against the end sidewall of the sacrificial part 600. In this embodiment, the sidewall of the sacrificial part 600 is a vertical sidewall, so that the sidewall of the upper electrode material layer 400a abutting against the sacrificial part 600 is also a vertical sidewall or a nearly vertical sidewall.
[0076] The upper electrode material layer 400 a may be formed by a sputtering process, and the material of the upper electrode material layer 400 a may include at least one of aluminum (Al), gold (Au), copper (Cu) and molybdenum (Mo).
[0077] Furthermore, the upper electrode material layer 400a can be a single-layer structure (in this case, the prepared upper electrode layer can also be a single-layer structure); or, the upper electrode material layer 400a can also be a multi-layer structure (in this case, the prepared upper electrode layer can also be a multi-layer structure). For example, the upper electrode material layer 400a may include at least two conductive material layers of different materials stacked in sequence from bottom to top.
[0078] Continue to refer Figure 7 As shown, in this embodiment, the anti-reflection layer 800 is spaced between the first photoresist layer 700 and the piezoelectric material layer 300, and the end of the anti-reflection layer 800 is retracted so that there is a gap between the side wall of the first photoresist layer 700 and the top surface of the piezoelectric material layer 300. In this way, the part of the upper electrode material layer 400a covering the first photoresist layer 700 and the part covering the piezoelectric material layer 300 can be more easily separated from each other. Based on this, when the first photoresist layer 700 is subsequently peeled off, not only can the peeling difficulty of the first photoresist layer 700 be reduced, but also damage to the electrode material on the piezoelectric material layer can be avoided.
[0079] Furthermore, the thickness of the portion of the upper electrode material layer 400a covering the piezoelectric material layer 300 is not greater than the thickness of the sacrificial portion 600. In this way, it is beneficial to avoid the electrode material on the piezoelectric material layer from being connected to the first photoresist layer 700 (that is, it is beneficial to separate the electrode material on the piezoelectric material layer from the first photoresist layer 700) and control the height of the suspended portion formed subsequently. In this embodiment, the thickness of the portion of the upper electrode material layer 400a covering the piezoelectric material layer 300 can be the same as the thickness of the sacrificial portion 600, or in other words, the top surface of the upper electrode material layer 400a covering the piezoelectric material layer 300 is flush with the top surface of the sacrificial portion 600.
[0080] In step S500, refer to Figure 8 As shown, the first photoresist layer is peeled off to remove the portion of the upper electrode material layer covering the first photoresist layer, and the portion of the upper electrode material layer located in the upper electrode forming area is retained to form an upper electrode layer 400 .
[0081] That is, the portion of the upper electrode material layer covering the piezoelectric material layer 300 is retained to form the upper electrode layer 400. As described above, the electrode material on the piezoelectric material layer 300 is not connected to the first photoresist layer 700, so the difficulty of stripping the first photoresist layer can be effectively reduced, and the electrode material on the piezoelectric material layer 300 can be prevented from being pulled during the stripping process of the first photoresist layer, thereby preventing the edge of the formed upper electrode layer 400 from being damaged. At this time, the end of the upper electrode layer 400 and the end of the sacrificial portion 600 can maintain good mutual contact.
[0082] It should be noted that, in the present embodiment, after the first photoresist layer 700 is used to form a patterned sacrificial portion 600, the first photoresist layer 700 is continued to be used to form the upper electrode layer 400. On the one hand, this is beneficial to reducing the number of executions of the photolithography process; on the other hand, for example, compared with using the sacrificial portion 600 as a grinding stop layer to perform a grinding process and then prepare the upper electrode layer, since the control accuracy of the sputtering process is higher than the control accuracy of the grinding process, the stripping process used in the present embodiment will be more conducive to achieving the top surface of the upper electrode layer 400 being flush with the top surface of the sacrificial portion 600.
[0083] In addition, in this embodiment, when the stripping process is used to form the upper electrode layer 400, since the sacrificial portion 600 is always covered by the mask of the first photoresist layer 700, and a patterned upper electrode layer 400 can be formed after stripping the first photoresist layer 700, there is no need to use an etching process or a grinding process, thereby avoiding surface damage to the upper electrode layer 400 and the sacrificial portion 600, thereby ensuring the quality of the upper electrode layer 400, and since the surface of the sacrificial portion 600 is smoother, the height dimension of the suspended portion formed by the subsequent release of the sacrificial portion is more balanced in the height direction.
[0084] Furthermore, in this embodiment, the anti-reflection layer is removed to expose the sacrificial portion 600 .
[0085] Continue to refer Figure 8 As shown, in this embodiment, the sacrificial portion 600 is formed first before the upper electrode layer 400 is prepared, so that the upper electrode layer 400 can be formed on at least two opposite ends of the sacrificial portion 600, and the upper electrode layers 400 at different positions are separated from each other to form upper electrode layers in different devices. It can be understood that the sacrificial portion 600 is formed between at least two adjacent devices, so that the upper electrode layers in the adjacent devices are all prepared based on the sacrificial portion 600.
[0086] In step S600, refer to Fig. 9 and Fig.10 As shown, a passivation layer 500 is formed, and the passivation layer 500 covers the upper electrode layer 400 and extends laterally to a portion of the sacrificial portion 600 .
[0087] Specifically, the method for forming the passivation layer 500 may include the following steps.
[0088] The first step is to refer to Fig. 9 As shown, a passivation material layer 500a is formed on the upper electrode layer 400 and the sacrificial portion 600, and a patterned second photoresist layer 900 is formed on the passivation material layer 500a, and a side boundary of the patterned second photoresist layer 900 corresponds to a second position S2, and the second position S2 is located within the region of the sacrificial portion 600, and a predetermined width dimension D is defined in the horizontal direction from the second position S2 to the first position S1.
[0089] The passivation material layer 500a covers the sacrificial portion 600 and the upper electrode layer 400. Also, the passivation material layer 500a can be formed of the same material as the piezoelectric material layer 300, for example, both of them include aluminum nitride (AlN).
[0090] In this embodiment, the top surfaces of the upper electrode layer 400 and the sacrificial portion 600 are flush, and accordingly the top surface of the passivation layer 500a is a flat surface at the corresponding position, thereby improving the patterning accuracy of the second photoresist layer 900 when forming the patterned second photoresist layer 900.
[0091] The second step, specific reference Fig.10 As shown, the passivation material layer is etched using the second photoresist layer 900 as a mask to form a passivation layer 500 , and the side boundary of the passivation layer 500 corresponds to the second position S2 , so that the passivation layer 500 covers the upper electrode layer 400 and extends laterally to the sacrificial portion 600 .
[0092] Specifically, the passivation material layer may be etched using a dry etching process to improve the etching accuracy of the passivation material layer, thereby accurately controlling the size of the formed passivation layer 500 .
[0093] In step S700, refer to Fig.11 As shown, the sacrificial portion is removed to release a gap below the passivation layer 500, and the suspended and covered portion of the passivation layer 500 constitutes a suspended portion, and the width of the suspended portion corresponds to the predetermined width D. Further, the width of the gap below the passivation layer 500 (i.e., the predetermined width D) is, for example, between 0.7 μm and 3 μm, that is, the size of the suspended portion may be between 0.7 μm and 3 μm.
[0094] Since at least part of the end of the passivation layer 500 constitutes a suspended portion, when the semiconductor device is applied to a bulk acoustic wave filter, the lateral acoustic waves excited in the bulk acoustic wave filter can be scattered more easily, thereby not easily exciting lateral modes that are harmful to the device, reducing energy losses caused by lateral excitation, and being beneficial to improving the quality factor (Q value) of the bulk acoustic wave filter.
[0095] It should be noted that compared with the traditional process of using lateral erosion to release the gap under the suspended part, this embodiment can more accurately and stably control the size of the released gap, thereby accurately controlling the size of the suspended part formed, and can also avoid surface damage to the upper electrode layer.
[0096] Specifically, in this embodiment, the size of the gap below the suspended portion is defined by the first position S1 defined by the first photoresist layer and the second position S2 defined by the second photoresist layer (i.e., the boundary position of the passivation layer), and is not affected by the thickness of the upper electrode layer 400, nor by the material of the upper electrode layer 400. Therefore, even for upper electrode layers of different thicknesses in different devices, a suspended portion of a desired size can still be accurately and stably prepared, and for upper electrode layers of different materials in the same device, a gap with consistent space from top to bottom can also be accurately released, so that the width of the suspended portion remains uniform from bottom to top.
[0097] Based on the formation method described above, this embodiment also provides a semiconductor device, which can be specifically referred to Fig.11 As shown, the semiconductor device comprises:
[0098] Substrate 100;
[0099] A lower electrode layer 200 is formed on the substrate 100;
[0100] A piezoelectric material layer 300 is formed on the substrate 100 and covers the lower electrode layer 200;
[0101] an upper electrode layer 400 formed on the piezoelectric material layer 300; and
[0102] The passivation layer 500 is formed on the upper electrode layer 400 , and the passivation layer 500 has a suspended portion extending from the upper electrode layer 400 , and the suspended portion is suspended and covers the piezoelectric material layer 300 .
[0103] It should be noted that, although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still belongs to the scope of protection of the technical solution of the present invention.
[0104] It should also be understood that, unless otherwise specified or indicated, the terms "first", "second", "third", etc. in the specification are merely used to distinguish between the various components, elements, steps, etc. in the specification, and are not used to indicate the logical relationship or sequential relationship between the various components, elements, steps, etc.
[0105] It should also be recognized that the terms described herein are only used to describe specific embodiments and are not intended to limit the scope of the invention. It should be noted that the singular forms "a" and "an" used herein and in the appended claims include plural references unless the context clearly indicates otherwise. For example, a reference to "a step" or "a device" means a reference to one or more steps or devices, and may include secondary steps and secondary devices. All conjunctions used should be understood in the broadest sense. And, the word "or" should be understood to have the definition of a logical "or", rather than a logical "exclusive or", unless the context clearly indicates otherwise. In addition, the implementation of the method and / or device in the embodiments of the present invention may include performing the selected task manually, automatically, or in combination.
Claims
1. A method for forming a semiconductor device, It is characterized in that include: Providing a substrate, and sequentially forming a lower electrode layer and a piezoelectric material layer on the substrate; Forming a sacrificial material layer on the piezoelectric material layer, and forming a patterned first photoresist layer on the sacrificial material layer, wherein the first photoresist layer at least exposes an upper electrode forming region; Using the first photoresist layer as a mask, etching the sacrificial material layer, the remaining sacrificial material layer forming a sacrificial portion; forming an upper electrode material layer, wherein the upper electrode material layer covers the first photoresist layer and the piezoelectric material layer; Stripping the first photoresist layer to form an upper electrode layer, wherein an end of the upper electrode layer abuts against an end of the sacrificial portion; forming a passivation layer, wherein the passivation layer covers the upper electrode layer and extends laterally to a portion of the sacrificial portion, and a side boundary of the passivation layer corresponds to a region of the sacrificial portion; as well as, The sacrificial portion is removed to release the space below the passivation layer, and the suspended and covered portion of the passivation layer constitutes a suspended portion.
2. The method for forming a semiconductor device according to claim 1, It is characterized in that The first photoresist layer is formed by using positive photoresist, and the angle between the sidewall of the first photoresist layer and the horizontal direction is 90°+ / -5°.
3. The method for forming a semiconductor device according to claim 1, It is characterized in that An anti-reflection layer is also formed between the first photoresist layer and the sacrificial material layer, and a method for forming the anti-reflection layer includes: When performing the development process to form the patterned first photoresist layer, the developer also laterally etches the anti-reflection layer so that the end of the patterned anti-reflection layer is retracted relative to the end of the patterned first photoresist layer.
4. The method for forming a semiconductor device according to claim 1, It is characterized in that The upper electrode material layer is formed by a sputtering process.
5. The method for forming a semiconductor device according to claim 1, It is characterized in that The thickness of the upper electrode layer is not greater than the thickness of the sacrificial portion.
6. The method for forming a semiconductor device according to claim 1, It is characterized in that The method of etching the sacrificial material layer using the first photoresist layer as a mask includes: etching the sacrificial material layer using a dry etching process.
7. The method for forming a semiconductor device according to claim 1, It is characterized in that The method for forming the passivation layer includes: etching the passivation material layer using a dry etching process to form the passivation layer.
8. The method for forming a semiconductor device according to claim 1, It is characterized in that The size of the suspended portion is between 0.7 μm and 3 μm.
9. The method for forming a semiconductor device according to claim 1, It is characterized in that The semiconductor device includes a bulk acoustic wave filter.
10. A semiconductor device manufactured by the method for forming a semiconductor device according to any one of claims 1 to 9, include: substrate; A lower electrode layer formed on the substrate; a piezoelectric material layer, covering the lower electrode layer; an upper electrode layer formed on the piezoelectric material layer; A passivation layer is formed on the upper electrode layer, and the passivation layer has a suspended portion extending from the upper electrode layer.
Citation Information
Patent Citations
Integration scheme for microelectromechanical systems (MEMS) devices and complementary metal-oxide-semiconductor (CMOS) devices
CN107662901A
Surface acoustic wave resonator and forming method thereof
CN111313861A
Semiconductor device and forming method thereof
CN111740001A
Semiconductor device and forming method thereof
CN111740007A
Semiconductor device and fabrication method thereof
TW200901379A