Laser lift-off mask

By using LLO mask technology in semiconductor device manufacturing, the filling material is protected from laser influence, and the problem of tiny LED breakage during the LLO process is solved, improving the manufacturing success rate and device reliability.

CN112352323BInactive Publication Date: 2024-11-19CTRL-LABS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980040585.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-07-30
Filing Date
2019-07-30
Publication Date
2024-11-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the manufacturing process of semiconductor devices, especially in laser stripping (LLO) technology, tiny LEDs are prone to breaking due to the interaction between laser and filler material, resulting in manufacturing failure.

Method used

Using LLO mask technology, masking materials are formed on the substrate to protect the filler from the laser, ensuring that the laser only transmits through the substrate without directly interacting with the filler material, thereby avoiding mechanical stress and rupture.

Benefits of technology

It effectively avoids the cracking of semiconductor devices, improves the success rate of the LLO process and the availability of devices, and ensures the integrity and reliability of micro LEDs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112352323B_ABST
    Figure CN112352323B_ABST
Patent Text Reader

Abstract

Technology related to laser lift-off masking is disclosed. In some embodiments, a masking material is applied to a substrate to which a plurality of semiconductor device assemblies are attached. More specifically, the masking material is applied to one or more regions of the substrate between the semiconductor device assemblies. When the semiconductor device assemblies are embedded in a filler material, the masking material may be located between the substrate and the filler material. Thus, light is transmitted through the substrate toward the semiconductor device assemblies so that the substrate becomes detached from the semiconductor device assemblies. However, the light is at least partially blocked by the masking material.
Need to check novelty before this filing date? Find Prior Art

Description

Background Art

[0001] The present disclosure relates generally to semiconductor device fabrication, and more particularly to laser lift-off masks.

[0002] Semiconductor devices have become common in electronics to provide benefits such as reduced size, improved durability, and increased efficiency. For example, compared to incandescent bulbs, light emitting diodes (LEDs) are typically smaller, last several times longer, and convert more energy proportionally into light rather than heat. Therefore, semiconductor devices have even found their way into display systems, such as those found in televisions, computer monitors, laptops, tablet computers, smartphones, and wearable electronic devices. In particular, tiny LEDs can be used to form sub-pixels of display systems. However, manufacturing such tiny LEDs can be challenging.

[0003] For example, some display systems contain tiny LEDs that are flip-chips. The manufacture of LED flip-chips often involves a laser lift-off (LLO) technique to separate the LED from the substrate on which the LED is epitaxially grown. However, if the LEDs are thin, they tend to crack when subjected to the LLO technique. There are many theories about the direct cause of the cracking, but the root cause in each theory is the interaction between the laser and the filler material in which the LED is embedded. Many unusable LEDs have been manufactured due to this interaction. Summary of the invention

[0004] The present disclosure relates to semiconductor device manufacturing involving an LLO mask. When performing LLO, the LLO mask can be used to protect the fill material from interacting with the laser. As a result, cracking of the semiconductor device can be avoided.

[0005] In some embodiments, one or more LLO masks are formed on a substrate attached to the semiconductor device set. At least, the one or more LLO masks cover one or more gap regions between the semiconductor device sets.

[0006] When performing LLO, the laser is transmitted through the substrate toward the semiconductor device set and the one or more LLO masks. There is only a little (if any) prevention of the laser from being absorbed by the semiconductor device set. However, the LLO mask can prevent any significant interaction between the laser and the fill material. As a result, LLO can be performed so that the semiconductor device set becomes detached from the substrate without causing the semiconductor device set to crack. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] Illustrative embodiments are described with reference to the following figures.

[0008] Figure 1An example semiconductor device according to one embodiment is shown.

[0009] FIG. 2A to FIG. 2D An example method for performing LLO is shown according to one embodiment.

[0010] Figure 3 Example results of performing LLO without an LLO mask are shown according to one embodiment.

[0011] FIG. 4A to FIG. 4B An example LLO mask is shown according to one embodiment.

[0012] FIG. 5A to FIG. 5D An example method for forming an LLO mask using a positive photoresist according to one embodiment is shown.

[0013] 6A to 6F An example method for forming an LLO mask using a negative photoresist is shown according to one embodiment.

[0014] FIG. 7A to FIG. 7B An example method for removing the LLO mask according to one embodiment is shown.

[0015] FIG. 8A to FIG. 8D An example method for removing a "winged" LLO mask is shown according to one embodiment.

[0016] Fig. 9 is a flow chart illustrating an example method for performing LLO using one or more LLO masks according to one embodiment.

[0017] Fig.10 An example manufacturing system is shown according to one embodiment.

[0018] The accompanying drawings depict embodiments of the present disclosure for illustrative purposes only. Those skilled in the art will readily recognize from the following description that alternative embodiments of the structures and methods shown may be employed without departing from the principles or benefits of the present disclosure. DETAILED DESCRIPTION

[0019] In the following description, for the purpose of explanation, specific details are set forth in order to provide a thorough understanding of certain inventive embodiments. However, it will be apparent that various embodiments can be practiced without these specific details. The drawings and descriptions are not intended to be limiting.

[0020] Disclosed herein are techniques related to performing LLO during the manufacture of semiconductor devices, such as LEDs and photodiodes. In some embodiments, the semiconductor devices manufactured are tiny inorganic LEDs known as micro-LEDs. As used herein, a micro-LED may refer to an LED having an active light emitting area with a linear dimension of less than 50 μm, less than 20 μm, or less than 10 μm. For example, the linear dimension may be as small as 2 μm or 4 μm. Their small size enables a display system to have a single pixel that includes three of them: a red micro-LED, a green micro-LED, and a blue micro-LED. Their small size also enables the micro-LED to be lightweight, making it particularly suitable for use in wearable display systems, such as watches and computing glasses. However, their small size makes them particularly susceptible to cracking when subjected to LLO.

[0021] Semiconductor Devices

[0022] refer to Figure 1 , a cross-sectional view of an example micro-LED 100 is provided. Among other components, the micro-LED 100 includes a semiconductor structure including semiconductor layers 102-104, and a light emitting layer 106 located between the semiconductor layers 102-104. For example, the micro-LED 100 may include a semiconductor structure in which the light emitting layer 106 is an indium gallium nitride layer sandwiched between a p-type gallium nitride layer and an n-type gallium nitride layer. In some embodiments, the semiconductor layer 102 is a p-type semiconductor, and the semiconductor layer 104 is an n-type semiconductor. In some embodiments, the semiconductor layer 102 is an n-type semiconductor, and the semiconductor layer 104 is a p-type semiconductor.

[0023] Semiconductor layers 102-104 are typically very thin. For example, semiconductor layer 104 may have a thickness of only one or two microns, and semiconductor layer 102 may be even thinner than that. This makes the micro-LED particularly susceptible to damage from even the smallest amount of mechanical stress, which may cause cracks to form in one or more of the semiconductor layers.

[0024] The semiconductor layers 102-104 are operably coupled to electrical contacts 108-110, respectively. The electrical contacts 108-110 are typically made of a conductive material such as a metallic material. Figure 1 In the example of FIG. 1 , both electrical contacts 108-110 are located on the top surface of the semiconductor structure so that when micro LED 100 is mounted on a substrate, both electrical contacts 108-110 can support micro LED 100. However, in some embodiments, the electrical contacts can be located on opposite surfaces of the semiconductor structure.

[0025] The light emitting layer 106 includes one or more quantum wells that output light 116 when a voltage is applied across the electrical contacts 108-110. The light emitting layer 106 typically has a very small area. For example, its area may be on the order of 1 μm 2 Up to 20μm 2 between.

[0026] To increase the brightness of light emitted from such a small area, the semiconductor structure can be formed into any of a variety of shapes (e.g., a parabola, a cylinder, or a cone) that enable collimation / quasi-collimation of light 116. Such a shape is referred to herein as a "mesa" shape; and collimation and quasi-collimation are collectively referred to herein as "collimation."

[0027] exist Figure 1 In the example of , the mesa 114 corresponds to a parabola shape that directs light 116 toward and through the light emitting surface 112 of the semiconductor structure. More specifically, the light emitting layer 106 is approximately located at the focus of the parabola so that some of the emitted light is reflected off the inner wall of the parabola toward the light emitting surface 112 within the critical angle for total internal reflection.

[0028] In some embodiments, the mesa shape also has a truncated top portion that can accommodate an electrical contact. Figure 1 In the example of FIG. 1 , the mesa 114 corresponds to a parabolic shape having a truncated vertex that accommodates the electrical contact 108 . The base 118 refers to the portion of the semiconductor structure that is not included in the mesa 114 .

[0029] Micro LED 100 may include other components, such as dielectric layers, reflective layers, and substrate layers. However, to avoid obscuring the present disclosure, such components are not described in detail in the accompanying drawings. Figure 1 Not shown.

[0030] Laser peeling

[0031] FIG. 2A to FIG. 2D An example semiconductor manufacturing process involving LLO is shown. FIG. 2A to FIG. 2D The semiconductor device shown is an abstraction of an LED device, but it should be understood that the techniques disclosed herein are equally applicable to any other semiconductor device.

[0032] refer to Figure 2A , a set of one or more semiconductor devices 202-204 is attached to a common substrate 200. Figure 2A In the example of , each set is an array of two unsingulated semiconductor devices. However, it should be understood that the techniques described herein are equally applicable to sets including any number of semiconductor devices, including a single set of one semiconductor device.

[0033] Substrate 200 may be composed of a transparent / quasi-transparent material on which assemblies 202-204 may be epitaxially grown. For example, substrate 200 may be composed of sapphire on which a gallium nitride layer is grown to produce a blue micro-LED. Example techniques for growing semiconductor structures include, but are not limited to, molecular beam epitaxy (MBE) or metal organic chemical vapor deposition (MOCVD).

[0034] In some embodiments, electrical contacts 108 - 110 are formed thereafter. Thus, one or more semiconductor layers may be located between substrate 200 and electrical contacts 108 - 110 .

[0035] The semiconductor devices of the set 202 - 204 may be separated by one or more gap regions of the substrate 200 . Figure 2A In the example shown in FIG. 2 , region 206 separates the rightmost semiconductor device of set 202 from the leftmost semiconductor device of set 204 .

[0036] refer to Figure 2B , substrate 200 and attached collections 202-204 are turned over and placed on substrate 208 so that collections 202-204 are located between substrates 200 and 208. Substrate 208 can be composed of glass, silicon, or any other inert material. In some embodiments, substrate 208 is a temporary carrier substrate for facilitating the transportation of collections 202-204.

[0037] At any time relative to having the collection 202-204 positioned on the substrate 208, the collection 202-204 can be embedded in the filling material 210. The filling material 210 can be any of a variety of polymers, including but not limited to polyvinyl alcohol, polyvinyl acetate, polyester, polymethyl methacrylate, polystyrene, polycarbonate, or polyvinyl butyral. Therefore, embedding the collection 202-204 in the filling material 210 can involve immersing the collection 202-204 in a monomer solution, which is then polymerized. Among other purposes, the filling material 210 can also be used to secure the collection 202-204 to the substrate 208, stabilize the collection 202-204 during transportation, and / or provide a flat surface for depositing an elastic material on the collection 202-204.

[0038] although Figure 2B The sets 202-204 are shown as being completely embedded in a filler material 210, which is used to at least fill the gaps separating the sets 202-204. Figure 2B In the example shown, filler material 210 contacts a surface of region 206 between sets 202 - 204 .

[0039] refer to Figure 2C, performing LLO based on transmitting light 212 through substrate 200 toward collection 202-204. In some embodiments, light 212 has a wavelength in the ultraviolet range of the electromagnetic spectrum. Light 212 can be a laser that is emitted in pulses at a predetermined repetition rate (e.g., 200kHz). Light 212 is absorbed by collection 202-204, which becomes heated to a high temperature (e.g., 850-1500 degrees Celsius). This causes collection 202-204 to decompose at the surface where they are attached to substrate 200 (e.g., to a depth of 50-100 nanometers), thereby causing collection 202-204 to become detached from substrate 200, as shown. Figure 2D shown.

[0040] For example, the collection 202-204 can be attached to the substrate 200 by epitaxially growing a semiconductor compound (e.g., GaN) layer on the substrate 200. Light 212 can penetrate the surface of the compound, and the heat generated can cause the intramolecular bonds to break. Different elements of the compound can have different states, thereby facilitating the removal of the elements. To illustrate, nitrogen can be released as a gas, leaving behind a solid gallium layer. The remaining elements (e.g., solid gallium) can be heated to above their melting point, such as by placing a hot plate under the substrate 208, so that the substrate 200 can be separated from the collection 202-204. Thereafter, any remaining elements remaining on the collection 202-204 can be removed, such as by an etching process (e.g., wet etching gallium with dilute hydrochloric acid).

[0041] However, light 212 interacts not only with the surface of assemblies 202-204, but also with the surface of filler material 210 that has been in contact with substrate 200. As a result, the surface of filler material 210 may be heated, melted, or vaporized, thereby causing mechanical stress that may cause assemblies 202-204 to break and become unusable.

[0042] Figure 3 2 is a top view of the assembly 202-204 when the substrate 200 is removed. As a result of performing LLO, a crack 300 is formed on the assembly 202. In some cases, performing LLO may cause a small crack to form, but then when pressure is applied, the size of the crack may increase. For example, when performing heat pressing to bond the assembly to a display system, the crack may propagate across the length of the assembly.

[0043] As described above, there are many theories as to what causes crack formation when performing LLO. Some theories suggest that cracks are caused by mechanical stresses induced when the filler material 210 changes state. According to these theories, the filler material 210 is heated when it absorbs laser light, causing the filler material 210 to liquefy and / or vaporize.

[0044] Some theories suggest that when heated, expansion of filler material 210 and / or all or part of assemblies 202-204 induces mechanical stress. Thus, the expansion may cause assemblies 202-204 to fracture due to being constrained to an insufficient amount of space.

[0045] Some theories suggest that the mechanical stress is caused by surface contamination. According to these theories, the laser scans the substrate 200 in overlapping patterns. Therefore, some areas of the substrate 200 are scanned multiple times. In addition, some of these areas include both semiconductor material and filler material 210. At such areas, the first scan may cause the semiconductor material to separate from the substrate 200, and the second scan may cause the adjacent filler material to be heated and expand into the area where the substrate 200 and the semiconductor material were previously attached. Therefore, the inserted filler material may act as a wedge to cause cracking.

[0046] LLO Mask

[0047] To reduce the amount of interaction between the laser and the fill material, a masking material may be used to protect the fill material from the laser. FIG. 4A to FIG. 4B An example LLO mask that enables prevention of semiconductor cracking is shown.

[0048] refer to Figure 4A , masking materials 400-404 are applied to a surface (e.g., a top surface) of substrate 200. In some embodiments, the application of masking materials 400-404 is performed before placing sets 202-204 on substrate 208. However, in some other embodiments, the application of masking materials 400-404 may be performed after placing sets 202-204 on substrate 208. For example, masking materials 400-404 may be applied to Figure 4A The opposite surface (eg, bottom surface) of the substrate 200 is formed such that the substrate 200 is located between the filling material 210 and the masking materials 400-404. Importantly, the masking material covers the gap region of the substrate 200, but does not cover the sets 202-204.

[0049] The masking materials 400-404 can be composed of any material with a sufficiently high melting point so as not to be vaporized by the laser. In some embodiments, the masking materials 400-404 are metal materials such as tungsten, which are relatively easy to apply and / or remove. The application and removal of the masking materials 400-404 are described in subsequent sections of this disclosure.

[0050] At least, masking material 400 is applied to one or more regions between sets 202-204, such as region 206. However, in some embodiments, masking material 402-404 is also applied to surfaces of substrate 200 outside of one or more regions between sets 202-204. Figure 4A In the example of FIG. 4 , masking materials 402-404 are applied to the surface of substrate 200 at one or more boundary regions between the set and the outer edge of substrate 200. Alternatively, sets 202-204 may be placed on substrate 200 such that there are no boundary regions.

[0051] refer to Figure 4B , the collection 202-204 is located on the substrate 208 and embedded in the filling material 210. Therefore, the masking materials 400-404 become located between the substrate 200 and the filling material 210. Accordingly, when the laser is transmitted through the substrate 200, the masking materials 400-404 can protect some of the filling material 210 from interacting with the laser.

[0052] LLO mask formation

[0053] The LLO mask can be formed based on applying the masking material 400-404 to the substrate 200 using any of a variety of sputtering techniques. Example sputtering techniques include, but are not limited to, direct current (DC) sputtering or radio frequency (RF) sputtering. As described above, in some embodiments, the masking material 400-404 is a metal material. However, the application of the metal material to the semiconductor device may cause a short circuit when the semiconductor device is operated. Therefore, the masking material 400-404 should be selectively applied to the substrate 200, rather than to the set 202-204. As described in further detail below, this can be achieved using a photoresist material.

[0054] FIG. 5A to FIG. 5D An example process is shown for selectively applying masking materials 400-404 using a positive photoresist material 500. Positive photoresist material 500 may be composed of a photosensitive polymer that becomes soluble in a photoresist developer when exposed to light within a specific wavelength range.

[0055] refer to Figure 5A , the sets 202-204 are embedded in a positive photoresist material 500. Importantly, the side (eg, the top side) of the sets 202-204 having the electrical contacts 108-110 is covered.

[0056] refer to Figure 5B, light 502 is transmitted through substrate 200 toward set 202-204. Light 502 has a wavelength within a specific range of the electromagnetic spectrum that causes exposed areas of positive photoresist material 500 to become soluble in a photoresist developer. For example, light 502 may be ultraviolet light having a wavelength less than 360 nanometers, so that a micro-LED including GaN (which strongly absorbs wavelengths below 360 nanometers) can be used as an efficient mask for the light.

[0057] Importantly, exposure to light 502 enables removal of positive photoresist material 500 from one or more exposed areas of substrate 200. These areas are one or more areas that are not attached to sets 202-204. However, areas 504-506 that remain unexposed to light 502 continue to cover the side of sets 202-204 where electrical contacts 108-110 are located.

[0058] refer to Figure 5C , masking materials 400-404 are applied to substrate 200. As described above, this can be achieved based on a sputtering process. For example, DC sputtering can be used to deposit a tungsten layer having a thickness of 150 nanometers. Importantly, masking materials 400-404 are applied to one or more areas of substrate 200 where positive photoresist material 500 has been removed.

[0059] refer to Figure 5D , as part of a photolithography stripping process, the remaining regions 504-506 of the positive photoresist material 500 are removed. Any of a variety of photoresist removal techniques may be used. For example, the regions 504-506 may be exposed to light 502 and washed away using a photoresist developer. Other examples include, but are not limited to, any of a variety of wet etching processes.

[0060] exist Figure 5D In the example of , etchant 508 is used to remove regions 504-506 and any masking material attached to them. Examples of etchant 508 include, but are not limited to, acetone or any other positive photoresist remover. In some embodiments, masking material attached to the walls of sets 202-204 is removed based on the use of another etchant. For example, tungsten can be removed by wet etching with hydrogen peroxide. This can be performed after depositing a sufficient amount of fill material 210 to cover masking material 400-404 without completely covering masking material attached to the walls. A partial dry etch of fill material 210 can be performed to achieve the sufficient amount. Thereafter, Figure 5D Can be based on FIG. 4A to FIG. 4B A process similar to that shown is continued.

[0061] 6A to 6FAn example process is shown for selectively applying masking materials 400-404 using a negative photoresist material 600. Negative photoresist material 600 may be composed of a photosensitive polymer that becomes insoluble in a photoresist developer when exposed to light within a specific wavelength range.

[0062] refer to Fig. 6A , the sets 202-204 are embedded in a negative photoresist material 600. Importantly, the side (eg, the top side) of the sets 202-204 having the electrical contacts 108-110 is covered.

[0063] refer to Figure 6B , light 602 is transmitted through substrate 200 toward sets 202-204. Light 602 has a wavelength within a specific range of the electromagnetic spectrum that causes exposed areas of negative photoresist material 600 to become insoluble in a photoresist developer. For example, light 602 may be ultraviolet light having a wavelength less than 360 nanometers.

[0064] Importantly, exposure to light 602 enables removal of negative photoresist material 600 from unexposed areas covering one side of sets 202-204 where electrical contacts 108-110 are located. However, areas 604-608 exposed to light 602 continue to cover one or more areas of substrate 200.

[0065] refer to Figure 6C , the negative photoresist material 600 removed from the regions 610-612 is actually replaced with a different material. The different material may be composed of any material that is not removed when the negative photoresist material 600 is removed. For example, the different material may be a positive photoresist material that is injected into the regions 610-612 and cured.

[0066] refer to Fig.6D , the remaining regions 604-608 of the negative photoresist material 600 are removed. Any of a variety of photoresist removal techniques may be used. For example, the negative photoresist material 600 may be a reversible photoresist material such that the regions 604-608 may be exposed to light and washed away using a photoresist developer. Other examples include, but are not limited to, etching processes involving acetone, oxygen plasma, or some other etchant.

[0067] refer to Fig. 6E , masking materials 400-404 are applied to substrate 200. As described above, this can be achieved based on a sputtering process. Importantly, masking materials 400-404 are applied to one or more areas of substrate 200 where negative photoresist material 600 was removed.

[0068] refer to Fig. 6F, regions 610-612 of different materials are removed. Any of a variety of removal techniques may be used. Fig. 6F In the example of FIG. 6 , an etchant 614 is used to remove regions 610 - 612 and any masking material attached thereto. The etchant 614 may be, for example, acetone or any other positive photoresist remover.

[0069] In some embodiments, masking material attached to the walls of the sets 202-204 is removed based on the use of another etchant. For example, tungsten can be removed by wet etching with hydrogen peroxide. This can be performed after depositing a sufficient amount of fill material 210 to cover the masking material 400-404 without completely covering the masking material attached to the walls. A partial dry etch of the fill material 210 can be performed to achieve the sufficient amount. Thereafter, Fig. 6F Can be based on FIG. 4A to FIG. 4B A process similar to that shown is continued.

[0070] LLO Mask Removal

[0071] After performing LLO, the masking materials 400-404 and / or the fill material 210 may be removed. For example, the masking materials 400-404 and / or the fill material 210 may be removed in preparation for a pick and place process. If any of the masking materials 400-404 become detached from the substrate 200, removal of any of the masking materials 400-404 may be performed. However, if all of the masking materials 400-404 remain attached to the substrate 200, one or more steps of the process described below may be skipped.

[0072] FIG. 7A to FIG. 7B An example process for removing an LLO mask without a "wing" is shown. As used herein, the term "wing" refers to a thin layer of excess masking material attached to the walls of the sets 202-204. Figure 5D and Fig. 6F As described above, the LLO mask wings can be removed, for example, by wet etching using hydrogen peroxide. FIG. 8A to FIG. 8D The LLO mask wing is further described.

[0073] refer to Fig. 7A , the etchant 700 is used to remove the "wingless" masking materials 400-404. For example, if the masking materials 400-404 are composed of tungsten, the etchant 700 can be hydrogen peroxide.

[0074] refer to Figure 7B, the etchant 702 is used to remove the filling material 210. For example, the etchant 702 can be a plasma used with a dry etching technique. Examples of dry etching techniques include, but are not limited to, radio frequency (RF) oxygen plasma etching, reactive ion etching (RIE), and / or inductively coupled plasma (ICP) etching.

[0075] FIG. 8A to FIG. 8D An example process for removing a "winged" LLO mask is shown. FIG. 8A to FIG. 8D In the example of , the wings include auxiliary masking material perpendicular to the masking materials 400 - 404. As described in more detail below, removal of the winged LLO mask can be performed in iterative stages.

[0076] refer to Fig. 8A , the etchant 800 is used to remove the "wingless" masking materials 400-404. As described above, if the masking materials 400-404 are composed of tungsten, the etchant 800 can be hydrogen peroxide.

[0077] refer to Figure 8B , some of the fill material 210 is removed using an etchant 802. More specifically, a predetermined depth (eg, a few microns) of the fill material 210 is removed. The predetermined depth may correspond to the height of the LLO mask wing. As described above, the etchant 702 may be a plasma used with a dry etching technique.

[0078] refer to Figure 8C , the masking material is again removed using etchant 800. However, this time the masking material removed corresponds to the LLO mask wings.

[0079] refer to Fig.8D , the etchant 802 is again used to remove the remaining portion of the fill material 210. The assemblies 202-204 can then be flip-chip mounted on a display substrate.

[0080] Process Overview

[0081] Fig. 9 An example process for performing LLO using one or more LLO masks is shown.In some embodiments, the example process is performed at a manufacturing system station where LEDs are incorporated into a display system.

[0082] At block 900, a station obtains sets of semiconductor devices that are spaced apart from one another. Each set may include one or more semiconductor devices. The sets are attached to a substrate, such as a substrate on which the sets are epitaxially grown.

[0083] At block 902, the station applies a masking material to a surface of a substrate. In some embodiments, the surface corresponds to one or more regions of the substrate from which the collection is to be separated. As described in more detail below, the application of the masking material can prevent the substrate from coming into contact with the fill material.

[0084] At block 904, the station embeds the collection in the fill material. In some embodiments, a masking material is located between the fill material and the substrate such that the masking material can block light from reaching the fill material.

[0085] At block 906, the station transmits light through the substrate toward the collection and masking material. This causes the collection to become decoupled from the substrate while avoiding interaction between the fill material and the light, which would otherwise cause crack formation.

[0086] System Overview

[0087] Fig.10 An example manufacturing system is shown. In some embodiments, the manufacturing system includes a station for incorporating LED devices into a display system. The manufacturing system includes a chamber 1000 that defines an internal environment for incorporating LED devices into a display system. The chamber 1000 houses various system components, including a laser 1002; a controller 1004; a depositor 1006; an etcher 1012; substrates 1016 and 1024; and stages 1014 and 1022. The chamber 1000 may also house Fig.10 For example, chamber 1000 may also house a scanning electron microscope in a high pressure atmosphere of water vapor.

[0088] Substrate 1016 may be a growth substrate on which collections 1018-1020 are grown. Collections 1018-1020 may be the same or similar to collections 202-204 described above. Substrate 1016 is attached to the semiconductor layers of collections 1018-1020. LLO is performed to separate substrate 1016 from collections 1018-1020. Thus, substrate 1016 is composed of a transparent / quasi-transparent material through which laser 1002 can transmit light.

[0089] The stage 1014 holds a substrate 1016. The stage 1014 may be movable in various directions, including but not limited to up and down; left and right; and front and back.

[0090] Substrate 1024 serves as a carrier for assemblies 1018-1020. LLO is performed when substrate 1016 and assemblies 1018-1020 are turned over and placed on substrate 1024. In some embodiments, substrate 1024 is also composed of a transparent / quasi-transparent material such as glass or silicon.

[0091] The stage 1022 holds a substrate 1024. The stage 1022 may be movable in various directions, including but not limited to up and down; left and right; and front and back.

[0092] Laser 1002 transmits light for performing LLO and / or changing the state of the photoresist material (e.g., soluble or insoluble). Laser 1002 can be positioned so that light is transmitted in a first direction (e.g., downward through substrate 1016) or a second direction opposite to the first direction (e.g., upward through substrate 1024).

[0093] The depositor 1006 applies material to the substrate 1016 and the collections 1018 - 1020. The material may include a masking material, a fill material, a photoresist material, and / or any of a variety of etchants.

[0094] The etcher 1012 can be used to perform dry etching based on instructions received from the controller 1004. More specifically, the etcher 1012 bombards the fill material with plasma, thereby eroding the fill material. The etcher 1012 can include inlet and outlet valves, an ionization plate, and any other standard etching components.

[0095] Controller 1004 is coupled to laser 1002, depositor 1006, and etcher 1012 and controls their operation accordingly. Controller 1004 may include, among other components, memory 1010 and processor 1008. Memory 1010 stores instructions for operating laser 1002, depositor 1006, and etcher 1012. Memory 1010 may be implemented using any of a variety of volatile or non-volatile computer-readable storage media, including but not limited to SRAM, DRAM, and / or ROM. Processor 1008 executes the instructions stored in memory 1010 and sends the instructions to laser 1002, depositor 1006, and etcher 1012. In some embodiments, processor 1008 executes Fig. 9 Example process shown.

[0096] Embodiments of the present invention may include an artificial reality system, or be implemented in combination with an artificial reality system. Artificial reality is a form of reality that has been adjusted in some way before being presented to a user, which may include, for example, virtual reality (VR), augmented reality (AR), mixed reality (MR), hybrid reality, or some combination and / or derivative thereof. Artificial reality content may include fully generated content, or generated content combined with captured (e.g., real-world) content. Artificial reality content may include video, audio, tactile feedback, or some combination thereof, and any of the content may be presented in a single channel or multiple channels (such as stereoscopic video that produces a three-dimensional effect to the viewer). In addition, in some embodiments, artificial reality may also be associated with an application, product, accessory, service, or some combination thereof, for example, the application, product, accessory, service, or some combination thereof is used to create content in artificial reality, and / or is otherwise used in artificial reality (e.g., to perform activities in artificial reality). Artificial reality systems that provide artificial reality content can be implemented on a variety of platforms, including a head-mounted display (HMD) connected to a host computer system, a standalone HMD, a mobile device or computing system, or any other hardware platform capable of providing artificial reality content to one or more viewers.

[0097] The foregoing description of the embodiments of the present disclosure has been presented for illustrative purposes; it is not intended to be exhaustive or to limit the disclosure to the precise form disclosed. Those skilled in the relevant art will appreciate that many modifications and variations are possible based on the above disclosure.

[0098] Some parts of this specification describe embodiments of the present disclosure in terms of algorithms and symbolic representations of operations on information. These algorithmic descriptions and representations are typically used by technicians in the field of data processing to effectively convey the essence of their work to other technicians in the field. Although described functionally, computationally, or logically, these operations are understood to be implemented by computer programs or equivalent circuits, microcodes, etc. In addition, it has also been demonstrated that it is sometimes convenient to refer to these operational arrangements as modules without loss of generality. The described operations and their associated modules can be embodied in software, firmware, and / or hardware.

[0099] The steps, operations or processes described may be performed or implemented using one or more hardware or software modules, alone or in combination with other devices. In some embodiments, the software module is implemented using a computer program product, which includes a computer readable medium containing a computer program code that can be executed by a computer processor to perform any or all of the steps, operations or processes described.

[0100] Embodiments of the present disclosure may also relate to an apparatus for performing the described operations. The apparatus may be specially constructed for the desired purpose, and / or it may include a general-purpose computing device selectively activated or reconfigured by a computer program stored in a computer. Such a computer program may be stored in a non-transient tangible computer-readable storage medium, or any type of medium suitable for storing electronic instructions, which may be coupled to a computer system bus. In addition, any computing system mentioned in the specification may include a single processor, or may be an architecture that uses multiple processors to increase computing power.

[0101] Embodiments of the present disclosure may also relate to products produced by the computing processes described herein. Such products may include information generated by the computing processes, wherein the information is stored on a non-transitory tangible computer-readable storage medium, and may include any embodiment of a computer program product or other data combination described herein.

[0102] The language used in this specification is selected primarily for readability and instructional purposes, and the language may not be selected to delimit or limit the technical solution of the present invention. Therefore, it is intended that the scope of the present disclosure is not limited by this detailed description, but by any claims filed based thereon. Accordingly, the disclosure of the embodiments is intended to illustrate rather than limit the scope of the present disclosure, which is set forth in the appended claims.

Claims

1. A method for manufacturing a semiconductor device, include: obtaining a plurality of semiconductor devices formed on a common substrate, the plurality of semiconductor devices comprising a first semiconductor device and a second semiconductor device separated by a gap region of the substrate; applying a masking material over the gap region of the substrate; embedding the plurality of semiconductor devices in a filling material; as well as transmitting a first light through the substrate toward the plurality of semiconductor devices and the masking material so that the substrate becomes disengaged from the plurality of semiconductor devices, wherein the first light is at least partially blocked by the masking material; The masking material is a metal material applied based on a sputtering process. 2 . The method for manufacturing a semiconductor device according to claim 1 , wherein the masking material blocks the first light so that there is substantially no interaction between the first light and the filling material. 3 . The method for manufacturing a semiconductor device according to claim 1 , wherein the masking material blocks the first light so that an amount of heat generated due to interaction between the first light and the filling material is reduced. 4 . The method for manufacturing a semiconductor device according to claim 1 , wherein the plurality of semiconductor devices are embedded such that the masking material is located between the filling material and the substrate.

5. The method for manufacturing a semiconductor device according to claim 1, further comprising: include: embedding the plurality of semiconductor devices in a positive photoresist material prior to applying the masking material; transmitting a second light through the gap region of the substrate toward the positive photoresist material, thereby exposing one or more regions of the positive photoresist material to the second light; as well as The one or more regions of the positive photoresist material are removed.

6. The method for manufacturing a semiconductor device according to claim 5, further comprising: include: After applying the masking material, areas of the positive photoresist material that remained unexposed to the second light are removed.

7. The method for manufacturing a semiconductor device according to claim 1, further comprising: include: embedding the plurality of semiconductor devices in a negative photoresist material prior to applying the masking material; transmitting a second light through the gap region of the substrate toward the negative photoresist material, thereby exposing one or more regions of the negative photoresist material to the second light; as well as replacing the areas of the negative photoresist material that remain unexposed to the second light with a different material; as well as The one or more regions of the negative photoresist material are removed.

8. The method for manufacturing a semiconductor device according to claim 7, further comprising: include: After applying the masking material, the different material is removed.

9. A semiconductor device manufactured by the following method, the method include: obtaining a plurality of semiconductor devices formed on a common substrate, the plurality of semiconductor devices comprising a first semiconductor device and a second semiconductor device separated by a gap region of the substrate; applying a masking material over the gap region of the substrate; embedding the plurality of semiconductor devices in a filling material; as well as transmitting a first light through the substrate toward the plurality of semiconductor devices and the masking material so that the substrate becomes disengaged from the plurality of semiconductor devices, wherein the first light is at least partially blocked by the masking material; The masking material is a metal material applied based on a sputtering process. 10 . The semiconductor device of claim 9 , wherein the masking material blocks the first light such that there is substantially no interaction between the first light and the fill material. 11 . The semiconductor device of claim 9 , wherein the masking material blocks the first light so that an amount of heat generated due to interaction between the first light and the filling material is reduced. 12 . The semiconductor device of claim 9 , wherein the plurality of semiconductor devices are embedded such that the masking material is located between the filling material and the substrate.

13. The semiconductor device according to claim 9, manufactured by the method, the method further comprising: include: embedding the plurality of semiconductor devices in a positive photoresist material prior to applying the masking material; transmitting a second light through the gap region of the substrate toward the positive photoresist material, thereby exposing one or more regions of the positive photoresist material to the second light; as well as The one or more regions of the positive photoresist material are removed.

14. The semiconductor device according to claim 13, manufactured by the method, the method further comprising: include: After applying the masking material, areas of the positive photoresist material that remained unexposed to the second light are removed.

15. The semiconductor device according to claim 9, manufactured by the method, the method further comprising: include: embedding the plurality of semiconductor devices in a negative photoresist material prior to applying the masking material; transmitting a second light through the gap region of the substrate toward the negative photoresist material, thereby exposing one or more regions of the negative photoresist material to the second light; as well as replacing the areas of the negative photoresist material that remain unexposed to the second light with a different material; as well as The one or more regions of the negative photoresist material are removed.

16. The semiconductor device according to claim 15, manufactured by the method, the method further comprising: include: After applying the masking material, the different material is removed.

17. A non-transitory computer-readable storage medium storing processor-executable instructions for: obtaining a plurality of semiconductor devices formed on a common substrate, the plurality of semiconductor devices comprising a first semiconductor device and a second semiconductor device separated by a gap region of the substrate; applying a masking material over the gap region of the substrate; embedding the plurality of semiconductor devices in a filling material; as well as transmitting a first light through the substrate toward the plurality of semiconductor devices and the masking material so that the substrate becomes disengaged from the plurality of semiconductor devices, wherein the first light is at least partially blocked by the masking material; The masking material is a metal material applied based on a sputtering process.

18. The non-transitory computer readable storage medium of claim 17, wherein the masking material blocks the first light such that there is substantially no interaction between the first light and the fill material.

19. The non-transitory computer readable storage medium of claim 17, wherein the masking material blocks the first light such that an amount of heat generated due to interaction between the first light and the fill material is reduced.