A planar photoelectric detector and a method for preparing the same

By using non-conductive semi-insulated substrates and undoped light absorbing layers in the photodetector, the epitaxial process is simplified and the dark current is reduced, and the leakage channel problem caused by large mismatch and high epitaxial defect density in the prior art is solved. , improves the performance and reliability of the detector.

CN112382687BActive Publication Date: 2024-12-06SUZHOU GALLIUM PORT SEMICON CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202011258052.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-11-11
Publication Date
2024-12-06
Estimated Expiration
2040-11-11

AI Technical Summary

Technical Problem

Existing photodetectors are prone to form leakage channels and dark currents under conditions of large mismatch and high epitaxial defect density, resulting in a degradation of detection performance. Existing solutions require increasing material or device complexity.

Method used

Using a non-conductive semi-insulating substrate and an undoped light absorbing layer, a diffusion doped region and an undoped region are formed by growing the GaAs and GaSb buffer layers on the buffer layer, and P-type diffusion is performed on the undoped light absorbing layer. , a passivation layer is formed and a window is opened separately to deposit multi-layer metal electrodes, simplifying the epitaxial process and reducing dark current.

Benefits of technology

The epitaxial process is simplified, dark current is reduced, the reliability and working temperature of the detector are improved, the leakage problem introduced by mesa etching is avoided, and the chip process is simplified.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112382687B_ABST
    Figure CN112382687B_ABST
Patent Text Reader

Abstract

The present invention discloses a planar photodetector and a preparation method thereof, wherein the detector comprises a substrate, a buffer layer grown on the substrate, and an undoped light absorbing layer grown on the buffer layer, wherein the substrate adopts a non-conductive semi-insulating substrate, and a part of the undoped light absorbing layer is subjected to P-type diffusion to form a diffuse doped region, and the rest is an undoped region, and the planar photodetector further comprises a passivation layer deposited on the surface of the undoped light absorbing layer, and windows are opened on the passivation layer corresponding to the diffuse doped region and the undoped region to deposit multiple layers of metal, forming a P region metal electrode and an undoped region metal electrode. The photodetector has a simple structure, does not require etching, has a simple epitaxial process, reduces the light absorption of free carriers, and avoids the occurrence of side leakage introduced by table etching.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of photoelectric detection technology, and in particular to a planar photoelectric detector and a preparation method thereof. Background Art

[0002] In the field of optical fiber communication and infrared detection, the device structure of photodetectors is commonly mesa-type and planar-type. Mesa-type devices have large design space and easy function control, but they require precise epitaxial growth and mesa etching control. The exposed sides after etching are prone to form leakage channels of the device. The structure and process of planar devices are simple, with high reliability and no dark current caused by side exposure. Common planar detectors usually use a conductive N-type substrate, grow an N-type epitaxial layer, and then perform selective P-type diffusion. The depletion region of the PN junction is used to generate photogenerated carriers, and the carriers are transported under an external or self-built electric field after photoelectric conversion. Finally, multiple layers of metal are deposited on the heavily doped N-type substrate or P-type diffusion layer to form ohmic contacts to lead out electrical signals. The above conventional device structures are not suitable for large mismatch (>2%) heteroepitaxial conditions with high epitaxial defect density (dislocation density greater than 10 8 cm -2 ) materials, because the high-density threading dislocations that penetrate from the substrate to the surface of the epitaxial layer constitute a large number of carrier recombination centers and leakage channels, resulting in non-radiative recombination of photogenerated carriers and generating higher dark currents. Common solutions include growing a composition gradient or thick film buffer layer on the substrate, growing a wide-bandgap barrier layer, and using a dual-mesa device structure. It is usually necessary to significantly increase the complexity of the material or device to reduce the impact of epitaxial defects on detection performance. How to solve the above technical problems is what the technicians in this field are committed to solving. Summary of the invention

[0003] The object of the present invention is to overcome the deficiencies of the prior art and provide a planar photoelectric detector.

[0004] To achieve the above-mentioned purpose, the technical solution adopted by the present invention is: a planar photodetector, including a substrate, a buffer layer grown on the substrate, and an undoped light absorbing layer grown on the buffer layer, wherein the substrate adopts a non-conductive semi-insulating substrate, a partial area of ​​the undoped light absorbing layer undergoes P-type diffusion to form a diffused doped area, and the rest is an undoped area, the planar photodetector also includes a passivation layer deposited on the surface of the undoped light absorbing layer, and windows are opened on the passivation layer corresponding to the diffused doped area and the undoped area to deposit multiple layers of metal to form a P-area metal electrode and an undoped area metal electrode.

[0005] As a specific implementation manner, the substrate adopts a non-conductive GaAs semi-insulating substrate, and the resistivity of the GaAs semi-insulating substrate is greater than 1E8 Ohm.cm.

[0006] As a specific implementation, the buffer layer includes a GaAs buffer layer and a GaSb buffer layer grown sequentially on a substrate, wherein the thickness of the GaAs buffer layer is between 200-500 nm, and the thickness of the GaSb buffer layer is between 5-50 nm.

[0007] As a specific embodiment, the undoped light absorbing layer is an InAsSb light absorbing layer grown on a GaSb buffer layer, the Sb component content in the InAsSb light absorbing layer is 5%-65%, the growth temperature of the InAsSb light absorbing layer is between 500-600°C, the layer thickness is between 500-10000nm, and the back doping concentration of the InAsSb light absorbing layer is lower than 5E16cm -3 .

[0008] Another object of the present invention is to provide a method for preparing the above-mentioned planar photodetector, comprising the following steps:

[0009] Preparation of buffer layer: growing the buffer layer on a non-conductive semi-insulating substrate by metal organic vapor deposition or molecular beam epitaxy at a growth temperature of 450° C. to 650° C. The material used for the buffer layer includes but is not limited to one or more of GaAs, InAs, GaSb, and InSb;

[0010] Preparation of undoped light absorbing layer: grow the undoped light absorbing layer on the buffer layer by metal organic chemical vapor deposition or molecular beam epitaxy, the growth temperature is 450°C-650°C, the ratio of group V elements to group III elements is 1-5:1, and P-type diffusion is performed in part of the undoped light absorbing layer to form a diffuse doped region, and the rest is an undoped region;

[0011] Passivation layer: A passivation layer is deposited on the surface of the undoped light absorbing layer, and windows are opened on the passivation layer corresponding to the diffuse doping area and the undoped area to deposit multiple layers of metal to form a P-area metal electrode and an undoped area metal electrode.

[0012] As a specific implementation, the P-type diffusion in the partial area of ​​the undoped light absorbing layer is carried out in an MOCVD device, the diffusing agent is DEZn or DMZn, the diffusion diameter is 50-500 μm, the diffusion depth is 100-2000 nm, and the P-type doping concentration is higher than 1E19 cm -3 .

[0013] As a specific implementation, the passivation layer is SiO2 or SiN x Passivation layer.

[0014] As a specific implementation, three metal layers are deposited through windows on the passivation layer, and the three metal layers are metal Ti, Pt, and Au, respectively. The thickness of the metal Ti layer is between 5-50nm, the thickness of the metal Pt layer is between 30-100nm, and the thickness of the metal Au is between 100-1000nm.

[0015] Due to the application of the above technical solution, the present invention has the following advantages compared with the prior art:

[0016] 1) The planar photodetector of the present invention uses a non-conductive semi-insulating substrate, and its epitaxial structure is simple. Only a single-layer light absorption layer needs to be grown for device preparation, without the need for complex buffer layer and barrier layer structures;

[0017] 2) The epitaxial layer used for light absorption in the planar photodetector of the present invention does not need to be doped, which simplifies the epitaxial process and reduces the light absorption of free carriers; the detector structure does not need to be etched, which simplifies the chip process and avoids the side leakage introduced by the table etching;

[0018] 3) In the planar photodetector of the present invention, the metal electrode in the P region and the metal electrode in the undoped region are made of the same metal, and Schottky and ohmic contacts are formed respectively after a single metal deposition. The two electrodes are located on the same side of the device, which is convenient for the extraction of electrical signals and device integration; the Schottky contact in the undoped region acts as an electron barrier, which can reduce the dark current of the device, increase the operating temperature of the device or increase the detection wavelength. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Attached Figure 1 is a schematic structural diagram of the planar photoelectric detector of the present invention;

[0020] Attached Figure 2 This is a flow chart of performing P-type diffusion and passivation on the undoped light absorbing layer and manufacturing electrodes in Example 1;

[0021] Attached Figure 3 is the energy band diagram of the device in Example 1;

[0022] Attached Figure 4 The blackbody responsivity of the device in Example 1 measured at a low temperature of 85K varies with voltage;

[0023] Attached Figure 5 is a spectral response curve of the device in Example 1 measured at a low temperature of 85K;

[0024] Among them: 001, substrate; 002, buffer layer; 003, undoped light absorption layer; 004, diffused doping region; 005, undoped region; 006, passivation layer; 007, P region metal electrode; 008, undoped region metal electrode. DETAILED DESCRIPTION

[0025] The technical solution of the present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0026] A planar photodetector, see Figure 1 As shown, it includes a substrate 001, a buffer layer 002 grown on the substrate 001, and an undoped light absorbing layer 003 grown on the buffer layer 002. The substrate 001 adopts a non-conductive semi-insulating substrate 001. A part of the undoped light absorbing layer 003 is subjected to P-type diffusion to form a diffuse doped area 004, and the rest is an undoped area 005. The planar photodetector also includes a passivation layer 006 deposited on the surface of the undoped light absorbing layer 003. Windows are opened on the passivation layer 006 corresponding to the diffuse doped area 004 and the undoped area 005 to deposit multiple layers of metal, forming a P-area metal electrode 007 and an undoped area metal electrode 008.

[0027] This example also provides a method for preparing a planar photoelectric detector, comprising the following steps:

[0028] Preparation of the buffer layer 002: growing the buffer layer 002 on the non-conductive semi-insulating substrate 001 by metal organic vapor deposition or molecular beam epitaxy at a growth temperature of 450° C. to 650° C. The materials used for the buffer layer include but are not limited to GaAs, InAs, GaSb and InSb;

[0029] Preparation of undoped light absorbing layer: grow the undoped light absorbing layer on the buffer layer 002 by metal organic chemical vapor deposition, the growth temperature is 450°C-650°C, the ratio of group V element / III element is 1-5:1, and P-type diffusion is performed in part of the undoped light absorbing layer to form a diffuse doping region 004, and the rest is an undoped region 005;

[0030] Passivation layer 006: The passivation layer 006 is deposited on the surface of the undoped light absorbing layer, and windows are opened on the passivation layer 006 corresponding to the diffuse doping area 004 and the undoped area 005 to deposit multiple layers of metal to form a P-area metal electrode 007 and an undoped area metal electrode 008.

[0031] Example 1

[0032] In this example, a non-conductive GaAs semi-insulating substrate is used, and the resistivity of the substrate is greater than 1E8Ohm.cm;

[0033] The buffer layer uses a metal organic vapor deposition (MOCVD) device to sequentially grow GaAs and GaSb buffer layers on a GaAs substrate, wherein the GaAs buffer layer has a thickness of 200-500nm and the GaSb buffer layer has a thickness of 5-50nm;

[0034] The undoped light absorption layer in this example uses an InAsSb light absorption layer. Specifically, the InAsSb light absorption layer is grown on a GaSb buffer. The Sb component in InAsSb is 19.5%, and the lattice mismatch with the GaAs semi-insulating substrate is 8.6%. The growth temperature of the InAsSb layer is 500-600°C, the layer thickness is 500-10000nm, and the back doping concentration of the InAsSb layer is less than 5E16cm -3 ;

[0035] See also Figure 2 As shown in the figure, after the InAsSb layer is grown, an alignment mark is made on the surface, a SiO2 diffusion mask is deposited, and after the mask is opened in the selected area, it is placed in the MOCVD equipment for P-type diffusion. The diffusant is DEZn or DMZn, the diffusion diameter is 50-500μm, the diffusion depth is 100-2000nm, and the P-type doping concentration is higher than 1E19cm -3 ; After P-type diffusion, a surface passivation layer of SiO2 or SiN is deposited x , and deposited multiple layers of metal in windows in the passivation layer corresponding to the undoped area and the diffused doped area, which were Ti (25nm) / Pt (55nm) / Au (300nm). After metal stripping, Schottky contact was formed between the metal in the undoped area and the InAsSb layer, and ohmic contact was formed between the metal in the P-type diffused doped area and the InAsSb layer.

[0036] The weak n-type InAsSb in the undoped region forms a Pn junction with the P-type diffuse doped region, and a depletion region is formed near the P-type diffuse doped region. When irradiated by photons corresponding to the InAsSb band gap energy, the depletion region generates photogenerated electron-hole pairs, where holes are freely transported under the action of the built-in electric field and collected by the P-region electrode. The device can work as a photovoltaic device without an external bias. Due to the formation of the Schottky barrier in the undoped region, the transport of photogenerated electrons is restricted by the concave conduction band, and the conductivity of electrons as majority carriers is hindered by the Schottky barrier, and the dark current of the device is reduced. See Figure 3 The blackbody responsivity of the device measured at low temperature of 85K and zero bias condition is about 3A / W, see Figure 4 As shown, an excellent spectral response is obtained with a cut-off wavelength of 5.5 μm. Figure 5 shown.

[0037] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with the technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.

Claims

1. A planar photodetector, It is characterized in that The invention comprises a substrate, a buffer layer grown on the substrate, and an undoped light absorbing layer grown on the buffer layer. The substrate adopts a non-conductive semi-insulating substrate. A partial area of ​​the undoped light absorbing layer undergoes P-type diffusion to form a diffusion area, and the rest is an undoped area. The planar photodetector also comprises a passivation layer deposited on the surface of the undoped light absorbing layer. Windows are opened on the passivation layer corresponding to the diffusion area and the undoped area to deposit multiple layers of metal to form a P-area metal electrode and an undoped area metal electrode. The substrate adopts a non-conductive GaAs semi-insulating substrate. The buffer layer comprises a GaAs buffer layer and a GaSb buffer layer grown in sequence on the substrate. The undoped light absorbing layer is an InAsSb light absorbing layer grown on the GaSb buffer layer. The Sb component content in the InAsSb light absorbing layer is between 5% and 65%. The growth temperature of the InAsSb light absorbing layer is between 500 and 600°C, the layer thickness is between 500 and 10000 nm, and the back doping concentration of the InAsSb light absorbing layer is lower than 5E16cm -3 .

2. The planar photodetector according to claim 1, It is characterized in that The resistivity of the GaAs semi-insulating substrate is greater than 1E8 ohm.cm.

3. The planar photodetector according to claim 2, It is characterized in that in, The thickness of the GaAs buffer layer is between 200-500 nm, and the thickness of the GaSb buffer layer is between 5-50 nm.

4. A method for preparing a planar photodetector as claimed in any one of claims 1 to 3, It is characterized in that The following steps are involved: Preparation of buffer layer: growing the buffer layer on a non-conductive semi-insulating substrate by metal organic vapor deposition method at a growth temperature of 450° C. to 650° C., wherein the material used for the buffer layer includes but is not limited to one or more of GaAs, InAs, GaSb, and InSb; Preparation of undoped light absorbing layer: grow the undoped light absorbing layer on the buffer layer by metal organic chemical vapor deposition or molecular beam epitaxy, the growth temperature is 450°C-650°C, the ratio of group V elements to group III elements is 1-5:1, P-type diffusion is performed in part of the undoped light absorbing layer to form a diffusion zone, and the rest is an undoped zone; Passivation layer: A passivation layer is deposited on the surface of the undoped light absorbing layer, and windows are opened on the passivation layer corresponding to the diffusion area and the undoped area to deposit multiple layers of metal to form a P-area metal electrode and an undoped area metal electrode.

5. The method for preparing the planar photodetector according to claim 4, It is characterized in that The P-type diffusion in the partial area of ​​the undoped light absorption layer is carried out in an MOCVD device, the diffusing agent is DEZn, the diffusion diameter is 50-500 μm, the diffusion depth is 100-2000 nm, and the P-type doping concentration is higher than 1E19 cm -3 .

6. The method for preparing a planar photodetector according to claim 4, It is characterized in that The passivation layer is SiO 2 Passivation layer.

7. The method for preparing the planar photodetector according to claim 6, It is characterized in that A window is opened on the passivation layer and three metal layers are deposited thereon. The three metal layers are metal Ti, Pt and Au respectively. The thickness of the metal Ti layer is between 5-50nm, the thickness of the metal Pt layer is between 30-100nm, and the thickness of the metal Au layer is between 100-1000nm.

Citation Information

Patent Citations

  • Method for manufacturing photoelectric detection unit or focal plane device by using molecular beam epitaxy method

    CN102130208A

  • Planar indium gallium arsenic light-sensitive chip with surface passivation improved and manufacturing method

    CN104538463A

  • Method for preparing large-scale small-pixel indium gallium arsenide focal plane detector

    CN109449238A

  • Indium-gallium-arsenic line array infrared focus plane detector