Liquid crystal composition containing polymerizable compound, liquid crystal display element and polymerizable compound

A liquid crystal composition with a specific polymerizable compound structure addresses slow polymerization and precipitation issues, ensuring fast polymerization, high voltage holding, and stable display quality, reducing defects and improving production efficiency.

CN112789344BActive Publication Date: 2024-12-03SHIJIAZHUANG CHENGZHI YONGHUA DISPLAY MATERIALS CO LTD
View PDF 20 Cites 0 Cited by

Patent Information

Application Number
CN201980064232.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-12-12
Filing Date
2019-10-10
Publication Date
2024-12-03
Estimated Expiration
2039-10-10

AI Technical Summary

Technical Problem

Existing liquid crystal compositions for PSA-type display elements face issues such as slow polymerization rates, precipitation of polymerizable compounds, and poor display quality due to changes in pretilt angle, leading to inefficiencies and defects like screen burn-in.

Method used

A liquid crystal composition containing a polymerizable compound with a specific chemical structure, represented by general formula (i), which suppresses precipitation, allows for fast polymerization, and maintains high voltage holding ratio and tilt stability, thereby improving display quality.

Benefits of technology

The composition achieves fast polymerization, reduces residual polymerizable compound, enhances display reliability, and prevents defects like screen burn-in, optimizing energy costs and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112789344B_ABST
    Figure CN112789344B_ABST
Patent Text Reader

Abstract

The present invention provides a liquid crystal composition containing a polymerizable compound, a liquid crystal display element using the same, and a polymerizable compound suitable for preparing the liquid crystal composition containing the polymerizable compound. The liquid crystal composition containing the polymerizable compound can simultaneously achieve the suppression of the precipitation of the polymerizable compound, a fast polymerization rate, a reduction in the residual amount of the unreacted polymerizable compound, a high voltage holding ratio (VHR), and a high tilt stability. The present invention solves the above-mentioned problems by providing a liquid crystal composition containing one or more polymerizable compounds represented by general formula (i). #imgabs0#
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a liquid crystal composition containing a polymerizable compound, a liquid crystal display element using the same, and a polymerizable compound. In this specification, a liquid crystal composition containing a polymerizable compound is referred to as a liquid crystal composition containing a polymerizable compound. In addition, a polymerizable compound refers to a compound having a polymerizable group. Background Art

[0002] A PSA (Polymer Sustained Alignment) type liquid crystal display element is a liquid crystal display element having a structure in which a polymer structure is formed in a cell in order to control the pretilt angle of liquid crystal molecules. It is used as a practical liquid crystal display element because of its high-speed responsiveness and high contrast.

[0003] The manufacture of a PSA type liquid crystal display element is carried out by injecting a liquid crystal composition containing a polymerizable compound between substrates, irradiating ultraviolet rays while applying a voltage to align the liquid crystal molecules, polymerizing the polymerizable compound, and fixing the orientation of the liquid crystal molecules. As a liquid crystal composition containing a polymerizable compound suitable therefor, Patent Documents 1 to 3 disclose liquid crystal compositions containing the following compounds (A) having a bisphenol skeleton, compounds (B) having a terphenyl skeleton, and compounds (C) having a cinnamic acid skeleton as polymerizable compounds.

[0004] [Chemistry 1]

[0005]

[0006] Prior art literature

[0007] Patent Literature

[0008] Patent Document 1: International Publication No. 2010 / 084823

[0009] Patent Document 2: Japanese Patent Application No. 2013-509457

[0010] Patent Document 3: Japanese Patent Application Publication No. 2011-202168 Summary of the invention

[0011] Problems to be solved by the invention

[0012] In recent years, in the manufacture of PSA-type liquid crystal display elements, in order to improve production efficiency, liquid crystal compositions containing polymerizable compounds with a suitably fast polymerization rate are sought. However, the polymerization rate of the liquid crystal composition containing compound (A) as the polymerizable compound is insufficient, so a longer ultraviolet irradiation time is required to reduce the residual amount of the polymerizable compound. Although the liquid crystal composition containing compound (B) as the polymerizable compound has a suitably fast polymerization rate, it is easy to cause a large change in the pretilt angle and cause poor display (screen burn-in). The liquid crystal composition containing compound (C) as the polymerizable compound has the problem that precipitation of the polymerizable compound is observed during storage. Therefore, it is sought to improve the physical properties of the liquid crystal composition containing the polymerizable compound.

[0013] The problem to be solved by the present invention is to provide a liquid crystal composition containing a polymerizable compound, a liquid crystal display element using the same, and a polymerizable compound suitable for the preparation of the above-mentioned liquid crystal composition containing a polymerizable compound, wherein the liquid crystal composition containing a polymerizable compound has the precipitation of the polymerizable compound suppressed, can be fully polymerized at a fast rate, and can simultaneously achieve a high voltage holding ratio (VHR) and high tilt stability.

[0014] Methods used to solve problems

[0015] The present inventors have conducted intensive studies to solve the above problems and have found that the above problems can be solved by a liquid crystal composition containing a polymerizable compound having a specific chemical structure, thereby completing the present invention.

[0016] That is, the present invention provides a liquid crystal composition containing one or more polymerizable compounds represented by general formula (i).

[0017] [Chemistry 2]

[0018]

[0019] (In the formula, A i1 and A i2 Each independently represents a group selected from the group consisting of the following groups (a) to (c),

[0020] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- groups in the group may be replaced by -O-),

[0021] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted by -N=), and

[0022] (c) naphthalenediyl, 1,2,3,4-tetrahydronaphthalenediyl or decahydronaphthalenediyl (one -CH= or two or more non-adjacent -CH= in naphthalenediyl or 1,2,3,4-tetrahydronaphthalenediyl may be substituted with -N=),

[0023] The above-mentioned groups (a), (b) and (c) may be independently substituted by an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a halogen group, a cyano group, a nitro group or a P i3 -S i3 -replace,

[0024] P i1 , P i2 and P i3 Each independently represents a group selected from the group consisting of formula (R-1) to formula (R-9),

[0025] [Chemistry 3]

[0026]

[0027] (Where R 11 , R 12 , R 13 , R 14 and R 15 Each independently represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom, and m r5 、m r7 、n r5 and n r7 Each independently represents 0, 1, or 2),

[0028] S i1 , S i2 and S i3 Each independently represents a single bond or an alkylene group having 1 to 15 carbon atoms, wherein one -CH2- or two or more non-adjacent -CH2- groups in the alkylene group may be substituted by -O-, -OCO- or -COO- in a manner that the oxygen atom is not directly adjacent to the -CH2- group.

[0029] R i1 represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom,

[0030] n i1 Indicates 1, 2, or 3,

[0031] In the presence of multiple A i2 , S i2 , P i3 and / or S i3 In the case of , they may be the same or different).

[0032] In addition, the present invention provides a liquid crystal display element, an active matrix driving liquid crystal display element, a PSA mode, PSVA mode, PS-IPS mode or PS-FFS mode liquid crystal display element using a liquid crystal composition containing one or more polymerizable compounds represented by the above general formula (i).

[0033] Furthermore, the present invention provides a polymerizable compound represented by the above general formula (i).

[0034] Effects of the Invention

[0035] The present invention provides a liquid crystal composition containing a polymerizable compound, which does not reduce the refractive index anisotropy (Δn) and the nematic-isotropic liquid phase transition temperature (Tni), shows low viscosity (η), low rotational viscosity (γ1), and high elastic constant (K33), the precipitation of the polymerizable compound is suppressed, the polymerization rate of the polymerizable compound is sufficiently fast and can be fully polymerized. Moreover, the liquid crystal display element using the liquid crystal composition containing a polymerizable compound of the present invention has a small amount of unreacted polymerizable compound residue, shows high voltage holding ratio (VHR), high speed responsiveness, high tilt stability, does not have poor orientation caused by changes in the pretilt angle, display defects such as screen burn-in, or poor orientation caused by changes in the pretilt angle. Display defects such as screen burn-in are suppressed, and excellent display quality can be displayed. DETAILED DESCRIPTION

[0036] I. Liquid crystal composition containing polymerizable compound

[0037] First, the liquid crystal composition containing a polymerizable compound of the present invention will be described. In the following description, "total amount" means "total mass", and the unit "%" of the content of each compound means "mass %".

[0038] The polymerizable compound-containing liquid crystal composition of the present invention is a liquid crystal composition containing one or more polymerizable compounds represented by general formula (i).

[0039] [Chemistry 4]

[0040]

[0041] (In the formula, A i1 and A i2 Each independently represents a group selected from the group consisting of the following groups (a) to (c),

[0042] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0043] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted with -N=), and

[0044] (c) naphthalenediyl, 1,2,3,4-tetrahydronaphthalenediyl or decahydronaphthalenediyl (one -CH= or two or more non-adjacent -CH= in naphthalenediyl or 1,2,3,4-tetrahydronaphthalenediyl may be substituted with -N=),

[0045] The above-mentioned groups (a), (b) and (c) may be independently substituted by an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a halogen group, a cyano group, a nitro group or a P i3 -S i3 -replace,

[0046] P i1 , P i2 and P i3 Each independently represents a group selected from the group consisting of formula (R-1) to formula (R-9),

[0047] [Chemistry 5]

[0048]

[0049] (Where R 11 , R 12 , R 13 , R 14 and R 15 Each independently represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom, and m r5 、m r7 、n r5 and n r7 Each independently represents 0, 1, or 2),

[0050] S i1 , S i2 and S i3 Each independently represents a single bond or an alkylene group having 1 to 15 carbon atoms, wherein one -CH2- or two or more non-adjacent -CH2- groups in the alkylene group may be substituted by -O-, -OCO- or -COO- in a manner that the oxygen atom is not directly adjacent to the -CH2- group.

[0051] R i1 represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom,

[0052] n i1 Indicates 1, 2, or 3,

[0053] In the presence of multiple A i2 , S i2 , P i3 and / or S i3In the case of , they may be the same or different).

[0054] According to the present invention, a liquid crystal composition containing a polymerizable compound can be formed, wherein the precipitation of the polymerizable compound represented by the general formula (i) is small, the polymerization rate of the polymerizable compound is sufficiently fast, and the polymerization reaction is fully carried out, so that the amount of unreacted polymerizable compound remaining after polymerization is small. The liquid crystal composition containing a polymerizable compound of the present invention satisfies various characteristics sought by liquid crystal display elements such as high-speed responsiveness, high contrast, and low power consumption, and can have the above-mentioned advantages. In addition, by using the liquid crystal composition containing a polymerizable compound of the present invention, a liquid crystal display element can be manufactured that can suppress the occurrence of display defects (screen burn-in) caused by changes in the pretilt angle and can simultaneously achieve a high voltage holding ratio (VHR) and high tilt stability.

[0055] Thus, the liquid crystal composition containing a polymerizable compound of the present invention is useful for manufacturing a PSA type or PSVA type liquid crystal display element with excellent reliability after the ultraviolet irradiation process. In addition, the liquid crystal composition containing a polymerizable compound of the present invention can control the tilt angle and the residual amount of the polymerizable compound, so the energy cost for manufacturing the liquid crystal display element can be optimized and reduced, and the production efficiency of the liquid crystal display element can be easily improved. Therefore, the liquid crystal composition containing a polymerizable compound of the present invention and the liquid crystal display element using the same are very useful.

[0056] (Polymerizable compound)

[0057] The polymerizable compound that is essentially contained in the present invention is represented by the above-mentioned general formula (i).

[0058] In the above general formula (i), A i1 and A i2 represents a group selected from the group consisting of groups (a) to (c),

[0059] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0060] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted with -N=), and

[0061] (c) naphthalenediyl, 1,2,3,4-tetrahydronaphthalenediyl or decahydronaphthalenediyl (one -CH= or two or more non-adjacent -CH= in naphthalenediyl or 1,2,3,4-tetrahydronaphthalenediyl may be substituted with -N=).

[0062] Here, A i1 and A i2 The preferred naphthalenediyl group is a group in which S is present at one of two positions selected from positions 1 to 8.i1 or S i2 A group that is bonded to a structural site (hereinafter referred to as a specific structural site) represented by the following formula in the above general formula (i) at another position.

[0063] [Chemistry 6]

[0064]

[0065] (In the above formula, between ★ and A i2 Combined with A i1 Combined

[0066] Examples of the naphthalenediyl group include naphthalene-1,2-diyl, naphthalene-1,3-diyl, naphthalene-1,4-diyl, naphthalene-1,5-diyl, naphthalene-1,6-diyl, naphthalene-1,7-diyl, naphthalene-1,8-diyl, naphthalene-2,3-diyl, naphthalene-2,6-diyl, and naphthalene-2,7-diyl.

[0067] In addition, A i1 and A i2 The preferred 1,2,3,4-tetrahydronaphthalenediyl group is a group in which S is present at one of the two positions selected from the 1 to 8 positions. i1 or S i2 A group that is bonded to the above-mentioned specific structural part in the general formula (i) at another position. Examples of 1,2,3,4-tetrahydronaphthalenediyl include 1,2,3,4-tetrahydronaphthalene-2,6-diyl, 1,2,3,4-tetrahydronaphthalene-1,4-diyl, and 1,2,3,4-tetrahydronaphthalene-1,5-diyl. i1 and A i2 A preferred decahydronaphthalenediyl group is a group in which S is present at one of two positions selected from positions 1 to 10. i1 or S i2 A group that is bonded to the above-mentioned specific structural part in the general formula (i) at another position. Examples of the decahydronaphthalenediyl group include decahydronaphthalene-2,6-diyl and the like.

[0068] The above-mentioned groups (a), (b) and (c) may be independently substituted by an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a halogen group, a cyano group, a nitro group or a P i3 -S i3 -replace.

[0069] Among them, the above A is preferred i1 and A i2 Each independently represents any of the following structures.

[0070] [Chemistry 7]

[0071]

[0072] (Where R i2 and R i3 Each independently represents an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a fluorine atom or P i3 -S i3 -)

[0073] A i1 and A i2 More preferably, each independently is 1,4-phenylene, 2-methyl-1,4-phenylene, 3-methyl-1,4-phenylene, 2-methoxy-1,4-phenylene, 3-methoxy-1,4-phenylene, 2-fluoro-1,4-phenylene, 3-fluoro-1,4-phenylene or naphthalene-2,6-diyl. Still more preferably, 1,4-phenylene, 2-fluoro-1,4-phenylene or 3-fluoro-1,4-phenylene is preferred, and 1,4-phenylene is particularly preferred.

[0074] In the above general formula (i), A i1 On the other hand, in the above general formula (i), A i2 The lookaround n i1 The polymerizable compound represented by the above general formula (i) has such a structure, and for example, A in the general formula (i) such as the above-mentioned compound (C) i1 Compared with a polymerizable compound having two or more rings, the solubility is improved, and it is presumed that the result is that precipitation becomes difficult. i2 In the case of multiple A i2 All of them may be the same group or different groups.

[0075] In the above general formula (i), P i1 , P i2 and P i3 Each independently represents a group selected from the group consisting of the above formula (R-1) to formula (R-9). i1 , P i2 and P i3 All of them may be the same polymerizable groups (formulae (R-1) to (R-9)), at least one polymerizable group may be different, or all of them may be different. i1 and P i2 At the same time, they can be the same polymerizable group or different polymerizable groups. However, if P i1 and P i2 At the same time, the same polymerizable group has the advantage of being easy to synthesize the compound represented by general formula (i). i3 In the case of multiple P i3 All of them may be the same group or different groups.

[0076] In the above general formula (i), P i1 , P i2 and P i3 Preferably, they are independently represented by formula (R-1), formula (R-2), formula (R-3), formula (R-4), formula (R-5) or formula (R-7), more preferably by formula (R-1), formula (R-2), formula (R-3) or formula (R-4), further preferably by formula (R-1), and particularly preferably by acryloyloxy or methacryloyloxy.

[0077] In addition, in P i1 , P i2 and P i3 Among them, P is preferred i1 and P i2 At least one of the above is of formula (R-1), more preferably an acryloyloxy group or a methacryloyloxy group, further preferably a methacryloyloxy group, and particularly preferably P i1 and P i2 The reason is that: by i1 and P i2 When all the methacryloyl groups are used in liquid crystal display elements, display defects caused by changes in the pretilt angle are less likely to occur. i1 and P i2 Compared with the case where all the groups are acryloyloxy groups, the degree of polymerization of the polymerizable compound can be increased.

[0078] In the above general formula (i), R in formulas (R-1) to (R-9) 11 , R 12 , R 13 , R 14 and R 15 Each independently represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom. Among them, R 11 , R 12 , R 13 , R 14 and R 15 Each independently represents a methyl group or a hydrogen atom. When importance is attached to the polymerization rate of the polymerizable compound, a hydrogen atom is preferred, and when importance is attached to reducing display defects caused by changes in the pretilt angle, a methyl group is preferred.

[0079] In addition, m in formulas (R-1) to (R-9) r5 、m r7 、n r5 and n r7 Each independently represents 0, 1 or 2.

[0080] In the above general formula (i), Si1 , S i2 and S i3 Each independently represents a single bond or an alkylene group having 1 to 15 carbon atoms. One -CH2- or two or more non-adjacent -CH2- in the alkylene group may be substituted by -O-, -OCO- or -COO- in a manner that the oxygen atom is not directly adjacent. Among them, S is preferred. i1 , S i2 and S i3 Each of them is independently a single bond or an alkylene group having 1 to 5 carbon atoms, and a single bond is particularly preferred. i1 , S i2 and S i3 In the case of single bonds, the amount of the polymerizable compound remaining after ultraviolet irradiation becomes sufficiently small, and display defects due to changes in the pretilt angle are less likely to occur. i2 In the case of multiple S i2 Can be all the same, or all S i2 Or at least one S i2 different.

[0081] In the above general formula (i), n i1 It represents 1, 2 or 3. Among them, 1 or 2 is more preferable from the viewpoint of improving the solubility in the liquid crystal composition, and 1 is particularly preferable from the viewpoint of further improving the solubility in the liquid crystal composition.

[0082] In the above general formula (i), R i1 represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom, wherein R i1 It is preferably a methyl group, an ethyl group, a fluorine atom or a hydrogen atom, and more preferably a hydrogen atom.

[0083] In the liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the content of the polymerizable compound represented by the general formula (i) is preferably 0.01%, preferably 0.02%, preferably 0.03%, preferably 0.04%, preferably 0.05%, preferably 0.06%, preferably 0.07%, preferably 0.08%, preferably 0.09%, preferably 0.1%, preferably 0.12%, preferably 0.15%, preferably 0.17%, preferably 0.2%, preferably 0.22%, preferably 0.25%, preferably 0.27%, preferably 0.3%, preferably 0.32%, preferably 0.35%, preferably 0.37%, preferably 0.4%, preferably 0.42%, preferably 0.45%, preferably 0.5%, preferably 0.55%. In the composition containing a polymerizable compound of the present invention, the upper limit of the content of the polymerizable compound represented by the general formula (i) is preferably 5%, preferably 4.5%, preferably 4%, preferably 3.5%, preferably 3%, preferably 2.5%, preferably 2%, preferably 1.5%, preferably 1%, preferably 0.95%, preferably 0.9%, preferably 0.85%, preferably 0.8%, preferably 0.75%, preferably 0.7%, preferably 0.65%, preferably 0.6%, preferably 0.55%, preferably 0.5%, preferably 0.45%, preferably 0.4%.

[0084] In further detail, in order to obtain a smaller amount of residual polymerizable compounds or a higher voltage holding ratio (VHR), the content of the polymerizable compound represented by the general formula (i) in the liquid crystal composition containing the polymerizable compound is preferably in the range of 0.2% to 1.5%. In addition, when it is important to suppress the precipitation of the polymerizable compound at low temperatures, the content of the polymerizable compound represented by the general formula (i) in the liquid crystal composition containing the polymerizable compound is preferably in the range of 0.01% to 1.0%. Furthermore, when the liquid crystal composition containing the polymerizable compound of the present invention contains a plurality of polymerizable compounds represented by the general formula (i), it is preferred that the respective contents are in the range of 0.01% to 0.6%. Therefore, in order to solve all these problems, it is particularly desirable to adjust the polymerizable compound represented by the general formula (i) in the range of 0.1% to 1.0%.

[0085] As the polymerizable compound represented by the general formula (i), specifically, compounds represented by the general formulae (i-1) to (i-33) are preferred.

[0086] [Chemistry 8]

[0087]

[0088] [Chemistry 9]

[0089]

[0090] [Chemistry 10]

[0091]

[0092] [Chemistry 11]

[0093]

[0094] [Chemistry 12]

[0095]

[0096] (Where R i4 and R i5 each independently represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom).

[0097] In the above formula, R i4 and R i5 Each independently represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom, and among them, preferably represents a methyl group or a hydrogen atom.

[0098] From the viewpoint of suppressing a decrease in the voltage holding ratio (VHR), among the compounds represented by the above-mentioned general formulae (i-1) to (i-33), more preferred are compounds represented by the general formulae (i-1) to (i-12) or the general formulae (i-17) to (i-33). In addition to the above-mentioned viewpoint, from the viewpoint of improving tilt stability (less prone to screen burn-in), further preferred are compounds represented by the general formulae (i-1) to (i-12), the general formulae (i-23) to (i-26). , or compounds represented by general formula (i-28) to general formula (i-33). Not only from the above-mentioned viewpoints, but also from the viewpoints of good solubility in liquid crystal compositions, high tilt stability, and the ability to fully polymerize at a faster rate, compounds represented by general formula (i-1) to general formula (i-5), general formula (i-25), general formula (i-26), or general formula (i-28) to general formula (i-33) are further more preferred, and compounds represented by general formula (i-1) are particularly preferred.

[0099] (Liquid Crystal Composition)

[0100] In the liquid crystal composition containing a polymerizable compound of the present invention, the liquid crystal composition is a mother liquid crystal to which a polymerizable compound represented by general formula (i) is added, and contains at least a liquid crystal compound. The liquid crystal composition preferably contains one or more compounds selected from the compounds represented by general formulas (N-1), (N-2) and (N-3). These compounds are equivalent to dielectrically negative compounds (the sign of Δε is negative and its absolute value is greater than 2).

[0101] [Chemistry 13]

[0102]

[0103] (Where R N11 , R N12 , R N21 , R N22 , R N31 and R N32 Each independently represents an alkyl group having 1 to 8 carbon atoms, and one or two or more non-adjacent -CH2- in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-,

[0104] A N11 , A N12 , A N21 , A N22 , A N31 and A N32 Each independently represents a group selected from the group consisting of the following (a), (b), (c), and (d):

[0105] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0106] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted by -N=),

[0107] (c) naphthalene-2,6-diyl, 1,2,3,4-tetrahydronaphthalene-2,6-diyl or decahydronaphthalene-2,6-diyl (one -CH= or two or more non-adjacent -CH= groups in naphthalene-2,6-diyl or 1,2,3,4-tetrahydronaphthalene-2,6-diyl may be substituted with -N=), and

[0108] (d) 1,4-cyclohexenylene,

[0109] The above-mentioned groups (a), (b), (c) and (d) may be substituted by cyano groups, fluorine atoms or chlorine atoms, respectively and independently.

[0110] Z N11 , Z N12 , Z N21 , Z N22 , Z N31 and Z N32 Each independently represents a single bond, -CH2CH2-, -(CH2)4-, -OCH2-, -CH2O-, -COO-, -OCO-, -OCF2-, -CF2O-, -CH=N-N=CH-, -CH=CH-, -CF=CF- or -C≡C-,

[0111] X N21 represents a hydrogen atom or a fluorine atom,

[0112] T N31 represents -CH2- or oxygen atom,

[0113] n N11 、n N12 、n N21 、n N22 、n N31 and n N32 Each independently represents an integer from 0 to 3, and n N11 +n N12 、n N21 +n N22 and n N31 +n N32 are independently 1, 2 or 3. When there are multiple A N11 ~A N32 , Z N11 ~Z N32 In the case of , they may be the same or different).

[0114] The compounds represented by the general formulae (N-1), (N-2) and (N-3) are preferably compounds having a negative Δε and an absolute value greater than 3.

[0115] In the general formulas (N-1), (N-2) and (N-3), R N11 , R N12 , R N21 , R N22 , R N31 and R N32 Each independently represents an alkyl group having 1 to 8 carbon atoms, and one or two or more non-adjacent -CH2- groups in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-. N11 , R N12 , R N21 , R N22 , R N31 and R N32 Preferably, they are each independently an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, an alkenyl group having 2 to 8 carbon atoms, or an alkenyloxy group having 2 to 8 carbon atoms; preferably, they are an alkyl group having 1 to 5 carbon atoms, an alkoxy group having 1 to 5 carbon atoms, an alkenyl group having 2 to 5 carbon atoms, or an alkenyloxy group having 2 to 5 carbon atoms; more preferably, they are an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms; further preferably, they are an alkyl group having 2 to 5 carbon atoms or an alkenyl group having 2 to 3 carbon atoms; and particularly preferably, they are an alkenyl group having 3 carbon atoms (propenyl).

[0116] In addition, RN11 , R N12 , R N21 , R N22 , R N31 and R N32 When the ring structure to which they are bonded is a phenyl group (aromatic), they are preferably a linear alkyl group having 1 to 5 carbon atoms, a linear alkoxy group having 1 to 4 carbon atoms, or an alkenyl group having 4 to 5 carbon atoms. N11 , R N12 , R N21 , R N22 , R N31 and R N32 When the ring structure to which they are bonded is a saturated ring structure such as cyclohexane, pyran, and dioxane, it is preferably a linear alkyl group having 1 to 5 carbon atoms, a linear alkoxy group having 1 to 4 carbon atoms, or a linear alkenyl group having 2 to 5 carbon atoms. N11 , R N12 , R N21 , R N22 , R N31 and R N32 The total number of carbon atoms and oxygen atoms, when present, is preferably 5 or less, and the chain is preferably straight-chain.

[0117] The alkenyl group is preferably a group represented by any one selected from the group consisting of Formula (R1) to Formula (R5) (the black dots in each formula represent carbon atoms in the ring structure).

[0118] [Chemistry 14]

[0119]

[0120] In the general formulas (N-1), (N-2) and (N-3), A N11 , A N12 , A N21 , A N22 , A N31 and A N32 Each independently represents a group selected from the group consisting of (a), (b), (c), and (d),

[0121] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0122] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted with -N=),

[0123] (c) naphthalene-2,6-diyl, 1,2,3,4-tetrahydronaphthalene-2,6-diyl or decahydronaphthalene-2,6-diyl (one -CH= or two or more non-adjacent -CH= in naphthalene-2,6-diyl or 1,2,3,4-tetrahydronaphthalene-2,6-diyl may be substituted with -N=), and

[0124] (d) 1,4-cyclohexene.

[0125] The above-mentioned group (a), group (b), group (c) and group (d) may be substituted by a cyano group, a fluorine atom or a chlorine atom, respectively, independently.

[0126] When it is required to increase Δn, A N11 , A N12 , A N21 , A N22 , A N31 and A N32 Preferably, each is independently aromatic, and preferably aliphatic in order to improve the response speed. The above-mentioned group (a), group (b), group (c) and group (d) preferably represent trans-1,4-cyclohexylene, 1,4-phenylene, 2-fluoro-1,4-phenylene, 3-fluoro-1,4-phenylene, 3,5-difluoro-1,4-phenylene, 2,3-difluoro-1,4-phenylene, 1,4-cyclohexenylene, 1,4-bicyclo[2.2.2]octylene, piperidine-1,4-diyl, naphthalene-2,6-diyl, decahydronaphthalene-2,6-diyl or 1,2,3,4-tetrahydronaphthalene-2,6-diyl, and more preferably represent the following structure,

[0127] [Chemistry 15]

[0128]

[0129] Particularly preferably, it represents a trans-1,4-cyclohexylene group, a 1,4-cyclohexenylene group, or a 1,4-phenylene group.

[0130] In the general formulas (N-1), (N-2) and (N-3), Z N11 , Z N12 , Z N21 , Z N22 , Z N31 and Z N32Each independently represents a single bond, -CH2CH2-, -(CH2)4-, -OCH2-, -CH2O-, -COO-, -OCO-, -OCF2-, -CF2O-, -CH=N-N=CH-, -CH=CH-, -CF=CF- or -C≡C-, among which -CH2O-, -CF2O-, -CH2CH2-, -CF2CF2- or a single bond is preferred, -CH2O-, -CH2CH2- or a single bond is more preferred, and -CH2O- or a single bond is particularly preferred.

[0131] In the general formulas (N-1), (N-2) and (N-3), X N21 represents a hydrogen atom or a fluorine atom, and among them, a fluorine atom is preferred.

[0132] In the general formulas (N-1), (N-2) and (N-3), T N31 It represents -CH2- or an oxygen atom, and among them, an oxygen atom is preferred.

[0133] In the general formulas (N-1), (N-2) and (N-3), n N11 、n N12 、n N21 、n N22 、n N31 and n N32 Each independently represents an integer from 0 to 3. N11 +n N12 、n N21 +n N22 and n N31 +n N32 are independently 1, 2 or 3. N11 +n N12 、n N21 +n N22 and n N31 +n N32 Preferably 1 or 2, in this case, preferably n N11 is 1, n N12 The combination of 0; n N11 is 2, n N12 The combination of 0; n N11 is 1, n N12 A combination of 1; n N11 is 2, n N12 A combination of 1; n N21 is 1, n N22 The combination of 0; n N21 is 2, n N22 The combination of 0; n N31 is 1, n N32 The combination of 0; n N31 is 2, n N32A combination of 0.

[0134] The preferred lower limit of the content of the compound represented by formula (N-1) relative to the total amount of the liquid crystal composition is 1%, 10%, 20%, 30%, 40%, 50%, 55%, 60%, 65%, 70%, 75%, 80%. The preferred upper limit of the content is 95%, 85%, 75%, 65%, 55%, 45%, 35%, 25%, 20%.

[0135] The preferred lower limit of the content of the compound represented by formula (N-2) relative to the total amount of the liquid crystal composition is 1%, 10%, 20%, 30%, 40%, 50%, 55%, 60%, 65%, 70%, 75%, 80%. The preferred upper limit of the content is 95%, 85%, 75%, 65%, 55%, 45%, 35%, 25%, 20%.

[0136] The preferred lower limit of the content of the compound represented by formula (N-3) relative to the total amount of the liquid crystal composition is 1%, 10%, 20%, 30%, 40%, 50%, 55%, 60%, 65%, 70%, 75%, 80%. The preferred upper limit of the content is 95%, 85%, 75%, 65%, 55%, 45%, 35%, 25%, 20%.

[0137] When the viscosity of liquid crystal compound is kept low, when the situation of the composition that response speed is fast is needed, it is preferably that the above-mentioned lower limit is low and the upper limit is low.When the Tni of liquid crystal compound is kept high, when the situation of the composition that temperature stability is good is needed, it is preferably that the above-mentioned lower limit is low and the upper limit is low.In addition, when wanting to increase dielectric anisotropy in order to keep driving voltage low, it is preferably that the above-mentioned lower limit is improved, and the upper limit is high.

[0138] Examples of the compound represented by the general formula (N-1) include the compound group represented by the following general formulae (N-1a) to (N-1g).

[0139] [Chemistry 16]

[0140]

[0141] (Where R N11 and R N12 Indicates that R in the general formula (N-1) N11 and R N12 Same meaning, n Na11 Indicates 0 or 1, n Nb11 Indicates 1 or 2, n Nc11 Indicates 0 or 1, nNd11 Indicates 1 or 2, n Ne11 Indicates 1 or 2, n Nf12 Indicates 1 or 2, n Ng11 Indicates 1 or 2, A Ne11 represents trans-1,4-cyclohexylene or 1,4-phenylene, A Ng11 represents trans-1,4-cyclohexylene, 1,4-cyclohexenylene or 1,4-phenylene, but in n Nd11 When the number is 2, at least 1 A Ng11 represents 1,4-cyclohexenylene, Z Ne11 represents a single bond or ethylene, but at least one Z in the molecule Ne11 Represents ethylene, multiple A in the molecule Ne11 , Z Ne11 , and / or A Ng11 Can be the same or different)

[0142] More specifically, the compound represented by the general formula (N-1) is preferably a compound selected from the group consisting of compounds represented by general formulae (N-1-1) to (N-1-21).

[0143] The compound represented by the general formula (N-1-1) is the following compound.

[0144] [Chemistry 17]

[0145]

[0146] (Where R N111 and R N112 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0147] R N111 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably a propyl group, a pentyl group or a vinyl group. N112 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably an ethoxy group or a butoxy group.

[0148] The compound represented by the general formula (N-1-1) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0149] Regarding the content of the compound represented by formula (N-1-1), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set lower. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0150] The lower limit of the content of the compound represented by formula (N-1-1) relative to the total amount of the liquid crystal composition is preferably 5%, 10%, 13%, 15%, 17%, 20%, 23%, 25%, 27%, 30%, 33%, and 35%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 50%, 40%, 38%, 35%, 33%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, 8%, 7%, 6%, 5%, and 3%.

[0151] The compound represented by the general formula (N-1-1) is preferably a compound selected from the group consisting of compounds represented by formulae (N-1-1.1) to (N-1-1.25), preferably a compound represented by formulae (N-1-1.1) to (N-1-1.4), and preferably a compound represented by formulae (N-1-1.1) and (N-1-1.3).

[0152] [Chemistry 18]

[0153]

[0154] The compounds represented by formula (N-1-1.1) to (N-1-1.25) can be used alone or in combination. The lower limits of the preferred contents of the compounds alone or in combination relative to the total amount of the liquid crystal composition are 5%, 10%, 13%, 15%, 17%, 20%, 23%, 25%, 27%, 30%, 33%, and 35%. The upper limits of the preferred contents relative to the total amount of the liquid crystal composition are 50%, 40%, 38%, 35%, 33%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, 8%, 7%, 6%, 5%, and 3%.

[0155] The compounds represented by the general formula (N-1-2) are the following compounds.

[0156] [Chemistry 19]

[0157]

[0158] (Where R N121 and R N122 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0159] R N121 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably an ethyl group, a propyl group, a butyl group or a pentyl group. N122 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably a methyl group, a propyl group, a methoxy group, an ethoxy group, or a propoxy group.

[0160] The compound represented by the general formula (N-1-2) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0161] Regarding the content of the compound represented by the general formula (N-1-2), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set lower. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0162] The lower limit of the content of the compound represented by formula (N-1-2) relative to the total amount of the liquid crystal composition is preferably 5%, 7%, 10%, 13%, 15%, 17%, 20%, 23%, 25%, 27%, 30%, 33%, 35%, 37%, 40%, and 42%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 50%, 48%, 45%, 43%, 40%, 38%, 35%, 33%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, 8%, 7%, 6%, and 5%.

[0163] The compound represented by the general formula (N-1-2) is preferably a compound selected from the group of compounds represented by formula (N-1-2.1) to formula (N-1-2.25), and is preferably a compound represented by formula (N-1-2.3) to formula (N-1-2.7), formula (N-1-2.10), formula (N-1-2.11), formula (N-1-2.13) and formula (N-1-2.20). When emphasis is placed on improving Δε, compounds represented by formula (N-1-2.3) to formula (N-1-2.7) are preferred. When emphasis is placed on improving Tni, compounds represented by formula (N-1-2.10), formula (N-1-2.11) and formula (N-1-2.13) are preferred. When emphasis is placed on improving the response speed, a compound represented by formula (N-1-2.20) is preferred.

[0164] [Chemistry 20]

[0165]

[0166] The compounds represented by formula (N-1-2.1) to formula (N-1-2.25) can be used alone or in combination, and the preferred lower limits of the content of the compounds alone or in combination relative to the total amount of the liquid crystal composition are 5%, 10%, 13%, 15%, 17%, 20%, 23%, 25%, 27%, 30%, 33%, and 35%. The preferred upper limits of the content relative to the total amount of the liquid crystal composition are 50%, 40%, 38%, 35%, 33%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, 8%, 7%, 6%, 5%, and 3%.

[0167] The compounds represented by the general formula (N-1-3) are the following compounds.

[0168] [Chemistry 21]

[0169]

[0170] (Where R N131 and R N132 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0171] R N131 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably an ethyl group, a propyl group or a butyl group. N132 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 3 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably a 1-propenyl group, an ethoxy group, a propoxy group, or a butoxy group.

[0172] The compound represented by the general formula (N-1-3) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0173] Regarding the content of the compound represented by formula (N-1-3), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0174] The preferred lower limit of the content of the compound represented by formula (N-1-3) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0175] The compound represented by the general formula (N-1-3) is preferably a compound selected from the group of compounds represented by formulas (N-1-3.1) to (N-1-3.21), preferably a compound represented by formulas (N-1-3.1) to (N-1-3.7) and (N-1-3.21), preferably a compound represented by formulas (N-1-3.1), (N-1-3.2), (N-1-3.3), (N-1-3.4) and (N-1-3.6), and preferably a compound represented by formulas (N-1-3.3), (N-1-3.4) and (N-1-3.6).

[0176] [Chemistry 22]

[0177]

[0178] The compounds represented by formula (N-1-3.1) to formula (N-1-3.4), formula (N-1-3.6) and formula (N-1-3.21) may be used alone or in combination. Preferably, it is a combination of formula (N-1-3.1) and formula (N-1-3.2) or a combination of two or three selected from formula (N-1-3.3), formula (N-1-3.4) and formula (N-1-3.6). Preferably, it is a combination of three of formula (N-1-3.3), formula (N-1-3.4) and formula (N-1-3.6). The lower limit of the content of these compounds alone or in combination relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17% and 20%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15% and 13%.

[0179] The compounds represented by the general formula (N-1-4) are the following compounds.

[0180] [Chemistry 23]

[0181]

[0182] (Where R N141 and R N142 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0183] R N141 and R N142 Preferably, each independently is an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and preferably a methyl group, a propyl group, an ethoxy group, or a butoxy group.

[0184] The compound represented by the general formula (N-1-4) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0185] Regarding the content of the compound represented by the general formula (N-1-4), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set lower. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0186] The preferred lower limit of the content of the compound represented by formula (N-1-4) relative to the total amount of the liquid crystal composition is 3%, 5%, 7%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 11%, 10%, and 8%.

[0187] The compound represented by the general formula (N-1-4) is preferably a compound selected from the group of compounds represented by formulas (N-1-4.1) to (N-1-4.24), preferably a compound represented by formulas (N-1-4.1) to (N-1-4.4), and preferably a compound represented by formula (N-1-4.1), formula (N-1-4.2) and formula (N-1-4.4).

[0188] [Chemistry 24]

[0189]

[0190] The compounds represented by formula (N-1-4.1) to (N-1-4.24) can be used alone or in combination, and the preferred lower limits of the content of the compounds alone or in combination relative to the total amount of the liquid crystal composition are 3%, 5%, 7%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limits of the content relative to the total amount of the liquid crystal composition are 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 11%, 10%, and 8%.

[0191] The compounds represented by the general formula (N-1-5) are the following compounds.

[0192] [Chemistry 25]

[0193]

[0194] (Where R N151 and R N152 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0195] R N151 and R N152 Preferably, each independently is an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and preferably is an ethyl group, a propyl group, or a butyl group.

[0196] The compound represented by the general formula (N-1-5) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0197] Regarding the content of the compound represented by the general formula (N-1-5), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set lower. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burn-in characteristics are improved, it is preferred to set the content in the middle range.

[0198] The preferred lower limit of the content of the compound represented by formula (N-1-5) relative to the total amount of the liquid crystal composition is 5%, 8%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 33%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0199] The compound represented by general formula (N-1-5) is preferably a compound selected from the group consisting of compounds represented by formula (N-1-5.1) to formula (N-1-5.12), and preferably a compound represented by formula (N-1-5.1), formula (N-1-5.2) and formula (N-1-5.4).

[0200] [Chemistry 26]

[0201]

[0202] The compounds represented by formula (N-1-5.1), formula (N-1-5.2) and formula (N-1-5.4) can be used alone or in combination. The lower limits of the preferred contents of the compounds alone or in combination relative to the total amount of the liquid crystal composition are 5%, 8%, 10%, 13%, 15%, 17%, and 20%. The upper limits of the preferred contents relative to the total amount of the liquid crystal composition are 35%, 33%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0203] The compounds represented by the general formula (N-1-10) are the following compounds.

[0204] [Chemistry 27]

[0205]

[0206] (Where R N1101 and R N1102 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0207] R N1101 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably an ethyl group, a propyl group, a butyl group, a vinyl group or a 1-propenyl group. N1102 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably an ethoxy group, a propoxy group, or a butoxy group.

[0208] The compound represented by the general formula (N-1-10) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0209] Regarding the content of the compound represented by the general formula (N-1-10), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set lower. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0210] The preferred lower limit of the content of the compound represented by formula (N-1-10) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, or 13%.

[0211] The compound represented by the general formula (N-1-10) is preferably a compound selected from the group consisting of compounds represented by formulae (N-1-10.1) to (N-1-10.14), preferably a compound represented by formulae (N-1-10.1) to (N-1-10.5), and preferably a compound represented by formulae (N-1-10.1) and (N-1-10.2).

[0212] [Chemistry 28]

[0213]

[0214] The compounds represented by formula (N-1-10.1) and formula (N-1-10.2) can be used alone or in combination. The lower limits of the preferred contents of the compounds alone or in combination relative to the total amount of the liquid crystal composition are 5%, 10%, 13%, 15%, 17%, and 20%. The upper limits of the preferred contents relative to the total amount of the liquid crystal composition are 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0215] The compound represented by the general formula (N-1-11) is the following compound.

[0216] [Chemistry 29]

[0217]

[0218] (Where R N1111 and R N1112 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0219] R N1111 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably an ethyl group, a propyl group, a butyl group, a vinyl group or a 1-propenyl group. N1112 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably an ethoxy group, a propoxy group, or a butoxy group.

[0220] The compound represented by the general formula (N-1-11) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0221] Regarding the content of the compound represented by the general formula (N-1-11), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set lower. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burn-in characteristics are improved, it is preferred to set the content in the middle range.

[0222] The preferred lower limit of the content of the compound represented by formula (N-1-11) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0223] The compound represented by the general formula (N-1-11) is preferably a compound selected from the group consisting of compounds represented by formulae (N-1-11.1) to (N-1-11.14), preferably a compound represented by formulae (N-1-11.1) to (N-1-11.14), and preferably a compound represented by formulae (N-1-11.2) and (N-1-11.4).

[0224] [Chemistry 30]

[0225]

[0226] The compounds represented by formula (N-1-11.2) and formula (N-1-11.4) can be used alone or in combination, and the preferred lower limits of the content of the compounds alone or in combination relative to the total amount of the liquid crystal composition are 5%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limits of the content relative to the total amount of the liquid crystal composition are 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0227] The compound represented by the general formula (N-1-12) is the following compound.

[0228] [Chemistry 31]

[0229]

[0230] (Where R N1121 and R N1122 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0231] R N1121 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably an ethyl group, a propyl group or a butyl group. N1122 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably an ethoxy group, a propoxy group, or a butoxy group.

[0232] The compound represented by the general formula (N-1-12) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0233] Regarding the content of the compound represented by the general formula (N-1-12), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set lower. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0234] The preferred lower limit of the content of the compound represented by formula (N-1-12) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, or 13%.

[0235] The compound represented by the general formula (N-1-13) is the following compound.

[0236] [Chemistry 32]

[0237]

[0238] (Where R N1131 and R N1132 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0239] R N1131 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably an ethyl group, a propyl group or a butyl group. N1132 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably an ethoxy group, a propoxy group, or a butoxy group.

[0240] The compound represented by the general formula (N-1-13) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0241] Regarding the content of the compound represented by the general formula (N-1-13), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0242] The preferred lower limit of the content of the compound represented by formula (N-1-13) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0243] The compound represented by the general formula (N-1-14) is the following compound.

[0244] [Chemistry 33]

[0245]

[0246] (Where R N1141 and R N1142 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0247] R N1141 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and is preferably a methyl group, an ethyl group, a propyl group or a butyl group. N1142 It is preferably an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms, and is preferably an ethoxy group, a propoxy group, or a butoxy group.

[0248] The compound represented by the general formula (N-1-14) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0249] Regarding the content of the compound represented by the general formula (N-1-14), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0250] The preferred lower limit of the content of the compound represented by formula (N-1-14) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, or 13%.

[0251] The compound represented by the general formula (N-1-14) is preferably a compound selected from the group of compounds represented by formulas (N-1-14.1) to (N-1-14.5), preferably a compound represented by formulas (N-1-14.1) to (N-1-14.3), and preferably a compound represented by formulas (N-1-14.2) and (N-1-14.3).

[0252] [Chemistry 34]

[0253]

[0254] The compound represented by the general formula (N-1-20) is the following compound.

[0255] [Chemistry 35]

[0256]

[0257] (Where R N1201 and R N1202 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0258] R 1201 and R N1202Preferably, each independently is an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and preferably is an ethyl group, a propyl group or a butyl group.

[0259] The compound represented by the general formula (N-1-20) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0260] Regarding the content of the compound represented by the general formula (N-1-20), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0261] The preferred lower limit of the content of the compound represented by formula (N-1-20) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0262] The compound represented by the general formula (N-1-21) is the following compound.

[0263] [Chemistry 36]

[0264]

[0265] (Where R N1211 and R N1212 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0266] R N1211 and R N1212 Preferably, each independently is an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and preferably is an ethyl group, a propyl group or a butyl group.

[0267] The compound represented by the general formula (N-1-21) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0268] Regarding the content of the compound represented by the general formula (N-1-21), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0269] The preferred lower limit of the content of the compound represented by formula (N-1-21) relative to the total amount of the liquid crystal composition is 5%, 10%, 13%, 15%, 17%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, or 13%.

[0270] The compound represented by the general formula (N-1-22) is the following compound.

[0271] [Chemistry 37]

[0272]

[0273] (Where R N1221 and R N1222 Each independently represents R in the general formula (N-1) N11 and R N12 same meaning).

[0274] R N1221 and R N1222 Preferably, each independently is an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and preferably is an ethyl group, a propyl group or a butyl group.

[0275] The compound represented by the general formula (N-1-22) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0276] Regarding the content of the compound represented by the general formula (N-1-22), when the improvement of Δε is emphasized, it is preferred to set the content higher. When the solubility at low temperature is emphasized, the effect is high if the content is set higher. When Tni is emphasized, the effect is high if the content is set higher. Furthermore, when the dripping mark and screen burning characteristics are improved, it is preferred to set the content in the middle range.

[0277] The preferred lower limit of the content of the compound represented by formula (N-1-22) relative to the total amount of the liquid crystal composition is 1%, 5%, 10%, 13%, 15%, 17%, and 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 35%, 30%, 28%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, and 5%.

[0278] The compound represented by the general formula (N-1-22) is preferably a compound selected from the group consisting of compounds represented by formulae (N-1-22.1) to (N-1-22.12), preferably a compound represented by formulae (N-1-22.1) to (N-1-22.5), and preferably a compound represented by formulae (N-1-22.1) to (N-1-22.4).

[0279] [Chemistry 38]

[0280]

[0281] The liquid crystal composition preferably contains one or more compounds represented by the general formula (L). The compound represented by the general formula (L) is equivalent to a compound with a substantially neutral dielectric property (the value of Δε is -2 to 2). Therefore, it is preferred that the number of polar groups such as halogen contained in the molecule is set to 2 or less, preferably to 1 or less, and preferably not to have.

[0282] [Chemistry 39]

[0283]

[0284] (Where R L1 and R L2 Each independently represents an alkyl group having 1 to 8 carbon atoms, and one or two or more non-adjacent -CH2- groups in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-.

[0285] n L1 represents 0, 1, 2 or 3,

[0286] A L1 , A L2 and AL3 Each independently represents a group selected from the group consisting of the following (a), (b), and (c):

[0287] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0288] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted by -N=), and

[0289] (c) naphthalene-2,6-diyl, 1,2,3,4-tetrahydronaphthalene-2,6-diyl or decahydronaphthalene-2,6-diyl (one -CH= or two or more non-adjacent -CH= groups in naphthalene-2,6-diyl or 1,2,3,4-tetrahydronaphthalene-2,6-diyl may be substituted with -N=),

[0290] The above-mentioned groups (a), (b) and (c) may be substituted by cyano groups, fluorine atoms or chlorine atoms, respectively and independently.

[0291] Z L1 and Z L2 Each independently represents a single bond, -CH2CH2-, -(CH2)4-, -OCH2-, -CH2O-, -COO-, -OCO-, -OCF2-, -CF2O-, -CH=N-N=CH-, -CH=CH-, -CF=CF- or -C≡C-,

[0292] When n L1 There are multiple A's for 2 or 3 L2 In the case of L1 There are multiple Zs for 2 or 3 L2 In the case of, they may be the same or different. However, it does not include compounds represented by general formula (N-1), (N-2) and (N-3))

[0293] The compound represented by the general formula (L) can be used alone or in combination. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to desired properties such as solubility at low temperatures, transition temperature, electrical reliability, and birefringence. The types of compounds used, for example, are 1 as one embodiment of the present invention. Or in other embodiments of the present invention, there are 2, 3, 4, 5, 6, 7, 8, 9, or 10 or more.

[0294] In the liquid crystal composition, the content of the compound represented by the general formula (L) must be appropriately adjusted according to the required properties such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, process adaptability, drip marks, screen burn-in, and dielectric anisotropy.

[0295] Relative to the total amount of the liquid crystal composition, the preferred lower limit of the content of the compound represented by formula (L) is 1%, 10%, 20%, 30%, 40%, 50%, 55%, 60%, 65%, 70%, 75%, 80%. The preferred upper limit of the content is 95%, 85%, 75%, 65%, 55%, 45%, 35%, 25%.

[0296] When the viscosity of liquid crystal composition is kept low, the situation of the composition with fast response speed is needed, the lower limit of the content of the compound represented by formula (L) is preferably high and the upper limit is high.When the Tni of liquid crystal composition is kept high, the situation of the composition with good temperature stability is needed, the lower limit of the content of the compound represented by formula (L) is preferably high and the upper limit is high.In order to keep the driving voltage low and want to increase dielectric anisotropy, it is preferably to reduce the lower limit of the content of the compound represented by formula (L), and the upper limit is low.

[0297] In the above general formula (L), when reliability is important, R L1 and R L2 All of them are alkyl groups. When emphasis is placed on reducing the volatility of the compound, an alkoxy group is preferred. When emphasis is placed on reducing the viscosity, at least one of them is preferably an alkenyl group.

[0298] In the above general formula (L), the number of halogen atoms present in the molecule is preferably 0, 1, 2 or 3, preferably 0 or 1, and preferably 1 when the compatibility with other liquid crystal molecules is emphasized.

[0299] In the above general formula (L), R L1 and R L2 , when the ring structure to which it is bonded is a phenyl (aromatic) group, it is preferably a linear alkyl group having 1 to 5 carbon atoms, a linear alkoxy group having 1 to 4 carbon atoms, or an alkenyl group having 4 to 5 carbon atoms. L1 and R L2 When the ring structure to which it is bonded is a saturated ring structure such as cyclohexane, pyran and dioxane, it is preferably a linear alkyl group having 1 to 5 carbon atoms, a linear alkoxy group having 1 to 4 carbon atoms and a linear alkenyl group having 2 to 5 carbon atoms. In order to stabilize the nematic phase, R L1 and R L2 The total number of carbon atoms and oxygen atoms, when present, is preferably 5 or less, and the group is preferably in a linear chain.

[0300] The alkenyl group is preferably a group represented by any one selected from the group consisting of Formula (R1) to Formula (R5) (the black dots in each formula represent carbon atoms in the ring structure).

[0301] [Chemistry 40]

[0302]

[0303] In the above general formula (L), when emphasis is placed on response speed, n L1 It is preferably 0, and in order to improve the upper limit temperature of the nematic phase, it is preferably 2 or 3, and in order to achieve a balance between these, it is preferably 1. In addition, in order to satisfy the characteristics required as a composition, it is preferred to set n L1 for different combinations of compounds.

[0304] In the above general formula (L), when it is required to increase Δn, A L1 , A L2 and A L3 Preferably, it is aromatic, and preferably, it is aliphatic in order to improve the response speed. L1 , A L2 and A L3 Each independently represents trans-1,4-cyclohexylene, 1,4-phenylene, 2-fluoro-1,4-phenylene, 3-fluoro-1,4-phenylene, 3,5-difluoro-1,4-phenylene, 1,4-cyclohexenylene, 1,4-bicyclo[2.2.2]octylene, piperidine-1,4-diyl, naphthalene-2,6-diyl, decahydronaphthalene-2,6-diyl or 1,2,3,4-tetrahydronaphthalene-2,6-diyl, and more preferably represents the following structure,

[0305] [Chemistry 41]

[0306]

[0307] Particularly preferably, it represents a trans-1,4-cyclohexylene group or a 1,4-phenylene group.

[0308] In the above general formula (L), when the response speed is important, Z L1 and Z L2 Preferred is a single bond.

[0309] The compound represented by the general formula (L) preferably has 0 or 1 halogen atom in the molecule.

[0310] The compound represented by the general formula (L) is preferably a compound selected from the group consisting of compounds represented by general formulae (L-1) to (L-7).

[0311] The compound represented by the general formula (L-1) is the following compound.

[0312] [Chemistry 42]

[0313]

[0314] (Where R L11 and R L12 Each independently represents R in the general formula (L) L1 and R L2 same meaning).

[0315] R L11 and R L12 Preferred are linear alkyl groups having 1 to 5 carbon atoms, linear alkoxy groups having 1 to 4 carbon atoms, and linear alkenyl groups having 2 to 5 carbon atoms.

[0316] The compound represented by the general formula (L-1) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0317] The preferred lower limit of the content of the compound represented by the general formula (L-1) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, 45%, 50%, and 55%. In addition, the preferred upper limit of the content of the compound represented by the general formula (L-1) relative to the total amount of the liquid crystal composition is 95%, 90%, 85%, 80%, 75%, 70%, 65%, 60%, 55%, 50%, 45%, 40%, 35%, 30%, and 25%.

[0318] When the viscosity of the liquid crystal composition is kept low and a composition with a fast response speed is required, it is preferred that the lower limit of the content of the compound represented by the general formula (L-1) is high and the upper limit is high. When the Tni of the liquid crystal composition is kept high and a composition with good temperature stability is required, it is preferred that the lower limit of the content of the compound represented by the general formula (L-1) is moderate and the upper limit is moderate. In addition, in order to keep the driving voltage low and increase the dielectric anisotropy, it is preferred that the lower limit of the content of the compound represented by the general formula (L-1) is low and the upper limit is low.

[0319] The compound represented by the general formula (L-1) is preferably a compound selected from the group consisting of compounds represented by the general formula (L-1-1).

[0320] [Chemistry 43]

[0321]

[0322] (Where R L12 has the same meaning as in the general formula (L-1).

[0323] The compound represented by general formula (L-1-1) is preferably a compound selected from the group consisting of compounds represented by formulae (L-1-1.1) to (L-1-1.3), preferably a compound represented by formula (L-1-1.2) and / or formula (L-1-1.3), and particularly preferably a compound represented by formula (L-1-1.3).

[0324] [Chemistry 44]

[0325]

[0326] The preferred lower limit of the content of the compound represented by formula (L-1-1.3) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, or 10%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 20%, 15%, 13%, 10%, 8%, 7%, 6%, 5%, or 3%.

[0327] The compound represented by the general formula (L-1) is preferably a compound selected from the group consisting of compounds represented by the general formula (L-1-2).

[0328] [Chemistry 45]

[0329]

[0330] (Where R L12 has the same meaning as in the general formula (L-1).

[0331] The lower limit of the content of the compound represented by formula (L-1-2) relative to the total amount of the liquid crystal composition is preferably 1%, 5%, 10%, 15%, 17%, 20%, 23%, 25%, 27%, 30%, and 35%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 60%, 55%, 50%, 45%, 42%, 40%, 38%, 35%, 33%, and 30%.

[0332] The compound represented by the general formula (L-1-2) is preferably a compound selected from the group of compounds represented by formula (L-1-2.1) to formula (L-1-2.4), and preferably a compound represented by formula (L-1-2.2) to formula (L-1-2.4). In particular, the compound represented by formula (L-1-2.2) is preferred because it particularly improves the response speed of the liquid crystal composition. In addition, when a higher Tni is required than the response speed, it is preferred to use a compound represented by formula (L-1-2.3) and / or formula (L-1-2.4). The content of the compound represented by formula (L-1-2.3) and formula (L-1-2.4) is not preferably set to more than 30% in order to make the solubility at low temperatures good.

[0333] [Chemistry 46]

[0334]

[0335] The lower limit of the content of the compound represented by formula (L-1-2.2) relative to the total amount of the liquid crystal composition is preferably 10%, 15%, 18%, 20%, 23%, 25%, 27%, 30%, 33%, 35%, 38%, and 40%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 60%, 55%, 50%, 45%, 43%, 40%, 38%, 35%, 32%, 30%, 27%, 25%, and 22%.

[0336] The lower limit of the preferred total content of the compound represented by formula (L-1-1.3) and the compound represented by formula (L-1-2.2) relative to the total amount of the liquid crystal composition is 10%, 15%, 20%, 25%, 27%, 30%, 35%, and 40%. The upper limit of the preferred content relative to the total amount of the liquid crystal composition is 60%, 55%, 50%, 45%, 43%, 40%, 38%, 35%, 32%, 30%, 27%, 25%, and 22%.

[0337] The compound represented by the general formula (L-1) is preferably a compound selected from the group consisting of compounds represented by the general formula (L-1-3).

[0338] [Chemistry 47]

[0339]

[0340] (Where R L13 and R L14 Each independently represents an alkyl group having 1 to 8 carbon atoms or an alkoxy group having 1 to 8 carbon atoms).

[0341] R L13 and RL14 Preferred are linear alkyl groups having 1 to 5 carbon atoms, linear alkoxy groups having 1 to 4 carbon atoms, and linear alkenyl groups having 2 to 5 carbon atoms.

[0342] The lower limit of the content of the compound represented by formula (L-1-3) relative to the total amount of the liquid crystal composition is preferably 1%, 5%, 10%, 13%, 15%, 17%, 20%, 23%, 25%, or 30%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 60%, 55%, 50%, 45%, 40%, 37%, 35%, 33%, 30%, 27%, 25%, 23%, 20%, 17%, 15%, 13%, or 10%.

[0343] The compound represented by the general formula (L-1-3) is preferably a compound selected from the group of compounds represented by formulas (L-1-3.1) to (L-1-3.13), preferably a compound represented by formula (L-1-3.1), formula (L-1-3.3) and / or formula (L-1-3.4), and preferably a compound represented by formula (L-1-3.1) and / or formula (L-1-3.3). In particular, the compound represented by formula (L-1-3.1) is preferred because it particularly improves the response speed of the liquid crystal composition. In addition, when a higher Tni is required than the response speed, it is preferred to use compounds represented by formulas (L-1-3.3), formula (L-1-3.4), formula (L-1-3.11) and formula (L-1-3.12). The total content of the compounds represented by Formula (L-1-3.3), Formula (L-1-3.4), Formula (L-1-3.11) and Formula (L-1-3.13) is not preferably 20% or more in order to improve solubility at low temperatures.

[0344] [Chemistry 48]

[0345]

[0346] The lower limit of the content of the compound represented by formula (L-1-3.1) relative to the total amount of the liquid crystal composition is preferably 1%, 2%, 3%, 5%, 7%, 10%, 13%, 15%, 18%, or 20%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 20%, 17%, 15%, 13%, 10%, 8%, 7%, or 6%.

[0347] The compound represented by the general formula (L-1) is preferably a compound selected from the group consisting of compounds represented by the general formula (L-1-4) and / or (L-1-5).

[0348] [Chemistry 49]

[0349]

[0350] (Where R L15 and R L16 Each independently represents an alkyl group having 1 to 8 carbon atoms or an alkoxy group having 1 to 8 carbon atoms).

[0351] R L15 and R L16 Preferred are linear alkyl groups having 1 to 5 carbon atoms, linear alkoxy groups having 1 to 4 carbon atoms, and linear alkenyl groups having 2 to 5 carbon atoms.

[0352] The preferred lower limit of the content of the compound represented by formula (L-1-4) relative to the total amount of the liquid crystal composition is 1%, 5%, 10%, 13%, 15%, 17%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 25%, 23%, 20%, 17%, 15%, 13%, or 10%.

[0353] The preferred lower limit of the content of the compound represented by formula (L-1-5) relative to the total amount of the liquid crystal composition is 1%, 5%, 10%, 13%, 15%, 17%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 25%, 23%, 20%, 17%, 15%, 13%, or 10%.

[0354] The compounds represented by general formulae (L-1-4) and (L-1-5) are preferably compounds selected from the group consisting of compounds represented by formulae (L-1-4.1) to (L-1-5.3), and are preferably compounds represented by formula (L-1-4.2) and / or formula (L-1-5.2).

[0355] [Chemistry 50]

[0356]

[0357] The preferred lower limit of the content of the compound represented by formula (L-1-4.2) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, 10%, 13%, 15%, 18%, or 20%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 20%, 17%, 15%, 13%, 10%, 8%, 7%, or 6%.

[0358] It is preferred to combine two or more compounds selected from the group consisting of compounds represented by formula (L-1-1.3), formula (L-1-2.2), formula (L-1-3.1), formula (L-1-3.3), formula (L-1-3.4), formula (L-1-3.11) and formula (L-1-3.12), and it is preferred to combine two or more compounds selected from the group consisting of compounds represented by formula (L-1-1.3), formula (L-1-2.2), formula (L-1-3.1), formula (L-1-3.3), formula (L-1-3.4) and formula (L-1-4.2). The preferred lower limit of the total content of these compounds, relative to the total amount of the liquid crystal composition, is 1%, 2%, 3%, 5%, 7%, 10%, 13%, 15%, 18%, 20%, 23%, 25%, 27%, 30%, 33%, and 35%, and the upper limit, relative to the total amount of the liquid crystal composition, is 80%, 70%, 60%, 50%, 45%, 40%, 37%, 35%, 33%, 30%, 28%, 25%, 23%, and 20%.

[0359] In addition, when emphasis is placed on the reliability of the composition, it is preferred to combine two or more compounds selected from the compounds represented by formula (L-1-3.1), formula (L-1-3.3) and formula (L-1-3.4), and when emphasis is placed on the response speed of the composition, it is preferred to combine two or more compounds selected from the compounds represented by formula (L-1-1.3) and formula (L-1-2.2).

[0360] The compound represented by the general formula (L-1) is preferably a compound selected from the group consisting of compounds represented by the general formula (L-1-6).

[0361] [Chemistry 51]

[0362]

[0363] (Where R L17 and R L18 each independently represents a methyl group or a hydrogen atom).

[0364] The lower limit of the content of the compound represented by formula (L-1-6) relative to the total amount of the liquid crystal composition is preferably 1%, 5%, 10%, 15%, 17%, 20%, 23%, 25%, 27%, 30%, and 35%. The upper limit of the content relative to the total amount of the liquid crystal composition is preferably 60%, 55%, 50%, 45%, 42%, 40%, 38%, 35%, 33%, and 30%.

[0365] The compound represented by the general formula (L-1-6) is preferably a compound selected from the group consisting of compounds represented by formula (L-1-6.1) to formula (L-1-6.3).

[0366] [Chemistry 52]

[0367]

[0368] The compound represented by the general formula (L-2) is the following compound.

[0369] [Chemistry 53]

[0370]

[0371] (Where R L21 and R L22 Each independently represents R in the general formula (L) L1 and R L2 same meaning).

[0372] R L21 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and R L22 An alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms is preferred.

[0373] The compound represented by the general formula (L-2) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0374] Regarding the content of the compound represented by the general formula (L-2), when the solubility at low temperature is emphasized, if the content is set higher, the effect is high. On the contrary, when the response speed is emphasized, if the content is set lower, the effect is high. Furthermore, when improving drip marks and screen burn-in characteristics, it is preferable to set the content in the middle range.

[0375] The preferred lower limit of the content of the compound represented by formula (L-2) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, or 10%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 20%, 15%, 13%, 10%, 8%, 7%, 6%, 5%, or 3%.

[0376] The compound represented by general formula (L-2) is preferably a compound selected from the group consisting of compounds represented by formula (L-2.1) to formula (L-2.6), and preferably a compound represented by formula (L-2.1), formula (L-2.3), formula (L-2.4) and formula (L-2.6).

[0377] [Chemistry 54]

[0378]

[0379] The compound represented by the general formula (L-3) is the following compound.

[0380] [Chemistry 55]

[0381]

[0382] (Where R L31 and R L32 Each independently represents R in the general formula (L) L1 and R L2 same meaning).

[0383] R L31 and R L32 Preferably, each of them is independently an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms.

[0384] The compound represented by the general formula (L-3) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0385] The preferred lower limit of the content of the compound represented by formula (L-3) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, or 10%. The preferred upper limit of the content relative to the total amount of the liquid crystal composition is 20%, 15%, 13%, 10%, 8%, 7%, 6%, 5%, or 3%.

[0386] Regarding the content of the compound represented by the general formula (L-3), when a high birefringence is obtained, the effect is high if the content is set higher, and conversely, when a high Tni is emphasized, the effect is high if the content is set lower. Furthermore, when drip marks and screen burn-in characteristics are improved, it is preferred to set the content in the middle range.

[0387] The compound represented by the general formula (L-3) is preferably a compound selected from the group consisting of compounds represented by formula (L-3.1) to formula (L-3.7), and preferably a compound represented by formula (L-3.2) to formula (L-3.5).

[0388] [Chemistry 56]

[0389]

[0390] The compound represented by the general formula (L-4) is the following compound.

[0391] [Chemistry 57]

[0392]

[0393] (Where R L41 and R L42 Each independently represents R in the general formula (L) L1 and R L2 same meaning).

[0394] R L41 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and R L42 An alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms is preferred.

[0395] The compound represented by the general formula (L-4) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0396] In the liquid crystal composition, the content of the compound represented by the general formula (L-4) must be appropriately adjusted according to the required properties such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, process adaptability, drip marks, screen burn-in, and dielectric anisotropy.

[0397] Relative to the total amount of the liquid crystal composition, the preferred lower limit of the content of the compound represented by formula (L-4) is 1%, 2%, 3%, 5%, 7%, 10%, 14%, 16%, 20%, 23%, 26%, 30%, 35%, and 40%. Relative to the total amount of the liquid crystal composition, the preferred upper limit of the content of the compound represented by formula (L-4) is 50%, 40%, 35%, 30%, 20%, 15%, 10%, and 5%.

[0398] The compound represented by the general formula (L-4) is preferably a compound represented by the formula (L-4.1) to the formula (L-4.3), for example.

[0399] [Chemistry 58]

[0400]

[0401] The liquid crystal composition may contain the compound represented by formula (L-4.1), the compound represented by formula (L-4.2), both the compound represented by formula (L-4.1) and the compound represented by formula (L-4.2), or all the compounds represented by formula (L-4.1) to formula (L-4.3), depending on the required performance such as solubility at low temperature, transition temperature, electrical reliability, and birefringence. The preferred lower limit of the content of the compound represented by formula (L-4.1) or formula (L-4.2) relative to the total amount of the liquid crystal composition is 3%, 5%, 7%, 9%, 11%, 12%, 13%, 18%, and 21%, and the preferred upper limit is 45%, 40%, 35%, 30%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, and 8%.

[0402] When containing both the compound represented by formula (L-4.1) and the compound represented by formula (L-4.2), the preferred lower limit of the content of the two compounds relative to the total amount of the liquid crystal composition is 15%, 19%, 24%, and 30%, and the preferred upper limit is 45%, 40%, 35%, 30%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0403] The compound represented by the general formula (L-4) is preferably a compound represented by, for example, the formula (L-4.4) to the formula (L-4.6), and is preferably a compound represented by the formula (L-4.4).

[0404] [Chemistry 59]

[0405]

[0406] Depending on the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc., the liquid crystal composition may contain a compound represented by formula (L-4.4), a compound represented by formula (L-4.5), or both a compound represented by formula (L-4.4) and a compound represented by formula (L-4.5).

[0407] The preferred lower limit of the content of the compound represented by formula (L-4.4) or formula (L-4.5) relative to the total amount of the liquid crystal composition is 3%, 5%, 7%, 9%, 11%, 12%, 13%, 18%, and 21%. The preferred upper limit is 45%, 40%, 35%, 30%, 25%, 23%, 20%, 18%, 15%, 13%, 10%, and 8%.

[0408] In the case of containing both the compound represented by formula (L-4.4) and the compound represented by formula (L-4.5), the preferred lower limit of the content of the two compounds relative to the total amount of the liquid crystal composition is 15%, 19%, 24%, and 30%, and the preferred upper limits are 45%, 40%, 35%, 30%, 25%, 23%, 20%, 18%, 15%, and 13%.

[0409] The compound represented by the general formula (L-4) is preferably a compound represented by formula (L-4.7) to formula (L-4.10), and particularly preferably a compound represented by formula (L-4.9).

[0410] [Chemistry 60]

[0411]

[0412] The compound represented by the general formula (L-5) is the following compound.

[0413] [Chemistry 61]

[0414]

[0415] (Where R L51 and R L52 Each independently represents R in the general formula (L) L1 and R L2 same meaning).

[0416] R L51 It is preferably an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and R L52 An alkyl group having 1 to 5 carbon atoms, an alkenyl group having 4 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms is preferred.

[0417] The compound represented by the general formula (L-5) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0418] In the liquid crystal composition, the content of the compound represented by the general formula (L-5) must be appropriately adjusted according to the required properties such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, process adaptability, drip marks, screen burn-in, and dielectric anisotropy.

[0419] Relative to the total amount of the liquid crystal composition, the preferred lower limit of the content of the compound represented by formula (L-5) is 1%, 2%, 3%, 5%, 7%, 10%, 14%, 16%, 20%, 23%, 26%, 30%, 35%, and 40%. Relative to the total amount of the liquid crystal composition, the preferred upper limit of the content of the compound represented by formula (L-5) is 50%, 40%, 35%, 30%, 20%, 15%, 10%, and 5%.

[0420] The compound represented by the general formula (L-5) is preferably a compound represented by the formula (L-5.1) and / or the formula (L-5.2), and is particularly preferably a compound represented by the formula (L-5.1). The preferred lower limits of the content of these compounds relative to the total amount of the liquid crystal composition are 1%, 2%, 3%, 5%, and 7%. The preferred upper limits of the content of these compounds are 20%, 15%, 13%, 10%, and 9%.

[0421] [Chemistry 62]

[0422]

[0423] The compound represented by the general formula (L-5) is preferably a compound represented by the formula (L-5.3) and / or the formula (L-5.4). The lower limit of the preferred content of these compounds relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, and 7%. The upper limit of the preferred content of these compounds is 20%, 15%, 13%, 10%, and 9%.

[0424] [Chemistry 63]

[0425]

[0426] The compound represented by the general formula (L-5) is preferably a compound selected from the group of compounds represented by formulas (L-5.5) to (L-5.7), and is particularly preferably a compound represented by formula (L-5.7). The preferred lower limit of the content of these compounds relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, and 7%. The preferred upper limit of the content of these compounds is 20%, 15%, 13%, 10%, and 9%.

[0427] [Chemistry 64]

[0428]

[0429] The compound represented by the general formula (L-6) is the following compound.

[0430] [Chemistry 65]

[0431]

[0432] (Where R L61 and R L62 Each independently represents R in the general formula (L) L1 and R L2 Same meaning, X L61 and X L62 each independently represents a hydrogen atom or a fluorine atom).

[0433] R L61 and R L62 Preferably, each independently represents an alkyl group having 1 to 5 carbon atoms or an alkenyl group having 2 to 5 carbon atoms, and X L61 and X L62 One of them is a fluorine atom and the other is a hydrogen atom.

[0434] The compound represented by the general formula (L-6) can be used alone or in combination of two or more compounds. The types of the compounds that can be combined are not particularly limited, and can be used in appropriate combinations according to the required performance such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, as one embodiment of the present invention, are 1, 2, 3, 4, 5 or more.

[0435] The lower limit of the preferred content of the compound represented by formula (L-6) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, 10%, 14%, 16%, 20%, 23%, 26%, 30%, 35%, and 40%. The upper limit of the preferred content of the compound represented by formula (L-6) relative to the total amount of the liquid crystal composition is 50%, 40%, 35%, 30%, 20%, 15%, 10%, and 5%. When the focus is on increasing Δn, it is preferred to increase the content, and when the focus is on precipitation at low temperature, it is preferred to have a smaller content.

[0436] The compound represented by the general formula (L-6) is preferably a compound represented by formula (L-6.1) to formula (L-6.9).

[0437] [Chemistry 66]

[0438]

[0439] The types of compounds that can be combined are not particularly limited, but preferably contain 1 to 3 of these compounds, and more preferably contain 1 to 4. In addition, since the molecular weight distribution of the selected compound is wide and also effective for solubility, it is preferred to select, for example, 1 compound represented by formula (L-6.1) and (L-6.2), 1 compound represented by formula (L-6.4) and (L-6.5), 1 compound represented by formula (L-6.6) and (L-6.7), 1 compound represented by formula (L-6.8) and (L-6.9), and appropriately combine these. Among them, it is preferred to contain compounds represented by formula (L-6.1), formula (L-6.3), formula (L-6.4), formula (L-6.6) and formula (L-6.9).

[0440] The compound represented by the general formula (L-6) is preferably, for example, a compound represented by the formula (L-6.10) to the formula (L-6.17), and among them, a compound represented by the formula (L-6.11) is preferred.

[0441] [Chemistry 67]

[0442]

[0443] The preferred lower limits of the content of these compounds relative to the total amount of the liquid crystal composition are 1%, 2%, 3%, 5%, and 7%. The preferred upper limits of the content of these compounds are 20%, 15%, 13%, 10%, and 9%.

[0444] The compound represented by the general formula (L-7) is the following compound.

[0445] [Chemistry 68]

[0446]

[0447] (Where R L71 and R L72 Each independently represents R in the general formula (L) L1 and R L2 The same meaning, A L71 and A L72 Each independently represents A in the general formula (L) L2 and A L3 The same meaning, A L71 and A L72 The hydrogen atoms on Z can also be replaced by fluorine atoms independently. L71 It represents the same as Z in the general formula (L) L2 Same meaning, X L71 and X L72 each independently represents a fluorine atom or a hydrogen atom).

[0448] In the formula, R L71 and R L72 Preferably, each of A and A is independently an alkyl group having 1 to 5 carbon atoms, an alkenyl group having 2 to 5 carbon atoms, or an alkoxy group having 1 to 4 carbon atoms. L71 and A L72 Preferably, each independently is 1,4-cyclohexylene or 1,4-phenylene, and A L71 and A L72 The hydrogen atoms on Z can also be replaced by fluorine atoms independently. L71 Preferably it is a single bond or -COO-, preferably a single bond, X L71 and X L72 Preferred is a hydrogen atom.

[0449] The types of compounds that can be combined are not particularly limited, and can be combined according to the required performance such as solubility at low temperature, transition temperature, electrical reliability, birefringence, etc. The types of compounds used, for example, are 1, 2, 3, or 4 as one embodiment of the present invention.

[0450] In the liquid crystal composition, the content of the compound represented by the general formula (L-7) must be appropriately adjusted according to the required properties such as solubility at low temperatures, transition temperature, electrical reliability, birefringence, process adaptability, drip marks, screen burn-in, and dielectric anisotropy.

[0451] The preferred lower limit of the content of the compound represented by formula (L-7) relative to the total amount of the liquid crystal composition is 1%, 2%, 3%, 5%, 7%, 10%, 14%, 16%, and 20%. The preferred upper limit of the content of the compound represented by formula (L-7) relative to the total amount of the liquid crystal composition is 30%, 25%, 23%, 20%, 18%, 15%, 10%, and 5%.

[0452] When a liquid crystal composition having a high Tni is desired, the content of the compound represented by formula (L-7) is preferably increased, and when a liquid crystal composition having a low viscosity is desired, the content is preferably decreased.

[0453] The compound represented by the general formula (L-7) is preferably a compound represented by formula (L-7.1) to formula (L-7.4), and preferably a compound represented by formula (L-7.2).

[0454] [Chemistry 69]

[0455]

[0456] The compound represented by the general formula (L-7) is preferably a compound represented by formula (L-7.11) to formula (L-7.13), and is preferably a compound represented by formula (L-7.11).

[0457] [Chemistry 70]

[0458]

[0459] The compound represented by the general formula (L-7) is a compound represented by formula (L-7.21) to formula (L-7.23), and preferably a compound represented by formula (L-7.21).

[0460] [Chemistry 71]

[0461]

[0462] The compound represented by the general formula (L-7) is preferably a compound represented by formula (L-7.31) to formula (L-7.34), and preferably a compound represented by formula (L-7.31) and / or formula (L-7.32).

[0463] [Chemistry 72]

[0464]

[0465] The compound represented by general formula (L-7) is preferably a compound represented by formula (L-7.41) to formula (L-7.44), and preferably a compound represented by formula (L-7.41) and / or formula (L-7.42).

[0466] [Chemistry 73]

[0467]

[0468] The compound represented by the general formula (L-7) is preferably a compound represented by formula (L-7.51) to formula (L-7.53).

[0469] [Chemistry 74]

[0470]

[0471] (Other compounds)

[0472] Although the polymerizable compound-containing liquid crystal composition of the present invention undergoes polymerization even in the absence of a polymerization initiator, a polymerization initiator may be contained to promote polymerization. Examples of the polymerization initiator include benzoin ethers, diphenyl ketones, acetophenones, benzyl ketals, acyl phosphine oxides, and the like.

[0473] The polymerizable compound-containing liquid crystal composition of the present invention contains a polymerizable compound represented by general formula (i), but may also contain other polymerizable compounds. Examples of such other polymerizable compounds include compounds represented by the following general formula (P).

[0474] [Chemistry 75]

[0475]

[0476] (In the above general formula (P), R p1 represents a hydrogen atom, a fluorine atom, a cyano group, an alkyl group having 1 to 15 carbon atoms, or -Sp p2 -P p2 , one or more non-adjacent -CH2- in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-, and one or more hydrogen atoms in the alkyl group may be independently substituted by cyano, fluorine or chlorine atoms,

[0477] P p1 and P p2 Each independently represents the general formula (P p1 -1)~Formula (P p1 -9) any one of the following,

[0478] [Chemistry 76]

[0479]

[0480] (Where R p11 and R p12 Each independently represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms, and W p11 represents a single bond, -O-, -COO- or methylene, t p11 Represents 0, 1 or 2, and there are multiple R in the molecule p11 , R p12 , W p11 and / or p11 In the case of

[0481] Sp p1 and Sp p2 Each independently represents a single bond or a spacer,

[0482] Z p1 and Z p2 Each independently represents a single bond, -O-, -S-, -CH2-, -OCH2-, -CH2O-, -CO-, -C2H4-, -COO-, -OCO-, -OCOOCH2-, -CH2OCOO-, -OCH2CH2O-, -CO-NRZP1 -, -NR ZP1 -CO-, -SCH2-, -CH2S-, -CH=CR ZP1 -COO-, -CH=CR ZP1 -OCO-, -COO-CR ZP1 =CH-, -OCO-CR ZP1 =CH-, -COO-CR ZP1 =CH-COO-, -COO-CR ZP1 =CH-OCO-, -OCO-CR ZP1 =CH-COO-, -OCO-CR ZP1 =CH-OCO-, -(CH2)2-COO-, -(CH2)2-OCO-, -OCO-(CH2)2-, -(C=O)-O-(CH2)2-, -CH=CH-, -CF= CF-, -CF=CH-, -CH=CF-, -CF2-, -CF2O-, -OCF2-, -CF2CH2-, -CH2CF2-, -CF2CF2- or -C≡C- (where, R ZP1 Each independently represents a hydrogen atom or an alkyl group having 1 to 4 carbon atoms, and a plurality of R ZP1 In the case of

[0483] A p1 , A p2 and A p3 Each independently represents a member selected from the following (a p )~(c p ),

[0484] (a p )1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0485] (b p ) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= in the group may be substituted by -N=), and

[0486] (c p ) naphthalene-2,6-diyl, 1,2,3,4-tetrahydronaphthalene-2,6-diyl, decahydronaphthalene-2,6-diyl, phenanthrene-2,7-diyl or anthracene-2,6-diyl (one -CH= or two or more non-adjacent -CH= in these groups may be substituted by -N=),

[0487] The above base (a p ), base (b p ) and base (c p) may be replaced by a halogen atom, a cyano group, an alkyl group having 1 to 8 carbon atoms, or -Sp p2 -P p2 One or two or more non-adjacent -CH2- in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-.

[0488] m p1 Represents 0, 1, 2 or 3, there are multiple Z in the molecule p1 , A p2 、Sp p2 and / or P p2 In the case of m, they can be the same or different. p1 is 0 and A p1 In the case of phenanthrene-2,7-diyl or anthracene-2,6-diyl, A p3 represents a single bond. However, compounds represented by general formula (i) are not included).

[0489] It is preferred that the compound represented by the above general formula (P) is contained at least one kind or two kinds.

[0490] In the above general formula (P), R p1 Preferably -Sp p2 -P p2 .

[0491] P p1 and P p2 Preferably, they are independently of each other and are of the formula (P p1 -1)~Formula (P p1 -3), preferably (P p1 -1).

[0492] R p11 and R p12 Preferably, they are each independently a hydrogen atom or a methyl group.

[0493] t p11 Preferably 0 or 1.

[0494] W p11 Preferred is a single bond, a methylene group or an ethylene group.

[0495] m p1 Preferably it is 0, 1 or 2, preferably 0 or 1.

[0496] Z p1 and Z p2Preferably, each independently represents a single bond, -OCH2-, -CH2O-, -CO-, -C2H4-, -COO-, -OCO-, -COOC2H4-, -OCOC2H4-, -C2H4OCO-, -C2H4COO-, -CH=CH-, -CF2-, -CF2O-, -(CH2)2-COO-, -(CH2)2-OCO-, -OCO-(CH2)2-, -CH=CH-COO-, -C OO-CH=CH-, -OCOCH=CH-, -COO-(CH2)2-, -OCF2- or -C≡C-, preferably a single bond, -OCH2-, -CH2O-, -C2H4-, -COO-, -OCO-, -COOC2H4-, -OCOC2H4-, -C2H4OCO-, -C2H4COO-, -CH=CH-, -(CH2)2-COO-, -(CH2)2-OCO-, -OCO- (CH2)2-, -CH=CH-COO-, -COO-CH=CH-, -OCOCH=CH-, -COO-(CH2)2- or -C≡C-, preferably only one of -OCH2-, -CH2O-, -C2H4-, -COO-, -OCO-, -COOC2H4-, -OCOC2H4-, -C2H4OCO-, -C2H4COO-, -CH=CH-, -(CH2)2- 2-COO-, -(CH2)2-OCO-, -OCO-(CH2)2-, -CH=CH-COO-, -COO-CH=CH-, -OCOCH=CH-, -COO-(CH2)2- or -C≡C-, and all the others are single bonds. Preferably, only one -OCH2-, -CH2O-, -C2H4-, -COO- or -OCO- exists in the molecule, and all the others are single bonds. Preferably, all are single bonds.

[0497] In addition, Z present in the molecule is preferably p1 and Z p2 Only one of them is a linking group selected from the group consisting of -CH=CH-COO-, -COO-CH=CH-, -(CH2)2-COO-, -(CH2)2-OCO-, -O-CO-(CH2)2-, and -COO-(CH2)2-, and the others are single bonds.

[0498] Sp p1 and Sp p2Each independently represents a single bond or a spacer, the spacer is preferably an alkylene group having 1 to 30 carbon atoms, the -CH2- in the alkylene group may be substituted by -O-, -CO-, -COO-, -OCO-, -CH=CH- or -C≡C- as long as the oxygen atoms are not directly connected to each other, the hydrogen atoms in the alkylene group may be substituted by halogen atoms, and is preferably a straight-chain alkylene group having 1 to 10 carbon atoms or a single bond.

[0499] A p1 , A p2 and A p3 Preferably, each is independently 1,4-phenylene or 1,4-cyclohexylene, and 1,4-phenylene is preferred. In order to improve compatibility with liquid crystal compounds, 1,4-phenylene is preferably substituted with one fluorine atom, one methyl group or one methoxy group.

[0500] The total content of the compounds represented by the general formula (P) is preferably in the range of 0.05 to 10%, preferably in the range of 0.1 to 8%, preferably in the range of 0.1 to 5%, preferably in the range of 0.1 to 3%, preferably in the range of 0.2 to 2%, preferably in the range of 0.2 to 1.3%, preferably in the range of 0.2 to 1%, and preferably in the range of 0.2 to 0.56%, relative to the total amount of the liquid crystal composition containing the polymerizable compound of the present invention containing the compounds represented by the general formula (P).

[0501] The preferred lower limit value of the total content of the compounds represented by the general formula (P) is 0.01%, 0.03%, 0.05%, 0.08%, 0.1%, 0.15%, 0.2%, 0.25%, and 0.3%, relative to the total amount of the liquid crystal composition containing polymerizable compounds of the present invention containing the compounds represented by the general formula (P).

[0502] The preferred upper limit value of the total content of the compounds represented by the general formula (P) is 10%, 8%, 5%, 3%, 1.5%, 1.2%, 1%, 0.8%, and 0.5%, relative to the total amount of the liquid crystal composition containing polymerizable compounds of the present invention containing the compounds represented by the general formula (P).

[0503] If the content of the compound represented by the general formula (P) contained in the liquid crystal composition containing the polymerizable compound of the present invention is small, the effect of adding the compound represented by the general formula (P) is difficult to be manifested, and the alignment control force of the liquid crystal composition is weak, or the alignment control force weakens over time. On the other hand, if the above content is too much, the amount remaining after curing becomes large, the curing takes time, and the reliability of the liquid crystal decreases. Therefore, the content is set in consideration of the balance between them.

[0504] Preferred examples of the compound represented by the general formula (P) include polymerizable compounds represented by the following formulae (P-1-1) to (P-1-46).

[0505] [Chemistry 77]

[0506]

[0507] [Chemistry 78]

[0508]

[0509] [Chemistry 79]

[0510]

[0511] [Chemistry 80]

[0512]

[0513] [Chemistry 81]

[0514]

[0515] (Where P p11 , P p12 、Sp p11 and Sp p12 Indicates that P in the general formula (P) p1 , P p2 、Sp p1 and Sp p2 same meaning).

[0516] Preferred examples of the compound represented by the general formula (P) include polymerizable compounds represented by the following formulae (P-2-1) to (P-2-9).

[0517] [Chemistry 82]

[0518]

[0519] (Where P p21 , P p22 、Sp p21 and Sp p22 Indicates that P in the general formula (P) p1 , P p2 、Sp p1 and Sp p2 same meaning).

[0520] Preferred examples of the compound represented by the general formula (P) include polymerizable compounds represented by the following formulae (P-3-1) to (P-3-15).

[0521] [Chemistry 83]

[0522]

[0523] [Chemistry 84]

[0524]

[0525] (Where P p31 , P p32 、Sp p31 and Sp p32 Indicates that P in the general formula (P) p1 , P p2 、Sp p1 and Sp p2 same meaning).

[0526] Preferred examples of the compound represented by the general formula (P) include polymerizable compounds represented by the following formulae (P-4-1) to (P-4-19).

[0527] [Chemistry 85]

[0528]

[0529] [Chemistry 86]

[0530]

[0531] [Chemistry 87]

[0532]

[0533] [Chemistry 88]

[0534]

[0535] (Where P p41 , P p42 、Sp p41 and Sp p42 Indicates that P in the general formula (P-4) p1 , P p2 、Sp p1 and Sp p2 same meaning).

[0536] When the liquid crystal composition containing a polymerizable compound of the present invention contains a compound represented by the general formula (P), the total content of the compound represented by the general formula (i) and the compound represented by the general formula (P) is preferably in the range of 0.05 to 10%, preferably in the range of 0.1 to 8%, preferably in the range of 0.1 to 5%, preferably in the range of 0.1 to 3%, preferably in the range of 0.2 to 2%, preferably in the range of 0.2 to 1.3%, preferably in the range of 0.2 to 1%, and preferably in the range of 0.2 to 0.56%, relative to the total amount of the liquid crystal composition containing a polymerizable compound.

[0537] In the case where the liquid crystal composition containing polymerizable compounds of the present invention contains a compound represented by the general formula (P), the preferred lower limit of the total content of the compound represented by the general formula (i) and the compound represented by the general formula (P) is 0.01%, 0.03%, 0.05%, 0.08%, 0.1%, 0.15%, 0.2%, 0.25%, and 0.3% relative to the liquid crystal composition containing the polymerizable compound.

[0538] In the case where the liquid crystal composition containing polymerizable compounds of the present invention contains a compound represented by the general formula (P), the preferred upper limit value of the total content of the compound represented by the general formula (i) and the compound represented by the general formula (P) is 10%, 8%, 5%, 3%, 1.5%, 1.2%, 1%, 0.8% and 0.5% relative to the liquid crystal composition containing the polymerizable compound.

[0539] The polymerizable compound-containing liquid crystal composition of the present invention may further contain a compound represented by General Formula (Q).

[0540] [Chemistry 89]

[0541]

[0542] (Where R Q represents a straight-chain alkyl group or a branched alkyl group having 1 to 22 carbon atoms, wherein one or more CH2 groups in the alkyl group may be substituted by -O-, -CH=CH-, -CO-, -OCO-, -COO-, -C≡C-, -CF2O-, or -OCF2- in a manner that the oxygen atom is not directly adjacent to the CH2 group. M Q represents trans-1,4-cyclohexylene, 1,4-phenylene or a single bond).

[0543] In the above general formula (Q), R QIt represents a straight-chain alkyl group or a branched-chain alkyl group having 1 to 22 carbon atoms, in which one or more CH2 groups can also be substituted by -O-, -CH=CH-, -CO-, -OCO-, -COO-, -C≡C-, -CF2O-, or -OCF2- in a manner that the oxygen atom is not directly adjacent. It is preferably a straight-chain alkyl group, a straight-chain alkoxy group, a straight-chain alkyl group in which one CH2 group is substituted by -OCO- or -COO-, a branched alkyl group, a branched alkoxy group, or a branched alkyl group in which one CH2 group is substituted by -OCO- or -COO-, having 1 to 10 carbon atoms. It is more preferably a straight-chain alkyl group, a straight-chain alkyl group in which one CH2 group is substituted by -OCO- or -COO-, a branched alkyl group, a branched alkoxy group, or a branched alkyl group in which one CH2 group is substituted by -OCO- or -COO-, having 1 to 20 carbon atoms.

[0544] In the above general formula (Q), M Q It represents a trans-1,4-cyclohexylene group, a 1,4-phenylene group or a single bond, and is preferably a trans-1,4-cyclohexylene group or a 1,4-phenylene group.

[0545] More specifically, the compound represented by the general formula (Q) is preferably a compound represented by the following general formula (Q-a) to general formula (Q-d).

[0546] [Chemistry 90]

[0547]

[0548] In the formula, R Q1 Preferably, it is a linear or branched alkyl group having 1 to 10 carbon atoms, Q2 Preferably, it is a linear or branched alkyl group having 1 to 20 carbon atoms, Q3 It is preferably a straight-chain alkyl group, a branched-chain alkyl group, a straight-chain alkoxy group or a branched-chain alkoxy group having 1 to 8 carbon atoms, Q It is preferably a linear or branched alkylene group having 1 to 8 carbon atoms.

[0549] As for the compound represented by the general formula (Q), among the compounds represented by the general formula (Q-a) to the general formula (Q-d), the compounds represented by the general formula (Q-c) and the general formula (Q-d) are more preferable.

[0550] The polymerizable compound-containing liquid crystal composition of the present invention preferably contains one or more compounds represented by the general formula (Q), and more preferably contains one to five compounds. In this case, the content of the compound represented by the general formula (Q) is preferably 0.001 to 1%, more preferably 0.001 to 0.1%, and particularly preferably 0.001 to 0.05%, relative to the total amount of the polymerizable compound-containing liquid crystal composition of the present invention.

[0551] The polymerizable compound-containing liquid crystal composition of the present invention may contain, in addition to the above-mentioned compounds, common nematic liquid crystals, smectic liquid crystals, cholesteric liquid crystals, antioxidants, ultraviolet absorbers, light stabilizers, infrared absorbers, and the like.

[0552] Specifically, preferred examples of the antioxidant and light stabilizer that can be used in the present invention include compounds represented by the following formulae (III-1) to (III-40).

[0553] [Chemistry 91]

[0554]

[0555] [Chemistry 92]

[0556]

[0557] [Chemistry 93]

[0558]

[0559] [Chemistry 94]

[0560]

[0561] [Chemistry 95]

[0562]

[0563] [Chemistry 96]

[0564]

[0565] [Chemistry 97]

[0566]

[0567] [Chemistry 98]

[0568]

[0569] [Chemistry 99]

[0570]

[0571] (In the above formulae (III-1) to (III-40), n represents an integer from 0 to 20).

[0572] The liquid crystal composition containing a polymerizable compound of the present invention preferably contains one or more compounds represented by the general formula (Q) or compounds selected from the general formulae (III-1) to (III-40), and more preferably contains one to five compounds, and the content thereof is preferably 0.001 to 1%, more preferably 0.001 to 0.1%, and particularly preferably 0.001 to 0.05%.

[0573] (other)

[0574] The dielectric anisotropy (Δε) of the polymerizable compound-containing liquid crystal composition of the present invention at 20° C. is preferably -2.0 to -8.0, more preferably -2.0 to -5.0, and particularly preferably -2.5 to -5.0.

[0575] The refractive index anisotropy (Δn) of the liquid crystal composition containing a polymerizable compound of the present invention at 20°C is preferably 0.08 to 0.14, more preferably 0.09 to 0.13, and particularly preferably 0.09 to 0.12. More specifically, it is preferably 0.10 to 0.13 for a thin cell gap, and preferably 0.08 to 0.10 for a thick cell gap.

[0576] The viscosity (η) of the liquid crystal composition containing a polymerizable compound at 20°C of the present invention is preferably 10 to 50 mPa·s, preferably 10 to 40 mPa·s, preferably 10 to 35 mPa·s, preferably 10 to 30 mPa·s, further preferably 10 to 25 mPa·s, particularly preferably 10 to 22 mPa·s.

[0577] The rotational viscosity (γ1) of the liquid crystal composition containing polymerizable compounds of the present invention at 20°C is preferably 50 to 160 mPa·s, preferably 60 to 160 mPa·s, preferably 60 to 150 mPa·s, preferably 60 to 140 mPa·s, preferably 60 to 130 mPa·s, preferably 60 to 125 mPa·s, more preferably 60 to 120 mPa·s, more preferably 60 to 115 mPa·s, more preferably 60 to 110 mPa·s, and particularly preferably 60 to 100 mPa·s.

[0578] The nematic-isotropic liquid phase transition temperature (Tni) of the polymerizable compound-containing liquid crystal composition of the present invention is preferably 60°C to 120°C, more preferably 70°C to 100°C, particularly preferably 70°C to 85°C.

[0579] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion of the components consisting only of compounds represented by the general formula (i), general formula (N-1), general formula (N-2), general formula (N-3) and general formula (L) is preferably 100 mass%, 99 mass%, 98 mass%, 97 mass%, 96 mass%, 95 mass%, 94 mass%, 93 mass%, 92 mass%, 91 mass%, 90 mass%, 89 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass%, 84 mass%.

[0580] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the components consisting solely of compounds represented by the general formula (i), general formula (N-1), general formula (N-2), general formula (N-3) and general formula (L) is preferably 78 mass%, 80 mass%, 81 mass%, 83 mass%, 85 mass%, 86 mass%, 87 mass%, 88 mass%, 89 mass%, 90 mass%, 91 mass%, 92 mass%, 93 mass%, 94 mass%, 95 mass%, 96 mass%, 97 mass%, 98 mass% or 99 mass%.

[0581] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion of the components consisting only of compounds represented by general formula (i), general formula (N-1a), general formula (N-1b), general formula (N-1c), general formula (N-1d), general formula (N-1e) and general formula (L) is preferably 100 mass%, 99 mass%, 98 mass%, 97 mass%, 96 mass%, 95 mass%, 94 mass%, 93 mass%, 92 mass%, 91 mass%, 90 mass%, 89 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass% and 84 mass%.

[0582] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the components consisting only of compounds represented by the general formula (i), general formula (N-1a), general formula (N-1b), general formula (N-1c), general formula (N-1d), general formula (N-1e) and general formula (L) is preferably 78 mass%, 80 mass%, 81 mass%, 83 mass%, 85 mass%, 86 mass%, 87 mass%, 88 mass%, 89 mass%, 90 mass%, 91 mass%, 92 mass%, 93 mass%, 94 mass%, 95 mass%, 96 mass%, 97 mass%, 98 mass% and 99 mass%.

[0583] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the component consisting only of the compounds represented by the general formula (i), the general formula (N-1c), the general formula (N-1d), and the general formula (L) is preferably 50 mass%, 61 mass%, 63 mass%, 65 mass%, 66 mass%, 67 mass%, 68 mass%, 70 mass%, 71 mass%, 73 mass%, 75 mass%, 78 mass%, 80 mass%, 81 mass%, 83 mass%, 85 mass%, 86 mass%, 87 mass%, 88 mass%, 89 mass%, 90 mass%, 91 mass%, 92 mass%, 93 mass%, 94 mass%, 95 mass%, 96 mass%, 97 mass%, 98 mass%, or 99 mass%.

[0584] In addition, in the entire liquid crystal composition containing polymerizable compounds of the present invention, the upper limit of the proportion of components consisting solely of compounds represented by general formula (i), general formula (N-1c), general formula (N-1d), and general formula (L) is preferably 100 mass%, 99 mass%, 98 mass%, 97 mass%, 96 mass%, 95 mass%, 94 mass%, 93 mass%, 92 mass%, 91 mass%, 90 mass%, 89 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass%, or 84 mass%.

[0585] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion of the components consisting only of compounds represented by general formula (i), general formula (N-1-4), general formula (N-1b), general formula (N-1c), general formula (N-1d), general formula (N-1e) and general formula (L) is preferably 100 mass%, 99 mass%, 98 mass%, 97 mass%, 96 mass%, 95 mass%, 94 mass%, 93 mass%, 92 mass%, 91 mass%, 90 mass%, 89 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass% or 84 mass%.

[0586] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the components consisting only of compounds represented by the general formula (i), general formula (N-1-4), general formula (N-1b), general formula (N-1c), general formula (N-1d), general formula (N-1e) and general formula (L) is preferably 78 mass%, 80 mass%, 81 mass%, 83 mass%, 85 mass%, 86 mass%, 87 mass%, 88 mass%, 89 mass%, 90 mass%, 91 mass%, 92 mass%, 93 mass%, 94 mass%, 95 mass%, 96 mass%, 97 mass%, 98 mass% and 99 mass%.

[0587] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion occupied by the component consisting only of the compounds represented by the general formula (i), general formula (N-1a), general formula (N-1b), general formula (N-1c), general formula (N-1d), general formula (N-1e), general formula (L-1), general formula (L-3), general formula (L-4), general formula (L-5) and general formula (L-6) is preferably 100% by mass, 99% by mass, 98% by mass, 97% by mass, 96% by mass, 95% by mass, 94% by mass, 93% by mass, 92% by mass, 91% by mass, 90% by mass, 89% by mass, 88% by mass, 87% by mass, 86% by mass, 85% by mass, 84% by mass, 83% by mass, 82% by mass, 81% by mass, or 80% by mass.

[0588] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the component consisting only of the compounds represented by the general formula (i), general formula (N-1a), general formula (N-1b), general formula (N-1c), general formula (N-1d), general formula (N-1e) and general formula (L-1), general formula (L-3), general formula (L-4), general formula (L-5) and general formula (L-6) is preferably 68 mass%, 70 mass%, 71 mass%, 73 mass%, 75 mass%, 78 mass%, 80 mass%, 81 mass%, 83 mass%, 85 mass%, 86 mass%, 87 mass%, 88 mass%, 89 mass%, 90 mass%, 91 mass%, 92 mass%, 93 mass%, 94 mass%, 95 mass%, 96 mass%, 97 mass%, 98 mass%, 99 mass%.

[0589] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion of the component consisting only of the compounds represented by the general formula (i), general formula (N-1a), general formula (L-1), general formula (L-3), general formula (L-4), general formula (L-5) and general formula (L-6) is preferably 100% by mass, 99% by mass, 98% by mass, 97% by mass, 96% by mass, 95% by mass, 94% by mass, 93% by mass, 92% by mass, 91% by mass, 90% by mass, , 89 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass%, 84 mass%, 83 mass%, 82 mass%, 81 mass%, 80 mass%, 79 mass%, 78 mass%, 77 mass%, 76 mass%, 75 mass%, 74 mass%, 73 mass%, 72 mass%, 71 mass%, 70 mass%, 69 mass%, 68 mass%, 67 mass%, 66 mass%, 65 mass%, 64 mass%, 63 mass%, and 62 mass%.

[0590] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the component consisting only of the compounds represented by the general formula (i), general formula (N-1a), general formula (L-1), general formula (L-3), general formula (L-4), general formula (L-5) and general formula (L-6) is preferably 38 mass%, 40 mass%, 41 mass%, 43 mass%, 45 mass%, 48 mass%, 50 mass%, 61 mass%, 63 mass%, 65 mass%, 66 mass%, 67 mass%, 68 mass%, 69 mass%, 70 mass%, 72 mass%, 74 mass%, 76 mass%, 78 mass%, 80 mass%, 82 mass%, 84 mass%, 86 mass%, 88 mass%, 90 mass%, 92 mass%.

[0591] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion of the component consisting only of the compounds represented by the general formula (i), general formula (N-1d), general formula (L-1), general formula (L-3), general formula (L-4), general formula (L-5) and general formula (L-6) is preferably 100% by mass, 99% by mass, 98% by mass, 97% by mass, 96% by mass, 95% by mass, 94% by mass, 93% by mass, 92% by mass, 91% by mass, 90% by mass, , 89 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass%, 84 mass%, 83 mass%, 82 mass%, 81 mass%, 80 mass%, 79 mass%, 78 mass%, 77 mass%, 76 mass%, 75 mass%, 74 mass%, 73 mass%, 72 mass%, 71 mass%, 70 mass%, 69 mass%, 68 mass%, 67 mass%, 66 mass%, 65 mass%, 64 mass%, 63 mass%, and 62 mass%.

[0592] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the component consisting only of the compounds represented by the general formula (i), general formula (N-1d), general formula (L-1), general formula (L-3), general formula (L-4), general formula (L-5) and general formula (L-6) is preferably 38 mass%, 40 mass%, 41 mass%, 43 mass%, 45 mass%, 48 mass%, 50 mass%, 61 mass%, 63 mass%, 65 mass%, 66 mass%, 67 mass%, 68 mass%, 69 mass%, 70 mass%, 72 mass%, 74 mass%, 76 mass%, 78 mass%, 80 mass%, 82 mass%, 84 mass%, 86 mass%, 88 mass%, 90 mass% or 92 mass%.

[0593] In the entire liquid crystal composition containing a polymerizable compound of the present invention, the lower limit of the proportion of the component consisting only of the compounds represented by the general formula (i), the general formula (N-1c), the general formula (N-1d), the general formula (L-1), the general formula (L-3), and the general formula (L-5) is preferably 38 mass%, 40 mass%, 41 mass%, 43 mass%, 45 mass%, 48 mass%, 50 mass%, 61 mass%, 63 mass%, 65 mass%, 66 mass%, 67 mass%, 68 mass%, 70 mass%, 71 mass%, 72 mass%, 73 mass%, 74 mass%, 76 mass%, 77 mass%, 78 mass%, 79 mass%, 80 mass%, 81 mass%, 82 mass%, 83 mass%, 84 mass%, 86 mass%, 87 mass%, 88 mass%, 89 mass%, 90 mass%, 91 mass%, 92 mass%, 93 mass%, 94 mass%, 95 mass%, 96 mass%, 97 mass%, 98 mass%, 99 mass%, 100 mass%, 101 mass%, 102 mass%, 103 mass%, 104 mass%, 105 mass%, 106 mass%, 107 mass%, 108 mass%, 109 mass%, 110 mass%, 111 mass%, 112 mass%, 113 mass%, 114 mass%, 115 mass%, 116 mass%, 117 mass%, 118 mass%, 119 mass%, 120 mass%, 121 mass%, 122 mass%, 123 mass%, 124 mass%, 125 mass%, 126 mass%, 127 mass%, 128 mass%, 129 mass%, 130 mass%, 131 mass%, 132 mass%, 133 mass%, 134 mass%, 135 mass%, 136 mass%, %, 67 mass %, 68 mass %, 69 mass %, 70 mass %, 72 mass %, 74 mass %, 76 mass %, 78 mass %, 80 mass %, 81 mass %, 83 mass %, 85 mass %, 86 mass %, 87 mass %, 88 mass %, 89 mass %, 90 mass %, 91 mass %, 92 mass %, 93 mass %, 94 mass %, 95 mass %, 96 mass %, 97 mass %, 98 mass %, 99 mass %.

[0594] In addition, in the entire liquid crystal composition containing a polymerizable compound of the present invention, the upper limit of the proportion of the component consisting only of the compounds represented by the general formula (i), general formula (N-1c), general formula (N-1d), general formula (L-1), general formula (L-3), and general formula (L-5) is preferably 100% by mass, 99% by mass, 98% by mass, 97% by mass, 96% by mass, 95% by mass, 94% by mass, 93% by mass, 92% by mass, 91% by mass, 90% by mass, 91% by mass, 92% by mass, 93% by mass, 94% by mass, 95% by mass, 96% by mass, 97 ... 9 mass%, 88 mass%, 87 mass%, 86 mass%, 85 mass%, 84 mass%, 83 mass%, 82 mass%, 81 mass%, 80 mass%, 79 mass%, 78 mass%, 77 mass%, 76 mass%, 75 mass%, 74 mass%, 73 mass%, 72 mass%, 71 mass%, 70 mass%, 69 mass%, 68 mass%, 67 mass%, 66 mass%, 65 mass%, 64 mass%, 63 mass%, and 62 mass%.

[0595] The liquid crystal composition containing a polymerizable compound of the present invention preferably does not contain a compound having a structure in which oxygen atoms are bonded to each other, such as a peroxy (-CO-OO-) structure, in the molecule. When the reliability and long-term stability of the liquid crystal composition are important, the content of the compound having a carbonyl group contained in the liquid crystal composition containing a polymerizable compound of the present invention is preferably 5% or less, more preferably 3% or less, further preferably 1% or less, and most preferably substantially free of the compound.

[0596] When emphasis is placed on stability under UV irradiation, in the liquid crystal composition containing a polymerizable compound of the present invention, the content of the compound substituted with chlorine atoms is preferably 15% or less, preferably 10% or less, preferably 8% or less, more preferably 5% or less, preferably 3% or less, and further preferably substantially free of the compound, relative to the total amount of the liquid crystal composition containing the polymerizable compound.

[0597] The liquid crystal composition containing a polymerizable compound of the present invention preferably contains a large amount of compounds whose ring structures in the molecules are all six-membered rings. The content of compounds whose ring structures in the molecules in the liquid crystal composition containing a polymerizable compound of the present invention is preferably 80% or more, more preferably 90% or more, further preferably 95% or more, and most preferably the liquid crystal composition containing a polymerizable compound is substantially composed only of compounds whose ring structures in the molecules are all six-membered rings.

[0598] In order to suppress the degradation caused by oxidation, the liquid crystal composition containing a polymerizable compound of the present invention preferably has a lower content of the compound having a cyclohexenylene group as a ring structure. The content of the compound having a cyclohexenylene group in the liquid crystal composition containing a polymerizable compound of the present invention is preferably 10% or less, preferably 8% or less, more preferably 5% or less, preferably 3% or less, and further preferably substantially free of the compound.

[0599] When the improvement of viscosity and Tni is emphasized, the liquid crystal composition containing a polymerizable compound of the present invention preferably has a lower content of a compound having a 2-methylbenzene-1,4-diyl group in which a hydrogen atom may be substituted by a halogen. The content of the compound having a 2-methylbenzene-1,4-diyl group in the molecule in the liquid crystal composition containing a polymerizable compound of the present invention is preferably 10% or less, preferably 8% or less, more preferably 5% or less, preferably 3% or less, and further preferably substantially free of the compound.

[0600] In the present application, the phrase “substantially not containing” means that the substance does not contain anything other than substances intentionally contained.

[0601] II. Liquid crystal display element

[0602] Next, the liquid crystal display element of the present invention is described. The liquid crystal display element of the present invention is a liquid crystal composition containing a polymerizable compound represented by one or more general formula (i). In other words, it is a liquid crystal display element using a liquid crystal composition containing a polymerizable compound described in the above-mentioned "I. Liquid crystal composition containing a polymerizable compound". The liquid crystal display element using the liquid crystal composition containing a polymerizable compound of the present invention has a significant feature such as high-speed response, and the tilt angle can be fully obtained, there is no unreacted polymerizable compound or so little that no problem occurs, and the voltage holding ratio (VHR) is high, so there is no bad orientation or display or the bad situation is fully suppressed. In addition, since the tilt angle and the residual amount of the polymerizable compound can be easily controlled, the energy cost used for manufacturing can be easily optimized and reduced, so it is most suitable for improving production efficiency and stable mass production.

[0603] The liquid crystal display element using the polymerizable compound-containing liquid crystal composition of the present invention is particularly useful for active matrix drive liquid crystal display elements, and can be used for PSA mode, PSVA mode, VA mode, PS-IPS mode, or PS-FFS mode liquid crystal display elements.

[0604] The liquid crystal display element of the present invention preferably has: a first substrate and a second substrate arranged opposite to each other, a common electrode arranged on the first substrate or the second substrate, a pixel electrode arranged on the first substrate or the second substrate and having a thin film transistor, and a liquid crystal layer arranged between the first substrate and the second substrate and containing a liquid crystal composition containing a polymerizable compound. It is also possible to arrange an orientation film for controlling the orientation direction of liquid crystal molecules on the opposite side of at least one of the first substrate and the second substrate in a manner abutting against the liquid crystal layer as needed, or it is also possible not to arrange an orientation film on both the first substrate and the second substrate. As the orientation film, a vertical orientation film, a horizontal orientation film, etc. can be appropriately selected in accordance with the driving mode of the liquid crystal display element, and a known orientation film such as a rubbing orientation film (for example, a polyimide orientation film) or a light orientation film (for example, a decomposable polyimide orientation film) can be used. Furthermore, a color filter can also be appropriately arranged on the first substrate or the second substrate, and a color filter can be arranged on the pixel electrode and the common electrode.

[0605] The two substrates of the liquid crystal unit used in the liquid crystal display element of the present invention can be made of glass or a flexible transparent material such as plastic, and one of them can also be an opaque material such as silicon. The transparent substrate with a transparent electrode layer can be obtained by sputtering indium tin oxide (ITO) on a transparent substrate such as a glass plate.

[0606] The color filter can be made, for example, by a pigment dispersion method, a printing method, an electrodeposition method or a dyeing method. Taking the method of making a color filter by a pigment dispersion method as an example, a curable coloring composition for a color filter is applied to the transparent substrate, subjected to a patterning treatment, and then cured by heating or irradiation. By performing this process on the three colors of red, green, and blue, a pixel portion for a color filter can be made. In addition, a pixel electrode having active elements such as a TFT, a thin film diode, and a metal insulator metal resistive element can also be provided on the substrate.

[0607] It is preferable that the first substrate and the second substrate are opposed to each other so that the common electrode and the pixel electrode layer are located inside.

[0608] The interval between the first substrate and the second substrate can also be adjusted via a spacer. At this time, it is preferably adjusted to a thickness of 1 to 100 μm, more preferably 1.5 to 10 μm. When a polarizing plate is used, it is preferred to adjust the product of the refractive index anisotropy Δn of the liquid crystal and the unit thickness d in such a way that the contrast is maximized. In addition, when there are two polarizing plates, the polarization axis of each polarizing plate can also be adjusted to adjust the viewing angle and contrast to be good. Furthermore, a phase difference film for expanding the viewing angle can also be used. As spacers, for example, glass particles, plastic particles, aluminum oxide particles, photoresist materials, etc. are listed. Then, a sealant such as an epoxy-based thermosetting composition is screen-printed on the substrate in a shape having a liquid crystal injection port, the substrates are bonded to each other, and heated to thermally cure the sealant.

[0609] As a method for sandwiching the liquid crystal composition containing a polymerizable compound between two substrates, a common vacuum injection method, an ODF method, or the like can be used.

[0610] As a method for polymerizing the polymerizable compound contained in the liquid crystal composition containing the polymerizable compound, in order to obtain good orientation performance of the liquid crystal, it is more desirable to have an appropriate polymerization speed. Therefore, it is preferred to polymerize by irradiating active energy lines such as ultraviolet rays or electron beams alone, in combination, or in sequence. When ultraviolet rays are used, a polarized light source can be used, or a non-polarized light source can be used. In addition, when the polymerized liquid crystal composition containing the polymerizable compound is sandwiched between two substrates, at least the substrate on the irradiated side must have appropriate transparency for the active energy line. In addition, the following method can also be used: after polymerizing only a specific part using a mask during irradiation, the conditions such as the electric field, magnetic field or temperature are changed, thereby changing the orientation state of the unpolymerized part, and further irradiating the active energy line to polymerize it. In particular, when ultraviolet exposure is performed, it is preferred to apply an alternating electric field to the liquid crystal composition containing the polymerizable compound and simultaneously perform ultraviolet exposure. The applied alternating electric field is preferably an alternating current with a frequency of 10 Hz to 10 kHz, more preferably a frequency of 60 Hz to 10 kHz, and the voltage is selected depending on the desired pretilt angle of the liquid crystal display element. That is, the pretilt angle of the liquid crystal display element can be controlled by the applied voltage. In the PSVA mode liquid crystal display element, the pretilt angle is preferably controlled to be 80 degrees to 89.9 degrees from the viewpoint of alignment stability and contrast.

[0611] The temperature at which the active energy rays such as ultraviolet rays or electron beams are irradiated when polymerizing the polymerizable compound contained in the liquid crystal composition containing the polymerizable compound is not particularly limited. For example, when the liquid crystal composition containing the polymerizable compound is applied to a liquid crystal display element having a substrate with an alignment film, it is preferably within a temperature range in which the liquid crystal composition containing the polymerizable compound maintains a liquid crystal state. It is preferably polymerized at a temperature close to room temperature, typically 15 to 35°C.

[0612] On the other hand, for example, when a liquid crystal composition containing a polymerizable compound is applied to a liquid crystal display element having a substrate without an oriented film, its temperature range can also be wider than the temperature range when it is applied to the liquid crystal display element having a substrate with an oriented film.

[0613] As the lamp generating ultraviolet rays, metal halide lamps, high pressure mercury lamps, ultra-high pressure mercury lamps, etc. can be used. In addition, as the wavelength of the ultraviolet rays to be irradiated, it is preferred to irradiate ultraviolet rays in a wavelength region that is not the absorption wavelength region of the liquid crystal composition containing the polymerizable compound, and it is preferred to filter out the ultraviolet rays before use as necessary. The intensity of the ultraviolet rays to be irradiated is preferably 0.1 mW / cm 2 ~100W / cm 2 , more preferably 2mW / cm 2 ~50W / cm 2The energy of the irradiated ultraviolet light can be adjusted appropriately, preferably 10 mJ / cm 2 ~500J / cm 2 , more preferably 100 mJ / cm 2 ~200J / cm 2 When irradiating ultraviolet rays, the intensity may be changed. The time for irradiating ultraviolet rays may be appropriately selected according to the intensity of the irradiated ultraviolet rays, and is preferably 10 seconds to 3600 seconds, and more preferably 10 seconds to 600 seconds.

[0614] III. Polymeric compounds

[0615] The polymerizable compound of the present invention is a compound represented by the general formula (i).

[0616] [Chemical 100]

[0617]

[0618] (In the formula, A i1 and A i2 Each independently represents a group selected from the group consisting of the following (a) to (c),

[0619] (a) 1,4-cyclohexylene (one -CH2- or two or more non-adjacent -CH2- in the group may be substituted by -O-),

[0620] (b) 1,4-phenylene (one -CH= or two or more non-adjacent -CH= groups in the group may be substituted with -N=), and

[0621] (c) naphthalenediyl, 1,2,3,4-tetrahydronaphthalenediyl or decahydronaphthalenediyl (one -CH= or two or more non-adjacent -CH= in naphthalenediyl or 1,2,3,4-tetrahydronaphthalenediyl may be substituted with -N=),

[0622] The above-mentioned groups (a), (b) and (c) may be independently substituted by an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a halogen group, a cyano group, a nitro group or a P i3 -S i3 -replace,

[0623] P i1 , P i2 and P i3 Each independently represents a group selected from the group consisting of formula (R-1) to formula (R-9),

[0624] [Chemistry 101]

[0625]

[0626] (Where R11 , R 12 , R 13 , R 14 and R 15 each independently represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom, and m r5 、m r7 、n r5 and n r7 Each independently represents 0, 1, or 2),

[0627] S i1 , S i2 and S i3 Each independently represents a single bond or an alkylene group having 1 to 15 carbon atoms, wherein one -CH2- or two or more non-adjacent -CH2- groups in the alkylene group may be substituted by -O-, -OCO- or -COO- in a manner that the oxygen atom is not directly adjacent to the -CH2- group.

[0628] R i1 represents an alkyl group having 1 to 5 carbon atoms, a fluorine atom or a hydrogen atom,

[0629] n i1 Indicates 1, 2, or 3,

[0630] In the presence of multiple A i2 , S i2 , P i3 and / or S i3 In the case of

[0631] The polymerizable compound of the present invention, when added to a liquid crystal composition to prepare a liquid crystal composition containing the polymerizable compound, is difficult to precipitate from the liquid crystal composition containing the polymerizable compound, has a high polymerization rate, and can be fully polymerized even with a short period of ultraviolet irradiation, thereby reducing the amount of unreacted polymerizable compound remaining. In addition, the polymerizable compound of the present invention can suppress display defects (screen burn-in) caused by large changes in the pretilt angle in a liquid crystal display element.

[0632] Since the details of the polymerizable compound of the present invention have been described in the above section “I. Liquid crystal composition containing a polymerizable compound”, the description here will be omitted.

[0633] The present invention is not limited to the above-mentioned embodiments. The above-mentioned embodiments are merely examples, and any invention having substantially the same configuration and achieving the same effects as the technical concept described in the claims of the present invention is included in the technical scope of the present invention.

[0634] Example

[0635] The present invention will be described in further detail with reference to the following examples, but the present invention is not limited to these examples. In addition, "%" in the compositions of the following examples and comparative examples means "mass %".

[0636] The following codes are used to describe the compounds in Examples and Comparative Examples.

[0637] (Sidechain)

[0638] -n -C n H 2n+1 A linear alkyl group with n carbon atoms

[0639] n-C n H 2n+1 - A linear alkyl group with n carbon atoms

[0640] -On -OC n H 2n+1 A linear alkoxy group with n carbon atoms

[0641] 1V-CH3-CH=CH-

[0642] (Linking base)

[0643] -1O--CH2-O-

[0644] -2--CH2-CH2-

[0645] (Ring structure)

[0646]

[0647] The properties measured in the following Examples and Comparative Examples are as follows.

[0648] Tni: Nematic-isotropic liquid phase transition temperature (°C)

[0649] Δn: refractive index anisotropy at 20°C

[0650] η: Viscosity at 20°C (mPa·s)

[0651] γ1: Rotational viscosity at 20°C (mPa·s)

[0652] Δε: Dielectric anisotropy at 20°C

[0653] The manufacturing method and evaluation method of the liquid crystal display element in the following Examples and Comparative Examples are as follows.

[0654] (Method for manufacturing liquid crystal display element)

[0655] First, the liquid crystal composition containing a polymerizable compound described later is injected into a liquid crystal cell with a cell gap of 3.5 μm containing an ITO-attached substrate coated with a polyimide alignment film that induces vertical alignment and subjected to a rubbing treatment by vacuum injection. After that, the liquid crystal cell injected with the liquid crystal composition containing a polymerizable compound is irradiated with ultraviolet light for an arbitrary period of time using a fluorescent UV lamp to obtain a liquid crystal display element. At this time, the illuminance measured at a central wavelength of 313 nm is 3 mW / cm 2 Adjust the fluorescent UV lamp in this way.

[0656] (Evaluation method of residual amount of polymerizable compound)

[0657] The residual amount [ppm] of the polymerizable compound in the liquid crystal display element after irradiation with ultraviolet light for 150 seconds, 15 minutes or 60 minutes is measured under the above irradiation conditions. The method for determining the residual amount of the polymerizable compound is described below. First, the decomposed liquid crystal display element and acetonitrile are placed in a test tube, shaken and filtered to obtain an acetonitrile solution containing the eluted components of the liquid crystal composition, polymer, and unreacted polymerizable compound. It is analyzed using a high performance liquid chromatograph (column: reverse phase non-polar column, developing solvent: a mixed solvent of 70% acetonitrile and 30% water) to calculate the peak area of ​​each component. The amount of the residual polymerizable compound is determined by the ratio of the peak area of ​​the liquid crystal compound as an indicator to the peak area of ​​the unreacted polymerizable compound. The residual amount of the polymerizable compound is determined based on this value and the amount of the polymerizable compound originally added. Furthermore, the detection limit of the residual amount of the polymerizable compound is 100ppm.

[0658] (VHR evaluation method)

[0659] The liquid crystal cell into which the liquid crystal composition containing the polymerizable compound was injected was irradiated with ultraviolet rays for 60 minutes under the above-mentioned irradiation conditions, and VHR was measured. The measurement conditions of VHR were 1 V, 0.6 Hz, and 60°C.

[0660] (Evaluation Method for Screen Burn-in)

[0661] After the liquid crystal unit injected with the liquid crystal composition containing the polymerizable compound was irradiated with ultraviolet rays for 60 minutes under the above-mentioned irradiation conditions, the display defect (burn-in) caused by the change of the pretilt angle was evaluated. First, the pretilt angle of the liquid crystal display element was measured and set as the pretilt angle (initial). While applying a voltage of 30V to this liquid crystal display element at a frequency of 100Hz, a backlight (back light) was irradiated for 3 hours. Then, the pretilt angle was measured and set as the pretilt angle (after the test). The value obtained by subtracting the pretilt angle (after the test) from the measured pretilt angle (initial) was set as the pretilt angle change (= absolute value of the pretilt angle change) [°]. The pretilt angle was measured using OPTIPRO manufactured by Shintec. The closer the pretilt angle change is to 0 [°], the lower the possibility of poor display caused by the change in the pretilt angle becomes. If it is above 0.5 [°], the possibility of poor display caused by the change in the pretilt angle becomes higher.

[0662] 1. Synthesis of polymerizable compounds

[0663] (Example 1A) Synthesis of polymerizable compound represented by formula (i-1a)

[0664] [Chemistry 102]

[0665]

[0666] First, under a nitrogen environment, 10.0 g of the compound represented by formula (i-1a-1), 8.9 g of tert-butyl acrylate, 12.0 g of potassium carbonate, 100 mL of N,N-dimethylacetamide, and 0.010 g of palladium (II) acetate were added to a reaction vessel and heated and stirred at 120°C for 5 hours. After cooling to room temperature, the reaction solution was injected into 5% hydrochloric acid. Ethyl acetate was used for extraction, and the organic layer was washed with water and brine in sequence. Column chromatography (alumina, ethyl acetate) was used for purification to obtain 10.2 g of the compound represented by formula (i-1a-2).

[0667] Next, under a nitrogen environment, 10.2 g of the compound represented by formula (i-1a-2), 4.4 g of methacrylic acid, 0.6 g of 4-dimethylaminopyridine, and 100 mL of dichloromethane were added to the reaction vessel. While cooling with ice, 7.0 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 7 hours. The precipitate was removed by filtration, and the filtrate was washed with 5% hydrochloric acid, water, and brine in sequence. Purification was performed by column chromatography (silica gel, dichloromethane / hexane), thereby obtaining 10.7 g of the compound represented by formula (i-1a-3).

[0668] Next, 10.7 g of the compound represented by formula (i-1a-3), 30 mL of dichloromethane, and 60 mL of formic acid were added to the reaction vessel, and heated and stirred at 40° C. for 6 hours. The solvent was distilled off under reduced pressure, and the obtained solid was washed with water and dried to obtain 8.2 g of the compound represented by formula (i-1a-4).

[0669] [Chemistry 103]

[0670]

[0671] Next, 10.0 g of the compound represented by formula (i-1a-5), 1.3 g of pyridinium p-toluenesulfonate, and 100 mL of dichloromethane were added to the reaction vessel. 5.0 g of 3,4-dihydro-2H-pyran was added dropwise while cooling with ice, and stirred at room temperature for 8 hours. The reaction solution was washed with saturated sodium bicarbonate aqueous solution and brine in sequence. Purification was performed by column chromatography (alumina, dichloromethane), thereby obtaining 12.8 g of the compound represented by formula (i-1a-6).

[0672] Next, 12.8 g of the compound represented by formula (i-1a-6), 50 mL of tetrahydrofuran, 50 mL of ethanol, and a palladium catalyst (manufactured by Evonic, E 106O / W 5% Pd) were added to a pressure-resistant reaction vessel. Stirring was heated at 50°C for 8 hours at a hydrogen pressure of 0.5 MPa. The catalyst was removed by filtration, and the filtrate was distilled under reduced pressure. Purification was performed by column chromatography (alumina, ethyl acetate), thereby obtaining 8.3 g of the compound represented by formula (i-1a-7).

[0673] Next, under a nitrogen environment, 8.3 g of the compound represented by formula (i-1a-7), 4.0 g of methacrylic acid, 0.5 g of 4-dimethylaminopyridine, and 90 mL of dichloromethane were added to a reaction vessel. While cooling with ice, 6.5 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 7 hours. The precipitate was removed by filtration, and the filtrate was washed with 5% hydrochloric acid, water, and saline in sequence. Purification was performed by column chromatography (alumina, dichloromethane), thereby obtaining 9.0 g of the compound represented by formula (i-1a-8).

[0674] Next, 9.0 g of the compound represented by formula (i-1a-8), 70 mL of tetrahydrofuran, 70 mL of methanol, and 0.1 mL of concentrated hydrochloric acid were added to a reaction vessel and stirred at room temperature for 6 hours. Ethyl acetate was added to the reaction solution, and washed with water and brine in sequence. Column chromatography (alumina, ethyl acetate) and recrystallization (ethyl acetate / hexane) were used for purification to obtain 5.5 g of the compound represented by formula (i-1a-9).

[0675] Under nitrogen environment, 5.5 g of the compound represented by formula (i-1a-9), 7.1 g of the compound represented by formula (i-1a-4), 0.4 g of 4-dimethylaminopyridine, and 100 mL of dichloromethane were added to a reaction vessel. While cooling with ice, 4.7 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 7 hours. The precipitate was removed by filtration, and the filtrate was washed with 5% hydrochloric acid, water, and brine in sequence. Purification was performed by column chromatography (silica gel, dichloromethane) and recrystallization (dichloromethane / methanol), thereby obtaining 9.7 g of the compound represented by formula (i-1a).

[0676] The phase transition temperature of the compound represented by the obtained formula (i-1a), 1 The H NMR peaks and LC-MS are shown below.

[0677] Phase transition temperature (temperature rise 5℃ / min): C 161I

[0678] · 1 H NMR(CDCl3)δ2.08(m,6H),5.78(d,2H),6.37(d,2H),6.59(d,1H),7.16-7.22(m,6H),7.63(d,2H),7.86(d,1H)ppm

[0679] LC-MS: 393[M+1]

[0680] (Example 2A) Synthesis of the polymerizable compound represented by formula (i-24a)

[0681] [Chemistry 104]

[0682]

[0683] First, 13.8 g of the compound represented by formula (i-24a-1), 1.4 g of p-toluenesulfonic acid monohydrate, and 150 mL of ethyl acetate were added to a reaction vessel equipped with a Dean-Stark apparatus. While removing the solvent, new ethyl acetate was added and heated to reflux for 5 hours. After cooling, the reaction solution was washed with a saturated sodium bicarbonate aqueous solution and brine in sequence. Purification was performed using column chromatography (alumina, ethyl acetate) and recrystallization (ethyl acetate / hexane), thereby obtaining 13.9 g of the compound represented by formula (i-24a-2).

[0684] Next, under nitrogen environment, 13.9 g of the compound represented by formula (i-24a-2), 0.3 g of pyridinium p-toluenesulfonate, and 60 mL of dichloromethane were added to the reaction vessel. While cooling with ice, 7.5 g of 3,4-dihydro-2H-pyran was added dropwise, and stirred at room temperature for 10 hours. The reaction solution was washed with saturated sodium bicarbonate aqueous solution and brine in sequence. Purification was performed by column chromatography (alumina, dichloromethane) and recrystallization (dichloromethane / methanol), thereby obtaining 16.6 g of the compound represented by formula (i-24a-3).

[0685] Next, 16.6 g of the compound represented by formula (i-24a-3) and 300 mL of methanol were added to the reaction container. 8.4 mL of 50% aqueous sodium hydroxide solution was added at room temperature, and heated and stirred at 50°C for 4 hours. The reaction solution was added to water. The aqueous layer was adjusted to pH 7 and extracted with ethyl acetate. The organic layer was washed with water and brine in sequence. Purification was performed by column chromatography (alumina, ethyl acetate) and recrystallization (ethyl acetate / hexane), thereby obtaining 12.7 g of the compound represented by formula (i-24a-4).

[0686] Next, under a nitrogen environment, 12.4 g of the compound represented by formula (i-24a-4), 0.6 g of 4-dimethylaminopyridine, 99 mL of dichloromethane, and 4.6 g of methacrylic acid were added to a reaction vessel. While cooling with ice, 6.8 g of diisopropylcarbodiimide was added dropwise, and the mixture was stirred at room temperature for 10 hours. The precipitated solid was removed by filtration, and the solvent was distilled under reduced pressure. Recrystallization (methanol) was performed. Purification was performed by column chromatography (NH2 silica gel, dichloromethane / hexane) and recrystallization (dichloromethane / methanol), thereby obtaining 5.4 g of the compound represented by formula (i-24a-5).

[0687] Next, 5.4 g of the compound represented by formula (i-24a-5), 50 mL of tetrahydrofuran, and 50 mL of methanol were added to the reaction container. 0.2 mL of concentrated hydrochloric acid was added, and the mixture was stirred at room temperature for 3 hours. The reaction solution was added to water and extracted with ethyl acetate. The organic layer was washed with saline. Purification was performed by column chromatography (alumina, ethyl acetate) and recrystallization (ethyl acetate / hexane), thereby obtaining 4.0 g of the compound represented by formula (i-24a-6).

[0688] Next, under a nitrogen environment, 4.0 g of the compound represented by formula (i-24a-6), 3.5 g of the compound represented by formula (i-1a-4) synthesized in Example 1A, 0.2 g of 4-dimethylaminopyridine, and 50 mL of dichloromethane were added to the reaction vessel. While cooling with ice, 2.3 g of diisopropylcarbodiimide was added dropwise, and the mixture was stirred at room temperature for 10 hours. The precipitated solid was removed by filtration, and the solvent was distilled under reduced pressure. Recrystallization (methanol) was performed. Purification was performed by column chromatography (silica gel, dichloromethane) and recrystallization (dichloromethane / methanol), thereby obtaining 5.9 g of the compound represented by formula (i-24a).

[0689] The phase transition temperature of the compound represented by the formula (i-24a) obtained, 1 The H NMR peaks and LC-MS are shown below.

[0690] Phase transition temperature (temperature rise 5℃ / min): C 179N>220I

[0691] · 1 H NMR(CDCl3)δ1.54-1.67(m,4H),1.95-2.01(m,5H),2.07(s,3H),2.14-2.14(m,2H),2.57(m,1H),4.85(m,1H),5.55(m,1H) ,5.79(m,1H),6.11(s,1H),6.37(s,1H),6.59(d,1H),7.09(d,2H),7.20(d,2H),7.24(d,2H),7.62(d,2H),7.85(d,1H)ppm.

[0692] LC-MS: 475[M+1]

[0693] (Example 3A) Synthesis of the polymerizable compound represented by formula (i-31a)

[0694] [Chemistry 105]

[0695]

[0696] First, under nitrogen environment, add 25.0 g of the compound represented by formula (i-31a-1), 0.7 g of pyridinium p-toluenesulfonate, and 120 mL of dichloromethane to a reaction container. Add 16.8 g of 3,4-dihydro-2H-pyran dropwise while cooling with ice, and stir at room temperature for 2 hours. Add water to the reaction solution, and wash the organic layer with saturated sodium bicarbonate aqueous solution and brine in sequence. Purify by column chromatography (NH2 silica gel, dichloromethane), thereby obtaining 38.2 g of the compound represented by formula (i-31a-2).

[0697] Next, under a nitrogen environment, 38.0 g of the compound represented by formula (i-31a-2), 0.5 g of dichlorobis[di-tert-butyl(p-dimethylaminophenyl)phosphino]palladium(II), 150 mL of potassium carbonate (2 mol / L aqueous solution), and 500 mL of tetrahydrofuran were added to a reaction vessel, and heated and stirred at 60°C. A solution of 23.1 g of the compound represented by formula (i-31a-3) in tetrahydrofuran (100 mL) / water (20 mL) was added dropwise, and heated and stirred at 60°C for 10 hours. After cooling to room temperature, water was added to the reaction solution. Extraction was performed with ethyl acetate, and the organic layer was washed with brine. Purification was performed by column chromatography (alumina, dichloromethane), thereby obtaining 45.7 g of the compound represented by formula (i-31a-4).

[0698] Next, under a nitrogen environment, 45.7 g of the compound represented by formula (i-31a-4), 1.6 g of 4-dimethylaminopyridine, 300 mL of dichloromethane, and 14.7 g of methacrylic acid were added to the reaction vessel. While cooling with ice, 22.3 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 6 hours. The precipitated solid was removed by filtration, and the organic layer was washed with 10% hydrochloric acid and brine in sequence. Purification was performed by column chromatography (alumina, dichloromethane) and recrystallization (dichloromethane / methanol, -78°C), thereby obtaining 25.0 g of the compound represented by formula (i-31a-5).

[0699] Next, 25.0 g of the compound represented by formula (i-31a-5), 250 mL of tetrahydrofuran, and 50 mL of methanol were added to the reaction container. 0.2 mL of concentrated hydrochloric acid was added, and the mixture was stirred at room temperature for 2 hours. Water was added to the reaction solution, and the mixture was extracted with ethyl acetate, and the organic layer was washed with saline. Column chromatography (silica gel, dichloromethane) and recrystallization (hexane) were used for purification, thereby obtaining 12.5 g of the compound represented by formula (i-31a-6).

[0700] Next, under a nitrogen environment, 3.7 g of the compound represented by formula (i-31a-6), 3.2 g of the compound represented by formula (i-1a-4) synthesized in Example 1A, 0.2 g of 4-dimethylaminopyridine, and 50 mL of dichloromethane were added to the reaction vessel. While cooling with ice, 2.1 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 4 hours. The precipitated solid was removed by filtration, and the organic layer was washed with 10% hydrochloric acid and brine in sequence. Purification was performed by column chromatography (silica gel, dichloromethane) and recrystallization (dichloromethane / methanol), thereby obtaining 5.9 g of the compound represented by formula (i-31a).

[0701] The phase transition temperature of the compound represented by the obtained formula (i-31a), 1 The H NMR peaks and LC-MS are shown below.

[0702] Phase transition temperature (temperature rise 5℃ / min): C 160N>220I

[0703] · 1 H NMR(CDCl3)δ2.08(s,3H),2.09(s,3H),2.29(s,3H),5.79(dt,2H),6.38(d,2H ),6.62(d,1H),7.06(m,2H),7.16-7.35(m,7H),7.64(d,2H),7.87(d,1H)ppm.

[0704] LC-MS: 483[M+1]

[0705] (Example 4A) Synthesis of the polymerizable compound represented by formula (i-33a)

[0706] [Chemistry 106]

[0707]

[0708] First, under a nitrogen environment, 25.0 g of the compound represented by formula (i-33a-2), 0.5 g of dichlorobis[di-tert-butyl(p-dimethylaminophenyl)phosphino]palladium(II), 160 mL of potassium carbonate (2 mol / L aqueous solution), and 500 mL of tetrahydrofuran were added to a reaction vessel, and heated and stirred at 60°C. A solution of 35.0 g of the compound represented by formula (i-33a-1) in tetrahydrofuran (100 mL) / water (20 mL) was added dropwise, and heated and stirred at 60°C for 3 hours. After cooling to room temperature, water was added to the reaction solution. Extraction was performed with ethyl acetate, and the organic layer was washed with brine. Purification was performed by column chromatography (alumina, dichloromethane), thereby obtaining 44.7 g of the compound represented by formula (i-33a-3).

[0709] Next, under a nitrogen environment, 44.7 g of the compound represented by formula (i-33a-3), 1.6 g of 4-dimethylaminopyridine, 300 mL of dichloromethane, and 12.7 g of methacrylic acid were added to a reaction vessel. While cooling with ice, 20.3 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 2 hours. The precipitated solid was removed by filtration, and the organic layer was washed with 10% hydrochloric acid and brine in sequence. Purification was performed by column chromatography (alumina, dichloromethane) and recrystallization (dichloromethane / methanol), thereby obtaining 37.0 g of the compound represented by formula (i-33a-4).

[0710] Then, 37.0 g of the compound represented by formula (i-33a-4), 250 mL of tetrahydrofuran, and 50 mL of methanol were added to the reaction container. 0.2 mL of concentrated hydrochloric acid was added, and the mixture was stirred at room temperature for 2 hours. Water was added to the reaction solution, and the mixture was extracted with ethyl acetate, and the organic layer was washed with saline. The mixture was purified by column chromatography (silica gel, dichloromethane) and reprecipitation (hexane), thereby obtaining 25.3 g of the compound represented by formula (i-33a-5).

[0711] Under nitrogen environment, 3.7 g of the compound represented by formula (i-33a-5), 3.2 g of the compound represented by formula (i-1a-4) synthesized in Example 1A, 0.2 g of 4-dimethylaminopyridine, and 50 mL of dichloromethane were added to the reaction container. While cooling with ice, 2.1 g of diisopropylcarbodiimide was added dropwise, and stirred at room temperature for 5 hours. The precipitated solid was removed by filtration, and the organic layer was washed with 10% hydrochloric acid and brine in sequence. Purification was performed by column chromatography (silica gel, dichloromethane), recrystallization (dichloromethane / methanol) and column chromatography (silica gel, dichloromethane / hexane), thereby obtaining 1.8 g of the compound represented by formula (i-33a).

[0712] The phase transition temperature of the compound represented by the obtained formula (i-33a), 1 The H NMR peaks and LC-MS are shown below.

[0713] Phase transition temperature (temperature rise 5°C / min): C 165N 200poly

[0714] · 1 H NMR(CDCl3)δ2.08(s,6H),2.29(s,3H),5.78(dt,2H),6.37(dt,2H),6.63(d ,1H),7.01(m,2H),7.22(m,5H),7.35(m,2H),7.64(d,2H),7.88(d,1H)ppm.

[0715] LC-MS: 483[M+1]

[0716] (Example 5A) Synthesis of polymerizable compounds represented by formula (i-2a) and (i-18a)

[0717] According to the method of Example 1A, polymerizable compounds represented by formula (i-2a) and (i-18a) were synthesized respectively.

[0718] 2. Preparation and evaluation results of liquid crystal compositions containing polymerizable compounds

[0719] (Preparation and Physical Properties of Liquid Crystal Composition)

[0720] Liquid crystal compositions LC-001 to LC-005 before adding a polymerizable compound were prepared, and their physical properties were measured. Table 1 shows the compositions of the liquid crystal compositions LC-001 to LC-005 and the results of their physical properties.

[0721] [Table 1]

[0722] LC-001 LC-002 LC-003 LC-004 LC-005 3-Cy-Cy-2 18 19 20 20 21 3-Cy-Cy-4 8 6.5 4 4 8.5 3-Cy-Cy-5 4 2.5 3-Cy-Ph-O1 2 6 4 3-Ph-Ph-1 13 10 12 10 4.5 3-Cy-Ph-Ph-1 2 5 5 3 3-Cy-Ph-Ph-2 6 3 5 5-Cy-Ph-Ph-2 4 6 3-Cy-Ph5-O2 15 3-Ph-Ph5-O2 12 6.5 3-Cy-1O-Ph5-O1 6 3.5 3-Cy-1O-Ph5-O2 7 11 9 2-Cy-Cy-1O-Ph5-O2 14 2 3-Cy-Cy-1O-Ph5-O2 3 13 10 12 1V-Cy-Cy-1O-Ph5-O2 5 5 2-Cy-Ph-Ph5-O2 7 7 10 7 3-Cy-Ph-Ph5-O2 8 8 10 7 3-Cy-Ph-Ph5-O3 6 2 7 3-Cy-Ph-Ph5-O4 7 7 9 7 4-Cy-Ph-Ph5-O3 8 3-Ph-2-Ph-Ph5-O2 5 8 Total (wt%) 100 100 100 100 100 Tni [℃] 73.8 75.1 76.7 76.2 74.6 Δn 0.111 0.105 0.118 0.128 0.119 Δε -3.2 -3.2 -3.3 -3.4 -2.3 γ1 [mPa·s] 125 97 132 134 95

[0723] (Comparative Examples 1-2)

[0724] Comparative Example 1 was a liquid crystal composition containing a polymerizable compound to which 0.3 parts by mass of a compound represented by the following formula (A) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-001.

[0725] Comparative Example 2 was a liquid crystal composition containing a polymerizable compound to which 0.3 parts by mass of a compound represented by the following formula (B) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-001.

[0726] [Chemistry 107]

[0727]

[0728] (Examples 1B to 4B)

[0729] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound with respect to 99.7 parts by mass of the liquid crystal composition LC-001 was referred to as Example 1B.

[0730] A polymerizable compound-containing liquid crystal composition containing 0.3 parts by mass of the compound represented by formula (i-24a) added as a polymerizable compound to 99.7 parts by mass of the liquid crystal composition LC-001 was referred to as Example 2B.

[0731] A polymerizable compound-containing liquid crystal composition containing 0.3 parts by mass of the compound represented by formula (i-31a) added as a polymerizable compound to 99.7 parts by mass of the liquid crystal composition LC-001 was referred to as Example 3B.

[0732] A polymerizable compound-containing liquid crystal composition containing 0.3 parts by mass of the compound represented by formula (i-33a) added as a polymerizable compound to 99.7 parts by mass of the liquid crystal composition LC-001 was referred to as Example 4B.

[0733] [Chemistry 108]

[0734]

[0735] For the liquid crystal compositions containing polymerizable compounds of Comparative Examples 1 to 2 and Examples 1B to 4B, the amount of polymerizable compound remaining after irradiation with ultraviolet rays for a predetermined time, the VHR after irradiation with ultraviolet rays for 60 minutes, and the amount of change in pretilt angle are shown in the following Table 2. In addition, the physical properties of the liquid crystal compositions containing polymerizable compounds of Comparative Examples 1 to 2 and Examples 1B to 4B are respectively equivalent to the physical properties of the liquid crystal composition LC-001.

[0736] [Table 2]

[0737]

[0738] Although the pretilt angle change of the liquid crystal composition containing a polymerizable compound of Comparative Example 1 is a sufficiently small value, the residual amount of the polymerizable compound after 60 minutes of ultraviolet irradiation is large. In addition, the residual amount of the polymerizable compound after 60 minutes of ultraviolet irradiation of the liquid crystal composition containing a polymerizable compound of Comparative Example 2 is less than the detection limit, but the pretilt angle change is a large value.

[0739] On the other hand, in Examples 1B to 4B of the liquid crystal composition containing a polymerizable compound of the present invention, the residual amount of the polymerizable compound after 60 minutes of ultraviolet irradiation is less than the detection limit, showing a significantly smaller amount than that of Comparative Example 1. It can be seen from this that the polymerization rate of the polymerizable compound of Examples 1B to 4B is sufficiently fast compared to Comparative Example 1. In addition, it was confirmed that the change in pretilt angle is a sufficiently small value compared to Comparative Example 2. Furthermore, compared with Comparative Examples 1 and 2, the VHR of Examples 1B to 4B after 60 minutes of ultraviolet irradiation is a sufficiently high value.

[0740] From the above content, it can be confirmed that: in the liquid crystal composition containing polymerizable compounds of the present invention, the polymerization rate of the polymerizable compound represented by general formula (i) is sufficiently fast, the residual amount of the unreacted polymerizable compound is also suppressed, and the VHR after 60 minutes of ultraviolet irradiation is sufficiently high, and it is difficult to produce display defects caused by changes in the pretilt angle.

[0741] (Comparative Example 3)

[0742] Comparative Example 3 was a liquid crystal composition containing a polymerizable compound to which 0.3 parts by mass of the compound represented by the formula (C) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-001.

[0743] [Chemistry 109]

[0744]

[0745] Although the results of the residual amount of polymerizable compound, VHR, and pretilt angle change of the polymerizable compound-containing liquid crystal composition of Comparative Example 3 after irradiation with ultraviolet rays for 60 minutes were equivalent to those of Examples 1B to 4B, precipitation of the polymerizable compound was confirmed after storage at room temperature for 240 hours. On the other hand, the polymerizable compound-containing liquid crystal composition of Examples 1B to 4B maintained a uniform nematic liquid crystal phase even after storage at room temperature for 240 hours, and precipitation of the polymerizable compound was not confirmed.

[0746] From the above, it can be confirmed that the precipitation of the polymerizable compound represented by the general formula (i) is suppressed in the liquid crystal composition containing the polymerizable compound of the present invention. i1 The result of Comparative Example 3 suggests that A in the general formula (i) i1 When there are two or more, the solubility is reduced and precipitation becomes easy; and in the compound represented by the general formula (i) of the present invention, A in the general formula (i) i1 When the amount is 1, the solubility is improved and precipitation becomes difficult.

[0747] (Examples 5B to 8B)

[0748] A polymerizable compound-containing liquid crystal composition to which 0.4 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound with respect to 99.6 parts by mass of the liquid crystal composition LC-001 was referred to as Example 5B.

[0749] A polymerizable compound-containing liquid crystal composition to which 0.6 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound with respect to 99.4 parts by mass of the liquid crystal composition LC-001 was referred to as Example 6B.

[0750] A polymerizable compound-containing liquid crystal composition obtained by further adding 50 ppm of an antioxidant represented by formula (H-1) to Example 1 was designated as Example 7B.

[0751] A polymerizable compound-containing liquid crystal composition obtained by further adding 50 ppm of an antioxidant represented by formula (H-2) to Example 1 was designated as Example 8B.

[0752] [Chemistry 110]

[0753]

[0754] The same evaluation as in Example 1B was also performed on the liquid crystal compositions containing polymerizable compounds of Examples 5B to 8B. The results are as follows: similarly to Example 1B, the amount of unreacted polymerizable compounds remaining after 60 minutes of ultraviolet irradiation in Examples 5B to 8B is less than the detection limit, the polymerization rate is higher than that in Comparative Example 1, and the change in pretilt angle is sufficiently smaller than that in Comparative Example 2. In addition, compared with Comparative Examples 1 and 2, the VHR of Examples 5B to 8B after 60 minutes of ultraviolet irradiation also shows a sufficiently high value. Furthermore, in Examples 5B to 8B, no precipitation of polymerizable compounds after storage at room temperature for 240 hours was confirmed. It can be confirmed that the liquid crystal compositions containing polymerizable compounds of Examples 5B to 8B also solve the subject of the present invention.

[0755] (Examples 9B to 12B)

[0756] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound with respect to 99.7 parts by mass of the liquid crystal composition LC-002 was referred to as Example 9B.

[0757] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound with respect to 99.7 parts by mass of the liquid crystal composition LC-003 was referred to as Example 10B.

[0758] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-004 was referred to as Example 11B.

[0759] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-1a) was added as a polymerizable compound with respect to 99.7 parts by mass of the liquid crystal composition LC-005 was referred to as Example 12B.

[0760] The same evaluation as in Example 1B was also performed on the liquid crystal compositions containing polymerizable compounds of Examples 9B to 12B. The results showed that the amount of unreacted polymerizable compounds remaining after 150 seconds of ultraviolet irradiation and 15 minutes of ultraviolet irradiation in all Examples 9B to 12B was the same as that in Example 1B and less than that in Comparative Example 1. In addition, the amount of unreacted polymerizable compounds remaining after 60 minutes of ultraviolet irradiation in Examples 9B to 12B was also less than the detection limit, as in Example 1B. Therefore, it is suggested that the polymerization rate of Examples 9B to 12B is higher than that of Comparative Example 1. In addition, Examples 9B to 12B all showed the same amount of change in pretilt angle as in Example 1B, suggesting that the amount of change in pretilt angle is sufficiently small compared to Comparative Example 2. In addition, the VHR of Examples 9B to 12B after 60 minutes of ultraviolet irradiation was the same as that of Example 1B, and the VHR after 60 minutes of ultraviolet irradiation showed a sufficiently high value compared to Comparative Examples 1 and 2. Furthermore, in Examples 9B to 12B, no precipitation of the polymerizable compound was observed after storage at room temperature for 240 hours. This confirmed that the polymerizable compound-containing liquid crystal compositions of Examples 9B to 12B solved the problem of the present invention.

[0761] (Examples 13B to 16B)

[0762] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-31a) was added as a polymerizable compound with respect to 99.7 parts by mass of the liquid crystal composition LC-002 was referred to as Example 13B.

[0763] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-31a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-003 was referred to as Example 14B.

[0764] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-31a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-004 was referred to as Example 15B.

[0765] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-31a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-005 was referred to as Example 16B.

[0766] The same evaluation as in Example 3B was also performed on the liquid crystal compositions containing polymerizable compounds of Examples 13B to 16B. The results showed that the amount of unreacted polymerizable compounds remaining after 150 seconds of ultraviolet irradiation and 15 minutes of ultraviolet irradiation in all Examples 13B to 16B was the same as that in Example 3B and less than that in Comparative Example 1. In addition, the amount of unreacted polymerizable compounds remaining after 60 minutes of ultraviolet irradiation in Examples 13B to 16B was less than the detection limit, as in Example 3B. Therefore, it is suggested that the polymerization rate of Examples 13B to 16B is higher than that of Comparative Example 1. In addition, Examples 13B to 16B all showed the same amount of change in pretilt angle as in Example 3B, suggesting that the amount of change in pretilt angle is sufficiently small compared to Comparative Example 2. In addition, the VHR of Examples 13B to 16B after 60 minutes of ultraviolet irradiation was the same as that of Example 3B, and the VHR after 60 minutes of ultraviolet irradiation showed a sufficiently high value compared to Comparative Examples 1 and 2. Furthermore, in Examples 13B to 16B, no precipitation of the polymerizable compound was observed after storage at room temperature for 240 hours. This confirmed that the polymerizable compound-containing liquid crystal compositions of Examples 13B to 16B solved the problem of the present invention.

[0767] (Examples 17B to 20B)

[0768] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-33a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-002 was referred to as Example 17B.

[0769] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-33a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-003 was referred to as Example 18B.

[0770] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-33a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-004 was referred to as Example 19B.

[0771] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-33a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-005 was referred to as Example 20B.

[0772] The same evaluation as in Example 4B was also performed on the liquid crystal compositions containing polymerizable compounds of Examples 17B to 20B. The results showed that the amount of unreacted polymerizable compounds remaining after 150 seconds of ultraviolet irradiation and 15 minutes of ultraviolet irradiation in all Examples 17B to 20B was the same as that in Example 4B and less than that in Comparative Example 1. In addition, the amount of unreacted polymerizable compounds remaining after 60 minutes of ultraviolet irradiation in Examples 17B to 20B was also less than the detection limit, as in Example 4B. Therefore, it is suggested that the polymerization rate of Examples 17B to 20B is higher than that of Comparative Example 1. In addition, Examples 17B to 20B all showed the same amount of change in pretilt angle as in Example 4B, suggesting that the amount of change in pretilt angle is sufficiently small compared to Comparative Example 2. In addition, the VHR of Examples 17B to 20B after 60 minutes of ultraviolet irradiation was the same as that of Example 4B, and the VHR after 60 minutes of ultraviolet irradiation showed a sufficiently high value compared to Comparative Examples 1 and 2. Furthermore, in Examples 17B to 20B, no precipitation of the polymerizable compound was observed after storage at room temperature for 240 hours. This confirmed that the polymerizable compound-containing liquid crystal compositions of Examples 17B to 20B solved the problem of the present invention.

[0773] (Examples 21B to 22B)

[0774] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-2a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-001 was referred to as Example 21B.

[0775] A polymerizable compound-containing liquid crystal composition to which 0.3 parts by mass of the compound represented by formula (i-18a) was added as a polymerizable compound relative to 99.7 parts by mass of the liquid crystal composition LC-001 was referred to as Example 22B.

[0776] [Chemistry 111]

[0777]

[0778] The same evaluation as in Example 1B was also performed on the liquid crystal compositions containing polymerizable compounds of Examples 21B to 22B. The results showed that the amount of unreacted polymerizable compounds remaining after 150 seconds of ultraviolet irradiation and 15 minutes of ultraviolet irradiation in all Examples 21B to 22B was the same as that in Example 1B and less than that in Comparative Example 1. In addition, the amount of unreacted polymerizable compounds remaining after 60 minutes of ultraviolet irradiation in Examples 21B to 22B was also less than the detection limit, as in Example 1B. Therefore, it is suggested that the polymerization rate of Examples 21B to 22B is higher than that of Comparative Example 1. In addition, Examples 21B to 22B all showed the same amount of change in pretilt angle as in Example 1B, suggesting that the amount of change in pretilt angle is sufficiently small compared to Comparative Example 2. In addition, the VHR of Examples 21B to 22B after 60 minutes of ultraviolet irradiation was the same as that of Example 1B, and the VHR after 60 minutes of ultraviolet irradiation showed a sufficiently high value compared to Comparative Examples 1 and 2. Furthermore, in Examples 21B to 22B, no precipitation of the polymerizable compound was observed after storage at room temperature for 240 hours. This confirmed that the polymerizable compound-containing liquid crystal compositions of Examples 21B to 22B solved the problem of the present invention.

Claims

1. A liquid crystal composition containing a polymerizable compound, comprising one or more polymerizable compounds represented by general formula (i), In the formula, A i1 A represents a group selected from the following groups (b); i2 represents a group selected from the group consisting of the following groups (a) and (b), (a) 1,4-cyclohexylene, in which one -CH2- or two or more non-adjacent -CH2- groups may be replaced by -O-, (b) 1,4-phenylene, in which one -CH= or two or more non-adjacent -CH= groups may be substituted with -N=, and The group (a) and the group (b) may be substituted independently by an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a halogen group, a cyano group or a nitro group. P i1 and P i2 Each independently represents a group selected from the group consisting of formula (R-1), formula (R-4) and formula (R-8), In the formula, R 11 represents any one of an alkyl group having 1 to 5 carbon atoms or a hydrogen atom, S i1 and S i2 Each independently represents a single bond, R i1 represents a hydrogen atom, n i1 Indicates 1, 2, or 3, In the presence of multiple A i2 and / or S i2 In the case of , they may be the same or different.

2. The liquid crystal composition containing a polymerizable compound according to claim 1, which contains one or more of n in the general formula (i): i1 It represents a polymerizable compound of 1.

3. The liquid crystal composition containing a polymerizable compound according to claim 1 or 2, further comprising one or more compounds selected from the group consisting of compounds represented by general formulae (N-1a) to (N-1g), In the formula, R N11 and R N12Each independently represents an alkyl group having 1 to 8 carbon atoms, and one or two or more non-adjacent -CH2- in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-, n Na11 Indicates 0 or 1, n Nb11 Indicates 1 or 2, n Nc11 Indicates 0 or 1, n Nd11 Indicates 1 or 2, n Ne11 Indicates 1 or 2, n Nf12 Indicates 1 or 2, n Ng11 Indicates 1 or 2, A Ne11 represents trans-1,4-cyclohexylene or 1,4-phenylene, A Ng11 represents trans-1,4-cyclohexylene, 1,4-cyclohexenylene or 1,4-phenylene, but in n Nd11 When the number is 2, at least 1 A Ng11 represents 1,4-cyclohexenylene, Z Ne11 represents a single bond or ethylene, but at least one Z in the molecule Ne11 Represents ethylene, multiple A in the molecule Ne11 , Z Ne11 , and / or A Ng11 Can be the same or different.

4. The liquid crystal composition containing a polymerizable compound according to claim 1 or 2, further comprising one or more compounds represented by the general formula (N-1-14), In the formula, R N1141 and R N1142 Each independently represents an alkyl group having 1 to 8 carbon atoms, and one or two or more non-adjacent -CH2- groups in the alkyl group may be independently replaced by -CH=CH-, The residue is substituted with -C=C-, -O-, -CO-, -COO- or -OCO-.

5. The liquid crystal composition containing a polymerizable compound according to any one of claims 1 or 2, further comprising one or more compounds selected from the group consisting of compounds represented by general formula (L), [Chemistry 4] In the formula, R L1 and R L2Each independently represents an alkyl group having 1 to 8 carbon atoms, and one or two or more non-adjacent -CH2- groups in the alkyl group may be independently substituted by -CH=CH-, -C≡C-, -O-, -CO-, -COO- or -OCO-. n L1 represents 0, 1, 2 or 3, A L1 , A L2 and A L3 Each independently represents a group selected from the group consisting of the following groups (a), (b), and (c): (a) 1,4-cyclohexylene, in which one -CH2- or two or more non-adjacent -CH2- groups may be replaced by -O-, (b) 1,4-phenylene, wherein one -CH= or two or more non-adjacent -CH= groups in the group may be substituted by -N=, and (c) naphthalene-2,6-diyl, 1,2,3,4-tetrahydronaphthalene-2,6-diyl or decahydronaphthalene-2,6-diyl, one -CH= or two or more non-adjacent -CH= groups in naphthalene-2,6-diyl or 1,2,3,4-tetrahydronaphthalene-2,6-diyl may be substituted with -N=, The group (a), group (b) and group (c) may also be independently substituted by a cyano group, a fluorine atom or a chlorine atom. Z L1 and Z L2 Each independently represents a single bond, -CH2CH2-, -(CH2)4-, -OCH2-, -CH2O-, -COO-, -OCO-, -OCF2-, -CF2O-, -CH=N-N=CH-, -CH=CH-, -CF=CF- or -C≡C-, When n L1 There are multiple A's for 2 or 3 L2 In the case of L1 There are multiple Zs for 2 or 3 L2 In the case of , they may be the same or different. 6 . A liquid crystal display element using the liquid crystal composition containing a polymerizable compound according to claim 1 . 7 . An active-matrix driven liquid crystal display element, comprising the liquid crystal composition containing a polymerizable compound according to claim 1 . 8 . A liquid crystal display element for a PSA mode, a PSVA mode, a PS-IPS mode, or a PS-FFS mode, comprising the liquid crystal composition containing a polymerizable compound according to claim 1 .

9. A polymerizable compound represented by the general formula (i): [Chemistry 5] In the formula, A i1 A represents a group selected from the following groups (b); i2 represents a group selected from the group consisting of the following groups (a) and (b), (a) 1,4-cyclohexylene, in which one -CH2- or two or more non-adjacent -CH2- groups may be replaced by -O-, (b) 1,4-phenylene, in which one -CH= or two or more non-adjacent -CH= groups may be substituted with -N=, and The group (a) and the group (b) may be substituted independently by an alkyl group having 1 to 8 carbon atoms, an alkoxy group having 1 to 8 carbon atoms, a halogen group, a cyano group or a nitro group. P i1 and P i2 Each independently represents a group selected from the group consisting of formula (R-1), formula (R-4) and formula (R-8), In the formula, R 11 represents any one of an alkyl group having 1 to 5 carbon atoms or a hydrogen atom, S i1 and S i2 Each independently represents a single bond, R i1 represents a hydrogen atom, n i1 Indicates 1, 2, or 3, In the presence of multiple A i2 and / or S i2 In the case of , they may be the same or different.

Citation Information

Patent Citations

  • Liquid crystal composition containing polymerizable compound and liquid crystal display element using the same

    JP2011202168A

  • Polymerizable compounds and their use in liquid crystal displays

    JP2013509457A

  • Liquid crystal composition and liquid crystal display element

    WO2010084823A1

  • Liquid crystal composition containing polymerizable compound and liquid crystal display element using same

    CN102395651A

  • Compound having four polymerizable groups, liquid crystal composition, and liquid crystal display element

    CN104245757A