Method for measuring wafer geometric parameters and thickness of mask layer on wafer
By suspending the wafer with an air-floating chuck and combining it with laser and capacitive sensor measurements, the problem of measurement errors caused by artifacts on the surface of the clamping tool or chuck is solved, and the measurement precision and accuracy of wafer thickness and warpage are improved.
Patent Information
- Application Number
- CN202011569092.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-09-02
- Filing Date
- 2020-12-25
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2040-12-25
Smart Images

Figure CN112864075B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of wafer measurement technology, and in particular to a method for measuring wafer geometric parameters and the thickness of a mask layer on a wafer. Background Art
[0002] The geometric parameters of wafers, such as wafer shape, wafer thickness, and wafer flatness, play a vital role in the quality of wafers. Therefore, measuring the geometric parameters of wafers is an important task in evaluating the quality of wafers. Usually, the wafer is fixed vertically in the measurement light path by clamping, or the wafer is adsorbed onto a chuck by vacuum adsorption to measure the wafer geometric parameters.
[0003] However, the above measurement method has certain defects. For example, in the clamping method, the clamping force is too strong, which can easily change the original shape of the wafer. In addition, since the cleanliness of the clamping tool is difficult to guarantee, it is also easy to produce debris particles or other contaminants on the wafer. In the vacuum adsorption method, the surface of the chuck itself may have artifacts or marks, etc., which will cause large measurement errors in the measurement of the wafer's geometric parameters. Summary of the invention
[0004] In view of this, an embodiment of the present application provides a method for measuring wafer geometric parameters and the thickness of a mask layer on a wafer, thereby avoiding large measurement errors in the measurement of wafer geometric parameters caused by artifacts or marks on the surface of a clamping tool or chuck.
[0005] The first aspect of the present application provides a method for measuring the thickness of a wafer. The method for measuring the thickness of a wafer includes: using an air-floating chuck to suspend the wafer at a predetermined distance D above the top surface of the air-floating chuck, where D≥0; using a laser and a position sensor to measure the position information of a first position point on the front side of the wafer to obtain a position sensor reading Vx, where the front side of the wafer is the surface of the wafer away from the air-floating chuck; using a capacitive sensor to measure the position information of a second position point on the back side of the wafer to obtain a capacitive sensor reading CPn, where the first position point and the second position point are two relative position points in the wafer that characterize the thickness, and the back side of the wafer is the surface of the wafer close to the air-floating chuck; obtaining the thickness T of the wafer based on Vx and CPn 晶圆 , T 晶圆 is the distance between the first position point and the second position point on the wafer.
[0006] In one embodiment of the present application, the thickness T of the wafer is obtained according to Vx and CPn. 晶圆 , including: Determine the formula T 晶圆=T0+(CP0-CPn)+S*(Vx–V0), where T0 in the formula is the thickness of the first standard wafer, CP0 is the reference capacitance sensor reading of the first standard wafer at the reference predetermined distance, V0 is the reference position sensor reading of the first standard wafer at the reference predetermined distance, S is the slope of the straight line in the relationship diagram with the horizontal coordinate Vx and the vertical coordinate being the difference hx between CPn and CP0; Substitute Vx and CPn into the formula to calculate the thickness T of the wafer 晶圆 .
[0007] In one embodiment of the present application, the above determination formula T 晶圆 =T0+(CP0-CPn)+S* (Vx–V0), including: using an air floating chuck to suspend the first standard wafer at different predetermined distances above the top surface of the air floating chuck; using a position sensor to measure the position information of a third position point on the first surface of the first standard wafer when the first standard wafer is at different predetermined distances, so as to obtain a position sensor reading Vx, wherein the first surface of the first standard wafer is a surface of the standard wafer away from the air floating chuck; using a capacitance sensor to measure the position information of a fourth position point on the second surface of the first standard wafer when the first standard wafer is at different predetermined distances, so as to obtain a capacitance sensor reading CPn, wherein the second surface of the first standard wafer is a surface of the first standard wafer close to the air floating chuck, the fourth position point and the third position point are two relative position points in the first standard wafer that characterize the thickness, the different predetermined distances include a reference predetermined distance, and the reference capacitance sensor reading when the first standard wafer is at the reference predetermined distance is CP0 and the reference position sensor reading is V0; construct a relationship diagram with the horizontal coordinate Vx and the vertical coordinate hx of the difference between CPn and CP0 to determine the slope S of the straight line from the straight line in the relationship diagram; determine the formula T according to T0, CP0 and S 晶圆 =T0+(CP0-CPn)+S*(Vx–V0).
[0008] In one embodiment of the present application, the reference predetermined distance is the distance between the second surface of the first standard wafer and the top surface of the air floating chuck when the first standard wafer is vacuum sucked onto the air floating chuck by means of the air floating chuck, or the reference predetermined distance is the distance between the second surface of the first standard wafer and the top surface of the air floating chuck when the first standard wafer is suspended at any position above the top surface of the air floating chuck by means of the air floating chuck.
[0009] The second aspect of the present application provides a method for measuring the warpage of a wafer. The method for measuring the warpage of a wafer includes: using at least one tilting stage to adjust the tilt angle of an air-floating chuck multiple times to form multiple tilted wafers and the multiple tilted wafers meet the slope requirements of the interferometer measurement, and at least one tilting stage is located below the air-floating chuck; measuring the corresponding thicknesses at multiple positions on the multiple tilted wafers according to any wafer thickness measurement method provided in the first aspect of the present application; combining the corresponding thicknesses at multiple positions to form a two-dimensional or three-dimensional image of the wafer; and obtaining the warpage of the wafer using the two-dimensional or three-dimensional image of the wafer.
[0010] The third aspect of the present application provides a method for measuring the thickness of a mask layer on a wafer. The method for measuring the thickness of a mask layer on a wafer comprises: measuring the thickness T of the wafer before the mask according to any wafer thickness measurement method provided in the first aspect of the present application; 晶圆掩膜前 ; using the suction force provided by the air floating chuck to adjust the back side of the wafer after the mask so that the back side of the wafer after the mask matches the back side of the wafer before the mask, the wafer after the mask is a wafer after a mask layer is added to the surface of the wafer before the mask; using the supporting force provided by the air floating chuck to adjust the wafer after the mask to float at the same predetermined distance between the top surface of the air floating chuck and the wafer before the mask; measuring the thickness T of the wafer after the mask according to any one of the wafer thickness measurement methods provided in the first aspect of the present application 晶圆掩膜后 ; By adding T 晶圆掩膜后 Subtract T 晶圆掩膜前 Get the thickness of the mask layer.
[0011] In one embodiment of the present application, any one of the wafer thickness measurement methods provided in the first aspect of the present application measures the thickness T of the wafer before the mask. 晶圆掩膜前 Previously, the method for measuring the thickness of the mask layer on the wafer also included: using the suction provided by the air floating chuck to adjust the back side of the wafer before the mask so that the back side of the wafer before the mask matches the top surface of the air floating chuck, the back side of the wafer before the mask being the surface of the wafer before the mask close to the air floating chuck; using the supporting force provided by the air floating chuck to adjust the wafer before the mask to be suspended at a predetermined distance from the top surface of the air floating chuck; wherein, the above-mentioned use of the suction provided by the air floating chuck to adjust the back side of the wafer after the mask so that the back side of the wafer after the mask matches the back side of the wafer before the mask includes: using the suction provided by the air floating chuck to adjust the back side of the wafer after the mask so that the back side of the wafer after the mask matches the top surface of the air floating chuck.
[0012] The fourth aspect of the present application provides a method for measuring the thickness of a wafer, which includes: receiving a position sensor reading Vx obtained by measuring the position information of a first position point on the front side of the wafer using a laser and a position sensor, wherein the wafer is suspended at a predetermined distance above the top surface of an air-floating chuck, and the front side of the wafer is the surface of the wafer away from the air-floating chuck; receiving a capacitive sensor reading CPn obtained by measuring the position information of a second position point on the back side of the wafer using a capacitive sensor, the first position point and the second position point are two relative position points in the wafer that characterize the thickness, and the back side of the wafer is the surface of the wafer close to the air-floating chuck; and obtaining the thickness T wafer of the wafer based on Vx and CPn.
[0013] The fifth aspect of the present application provides a wafer thickness measuring device, which includes: a receiving module, which is used to receive a position sensor reading Vx obtained by measuring the position information of a first position point on the front side of the wafer using a laser and a position sensor, wherein the wafer is placed on the top surface of an air-floating chuck, and the front side of the wafer is the surface of the wafer away from the air-floating chuck; and is also used to receive a capacitive sensor reading CPn obtained by measuring the position information of a second position point on the back side of the wafer using a capacitive sensor, wherein the first position point and the second position point are two relative position points in the wafer that characterize the thickness, and the back side of the wafer is the surface of the wafer close to the air-floating chuck; and an acquisition module, which is used to acquire the thickness T of the wafer according to Vx and CPn. 晶圆 .
[0014] The sixth aspect of the present application provides a computer-readable storage medium, characterized in that computer executable instructions are stored thereon, and when the executable instructions are executed by a processor, the wafer thickness measurement method as described in claim 9 is implemented.
[0015] According to the technical solution provided in the embodiment of the present application, the wafer is suspended at a predetermined distance D above the top surface of the air floating chuck by using an air floating chuck, where D≥0; the position information of a first position point on the front side of the wafer is measured by using a laser and a position sensor to obtain a position sensor reading Vx, where the front side of the wafer is the surface of the wafer away from the air floating chuck; the position information of a second position point on the back side of the wafer is measured by using a capacitive sensor to obtain a capacitive sensor reading CPn, where the first position point and the second position point are two relative position points in the wafer that characterize the thickness, and the back side of the wafer is the surface of the wafer close to the air floating chuck; the thickness T of the wafer is obtained according to Vx and CPn 晶圆 , T 晶圆 is the distance between the first position point and the second position point on the wafer. The embodiment of the present application can avoid large measurement errors caused by artifacts or traces on the surface of the clamping tool or chuck in measuring the wafer thickness. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1a A schematic diagram of a wafer thickness measurement method provided according to an embodiment of the present application is shown;
[0017] Figure 1b A schematic diagram of a method for obtaining wafer thickness is shown;
[0018] Figure 1c A schematic diagram showing a method for determining a formula used for wafer thickness;
[0019] Figure 1d A schematic diagram showing calibration of a position sensor;
[0020] Figure 1e A schematic diagram showing the relationship between the position sensor reading Vx and the capacitance sensor reading CPn during the calibration process of the position sensor is shown;
[0021] Figure 1f A schematic diagram showing the positions of a position sensor and a capacitive sensor relative to a wafer is shown;
[0022] Figure 2a A schematic diagram of a method for measuring wafer warpage according to an embodiment of the present application is shown;
[0023] Figure 2b A schematic diagram showing that a wafer in a vertical position is susceptible to deformation when the wafer is tilted;
[0024] Figure 2c A schematic structural diagram of an exemplary goniometer for measuring a wafer tilt platform with a designed pattern is shown;
[0025] Figure 3a A schematic diagram showing a method for measuring the thickness of a mask layer on a wafer provided according to an embodiment of the present application is shown;
[0026] Figure 3b A schematic diagram of a method for measuring the thickness of a mask layer on a wafer provided according to another embodiment of the present application is shown.
[0027] Figure 4 A schematic diagram showing a method for measuring wafer thickness is shown;
[0028] Figure 5 A schematic diagram of a method for measuring wafer warpage according to an embodiment of the present application is shown;
[0029] Figure 6 A schematic diagram of a method for measuring flatness of a double-polished wafer provided according to an embodiment of the present application is shown;
[0030] Figure 7a A schematic diagram of the structure of a device based on a double Fizeau interferometer is shown;
[0031] Figure 7b A schematic diagram of the structure of a device based on a shearing interferometer is shown.
[0032] Figure 7c A schematic diagram of a structure for measuring wafer geometric parameters is shown;
[0033] Figure 8a A schematic top view of an air flotation chuck is shown;
[0034] Figure 8b A schematic top view of another air flotation chuck is shown;
[0035] Figure 8c A schematic diagram showing a pressure nozzle and vacuum nozzle connection layer of an air flotation chuck is shown;
[0036] Figure 8d A schematic side view of a stacking structure of air-floating chucks is shown;
[0037] Figure 8e A schematic side view of another stacking structure of air-floating chucks is shown;
[0038] Figure 8f Shows Figure 8e a top surface of a top plate of a mid-stack structure;
[0039] Figure 8g Shows Figure 8e a bottom surface of a top plate of a mid-stack structure;
[0040] Figure 8h Shows Figure 8e A top view of an exemplary manifold in a stacked structure;
[0041] Figure 8i Shows Figure 8e A bottom view of an exemplary manifold in a stacked structure;
[0042] Figure 8j Shows Figure 8e A top view of the rear cover plate of the stacking structure;
[0043] Figure 8k Shows Figure 8e A bottom view of the rear cover plate of the middle stacking structure;
[0044] Figure 9a and Figure 9b A schematic structural diagram of an exemplary diversion chamber is shown.
[0045] Fig.10a and Fig.10b Shows a method of using Figure 7cA schematic diagram of a method for performing wafer shape measurement using the architecture shown;
[0046] Fig.11a and Fig.11b Shows a method of using Figure 7c Schematic diagram of the method for measuring wafer flatness TTV using the architecture shown;
[0047] Fig.12a A schematic diagram showing chuck marks / artifacts as the wafer is drawn down onto the vacuum chuck by the vacuum;
[0048] Figure 12b A schematic diagram showing a wafer suspended above an air-floating chuck with no chuck marks / artifacts;
[0049] Figures 13a-13c A schematic diagram showing a method of distinguishing real features from chuck marks / artifacts on the surface of a wafer. DETAILED DESCRIPTION
[0050] The following will combine the drawings required for use in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the drawings described below are only part of the embodiments of the present application, rather than all of the embodiments.
[0051] It should be noted that, based on the embodiments in this application, all related embodiments obtained by ordinary technicians in this field without making any creative work are within the scope of protection of this application.
[0052] In this article, "wafer geometry" can refer to wafer shape parameters or local flatness parameters (also known as local flatness parameters, such as site flatness (SFQR), site flatness back ideal range (SBIR), global flatness (GBIR)). Wafer flatness is also called total thickness variation (TTV) and can refer to high-density raw data (≥4M pixels / wafer) that can be used to derive SFQR, GBIR and many other related parameters. Flatness data is usually associated with the front and back information of the wafer. For example, wafer shape parameters can be derived from a height map of a single surface, which can be the front or back of the wafer, or an intermediate surface between the two surfaces (wafer shape defined by Semiconductor Equipment and Materials International (SEMI)). For advanced 300mm wafers, the difference between the intermediate values of the front and back shapes, the front only or the back only is very small. This is because the wafer shape is in the order of several microns to hundreds of microns, while TTV or GBIR is in the order of tens or hundreds of nanometers. In wafer geometry parameter measurement equipment with designed patterns, the wafer shape can be calculated from the front side or the back side, depending on the supplier.
[0053] Figure 1a A schematic diagram of a wafer thickness measurement method provided according to an embodiment of the present application is shown. The wafer thickness measurement method can be performed using a wafer measurement device, wherein the wafer measurement device can include an air floating chuck, a laser, a capacitive sensor, and a position sensor. Figure 1a As shown, the wafer thickness measurement method includes the following steps.
[0054] S110: suspending the wafer at a predetermined distance D above the top surface of the air floating chuck by using the air floating chuck, where D≥0.
[0055] It should be understood that the value of the predetermined distance D can be 0 or other values, as long as the laser in the laser can be received by the position sensor after being reflected by the front side of the wafer. This application does not make any specific limitation on this.
[0056] S120: Using a laser and a position sensor to measure position information of a first position point on the front side of the wafer to obtain a position sensor reading Vx, where the front side of the wafer is a surface of the wafer away from the air floating chuck.
[0057] S130: Use a capacitive sensor to measure the position information of a second position point on the back side of the wafer to obtain a capacitive sensor reading CPn, where the first position point and the second position point are two relative position points in the wafer that represent the thickness, and the back side of the wafer is the surface of the wafer close to the air floating chuck.
[0058] It should be understood that the reading Vx of the position sensor can be calibrated using a wafer of known thickness, i.e., a first standard wafer. The position of the position sensor can be associated with the height of the top surface of the wafer. The capacitive sensor can measure the position of the bottom surface of the wafer. The combined information of the position of the top surface and the position of the bottom surface can be used to accurately determine the thickness of the wafer.
[0059] S140: Obtain the thickness T of the wafer based on Vx and CPn 晶圆 , T 晶圆 is the distance between the first position point and the second position point on the wafer.
[0060] According to the technical solution provided in the embodiment of the present application, the wafer is suspended at a predetermined distance D above the top surface of the air-floating chuck by using an air-floating chuck, so that the front and back sides of the wafer will not be contaminated by traditional clamping tools. In addition, by using a capacitive sensor, a laser and a position sensor to measure the thickness of the wafer, the measurement result of the wafer thickness is not affected by artifacts or traces on the top surface of the air-floating chuck, thereby improving the precision and accuracy of measuring the wafer thickness.
[0061] Figure 1b A schematic diagram showing a method for obtaining wafer thickness is shown. Figure 1b Steps S141-S142 in the illustrated embodiment are: Figure 1a An implementation of step S140 in the illustrated embodiment.
[0062] S141: Determine formula T 晶圆 =T0+(CP0-CPn)+S*(Vx–V0), wherein T0 in the formula is the thickness of the first standard wafer, CP0 is the reference capacitance sensor reading of the first standard wafer at the reference predetermined distance, V0 is the reference position sensor reading of the first standard wafer at the reference predetermined distance, and S is the slope of the straight line in the relationship diagram with Vx as the horizontal coordinate and hx as the vertical coordinate of the difference between CPn and CP0.
[0063] It should be understood that the values of T0, V0, and S can be known values stored in the wafer measurement device after calibration before leaving the factory, or can be values obtained after calibration using the first standard wafer when the wafer measurement device is used. This application does not make specific restrictions on this. The reference predetermined distance can be greater than or equal to 0. For example, the reference predetermined distance can be the distance between the first standard wafer and the air-floating chuck when the first standard wafer is adsorbed on the top surface of the air-floating chuck using the suction provided by the air-floating chuck, or can be the distance between the first standard wafer and the air-floating chuck when the first standard wafer is directly placed on the top surface of the air-floating chuck; it can also be the distance between the first standard wafer and the air-floating chuck when the first standard wafer is suspended at any distance on the top surface of the air-floating chuck using the air-floating chuck. This application does not make specific restrictions on the value of the reference predetermined distance.
[0064] S142: Substitute Vx and CPn into the formula to calculate the thickness T of the wafer 晶圆 .
[0065] According to the technical solution provided in the embodiment of the present application, by determining the formula T 晶圆 =T0+(CP0-CPn) +S*(Vx–V0), substitute Vx and CPn into the formula to calculate the thickness T of the wafer 晶圆 , so that the thickness of the wafer can be accurately calculated using the formula, which is also conducive to further clarifying the factors affecting the wafer thickness and improving the accuracy of wafer thickness measurement.
[0066] Figure 1c A schematic diagram showing a method for determining a formula used for wafer thickness. Figure 1c Steps S1411-S1415 in the illustrated embodiment are: Figure 1b An implementation of step S141 in the illustrated embodiment. The method for determining the formula used for wafer thickness includes the following steps.
[0067] S1411: Using an air floating chuck, suspend a first standard wafer at different predetermined distances above a top surface of the air floating chuck.
[0068] S1412: Use a position sensor to measure position information of a third position point on the first surface of the first standard wafer when the first standard wafer is at different predetermined distances to obtain a position sensor reading Vx, where the first surface of the first standard wafer is a surface of the first standard wafer away from the air floating chuck.
[0069] S1413: Use a capacitive sensor to measure the position information of a fourth position point on the second surface of the first standard wafer when the first standard wafer is at different predetermined distances to obtain a capacitive sensor reading CPn, wherein the second surface of the first standard wafer is the surface of the first standard wafer close to the air floating chuck, the fourth position point and the third position point are two relative position points in the first standard wafer that characterize the thickness, the different predetermined distances include a benchmark predetermined distance, and the benchmark capacitive sensor reading when the first standard wafer is at the benchmark predetermined distance is CP0 and the benchmark position sensor reading is V0.
[0070] In one embodiment of the present application, the reference predetermined distance is the distance between the second surface of the first standard wafer and the top surface of the air floating chuck when the first standard wafer is vacuum sucked onto the air floating chuck by means of the air floating chuck, or the reference predetermined distance is the distance between the second surface of the first standard wafer and the top surface of the air floating chuck when the first standard wafer is suspended at any position above the top surface of the air floating chuck by means of the air floating chuck.
[0071] S1414: Construct a relationship diagram with the horizontal coordinate Vx and the vertical coordinate hx of the difference between CPn and CP0 to determine the slope S of the straight line from the straight line in the relationship diagram.
[0072] S1415: Determine formula T based on T0, CP0 and S 晶圆 =T0+(CP0-CPn)+S*(Vx–V0).
[0073] For example, Figure 1d A schematic diagram showing the calibration of a position sensor is shown. Figure 1d The schematic diagram shows the relationship between the position sensor reading Vx and the capacitance sensor reading CPn during the calibration process of the position sensor. The wafer measurement device includes a capacitance sensor 130 , a laser (not shown), a position sensor 140 and a first standard wafer 161 . Figure 1d The elliptical structure in represents the light spot formed when the laser is irradiated onto the surface of the standard wafer 161 .
[0074] like Figure 1dAs shown, in order to calibrate the position sensor 140, the first standard wafer 161 can be adjusted up and down at various positions. In this example, although each wafer is slightly different, the thickness T0 of the first standard wafer 161 can be set to 725μm, the thickness T0 of the first standard wafer 161 can also be set to 775μm, or other thickness values, which are not specifically limited in this application. The thickness of the first standard wafer 161 can be measured by a coordinate measuring machine (CMM) or other thickness measuring tools. When the first standard wafer 161 is at position A0, it is at a reference predetermined distance (also referred to as zero suspension height). Position A0 can be the position of the first standard wafer 161 when the first standard wafer 161 is vacuumed onto the air-floating chuck, or it can be the position of the first standard wafer 161 when the first standard wafer 161 is suspended above the top surface of the air-floating chuck at a reference predetermined distance. The reference predetermined distance is greater than or equal to 0, which is not specifically limited in this application. And the reference capacitance sensor reading read by the capacitance sensor when the first standard wafer is at position A0 is CP0, and CP0 can be CP set to 0. Then the reference position sensor reading (V0 (±10V)) from the position sensor 140 can be read. After that, the vacuum and pressure can be adjusted to make the first standard wafer 161 suspended at position A1, and the capacitance sensor reading at position A1 is CP1, and CP1 minus CP0 is equal to 20μm (or approximately equal to 20μm). At the same time, the position sensor reading V1 when CP1-CP0 is equal to 20μm is recorded.
[0075] Next, the vacuum and pressure can be adjusted again until the first standard wafer 161 is suspended at position A2, and the reading of the capacitance sensor at position A2 is CP2, and CP2 minus CP0 is about 30μm. At the same time, the reading V2 of the position sensor when CP2-CP0 is about 30μm is recorded. The above steps can be repeated for the readings CP3, CP4, CP5, etc. of the capacitance sensor at 40μm, 50μm, 60μm, etc.
[0076] Next, Δ(CPn-CP0) can be calculated, such as CP1-CP0, CP2-CP0, etc. Table 1 shows exemplary results of the calculation.
[0077] Table 1
[0078]
[0079] Figure 1eThe diagram shows the relationship between the position sensor reading Vx and the capacitance sensor reading CPn during the calibration process of the position sensor. Based on the above data, a hx vs Vx diagram can be drawn, and a linear fit can be performed on the hx vs Vx diagram to obtain the slope Sμm / V (see Figure 1e ). Where hx is the difference between the capacitance sensor reading CPn and the reference capacitance sensor reading CP0, i.e., the relative wafer surface height. The calibration data includes: 1) slope, Sμm / V; 2) wafer thickness T0 = 725μm; 3) reference position sensor (or PSD) reading: V0; 4) reference capacitance sensor reading: CP0. The calibration data can be saved, and the software implementation of the calibration can be performed by using the following formula:
[0080] T 晶圆 =T0+ (CP0-CPn) +S*(Vx–V0)
[0081] Wherein, CPn is the reading of the capacitance sensor when the first standard wafer 161 is at a predetermined distance or levitation height.
[0082] CP0 may be a reading of the capacitance sensor when the first standard wafer 161 is vacuum-sucked onto the air-floating chuck.
[0083] Vx is the reading of the position sensor in volts.
[0084] The capacitance sensor reading in μm can be calculated based on the factory calibration constant C, where C = Δh / ΔV, μm / volt, and the capacitance sensor reading in μm CPn = C*ΔVcp.
[0085] According to the technical solution provided in the embodiment of the present application, by using a first standard wafer with a known thickness of T0, the position sensor can be calibrated at any time to avoid position deviation of the wafer measuring device or the presence of dust or other contaminants on the wafer measuring device, which may cause large errors in the values of CP0 and V0, thereby improving the precision and accuracy of wafer thickness measurement.
[0086] In one embodiment, a method of determining an optimal angle for a laser and / or position sensor is disclosed. Figure 1f A schematic diagram showing the positions of a position sensor and a capacitive sensor relative to a wafer is shown. Figure 1f The elliptical structure in represents the light spot formed when the laser is irradiated on the surface of the standard wafer 161. Figure 1fTo obtain the best Z-axis resolution, the position sensor 140 is preferably located at a position permitted by the size of the position sensor and at a position with a maximum angle β with the first standard wafer 161. If Δh is the Z-axis resolution (or z-sensitivity), the angle β is dominant.
[0087] Δh=ΔL*Cosβ / (2Cosα)
[0088] Here, ΔL is the minimum displacement detectable by the position sensor 140 . The position sensor 140 may be some commercially available sensors. For example, the minimum displacement of the sensor may be about 0.75 μm.
[0089] Δh=ΔL / M
[0090] Among them, M=[Cosβ / (2Cos(α))]^-1.
[0091] Due to the influence of the grazing angle α, Cos(α) is approximately equal to 1, where α is the light source (such as a laser ( Figure 1f The angle between the position sensor 140 (not shown) and the first standard wafer 161 is typically set to 10-15°. As β increases, based on the above formula, it can be seen that M will also increase, which means that the sensitivity of the position sensor 140 will also increase. However, due to the potential amplification effect on the spot size on the detector in the position sensor (for example, the size of the spot cannot be larger than the size that the detector can detect), β may not be too large. There may also be physical limitations related to how far the position sensor can be placed in the device. For example, at this grazing angle, the spot size of the laser on the sensor surface can be increased by 1 / Sin(90°-β) =1 / Sin30°. Table 2 below lists various PSD resolutions based on different angles α and β, in nm.
[0092] Table 2
[0093]
[0094] Figure 2a A schematic diagram of a method for measuring wafer warpage according to an embodiment of the present application is shown. The method for measuring wafer warpage includes the following steps.
[0095] S210: using at least one tilting stage to adjust the tilt angle of the air-floating chuck multiple times to form a plurality of tilted wafers, and the plurality of tilted wafers meet the slope requirement of interferometer measurement, wherein the at least one tilting stage is located below the air-floating chuck.
[0096] It should be understood that the tilting platform can be a tilting platform or a swinging slide, etc., as long as it can achieve tilting, and this application does not make specific restrictions on this. The number of tilting platforms can be one, two or even more, and this application does not make specific restrictions on this. The tilting angle can be 1°, 5°, 10°, or even 80° or other, and this application does not make specific restrictions on the value of the tilting angle.
[0097] S220: Measure the corresponding thicknesses at multiple positions on the multiple tilted wafers according to any wafer thickness measurement method in the above embodiments of the present application.
[0098] It should be understood that the number of position points can be 10, 20 or even more, as long as the corresponding thicknesses at multiple position points can reflect the warpage of the wafer after being combined. The present application does not make any specific restrictions on the number of position points. Multiple position points can be located on the same diameter of the wafer, or on different diameters of the wafer. The present application does not make any specific restrictions on this. S230: Combine the corresponding thicknesses at multiple position points to form a two-dimensional or three-dimensional image of the wafer.
[0099] It should be understood that when multiple position points are located on the same diameter of the wafer, the corresponding thicknesses at the multiple position points can form a two-dimensional image of the wafer corresponding to the diameter. When multiple position points are located on different diameters of the wafer, the corresponding thicknesses at the multiple position points can form a three-dimensional image of the wafer. As long as the warping of the wafer can be reflected, the present application does not make any specific limitations on this.
[0100] S240: Obtain the warpage of the wafer using a two-dimensional or three-dimensional image of the wafer.
[0101] According to the technical solution provided by the embodiment of the present application, by using at least one tilting table to adjust the tilt angle of the air-floating chuck multiple times to form multiple tilted wafers and the multiple tilted wafers meet the slope requirements of the interferometer measurement, the thickness at any position on the wafer can be measured, avoiding the position of the wafer with a larger warpage being ignored due to being blocked, increasing the measurement range of the wafer warpage, and thus effectively improving the precision and accuracy of measuring the wafer warpage. For wafers with a larger warpage, the two-dimensional tilting platform such as the Z-shaped deflection table in the method of the present application can be used to overcome the dynamic range limitation of the interferometer. In addition, according to any of the wafer thickness measurement methods in the above embodiments of the present application, the corresponding thicknesses at multiple positions on the multiple tilted wafers are measured; the corresponding thicknesses at multiple positions are combined to form a two-dimensional or three-dimensional wafer image; the warpage of the wafer is obtained using the two-dimensional or three-dimensional wafer image, so that the measurement result of the wafer thickness is not affected by the contamination of the clamping tool or the artifacts or traces on the top surface of the air-floating chuck, thereby improving the precision and accuracy of measuring the wafer thickness.
[0102] Figure 2b Schematic diagram showing that a wafer 1' in a vertical position is susceptible to deformation when the wafer is tilted. When tilted, the shape of a wafer 1 in a horizontal position can be better maintained than the same wafer 1' in a vertical position. Figure 2b As shown in FIG. 1 , in the case of the same wafer 1' in a vertical position, if the wafer 1' is not completely vertical, gravity can change the shape of the wafer 1'. This is because when the vertically clamped wafer 1' tilts, a torque T is applied to the wafer 1'. This torque will change the shape of the wafer. This limits the measurement accuracy of the traditional double Fizeau interferometer device. In contrast, Figure 2b As shown in the horizontal setting, the architecture of the present application supports the wafer 1 on a thin air cushion, which helps to maintain the natural shape of the wafer 1 even if the wafer 1 is at a small tilt angle (usually less than a fraction of a degree).
[0103] The architecture of the present application can be used to measure the warpage of thin wafers, where the wafer is too thin to be placed in a vertical position or too thin to maintain its shape when the wafer is tilted in a vertical position. For some thin wafers, it may be too thin to form support at two points on the edge of the wafer. In this architecture, the wafer is in a horizontal position and supported by an air cushion. When the wafer is tilted, a very small radial force is applied to the wafer to maintain the position of the wafer. Under appropriate suspension height, vacuum / air pressure settings, the warpage of thin wafers can be measured.
[0104] Therefore, the wafer geometry measurement equipment and the wafer geometry measurement equipment with designed patterns using the above method can have high accuracy and throughput, but the price is only half of that of the dual Fizeau architecture. This method is a cost-effective and high-precision solution for wafer flatness, nano-topography and shape measurement equipment for any size wafers such as 200mm, 300mm and 450mm.
[0105] Figure 2c The schematic diagram of an exemplary goniometer structure for measuring a wafer tilt platform with a design pattern is shown. The steps shown include two stacked goniometers 200, which are used to increase the dynamic range and throughput of wafer warpage. When tilting the wafer, the wafer focus can be maintained. It should be noted that the X and Y platforms 201 and 202 intersect at 90 degrees, and Figure 2c The X and Y platforms 201 and 202 are drawn on the same plane for the convenience of illustrating the common rotation center.
[0106] Figure 3a A schematic diagram of a method for measuring the thickness of a mask layer on a wafer provided according to an embodiment of the present application is shown. The method for measuring the thickness of a mask layer on a wafer includes the following steps.
[0107] S310: Measure the thickness T of the wafer before the mask according to any one of the wafer thickness measurement methods provided in the above embodiments of the present application. 晶圆掩膜前 .
[0108] S320: Using suction provided by the air floating chuck to adjust the back side of the masked wafer so that the back side of the masked wafer matches the back side of the pre-masked wafer, wherein the masked wafer is a wafer after a mask layer is added to the surface of the pre-masked wafer.
[0109] S330: Using the support force provided by the air floating chuck, adjust the wafer behind the mask to float at a predetermined distance that is the same as the top surface of the air floating chuck and the wafer before the mask.
[0110] It should be understood that in the embodiment of the present application, step S320 may be performed first and then step S330, or step S330 may be performed first and then step S320, and the present application does not make specific limitations on this. In step S330, the suction force and the supporting force provided by the air-floating chuck may also be used simultaneously to adjust the wafer in front of the mask to float at a predetermined distance from the top surface of the air-floating chuck, and the present application does not make specific limitations on this.
[0111] S340: Measure the thickness T of the wafer after masking according to any wafer thickness measurement method provided in the above embodiments of the present application. 晶圆掩膜后 .
[0112] S350: By integrating T 晶圆掩膜后 Subtract T 晶圆掩膜前 Get the thickness of the mask layer.
[0113] For example, in the 3D NAND process, the measurement of the thickness of the highly opaque hard mask (or film) is not met because traditional optical methods cannot be applied well to opaque films. The characteristics of wafer thickness measurement can be used to measure the thickness of the hard mask, such as two types of wafer thickness measurements, one is "pre-mask" (T 晶圆掩膜前 ) thickness measurement, one is the "behind the mask" thickness measurement (T 晶圆掩膜后 )). 晶圆掩膜前 =T0+E_RTE_pre
[0114] T 晶圆掩膜后 =T1+E_RTE-post
[0115] T0 and T1 are the thickness measurements before and after mask deposition, respectively. E_RTE_pre and E_RTE-post are the Ray Tracing Errors (RTE) before and after the wafer mask, respectively. Therefore, the thickness ΔT of the mask layer can be obtained by the following formula.
[0116] ΔT=T 晶圆掩膜后 –T 晶圆掩膜前 =(T1-T0)+(E_RTE-post-E_RTE_pre)
[0117] Because the wafer can warp dramatically after the mask is applied, RTE (ie, E_RTE-post-E_RTE_pre) can significantly affect T 晶圆掩膜前 and T 晶圆掩膜后 measurement results, resulting in significant errors in the ΔT calculation.
[0118] After the mask is applied to the surface of the wafer, the suction force generated by the air floating chuck can make the wafer substantially flat, so that the shape of the wafer before and after the mask is substantially the same, thereby minimizing RTE (i.e. ), and increase the accuracy of thickness measurement.
[0119] According to the technical solution provided in the embodiment of the present application, the air-floating chuck can be used to force the back of the wafer before the mask to match the back of the wafer after the mask, that is, the shape of the back of the wafer before the mask is equivalent to the shape of the back of the wafer after the mask. When the difference in film thickness is calculated by subtracting the thickness of the wafer before the film is deposited from the thickness of the wafer after the film is deposited, the ray tracing error will eventually be eliminated or reduced. When this method is applied to the thickness measurement of the opaque hard mask layer, it can greatly reduce or eliminate the ray tracing error caused by the highly warped wafer in the interferometer, thereby improving the accuracy of the thickness measurement of the mask layer applied on the wafer.
[0120] Figure 3b A schematic diagram of a method for measuring the thickness of a mask layer on a wafer provided according to another embodiment of the present application is shown. Figure 3b The embodiment shown is Figure 3a A variation of the embodiment shown in FIG. 3b, with Figure 3a The difference of the embodiment shown is that in the method for measuring the thickness of the mask layer on the wafer, steps S360-S370 are included before step S310, wherein step S321 corresponds to Figure 3a Step S320 in the illustrated embodiment.
[0121] S360: Using the suction provided by the air floating chuck, adjust the back side of the wafer in front of the mask so that the back side of the wafer in front of the mask matches the top surface of the air floating chuck, wherein the back side of the wafer in front of the mask is the surface of the wafer close to the air floating chuck.
[0122] S370: Using the support force provided by the air floating chuck, adjust the wafer in front of the mask to float at a predetermined distance from the top surface of the air floating chuck.
[0123] It should be understood that in the embodiment of the present application, step S360 may be performed first and then step S370, or step S360 may be performed first and then step S370, and the present application does not make specific limitations on this. In step S370, the suction force and support force provided by the air-floating chuck may also be used simultaneously to adjust the wafer in front of the mask to float at a predetermined distance from the top surface of the air-floating chuck, and the present application does not make specific limitations on this.
[0124] S321: Using the suction provided by the air floating chuck, adjust the back side of the masked wafer so that the back side of the masked wafer matches the top surface of the air floating chuck. The masked wafer is a wafer with a mask layer added to the surface of the pre-masked wafer.
[0125] According to the technical solution provided in the embodiment of the present application, an air floating chuck is used to force the back sides of the wafers before and after the mask to match the top surface of the air floating chuck, and the top surface of the air floating chuck is used as a reference to adjust the wafers before and after the mask, so as to better control the back sides of the wafers before and after the mask to have the same shape, thereby greatly reducing the ray tracing error caused by highly warped wafers and improving the accuracy of the thickness measurement of the mask layer applied on the wafer.
[0126] Figure 4 A schematic diagram of a wafer thickness measurement method provided according to an embodiment of the present application is shown. The wafer thickness measurement method is performed by a processor as an example. Figure 4 As shown, the wafer thickness measurement method includes the following steps.
[0127] S410: Receive a position sensor reading Vx obtained by measuring position information of a first position point on the front side of the wafer using a laser and a position sensor, wherein the wafer is placed on the top surface of an air floating chuck, and the front side of the wafer is the surface of the wafer away from the air floating chuck.
[0128] S420: Receive a capacitance sensor reading CPn obtained by measuring the position information of a second position point on the back side of the wafer using a capacitance sensor, wherein the first position point and the second position point are two relative position points in the wafer representing the thickness, and the back side of the wafer is the surface of the wafer close to the air floating chuck.
[0129] S430: Obtain the thickness T of the wafer according to Vx and CPn 晶圆 .
[0130] In one embodiment, step S430 includes: determining the formula T 晶圆=T0+(CP0-CPn)+S* (Vx–V0), where T0 in the formula is the thickness of the first standard wafer, CP0 is the reference capacitance sensor reading of the first standard wafer at the reference predetermined distance, V0 is the reference position sensor reading of the first standard wafer at the reference predetermined distance, S is the slope of the straight line in the relationship diagram with the horizontal coordinate Vx and the vertical coordinate being the difference hx between CPn and CP0; Substitute Vx and CPn into the formula to calculate the thickness T of the wafer 晶圆 It should be understood that the formula can be pre-stored in the memory, and the processor calls the formula from the memory to calculate the thickness T of the wafer. 晶圆 .
[0131] According to the technical solution provided in the embodiment of the present application, by receiving the position sensor reading Vx obtained by measuring the position information of the first position point on the front side of the wafer using a laser and a position sensor; receiving the capacitive sensor reading CPn obtained by measuring the position information of the second position point on the back side of the wafer using a capacitive sensor, the thickness T of the wafer is obtained according to Vx and CPn. 晶圆 , thereby measuring the thickness of the wafer. Since the wafer is suspended at a predetermined distance above the top surface of the air-floating chuck during the measurement process, the measurement result of the wafer thickness is not affected by artifacts or traces on the top surface of the air-floating chuck, and is not affected by traditional clamping tools, thereby improving the precision and accuracy of measuring the wafer thickness.
[0132] Figure 5 FIG. 1 is a schematic diagram of a wafer thickness measuring device provided according to an embodiment of the present application. Figure 5 As shown, the wafer thickness measuring device 500 includes a receiving module 510, which is used to receive a position sensor reading Vx obtained by measuring the position information of a first position point on the front side of the wafer using a laser and a position sensor, wherein the wafer is suspended at a predetermined distance above the top surface of the air-floating chuck, and the front side of the wafer is the surface of the wafer away from the air-floating chuck; and is also used to receive a capacitance sensor reading CPn obtained by measuring the position information of a second position point on the back side of the wafer using a capacitance sensor, wherein the first position point and the second position point are two relative position points in the wafer that characterize the thickness, and the back side of the wafer is the surface of the wafer close to the air-floating chuck; an acquiring module 520, which is used to acquire the thickness T of the wafer according to Vx and CPn. 晶圆 .
[0133] It should be understood that the receiving module 510 is communicatively connected with the position sensor and the capacitance sensor, so as to be able to receive the position sensor reading Vx and the capacitance sensor reading CPn.
[0134] According to the technical solution provided in the embodiment of the present application, the position sensor reading Vx and the capacitance sensor reading CPn are received by the receiving module, and the thickness T of the wafer is obtained according to Vx and CPn by the obtaining module. 晶圆 , thereby measuring the thickness of the wafer. Since the wafer is suspended at a predetermined distance above the top surface of the air-floating chuck during the measurement process, the measurement result of the wafer thickness is not affected by artifacts or traces on the top surface of the air-floating chuck, and is not affected by traditional clamping tools, thereby improving the precision and accuracy of measuring the wafer thickness.
[0135] Figure 6 A block diagram of a wafer thickness measurement system provided according to an embodiment of the present application is shown.
[0136] Reference Figure 6 The measurement system 600 includes a processing component 610, which further includes one or more processors, and a memory resource represented by a memory 620 for storing instructions executable by the processing component 610, such as an application. The application stored in the memory 620 may include one or more modules, each corresponding to a set of instructions. In addition, the processing component 610 is configured to execute instructions to perform the above-mentioned method of action authorization.
[0137] The measurement system 600 may also include a power supply component configured to perform power management of the measurement system 600, a wired or wireless network interface configured to connect the measurement system 600 to a network, and an input / output (I / O) interface. The measurement system 600 may operate based on an operating system stored in the memory 620, such as Windows Server™, Mac OSX™, Unix™, Linux™, FreeBSD™, or the like.
[0138] A non-temporary computer-readable storage medium, when the instructions in the storage medium are executed by the processor of the above-mentioned measurement system 600, enables the above-mentioned measurement system 600 to execute a wafer thickness measurement method, the method being executed by an agent program, the method comprising: receiving a position sensor reading Vx obtained by measuring position information of a first position point on the front side of the wafer using a laser and a position sensor, wherein the wafer is placed on the top surface of an air-floating chuck, and the front side of the wafer is the surface of the wafer away from the air-floating chuck; receiving a capacitance sensor reading CPn obtained by measuring position information of a second position point on the back side of the wafer using a capacitance sensor, wherein the first position point and the second position point are two relative position points in the wafer representing the thickness, and the back side of the wafer is the surface of the wafer close to the air-floating chuck; and obtaining the thickness T of the wafer according to Vx and CPn. 晶圆 .
[0139] Those of ordinary skill in the art will appreciate that the algorithmic steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professional and technical personnel can use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of this application.
[0140] In the several embodiments provided in this application, it should be understood that the disclosed methods, devices and systems can be implemented in other ways. For example, the device embodiments described above are only schematic, for example, the division of the modules is only a logical function division, and there may be other division methods in actual implementation, for example, multiple modules can be combined or integrated into another system, or some features can be ignored or not executed.
[0141] If the function is implemented in the form of a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, the technical solution of the present application can be essentially or partly embodied in the form of a software product that contributes to the prior art. The computer software product is stored in a storage medium, including several instructions for a computer device (which can be a personal computer, a server, or a network device, etc.) to perform all or part of the steps of the method described in each embodiment of the present application. The aforementioned storage medium includes: U disk, mobile hard disk, read-only memory (ROM), random access memory (RAM), disk or optical disk, etc., various media that can store program check codes.
[0142] Those skilled in the art can clearly understand that, for the convenience and brevity of description, the specific working process of the above-described device and system can refer to the corresponding process in the aforementioned method embodiment, and will not be repeated here.
[0143] It should also be noted that the combination of the various technical features in the embodiments of the present application is not limited to the combination recorded in the embodiments of the present application or the combination recorded in the specific embodiments, and all technical features recorded in this case can be freely combined or combined in any way unless there is a contradiction between them.
[0144] WGT Architecture
[0145] Wafer Geometry Tool (WGT) is a measurement device that can be used in silicon wafer manufacturing plants to characterize the flatness, nanotopography and shape (bow and warp) of wafers. It can also be used in glass wafer plants. Typically, each wafer must be certified by a WGT-type device before being shipped to customers. There are several existing devices that can achieve this purpose. For example, wafer geometry measurement equipment based on capacitive sensors is widely used in 200mm wafer plants. Figure 7a A schematic diagram of the structure of a device based on a double Fizeau interferometer is shown, which is a device for measuring wafer geometric parameters of 300mm wafers. Wafer geometric parameter measurement equipment based on interferometers has advantages in both accuracy and throughput. Despite the fact that 300mm wafers are more prone to vibration than 200mm wafers, the accuracy of wafer geometric parameter measurement equipment based on interferometers is about one to two orders of magnitude higher than that of equipment based on capacitive sensors. However, there is no interferometer-based 200mm wafer geometric parameter measurement equipment on the market. Wafer geometric parameter measurement equipment based on capacitive sensors is designed for 250nm, 180nm and 130nm node processes. Capacitive sensor equipment cannot meet the accuracy and throughput requirements of design nodes less than 130nm.
[0146] Figure 7b A schematic diagram of the structure of a device based on a shearing interferometer is shown. The shearing interferometer can also work together with the air-floating chuck in the present application to measure geometric parameters such as the shape and flatness of the wafer.
[0147] On the one hand, the present application relates to a semiconductor device architecture for measuring wafer flatness and wafer shape for various types of wafers such as 200mm wafers, which architecture can also be referred to as a wafer measurement device. Relative to scanning equipment based on capacitive sensors or optical sensors, the architecture can have better accuracy and higher throughput. Embodiments of the architecture of the present application can also be used for 300mm and 450mm wafer geometric parameter measurement. In addition to wafer geometric parameter measurement equipment, the architecture of the present application can also be applied to the measurement of wafer geometry (Patterned Wafer Geometry, PWG) with a design pattern. The air-floating chuck uses an air cushion to support the wafer during the wafer shape measurement. The air-floating film or air cushion of the air-floating chuck has very little rigidity, and the air-floating film or air cushion applies a small force to support the wafer, but does not deform the wafer, which is an ideal situation for wafer shape measurement.
[0148] Figure 7cA schematic diagram of a structure for measuring wafer geometric parameters is shown, which can perform the same measurements as a double Fizeau device, but at a fraction of the cost of a double Fizeau device. In terms of wafer shape measurement, this architecture has many advantages over existing double Fizeau devices. As shown in FIG7c, the architecture 700 may include a single interferometer 120, which includes a camera 122, a relay lens 123, a polarization beam splitter PBSC124, a light source 125 (e.g., an illuminator), a collimator 126, and a standard mirror 121 (Transmission Flat, TF), all of which are shown in the figure. The operation of the interferometer is well known and will not be described in detail here. In this architecture, a single interferometer is configured to measure the shape of a wafer 1. It should be understood that the standard mirror may also be referred to as a test flat, a transmission flat, etc. This architecture is not limited to the use of a Fizeau interferometer, and other types of vertically incident interferometers may also be used, such as a shear interferometer based on a grating structure.
[0149] like Figure 7c As shown, the wafer can be placed horizontally on the air cushion generated by the top surface of the air flotation chuck 110. The air flotation chuck 110 can include a plurality of alternating pressure channels and vacuum channels for forming and maintaining an air cushion on the top surface of the air flotation chuck 110. The air flotation chuck 110 can also include a Z-shaped deflection table 111, which can offset and / or tilt the air flotation chuck 110. A plurality of lifting pins 112 can be provided to lift the wafer from the surface of the air flotation chuck 110.
[0150] Refer again Figure 7c In order to measure the thickness of the wafer 1, a capacitive sensor 130 (embedded in the air-floating chuck 110) at the bottom of the wafer 1 and a combination of one or more optical position sensors 140 (bi-cell or PSD, Position Sensing Diode) and a laser 150 at the top of the wafer 1 are incorporated into the architecture 700. Figure 1d and 1e, the reading of the position sensor can be calibrated using a wafer 161 of known thickness, i.e., the first standard wafer 161. The position of the position sensor can be correlated to the height of the top surface of the wafer. The capacitive sensor 130 can measure the position of the bottom surface of the wafer. The combined information of the position of the top surface and the position of the bottom surface can be used to accurately determine the thickness of wafer 1. There is an additional advantage of the bi-cell or PSD position sensor on top of wafer 1. The reading of the position sensor can be directly correlated to the wafer thickness. The reading of the position sensor on top of the wafer can also distinguish the relative movement / vibration between wafer 1 and TF 121. Wafer vibrations may be caused by the air floating chuck / flange / support mechanism, which cannot be sensed by the capacitive sensor 130 because the capacitive sensor 130 moves together with the unit including wafer 1 and air floating chuck 110.
[0151] The interferometer tool can be used to calibrate both capacitive sensors and optical (bi-cell or PSD) position sensors. Both capacitive sensors 130 and optical (bi-cell) position sensors 150 can sense air bearing stability, but only optical (bi-cell) sensors can sense vibrations of the chuck assembly. Optical (bi-cell) sensors are useful when it is necessary to isolate the source of vibration.
[0152] It should be understood that Figure 7c The architecture shown for wafer geometry measurement including wafer shape and wafer thickness variation (also known as wafer flatness or wafer flatness) is not limited to the use of Fizeau interferometers, and other interferometers such as shearing interferometers can also be used in the architecture of the present application using a reflective air-floating chuck.
[0153] Compared with the dual Fizeau interferometer architecture, the architecture of the present application has better accuracy, matching and lower cost. The architecture can use a grating-based shearing interferometer instead of a Fizeau interferometer, and use an air-floating chuck instead of three supporting lift pins, thereby improving the accuracy of the shearing interferometer measurement and increasing the measured warpage dynamic range by tilting the wafer. This may be an ideal device structure for patterned wafer geometry (PWG) equipment.
[0154] The method of wafer geometry measurement using an air-bearing chuck and a single interferometer has many advantages. For example, the air-bearing chuck can provide effective gas damping for the wafer located on the air-bearing chuck. The gas damping effect not only makes the interferometer measurement more accurate, but also reduces the cost by eliminating the need for expensive active vibration isolation systems and heavy acoustic vibration isolation shakers. The gas damping effect also saves the cost of wafer transfer within the architecture due to the simplified wafer loading process, for example, horizontal loading of wafers under a single interferometer. Compared to the double Fizeau interferometer, the single interferometer architecture saves cost by eliminating one interferometer and associated optics. There is also no need for the mechanism required to rotate the wafer 90° from horizontal to vertical in the double Fizeau interferometer architecture. The acoustic isolation box in the double Fizeau architecture is also not required in the architecture. In addition, the air cushion can provide gas damping performance. The entire system has fewer moving parts, making the system more reliable than the double Fizeau architecture. Wafers can be loaded directly on the chuck to reduce the wafer transfer time required when using double Fizeau interferometer-based equipment. The advantages of this WGT architecture equipment are even greater for 300mm or 450mm wafers, where vibration of the 300mm or 450mm wafer can be the most significant source of noise, making it difficult to achieve high accuracy in flatness measurement. For 300mm or 450mm equipment, the optical components collimator, standard mirror and folding mirror are large and expensive. Eliminating an interferometer, a wafer vertical loading system, an acoustic box and a channel for a data acquisition system can significantly reduce costs for original equipment manufacturers (OEMs) and their customers.
[0155] Air floating chuck
[0156] Figure 7c The embodiment of the illustrated architecture 700 can achieve artifact-free measurements. In the architecture 700, the wafer 1 under test can be loaded directly from the operator end effector into the measurement chamber. In another aspect of the present application, an air-floating chuck is disclosed. Figures 8a-8d The structure of the air flotation chuck is discussed in further detail.
[0157] Figure 8a FIG. 2 shows a schematic top view of an air-floating chuck. Figure 8aAs shown, the air flotation chuck 110 has an array of pressure and vacuum nozzles on the chuck surface, wherein alternating pressure nozzles 802 and vacuum nozzles 804 are arranged into concentric nozzle rings that are evenly spaced. Multiple pressure nozzles 802 and multiple vacuum nozzles can cover the entire top surface of the nozzle portion so that the support force on the wafer is balanced, which is conducive to keeping the original shape of the wafer suspended above the top surface of the chuck. The vacuum suction and pressure support force can keep the wafer suspended on an air cushion of several microns to hundreds of microns on the air flotation chuck 110. The thinner the air cushion and the greater the air flow, the stiffer the air flotation. At appropriate vacuum and pressure flow rates, the air flotation can be very stiff (e.g., >1N / μm). For an air gap of about 20μm, the air flotation will also have a significant ability to flatten the wafer. However, the rigidity of a 100μm thick air flotation can be as low as one-tenth of 1N / μm, where the force that deforms the shape of the wafer is very small.
[0158] To measure wafer flatness or TTV from the front side of the wafer, the back side of the wafer may be flattened and matched to the chuck surface by the air-floating chuck 110. When the air-floating gap is set at an appropriate height (e.g., 15 μm to 20 μm), no artifacts are detected on the air-floating chuck 110. To measure the shape of the wafer, the wafer is suspended on the surface of the air-floating chuck 110, and the air-floating gap is set to be approximately equal to 60 μm-300 μm, wherein the wafer is supported by the air cushion generated by the air-floating chuck 110, and since the suction force under the large gap is very small, the wafer is able to maintain its original shape.
[0159] In order to meet the WGT requirements for wafer flatness and shape measurement, the air bearing chuck 110 may have the following features, such as Figure 8a shown.
[0160] (1) Axisymmetric, alternating pressure and vacuum nozzles 802, 804 arranged in concentric rings.
[0161] (2) The radius of the nozzle ring farthest from the center of the circle is smaller than the radius of the wafer. Nozzles such as vacuum nozzles or pressure nozzles extend outward from the center of the circle to approximately the last 0-20 mm (greater than 0), preferably 2-4 mm, of the radius of the air-floating chuck 110, thereby supporting the wafer. For example, for a 200 mm chuck, nozzles such as pressure nozzles 802 or vacuum nozzles 804 extend radially so that the center of the last group of nozzles is located at a position on the air-floating chuck with a diameter of 199 mm, 198 mm, 196 mm, 190 mm, or 180 mm. In this embodiment, the surface of the air-floating chuck 110 is preferably larger than the surface of the wafer, so that the wafer does not extend beyond the edge of the air-floating chuck 110 when suspended in the air.
[0162] (3) As the radius increases, preferably, 6 nozzles are added to each nozzle ring, while the tangential spacing between the nozzles remains constant. To achieve this, the following formula N=6*n is used. Where n is the nth concentric nozzle ring, N is the number of nozzles per nozzle ring, and n=0 is the first "nozzle ring" at the center of the wafer. The number "6" is preferably used to achieve that the displacement between the nozzles in the radial and tangential directions is also approximately the same.
[0163] The selection of number "6" is based on the following method. The tangential spacing ΔT between vacuum nozzle 804 and pressure nozzle 802 can be the same across the entire air flotation chuck 110. Adjacent nozzle rings are spaced a constant distance ΔR. For a given ΔR, ΔT can be calculated using the following method.
[0164] Assume that for each adjacent nozzle ring, the number of nozzles increases with the radius by an even integer m (the even integer is because the vacuum and pressure nozzles are paired):
[0165] N=m*n
[0166] Where "N" is the number of nozzles per nozzle ring;
[0167] "n" is the nth nozzle ring; each nozzle ring is separated by ΔR, and the radius of the nth nozzle ring is Rn=n*ΔR.
[0168] Since the number of nozzles increases in pairs, "m" is an even integer (eg, 2, 4, 6, 8, 10).
[0169] ΔT=2p*n*ΔR / N=2p*ΔR / m=(2p / 6)*ΔR
[0170] Wherein, p is the circumference constant π. When m=6, based on the above formula, ΔR and ΔT have almost the same value.
[0171] (4) The chuck flatness of WGT 200 (wafer geometric parameter measurement equipment for measuring 200 mm wafers) is preferably less than or equal to 1.5 μm. The chuck flatness of WGT 300 (wafer geometric parameter measurement equipment for measuring 300 mm wafers) is preferably less than or equal to 2 μm.
[0172] (5) The chuck surface needs to meet the standard of mirror polished chuck surface > N4 (according to ISO standard).
[0173] (6) The diameter of the air-floating chuck 110 is preferably 10 mm larger than the diameter of the wafer. The area of the air-floating chuck that is larger than the wafer can be used for calibration during wafer measurement because it is not blocked by the wafer during measurement.
[0174] (7) 3 wafer clamps 808, 2 fixtures (90° apart, used to fix any two wafer clamps 808), and a driving clamp at the center of the wafer. The force on the wafer 1 can be adjusted (e.g. 0.05lb-1lb).
[0175] (8) The four lifting pins 112 can lift the wafer a certain distance from the top surface of the air-floating chuck 110 in a stable manner to facilitate the removal of the wafer from the chuck.
[0176] Figure 8b A top view of another air flotation chuck 110 is shown. The vacuum nozzle and the pressure nozzle on the air flotation chuck 110 are arranged at ΔR and ΔT as shown in the figure. Among them, ΔR = 11.0 mm, ΔT = 9.0 mm. Since the difference between ΔR and ΔT is only 2 mm, it can be considered that ΔR and ΔT are substantially the same.
[0177] Figure 8c A schematic diagram of the connection layer of a pressure nozzle 802 and a vacuum nozzle 804 of an air flotation chuck is shown. Figure 8c A top view of the stacked layers of the air-floating chuck 110 is provided. The stacked layers include a vacuum shunt layer 832, a pressure shunt layer 833, and a top chuck layer 834. The vacuum shunt layer 832 includes vacuum channels 835, which connect all vacuum channels 835 to a vacuum supply. The pressure shunt layer 833 includes pressure channels 836, which connect all pressure channels 836 to a pressure supply. The top chuck layer 834 includes a plurality of through holes, which are used to connect the vacuum channels 835 in the vacuum shunt layer 832 to the vacuum nozzles on the top surface of the top chuck layer 834. The top chuck layer 834 also includes additional through holes, which are used to connect the pressure channels 836 in the pressure shunt layer 833 to the pressure nozzles on the top surface of the top chuck layer 834. The through holes for vacuum and pressure are connected to Figure 8a and 8b The vacuum and pressure nozzle arrangements shown correspond to those arranged in an alternating fashion.
[0178] Figure 8d A schematic side view of a stacked structure of an air flotation chuck 110 is shown. The air flotation chuck 110 includes a top chuck layer 834', a vacuum diverter layer 832', and a pressure diverter layer 933'. Alternating through holes 840, 842 connect the vacuum channel 835' and the pressure channel 836' to the vacuum nozzle and the pressure nozzle on the top surface of the air flotation chuck 110, respectively. Figure 8d As shown in the side view of the air flotation chuck, the spacing ΔT between alternating vacuum nozzles and pressure nozzles can be substantially the same.
[0179] Figure 8eFIG. 8 is a schematic side view of another stacking structure of an air flotation chuck 110. In this embodiment, the stacking structure may include a top plate 890, a rear cover plate 892, and a diverter plate 894 sandwiched between the top plate 890 and the rear cover plate 892. The top plate 890 may be made of aluminum, ceramic, glass, or microcrystalline silicon, and the preferred thickness of the top plate 890 is in the range of 10-60 mm. Figure 8d In the embodiment, the through holes 880 and 882 alternately arranged in the top plate 890 respectively provide pressure support force and vacuum suction force to keep the wafer suspended ( Figure 8d The diameter of through holes 880 and 882 may be 1.25-1.5 mm.
[0180] The top surface and the bottom surface of the diverter plate 894 may each have one or more grooves, and the vacuum channel 896 and the pressure channel 898 may be located in the above grooves, respectively. Figure 8e In the example shown, the groove on the top surface of the manifold 894 can embed a vacuum channel 896, which connects the vacuum nozzle on the top plate 890 of the stack structure to the vacuum outlet 897 on the bottom plate of the stack structure through the through hole 880. Similarly, the groove on the bottom surface of the manifold 894 can embed a pressure channel 898, which connects the pressure nozzle on the top plate 890 of the stack structure to the pressure outlet 899 on the bottom plate of the stack structure through the through hole 882. The grooves on the top and bottom surfaces of the manifold can be set according to the structure of the vacuum channel and the pressure channel, respectively, and can be several millimeters wide and several millimeters deep, preferably 2 mm wide and 2 mm deep.
[0181] Figure 8f Shows Figure 8e The top surface 890f of the top plate 890 of the stacked structure. The top surface includes pressure and vacuum nozzles (or holes) 802, 804 with equal or unequal spacing, such as radial and tangential spacing of 5-25mm, preferably 8-12mm. The diameter of the vacuum nozzle 804 can be several millimeters, such as 1.5mm. The diameter of the pressure nozzle 802 can be several millimeters, such as 1.25mm. Both the vacuum nozzle 804 and the pressure nozzle 802 can have chamfers.
[0182] Figure 8g Shows Figure 8e The bottom surface 890g of the top plate of the stack structure shows the same pattern of pressure nozzles and vacuum nozzles 802', 804'. The bottom surface 1g may also include M3.5 or M4 threaded holes 812 for fastening the plates of the stack structure together and sealing the vacuum and pressure channels. Alternatively, glue can be used to fasten the plates together, which can improve the flatness of the top surface. If glue is used, there is no need for any M3.5 or M4 or any other threaded holes on the plates.
[0183] Figure 8h Shows Figure 8e 8h. All vacuum nozzles from the top plate (not shown in FIG. 8h) are connected to corresponding vacuum holes 820 in the top surface 894A of the manifold 894. In contrast, all vacuum nozzles from the top plate (not shown in FIG. 8h) are connected to corresponding vacuum holes 820 in the top surface 894A of the manifold 894. Figure 8h All pressure nozzles (not shown) are connected to the corresponding pressure holes 822 in the manifold 894, forming a straight hole (such as Figure 8e ), thereby connecting the pressure nozzle on the top plate to the pressure channel (as shown) embedded in the bottom groove of the diverter plate 894 Figure 8i In one embodiment, the vacuum channel 820A on the top surface of the diverter plate 894 may be Figure 8h The channels are aligned with the vacuum nozzles on the top plate and connected by external circular channels 824 along the edge of the manifold 894. Figure 8h Also shown are M3.5 or M4 threaded holes 812' for securing the panels of the stack together.
[0184] Figure 8i Shows Figure 8e 894 in a stacked configuration. In this embodiment, the pressure channels / grooves 830 may be in an inner annular pattern ("pressure supply ring") that connects the pressure holes through the diverter plate 894. The pressure supply ring has less resistance due to the increased cross-section of the pressure supply ring. Figure 8i The bottom view also shows the Figure 8h 5 or M4 threaded holes 812' are visible in the top view of the embodiment. Although the bottom view also shows the superimposed vacuum channel 820A', it should be understood that this is for illustration purposes only. Figure 8h As shown, the actual vacuum channel 820A′ is located in a groove on the top surface of the diverter plate 894.
[0185] Figure 8j Shows Figure 8e A top view of the rear cover plate 892 of the stacked structure. Figure 8k FIG8e shows a bottom view of the back cover plate 892 of the stacked structure. Figure 8i As shown, the top surface of the rear cover plate 892 can be polished to seal the bottom surface of the manifold with the pressure groove embedded in it. In this embodiment, there are three openings 1j, which are used to connect the pressure channel from the bottom surface of the manifold 892 to the pressure fitting ( Figure 8j In addition, there are three other openings 2j for connecting the vacuum channel from the top surface of the manifold to the vacuum fittings ( Figure 8j (not shown in the figure). Figure 8k The same pressure and vacuum openings 1j', 2j' are also shown on the bottom view of the rear cover plate 892 in FIG. Figure 8j The top view of the rear cover plate 892 is shown and Figure 8k The bottom view of the rear cover plate 892 shown also shows M3.5 or M4 threaded holes 812'" which are used to fasten the rear cover plate to other plates in the stacked structure.
[0186] although Figure 8e-8k A stacking structure of an air flotation chuck is shown, the stacking structure having a pressure channel and a vacuum channel, which are respectively located in grooves on the bottom surface and the top surface of the diverter layer, but it should be understood that these channels can also be embedded in the grooves of other layers. For example, the vacuum channel can be located in a groove on the bottom layer of the top plate, and the pressure channel can be located in a groove on the top layer of the back cover plate. In addition, it should be understood that in other embodiments, the arrangement of the vacuum channel and the pressure channel can be interchanged. In various embodiments, different numbers of vacuum and / or pressure nozzles can be included. The paths of the vacuum and pressure channels can be adjusted according to the number and position of the nozzles. The number of vacuum fittings and pressure fittings at the bottom of the stacking structure is not limited, for example, it can be 3 or more.
[0187] Figure 9a and 9b FIG. 9 is a schematic diagram showing an exemplary structure of a flow divider chamber 900. The flow divider chamber 900 is used to separate the pressure nozzle from the vacuum nozzle. Figure 9a and 9b , the flow divider 900 includes a pressure flow divider 904 and a vacuum flow divider 902, all vacuum nozzles are connected to the vacuum flow divider 902, and all pressure nozzles directly pass through the vacuum flow divider 902 to reach the pressure flow divider 904 located below the vacuum flow divider. Computer fluid dynamics (CFD) simulation shows that this flow divider greatly improves the uniformity of the vacuum nozzle and the pressure nozzle. The flow divider can provide a uniform amount of gas and optimize the increased channel size to the greatest extent. In addition, the chamber height can be adjusted to a height that minimizes the change in orifice flow.
[0188] The air cushions used to support the wafers also feature gas damping, which effectively isolates them from ground and acoustic vibrations while eliminating or reducing the need for soundproof boxes and active vibration isolation systems.
[0189] Shape measurement method
[0190] Fig.10a and Fig.10b Shows a method of using Figure 7c Schematic diagram of the shape measurement method of the architecture shown. Fig.10a To measure the shape, first, a reference TF 1002 (TF-ref) is placed on the surface of the air bearing chuck 110 to calibrate the TF 121 in the device. Cal = S TF –S TF-ref The reference TF flatness (in nm) can be much better than the wafer shape warp (in μm). TF-ref is a translation term and can be removed. If TF 121 is thick and has minimal TF depression, the cavity calibration step can also be skipped. In this step, there is no wafer on the chuck. This calibration can be done before shipment. Assuming the TF shape does not change, the tilt correction can be done only at the time of measurement.
[0191] refer to Fig.10b In the next step, wafer 1 is placed on the top surface of the air-floating chuck 110. In order to measure the wafer shape, wafer 1 is suspended at a larger air gap (e.g., 60μm-1500μm, preferably 60μm-300μm). The design and operation of the air-floating chuck enable the pressure to balance the gravity and enable the pressure of the high-pressure gas on the wafer to be vertically upward, with an axisymmetric uniform support force centered on the center of the wafer. Under the larger air gap, the wafer air cushion provides an axisymmetric support force that is not affected by the flatness of the chuck to maintain its natural shape. SWFR=(S TF –S 正面 )
[0192] Next, the difference between Cal and the wafer surface measurement is taken to calculate the wafer shape:
[0193] Wafer shape = Cal–SWFR = (S TF –S TF-ref )–(S TF –S 正面 )=S 正面 –S TF-ref =S 正面
[0194] Since the reference TF has a high flatness, S TF-ref Can be equivalent to a constant, S 正面 –S TF-ref With S 正面All can reflect the shape of the wafer, that is, the shape of the front of the wafer. The wafer shape measurement performed by the above steps is accurate. This may be an ideal equipment structure for patterned wafer geometry measurement (Patterned Wafer Geometry, PWG) equipment. Compared with the dual Fizeau interferometer architecture, the architecture of the present application has better accuracy, matching and lower cost. The architecture can use a grating-based shearing interferometer instead of a Fizeau interferometer, and use an air-floating chuck instead of three supporting lifting pins, thereby improving the accuracy of the shearing interferometer measurement and increasing the measured warpage dynamic range by tilting the wafer.
[0195] TTV measurement method
[0196] The following references Fig.11a , 11b Provides detailed instructions for use Figure 7c An exemplary method of measuring wafer flatness is shown in architecture 700 .
[0197] Fig.11a and 11b Shows a method of using Figure 7c Schematic diagram of the method for measuring wafer flatness TTV using the architecture shown. First, refer to Fig.11a , measuring the optical cavity formed by the TF 121 and the reflective air-floating chuck 110. In other words, the distance between the opposing surfaces of the standard mirror TF 121 and the air-floating chuck 110 changes. The TF 121 may sag in the middle due to gravity. Fig.11a and 11b As shown, the surface of the air bearing chuck 110 may not be completely flat. These imperfections need to be calibrated in order to make the flatness measurement of the wafer accurate. The calibration of the cavity is to measure the change in the thickness of the cavity. Mathematically speaking, the change in the thickness of the cavity is the standard mirror surface S TF (x,y) and the chuck surface S CK The difference between (x,y): Δ S 空腔 =S TF -S CK At this step, there is no wafer on the chuck.
[0198] refer to Fig.11b After calibration, the wafer 1 is placed on the surface of the air-floating chuck 110. In order to measure the flatness of the wafer 1, the wafer is suspended at a small air gap (e.g., 0 μm-50 μm, preferably 5 μm-30 μm) from the top of the air-floating chuck 110. The small air gap is generated by the air-floating chuck 110. At these small air gaps, the air-floating chuck design has the ability to flatten the back side of the wafer or to flatten the back side of the wafer. 背面 The top surface S of the chuck CK In this case, the front side of the wafer (S正面 , which can also be called the top surface of the wafer) is only the top surface S of the chuck. CK The sum of the position information and the total thickness change of the wafer, S 正面 =S CK +TTV. However, the back side of the wafer S 背面 is not completely aligned with the top surface S of the chuck CK In practice, in order to accurately determine the front side of the wafer, it is necessary to add a mismatch term (S N.C. ): S 正面 =(S CK +TTV+S N.C. ).
[0199] Interferometer measurement can measure the distance between wafer 1 and the standard mirror: ΔS WFR =(S TF –S 正面 ) =(S TF –S CK –TTV–S N.C. ).
[0200] Next, the difference between the cavity and the wafer surface (ΔS 空腔 –ΔS WFR ) to calculate TTV. Then, the total thickness change can be calculated by the following formula: TTV actual = (ΔS 空腔 –ΔS WFR –S N.C. ), where ΔS 空腔 and ΔS WFR Can be Figure 7c The WGT architecture shown is used to measure the interferometer. N.C. Can be obtained according to calibration. N.C. This can be obtained by using a wafer with known TTV (such as a double-sided polished 200 mm wafer): N.C. =(ΔS 空腔 –ΔS WFR –TTV known ). N.C.E May drift over time, requiring frequent calibration. N.C. It is a function of wafer thickness, temperature, air bearing height FH and chuck flatness. All these parameters can be measured simultaneously with the interferometer data and can also be used for correction.
[0201] Methods to distinguish real wafer surface features from chuck marks / artifacts
[0202] Figure 7cThe embodiment of the illustrated architecture 700 can achieve artifact-free measurement. In this architecture 700, the wafer 1 can be loaded directly from the operator end effector into the measurement chamber.
[0203] Figure 7c The illustrated embodiment of the WGT architecture 700 utilizes a vertically mounted Fizeau interferometer for flatness measurement and wafer shape measurement. However, in practice, methods for wafer flatness measurement and wafer shape measurement have many challenges. The air chuck itself may not be flat, and there may be artifacts, such as grains, on the surface of the air chuck. When the wafer is vacuumed onto the air chuck, artifacts may appear on the top surface of the wafer. For example, Fig.12a Schematic diagram showing chuck marks / artifacts as the wafer is vacuumed down onto the vacuum chuck. Fig.12a As shown, large grains 1202 may appear as protrusions on wafer 1 on the top side of air-floating chuck 110. According to another embodiment of the present application, these types of artifacts can be calibrated by using the method of the embodiments herein. Figure 12b A schematic diagram of a wafer 1 ′ suspended above an air-floating chuck 110 ′ is shown, wherein no chuck marks / artifacts are visible on the wafer 1 ′.
[0204] Figures 13a-13c A schematic diagram of a method of distinguishing real features 1304 from chuck marks / artifacts 1306 on the surface of wafer 1 is shown. Fig.13a A schematic diagram of measuring the geometric parameters of a wafer on the S1 surface is shown, where real features 1304 are mixed with chuck marks / artifacts 1306 in the interferometer measurement. Fig.13b 1 shows a schematic diagram of measuring the geometric parameters of a wafer on the S2 surface, where the S2 surface is the chuck surface after the chuck is rotated 180° from the original position where the S1 surface measurement is performed. When the chuck mark / artifact 1306 rotates 180° with the chuck 110, the real feature 1304 stays in the same position. Therefore, by placing the wafer 1 on the chuck surface S2 after rotating 180° (as shown in FIG. Fig.13b ), and the surface S2 of the wafer 1 at 180° is aligned with the surface S1 at 0° (as shown in FIG. Fig.13a By comparing the measurement results of wafer 1 with those of wafer 2 (shown in FIG. 1 ), the true features 1304 of the wafer (those features that remain in the same position in the wafer coordinate system before and after rotation) can be identified. In contrast, when wafer 1 is rotated 180°, the position of the chuck mark / artifact 1306 in the coordinate system of wafer 1 deviates by 180°.
[0205] Fig.13cS1 and S2 difference plots are provided showing chuck artifacts as pairs 1316, 1320. These chuck artifacts can be calibrated out if they do not move around on the chuck. These chuck artifacts also have special characteristics that can be removed by the algorithm if the chuck is clean and the chuck artifacts are isolated. When limited artifacts are on the chuck and / or back side of the wafer, the wafer or chuck rotation method can be used to distinguish the artifacts and eliminate them.
[0206] Although the embodiments of the present application have been fully described with reference to the accompanying drawings, it should be noted that various changes and modifications will become apparent to those skilled in the art. Such changes and modifications should be understood to be included within the scope of the embodiments of the present application defined by the appended claims.
Claims
1. A method for measuring wafer thickness, characterized in that: include: Using an air floating chuck to suspend the wafer at a predetermined distance D above the top surface of the air floating chuck, D ≥ 0; Using a laser and a position sensor to measure position information of a first position point on the front side of the wafer to obtain a position sensor reading Vx, wherein the front side of the wafer is a surface of the wafer away from the air floating chuck; Using a capacitive sensor to measure position information of a second position point on the back side of the wafer to obtain a capacitive sensor reading CPn, wherein the first position point and the second position point are two relative position points in the wafer that characterize thickness, and the back side of the wafer is a surface of the wafer close to the air floating chuck; Determine the formula T 晶圆 =T0+(CP0-CPn)+S*(Vx–V0), wherein T0 in the formula is the thickness of the first standard wafer, CP0 is the reference capacitance sensor reading of the first standard wafer at the reference predetermined distance, V0 is the reference position sensor reading of the first standard wafer at the reference predetermined distance, and S is the slope of the straight line in the relationship diagram with the horizontal coordinate Vx and the vertical coordinate being the difference hx between CPn and CP0; Substituting Vx and CPn into the formula, the thickness T of the wafer is calculated. 晶圆, The T 晶圆 is the distance between the first position point and the second position point on the wafer.
2. The method for measuring wafer thickness according to claim 1, characterized in that: The determination formula T 晶圆 =T0+(CP0-CPn)+S*(Vx–V0), including: suspending the first standard wafer at different predetermined distances above a top surface of the air floating chuck using the air floating chuck; Using the position sensor to measure position information of a third position point on the first surface of the first standard wafer when the first standard wafer is at the different predetermined distances, so as to obtain a position sensor reading Vx, wherein the first surface of the first standard wafer is a surface of the first standard wafer away from the air floating chuck; Using the capacitance sensor to measure the position information of a fourth position point on the second surface of the first standard wafer when the first standard wafer is at the different predetermined distances, so as to obtain a capacitance sensor reading CPn, wherein the second surface of the first standard wafer is a surface of the first standard wafer close to the air floating chuck, the fourth position point and the third position point are two relative position points in the first standard wafer that characterize the thickness, the different predetermined distances include a reference predetermined distance, and the reference capacitance sensor reading when the first standard wafer is at the reference predetermined distance is CP0 and the reference position sensor reading is V0; Constructing a relationship diagram with the abscissa being the Vx and the ordinate being the difference hx between the CPn and CP0, so as to determine the slope S of the straight line from the straight line in the relationship diagram; Determine the formula T according to T0, CP0 and S 晶圆 =T0+(CP0-CPn)+S*(Vx–V0).
3. The method for measuring wafer thickness according to claim 1, characterized in that: The reference predetermined distance is the distance between the second surface of the first standard wafer and the top surface of the air floating chuck when the first standard wafer is vacuum sucked onto the air floating chuck by the air floating chuck, or the reference predetermined distance is the distance between the second surface of the first standard wafer and the top surface of the air floating chuck when the first standard wafer is suspended at any position above the top surface of the air floating chuck by the air floating chuck.
4. A method for measuring wafer warpage, characterized in that: include: Using at least one tilting platform to adjust the tilt angle of the air-floating chuck multiple times to form a plurality of tilted wafers, and the plurality of tilted wafers meet the slope requirement of interferometer measurement, wherein the at least one tilting platform is located below the air-floating chuck; Measuring the thickness of a wafer at a plurality of positions on a plurality of tilted wafers according to the wafer thickness measurement method as described in any one of claims 1 to 3; Combining the thicknesses corresponding to the plurality of locations to form a two-dimensional or three-dimensional image of the wafer; The warpage of the wafer is acquired using the two-dimensional or three-dimensional image of the wafer.
5. A method for measuring the thickness of a mask layer on a wafer, characterized in that: include: The thickness T of the wafer before the mask is measured according to any wafer thickness measurement method as described in claim 1-3 晶圆掩膜前 ; Using the suction force provided by the air floating chuck to adjust the back side of the wafer after the mask so that the back side of the wafer after the mask matches the back side of the wafer before the mask, the wafer after the mask is a wafer after a mask layer is added to the surface of the wafer before the mask; Using the support force provided by the air floating chuck, the wafer behind the mask is adjusted to float at the same predetermined distance from the top surface of the air floating chuck as the wafer before the mask; The thickness T of the wafer after the mask is measured according to any one of the wafer thickness measurement methods described in claims 1-3. 晶圆掩膜后 ; By placing the T 晶圆掩膜后 Subtract the T 晶圆掩膜前 The thickness of the mask layer is obtained.
6. The method for measuring the thickness of a mask layer on a wafer according to claim 5, characterized in that: The wafer thickness T before the mask is measured according to any wafer thickness measurement method as described in claim 1-3. 晶圆掩膜前 Previously, it also included: Using the suction force provided by the air floating chuck to adjust the back side of the wafer before the mask so that the back side of the wafer before the mask matches the top surface of the air floating chuck, the back side of the wafer before the mask being the surface of the wafer before the mask close to the air floating chuck; Using the support force provided by the air-floating chuck, the masked wafer is adjusted to float at a predetermined distance from the top surface of the air-floating chuck; Wherein, the method of adjusting the back side of the wafer after the mask by using the suction force provided by the air floating chuck so that the back side of the wafer after the mask matches the back side of the wafer before the mask comprises: The suction force provided by the air-floating chuck is used to adjust the back side of the masked wafer so that the back side of the masked wafer matches the top surface of the air-floating chuck.
7. A method for measuring wafer thickness, characterized in that: include: Receiving a position sensor reading Vx obtained by measuring position information of a first position point on the front side of a wafer using a laser and a position sensor, wherein the wafer is placed on the top surface of an air-floating chuck, and the front side of the wafer is a surface of the wafer away from the air-floating chuck; Receiving a capacitance sensor reading CPn obtained by measuring position information of a second position point on the back side of the wafer using a capacitance sensor, wherein the first position point and the second position point are two relative position points in the wafer representing thickness, and the back side of the wafer is a surface of the wafer close to the air floating chuck; Obtain the thickness T of the wafer according to the Vx and the CPn 晶圆, include: Determine the formula T 晶圆 =T0+(CP0-CPn)+S*(Vx–V0), wherein T0 in the formula is the thickness of the first standard wafer, CP0 is the reference capacitance sensor reading of the first standard wafer at the reference predetermined distance, V0 is the reference position sensor reading of the first standard wafer at the reference predetermined distance, and S is the slope of the straight line in the relationship diagram with the horizontal coordinate Vx and the vertical coordinate being the difference hx between CPn and CP0; Substituting Vx and CPn into the formula, the thickness T of the wafer is calculated. 晶圆 .
8. A wafer thickness measuring device, characterized in that: include: A receiving module, used for receiving a position sensor reading Vx obtained by measuring position information of a first position point on the front side of a wafer using a laser and a position sensor, wherein the wafer is placed on the top surface of an air-floating chuck, and the front side of the wafer is the surface of the wafer away from the air-floating chuck; and also used for receiving a capacitive sensor reading CPn obtained by measuring position information of a second position point on the back side of the wafer using a capacitive sensor, wherein the first position point and the second position point are two relative position points in the wafer that characterize thickness, and the back side of the wafer is the surface of the wafer close to the air-floating chuck; An acquisition module is used to acquire the thickness T of the wafer according to the Vx and the CPn. 晶圆, include: Determine the formula T 晶圆 =T0+(CP0-CPn)+S*(Vx–V0), wherein T0 in the formula is the thickness of the first standard wafer, CP0 is the reference capacitance sensor reading of the first standard wafer at the reference predetermined distance, V0 is the reference position sensor reading of the first standard wafer at the reference predetermined distance, and S is the slope of the straight line in the relationship diagram with the horizontal coordinate Vx and the vertical coordinate being the difference hx between CPn and CP0; Substituting Vx and CPn into the formula, the thickness T of the wafer is calculated. 晶圆 .
9. A computer-readable storage medium, characterized in that: Computer executable instructions are stored thereon, wherein the executable instructions, when executed by a processor, implement the wafer thickness measurement method as described in claim 7.