Temperature-deformation-resistant conveying belt and preparation method thereof

A conveyor belt and temperature-resistant technology, which is applied in the field of temperature-resistant deformed conveyor belt and its preparation, can solve the problems of affecting the wear resistance of the conveyor belt, shortening the service life, and reducing the structural stability of the conveyor belt, so as to improve the resistance to oxidation and degradation Performance, anti-aging shrinkage, good anti-oxidation effect

CN113290950AInactive Publication Date: 2021-08-24上海米莜凯自动化装备有限公司
7 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2021-08-24
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 1
    Figure 1
Patent Text Reader

Abstract

The invention relates to the field of conveying belts, and particularly discloses a temperature-deformation-resistant conveying belt and a preparation method thereof. The temperature-deformation-resistant conveyor belt is prepared from the following raw materials in parts by weight: 60 to 100 parts of acrylate rubber, 120 to 200 parts of silicone rubber, 30 to 50 parts of carbon black, 20 to 40 parts of skeleton woven fabric, 5 to 15 parts of epoxy resin, 15 to 20 parts of dicumyl peroxide, 10 to 15 parts of carbon fiber, 5 to 20 parts of calcium carbonate, 5 to 10 parts of titanium dioxide, 5 to 16 parts of m-phenylenediamine, 5 to 10 parts of iron sulfide, 5 to 10 parts of stearic acid, 5 to 8 parts of anti-aging agent and 6 to 15 parts of argil. The preparation method comprises the following steps: drying the skeleton woven fabric for later use, preparing the adhesive layer, preparing the rubber layer, and carrying out hot-pressing lamination on the adhesive layer and the rubber layer. The conveyor belt prepared by the invention has high temperature resistance and wear resistance.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The application relates to the field of conveyor belts, more specifically, it relates to a temperature-resistant deformed conveyor belt and a preparation method thereof. Background technique

[0002] Conveyor belts are widely used in agriculture, industrial and mining enterprises, and transportation industries to transport various solid block and powder materials or finished items. Occasions where the length is short and the conveying volume is small. The conveyor belt can be transported in a continuous, high-efficiency, and large-inclination angle. The conveyor belt is safe to operate, easy to use, easy to maintain, and low in freight. It can also shorten the transportation distance, reduce the engineering cost, and save manpower and material resources.

[0003] In 2005, the country formulated the recommended standard GB / T20021-2005 for canvas core heat-resistant conveyor belts, which stipulated four heat-resistant grades (T1 / 100°C, T2 / 125°C, T3 / 150°...

Examples

Embodiment 1

[0052] A temperature-resistant conveyor belt, including the following raw materials: 60kg of acrylic rubber, 200kg of silicone rubber, 50kg of carbon black, 20kg of skeleton fabric, 15kg of epoxy resin, 20kg of dicumyl peroxide, 10kg of carbon fiber, 20kg of calcium carbonate, Titanium dioxide 5kg, m-phenylenediamine 16kg, iron sulfide 5kg, stearic acid 10kg, antioxidant 5kg, clay 15kg.

[0053] Among them, the skeleton fabric is polyester canvas, and the anti-aging agent is paraffin.

[0054] A method for preparing a temperature-resistant deformed conveyor belt, comprising the following steps: after stirring epoxy resin and m-phenylenediamine at 250°C, uniformly apply it at 180°C, and dry it for 2 hours Skeleton woven polyester canvas on both sides to form a bonding layer; acrylic rubber, silicone rubber, dicumyl peroxide, carbon fiber, calcium carbonate, titanium dioxide iron sulfide, stearic acid, anti-aging agent and clay are stirred and mixed After uniformity, it was mel...

Embodiment 2

[0056] The difference with Example 1: 80kg of acrylate rubber, 180kg of silicone rubber, 40kg of carbon black, 30kg of skeleton fabric, 10kg of epoxy resin, 18kg of dicumyl peroxide, 12kg of carbon fiber, 15kg of calcium carbonate, 8kg of titanium dioxide, 10kg of phenylenediamine, 8kg of iron sulfide, 12kg of stearic acid, 6kg of antioxidant, and 12kg of clay.

Embodiment 3

[0058] The difference with Example 1: 100kg of acrylate rubber, 120kg of silicone rubber, 50kg of carbon black, 20kg of skeleton fabric, 15kg of epoxy resin, 15kg of dicumyl peroxide, 15kg of carbon fiber, 5kg of calcium carbonate, 10kg of titanium dioxide, 5kg of phenylenediamine, 10kg of iron sulfide, 5kg of stearic acid, 8kg of antioxidant, and 6kg of clay.