SGT power MOS device with integrated barrier pinch-off diode and its processing technology

By introducing a barrier-pinch diode structure into the SGT power MOS device, the problem of slow reverse recovery speed and large forward loss of the device is solved, and faster reverse recovery and lower power loss are achieved.

CN113611747BActive Publication Date: 2024-11-05JINAN JINGHENG ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110894292.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-08-04
Publication Date
2024-11-05
Estimated Expiration
2041-08-04

AI Technical Summary

Technical Problem

In the low-side power switching application of DC voltage regulation modules, the large forward injection effect of the parasitic diode inside the device delays the reverse recovery time, resulting in a decrease in the operating frequency and a high forward voltage drop increases the power. loss.

Method used

Using the design of integrated barrier-pinch diodes, a barrier-pinch structure is formed by introducing the first and second polysilicon layers into the device and a thick oxide layer and well area layer are arranged in the trench to form a barrier-pinch structure to reduce the forward guide Through loss and improve reverse recovery speed.

Benefits of technology

It effectively reduces the reverse recovery time and forward voltage drop of SGT power MOS devices, improves the reverse recovery speed and frequency characteristics of the device, and reduces forward conduction power consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113611747B_ABST
    Figure CN113611747B_ABST
Patent Text Reader

Abstract

The present invention discloses an SGT power MOS device with an integrated barrier pinch-off diode and a processing technology. The SGT power MOS device comprises a drain region of a first conductivity type and an epitaxial layer, a trench with an opening upward is arranged on the epitaxial layer, a thick oxide layer filled with a first polysilicon is arranged in the trench, a gate oxide layer filled with a second polysilicon is arranged in the trench above the first polysilicon, a well region layer of a second conductivity type is arranged on the upper part of the epitaxial layer and around the trench; a source region layer is arranged above the well region layer, an insulating dielectric layer is arranged above the source region layer and the trench, a plurality of contact holes are opened on the insulating dielectric layer, and the contact holes are connected to the epitaxial layer, the well region layer and the source region layer; a metal region layer is laid above the insulating dielectric layer; and metal is arranged in the contact holes. The present invention improves the reverse recovery speed of the SGT power MOS device and reduces the forward conduction power consumption of the SGT power MOS device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an SGT power MOS device with an integrated barrier pinch-off diode and a processing technology, belonging to the technical field of semiconductor power devices. Background Art

[0002] SGT power MOS devices can improve the device's withstand voltage, save device area, and obtain lower on-resistance, with lower conduction loss; and the source polycrystalline of SGT power MOS devices can effectively reduce the gate-drain capacitance, increase the switching frequency of the device, and reduce the switching loss of the device. As a result, SGT power MOS structure devices have a trend of replacing trench gate power MOS in the medium and low voltage fields. However, when SGT power MOS devices are used as low-side power switches in DC voltage regulation modules, the large forward injection effect of the parasitic body diode inside the device delays the reverse recovery time of the device, resulting in a reduction in the operating frequency of the entire module. At the same time, the high forward voltage drop of the parasitic body diode inside the device leads to higher power loss. How to improve the reverse recovery speed of SGT power MOS devices and reduce the forward conduction loss of the parasitic body diode to meet the needs of high-frequency applications of synchronous switches is of great significance.

[0003] The main reason for the slow reverse recovery speed of the device is that when the source of the device is at a high potential, the parasitic body diode is forward biased, and a large number of hole carriers are injected into the N drift region by the P body region and accumulated in the N drift region, forming a large injection effect. When the parasitic body diode changes from forward bias to reverse bias, a large number of hole carriers in the N drift region are extracted under the action of the reverse electric field, and the body diode forms a reverse withstand voltage. This process is the reverse recovery process of the device. The speed of the reverse recovery process is determined by the concentration of holes injected into the N drift region by the receptor diode forward. The higher the hole concentration, the slower the reverse extraction, and the lower the hole concentration, the faster the reverse extraction. When the body diode is forward biased, there is a forward voltage drop. Part of this forward voltage drop comes from the built-in potential of the body diode, and the other part comes from the internal resistance. The existence of the forward voltage drop leads to power loss when the device is forward-conducted.

[0004] Therefore, in order to solve the problems of slow reverse recovery and large forward loss of the SGT power MOS device, the present invention provides an SGT power MOS device with an integrated barrier pinch-off diode. Summary of the invention

[0005] In order to solve the above problems, the present invention proposes an SGT power MOS device with an integrated barrier pinch-off diode and a processing technology, which can greatly reduce the reverse recovery time and forward voltage drop of the device.

[0006] The technical solution adopted by the present invention to solve the technical problem is:

[0007] In a first aspect, an SGT power MOS device with an integrated barrier pinch-off diode provided in an embodiment of the present invention comprises a drain region of a first conductivity type located at the bottom of the SGT power MOS device and an epitaxial layer of the first conductivity type extending upward from the upper surface of the drain region, a trench opening upward is provided on the epitaxial layer, a thick oxide layer is provided on the bottom and the inner side surface of the lower end of the trench, a first polysilicon is filled inside the thick oxide layer, and the upper surface of the first polysilicon is flush with the upper surface of the thick oxide layer; a gate oxide layer is provided in the trench above the first polysilicon, and the bottom of the gate oxide layer is flush with the upper surface of the first polysilicon. The gate oxide layer is connected to the upper surface of the thick oxide layer, the outer side surface of the gate oxide layer is connected to the inner side surface of the upper end of the groove, the second polysilicon is filled inside the gate oxide layer, and the upper surface of the second polysilicon is flush with the upper surface of the thick oxide layer; a well region layer of a second conductivity type is arranged on the upper part of the epitaxial layer and around the groove; a source region layer is arranged above the well region layer around the top of the groove, an insulating dielectric layer is arranged above the source region layer and the groove, and a plurality of contact holes are opened in the insulating dielectric layer, and the contact holes are connected to the epitaxial layer, the well region layer and the source region layer; a metal region layer is laid on the insulating dielectric layer; and metal is arranged in the contact holes.

[0008] As a possible implementation manner of this embodiment, the horizontal cross-sectional area of ​​the first polysilicon is not greater than the horizontal cross-sectional area of ​​the second polysilicon.

[0009] As a possible implementation manner of this embodiment, the metal in the contact hole is in contact with the first conductivity type epitaxial layer, the second conductivity type well region layer and the source region layer respectively.

[0010] As a possible implementation manner of this embodiment, the metal in the contact hole forms an ohmic contact with the first conductivity type epitaxial layer.

[0011] As a possible implementation of this embodiment, the horizontal cross-section of the groove is circular, square, rectangular or polygonal.

[0012] As a possible implementation manner of this embodiment, the shapes of the horizontal cross sections of the first polysilicon and the second polysilicon are the same as the shape of the horizontal cross section of the trench, but the sizes are different from each other.

[0013] As a possible implementation manner of this embodiment, the lower surface of the well region layer is higher than the lower surface of the second polysilicon, and the upper surface of the well region layer is lower than the upper surface of the second polysilicon.

[0014] As a possible implementation manner of this embodiment, the upper surface of the second polysilicon is not lower than the lower surface of the source region layer.

[0015] In a second aspect, an embodiment of the present invention provides a processing technology for a SGT power MOS device with an integrated barrier pinch-off diode, comprising the following steps:

[0016] A first conductive type drain region is formed on a silicon wafer, and a first conductive type epitaxial layer is formed by epitaxially growing upward from the upper surface of the drain region;

[0017] Depositing silicon nitride on the upper surface of the epitaxial layer to form a hard mask;

[0018] Etching a trench opening upward on the epitaxial layer by dry etching silicon nitride and dry etching silicon;

[0019] Dry-etching silicon nitride until it is completely etched and then stripping off the hard mask;

[0020] A wet oxygen oxidation method is used to oxidize the thick oxide layer in the trench;

[0021] Depositing polysilicon on the thick oxide layer, and etching the polysilicon deposited on the thick oxide layer to form first polysilicon;

[0022] etching a thick oxide layer in the trench above the first polysilicon;

[0023] A gate oxide layer is formed by oxidation using a dry oxygen oxidation method;

[0024] Depositing polysilicon on the gate oxide layer, and etching the polysilicon deposited on the gate oxide layer to form a second polysilicon;

[0025] Implanting second conductivity type impurities on the upper part of the epitaxial layer and around the trench to form a second conductivity type well region layer, and performing push-junction of the second conductivity type well region layer;

[0026] Implanting source region impurities above the well region layer around the top of the trench to form a source region layer;

[0027] Depositing silicon dioxide on the source region layer and the trench to form an insulating dielectric layer;

[0028] Dry etching silicon dioxide on the insulating dielectric layer until it is completely etched, and dry etching silicon to form a contact hole;

[0029] Metal is deposited on the insulating dielectric layer and in the contact holes to form a metal layer.

[0030] As a possible implementation of this embodiment, the specific steps of etching a groove on the epitaxial layer include:

[0031] ① Perform photoresist deposition, pre-baking, exposure, development, and hardening to cover the surface of the silicon wafer with a barrier layer;

[0032] ② Perform isotropic etching of silicon nitride;

[0033] ③ Perform isotropic deposition to cover the silicon etched surface, sidewalls and photoresist surface with a barrier layer;

[0034] ④ Perform anisotropic etching to remove the barrier layer covering the etched surface and expose the etched surface;

[0035] ⑤Perform isotropic etching of silicon;

[0036] ⑥ Repeat steps ③ to ⑤ until the predetermined etching depth is reached.

[0037] The technical solution of the embodiment of the present invention may have the following beneficial effects:

[0038] The present invention achieves the purpose of improving the reverse recovery speed of SGT power MOS devices and reducing forward conduction power consumption by integrating a barrier pinch-off diode. When the drain of the device is connected to a high potential and the gate source is short-circuited, the barrier pinch-off diode bears the reverse withstand voltage. When the source of the device is connected to a high potential and the gate source is short-circuited, the barrier pinch-off diode is forward-conducted, the conduction mode is unipolar conduction, the current formed is a majority current, and the process of minority carrier extraction during reverse recovery of the device is short, thereby improving the reverse recovery characteristics of the device. When the device is forward-conducted, the current path from the source to the drain is of the same conductivity type, and there is no built-in potential, thereby reducing the forward conduction voltage drop and reducing the forward power dissipation of the device.

[0039] The present invention reduces the large injection effect of hole carriers through the forward unipolar working mode of the barrier pinch-off diode, thereby greatly improving the reverse recovery speed of the SGT power MOS device; reduces the forward conduction voltage drop of the SGT power MOS device through the forward conduction characteristic of the barrier pinch-off diode, thereby greatly reducing the forward conduction power consumption of the SGT power MOS device.

[0040] The integrated barrier pinch-off diode in the present invention can also be integrated into other devices such as a planar gate power MOS device, a trench gate power MOS device, and a super junction power MOS device.

[0041] The processing technology of the present invention is compatible with the traditional SGT power MOS device technology, does not require additional process steps and photomasks, and can be achieved by only adjusting the original individual photomasks and individual process conditions. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 is a schematic cross-sectional structure diagram of an SGT power MOS device with an integrated barrier pinch-off diode according to an exemplary embodiment;

[0043] Figure 2 is a schematic diagram showing a hard mask after formation according to an exemplary embodiment;

[0044] Figure 3is a schematic diagram showing a method of etching a trench opening upward on an epitaxial layer according to an exemplary embodiment;

[0045] Figure 4 is a schematic diagram showing a hard mask after stripping according to an exemplary embodiment;

[0046] Figure 5 is a schematic diagram showing oxidation of a thick oxide layer according to an exemplary embodiment;

[0047] Figure 6 is a schematic diagram showing a method of depositing polysilicon on a thick oxide layer according to an exemplary embodiment;

[0048] Figure 7 is a schematic diagram showing a process of etching polysilicon deposited on a thick oxide layer to form first polysilicon according to an exemplary embodiment;

[0049] Figure 8 is a schematic diagram showing an etching of a thick oxide layer according to an exemplary embodiment;

[0050] Fig. 9 is a schematic diagram showing a method of forming a gate oxide layer according to an exemplary embodiment;

[0051] Fig.10 is a schematic diagram showing a method of depositing polysilicon on a gate oxide layer according to an exemplary embodiment;

[0052] Fig.11 is a schematic diagram showing a method of etching polysilicon deposited on a gate oxide layer to form a second polysilicon according to an exemplary embodiment;

[0053] Fig.12 is a schematic diagram showing a method of injecting second conductive type impurities according to an exemplary embodiment;

[0054] Fig.13 is a schematic diagram showing a second conductivity type well region layer push-junction according to an exemplary embodiment;

[0055] Fig.14 is a schematic diagram showing a method of forming a source region layer according to an exemplary embodiment;

[0056] Fig.15 is a schematic diagram showing a method of forming an insulating dielectric layer according to an exemplary embodiment;

[0057] Fig.16 is a schematic diagram showing a method of forming a contact hole according to an exemplary embodiment;

[0058] Fig.17is a schematic diagram showing a method of forming a metal layer according to an exemplary embodiment. DETAILED DESCRIPTION

[0059] The present invention will be further described below in conjunction with the accompanying drawings and embodiments:

[0060] In order to clearly illustrate the technical features of the present solution, the present invention is described in detail below through specific implementation methods and in conjunction with the accompanying drawings. The disclosure below provides many different embodiments or examples for realizing different structures of the present invention. In order to simplify the disclosure of the present invention, the components and settings of specific examples are described below. In addition, the present invention may repeat reference numbers and / or letters in different examples. This repetition is for the purpose of simplification and clarity, and does not itself indicate the relationship between the various embodiments and / or settings discussed. It should be noted that the components illustrated in the accompanying drawings are not necessarily drawn to scale. The present invention omits the description of known components and processing techniques and processes to avoid unnecessary limitations on the present invention.

[0061] Figure 1 FIG. 1 is a schematic cross-sectional structure diagram of an SGT power MOS device with an integrated barrier pinch-off diode according to an exemplary embodiment. Figure 1 As shown, an SGT power MOS device with an integrated barrier pinch-off diode provided in an embodiment of the present invention comprises a drain region of the first conductivity type located at the bottom of the SGT power MOS device and an epitaxial layer 2 of the first conductivity type extending upward from the upper surface of the drain region 1, a trench 3 opening upward is arranged on the epitaxial layer 2, a thick oxide layer 4 is arranged on the bottom and the inner side surface of the lower end of the trench 3, a first polysilicon 5 is filled inside the thick oxide layer 4, and the upper surface of the first polysilicon 5 is flush with the upper surface of the thick oxide layer 4; a gate oxide layer 6 is arranged in the trench 3 above the first polysilicon 5, and the bottom of the gate oxide layer 6 is flush with the upper surface of the first polysilicon 5 and the upper surface of the thick oxide layer 4. The outer side of the gate oxide layer 6 is connected to the inner side of the upper end of the groove 3, and the second polysilicon 7 is filled inside the gate oxide layer 6, and the upper surface of the second polysilicon 7 is flush with the upper surface of the thick oxide layer 4; a well region layer 8 of a second conductivity type is arranged on the upper part of the epitaxial layer 2 and around the groove 3; a source region layer 9 is arranged above the well region layer 8 around the top of the groove, an insulating dielectric layer 10 is arranged above the source region layer 9 and the groove 3, and a plurality of contact holes 11 are opened on the insulating dielectric layer 10, and the contact holes 11 are connected to the epitaxial layer 2, the well region layer 8 and the source region layer 9; a metal region layer 12 is laid on the insulating dielectric layer 10; and the contact holes 11 are provided with metal.

[0062] In this embodiment, the trench 3 passes through the second conductive type well region layer 8 from top to bottom and extends to the inside of the first conductive type epitaxial layer 2. The thick oxide layer 4 in the trench contacts the lower part and the bottom of the inner side surface of the trench 3, forming a side end 14 of the thick oxide layer in the trench and a bottom end 13 of the thick oxide layer in the trench; the thick oxide layer 4 in the trench 3 encloses a first space, and the first polysilicon layer 5 is filled in the first space; and the gate oxide layer 5 encloses a second space, and the second polysilicon layer 7 is filled in the second space; the gate oxide layer 6 contacts the upper part of the inner side surface of the trench 3 and the top of the first polysilicon layer, forming a side end 16 of the gate oxide layer and a bottom end 15 of the gate oxide layer, and the gate oxide layer 6 is connected to the top of the thick oxide layer 4 located in the trench 3.

[0063] As a possible implementation of this embodiment, the horizontal cross-sectional area of ​​the first polysilicon 5 is not greater than the horizontal cross-sectional area of ​​the second polysilicon 7 .

[0064] As a possible implementation of this embodiment, the metal in the contact hole 11 is in contact with the first conductivity type epitaxial layer 2, the second conductivity type well region layer 8 and the source region layer 9. The contact hole passes through the insulating dielectric layer and is connected to the first conductivity type epitaxial layer and the second conductivity type well region layer.

[0065] As a possible implementation of this embodiment, the metal in the contact hole 11 forms an ohmic contact with the first conductivity type epitaxial layer 2 .

[0066] As a possible implementation of this embodiment, the horizontal cross-section of the groove 3 is a strip, a circle, a square, a rectangle or a polygon.

[0067] As a possible implementation of this embodiment, the shapes of the horizontal cross sections of the first polysilicon 5 and the second polysilicon 7 are the same as the shape of the horizontal cross section of the trench 3 but they are different in size.

[0068] As a possible implementation of this embodiment, the lower surface of the well region layer 8 is higher than the lower surface of the second polysilicon 7 , and the upper surface of the well region layer 8 is lower than the upper surface of the second polysilicon 7 .

[0069] As a possible implementation of this embodiment, the upper surface of the second polysilicon 7 is not lower than the lower surface of the source region layer 9 .

[0070] The SGT power MOS device with integrated barrier pinch-off diode of this embodiment integrates an input barrier pinch-off diode in the traditional SGT power MOS device structure, thereby improving the reverse recovery high-frequency characteristics of the SGT power MOS device and reducing the forward conduction power loss of the SGT power MOS device.

[0071] like Figures 2 to 17 As shown, a processing technology of a SGT power MOS device with an integrated barrier pinch-off diode provided in an embodiment of the present invention includes the following steps:

[0072] S1, a first conductive type drain region is formed on a silicon wafer, and a first conductive type epitaxial layer is formed by epitaxy upward on the upper surface of the drain region. Before forming the first conductive type epitaxial layer, a semiconductor substrate may be provided on the upper surface of the first conductive type drain region, and then the first conductive type epitaxial layer is formed on the semiconductor substrate.

[0073] S2, depositing silicon nitride on the upper surface of the epitaxial layer to form a hard mask.

[0074] The specific steps of forming the hard mask include: ① placing the silicon wafer after forming the first conductive type epitaxial layer in the reaction chamber; ② introducing ammonia and silane with a volume ratio of 3.3:1 into the reaction chamber after evacuating the chamber; the total volume of ammonia and silane is 2200sccm; the final pressure value of the reaction chamber is controlled to be 0.29mbar; ③ depositing the coating, the coating temperature is set to 370℃, and the RF power is set to 4500W. Deposit silicon nitride to form a hard mask with a thickness of 500nm, such as Figure 2 shown.

[0075] S3, etching a trench with an opening upward on the epitaxial layer by dry etching silicon nitride and dry etching silicon.

[0076] The specific steps of etching the groove on the epitaxial layer include: ① performing photoresist deposition, pre-baking, exposure, development, and hardening to cover the surface of the silicon wafer with a barrier layer; ② performing isotropic etching of silicon nitride; ③ performing isotropic deposition to cover the silicon etched surface, sidewalls, and photoresist surface with a barrier layer; ④ performing anisotropic etching to remove the barrier layer covering the etched surface and expose the etched surface; ⑤ performing isotropic etching of silicon; ⑥ repeating steps ③ to ⑤ until the predetermined etching depth is reached. The depth of the groove etched on the epitaxial layer is 7.5μm, such as Figure 3 shown.

[0077] S4, dry-etching the silicon nitride until it is completely etched and then stripping off the hard mask.

[0078] The specific steps of stripping the hard mask include: ① the magnetic field in the etching chamber is controlled at 30 Gauss; ② the pressure of the etching chamber is 100 mTorr; ③ the etching gas is introduced, the CF4 flow rate is 50sccm, the CHF3 flow rate is 50sccm, the CH3F flow rate is 50sccm, the auxiliary gas Ar flow rate is 100sccm, and the O2 flow rate is 100sccm; ④ the etching RF power is controlled at 300W. Figure 4 shown.

[0079] S5, oxidizing the thick oxide layer in the trench by using a wet oxygen oxidation method.

[0080] The specific steps of thick oxide layer oxidation include: ① raising the temperature of the oxidation furnace to 600℃; ② placing the silicon wafer in the oxidation furnace; ③ raising the temperature of the oxidation furnace to 1100℃; ④ maintaining the temperature of the oxidation furnace at 1100℃, introducing O2 at a flow rate of 3000sccm for 5min; ⑤ maintaining the temperature of the oxidation furnace at 1100℃, introducing O2 at a flow rate of 3000sccm and H2 at a flow rate of 4000sccm, igniting for 10min; ⑥ maintaining the temperature of the oxidation furnace at 1100℃, introducing O2 at a flow rate of 3000sccm for 5min. The thickness of the thick oxide layer in the groove is 300nm, such as Figure 5 shown.

[0081] S6, depositing polysilicon on the thick oxide layer.

[0082] The specific steps of depositing polysilicon include: ① introducing silane with a silane flow rate of 180 sccm; ② performing deposition at a temperature of 650°C, a gas pressure of 0.2 Torr, and a deposition time of 2 hours. The upper surface of the polysilicon deposited on the thick oxide layer is 2 μm higher than the upper surface of the thick oxide layer. Figure 6 shown.

[0083] S7, etching the polysilicon deposited on the thick oxide layer to form first polysilicon.

[0084] The specific steps of etching the polysilicon deposited on the thick oxide layer to form the first polysilicon include: ① introducing etching gas, with ammonia flow rate of 200 sccm and HF gas flow rate of 100 sccm; ② controlling the chamber pressure to 3 Torr and the temperature to 50°C; and etching time to 30 min. The depth of etching the polysilicon is 6 μm. Figure 7 shown.

[0085] S8, etching a thick oxide layer in the trench above the first polysilicon.

[0086] The specific steps of etching the thick oxide layer in the groove above the first polysilicon include: ① introducing etching gas, the flow rate of octafluorocyclobutane is 40sccm, and the flow rate of Ar gas is 80sccm; ② controlling the reaction gas pressure to 4mTorr; the RF power of the upper electrode is 1500W, and the RF power of the lower electrode is 500W; the etching time is 15min. Etching the oxide layer, the etching depth is 350nm, such as Figure 8 shown.

[0087] S9, using a dry oxygen oxidation method to oxidize to form a gate oxide layer.

[0088] The specific steps of using dry oxygen oxidation to oxidize and form a gate oxide layer include: ① raising the temperature of the oxidation furnace to 600℃; ② placing the silicon wafer in the oxidation furnace; ③ raising the temperature of the oxidation furnace to 900℃; ④ controlling the temperature of the oxidation furnace to 900℃, introducing an O2 flow rate of 3000sccm, and the oxidation time to 30min. The thickness of the gate oxide layer is 60nm. Fig. 9 shown.

[0089] S10, depositing polysilicon on the gate oxide layer.

[0090] The specific steps of depositing polysilicon on the gate oxide layer include: ① introducing silane with a silane flow rate of 180 sccm; ② performing deposition at a temperature of 650°C; a gas pressure of 0.2 Torr; and a deposition time of 1 hour. The upper surface of the polysilicon deposited on the gate oxide layer is 1 μm higher than the upper surface of the gate oxide layer. Fig.10 shown.

[0091] S11, etching the polysilicon deposited on the gate oxide layer to form second polysilicon.

[0092] The specific steps of etching the polysilicon deposited on the gate oxide layer to form the second polysilicon include: ① introducing etching gas, with ammonia flow rate of 200 sccm and HF gas flow rate of 100 sccm; ② controlling the chamber pressure to 3 Torr and the temperature to 50°C; and etching time to 30 min. Etching polysilicon, the etching depth is 1 μm, such as Fig.11 shown.

[0093] S12, implanting second conductivity type impurities into the upper part of the epitaxial layer and around the trench, such as Fig.12 As shown, a second conductivity type well region layer is formed.

[0094] The specific steps of implanting the second conductive type impurity include: ① implanting impurity ions of boron with a dose of 5×10 13 / cm 2 ; ② Control the relative atomic mass to 5, the charge to 1+, the energy to 90keV, and the angle to 7°.

[0095] S13, performing push-junction of the second conductivity type well region layer.

[0096] The specific steps of pushing the second conductive type well region layer include: ① raising the temperature of the diffusion furnace to 600℃; ② placing the silicon wafer in the diffusion furnace; ③ raising the temperature of the diffusion furnace to 1150℃; ④ controlling the temperature of the diffusion furnace to be constant at 1150℃, introducing N2 at a flow rate of 3000sccm, and pushing the junction for 90min. Fig.13 shown.

[0097] S14, injecting source region impurities above the well region layer around the top of the trench to form a source region layer, such as Fig.14 shown.

[0098] The specific steps of injecting impurities into the source region include: ① injecting impurity ions of phosphorus with a dose of 5×10 15 / cm 2 ;② Control the relative atomic mass to 15, charge to 1-, energy to 50keV, and angle to 7°.

[0099] S15, depositing silicon dioxide on the source region layer and the trench to form an insulating dielectric layer.

[0100] The specific steps of depositing silicon dioxide on the source region layer and the trench include: ① introducing 30 sccm of ethyl orthosilicate and 30 sccm of O2 gas into the reaction chamber; ② controlling the chamber pressure to 100 mTorr, the temperature to 700°C, and the deposition time to 120 min. Deposit silicon dioxide to form an insulating dielectric layer with a thickness of 1 μm, such as Fig.15 shown.

[0101] S16, dry-etching silicon dioxide on the insulating dielectric layer until it is completely etched, and dry-etching silicon to form a contact hole, wherein the contact hole passes through the insulating dielectric layer and is connected to the first conductive type epitaxial layer and the second conductive type well region layer, and the etching depth of the contact hole is 1 μm. Fig.16 shown.

[0102] The process of forming the contact hole includes two steps: etching silicon dioxide and etching silicon. The specific steps of etching silicon dioxide include: ① introducing etching gas, the flow rate of octafluorocyclobutane is 40sccm, and the flow rate of Ar gas is 80sccm; ② controlling the reaction gas pressure to 4mTorr, the upper electrode RF power to 1500W, the lower electrode RF power to 500W, and the etching time to 18min. The specific steps of etching silicon include: ① introducing etching gas, the flow rate of ammonia is 200sccm, and the flow rate of HF gas is 100sccm; ② controlling the chamber pressure to 3Torr, the temperature to 50℃, and the etching time to 5min.

[0103] S17, depositing metal on the insulating dielectric layer and in the contact holes to form a metal layer.

[0104] The specific steps of forming the metal layer include: ① injecting metal, ② controlling the vacuum degree of the chamber to 1×10 -7 Torr, temperature is 120℃, voltage is 10KV, current is 30A, and deposition time is 40min. A metal layer is deposited on the insulating dielectric layer to form a metal layer with a thickness of 4μm. Fig.17 shown.

[0105] The processing technology of the present invention is compatible with the traditional SGT power MOS device technology, does not require additional process steps and photomasks, and can be achieved by only adjusting the original individual photomasks and individual process conditions.

[0106] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.

Claims

1. An SGT power MOS device with an integrated barrier pinch-off diode, comprising a drain region (1) of a first conductivity type located at the bottom of the SGT power MOS device and an epitaxial layer (2) of the first conductivity type extending upward from the upper surface of the drain region (1), wherein The epitaxial layer (2) is provided with a groove (3) opening upward, an oxide layer (4) is provided on the bottom and the inner side surface of the lower end of the groove (3), and a first polysilicon (5) is filled inside the oxide layer (4), and the upper surface of the first polysilicon (5) is flush with the upper surface of the oxide layer (4); a gate oxide layer (6) is provided in the groove (3) above the first polysilicon (5), the bottom of the gate oxide layer (6) is connected to the upper surface of the first polysilicon (5) and the upper surface of the oxide layer (4), the outer side surface of the gate oxide layer (6) is connected to the inner side surface of the upper end of the groove (3), and a second polysilicon (7) is filled inside the gate oxide layer (6), and the upper surface of the second polysilicon (7) is flush with the upper surface of the gate oxide layer (6); a gate oxide layer (6) is provided on the upper part of the epitaxial layer (2) and located in the groove A second conductive type well region layer (8) is arranged around the groove (3); a source region layer (9) is arranged above the well region layer (8) around the top of the groove; an insulating dielectric layer (10) is arranged above the source region layer (9) and the groove (3); a plurality of contact holes (11) are opened on the insulating dielectric layer (10), and the contact holes (11) are connected to the epitaxial layer (2), the well region layer (8) and the source region layer (9); a metal region layer (12) is laid on the insulating dielectric layer (10); the contact holes (11) are provided with metal; the metal in the contact holes (11) is in contact with the first conductive type epitaxial layer (2), the second conductive type well region layer (8) and the source region layer (9) respectively; the metal in the contact holes (11) forms an ohmic contact with the first conductive type epitaxial layer (2).

2. The SGT power MOS device with integrated barrier pinch-off diode according to claim 1, characterized in that: The horizontal cross-sectional area of ​​the first polycrystalline silicon (5) is not greater than the horizontal cross-sectional area of ​​the second polycrystalline silicon (7).

3. The SGT power MOS device with integrated barrier pinch-off diode according to claim 1, characterized in that: The horizontal cross section of the groove (3) is circular or polygonal.

4. The SGT power MOS device with integrated barrier pinch-off diode according to claim 3, characterized in that: The shapes of the horizontal cross-sections of the first polysilicon (5) and the second polysilicon (7) are the same as the shape of the horizontal cross-section of the groove (3), but their sizes are different.

5. The SGT power MOS device with integrated barrier pinch-off diode according to claim 1, characterized in that: The lower surface of the well region layer (8) is higher than the lower surface of the second polysilicon (7), and the upper surface of the well region layer (8) is lower than the upper surface of the second polysilicon (7).

6. The SGT power MOS device with integrated barrier pinch-off diode according to claim 1, characterized in that: The upper surface of the second polysilicon (7) is not lower than the lower surface of the source region layer (9).

7. The processing technology of the SGT power MOS device with integrated barrier pinch-off diode according to any one of claims 1 to 6, characterized in that: The following steps are involved: A first conductive type drain region is formed on a silicon wafer, and a first conductive type epitaxial layer is formed by epitaxially growing upward from the upper surface of the drain region; Depositing silicon nitride on the upper surface of the epitaxial layer to form a hard mask; Etching a trench opening upward on the epitaxial layer by dry etching silicon nitride and dry etching silicon; Dry-etching silicon nitride until it is completely etched and then stripping off the hard mask; Oxidation of the oxide layer in the trench is performed by wet oxygen oxidation; Depositing polysilicon on the oxide layer, and etching the polysilicon deposited on the oxide layer to form first polysilicon; etching an oxide layer in the trench above the first polysilicon; A gate oxide layer is formed by oxidation using a dry oxygen oxidation method; Depositing polysilicon on the gate oxide layer, and etching the polysilicon deposited on the gate oxide layer to form a second polysilicon; Implanting second conductivity type impurities on the upper part of the epitaxial layer and around the trench to form a second conductivity type well region layer, and performing push-junction of the second conductivity type well region layer; Implanting source region impurities above the well region layer around the top of the trench to form a source region layer; Depositing silicon dioxide on the source region layer and the trench to form an insulating dielectric layer; Dry etching silicon dioxide on the insulating dielectric layer until it is completely etched, and dry etching silicon to form a contact hole; Depositing metal on the insulating dielectric layer and in the contact hole to form a metal layer; The specific steps of forming the hard mask include: ① placing the silicon wafer after forming the first conductive type epitaxial layer in the reaction chamber; ② introducing ammonia and silane with a volume ratio of 3.3:1 into the reaction chamber after evacuating the chamber; the total amount of ammonia and silane is 2200 sccm; the final pressure value of the reaction chamber is controlled to be 0.29 mbar; ③ depositing a coating, the coating temperature is set to 370°C, and the RF power is set to 4500W; The specific steps of etching the groove on the epitaxial layer include: ① performing photoresist deposition, pre-baking, exposure, development, and hardening to cover the barrier layer on the surface of the silicon wafer; ② performing isotropic etching of silicon nitride; ③ performing isotropic deposition to cover the barrier layer on the silicon etched surface, sidewalls, and the surface of the photoresist layer; ④ performing anisotropic etching to remove the barrier layer covering the etched surface to expose the etched surface; ⑤ performing isotropic etching of silicon; ⑥ repeating steps ③ to ⑤ until the predetermined etching depth is reached; The specific steps of stripping the hard mask include: ① the magnetic field in the etching chamber is controlled at 30 Gauss; ② the pressure of the etching chamber is 100 mTorr; ③ the etching gas is introduced, the CF4 flow rate is 50 sccm, the CHF3 flow rate is 50 sccm, the CH3F flow rate is 50 sccm, the auxiliary gas Ar flow rate is 100 sccm, and the O2 flow rate is 100 sccm; ④ the etching RF power is controlled to 300 W; The specific steps of oxidation of the oxide layer include: ① raising the temperature of the oxidation furnace to 600°C; ② placing the silicon wafer in the oxidation furnace; ③ raising the temperature of the oxidation furnace to 1100°C; ④ maintaining the temperature of the oxidation furnace at 1100°C, introducing O2 at a flow rate of 3000sccm for 5 minutes; ⑤ maintaining the temperature of the oxidation furnace at 1100°C, introducing O2 at a flow rate of 3000sccm and H2 at a flow rate of 4000sccm, and igniting for 10 minutes; ⑥ maintaining the temperature of the oxidation furnace at 1100°C, introducing O2 at a flow rate of 3000sccm for 5 minutes; The specific steps of using dry oxygen oxidation to oxidize and form a gate oxide layer include: ① raising the temperature of the oxidation furnace to 600°C; ② placing the silicon wafer in the oxidation furnace; ③ raising the temperature of the oxidation furnace to 900°C; ④ controlling the temperature of the oxidation furnace to be 900°C, introducing an O2 flow rate of 3000sccm, and the oxidation time to be 30min; The process of forming a contact hole includes two steps of etching silicon dioxide and etching silicon. The specific steps of etching silicon dioxide include: ① introducing etching gas, the flow rate of octafluorocyclobutane is 40sccm, and the flow rate of Ar gas is 80sccm; ② controlling the reaction gas pressure to 4 mTorr, the upper electrode RF power to 1500W, the lower electrode RF power to 500W, and the etching time to 18min; the specific steps of etching silicon include: ① introducing etching gas, the flow rate of ammonia is 200sccm, and the flow rate of HF gas is 100sccm; ② controlling the chamber pressure to 3 Torr, the temperature to 50°C, and the etching time to 5min.