Semiconductor structure and method for forming semiconductor structure

By forming a pseudo gate structure and a second opening design in the semiconductor structure, the isolation structure is ensured to be completely within the gate control range, which solves the problem of the fork-shaped nanosheet performance being affected by stress imbalance and improves the performance of the semiconductor structure.

CN113782602BActive Publication Date: 2024-10-22SEMICON MFG INT (SHANGHAI) CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010525162.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-06-10
Publication Date
2024-10-22
Estimated Expiration
2040-06-10

AI Technical Summary

Technical Problem

The performance of forked nanosheets has not yet reached its optimal state, mainly due to the stress imbalance caused by the large volume of the isolation structure, which affects the performance of the semiconductor structure.

Method used

By first forming a dummy gate structure in the semiconductor structure, then removing the dummy gate structure in the dielectric layer to form a vertically extending second opening, and finally forming an isolation structure at the bottom of the second opening, so that the isolation structure is completely within the gate structure. Within the control range, stress imbalance is avoided.

Benefits of technology

This effectively reduces the volume of the isolation structure and avoids the problem of stress imbalance, thus improving the performance of the semiconductor structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113782602B_ABST
    Figure CN113782602B_ABST
Patent Text Reader

Abstract

A semiconductor structure and a method for forming the semiconductor structure are disclosed. The structure includes: a substrate; a first nanostructure and a second nanostructure located on the substrate, with a first opening between the first nanostructure and the second nanostructure; an isolation structure located within a portion of the first opening; and a dielectric layer located on the substrate, the dielectric layer being located within a portion of the first opening, a portion of the sidewalls of the first nanostructure, and a portion of the sidewalls of the second nanostructure. The dielectric layer has a second opening, the extension direction of the second opening being perpendicular to the extension direction of the first opening, and the second opening exposing the isolation structure. The performance of the semiconductor structure is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the semiconductor structure. Background Art

[0002] FinFET transistor architecture is the main force in today's semiconductor industry. However, with the continuous miniaturization of devices, when the channel length is small to a certain value, the FinFET structure cannot provide sufficient electrostatic control and sufficient drive current. Therefore, the nanosheet structure, namely the gate-all-around technology (GAA), was introduced. Compared with the FinFET, the surrounding gate feature of the nanosheet provides excellent channel control capabilities. At the same time, the excellent distribution of the channel in three dimensions enables the optimization of the effective drive current per unit area.

[0003] As the journey towards smaller track heights continues, further reductions in cell height will require even smaller spacing between NMOS and PMOS devices within a standard cell. However, for FinFETs and nanosheets, the process limits the spacing between these NMOS and PMOS devices. To expand the scalability of these devices, an innovative architecture, called a forksheet device, has been proposed. A forksheet can be considered a natural extension of a nanosheet. Compared to a nanosheet, the channel of a forksheet is controlled by a forked gate structure, which is achieved by introducing a "dielectric wall" between the NMOS and PMOS devices before gate patterning. This wall physically isolates the NMOS gate trench from the PMOS gate trench, thereby significantly reducing the spacing between NMOS and PMOS, giving the forksheet better scalability in terms of area and performance.

[0004] However, the performance of fork-shaped nanosheets still needs to be improved. Summary of the Invention

[0005] The technical problem solved by the present invention is to provide a semiconductor structure and a method for forming the semiconductor structure, so as to improve the performance of fork-shaped nanosheets.

[0006] To solve the above technical problems, the technical solution of the present invention provides a semiconductor structure, comprising: a substrate; a first nanostructure and a second nanostructure located on the substrate, with a first opening between the first nanostructure and the second nanostructure; an isolation structure located within a portion of the first opening; a dielectric layer located on the substrate, the dielectric layer located within a portion of the first opening, a portion of the first nanostructure sidewall, and a portion of the second nanostructure sidewall, the dielectric layer having a second opening, an extension direction of the second opening being perpendicular to the extension direction of the first opening, and the second opening exposing the isolation structure.

[0007] Optionally, the second opening further exposes a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall; and the isolation structure is located at the bottom of the second opening.

[0008] Optionally, it further includes: a gate structure located in the second opening.

[0009] Optionally, the method further includes: a first isolation layer located on a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall, and the gate structure is located on the first isolation layer.

[0010] Optionally, the first nanostructure includes a plurality of first nanowires, and the plurality of first nanowires are separated from each other; the second nanostructure includes a plurality of second nanowires, and the plurality of second nanowires are separated from each other.

[0011] Optionally, the material of the isolation structure is different from the material of the dielectric layer.

[0012] Optionally, the material of the isolation structure includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbide nitride.

[0013] Correspondingly, the technical solution of the present invention also provides a method for forming a semiconductor structure, including: providing a substrate; forming an initial first nanostructure and an initial second nanostructure on the substrate, with a first opening between the initial first nanostructure and the initial second nanostructure; forming a dummy gate structure on part of the initial first nanostructure, part of the initial second nanostructure and part of the first opening, the dummy gate structure spanning the initial first nanostructure and the initial second nanostructure; forming a dielectric layer on the substrate, the dielectric layer being located on the sidewalls of the dummy gate structure, the sidewalls of the initial first nanostructure and the sidewalls of the initial second nanostructure; removing the dummy gate structure, forming a second opening in the dielectric layer, the extension direction of the second opening being perpendicular to the extension direction of the first opening, and the bottom of the second opening exposing part of the first opening; and forming an isolation structure in the part of the first opening exposed at the bottom of the second opening.

[0014] Optionally, the method of forming an isolation structure within the portion of the first opening exposed at the bottom of the second opening includes: forming an isolation material layer within the portion of the first opening and on the surface of the initial first nanostructure and the initial second nanostructure; removing the isolation material layer on the surface of the initial first nanostructure and the initial second nanostructure, and forming an isolation structure within the portion of the first opening.

[0015] Optionally, the process of forming the isolation material layer includes an atomic layer deposition process.

[0016] Optionally, the process of removing the isolation material layer on the surfaces of the initial first nanostructure and the initial second nanostructure includes a wet etching process.

[0017] Optionally, the material of the isolation structure is different from the material of the dielectric layer.

[0018] Optionally, the material of the isolation structure includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbide nitride.

[0019] Optionally, the initial first nanostructure includes several first composite layers, the first composite layers include first nanowires and a first sacrificial layer located on the first nanowires; the initial second nanostructure includes several second composite layers, the second composite layers include second nanowires and a second sacrificial layer located on the second nanowires; the second opening also exposes part of the sidewalls of the initial first nanostructure and part of the sidewalls of the initial second nanostructure.

[0020] Optionally, the method for forming the initial first nanostructure and the initial second nanostructure includes: forming a stacked material structure on a substrate, the stacked material structure including a plurality of nanowire material layers and a stack of sacrificial material layers located on the nanowire material layers; forming a mask layer on the stacked material structure, the mask layer exposing a portion of the surface of the sacrificial material layer; using the mask layer as a mask, removing a portion of the stacked material structure until the substrate surface is exposed, thereby forming the initial first nanostructure and the initial second nanostructure.

[0021] Optionally, before forming the dummy gate structure, the method further includes: forming a first isolation layer on the sidewall surface of the initial first nanostructure portion and the sidewall surface of the initial second nanostructure portion; and the dummy gate structure is located on the first isolation layer.

[0022] Optionally, after forming the isolation structure, the first sacrificial layer and the second sacrificial layer exposed by the second opening are removed to form the first nanostructure and the second nanostructure, and a fourth opening is formed between adjacent first nanowires and between adjacent second nanowires; a gate structure is formed within the second opening and the fourth opening, and the gate structure spans the isolation structure, the first nanostructure and the second nanostructure.

[0023] Optionally, before forming the dummy gate structure, the method further includes: forming a protective layer on the surface of the initial first nanostructure and the surface of the initial second nanostructure.

[0024] Optionally, the material of the protective layer includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbide nitride.

[0025] Optionally, after forming the isolation structure, the method further includes: removing the protective layer.

[0026] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0027] In the semiconductor structure in the technical solution of the present invention, the gate structure spans the isolation structure, the first nanostructure and the second nanostructure. In the extension direction of the first nanostructure and the second nanostructure, the width of the gate structure is the same as the width of the isolation structure, so that the isolation structure can be completely within the effective control range of the gate structure, thereby making the volume of the isolation structure smaller, thereby avoiding the problem of stress imbalance on both sides of the first nanostructure and the second nanostructure when the volume of the isolation structure is large, thereby improving the performance of the semiconductor structure.

[0028] The method for forming a semiconductor structure in the technical solution of the present invention first forms a dummy gate structure on a portion of an initial first nanostructure, a portion of an initial second nanostructure, and within a portion of a first opening, then forms a dielectric layer on a substrate, the dielectric layer being located on the sidewalls of the dummy gate structure, the sidewalls of the initial first nanostructure, and the sidewalls of the initial second nanostructure, then removes the dummy gate structure, forms a second opening in the dielectric layer, the second opening extending perpendicularly to the direction of the first opening, and the bottom of the second opening exposing a portion of the first opening, and finally forms an isolation structure within the portion of the first opening exposed at the bottom of the second opening. The method first forms the dummy gate structure, then removes the dummy gate structure to form a second opening, the bottom of the second opening exposing a portion of the first opening, while positioning the dielectric layer within the portion of the first opening, and then forms an isolation structure within the portion of the first opening exposed at the bottom of the second opening. When a gate structure is subsequently formed within the second opening, the isolation structure is completely within the effective control range of the gate structure, thereby reducing the size of the isolation structure and avoiding the problem of stress imbalance between the first and second nanostructures that occurs when the isolation structure is larger, thereby improving the performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figures 1 to 3 is a schematic cross-sectional structural diagram and a top view of a semiconductor structure in one embodiment;

[0030] Figures 4 to 15 It is a cross-sectional structural schematic diagram and a top view of the semiconductor structure forming process in an embodiment of the present invention. DETAILED DESCRIPTION

[0031] As described in the background art, the performance of existing fork-shaped nanosheets still needs to be improved. This will now be analyzed and explained in conjunction with specific embodiments.

[0032] Figures 1 to 3 It is a cross-sectional structural schematic diagram and a top view of a semiconductor structure forming process in one embodiment.

[0033] Please refer to Figure 1 , providing a substrate 100; forming a stacking structure on the substrate 100, the stacking structure including a plurality of composite layers, the composite layers including initial nanowires (not shown) and an initial sacrificial layer (not shown) located on the initial nanowires; forming a groove (not shown) in the stacking structure to form an initial first nanostructure and an initial second nanostructure, the initial first nanostructure including a composite layer of a plurality of first nanowires 101 and a first sacrificial layer 102 located on the first nanowires 101, the initial second nanostructure including a composite layer of a plurality of second nanowires 104 and a second sacrificial layer 105 located on the second nanowires 104; forming an isolation structure 103 in the groove; forming an isolation layer 106 on part of the sidewalls of the initial first nanostructure and the sidewalls of the initial second nanostructure.

[0034] Please refer to Figure 2 and Figure 3 , Figure 2 for Figure 3 Schematic diagram of the cross-section structure along the section line AA'. Figure 3 for Figure 2 The top view of the dielectric layer is omitted, and a dummy gate structure (not shown) is formed on the substrate, wherein the dummy gate structure spans the isolation structure 103, the initial first nanostructure and the initial second nanostructure; a dielectric layer (not shown) is formed on the substrate, wherein the dielectric layer is located on the sidewall of the dummy gate structure; the dummy gate structure is removed, and an initial gate opening (not shown) is formed in the dielectric layer to form the first nanostructure and the second nanostructure; the first sacrificial layer 102 and the second sacrificial layer 105 exposed by the initial gate opening are removed to form a gate opening (not shown); and a gate structure 107 is formed in the gate opening.

[0035] During the process of forming the semiconductor structure, an isolation structure 103 is first formed within the stacked structure, and then a dummy gate structure is formed on the isolation structure 103, the initial first nanostructure, and the initial second nanostructure. Finally, a gate-last process is used to form the gate structure 107. Since the isolation structure 103 is formed first, the size of the isolation structure 103 is larger. This allows the gate structure 107, which spans the isolation structure 103, the first nanostructure, and the second nanostructure, to cover the surface of the isolation structure 103 when the gate structure 107 is subsequently formed. This allows the first nanostructure and the second nanostructure to be electrically isolated from each other.

[0036] However, the material of the isolation structure 103 is typically a material with a high dielectric constant, such as silicon nitride, to prevent electromigration of the device formed by the subsequent first and second nanostructures. Furthermore, the material of the isolation structure 103 needs to be different from that of the dielectric layer to prevent damage to the isolation structure 103 during etching of the dielectric layer in the back-end process. Consequently, the thermal expansion coefficients of the materials of the isolation structure 103 and the dielectric layer differ. In the area not covered by the gate structure 107, the isolation structure 103 and the dielectric layer are located on either side of the first nanostructure, and the isolation structure 103 and the dielectric layer are located on either side of the second nanostructure. Consequently, the stresses on both sides of the first and second nanostructures are unbalanced, causing the first and second nanostructures to bend and deform, thereby affecting the performance of the semiconductor structure.

[0037] To address the above-mentioned problems, the technical solution of the present invention provides a semiconductor structure and its performance. The method comprises first forming a dummy gate structure on a portion of an initial first nanostructure, a portion of an initial second nanostructure, and within a portion of a first opening, then forming a dielectric layer on a substrate, the dielectric layer being located on the sidewalls of the dummy gate structure, the sidewalls of the initial first nanostructure, and the sidewalls of the initial second nanostructure. The dummy gate structure is then removed, and a second opening is formed in the dielectric layer. The second opening extends in a direction perpendicular to the direction of the first opening, and the bottom of the second opening exposes a portion of the first opening. Finally, an isolation structure is formed within the portion of the first opening exposed at the bottom of the second opening. The method first forms the dummy gate structure, then removes the dummy gate structure to form a second opening, the bottom of the second opening exposes a portion of the first opening, and then forms an isolation structure within the portion of the first opening exposed at the bottom of the second opening. Thus, when a gate structure is subsequently formed within the second opening, the isolation structure can be completely within the effective control range of the gate structure, thereby reducing the volume of the isolation structure and avoiding the problem of stress imbalance between the first nanostructure and the second nanostructure when the isolation structure is larger, thereby improving the performance of the semiconductor structure.

[0038] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0039] Figures 4 to 15 It is a cross-sectional structural schematic diagram and a top view of the semiconductor structure forming process in an embodiment of the present invention.

[0040] Please refer to Figure 4 , providing a substrate 200.

[0041] In this embodiment, the substrate 200 is made of silicon.

[0042] In other embodiments, the substrate material includes silicon carbide, silicon germanium, a multinary semiconductor material composed of group III-V elements, silicon-on-insulator (SOI), or germanium-on-insulator (GOI). The multinary semiconductor material composed of group III-V elements includes InP, GaAs, GaP, InAs, InSb, InGaAs, or InGaAsP.

[0043] Please refer to Figure 5 An initial first nanostructure and an initial second nanostructure are formed on a substrate 200 , with a first opening 205 between the initial first nanostructure and the initial second nanostructure.

[0044] The initial first nanostructure includes a plurality of first composite layers, each of which includes a first nanowire 201 and a first sacrificial layer 202 located on the first nanowire 201 .

[0045] The initial second nanostructure includes a plurality of second composite layers, each of which includes a second nanowire 203 and a second sacrificial layer 204 located on the second nanowire 203 .

[0046] The method for forming the initial first nanostructure and the initial second nanostructure includes: forming a stacked material structure (not shown) on a substrate 200, wherein the stacked material structure includes a plurality of nanowire material layers (not shown) and a stack of sacrificial material layers (not shown) located on the nanowire material layers; forming a mask layer (not shown) on the stacked material structure, wherein the mask layer exposes a portion of the surface of the sacrificial material layer; using the mask layer as a mask, removing a portion of the stacked material structure until the surface of the substrate 200 is exposed, thereby forming the initial first nanostructure, the initial second nanostructure and the first opening 205.

[0047] Please refer to Figure 6 , forming a protective layer 206 on the surface of the initial first nanostructure and the surface of the initial second nanostructure.

[0048] The protective layer 206 can protect the surface of the initial first nanostructure and the surface of the initial second nanostructure, thereby preventing the initial first nanostructure and the initial second nanostructure from being damaged during subsequent processes.

[0049] The protective layer 206 may be made of a dielectric material, including one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbon nitride, and silicon carbon nitride oxynitride. The protective layer 206 may be formed using a chemical vapor deposition (CVD) process or an atomic layer deposition (ALD) process.

[0050] In this embodiment, the material of the protective layer 206 includes silicon nitride; the process of forming the protective layer 206 includes an atomic layer deposition process, and the atomic layer deposition process can form a protective layer 206 with a dense structure and a relatively thin thickness.

[0051] In other embodiments, the protective layer may not be formed.

[0052] Please continue to refer to Figure 6 After forming the protection layer 206 , a first isolation layer 207 is formed on the sidewall surface of the initial first nanostructure portion and the sidewall surface of the initial second nanostructure portion.

[0053] The method for forming the first isolation layer 207 includes: forming an isolation material layer (not shown) on the substrate 200; planarizing the isolation material layer until the surface of the protective layer 206 is exposed to form an initial isolation structure (not shown); and etching back the initial isolation structure to form the first isolation layer 207.

[0054] The material of the first isolation layer 207 includes a dielectric material, and the dielectric material includes one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbon nitride, and silicon carbon nitride oxynitride. In this embodiment, the material of the first isolation layer 207 includes silicon oxide.

[0055] The first isolation layer 207 exposes the sidewall surfaces of the first sacrificial layer 202 and the second sacrificial layer 204 to prevent the first isolation layer 207 from blocking the subsequent removal process of the first sacrificial layer 202 and the second sacrificial layer 204 .

[0056] Please refer to Figure 7 and 8 , Figure 7 for Figure 8 Schematic diagram of the cross-section structure along the section line BB'. Figure 8 for Figure 7 In the top view, a dummy gate structure 208 is formed on part of the initial first nanostructure, part of the initial second nanostructure and part of the first opening 205, and the dummy gate structure 208 spans the initial first nanostructure and the initial second nanostructure, and the dummy gate structure 208 is located on the first isolation layer 207.

[0057] The dummy gate structure 208 includes a dummy gate dielectric layer (not shown) and a dummy gate layer (not shown) located on the dummy gate dielectric layer. The dummy gate dielectric layer is made of silicon oxide or a low-K (K less than 3.9) material; and the dummy gate layer is made of polysilicon.

[0058] The method for forming the dummy gate structure 208 is a common process in the art and will not be described in detail here.

[0059] Please refer to Figure 9 , Figure 9 For Figure 8 Based on the schematic diagram, a dielectric layer 209 is formed on the substrate 200 , and the dielectric layer 209 is located on the sidewalls of the dummy gate structure 208 , the sidewalls of the initial first nanostructure, and the sidewalls of the initial second nanostructure.

[0060] First, a dummy gate structure is formed on part of the initial first nanostructure, part of the initial second nanostructure and part of the first opening 205, and then a dielectric layer 209 is formed on the substrate 200. The dielectric layer 209 is located on the sidewalls of the dummy gate structure 208, the sidewalls of the initial first nanostructure and the sidewalls of the initial second nanostructure, so that the dielectric layer 209 is also located in part of the first opening 205, and then the dummy gate structure is removed to form a second opening, and the bottom of the second opening exposes part of the first opening, and then an isolation structure is formed in the part of the first opening exposed at the bottom of the second opening, so that when a gate structure is subsequently formed in the second opening, the isolation structure can be completely within the effective control range of the gate structure, so that the volume of the isolation structure is small, thereby avoiding the problem of stress imbalance on both sides of the first nanostructure and the second nanostructure when the volume of the isolation structure is large.

[0061] The method for forming the dielectric layer 209 includes: forming a dielectric material layer (not shown) on the substrate 200, the sidewalls of the dummy gate structure 208, the initial first nanostructure sidewalls, and the initial second nanostructure sidewalls; and planarizing the dielectric material layer until the top surface of the dummy gate structure 208 is exposed to form the dielectric layer 209.

[0062] The dielectric layer 209 is made of a dielectric material, which may be a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbon nitride, and silicon carbon nitride oxynitride. In this embodiment, the dielectric layer 209 is made of silicon oxide.

[0063] Please refer to Figure 10 and Figure 11 , Figure 10 for Figure 11 Schematic diagram of the cross-section structure along the section line CC'. Figure 11 for Figure 10 In the top view, the dummy gate structure 208 is removed, and a second opening 210 is formed in the dielectric layer 209. The extension direction of the second opening 210 is perpendicular to the extension direction of the first opening 205. The bottom of the second opening 210 exposes a portion of the first opening 205.

[0064] The second opening 210 also exposes a portion of the sidewall of the initial first nanostructure and a portion of the sidewall of the initial second nanostructure.

[0065] The process of removing the dummy gate structure 208 includes a dry etching process and a wet etching process or a combination of one or more of the above.

[0066] Please refer to Figure 12 and Figure 13 , Figure 12 for Figure 13 Schematic diagram of the cross-section structure along the section line DD'. Figure 13 for Figure 12 In the top view, an isolation structure 211 is formed in the portion of the first opening 205 exposed at the bottom of the second opening 210.

[0067] The method for forming an isolation structure 211 in the portion of the first opening 205 exposed at the bottom of the second opening 210 includes: forming an isolation material layer (not shown) in the portion of the first opening 205, on the surface of the initial first nanostructure, on the surface of the initial second nanostructure, and on the surface of the dielectric layer 209; and removing the isolation material layer on the surface of the initial first nanostructure, on the surface of the initial second nanostructure, and on the surface of the dielectric layer 209 to form an isolation structure 211 in the portion of the first opening 205.

[0068] The process of forming the isolation material layer includes an atomic layer deposition process or a chemical vapor deposition process.

[0069] In this embodiment, the process of forming the isolation material layer includes an atomic layer deposition process.

[0070] The process of removing the isolation material layer on the surfaces of the initial first nanostructure and the initial second nanostructure includes a wet etching process or an isotropic dry etching process.

[0071] The material of the isolation structure 211 is different from that of the dielectric layer 209 , so when removing the isolation material layer on the surface of the initial first nanostructure, the surface of the initial second nanostructure, and the surface of the dielectric layer 209 , the etching process causes less damage to the dielectric layer 209 .

[0072] The material of the isolation structure 211 includes a dielectric material, and the dielectric material includes one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbon nitride, and silicon carbon nitride oxynitride. In this embodiment, the material of the isolation structure 211 includes silicon nitride.

[0073] At this point, the isolation structure 211 formed has a width that is the same as the width of the pseudo gate structure 209 in the extension direction of the initial first nanostructure and the initial second nanostructure. After the gate structure is subsequently formed in the second opening 210, the width of the gate structure is the same as the width of the isolation structure, so that the isolation structure can be completely within the effective control range of the gate structure, thereby making the volume of the isolation structure smaller, thereby avoiding the problem of stress imbalance on both sides of the first nanostructure and the second nanostructure when the isolation structure is large, thereby improving the performance of the semiconductor structure.

[0074] Please continue to refer to Figure 12 and Figure 13 After forming the isolation structure 211 , the protection layer 206 exposed by the second opening 210 is removed.

[0075] The process of removing the protection layer 206 includes a wet etching process or an isotropic dry etching process.

[0076] Please refer to Figure 14 and Figure 15 , Figure 14 for Figure 15 Schematic diagram of the cross-section structure along the section line EE'. Figure 15 for Figure 14 In the top view, after removing the protective layer 206, the first sacrificial layer 202 and the second sacrificial layer 204 exposed by the second opening 210 are removed to form a first nanostructure and a second nanostructure, and a fourth opening (not shown) is formed between adjacent first nanowires 201 and between adjacent second nanowires 203; a gate structure 212 is formed in the second opening 210 and the fourth opening, and the gate structure 212 spans the isolation structure 211, the first nanostructure and the second nanostructure.

[0077] The gate structure 212 includes a gate dielectric layer (not shown) and a gate layer (not shown) located on the gate dielectric layer. In this embodiment, the gate structure 212 further includes a work function layer (not shown) located between the gate dielectric layer and the gate layer.

[0078] The material of the gate dielectric layer includes a high dielectric constant material, the dielectric constant of the high dielectric constant material is greater than 3.9, and the high dielectric constant material includes aluminum oxide or hafnium oxide; the material of the gate layer includes a metal, and the metal includes tungsten; the material of the work function layer includes an N-type work function material or a P-type work function material, the N-type work function material includes titanium aluminum, and the P-type work function material includes titanium nitride or tantalum nitride.

[0079] Accordingly, the embodiment of the present invention further provides a semiconductor structure, please continue to refer to Figure 14 and Figure 15 ,include:

[0080] substrate 200;

[0081] A first nanostructure and a second nanostructure are located on the substrate 200, with a first opening (not shown) between the first nanostructure and the second nanostructure;

[0082] an isolation structure 211 located within a portion of the first opening;

[0083] A dielectric layer 209 is located on the substrate 200, and the dielectric layer 209 is located in part of the first opening, part of the first nanostructure sidewall and part of the second nanostructure sidewall. The dielectric layer 209 has a second opening (not shown), and the extension direction of the second opening is perpendicular to the extension direction of the first opening. The second opening exposes the isolation structure 211.

[0084] In this embodiment, the second opening further exposes a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall; the isolation structure 211 is located at the bottom of the second opening.

[0085] In this embodiment, the device further includes a gate structure 212 located in the second opening.

[0086] In this embodiment, the present invention further includes: a first isolation layer 207 located on a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall, and the gate structure 212 is located on the first isolation layer 207 .

[0087] In this embodiment, the first nanostructure includes a plurality of first nanowires 201 , and the plurality of first nanowires 201 are separated from each other; the second nanostructure includes a plurality of second nanowires 203 , and the plurality of second nanowires 203 are separated from each other.

[0088] In this embodiment, the material of the isolation structure 211 is different from the material of the dielectric layer.

[0089] In this embodiment, the material of the isolation structure 211 includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbide nitride.

[0090] The semiconductor structure, the gate structure 212 spans the isolation structure 211, the first nanostructure and the second nanostructure. In the extension direction of the first nanostructure and the second nanostructure, the width of the gate structure 212 is the same as the width of the isolation structure 211, so that the isolation structure 211 can be completely within the effective control range of the gate structure 212, thereby making the volume of the isolation structure 211 smaller, thereby avoiding the problem of stress imbalance on both sides of the first nanostructure and the second nanostructure when the isolation structure 211 is larger, thereby improving the performance of the semiconductor structure.

[0091] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be based on the scope defined by the claims.

Claims

1. A semiconductor structure, characterized in that: include: substrate; A first nanostructure and a second nanostructure are located on a substrate, wherein a first opening is formed between the first nanostructure and the second nanostructure; an isolation structure located within a portion of the first opening; A dielectric layer located on the substrate, the dielectric layer is located in a portion of the first opening, a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall, the dielectric layer has a second opening, the extension direction of the second opening is perpendicular to the extension direction of the first opening, the second opening exposes the isolation structure, the second opening also exposes a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall, and the isolation structure is located at the bottom of the second opening; A gate structure is located in the second opening.

2. The semiconductor structure according to claim 1, wherein: Also includes: A first isolation layer is located on a portion of the first nanostructure sidewall and a portion of the second nanostructure sidewall, and the gate structure is located on the first isolation layer.

3. The semiconductor structure according to claim 1, wherein: The first nanostructure includes a plurality of first nanowires, and the plurality of first nanowires are separated from each other; the second nanostructure includes a plurality of second nanowires, and the plurality of second nanowires are separated from each other.

4. The semiconductor structure according to claim 1, wherein: The material of the isolation structure is different from the material of the dielectric layer.

5. The semiconductor structure according to claim 4, characterized in that The material of the isolation structure includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbide nitride.

6. A method for forming a semiconductor structure, characterized in that: include: providing a substrate; Forming an initial first nanostructure and an initial second nanostructure on a substrate, wherein a first opening is provided between the initial first nanostructure and the initial second nanostructure; forming a dummy gate structure on a portion of the initial first nanostructure, on a portion of the initial second nanostructure, and in a portion of the first opening, wherein the dummy gate structure spans the initial first nanostructure and the initial second nanostructure; Forming a dielectric layer on the substrate, wherein the dielectric layer is located on the sidewalls of the dummy gate structure, the sidewalls of the initial first nanostructure, and the sidewalls of the initial second nanostructure; The dummy gate structure is removed to form a second opening in the dielectric layer, wherein the extension direction of the second opening is perpendicular to the extension direction of the first opening, and the bottom of the second opening exposes a portion of the first opening; An isolation structure is formed in a portion of the first opening exposed at the bottom of the second opening.

7. The method for forming a semiconductor structure according to claim 6, wherein: The method for forming an isolation structure in a portion of the first opening exposed at the bottom of the second opening includes: forming an isolation material layer in a portion of the first opening and on the surface of the initial first nanostructure and the initial second nanostructure; removing the isolation material layer on the surface of the initial first nanostructure and the initial second nanostructure to form an isolation structure in a portion of the first opening.

8. The method for forming a semiconductor structure according to claim 7, wherein: The process of forming the isolation material layer includes an atomic layer deposition process.

9. The method for forming a semiconductor structure according to claim 7, wherein: The process of removing the isolation material layer on the surface of the initial first nanostructure and the initial second nanostructure includes a wet etching process.

10. The method for forming a semiconductor structure according to claim 6, wherein: The material of the isolation structure is different from the material of the dielectric layer.

11. The method for forming a semiconductor structure according to claim 10, wherein: The material of the isolation structure includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbide nitride.

12. The method for forming a semiconductor structure according to claim 6, wherein: The initial first nanostructure includes a plurality of first composite layers, wherein the first composite layers include a first nanowire and a first sacrificial layer located on the first nanowire; the initial second nanostructure includes a plurality of second composite layers, wherein the second composite layers include a second nanowire and a second sacrificial layer located on the second nanowire; the second opening also exposes a portion of the initial first nanostructure sidewall and a portion of the initial second nanostructure sidewall.

13. The method for forming a semiconductor structure according to claim 12, wherein: The method for forming the initial first nanostructure and the initial second nanostructure includes: forming a stacked material structure on a substrate, the stacked material structure including a plurality of nanowire material layers and a stack of sacrificial material layers on the nanowire material layers; forming a mask layer on the stacked material structure, the mask layer exposing a portion of the surface of the sacrificial material layer; using the mask layer as a mask, removing a portion of the stacked material structure until the substrate surface is exposed, thereby forming the initial first nanostructure and the initial second nanostructure.

14. The method for forming a semiconductor structure according to claim 12, wherein: Before forming the dummy gate structure, the method further includes: forming a first isolation layer on the side wall surface of the initial first nanostructure portion and the side wall surface of the initial second nanostructure portion; and the dummy gate structure is located on the first isolation layer.

15. The method for forming a semiconductor structure according to claim 12, wherein: After forming the isolation structure, removing the first sacrificial layer and the second sacrificial layer exposed by the second opening, forming the first nanostructure and the second nanostructure, and forming a fourth opening between adjacent first nanowires and between adjacent second nanowires; A gate structure is formed in the second opening and in the fourth opening, the gate structure spanning the isolation structure, the first nanostructure, and the second nanostructure.

16. The method for forming a semiconductor structure according to claim 6, wherein: Before forming the dummy gate structure, the method further includes: forming a protective layer on the surface of the initial first nanostructure and the surface of the initial second nanostructure.

17. The method for forming a semiconductor structure according to claim 16, wherein: The material of the protective layer includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbide nitride.

18. The method for forming a semiconductor structure according to claim 17, wherein: After forming the isolation structure, the method further includes: removing the protective layer.