A wireless passive resistance corrosion monitoring method and system
By embedding flexible corrosion probes during pipeline manufacturing and using mutual inductance coils for wireless data acquisition, the problems of opening and bus cable restrictions in the prior art are solved, and contactless and non-destructive pipeline corrosion monitoring is achieved, which is suitable for The narrow space improves the flexibility and efficiency of the monitoring system.
Patent Information
- Application Number
- CN202111062024.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-10
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2041-09-10
AI Technical Summary
The existing pipeline resistance probe corrosion monitoring technology requires opening holes to destroy the pipeline structure, occupying a large space, and data transmission relies on bus cables, limiting the flexibility and efficiency of the monitoring system.
Using wireless passive resistive corrosion monitoring method, by embedding flexible corrosion probes in the pipeline manufacturing process, wireless data acquisition is performed using mutual inductance coils and signal generators, and a gain curve is drawn to determine the degree of corrosion, avoiding the opening and bus cables. use.
It realizes contactless and non-destructive monitoring of pipeline corrosion, occupies a small volume, is suitable for narrow spaces, and can monitor pipeline corrosion rates in real time, improving the flexibility and efficiency of the monitoring system.
Smart Images

Figure CN113820362B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of pipeline corrosion detection, and in particular to a wireless passive resistance probe pipeline corrosion detection method and system. Background Art
[0002] As human beings' demand for energy continues to grow, the storage and transportation safety of energy has received more and more attention. Among them, the anti-corrosion of oil and gas pipelines is of utmost importance. In the actual use process, many factors will directly lead to the corrosion of pipelines. Therefore, some equipment pipelines are added with an outer protective layer during the manufacturing process to ensure the anti-corrosion safety of oil and gas transportation pipelines. Due to the large-scale refining of high-sulfur crude oil in recent years, oil and gas field pipelines contain a large amount of corrosive media such as chloride ions, carbon dioxide, hydrogen sulfide, dissolved oxygen, bacteria, etc. in daily production and transportation, which will cause internal corrosion of the pipeline. On the other hand, the complex environment such as humidity and high temperature outside the pipeline will make the outer protective layer of the pipeline ineffective, and then cause serious corrosion to the pipeline.
[0003] Commonly used pipeline corrosion monitoring methods include hanging film method, resistance probe method, electrochemical method, magnetic induction method, etc. Since the resistance probe method is suitable for electrolyte and non-electrolyte corrosive media and has low cost, it has been widely used in oil fields and other fields. The principle is that the corrosion products (such as metal oxides, etc.) produced by metals during the corrosion process are mostly non-conductive substances. If a current is passed through a metal sheet, then as the corrosion proceeds, the thickness of the energized metal sheet will decrease, thereby increasing its energized resistance. By measuring the resistance change of the metal specimen during the corrosion process, the corrosion loss and corrosion rate data can be obtained. The resistance probe method originated in the 1950s. During this period, the resolution and sensitivity of the probe were improved by reasonably adjusting the probe structure. After the early 21st century, coating technology was introduced into the preparation of resistance probe materials, and magnetron sputtering technology was used to prepare probe materials, which greatly reduced the thickness of the resistance probe metal specimen and increased the initial resistance. Many advances have been made in improving the measurement accuracy and stability of the probe.
[0004] In the existing pipeline resistance probe corrosion monitoring technology, since the sensitive element of the resistance probe needs to be attached to the probe rod, one end of the data transmission line must be connected to the sensitive element, and the other end must be connected to the external monitoring equipment through an aviation connector. This requires opening a hole in the on-site process pipeline and connecting it with a flange, which not only causes great damage to the original structure of the pipeline, but also occupies a large amount of space and is not suitable for pipeline monitoring in a narrow space. On the other hand, most of the current online resistance probe corrosion monitoring systems use bus transmission technology for data transmission, and it is necessary to lay a data transmission cable between the equipment monitoring point and the monitoring room, which will be subject to many restrictions, such as bus length, the number of connected monitoring equipment, etc. Often, multiple data transmission bus cables need to be laid in one site to meet the needs of the corrosion monitoring system, resulting in a large waste of manpower and material resources.
[0005] Therefore, it is necessary to propose a wireless resistance probe monitoring method and system that does not require opening holes to destroy the original structure of the pipeline, occupies a small volume, and obtains probe data non-contact. Summary of the invention
[0006] The purpose of the present invention is to provide a wireless passive resistance corrosion monitoring method and system to solve the problems raised in the above background technology.
[0007] To achieve the above object, the present invention provides the following technical solutions:
[0008] A wireless passive resistance corrosion monitoring method comprises the following steps:
[0009] S101, prepare a pipeline to be tested with a flexible corrosion probe embedded therein; and when a service environment is selected, embed the prepared flexible corrosion probe between the protective layer and the reinforcement layer of the pipeline during pipeline processing; the flexible corrosion probe includes an inductor coil L R and a sensitive element; the sensitive element is composed of a plurality of resistors, and the resistance values of the plurality of resistors gradually increase as the pipeline corrosion proceeds;
[0010] S102, wrapping the outer wall of the pipeline with a flexible detection probe, wherein the flexible detection probe comprises a signal generator V1, a fixed resistor R1 and an inductor L T , thereby determining a fixed mutual inductance coil spacing H1, which is used to receive the detection signal voltage value Uni at both ends of the fixed resistor R1 under continuous n frequency excitation with an excitation voltage with an amplitude of Ui; when the probe coating position has been corroded for a certain period, the detection signal at both ends of the fixed resistor R1 of the detection probe is received, and a finite number of continuously increasing detection frequencies f1 are obtained in each corrosion period Ti. <f2<……<f n-1 <f n The detection signal voltage value U generated at both ends of the fixed resistor R1 1i , U2i ,……,U (n-1)i , U ni , used to draw sampling point-gain curves for different corrosion cycles;
[0011] S103, select s sampling points, the sampling points are selected to be equally spaced, and the voltage gain G=10log at each frequency sampling point is calculated for the n frequencies. 10 (U o / U i ), the single point value of the voltage value Uni at both ends of the fixed resistor R1 is U o , calculating the gain of the detection signal voltage value obtained based on the change in the resistance value of the sensitive element of the corrosion probe embedded in the pipeline at the detection probe end under the fixed mutual inductance coil spacing;
[0012] S104, drawing a sampling point-gain curve, calculating the gain G of the excitation voltage with an amplitude of Ui for the detection signal voltage value Uni under the fixed mutual inductance coil spacing H1, and drawing a curve of the gain G with respect to the number of sampling points;
[0013] S105. Comprehensively considering the curve characteristics, determine the increase value of the resistance value of the embedded sensitive element, so as to reflect the degree of corrosion.
[0014] Preferably, the detection signal voltage value Uni is used to calculate the gain G of the excitation voltage with an amplitude of Ui, and the detection signal voltage value is obtained by means of labview software control and matlab software programming to calculate the gain of the detection signal; the sampling point-gain curve is drawn, and the increase value of the resistance value of the sensitive element is determined, thereby reflecting the degree of corrosion.
[0015] Preferably, in said S103, the sampling points are selected to be processed with equal intervals, and are determined according to the resistance characteristics of the embedded sensitive element; in said S103, the number of sampling points selected is s, which is determined according to the required drawing resolution and is greater than 1000.
[0016] Compared with the prior art, the present invention has the following beneficial effects:
[0017] The wireless passive resistance corrosion monitoring method and system can be used to detect corrosion events of a single pipeline or equipment without contact, and monitor the integrated corrosion rate of the pipeline or equipment over a period of time; it has the advantages of not requiring opening holes to destroy the original structure of the pipeline, occupying a small volume, and being able to obtain probe data without contact. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 A schematic diagram of a wireless passive corrosion monitoring method based on mutual inductance effect provided in Embodiment 1 of the present invention;
[0019] Figure 2 A schematic diagram of the structure of the corrosion probe provided by the present invention being embedded in a multi-layer pipeline having an outer protective layer provided by the background art;
[0020] Figure 3 A schematic cross-sectional view of a structure in which a flexible corrosion probe provided by the present invention is embedded in a multi-layer pipeline;
[0021] Figure 4 The basic principle diagram of the wireless passive corrosion monitoring method circuit provided by the invention;
[0022] Figure 5 A schematic diagram of multiple resistors of a specially made sensitive element provided in Embodiment 1 of the present invention;
[0023] Figure 6 A curve diagram of the gain G at the above sampling points provided in the second embodiment of the present invention;
[0024] Figure numerals: 1. inner lining layer; 2. reinforcement layer; 3. corrosion probe body; 4. outer protective layer. DETAILED DESCRIPTION
[0025] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments; based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0026] Figure 1 The diagram depicts the embedded structure of the corrosion probe body in a typical pipe with an outer protective layer. This embedded installation method is completed when the pipe is manufactured, avoiding the situation of drilling holes in the detection pipe on site and connecting the data transmission system with flanges. It has little damage to the strength of the pipe and occupies less space, and is suitable for pipeline corrosion detection in narrow areas.
[0027] exist Figure 2 and Figure 3 In the figure, the typical structure includes: an inner lining layer 1, a reinforcement layer 2, and an outer protective layer 4; and the corrosion probe body 3 is pre-embedded between the outer protective layer 4 and the reinforcement layer 2; according to the corrosion monitoring part of interest, the sensor can be installed circumferentially or axially to achieve different monitoring purposes.
[0028] Figure 4 The basic principle diagram of the wireless passive detection circuit provided by the method of the present invention is given; the left side is the detection probe end, which includes a signal generator V1 for generating AC sinusoidal excitation signals of various frequencies; a fixed resistor R1, which serves as the output end of the detection signal, and an inductor L TThe right side shows the flexible corrosion probe body embedded in the pipeline, including the inductor coil L R , used to detect the probe end inductance coil L T A mutual inductance coil is formed to obtain wireless passive internal corrosion information; the sensitive element is composed of multiple specially made resistors.
[0029] In particular, Figure 5 It is a schematic diagram of multiple resistors of the above-mentioned special sensitive element. Its original resistance R0 can be determined by the number of resistors and the length and thickness of each resistor line. The size of the resistance R0 can be defined by oneself according to needs. Except for the square part connected to the circuit, the remaining resistors are exposed wires made of the same material as the pipeline lining layer without an anti-corrosion layer. In the initial state, the resistance value of the sensitive element is R0. When the external complex environment causes the outer protective layer of the pipeline to fail or the pipeline corrodes from the inside and causes the reinforcement layer to rupture, the exposed wire will be gradually corroded, causing the resistance of the entire embedded probe to change. The changed resistance is R0+ΔR.
[0030] In the embodiment of the present invention, when the method is applied, it is ensured that when the mutual inductance method is used to measure the signal at both ends of the detection probe resistor R1 for multiple times, the distance between the excitation probe and the inductance coil embedded in the flexible corrosion probe body remains unchanged; according to the mutual inductance circuit principle, when the resistance of the sensitive element in the flexible corrosion probe body embedded in the pipeline changes, it will inevitably cause the impedance of this end to change, and further react to the detection probe end through the mutual inductance effect. In order to amplify the observability of the signal, the response signal U0 at both ends of the resistor R1 under different frequency excitation is measured. The response signal obtained based on the change in the resistance of the probe body embedded in the pipeline at the detection probe end under a fixed mutual inductance coil spacing includes a finite number of continuously increasing detection frequencies f1 <f2<……<f n-1 <f n The detection signal voltage value U generated by the probe 1i , U 2i ,……,U (n-1)i , U ni By subsequent processing and analysis of the acquired voltage signal, the corrosion degree of the exposed coil can be quantitatively analyzed to complete the wireless passive corrosion monitoring of the pipeline. Embodiment 1
[0031] refer to Figures 1 to 6 , a wireless passive resistance corrosion monitoring method, comprising the following steps: S101, preparing a pipeline to be tested with a flexible corrosion probe installed, and selecting a service environment;
[0032] Specifically, the flexible corrosion probe comprises an inductor coil L R , used to detect the inductance coil L at the probe end TA mutual inductance coil is formed to obtain wireless passive internal corrosion information; and multiple resistors are specially made for sensitive elements; the flexible probe is pre-embedded between the outer protective layer 4 and the reinforcement layer 2 of the pipeline, and the resistance of the multiple resistors gradually increases as the pipeline corrosion proceeds.
[0033] S102, wrap the flexible detection probe around the position to be detected on the pipeline, thereby determining a fixed mutual inductance coil spacing H1, and collecting the amplitude U i The voltage value U across the resistor under continuous n frequency excitation ni .
[0034] Specifically, the response signal obtained by detecting the change in the resistance of the probe body embedded in the pipeline at the end of the detection probe based on the fixed mutual inductance coil spacing includes a finite number of continuously increasing detection frequencies f1 <f2<……<f n-1 <f n The detection signal voltage value U generated at both ends of the probe resistor R1 1i , U 2i ,……,U (n-1)i , U ni .
[0035] S103, define gain G = 10log 10 (U o / U i ), the single point value of the voltage value Uni at both ends of the fixed resistor R1 is U o , the voltage signal U across the resistor obtained according to the method described in 102 i The gain under different resistance values of sensitive elements is calculated based on the amplitude of the excitation signal.
[0036] Specifically, the sampling points are selected to be equally spaced and varied from the processing according to the characteristics of the embedded resistor string, and the number of sampling points selected is determined according to the required drawing resolution, which should generally be greater than 1000. The detection signal voltage value U under the fixed coil spacing H1 n Calculation of the excitation voltage U i The gain G is calculated and a curve of the gain G with respect to the number of sampling points, i.e. different excitation frequencies, is plotted.
[0037] S104, using the gain data obtained in S103, plotting the detection signal voltage value to plot a gain-sampling point curve, and determining the increase value of the resistance of the embedded sensitive element, thereby reflecting the degree of corrosion.
[0038] Preferably, when drawing the image, the voltage signal can be obtained with the help of labview software controls and the gain G of the detection signal can be calculated using matlab software programming; and the gain-sampling point curve can be drawn using Origin software, and the characteristics of the curve, the trend and law of gain changing with resistance can be comprehensively considered to determine the degree of corrosion.
[0039] The wireless passive resistance probe pipeline corrosion detection method provided by the present invention designs an embedded resistance probe including an inductor coil, wherein the original resistance R0 can be determined by the number of resistance strips and the length and thickness of each resistance wire, and the size of the resistance R0 can be defined by oneself according to needs; wherein, except for the square part connected to the circuit, the remaining resistance strips are all exposed wires made of the same material as the pipeline lining layer without an anti-corrosion layer; in the initial state, the resistance value of the sensitive element is R0, and when the external complex environment causes the outer protective layer of the pipeline to fail or the pipeline corrodes from the inside and causes the reinforcement layer to rupture, the exposed wire will be gradually corroded, causing the resistance of the entire embedded probe to change, and the transformed resistance is R0+ΔR; mutual inductance is formed between an external detection probe also including an inductor coil and the new embedded probe, so that the influence of the change in the resistance value of the sensitive element through excitation of different frequencies is amplified and distinguished; and a gain-sampling point curve is drawn to comprehensively judge the degree of corrosion.
[0040] Compared with the existing pipeline resistance probe corrosion monitoring technology, the technology provided by the present invention does not require opening holes to destroy the original structure of the pipeline, occupies a small volume, and can obtain probe data non-contactly; different characterization resistance combinations can be comprehensively considered according to the service environment, and the corrosion rate can be linearly or nonlinearly characterized to determine the pipeline corrosion situation. Embodiment 2
[0041] Based on the wireless passive resistance probe pipeline corrosion detection method provided in Example 1, this embodiment provides an experimental implementation method with specific values of the mutual inductance coil spacing H1, the excitation frequency, and the number of sampling points to verify the effectiveness of the method.
[0042] The analysis tool used is Network Analyzer. The excitation frequency is 1kHz to 12MHz. 1000 sampling points with equidistant frequencies between the frequency range are obtained. <f2<……<f n-1 <f n , n=1000 (f1=1000Hz, f2=13011Hz, f3=25022Hz,...f 1000 =11.9MHz); the result is as follows Figure 6As shown; for the convenience of verification, organic glass was placed between the detection probe and the embedded resistance probe body to simulate the outer protective layer of the pipeline during the experiment, and a variable resistor was used to simulate the resistance change caused by corrosion. The resistance change was selected 5 times, namely 1.6Ω, 4.6Ω, 12Ω, 21Ω, and 28.9Ω; Figure 6 A curve diagram of the gain G at the above sampling points provided in an embodiment of the present invention.
[0043] according to Figure 6 It can be seen that when the resistance is constant, the gain will change regularly with the change of the excitation frequency. In the case of 5 kinds of resistance, the difference between the sampling points 300 and 600 is obvious, corresponding to the excitation frequency of 3.6MHz to 7.2MHz, and as the resistance increases, the gain value in this range will increase successively; while at the lower frequency at the left sampling point or the higher frequency at the right sampling point, the change trend is just the opposite, and the gain is smaller when the resistance is large.
[0044] It can be considered that the pipeline corrosion detection method based on wireless passive resistance probe provided by the present invention can complete the monitoring of pipeline corrosion conditions. Embodiment 3
[0045] A wireless passive resistance corrosion monitoring method comprises the following steps:
[0046] S101, preparing a pipeline to be tested embedded with a flexible corrosion probe;
[0047] S102, using a flexible detection probe wrapped around the outer wall of the pipeline to receive the amplitude U i The voltage value U across the resistor under continuous n frequency excitation o ;
[0048] S103, calculate the voltage gain at each frequency for the n points, G=10log 10 (U o / U i );
[0049] S104, drawing a sampling point-gain curve diagram;
[0050] S105. Consider the curve characteristics comprehensively and determine the degree of corrosion.
[0051] When the probe coating position has been corroded for a certain period, the detection signals at both ends of the detection probe R1 are received, including: in each corrosion period T i Get each excitation frequency f1 <f2<……<f n-1 <f n The detection signal voltage value U generated at both ends of the probe resistor R1 1i , U 2i ,……,U (n-1)i, U ni , used to draw the gain-sampling point curve for different corrosion cycles.
[0052] The gain G of the detection signal voltage value with respect to the input voltage is calculated, including: calculating the gain of the detection signal voltage value obtained based on the change of the resistance of the probe body embedded in the pipeline at the detection probe end under a fixed mutual inductance coil spacing; obtaining the detection signal voltage value with the help of labview software control and calculating the gain of the detection signal with matlab software programming; drawing the gain-sampling point curve, and determining the increase value of the embedded resistance, thereby reflecting the degree of corrosion.
[0053] In the step S101, a pipeline to be tested is prepared with a flexible corrosion probe embedded therein, and when a service environment is selected, the prepared flexible corrosion probe is embedded between the protective layer and the reinforcing layer of the pipeline during pipeline processing.
[0054] Wherein, S102 uses a flexible detection probe wrapped around the outer wall of the pipeline to receive the voltage value U across the resistor under n consecutive frequency excitations with an amplitude of U1. n When the flexible corrosion probe comprises an inductor coil L R Used to detect the inductance coil L at the probe end T A mutual inductance coil is formed to obtain wireless passive internal corrosion information; and a plurality of specially made resistors of the sensitive element can gradually increase the resistance as the pipeline corrosion proceeds.
[0055] Wherein, S103 calculates the voltage gain at each frequency for the n points, G=10log 10 (U o / U i ), select the service environment and corrode for a certain period, wrap the flexible detection probe around the position to be detected in the pipeline, and determine a fixed mutual inductance coil spacing H1. The response signal obtained by the change in the resistance of the probe body embedded in the pipeline at the detection probe end based on the fixed mutual inductance coil spacing includes a finite number of continuously increasing detection frequencies. <f2<……<f n-1 <f n The detection signal voltage value U generated at both ends of the probe resistor R1 1i , U 2i ,……,U (n-1)i , U ni ; Define gain G = 10log 10 (U o / U i ), the single point value of the voltage value Uni at both ends of the fixed resistor R1 is U o; The gain is calculated for different corrosion degrees and resistance values of different sensitive components respectively; the sampling points are selected to be equally spaced; and s sampling points are selected.
[0056] When the sampling point-gain curve is drawn in S104, the voltage value U of the detection signal under the fixed coil spacing H1 is o Calculation of the excitation voltage U i The gain G is obtained, and a curve of the gain G with respect to the number of sampling points is drawn; when determining the degree of corrosion, the S105 comprehensively considers the characteristics of the curve, uses the obtained gain data to draw a curve of the gain-sampling point of the detection signal voltage value, and determines the increase value of the embedded resistance, thereby reflecting the degree of corrosion.
[0057] Among them, in said S103, the sampling points are selected to be processed with equal intervals, and are determined according to the characteristics of the embedded resistor string; in said S103, the number of sampling points selected is s, which is determined according to the required drawing resolution and is greater than 1000.
[0058] This embodiment also provides a wireless passive resistance corrosion monitoring system, including the equipment included in any of the above steps.
[0059] Among them, the wireless passive resistance corrosion monitoring method and system can be used to detect single pipeline or equipment corrosion events without contact, and monitor the integrated corrosion rate of the pipeline or equipment over a period of time; it has the advantages of not requiring opening holes to destroy the original structure of the pipeline, occupying a small volume, and being able to obtain probe data without contact.
[0060] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A wireless passive resistance corrosion monitoring method, characterized in that: The following steps are involved: S101, prepare a pipeline to be tested with a flexible corrosion probe embedded therein; and when a service environment is selected, embed the prepared flexible corrosion probe between the protective layer and the reinforcement layer of the pipeline during pipeline processing; the flexible corrosion probe includes an inductor coil L R and a sensitive element; the sensitive element is composed of a plurality of resistors, and the resistance values of the plurality of resistors gradually increase as the pipeline corrosion proceeds; S102, wrapping the outer wall of the pipeline with a flexible detection probe, wherein the flexible detection probe comprises a signal generator V1, a fixed resistor R1 and an inductor L T , thereby determining a fixed mutual inductance coil spacing H1, which is used to receive the detection signal voltage value Uni at both ends of the fixed resistor R1 under continuous n frequency excitation with an excitation voltage with an amplitude of Ui; when the probe coating position has been corroded for a certain period, the detection signal at both ends of the fixed resistor R1 of the detection probe is received, and a finite number of continuously increasing detection frequencies f1 are obtained in each corrosion period Ti. <f2<……<f n-1 <f n The detection signal voltage value U generated at both ends of the fixed resistor R1 1i , U 2i ,……,U (n-1)i , U ni , used to draw sampling point-gain curves for different corrosion cycles; S103, select s sampling points, the sampling points are selected to be equally spaced, and the voltage gain G=10log at each frequency sampling point is calculated for the n frequencies. 10 (U o / U i ), the single point value of the detection signal voltage value Uni at both ends of the fixed resistor R1 is U o , calculating the gain of the detection signal voltage value obtained based on the change in the resistance value of the sensitive element of the corrosion probe embedded in the pipeline at the detection probe end under the fixed mutual inductance coil spacing; S104, drawing a sampling point-gain curve, calculating the gain G of the excitation voltage with an amplitude of Ui for the detection signal voltage value Uni under the fixed mutual inductance coil spacing H1, and drawing a curve of the gain G with respect to the number of sampling points; S105. Comprehensively considering the curve characteristics, determine the increase value of the resistance value of the embedded sensitive element, so as to reflect the degree of corrosion.
2. A wireless passive resistance corrosion monitoring method according to claim 1, characterized in that: The detection signal voltage value Uni is used to calculate the gain G of the excitation voltage with an amplitude of Ui, and the detection signal voltage value is obtained by means of labview software control and matlab software programming to calculate the gain of the detection signal; the sampling point-gain curve is drawn, and the increase value of the resistance value of the sensitive element is determined, thereby reflecting the degree of corrosion.
3. A wireless passive resistance corrosion monitoring method according to claim 1, characterized in that: In the S103, the sampling points are selected to be equally spaced and determined according to the resistance characteristics of the embedded sensitive element; in the S103, the number of sampling points selected is s, determined according to the required drawing resolution and greater than 1000.
Citation Information
Patent Citations
Metallic corrosion velocity measurer and its measuring method adopting AC resistance probe
CN101246114A
Oil and gas pipeline corrosion online monitor
CN101846644A
Compound probe, device and method for monitoring corrosion of down-hole string on line and in real time
CN104458561A
Stress-defect-free bamboo winding composite pressure pipe with rebated joint
CN108150734A
High pressure corrodes electric resistance probe
CN207133328U