Substrate and maintenance method thereof, and display device
By coating the open circuit area with conductive material and forming an organic protective film, the problem of ITO material touch electrodes easily falling off after repair is solved, improving the product yield and repair effect of the substrate.
Patent Information
- Application Number
- CN202010597610.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-06-28
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-06-28
AI Technical Summary
In the existing technology, the ITO material touch electrodes of the touch display panel are prone to metal detachment after repair of the open circuit area, which affects the product yield.
A conductive material is coated on the open circuit area, and an organic insulating material is coated on the side away from the substrate to form an organic protective film, which enhances adhesion and prevents the conductive material from falling off.
This improved the product yield of the substrate, ensured the stability of the repair effect, and avoided the problem of conductive materials falling off during the reliability verification process.
Smart Images

Figure CN113851421B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to a substrate and a maintenance method thereof, and a display device. Background Art
[0002] In the touch display panel of the related art, touch electrodes are made on the surface of the display panel to realize the touch function. The defects caused by the process are mainly open circuit and short circuit. For short defects, laser can be used to directly cut off the short point for repair; for open defects, touch electrodes are mostly made of ITO. Due to the special nature of ITO material, the direct metal connection repair method will cause the metal to fall off during the reliability verification process, affecting the repair effect. Summary of the invention
[0003] The technical problem to be solved by the present disclosure is to provide a substrate and a maintenance method thereof, and a display device, which can improve the product yield of the substrate.
[0004] To solve the above technical problems, the embodiments of the present disclosure provide the following technical solutions:
[0005] In one aspect, a substrate repair method is provided, the substrate comprising a substrate, at least one conductive pattern is arranged on the substrate, at least one of the at least one conductive pattern has a short circuit and the conductive pattern is divided into a first sub-conductive pattern and a second sub-conductive pattern, the repair method comprising:
[0006] Coating a conductive material in the disconnection area, wherein the conductive material covers both the first sub-conductive pattern and the second sub-conductive pattern;
[0007] An organic insulating material is coated on a side of the conductive material away from the substrate, and the organic insulating material is cured to form an organic protective film covering the conductive material.
[0008] In some embodiments, before coating the conductive material on the disconnection area, the method further comprises:
[0009] Performing a groove process on the substrate at the disconnection area to form a groove on the surface of the substrate, wherein the groove extends from the first sub-conductive pattern to the second sub-conductive pattern;
[0010] The conductive materials applied to the disconnect area include:
[0011] The conductive material is filled in the groove.
[0012] In some embodiments, before coating the conductive material on the disconnection area, the method further comprises:
[0013] Remove foreign matter from the disconnection area.
[0014] An embodiment of the present disclosure further provides a substrate, comprising a substrate, on which at least one conductive pattern is arranged, at least one of the at least one conductive pattern has a disconnection and the conductive pattern is divided into a first sub-conductive pattern and a second sub-conductive pattern, and the substrate further comprises:
[0015] A conductive material located in the disconnection area, wherein the conductive material covers both the first sub-conductive pattern and the second sub-conductive pattern;
[0016] An organic protection film is located on a side of the conductive material away from the substrate.
[0017] In some embodiments, an orthographic projection of the conductive material on the substrate is located within an orthographic projection of the organic protection film on the substrate.
[0018] In some embodiments, the organic protective film is circular, and the diameter of the organic protective film is 70-100 um.
[0019] In some embodiments, a first orthographic projection of the disconnection region on the substrate is located within a second orthographic projection of the conductive material on the substrate.
[0020] In some embodiments, the shortest distance between the outline of the first orthographic projection and the outline of the second orthographic projection is greater than 2 um.
[0021] In some embodiments, a surface of the conductive material away from the substrate and a surface of the conductive pattern away from the substrate are located in the same plane.
[0022] In some embodiments, the substrate further comprises:
[0023] A groove extends from the first sub-conductive pattern to the second sub-conductive pattern, and the conductive material is located in the groove.
[0024] In some embodiments, the orthographic projection of the groove on the substrate is radial.
[0025] In some embodiments, the conductive pattern is made of a transparent conductive material, and the conductive material is made of tungsten powder, silver powder or cobalt powder.
[0026] In some embodiments, the substrate is a touch substrate, and the conductive pattern is a touch electrode trace.
[0027] An embodiment of the present disclosure further provides a display device, comprising the substrate as described above.
[0028] The embodiments of the present disclosure have the following beneficial effects:
[0029] In the above scheme, after a short circuit occurs in the conductive pattern, a conductive material is coated on the short circuit area, and the conductive material can connect the short circuit conductive pattern. In addition, an organic insulating material is coated on the side of the conductive material away from the substrate, and the organic insulating material is cured to form an organic protective film covering the conductive material. The organic protective film has a strong adhesion to the substrate, which can prevent the conductive material from falling off the substrate, avoiding the problem of conductive material falling off at the repair point during the reliability verification process, ensuring the repair effect, and improving the product yield of the substrate. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of a short circuit in a conductive pattern;
[0031] Figure 2 A schematic diagram of performing a trenching process on a substrate at a disconnection area according to an embodiment of the present disclosure;
[0032] Figure 3 A schematic diagram of coating a conductive material according to an embodiment of the present disclosure;
[0033] Figure 4 It is a schematic diagram of forming an organic protective film according to an embodiment of the present disclosure.
[0034] Reference numerals
[0035] 1 Touch electrode routing
[0036] 11. First sub-conductive pattern
[0037] 12. Second sub-conductive pattern
[0038] 2 Grooves
[0039] 3 Conductive materials
[0040] 4 Organic protective film DETAILED DESCRIPTION
[0041] In order to make the technical problems, technical solutions and advantages to be solved by the embodiments of the present disclosure more clear, a detailed description will be given below with reference to the accompanying drawings and specific embodiments.
[0042] Embodiments of the present disclosure provide a substrate and a maintenance method thereof, and a display device, which can improve the product yield of the substrate.
[0043] An embodiment of the present disclosure provides a substrate repair method, the substrate comprising a substrate, at least one conductive pattern is arranged on the substrate, at least one conductive pattern of the at least one conductive pattern has a short circuit and the conductive pattern is divided into a first sub-conductive pattern and a second sub-conductive pattern, the repair method comprising:
[0044] Coating a conductive material in the disconnection area, wherein the conductive material covers both the first sub-conductive pattern and the second sub-conductive pattern;
[0045] An organic insulating material is coated on a side of the conductive material away from the substrate, and the organic insulating material is cured to form an organic protective film covering the conductive material.
[0046] In this embodiment, after a short circuit occurs in the conductive pattern, a conductive material is coated on the short circuit area, and the conductive material can connect the short circuit conductive pattern. In addition, an organic insulating material is coated on the side of the conductive material away from the substrate, and the organic insulating material is cured to form an organic protective film covering the conductive material. The organic protective film has a strong adhesion to the substrate, which can prevent the conductive material from falling off the substrate, avoiding the problem of conductive material falling off at the repair point during the reliability verification process, ensuring the repair effect, and improving the product yield of the substrate.
[0047] In some embodiments, the conductive pattern of the substrate is made of a transparent conductive material such as ITO, and the conductive material for repairing the open circuit area is mostly made of metal powder, such as tungsten powder. Since the bonding between ITO material and metal powder is poor, after the open circuit area is repaired with metal powder, the metal at the repair point is prone to fall off, affecting the yield of the substrate. In this embodiment, an organic protective film is covered on the outside of the conductive material. The organic protective film has a strong adhesion to the substrate, which can prevent the metal at the repair point from falling off the substrate, thereby ensuring the repair effect and improving the product yield of the substrate.
[0048] Among them, the organic insulating material can be organic resin, and the conductive material used for maintenance can be tungsten powder, silver powder or cobalt powder. Compared with conductive materials, organic insulating materials have stronger adhesion to the substrate and are not easy to fall off from the substrate, thereby preventing the conductive material from falling off the substrate.
[0049] In addition, if there are foreign objects in the disconnection area, such as residual conductive patterns, the adhesion between the conductive material and the substrate will be reduced, and the risk of the conductive material falling off the substrate will be increased. Therefore, before coating the conductive material in the disconnection area, the method further includes:
[0050] Foreign matters in the disconnection area, including residual conductive patterns and foreign particles, etc., are removed, so that there are no impurities in the disconnection area, the conductive material can be evenly coated on the substrate, the adhesion between the conductive material and the substrate is increased, and the risk of the conductive material falling off the substrate is reduced. Specifically, the foreign matters in the disconnection area can be removed by laser, which has high precision and can accurately remove the foreign matters in the disconnection area without affecting other areas.
[0051] In addition, the larger the contact area between the conductive material and the substrate, the greater the adhesion between the conductive material and the substrate. In order to improve the adhesion between the conductive material and the substrate, more contact area between the coated conductive material and the substrate can be provided. Therefore, before coating the conductive material on the disconnection area, the method further includes:
[0052] Performing a groove process on the substrate at the disconnection area to form a groove on the surface of the substrate;
[0053] The conductive materials applied to the disconnect area include:
[0054] The conductive material is filled in the groove. The design of the groove can increase the contact area between the conductive material and the substrate, thereby increasing the adhesion between the conductive material and the substrate, ensuring the stability of the combination between the conductive material and the conductive pattern, and preventing the conductive material from falling off the substrate due to the different thermal expansion coefficients of the conductive material and the conductive pattern.
[0055] The range of the groove should extend from the first sub-conductive pattern to the second sub-conductive pattern, that is, the orthographic projection of the groove on the substrate overlaps with the orthographic projections of the first sub-conductive pattern and the second sub-conductive pattern on the substrate. In order to increase the area of the groove and thus increase the contact area between the conductive material and the substrate, the orthographic projection of the groove on the substrate can be radial, for example, the orthographic projection of the groove on the substrate can be a cross, a cross, etc.
[0056] The width of the groove can be adjusted according to the line width of the conductive pattern. The width of the groove can be 1 / 3 of the line width of the conductive pattern. If the width of the conductive pattern is relatively large, multiple parallel or intersecting grooves can be formed. The range of each groove should extend from the first sub-conductive pattern to the second sub-conductive pattern.
[0057] After the substrate is grooved, a conductive material may be filled in the groove to connect the first sub-conductive pattern and the second sub-conductive pattern. The surface of the conductive material away from the substrate side may be located in the same plane as the surface of the conductive pattern away from the substrate side. In this way, after the conductive pattern is repaired with the conductive material, the surface of the conductive material away from the substrate side and the surface of the conductive pattern away from the substrate side can form a flat surface, which is beneficial to the subsequent process.
[0058] In order to increase the contact area between the conductive material and the substrate as much as possible, the conductive material should not only cover the disconnection area but also extend beyond the disconnection area, that is, the first orthographic projection of the disconnection area on the substrate is located within the second orthographic projection of the conductive material on the substrate. In some embodiments, the shortest distance between the outline of the first orthographic projection and the outline of the second orthographic projection can be greater than 2um, so as to ensure that the conductive material has sufficient contact area with the substrate, so that the conductive material is not easy to fall off the substrate.
[0059] In this embodiment, the organic protective film is used to prevent the conductive material from falling off from the substrate. To achieve this purpose, the orthographic projection of the conductive material on the substrate should be located within the orthographic projection of the organic protective film on the substrate. After the conductive material is coated to achieve the connection between the first sub-conductive pattern and the second sub-conductive pattern, an organic protective liquid material is coated on the conductive material. The organic protective liquid material is first UV-cured and then thermally cured to form an organic protective film. This allows the organic protective film to be firmly combined with the substrate, better preventing the conductive material from falling off from the substrate and increasing the stability of maintenance. The process conditions for thermal curing can be heating at a temperature of 120°C for about 60 minutes. Of course, in this embodiment, the process conditions for thermal curing are not limited to heating at a temperature of 120°C for 60 minutes, and other process parameters can also be used.
[0060] The thickness of the organic protective film is based on not affecting the subsequent processes. For example, it will not affect the subsequent attachment of the polarizer. The thickness of the organic protective film can be less than 1.5um.
[0061] The area of the organic protective film is limited to not affecting the appearance of the substrate. In some embodiments, the organic protective film may be circular, and the diameter of the organic protective film may be 70-100um. When the diameter of the organic protective film adopts the above value, it can completely cover the maintenance area without affecting the appearance of the substrate.
[0062] The substrate of this embodiment may be a display substrate or a touch control substrate. The conductive pattern may be an electrode of the substrate or a signal line of the substrate.
[0063] When the conductive pattern uses a transparent conductive material such as ITO, due to the particularity of the transparent conductive material, the problem of metal falling off is prone to occur when using metal to repair the disconnection area. The technical solution of this embodiment can effectively solve this problem.
[0064] In a specific embodiment, the substrate may be a touch substrate, and the conductive pattern may be a touch electrode trace of the touch substrate. Figure 1As shown, a plurality of parallel touch electrode traces 1 are arranged on the substrate, and the touch electrode traces 1 are made of transparent conductive material ITO. One of the touch electrode traces 1 is broken and divided into a first sub-conductive pattern 11 and a second sub-conductive pattern 12 that are broken, wherein the area within the dotted line frame is the broken area; before repairing the broken area, firstly remove foreign matter in the broken area, specifically, laser can be used to remove the residual ITO, particles, etc. in the broken area; then, as shown in FIG. Figure 2 As shown, the conductive pattern on the substrate is grooved in the disconnection area to form a groove 2. The depth of the groove 2 can be greater than the thickness of the touch electrode wiring 1, that is, the groove 2 can penetrate from the touch electrode wiring 1 to the inside of the substrate. The groove 2 can be in a matrix and form a cross with the crack in the disconnection area to connect the first sub-conductive pattern 11 and the second sub-conductive pattern 12. The depth of the groove 2 can be designed as needed; then, as shown in Figure 3 As shown, a conductive material 3 is coated on the disconnection area. The conductive material 3 can be made of tungsten powder, silver powder or cobalt powder. In addition to filling the groove 2, the conductive material 3 also exceeds the area where the groove 2 is located and the disconnection area. The area covered by the conductive material 3 can be rectangular, connecting the first sub-conductive pattern 11 and the second sub-conductive pattern 12, and being at a certain distance from the surrounding touch electrode traces 1 to avoid short circuits with the surrounding touch electrode traces 1. Of course, the area covered by the conductive material 3 is not limited to a rectangle, and can also be other shapes, such as an ellipse. Then, as shown in FIG. Figure 4 As shown, an organic protective liquid material is coated on the conductive material 2, and the organic protective liquid material is first cured by ultraviolet light, and then thermally cured to form an organic protective film 4. The organic protective film 4 is firmly combined with the substrate to prevent the conductive material from falling off the substrate, thereby increasing the stability of maintenance. Since the organic protective film 4 is insulating, the organic protective film 4 can cover the surrounding touch electrode traces 1 without affecting the performance of the substrate. Therefore, the area of the organic protective film 4 can be designed to be relatively large, which can increase the adhesion between the organic protective film 4 and the substrate. Figure 4 As shown, the organic protective film 4 may be circular, and the diameter may be 70-100 um.
[0065] The above embodiment is described by taking the conductive pattern using transparent conductive material as an example, but the conductive pattern of this embodiment is not limited to using transparent conductive material, and can also be made of metal. When the conductive pattern is made of metal, the adhesion between the conductive material and the substrate can be increased by setting grooves and organic protective films, preventing the conductive material from falling off the substrate, avoiding the problem of conductive material falling off at the repair point during the reliability verification process, ensuring the repair effect, and improving the product yield of the substrate.
[0066] In addition, the above embodiment is described by taking the conductive pattern as the touch electrode routing of the touch substrate as an example. The technical solution of this embodiment can improve the maintenance reliability and product yield of the touch substrate; however, the conductive pattern of this embodiment is not limited to the touch electrode routing of the touch substrate, but can also be the signal line of the display substrate, such as the gate line, the data line, etc. The technical solution of this embodiment can improve the maintenance reliability and product yield of the display substrate.
[0067] The embodiment of the present disclosure also provides a substrate, which is obtained by repairing a substrate with a short circuit using the substrate repair method described above. The substrate includes a substrate, on which at least one conductive pattern is arranged, at least one conductive pattern of the at least one conductive pattern has a short circuit and the conductive pattern is divided into a first sub-conductive pattern and a second sub-conductive pattern, and the substrate also includes:
[0068] A conductive material located in the disconnection area, wherein the conductive material covers both the first sub-conductive pattern and the second sub-conductive pattern;
[0069] An organic protection film is located on a side of the conductive material away from the substrate.
[0070] In this embodiment, a conductive material is used to connect the broken conductive pattern. In addition, an organic protective film covering the conductive material is provided on the side of the conductive material away from the substrate. The organic protective film has a strong adhesion to the substrate, which can prevent the conductive material from falling off the substrate and avoid the problem of conductive material falling off at the repair point during the reliability verification process, thereby ensuring the repair effect and improving the product yield of the substrate.
[0071] In some embodiments, the conductive pattern of the substrate is made of a transparent conductive material such as ITO, and the conductive material for repairing the broken area is mostly made of metal powder, such as tungsten powder, silver powder or cobalt powder. Since the bonding between ITO material and metal powder is poor, after the broken area is repaired with metal powder, the metal at the repair point is prone to fall off, affecting the yield of the substrate. In this embodiment, an organic protective film is covered on the outside of the conductive material. The organic protective film has a strong adhesion to the substrate, which can prevent the metal at the repair point from falling off the substrate, thereby ensuring the repair effect and improving the product yield of the substrate.
[0072] Among them, the organic protective film can be made of organic insulating materials such as organic resin, and the conductive materials used for maintenance can be made of tungsten powder, silver powder or cobalt powder. Compared with conductive materials, organic insulating materials have stronger adhesion to the substrate and are not easy to fall off from the substrate, thereby preventing the conductive material from falling off the substrate.
[0073] In order to increase the contact area between the conductive material and the substrate as much as possible, the conductive material should not only cover the disconnection area but also extend beyond the disconnection area, that is, the first orthographic projection of the disconnection area on the substrate is located within the second orthographic projection of the conductive material on the substrate. In some embodiments, the shortest distance between the outline of the first orthographic projection and the outline of the second orthographic projection can be greater than 2um, so as to ensure that the conductive material has sufficient contact area with the substrate, so that the conductive material is not easy to fall off the substrate.
[0074] In this embodiment, the organic protective film is used to prevent the conductive material from falling off from the substrate. To achieve this purpose, the orthographic projection of the conductive material on the substrate should be located within the orthographic projection of the organic protective film on the substrate. After the conductive material is applied to achieve the connection between the first sub-conductive pattern and the second sub-conductive pattern, an organic protective liquid material is applied to the conductive material, and the organic protective liquid material is first cured by ultraviolet light and then thermally cured to form an organic protective film, so that the organic protective film can be firmly combined with the substrate, better preventing the conductive material from falling off from the substrate and increasing the stability of maintenance.
[0075] The thickness of the organic protective film is based on not affecting the subsequent processes. For example, it will not affect the subsequent attachment of the polarizer. The thickness of the organic protective film can be less than 1.5um.
[0076] The area of the organic protective film is limited to not affecting the appearance of the substrate. In some embodiments, the organic protective film may be circular, and the diameter of the organic protective film may be 70-100um. When the diameter of the organic protective film adopts the above value, it can completely cover the maintenance area without affecting the appearance of the substrate.
[0077] In addition, the larger the contact area between the conductive material and the substrate, the greater the adhesion between the conductive material and the substrate. In order to improve the adhesion between the conductive material and the substrate, the coated conductive material can be provided with more contact area with the substrate. The substrate further includes: a groove extending from the first sub-conductive pattern to the second sub-conductive pattern, and the conductive material is located in the groove. The design of the groove can increase the contact area between the conductive material and the substrate, thereby increasing the adhesion between the conductive material and the substrate, ensuring the stability of the combination between the conductive material and the conductive pattern, and preventing the conductive material from falling off the substrate due to the different thermal expansion coefficients of the conductive material and the conductive pattern.
[0078] The range of the groove should extend from the first sub-conductive pattern to the second sub-conductive pattern, that is, the orthographic projection of the groove on the substrate overlaps with the orthographic projections of the first sub-conductive pattern and the second sub-conductive pattern on the substrate. In order to increase the area of the groove and thus increase the contact area between the conductive material and the substrate, the orthographic projection of the groove on the substrate can be radial, for example, the orthographic projection of the groove on the substrate can be a cross, a cross, etc.
[0079] The width of the groove can be adjusted according to the line width of the conductive pattern. The width of the groove can be 1 / 3 of the line width of the conductive pattern. If the width of the conductive pattern is relatively large, multiple parallel or intersecting grooves can be formed. The range of each groove should extend from the first sub-conductive pattern to the second sub-conductive pattern.
[0080] After the substrate is grooved, a conductive material may be filled in the groove to connect the first sub-conductive pattern and the second sub-conductive pattern. The surface of the conductive material away from the substrate side may be located in the same plane as the surface of the conductive pattern away from the substrate side. In this way, after the conductive pattern is repaired with the conductive material, the surface of the conductive material away from the substrate side and the surface of the conductive pattern away from the substrate side can form a flat surface, which is beneficial to the subsequent process.
[0081] When the conductive pattern uses a transparent conductive material such as ITO, due to the particularity of the transparent conductive material, the problem of metal falling off is prone to occur when using metal to repair the disconnection area. The technical solution of this embodiment can effectively solve this problem.
[0082] In a specific embodiment, the substrate may be a touch substrate, and the conductive pattern may be a touch electrode trace of the touch substrate. Figure 4As shown, a plurality of parallel touch electrode traces 1 are arranged on the substrate, and the touch electrode traces 1 are made of transparent conductive material ITO. One of the touch electrode traces 1 is broken and is divided into a first sub-conductive pattern 11 and a second sub-conductive pattern 12 that are broken, wherein the area within the dotted line frame is the broken area; a groove 2 is provided in the broken area, and the depth of the groove 2 can be greater than the thickness of the touch electrode trace 1, that is, the groove 2 can penetrate from the touch electrode trace 1 to the inside of the substrate, and the groove 2 can be in a matrix, forming a cross with the cracks in the broken area, connecting the first sub-conductive pattern 11 and the second sub-conductive pattern 12, and the depth of the groove 2 can be designed as needed; in addition to filling the groove 2, the conductive material 3 also exceeds the area where the groove 2 is located and the broken area, and the conductive material 3 is provided at the bottom of the substrate ... The coverage area of the material 3 can be rectangular, connecting the first sub-conductive pattern 11 and the second sub-conductive pattern 12, and being at a certain distance from the surrounding touch electrode traces 1 to avoid short circuit with the surrounding touch electrode traces 1. Of course, the coverage area of the conductive material 3 is not limited to a rectangle, and can also be other shapes, such as an ellipse, etc. An organic protective film 4 is arranged on the conductive material 2, and the organic protective film 4 is firmly combined with the substrate to prevent the conductive material from falling off the substrate and increase the stability of maintenance. Since the organic protective film 4 is insulating, the organic protective film 4 can cover the surrounding touch electrode traces 1 without affecting the performance of the substrate. Therefore, the area of the organic protective film 4 can be designed to be relatively large, which can increase the adhesion between the organic protective film 4 and the substrate. Figure 4 As shown, the organic protective film 4 may be circular, and the diameter may be 70-100 um.
[0083] The above embodiment is described by taking the conductive pattern using transparent conductive material as an example, but the conductive pattern of this embodiment is not limited to using transparent conductive material, and can also be made of metal. When the conductive pattern is made of metal, the adhesion between the conductive material and the substrate can be increased by setting grooves and organic protective films, preventing the conductive material from falling off the substrate, avoiding the problem of conductive material falling off at the repair point during the reliability verification process, ensuring the repair effect, and improving the product yield of the substrate.
[0084] In addition, the above embodiment is described by taking the conductive pattern as the touch electrode routing of the touch substrate as an example, but the conductive pattern of the present embodiment is not limited to the touch electrode routing of the touch substrate, but can also be the touch electrode of the touch substrate. The technical solution of the present embodiment can improve the maintenance reliability and product yield of the touch substrate; in addition, the conductive pattern of the present embodiment can also be the signal line or display electrode of the display substrate, such as the gate line, the data line, etc. The technical solution of the present embodiment can improve the maintenance reliability and product yield of the display substrate.
[0085] An embodiment of the present disclosure further provides a display device, comprising the substrate as described above.
[0086] The display device includes but is not limited to: a radio frequency unit, a network module, an audio output unit, an input unit, a sensor, a display unit, a user input unit, an interface unit, a memory, a processor, and a power supply. Those skilled in the art will appreciate that the structure of the above display device does not constitute a limitation on the display device, and the display device may include more or less of the above components, or a combination of certain components, or different component arrangements. The display device may be: any product or component with a display function, such as a television, a monitor, a digital photo frame, a mobile phone, a tablet computer, etc., wherein the display device also includes a flexible circuit board, a printed circuit board, and a backplane.
[0087] It should be noted that each embodiment in this specification is described in a progressive manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the embodiments, since they are basically similar to the product embodiments, the description is relatively simple, and the relevant parts can be referred to the partial description of the product embodiments.
[0088] Unless otherwise defined, the technical terms or scientific terms used in the present disclosure should be understood by people with ordinary skills in the field to which the present disclosure belongs. The "first", "second" and similar words used in the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. "Include" or "comprise" and similar words mean that the elements or objects appearing before the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.
[0089] It will be understood that when an element such as a layer, film, region, or substrate is referred to as being “on” or “under” another element, it can be “directly on” or “under” the other element or intervening elements may be present.
[0090] In the description of the above embodiments, specific features, structures, materials or characteristics may be combined in a suitable manner in any one or more embodiments or examples.
[0091] The above is only a specific embodiment of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any person skilled in the art who is familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.
Claims
1. A method for repairing a substrate, characterized in that: The substrate comprises a substrate, on which at least one conductive pattern is arranged, at least one of the at least one conductive pattern has a short circuit and the conductive pattern is divided into a first sub-conductive pattern and a second sub-conductive pattern, and the repair method comprises: Coating a conductive material in the disconnection area, wherein the conductive material covers both the first sub-conductive pattern and the second sub-conductive pattern; Coating an organic insulating material on a side of the conductive material away from the substrate, and curing the organic insulating material to form an organic protective film covering the conductive material; Before coating the conductive material on the disconnection area, the method further comprises: Performing a groove processing on the substrate at the disconnection area to form a groove on the surface of the substrate, the groove extending from the first sub-conductive pattern to the second sub-conductive pattern, and the orthographic projection of the groove on the substrate and the orthographic projections of the first sub-conductive pattern and the second sub-conductive pattern on the substrate have overlapping parts; The conductive materials applied to the disconnect area include: The groove is filled with the conductive material.
2. The substrate repair method according to claim 1, characterized in that: Before coating the conductive material on the disconnection area, the method further comprises: Remove foreign matter from the disconnection area.
3. A substrate, characterized in that: The method according to claim 1 or 2 is used for repair, wherein the substrate comprises a substrate, at least one conductive pattern is arranged on the substrate, at least one conductive pattern of the at least one conductive pattern has a short circuit and the conductive pattern is divided into a first sub-conductive pattern and a second sub-conductive pattern, and the substrate further comprises: A conductive material located in the disconnection area, wherein the conductive material covers both the first sub-conductive pattern and the second sub-conductive pattern; An organic protection film is located on a side of the conductive material away from the substrate.
4. The substrate according to claim 3, characterized in that The orthographic projection of the conductive material on the substrate is located within the orthographic projection of the organic protection film on the substrate.
5. The substrate according to claim 3, characterized in that The organic protective film is circular, and the diameter of the organic protective film is 70-100 um.
6. The substrate according to claim 3, characterized in that A first orthographic projection of the disconnection region on the substrate is located within a second orthographic projection of the conductive material on the substrate.
7. The substrate according to claim 6, characterized in that The shortest distance between the outline of the first orthographic projection and the outline of the second orthographic projection is greater than 2 um.
8. The substrate according to claim 3, characterized in that A surface of the conductive material away from the substrate and a surface of the conductive pattern away from the substrate are located in the same plane.
9. The substrate according to claim 3, characterized in that Also includes: A groove extends from the first sub-conductive pattern to the second sub-conductive pattern, and the conductive material is located in the groove.
10. The substrate according to claim 9, characterized in that The orthographic projection of the groove on the substrate is radial.
11. The substrate according to any one of claims 3 to 10, characterized in that The conductive pattern is made of transparent conductive material, and the conductive material is made of tungsten powder, silver powder or cobalt powder.
12. The substrate according to claim 11, characterized in that The substrate is a touch substrate, and the conductive pattern is a touch electrode wiring.
13. A display device, characterized in that: Comprising a substrate as claimed in any one of claims 3 to 12.