Preparation method of filter defining layer, filter defining layer, filter and display device

By forming a reflective bank in the QD filter and using chemical silver plating technology to increase the blue light absorption rate, the problems of low blue light absorption rate and optical crosstalk of the QD filter are solved, achieving more efficient light conversion and reducing optical crosstalk.

CN113985512BActive Publication Date: 2024-10-01BOE TECHNOLOGY GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111413116.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-25
Publication Date
2024-10-01
Estimated Expiration
2041-11-25

AI Technical Summary

Technical Problem

The blue light absorption rate of existing QD filters is not high, which requires a thicker film layer to increase the absorption rate, but this increases the chance of optical crosstalk.

Method used

The first structural layer and the second structural layer are formed on the substrate, and a reflective film is formed therein. A reflective bank is formed through chemical silver plating to improve blue light utilization and reduce optical crosstalk.

Benefits of technology

It effectively improves blue light utilization and light conversion efficiency, while reducing the occurrence of optical crosstalk.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113985512B_ABST
    Figure CN113985512B_ABST
Patent Text Reader

Abstract

The present application generally relates to the field of display technology, and specifically, to a method for preparing a filter defining layer, a filter defining layer, a filter and a display device. The filter defining layer is processed by the above-mentioned filter defining layer preparation method, the filter is installed with the above-mentioned filter defining layer, the display device includes a substrate and the above-mentioned filter, the substrate is provided with an encapsulation layer, and the filter is located outside the encapsulation layer. The preparation method includes: forming a first structural layer on the substrate, forming a second structural layer on the first structural layer, patterning the first structural layer, and forming a reflective film on the second structural layer, the reflective film effectively improves the utilization rate of blue light, improves the light conversion efficiency, and effectively reduces the light crosstalk phenomenon.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application generally relates to the field of display technology, and in particular, to a method for preparing a filter defining layer, a filter defining layer, a filter, and a display device. Background Art

[0002] QDCF (Quantum Dots Color Filter) is usually used in display screens. QD quantum dots have the advantages of high light conversion rate, high color gamut and high color purity. Since QD quantum dot display technology is still immature, existing QD displays mainly use photoinduced QD quantum dots to display, replacing traditional color films with QD quantum dots to effectively improve the display color gamut and truly restore the display colors.

[0003] Since QD quantum dots have a low absorption rate for blue light, a thicker QD film layer needs to be prepared to effectively absorb blue light and improve the blue light conversion rate. Usually, the required thickness of QD is above 10um. Therefore, a thicker bank (definition layer) is required, but the probability of optical crosstalk problems will increase. Summary of the invention

[0004] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Application does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.

[0005] In order to solve the technical problem that the existing QD filter has low blue light absorption rate, the main purpose of the present application is to provide a method for preparing a filter defining layer, a filter defining layer, a filter and a display device.

[0006] In order to achieve the above invention objectives, this application adopts the following technical solutions:

[0007] A method for preparing a filter defining layer, comprising:

[0008] forming a first structural layer on a substrate;

[0009] forming a second structural layer on the first structural layer;

[0010] patterning the first structural layer;

[0011] A reflective film is formed on the second structural layer.

[0012] Further, in some embodiments of the present application, forming the second structure layer on the first structure layer includes:

[0013] Preparing a photoresist on the first structural layer, and patterning the photoresist to form a photoresist layer and a preparation area;

[0014] Electroplating Cu on the first structural layer located in the preparation area to form a second structural layer;

[0015] The photoresist layer is removed.

[0016] Further, in some embodiments of the present application, forming the second structure layer on the first structure layer includes:

[0017] Electroplating to form a Cu layer on the first structural layer;

[0018] forming a patterned photoresist layer on the Cu layer;

[0019] The Cu layer is patterned through a photoresist layer to form the second structure layer.

[0020] Further, in some embodiments of the present application, preparing a reflective film on the second structural layer includes:

[0021] Forming a reflective film on the second structural layer by chemically plating Ag;

[0022] The reflective film wraps the first structural layer and the second structural layer.

[0023] Furthermore, in some embodiments of the present application, the thickness of the second structural layer is between 2 μm and 100 μm.

[0024] Further, in some embodiments of the present application, forming a first structural layer on the substrate includes:

[0025] MTD / Cu or Ti / Cu is selected to form the first structural layer on the substrate (100).

[0026] Furthermore, in some embodiments of the present application, the thickness of the reflective film is between 0.001 μm and 1 μm.

[0027] A filter defining layer is manufactured by adopting the preparation method of the filter defining layer.

[0028] A filter is provided with the filter defining layer.

[0029] A display device comprises a substrate and the above-mentioned filter, wherein the substrate is provided with a packaging layer, and the filter is located outside the packaging layer.

[0030] It can be seen from the above technical solutions that the advantages and positive effects of the preparation method of the filter defining layer, the filter defining layer, the filter and the display device of the present application are:

[0031] The present application provides a method for preparing a filter defining layer, including forming a first structural layer on a substrate, forming a second structural layer on the first structural layer, patterning the first structural layer, and forming a reflective film on the second structural layer to form a reflective bank. The reflective film effectively improves the utilization rate of blue light, improves the light conversion efficiency, and reduces the light crosstalk phenomenon. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0033] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0034] Figure 1-Figure 6 is a schematic diagram showing a method for preparing a filter bank according to an exemplary embodiment.

[0035] Figure 7-Figure 11 FIG. 4 is a schematic diagram showing another method for preparing a filter bank according to an exemplary embodiment.

[0036] Fig.12 is a schematic diagram of a structure including a filter according to an exemplary embodiment.

[0037] Fig.13 is a schematic diagram of a display device according to an exemplary embodiment.

[0038] The reference numerals are described as follows:

[0039] 100-substrate; 200-first structural layer; 300-second structural layer; 400-reflective film; 500-pixel layer; 600-photoresist layer; 700-LED light-emitting layer; 800-optical adhesive layer; 900-protective layer; 1000-light filter layer;

[0040] 110-glass cover;

[0041] 610-Preparation area. DETAILED DESCRIPTION

[0042] In order to make the purpose, technical solutions and advantages of the embodiments of the present application clearer, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of this application. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the invention claimed for protection, but merely represents the selected embodiments of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of the present invention.

[0043] QDCF (Quantum Dots Color Filter) is usually used in display screens. QD quantum dots have the advantages of high light conversion rate, high color gamut and high color purity. Since the electro-QD display technology is still immature, the existing QD display mainly uses photo-QD display, which replaces the traditional color filter with QD to effectively improve the display color gamut and truly restore the display color. Since QD has a low absorption rate for blue light, a thicker QD film layer needs to be prepared to effectively absorb blue light and improve the blue light conversion rate. Usually, the thickness of the QD film layer is required to be more than 10um, so a thicker bank is required, but a thicker bank will increase the light absorption rate. The probability of crosstalk problem occurring. In order to solve the technical problem that the existing QD filter has low blue light absorption rate, the present application provides a method for preparing a filter bank, a filter bank, a filter and a display device. The method for preparing the filter bank includes: forming a first structure layer 200 on a substrate 100, forming a second structure layer 300 on the first structure layer 200, patterning the first structure layer 200, and forming a reflective film 400 on the second structure layer 300. The reflective film 400 effectively improves the utilization rate of blue light, improves the light conversion efficiency, and effectively reduces the light crosstalk phenomenon.

[0044] Figure 1-Figure 6 is a schematic diagram showing a method for preparing a filter bank according to an exemplary embodiment.

[0045] Fig.12 is a schematic diagram of a structure including a filter according to an exemplary embodiment.

[0046] Fig.13 is a schematic diagram of a display device according to an exemplary embodiment.

[0047] refer to Figure 1-6As shown, the embodiments of the present application provide a method for preparing a filter bank, a filter bank, a filter and a display device. The filter bank is processed by the above-mentioned method for preparing the filter bank, the filter is installed with the above-mentioned filter bank, and the display device includes a substrate 100 and the above-mentioned filter.

[0048] The preparation method of the filter bank includes:

[0049] Step 1: forming a first structure layer 200 on a substrate 100;

[0050] Specifically, Figure 1 The substrate 100 can be an LED light emitting (EL) substrate, a micro-light emitting diode display substrate, a substrate for completing LED bonding, or a glass plate. MTD / Cu or Ti / Cu, that is, molybdenum nickel titanium / copper or titanium / copper alloy material can be used to prepare the first structural layer 200.

[0051] As understood by those skilled in the art, the first structural layer 200 may also be made of other conductive metals, such as a single layer of Mo, Al, Au, etc., a multilayer structure formed by one metal, or a multilayer structure formed by multiple metals.

[0052] Step 2: forming a second structure layer 300 on the first structure layer 200;

[0053] Specifically, Figure 2-4 , prepare a photoresist on the first structure layer 200, and pattern the photoresist to form a patterned photoresist layer 600, remove part of the photoresist to form a preparation area 610, electroplate Cu on the first structure layer 200 located in the preparation area 610 to form a second structure layer 300, and remove the photoresist layer 600.

[0054] As understood by those skilled in the art, the second structural layer 300 may also be prepared by using other electroplated metals, such as Sn, Ni, Au, Ag, Pt, etc.

[0055] The thickness of the second structural layer 300 is between 2 μm and 100 μm, and preferably, the second structural layer 300 is greater than 6 μm. The thickness of the photoresist layer 600 needs to be greater than 10% of the thickness of the second structural layer 300 and less than 200% of the thickness of the second structural layer 300. The second structural layer 300 is prepared using copper material, which can realize the preparation of thick film layers and can also improve the heat dissipation effect of the protective layer 900 in the display device.

[0056] Step 3: patterning the first structural layer 200;

[0057] Specifically, refer to Figure 5, using the second structure layer 300 as a mask layer, the first structure layer 200 is etched with an etching solution to form a patterned first structure layer 200 .

[0058] Step 4: forming a reflective film 400 on the second structural layer 300;

[0059] Specifically, the reflective film 400 is formed on the second structure layer 300 by chemically plating Ag, and the reflective film 400 wraps the first structure layer 200 and the second structure layer 300, and the thickness of the reflective film 400 is between 0.001 μm and 1 μm. The use of Ag (silver) material to prepare the reflective film can effectively improve the utilization rate of blue light, improve the light conversion efficiency, and effectively reduce the light crosstalk phenomenon.

[0060] In the present application, the filter bank is manufactured by using the above-mentioned preparation method of the filter bank, and the bank (definition layer) includes a first structure layer 200, a second structure layer 300 and a reflective layer.

[0061] refer to Figure 12-13 As shown, the filter is a quantum dot color filter, and the filter includes a first structure layer 200, a second structure layer 300, a reflective layer and a pixel layer 500. The first structure layer 200 is a patterned MTD / Cu layer or Ti / Cu layer, the second structure layer 300 is a patterned Cu (copper) layer, the second structure layer 300 is formed on the first structure layer 200, and the reflective film 400 is chemically plated with Ag (silver) to wrap the first structure layer 200 and the second structure layer 300, and the pixel layer 500 is filled with quantum dots. The filter is arranged on a substrate 100, and the substrate 100 can be a light emitting (EL) substrate of an LED, a micro-light emitting diode display substrate, a substrate for completing LED bonding, or a glass plate.

[0062] Embodiments of the present application Fig.13 It is a schematic diagram of a partial structure of a display device, which includes a protective layer 900, an optical adhesive layer 800, an LED light-emitting layer 700, a filter and a substrate 100. The substrate 100 is a glass cover plate 110, and the filter layer 1000 is located above the filter.

[0063] In some embodiments, the filter in the present application scheme can be set on the light-emitting (EL) substrate of the LED or the micro-light-emitting diode display substrate, and a packaging layer can be set between the light-emitting (EL) substrate of the LED and the filter or between the micro-light-emitting diode display substrate and the filter to reduce the probability of parasitic capacitance formation.

[0064] In the embodiment of the present application, the bank of the filter plate only requires one patterning process, the processing technology is simple, and the processing efficiency is high. The reflective film is prepared using Ag (silver) material. Ag can prevent the second structural layer 300 from oxidizing and improve the reflectivity of Cu, thereby effectively improving the utilization rate of blue light and the light conversion efficiency. At the same time, the probability of optical crosstalk is effectively reduced. The second structural layer 300 is prepared using copper material, which can improve the heat dissipation effect of the protective layer 900.

[0065] Example 2

[0066] Figure 7-Figure 11 FIG. 4 is a schematic diagram showing another method for preparing a filter bank according to an exemplary embodiment.

[0067] Fig.12 is a schematic diagram of a structure including a filter according to an exemplary embodiment.

[0068] Fig.13 is a schematic diagram of a display device according to an exemplary embodiment.

[0069] refer to Figure 7-11 As shown, the embodiments of the present application provide a method for preparing a filter bank, a filter bank, a filter and a display device. The filter bank is processed by the above-mentioned method for preparing the filter bank, the filter is installed with the above-mentioned filter bank, and the display device includes a substrate 100 and the above-mentioned filter.

[0070] The preparation method of the filter bank includes:

[0071] Step 1: forming a first structure layer 200 on a substrate 100;

[0072] Specifically, refer to Figure 7 The substrate 100 can be an LED light emitting (EL) substrate, a micro-LED display substrate, a substrate for LED bonding, or a glass plate. MTD / Cu or Ti / Cu can be selected, and the first structural layer 200 can be prepared using molybdenum nickel titanium / copper or titanium / copper alloy material.

[0073] As understood by those skilled in the art, the first structural layer 200 may also be made of other conductive metals, such as a single-layer structure of Mo, Al, Au, etc., a multi-layer structure formed by one metal, or a multi-layer structure formed by multiple metals.

[0074] Step 2: forming a second structure layer 300 on the first structure layer 200;

[0075] Specifically, refer to Figure 8, Cu is electroplated on the first structural layer 200 to form a Cu layer. The thickness of the Cu layer is between 2 μm and 100 μm. Preferably, the second structural layer 300 is greater than 6 μm. The second structural layer 300 is prepared using copper material. Copper can realize the preparation of a thick film layer, which can improve the heat dissipation effect of the protective layer 900 in the display device.

[0076] As understood by those skilled in the art, the second structural layer 300 may also be prepared by using other electroplated metals, such as Sn, Ni, Au, Ag, Pt, etc.

[0077] Step 3: forming a patterned photoresist layer 600 on the second structure layer 300;

[0078] Specifically, refer to Fig. 9 , prepare a photoresist on the second structure layer 300 , and pattern the photoresist according to requirements to form a patterned photoresist layer 600 .

[0079] Step 4: Reference Fig.10 , using the patterned photoresist layer 600 as a mask, the Cu layer and the first structure layer 200 are patterned in sequence, and the Cu layer is patterned to form the second structure layer 300 .

[0080] Step 5: forming a reflective film 400 on the second structural layer 300;

[0081] Specifically, refer to Fig.11 The reflective film 400 is formed on the second structure layer 300 by chemically plating Ag. The reflective film 400 wraps the first structure layer 200 and the second structure layer 300. The thickness of the reflective film 400 is between 0.001μm and 1μm. The reflective film is made of Ag (silver). Ag can prevent the second structure layer 300 from oxidizing and improve the reflectivity of Cu, thereby effectively improving the utilization rate of blue light and the light conversion efficiency, while effectively reducing the probability of light crosstalk.

[0082] In the present application, the filter bank is manufactured by using the above-mentioned preparation method of the filter bank, and the bank (definition layer) includes a first structure layer 200, a second structure layer 300 and a reflective layer.

[0083] refer to Figure 12-13As shown, the filter is a quantum dot color filter, and the filter includes a first structure layer 200, a second structure layer 300, a reflective layer and a pixel layer 500. The first structure layer 200 is a patterned MTD / Cu layer or Ti / Cu layer, the second structure layer 300 is a patterned Cu (copper) layer, and the second structure layer 300 is formed on the first structure layer 200. The reflective film 400 is coated with the first structure layer 200 and the second structure layer 300 by chemical Ag (silver) plating. The pixel layer 500 is formed on the patterned Cu layer and the Cu area is removed. The pixel layer 500 is filled with quantum dots. The filter is arranged on a substrate 100, and the substrate 100 can be a light-emitting (EL) substrate of an LED, a micro-light-emitting diode display substrate, a substrate for completing LED bonding, or a glass plate.

[0084] Embodiments of the present application Fig.13 The partial structural diagram of a display device includes a protective layer 900, an optical adhesive layer 800, an LED light-emitting layer 700, a filter and a substrate 100. The substrate 100 includes a glass cover plate 110. The filter layer 1000 is located above the filter. In some embodiments, the filter in the present application can be disposed on the LED light-emitting (EL) substrate or the micro-LED display substrate. A packaging layer can be disposed between the LED light-emitting (EL) substrate and the filter or between the micro-LED display substrate and the filter to reduce the possibility of parasitic capacitance formation.

[0085] In the embodiment of the present application, the bank of the filter plate only requires one patterning process, the processing technology is simple, and the processing efficiency is high. The reflective film is prepared using Ag (silver) material. Ag can prevent the second structural layer 300 from oxidizing and improve the Cu reflectivity, thereby effectively improving the utilization rate of blue light and the light conversion efficiency. At the same time, the probability of optical crosstalk problems is effectively reduced. The second structural layer 300 is prepared using copper material, which can also improve the heat dissipation effect of the protective layer 900.

[0086] In summary, the present application provides a method for preparing a filter bank, a filter bank, a filter and a display device. The filter bank is processed by the preparation method of the filter bank, the filter is installed with the filter bank, the display device includes a substrate 100 and the filter, and the second structural layer 300 in the filter bank can adopt two processing forms. Both processing forms only require one patterning process, and the processing process is simple and the processing efficiency is high. During the processing of the filter bank, a first structure layer 200 is first formed on the substrate 100, and then a second structure layer 300 is prepared. In a first method of processing the second structure layer 300, a photoresist is prepared on the first structure layer 200, and the photoresist is patterned according to a processing pattern of the second structure layer 300 to form a patterned photoresist layer 600, and then the second structure layer 300 is formed in the area where the photoresist is removed by an electroplating process, and the photoresist layer 600 is removed to complete the preparation of the second structure layer 300; in a second processing method of the second structure layer 300, a Cu layer and a photoresist are sequentially prepared on the first structure layer 200, the photoresist is patterned to form a patterned photoresist layer 600, and then the Cu layer and the first structure layer 200 are patterned using the patterned photoresist layer 600 as a mask, and the photoresist layer 600 is removed to complete the preparation of the second structure layer 300.

[0087] In the first processing method of the second structure layer 300, after the second structure layer 300 is formed, the first structure layer 200 is patterned using the second structure layer 300 as a mask. In the second processing method of the second structure layer 300, the second structure layer 300 and the first structure layer 200 are patterned in sequence using the patterned photoresist layer 600 as a mask. No matter which processing method is used, only one patterning process is required in the filter bank processing method, and the processing process is simple and the processing efficiency is high. Finally, a reflective film 400 is formed on the second structure layer 300 by chemical plating Ag. The reflective film 400 wraps the first structure layer 200 and the second structure layer 300, and the thickness of the reflective film 400 is between 0.001μm-1μm. The reflective film is prepared using Ag (silver) material. Ag can prevent the second structure layer 300 from oxidizing, improve the Cu reflectivity, and form a reflective bank, thereby effectively improving the utilization rate of blue light, improving the light conversion efficiency, and effectively reducing the probability of light crosstalk problems.

[0088] In the present application, the filter can be set on the LED light-emitting (EL) substrate or the micro-light-emitting diode display substrate. During the processing of the filter bank, a packaging layer can be prepared first, and then a first structural layer 200 can be prepared on the packaging layer. The packaging layer separates the filter bank from the wires in the substrate 100 to reduce the possibility of parasitic capacitance formation.

[0089] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0090] The above description is only a specific embodiment of the present invention, so that those skilled in the art can understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the general inventive concept of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but should conform to the widest scope consistent with the principles and novel features applied herein.

Claims

1. A method for preparing a filter defining layer, characterized in that: include: forming a first structural layer (200) on a substrate (100); forming a second structural layer (300) on the first structural layer (200); Patterning the first structural layer (200); forming a reflective film (400) on the second structural layer (300); Forming a second structural layer (300) on the first structural layer (200) includes: Preparing a photoresist on the first structural layer (200), and patterning the photoresist to form a photoresist layer (600) and a preparation area (610); electroplating Cu on the first structural layer (200) located in the preparation area (610) to form a second structural layer (300); and removing the photoresist layer (600); or Forming a Cu layer by electroplating on the first structural layer (200); forming a patterned photoresist layer (600) on the Cu layer; and patterning the Cu layer through the photoresist layer (600) to form the second structural layer (300); The method of preparing a reflective film (400) on the second structural layer (300) includes: Forming a reflective film (400) on the second structural layer (300) by chemically plating Ag; The reflective film (400) wraps the first structural layer (200) and the second structural layer (300).

2. The method for preparing a filter defining layer according to claim 1, characterized in that: The thickness of the second structural layer (300) is between 2 μm and 100 μm.

3. The method for preparing a filter defining layer according to claim 1, characterized in that: Forming a first structural layer (200) on a substrate (100) includes: MTD / Cu or Ti / Cu is selected to form the first structural layer (200) on the substrate (100).

4. The method for preparing a filter defining layer according to claim 1, characterized in that: The thickness of the reflective film (400) is between 0.001 μm and 1 μm.

5. A filter defining layer, characterized in that: The filter defining layer is processed by the preparation method of any one of claims 1 to 4.

6. A filter, characterized in that: The filter defining layer according to claim 5 is installed.

7. A display device, characterized in that: It comprises a substrate (100) and the optical filter according to claim 6, wherein the substrate (100) is provided with a packaging layer, and the optical filter is located outside the packaging layer.