Photoelectric sensor and method for manufacturing the same
By forming a second isolation structure with a larger embedded depth and a third isolation structure connected to it on the semiconductor substrate of the photoelectric sensor, the problem of deep trench isolation DTI etching penetration is solved, and efficient pixel isolation and Miniaturization improves device quality and reliability.
Patent Information
- Application Number
- CN202111308541.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-05
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-11-05
AI Technical Summary
When manufacturing deep trench isolation DTI for existing photoelectric sensors, it is easy to etch through the shallow trench isolation STI that has been formed on the front, resulting in pixel performance failure and making it difficult to achieve efficient pixel isolation and shrinkage.
The first and second isolation structures are embedded on the front side of the semiconductor substrate. The depth of the second isolation structure is more than 1.5 times that of the first isolation structure, and a third isolation structure is formed on the back side, which is connected up and down with the second isolation structure. Ensure excellent isolation effect between adjacent pixels and reduce etching difficulty.
It improves the pixel isolation effect and device quality of the photoelectric sensor, reduces crosstalk between adjacent pixels, achieves shrinkage of pixel size and spacing, avoids substrate etching penetration, and improves the reliability of the device.
Smart Images

Figure CN114023776B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of photosensitive technology, and in particular to a photoelectric sensor and a method for manufacturing the photoelectric sensor. Background Art
[0002] A photoelectric sensor is a device that converts light signals into electrical signals. Its working principle is based on the photoelectric effect, that is, when light shines on certain substances in the photoelectric sensor, the electrons of the substance absorb the energy of the photons and change their state. The photogenerated charge formed causes the photoelectric sensor to produce a corresponding electrical effect.
[0003] Chinese patent CN102938409A discloses a photoelectric sensor based on a composite dielectric gate MOSFET, in which each pixel includes a photosensitive transistor (also called a MOS capacitor) and a reading transistor. Figure 1 It is a planar schematic diagram of the pixel structure of a photoelectric sensor. Figure 2 yes Figure 1 Schematic diagram of the AB section and CD section. Figure 1 and Figure 2 In each pixel of the photoelectric sensor, a substrate (e.g., p-doped) is separated into a photosensitive region 110 and a charge reading region 120 by shallow trench isolation (STI), and a gate stack including a gate oxide layer, a floating gate, an inter-gate dielectric layer, and a control gate (CG) is formed on the substrate of the photosensitive region 110 and the charge reading region 120, wherein the substrate of the photosensitive region 110 and the gate stack above constitute a MOS capacitor (e.g., Figure 2 The substrate of the charge reading region 120 is formed with a p-well region, a source region S and a drain region D. The substrate of the charge reading region 120 and the gate stack above constitute a read transistor (such as Figure 2 The cross-sectional structure on the right is shown in the figure).
[0004] The above-mentioned photosensitive capacitor and the floating gate, inter-gate dielectric layer and control gate of the read transistor are usually connected as one (especially the floating gate). When the photoelectric sensor is working, the photogenerated charge formed in the photosensitive area 110 of the substrate is collected under the gate oxide layer under the action of the vertical electric field, and crosses the potential barrier to enter the floating gate for storage. Therefore, it is also called a vertical charge photoelectric sensor (Vertical-transferring-charge pixel Sensor, VPS). By using MOS capacitors and read transistors to control the generation, collection, readout and reset of photogenerated charges, the charge amount or charge change in the floating gate of the VPS can be obtained, thereby realizing light signal detection.
[0005] Compared with traditional semiconductor photosensitive devices based on photodiodes (such as CMOS image sensors), VPS has a simpler structure and can achieve smaller pixel sizes, or in other words, it can achieve higher full well charges at the same pixel size, thus having a higher signal-to-noise ratio. Therefore, the miniaturization of pixel size and the spacing between pixels is the main development direction of VPS. Due to the small pixel size and the spacing between pixels, how to avoid crosstalk between adjacent pixels also faces greater challenges than traditional semiconductor photosensitive devices, so the isolation between adjacent pixels in VPS is crucial.
[0006] For the isolation between pixels of VPS, the existing technology usually adopts the method of "front STI + back DTI", that is, a shallow trench isolation STI (shallow trench isolation) is made on the front side of the substrate, and the shallow trench isolation STI is set between two adjacent pixels and between the photosensitive area and the charge reading area in the same pixel, and a deep trench isolation DTI (deep trench isolation) is made on the back side of the substrate, and the deep trench isolation DTI is aligned with the shallow trench isolation STI between adjacent pixels on the front side, and is connected up and down with the aligned shallow trench isolation STI in at least part of the area, so as to form a complete physical isolation between pixels. However, research has found that when the trench (DTI trench) of the deep trench isolation DTI is opened from the back side, it is easy to etch through the substrate around the shallow trench isolation STI formed on the front side (such as Figure 3 The dotted circle area shown in the figure) causes pixel performance failure. Summary of the invention
[0007] The present invention provides a method for manufacturing a photoelectric sensor, so as to ensure that the pixels of the VPS have a better isolation effect while improving the device quality, facilitating the miniaturization of the pixel size and the spacing between pixels, and avoiding crosstalk. The present invention also provides a photoelectric sensor.
[0008] In one aspect, the present invention provides a method for manufacturing a photoelectric sensor, comprising:
[0009] Providing a semiconductor substrate, the semiconductor substrate having a plurality of pixel regions, each of the pixel regions being used to form a MOS capacitor and a read transistor that use a common floating gate to realize light sensing;
[0010] A first isolation structure is formed on the front surface of the semiconductor substrate, wherein the first isolation structure separates each pixel region into a photosensitive region and a charge readout region, wherein the photosensitive region is used to manufacture the MOS capacitor, and the charge readout region is used to manufacture a read transistor;
[0011] forming an embedded second isolation structure on the front surface of the semiconductor substrate, wherein the second isolation structure is located between adjacent pixel regions; and,
[0012] An embedded third isolation structure is formed on the back side of the semiconductor substrate, and the third isolation structure is located between adjacent pixel areas. The third isolation structure corresponds to the second isolation structure up and down and is connected to each other, wherein the embedding depth of the second isolation structure in the semiconductor substrate is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate.
[0013] Optionally, the step of forming the first isolation structure includes:
[0014] forming a pad oxide layer and a first nitride layer in sequence on the front surface of the semiconductor substrate;
[0015] Etching the first nitride layer, the pad oxide layer, and the semiconductor substrate to form a first trench penetrating the first nitride layer and the pad oxide layer and having a bottom surface located in the semiconductor substrate;
[0016] Filling the first trench with an isolation dielectric, and using a planarization process to make the upper surface of the isolation dielectric in the first trench flush with the upper surface of the first nitride layer;
[0017] The first nitride layer is removed, and the isolation medium in the first trench is used as the first isolation structure.
[0018] Optionally, the step of forming the second isolation structure includes:
[0019] forming a second nitride layer on the semiconductor substrate, wherein the second nitride layer covers the pad oxide layer and the first isolation structure, and an upper surface of the second nitride layer is higher than an upper surface of the first isolation structure as a whole;
[0020] Etching the second nitride layer, the pad oxide layer, and the semiconductor substrate to form a second trench penetrating the second nitride layer and the pad oxide layer and having a bottom surface located in the semiconductor substrate, wherein the depth of the second trench in the semiconductor substrate is more than 1.5 times the depth of the first isolation structure in the semiconductor substrate;
[0021] Filling the second trench with an isolation dielectric, and using a planarization process to make the upper surface of the isolation dielectric in the second trench flush with the upper surface of the second nitride layer;
[0022] The second nitride layer is removed, and the isolation medium in the second trench is used as the second isolation structure, wherein the upper surface of the second isolation structure is above the first isolation structure.
[0023] Optionally, after forming the second isolation structure and before forming the third isolation structure, the method for manufacturing the photoelectric sensor further includes:
[0024] removing the pad oxide layer, and forming a gate oxide material layer and a floating gate material layer on the semiconductor substrate, wherein the gate oxide material layer covers the upper surface of the semiconductor substrate, the floating gate material layer covers the gate oxide material layer and the first isolation structure and the second isolation structure, and the upper surface of the floating gate material layer is entirely located above the second isolation structure;
[0025] Using a planarization process to remove a portion of the thickness of the floating gate material layer, so that the upper surface of the remaining floating gate material layer is flush with the upper surface of the second isolation structure, and the remaining floating gate material layer continuously covers the photosensitive area and the charge readout area of each pixel area, serving as a floating gate shared by the MOS capacitor and the read transistor; and
[0026] An inter-gate dielectric material layer and a control gate material layer are sequentially formed on the semiconductor substrate.
[0027] Optionally, before forming the inter-gate dielectric material layer, the method for manufacturing the photoelectric sensor further includes:
[0028] The second isolation structure is etched back so that the upper surface of the second isolation structure is lower than the upper surface of the floating gate, thereby forming a groove between adjacent floating gates, the inter-gate dielectric material layer covers the inner surface of the groove, the control gate material layer covers the inter-gate dielectric material layer and fills the groove, and the second isolation structure after the back etching serves as a front pixel separation structure.
[0029] Optionally, the step of forming the third isolation structure includes:
[0030] Thinning the semiconductor substrate from the back side;
[0031] forming a patterned mask layer on the back side of the semiconductor substrate, wherein an opening in the mask layer is formed in a region where the second isolation structure vertically extends toward the back side of the semiconductor substrate;
[0032] Using the patterned mask layer, etching the semiconductor substrate from the back to form a third trench, wherein the bottom surface of the third trench exposes the second isolation structure;
[0033] Filling the third trench with an isolation dielectric, and using a planarization process to make a surface of the isolation dielectric in the third trench away from the bottom surface of the third trench flush with a surface of the patterned mask layer;
[0034] The patterned mask layer is removed, and the isolation medium in the third trench is used as the third isolation structure.
[0035] Optionally, the isolation medium in the second trench and / or the third trench is formed by an atomic layer deposition process.
[0036] Optionally, the isolation dielectric in the second trench and / or the third trench includes a high-k dielectric layer and an insulating layer covering the high-k dielectric layer and having a lower dielectric constant than the high-k dielectric layer.
[0037] Optionally, the semiconductor substrate has a plurality of substrate lead-out regions arranged between the plurality of pixel regions, each of the substrate lead-out regions being connected to the substrates of more than two pixel regions so as to apply a voltage to the substrates of the pixel regions through the substrate lead-out regions; and the first isolation structure limits the range of the substrate lead-out regions.
[0038] Optionally, the embedding depth of the first isolation structure in the semiconductor substrate is The embedding depth of the second isolation structure in the semiconductor substrate is
[0039] In one aspect, the present invention provides a photoelectric sensor, the photoelectric sensor comprising:
[0040] A semiconductor substrate having a plurality of pixel regions, each of which is used to form a MOS capacitor and a read transistor that use a common floating gate to realize light sensing;
[0041] A first isolation structure is embedded on the front side of the semiconductor substrate, wherein the first isolation structure separates each pixel region into a photosensitive region and a charge readout region, wherein the photosensitive region is used to construct the MOS capacitor, and the charge readout region is used to construct a read transistor;
[0042] A front pixel separation structure is embedded on the front side of the semiconductor substrate, wherein the front pixel separation structure is located between adjacent pixel regions; and
[0043] A third isolation structure is embedded on the back side of the semiconductor substrate, the third isolation structure is located between adjacent pixel areas, and the third isolation structure corresponds to the front pixel separation structure in upper and lower directions and is interconnected, wherein the embedding depth of the front pixel separation structure in the semiconductor substrate is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate.
[0044] The manufacturing method of the photoelectric sensor provided by the present invention forms a first isolation structure and a second isolation structure on the front side of the semiconductor substrate, and the embedding depth of the second isolation structure in the semiconductor substrate is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate, which is convenient for ensuring the working performance of the photosensitive area and the charge readout area, and a third isolation structure is formed on the back side of the semiconductor substrate, and the second isolation structure corresponds to the third isolation structure up and down and is connected to each other, so that there is an excellent isolation effect between adjacent pixel areas, and because the second isolation structure is embedded deeper than the first isolation structure, the manufacturing difficulty of the third isolation structure is lower, and it is not easy to carve through the substrate. Since the manufacturing method is convenient for ensuring the working performance of the photosensitive area and the charge readout area, there is an excellent isolation effect between adjacent pixel areas and it is not easy to carve through the substrate, the crosstalk between adjacent pixels of the photoelectric sensor provided by the present invention is small, which is convenient for miniaturization of pixel size and spacing between pixels, and the device has better quality and reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 It is a planar schematic diagram of the pixel structure of a photoelectric sensor.
[0046] Figure 2 yes Figure 1 Schematic diagram of the AB section and the CD section.
[0047] Figure 3 The invention is a cross-sectional schematic diagram of a photoelectric sensor substrate using front shallow trench isolation STI and back deep trench isolation DTI.
[0048] Figure 4 A schematic flow chart of a method for manufacturing a photoelectric sensor according to an embodiment of the present invention.
[0049] Figure 5 FIG. 4 is a schematic plan view of a photoelectric sensor according to an embodiment of the present invention.
[0050] FIG. 6A to FIG. 6O It is a cross-sectional schematic diagram of a photoelectric sensor during the manufacturing process using a manufacturing method according to an embodiment of the present invention.
[0051] Description of reference numerals:
[0052] 100-pixel area; 110-photosensitive area; 120-charge reading area; 200-substrate lead-out area; 10-semiconductor substrate; 101-pad oxide layer; 102-first nitride layer; 103, 105-isolation dielectric; 10a-first groove; 104-second nitride layer; 10b-second groove; 106-gate oxide material layer; 107-floating gate material layer; 108-inter-gate dielectric material layer; 109-control gate material layer; 10c-groove; 110-front pixel separation structure; 10d-third groove; 121-high-k dielectric layer; 122-insulating layer; 120-back pixel separation structure. DETAILED DESCRIPTION
[0053] The photoelectric sensor and the method for making the same of the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become clearer based on the following description. It should be noted that the accompanying drawings are in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the embodiments of the present invention. The embodiments of the present invention should not be considered to be limited to the specific shapes of the areas shown in the drawings. For the sake of clarity, in all the drawings used to assist in explaining the embodiments of the present invention, the same components are marked with the same reference numerals in principle, and repeated descriptions thereof are omitted.
[0054] The photoelectric sensor of the embodiment of the present invention adopts the pixel structure of the dual-transistor photoelectric sensor disclosed in Chinese patent CN102938409A. Figure 2 As an example, in this type of photoelectric sensor, the pixel can realize photoelectric sensing in the following way: first, in the exposure stage, a negative bias voltage less than 0V and greater than or equal to -20V (for example, -3V) is applied to the substrate, and a positive bias voltage greater than 0V and less than or equal to 20V is connected to the control gate, thereby forming a continuous depletion region in the substrate. When light is incident from the lower surface (i.e., the back side) of the substrate, the photons reaching the depletion region can excite photogenerated charges under appropriate conditions and migrate to the floating gate under the drive of the electric field. The floating gate plays a charge storage role. This process mainly forms the photosensitivity of the MOS capacitor. Then, in the charge reading stage, the source region S and the substrate are grounded (0V), the drain region D is connected to a suitable positive bias voltage (for example, greater than 0 and less than 3V), and the above-mentioned reading transistor is operated in the linear region by adjusting the voltage of the control gate. Since the MOS capacitor is connected to the floating gate of the reading transistor, the number of photogenerated charges stored in the floating gate during the exposure stage can be obtained by measuring the drift of the drain current; then in the reset stage, the control gate is connected to a negative bias voltage, the substrate and the source region S of the reading transistor are connected to the same positive bias voltage (for example, greater than 0 and less than 3V), and the photogenerated charges stored in the floating gate reach the source region.
[0055] The substrate in the above-mentioned photoelectric sensor can be any suitable substrate in the art, for example, a p-type (for example, doped with boron or boron difluoride) doped silicon substrate. The doping concentration of the silicon substrate is relatively low (p-), for example, the doped boron ion density is 1×10 12 / cm 2 ~2×10 12 / cm 2 In order to obtain a wider depletion region in the substrate during the exposure stage, it is helpful to improve the light conversion quantum efficiency. The charge reading region 120 of the substrate is formed with a p-well, and the source region and the drain region are heavily doped with n-type and formed on the top of the p-well. It should be noted that this article mainly uses the reading transistor in the photoelectric sensor pixel as an example to illustrate that the n-type is used as the example. It can be understood that in the case where the reading transistor is p-type, the source region and the drain region need to be formed as p-type heavily doped. Correspondingly, the substrate can use an n-type lightly doped substrate (for example, doped with phosphorus or arsenic).
[0056] When the above-mentioned pixel structure is used to form a photoelectric sensor, in order to give full play to the advantages of its relatively simple structure and the ability to achieve smaller pixels, the pixel size is designed to be smaller. Usually, the maximum radial dimension of each pixel area on the substrate is less than 1 μm, or even less than 0.5 μm. In order to improve the photosensitivity, it is very important to minimize the crosstalk between adjacent pixels. In order to ensure better isolation between pixels while improving device quality, thereby facilitating the miniaturization of pixel size and spacing between pixels and avoiding crosstalk, an embodiment of the present invention introduces a method for manufacturing a photoelectric sensor.
[0057] Figure 4 FIG. 1 is a flow chart of a method for manufacturing a photoelectric sensor according to an embodiment of the present invention. Figure 4 The method for manufacturing the photoelectric sensor of the embodiment of the present invention comprises the following steps:
[0058] S1: providing a semiconductor substrate, wherein the semiconductor substrate has a plurality of pixel regions, each of the pixel regions being used to form a MOS capacitor and a read transistor that use a common floating gate to realize light sensing;
[0059] S2: forming a first isolation structure embedded on the front surface of the semiconductor substrate, wherein the first isolation structure separates each pixel region into a photosensitive region and a charge readout region, wherein the photosensitive region is used to manufacture the MOS capacitor, and the charge readout region is used to manufacture a read transistor;
[0060] S3: forming an embedded second isolation structure on the front surface of the semiconductor substrate, wherein the second isolation structure is located between adjacent pixel regions;
[0061] S4: A third isolation structure is formed on the back side of the semiconductor substrate, wherein the third isolation structure is located between adjacent pixel regions, and the third isolation structure corresponds to the second isolation structure up and down and is interconnected, wherein the embedding depth of the second isolation structure in the semiconductor substrate is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate (here "more than 1.5 times" includes 1.5 times, the same below).
[0062] In the semiconductor substrate of step S1, a plurality of pixel regions are arranged in an array, for example, and the pixel regions separated in the substrate and the regions extending vertically above the substrate are referred to as pixel regions. Each of the pixel regions is used to form a VPS pixel that uses a shared floating gate to realize photosensitivity, that is, a MOS capacitor and a reading transistor that shares a floating gate with the MOS capacitor are planned to be formed in each pixel region (see the pixel structure described in the background technology). The semiconductor substrate is, for example, a silicon substrate with p-type conductive doping. The front side of the semiconductor substrate refers to the side used to form a photosensitive pixel by deposition, etching, ion implantation and other processes, that is, the substrate side that forms the gate stack described in the background technology, and the back side of the substrate is opposite to the front side, where the back side is the side where the light to be sensed is incident.
[0063] The method for manufacturing a photoelectric sensor according to an embodiment of the present invention forms a first isolation structure embedded in the front surface of the semiconductor substrate in step S2. The first isolation structure is, for example, a shallow trench isolation STI, and its embedding depth in the semiconductor substrate is about The position of the first isolation structure is defined by the first graphical process. The first isolation structure is formed in each pixel area. The first isolation structure is embedded in a shallow position in the substrate and does not penetrate the substrate. In an embodiment of the present invention, the first isolation structure is used to separate the photosensitive area and the charge readout area in each pixel area, which are used to make MOS capacitors and read transistors respectively. That is, in each pixel area, the photosensitive area and the charge readout area are isolated by the first isolation structure, but the substrates of the photosensitive area and the charge readout area are connected under the first isolation structure, so that the normal operation of the pixel will not be affected. In addition, in some embodiments, in order to facilitate the application of the same voltage to the substrate of each pixel so as to perform equipotential operation on the substrate of each pixel in the aforementioned photoelectric sensing process (for example, the depletion electric field generated by the substrate corresponding to each pixel needs to be basically the same during the exposure stage), refer to Figure 5In one embodiment, the photoelectric sensor includes a plurality of pixel areas 100, and the plurality of pixel areas 100 are arranged in an array along the row direction and the column direction. Each pixel area 100 includes a photosensitive area 110 and a charge readout area 120. The photosensitive area 110 is used to form the above-mentioned MOS capacitor, and the charge readout area 120 is used to form the above-mentioned reading transistor. In addition, the photoelectric sensor also has a plurality of substrate lead-out areas 200 arranged between the plurality of pixel areas 100, and each of the substrate lead-out areas 200 is connected to the substrates of more than two of the pixel areas. The purpose is to apply a voltage to the substrate of the adjacent pixel area through the substrate lead-out area 200 when the photoelectric sensor is working. Each substrate lead-out area 200 is connected to an external power supply, so that by applying a voltage to each substrate lead-out area 200, a voltage is applied to the substrate of each pixel area. In this embodiment, the first isolation structure formed in step S1 is also used to limit the range of the substrate lead-out area 200, that is, the first isolation structure only separates each substrate lead-out area 200 and the pixel area 100 connected to its substrate in the upper part of the substrate, such as Figure 5 Each substrate lead-out region 200 is connected to the substrates of the four surrounding pixel regions 100, so that a voltage can be applied to the substrates of the four surrounding pixel regions 100 through one substrate lead-out region 200. It should be noted that the arrangement of the substrate lead-out region 200 is not limited to Figure 5 The example is not limited to the example of the semiconductor substrate, but can be changed as needed, and can be specifically arranged in a manner disclosed in the art. For example, in some embodiments, the substrate lead-out region may not be arranged on the front side of the semiconductor substrate, but on the back side.
[0064] FIG. 6A to FIG. 6O FIG. 1 is a cross-sectional diagram of a method for manufacturing a photoelectric sensor according to an embodiment of the present invention during the manufacturing process. Figure 4 and FIG. 6A to FIG. 6O The production method is described in detail.
[0065] 6A to 6F FIG. 4 shows an exemplary formation process of the first isolation structure. Fig. 6A As shown, a pad oxide layer 101 and a first nitride layer 102 are first formed on the front surface of the semiconductor substrate 10 in sequence. The pad oxide layer 101 has a thickness of, for example, The silicon oxide layer is, for example, The first nitride layer 102 is, for example, The silicon nitride layer is specifically, for example, Then, if Figure 6BAs shown, a first patterning process is used, for example, a photoresist is coated on the first nitride layer, and a corresponding photomask is used for exposure and development, so that the photoresist covers the area to be protected, and then a suitable etching process is used to etch the first nitride layer 102, so as to form an opening in the first nitride layer 102, and then the first nitride layer 102 is used as a mask, and a suitable etching process is used to etch the pad oxide layer 101 exposed by the first nitride layer 102 and the semiconductor substrate 10 thereunder, so as to form a first trench 10a that penetrates the first nitride layer 102 and the pad oxide layer 101 and has a bottom surface located in the semiconductor substrate 10, and the etching depth of the first trench 10a is, for example, about Its opening width is about 50nm; then, Figure 6C As shown, an isolation dielectric 103 (eg, silicon oxide) is filled in the first trench 10a. The isolation dielectric 103 is filled in the first trench 10a and covers the first nitride layer 102. Then, as shown in FIG. Fig.6D As shown, a planarization process (such as CMP) is used to remove part of the isolation dielectric 103 (part of the thickness of the first nitride layer 102 may also be removed), and the remaining isolation dielectric 103 is filled in the first trench 10a, and the upper surface of the isolation dielectric 103 in the first trench 10a is flush with the upper surface of the first nitride layer 102; then, as shown in Fig. 6E As shown, the first nitride layer 102 is etched away, and the isolation dielectric 103 in the first trench 10a is used as a first isolation structure embedded in the semiconductor substrate 10 from the front. The upper surface of the first isolation structure is higher than the upper surface of the pad oxide layer 101, and the height difference between the two is approximately the thickness of the first nitride layer 102 removed by etching, and the height difference is small.
[0066] After forming the first isolation structure, the method for manufacturing a photosensor according to an embodiment of the present invention then forms an embedded second isolation structure on the front surface of the semiconductor substrate 10, wherein the second isolation structure is located between adjacent pixel regions. The second isolation structure is used to separate adjacent pixel regions from the front side.
[0067] FIG. 6F to FIG. 6I FIG. 4 shows an exemplary formation process of the second isolation structure. Fig. 6F As shown, first, a second nitride layer 104 is formed on the semiconductor substrate 10, and the second nitride layer 104 covers the pad oxide layer 101 and the first isolation structure formed on the front side. The second nitride layer 104 has a thickness of, for example, The thickness of the second nitride layer 104 in this embodiment is The thickness of the second nitride layer 104 is greater than that of the first nitride layer 102, so that the upper surface exceeds the first isolation structure; then, as Figure 6GAs shown, a second patterning process is adopted, for example, a photoresist is coated on the second nitride layer 104, and a corresponding mask (different from the first patterning process) is used for exposure and development, so that the photoresist covers the area to be protected, and then a suitable etching process is used to etch the second nitride layer 104, thereby forming an opening in the second nitride layer 104, and then the second nitride layer 104 is used as a mask to etch the pad oxide layer 101 and the semiconductor substrate 10 to form a second trench 10b that penetrates the second nitride layer 104 and the pad oxide layer 101 and has a bottom surface located in the semiconductor substrate 10, wherein the second trench 10b is deeper than the first trench 10a, and specifically, the depth of the second trench 10b in the semiconductor substrate 10 is more than 1.5 times the depth of the first isolation structure (or the first trench 10a) in the semiconductor substrate 10, for example, 2 times or 3 times, so that the second trench 10b is much deeper than the isolation structure (or the first trench 10a). Here, the depth of the second trench 10b and the first isolation structure (or the first trench 10a) in the semiconductor substrate 10 refers to the distance extending into the interior of the semiconductor substrate 10 along the substrate thickness direction with the upper surface of the semiconductor substrate 10 as the reference, that is, the depth of the second trench 10b in the semiconductor substrate 10 is equal to the longitudinal distance between the bottom surface of the second trench 10b and the upper surface of the semiconductor substrate 10, the depth of the first trench 10a in the semiconductor substrate 10 is equal to the longitudinal distance between the bottom surface of the first trench 10a and the upper surface of the semiconductor substrate 10, and the (embedded) depth of the first isolation structure in the semiconductor substrate 10 is equal to the longitudinal distance between the bottom end of the first isolation structure away from the upper surface of the semiconductor substrate 10 and the upper surface of the semiconductor substrate 10. The etching depth of the second trench 10b is about For example The opening width (i.e., the dimension of the second groove 10b in a direction perpendicular to both the depth direction and the extension direction) is about 50 nm to 100 nm; then, as Figure 6H As shown, the isolation dielectric 105 is filled in the second trench 10b, the isolation dielectric 105 is filled in the second trench 10b and covers the second nitride layer 104, and a planarization process (such as CMP) is used to remove part of the isolation dielectric 105 (part of the thickness of the second nitride layer 104 may also be removed), and the remaining isolation dielectric 105 is filled in the second trench 10b, and the upper surface of the isolation dielectric 105 in the second trench 10b is flush with the upper surface of the second nitride layer 104; then, as shown Fig.6IAs shown, the second nitride layer 104 is removed, and the isolation dielectric 105 in the second trench 10b is used as the second isolation structure. The depth of the second isolation structure in the semiconductor substrate 10 is equal to the longitudinal distance between the bottom of the second isolation structure away from the upper surface of the semiconductor substrate 10 and the upper surface of the semiconductor substrate 10. Since the depth of the second trench 10b in the semiconductor substrate 10 is more than 1.5 times the depth of the first isolation structure in the semiconductor substrate 10, the depth of the second isolation structure formed based on the second trench 10b in the semiconductor substrate 10 is more than 1.5 times the depth of the first isolation structure in the semiconductor substrate 10. In this embodiment, the upper surface of the second nitride layer 104 is formed to be higher than the upper surface of the first isolation structure. After removing the second nitride layer 104, the upper surface of the second isolation structure is above the first isolation structure. The embedded depth of the second isolation structure in the semiconductor substrate is about
[0068] In the above-mentioned process of forming the second isolation structure, since the second trench 10b is formed deeper than the first trench 10a, the second trench 10b and the first trench 10a can be formed using different etching conditions (such as etching pressure, intracavity pressure, type and flow rate of process gas, etching time, etc.), and the method of filling the isolation medium 105 in the second trench 10b can also adopt a filling method different from that of filling the isolation medium 103 in the first trench 10a. For example, the isolation medium 103 can be filled in the first trench 10a using a traditional CVD (chemical vapor deposition) process, and it is not necessary to deposit it layer by layer in an atomic layer manner, while the isolation medium 105 can be filled in the second trench 10b using an atomic layer deposition (ALD) process, so that the isolation medium 105 is deposited layer by layer on the inner surface of the second trench 10b in the form of a single atomic film until the opening of the second trench 10b is closed, and the isolation medium 105 continues to be deposited on the second trench 10b to a certain thickness.
[0069] In one embodiment, the isolation dielectric filled in the second trench 10b is silicon oxide, which is deposited to a thickness of about After the silicon oxide is formed, the opening of the second trench 10b is closed. However, since the second trench 10b is deep, there may be gaps inside the second trench 10b, but it does not affect the isolation effect of the second isolation structure. In another embodiment, when filling the isolation dielectric in the second trench 10b, a layer of high-k (dielectric constant) dielectric material is first deposited along the upper surface of the second nitride layer 104 and the inner surface of the second trench 10b to form a high-k dielectric layer. The dielectric constant of the high-k dielectric layer is higher than that of silicon oxide, for example, more than 3.9. Then, an insulating material (such as silicon oxide) with a dielectric constant lower than that of the high-k dielectric layer is used to cover the high-k dielectric layer and fill the second trench 10b. That is, the isolation dielectric filled in the second trench 10b in this embodiment includes a high-k dielectric layer and an insulating layer covering the high-k dielectric layer and having a dielectric constant lower than that of the high-k dielectric layer. The insulating layer is, for example, a silicon oxide layer. The material of the high-k dielectric layer may include at least one of Al2O3, Ta2O5, ZrO2, LaO, BaZrO, AlO, HfZrO, HfZrON, HfLaO, HfSiON, HfSiO, LaSiO, AlSiO, HfTaO, HfTiO, (Ba, Sr)TiO3 (BST), Si3N4, TiO2, nitride oxide or other suitable materials, and the thickness range is, for example, to The high-k dielectric layer can be formed by a suitable process such as CVD, ALD or PVD. Since there are charges of different properties in the high-k dielectric layer, by making the isolation dielectric of the second isolation structure include the high-k dielectric layer, that is, by arranging the high-k dielectric layer between two adjacent pixel areas separated by the second isolation structure, the charges (such as photogenerated charges) moving to the vicinity of the high-k dielectric layer can be absorbed, thereby helping to reduce the crosstalk between adjacent pixel areas.
[0070] In this embodiment, before step S4, the front device manufacturing is completed first, including the manufacturing of the gate stack described below. Specifically, the gate stack includes the following manufacturing process:
[0071] First, if Figure 6J As shown, after forming the above-mentioned second isolation structure and before forming the third isolation structure on the back side, the pad oxide layer 101 is removed, and a gate oxide material layer 106 and a floating gate material layer 107 are formed on the semiconductor substrate 10, wherein the gate oxide material layer 106 covers the upper surface of the semiconductor substrate 10, and the floating gate material layer 107 covers the gate oxide material layer 106 and the above-mentioned first isolation structure and the second isolation structure embedded in the semiconductor substrate 10, and the upper surface of the floating gate material layer 107 is entirely located above the second isolation structure;
[0072] Then, if Figure 6KAs shown, a planarization process is used to remove a portion of the floating gate material layer 107, so that the upper surface of the remaining floating gate material layer 107 is flush with the upper surface of the second isolation structure. Since the upper surface of the second isolation structure is higher than the upper surface of the first isolation structure, after the planarization process, the floating gate material layer 107 can continuously cover the photosensitive area and the charge readout area of each pixel area within the range of each pixel area (the photosensitive area and the charge readout area of each pixel area are isolated by the first isolation structure), and due to the isolation of the second isolation structure, the floating gate material layers 107 between adjacent pixel areas are disconnected from each other. Therefore, at this time, the floating gate material layer 107 within the range of each pixel area can be used as a floating gate (FG) shared by the MOS capacitor and the read transistor of the pixel area;
[0073] Next, an inter-gate dielectric material layer 108 and a control gate material layer 109 are sequentially formed on the semiconductor substrate 10 to form a gate stack in each pixel region. Specifically, as shown in FIG. Figure 6L As shown, the second isolation structure is first etched back so that the upper surface of the second isolation structure is lower than the upper surface of the floating gate, thereby forming a groove 10c between adjacent floating gates. The lowering of the upper surface of the second isolation structure does not affect its isolation effect on the adjacent pixel region substrate. Here, the upper surface of the second isolation structure after back etching is, for example, higher than the upper surface of the gate oxide material layer 106. When the second isolation structure includes a high-k dielectric layer, the back etching can also remove the high-k dielectric layer within the etching depth range. For simplicity, the second isolation structure after back etching is recorded as a front pixel separation structure 110. The upper surface of the front pixel separation structure 110 can be higher or lower than the upper surface of the first isolation structure, or it can be flush with the upper surface of the first isolation structure. Subsequently, as Figure 6M As shown, an inter-gate dielectric material layer 108 and a control gate material layer 109 are sequentially deposited on a semiconductor substrate 10, and the inter-gate dielectric material layer 108 conformally covers the surface of the floating gate and the front pixel separation structure 110, thereby covering the inner surface of the groove 10c and not filling the groove 10c. The control gate material layer 109 covers the inter-gate dielectric material layer 108 and fills the groove 10c. In this embodiment, the control gate material layer 109 continuously covers the upper surface and the side surface of the floating gate with the inter-gate dielectric material layer 108 interposed therebetween, which can improve the coupling efficiency compared to only covering the upper surface of the floating gate.
[0074] The inter-gate dielectric material layer 108 may be made of silicon oxide, silicon nitride, silicon oxynitride or other suitable materials, and may be a single layer or a stack of two or more layers, for example, an ON stack formed by stacking a silicon oxide layer with silicon nitride, or an ONO stack formed by stacking a bottom silicon oxide layer, a silicon nitride layer and a top silicon oxide layer in sequence. The control gate material layer 109 includes, for example, conductive polysilicon.
[0075] After forming the control gate material layer 109, other processes on the front side of the semiconductor substrate can be further completed. For example, after forming the above-mentioned control gate material layer 109, the control gate material layer 109, the inter-gate dielectric material layer 108 and the gate oxide material layer 106 are etched so that the remaining control gate material layer 109 is arranged into multiple rows as multiple control gates, and each control gate is shared by multiple pixel areas on the same row below. In each pixel area, a gate stack is formed on the surface of the substrate covering the photosensitive area and the readout charge area, and the gate stack includes a gate oxide material layer 106, a floating gate, an inter-gate dielectric material layer 108 and a control gate formed in sequence from bottom to top. Furthermore, a spacer process can be used to form a side wall on the side of the gate stack, and a source region S and a drain region D are formed in the substrate of the readout charge area by ion implantation (refer to Figure 1 and Figure 2 ). Thus, a MOS capacitor and a reading transistor for realizing photosensitivity can be formed corresponding to each pixel area. In addition, an interconnection structure (not shown) can be further made on the front side of the semiconductor substrate to electrically lead out and interconnect the control gate, source region S and drain region D of each pixel area. In addition, a passivation layer (not shown) can be made on the interconnection structure for protection. After completing the process on the front side of the substrate, in order to facilitate thinning and the production of the third isolation structure after flipping, a substrate can be bonded to the passivation layer first and then flipped. The following figures only illustrate the production of the third isolation structure, and the flipping and thinning process are not shown.
[0076] The method for manufacturing a photoelectric sensor according to an embodiment of the present invention forms a third isolation structure embedded on the back side of the semiconductor substrate 10 in step S4. The third isolation structure is similar to the second isolation structure in that a trench is first formed on the back side and then filled with an isolation medium. For example, the formation of the third isolation structure may include the following steps:
[0077] First, the semiconductor substrate 10 is thinned from the back side;
[0078] Then, a patterned mask layer (not shown) is formed on the back side of the semiconductor substrate 10 by a third patterning process, and an opening in the mask layer is formed in a region where the front pixel separation structure 110 vertically extends toward the back side of the semiconductor substrate 10;
[0079] Then, if Figure 6NAs shown, the patterned mask layer is used as a mask to etch the semiconductor substrate 10 from the back to form a third trench 10d. The bottom surface of the third trench 10d exposes the front pixel separation structure 110. Since the second isolation structure is formed deeper on the front side, when the third trench 10b is formed to expose the front pixel separation structure 110, it is possible to avoid etching through the semiconductor substrate 10. The etching depth of the third trench 10d is, for example, greater than that of the first trench 10a, and can even be greater than that of the second trench 10b. However, the present invention is not limited thereto. In the embodiment, the etching depth of the third groove 10d is sufficient to expose the front pixel separation structure 110 from the back side of the substrate.
[0080] Then, an isolation dielectric is filled in the third trench 10d, and a planarization process is used to make the surface of the isolation dielectric in the third trench 10d away from the bottom surface of the third trench flush with the surface of the patterned mask layer;
[0081] Next, the patterned mask layer is removed, and the isolation medium in the third trench 10d is used as the third isolation structure, such as Fig.6O shown.
[0082] The isolation dielectric in the third trench 10d is formed by atomic layer deposition. Fig.6O As shown, the isolation medium in the third groove 10d may include a high-k dielectric layer 121 and an insulating layer 122 covering the high-k dielectric layer 121 and having a lower dielectric constant than the high-k dielectric layer. The high-k dielectric layer 121 is used to improve the isolation effect between pixel areas and avoid crosstalk. The third isolation structure corresponds to and is connected to the front pixel separation structure 110, and is also used to separate adjacent pixel areas. That is, for the substrate isolation area with the front pixel separation structure 110 between two adjacent pixel areas, it is isolated on the back side of the semiconductor substrate by the third isolation structure, and the front pixel separation structure 110 (the second isolation structure before the groove 10c is formed) embedded on the front side and the third isolation structure embedded on the back side of the same substrate isolation area are connected up and down to form complete physical isolation. The third isolation structure can be recorded as a back pixel separation structure 120, that is, the back pixel separation structure 120 corresponds to the front pixel separation structure 110 and is connected to each other. For the front pixel separation structure 110 and the back pixel separation structure 120 connected up and down, their central axes or side walls can be aligned up and down, but the alignment is not necessary, and the central axis or the outer side wall can also have a certain deviation.
[0083] The manufacturing method of the photoelectric sensor of the embodiment of the present invention forms a first isolation structure and a second isolation structure on the front side of the semiconductor substrate 10. The second isolation structure can be regarded as deep isolation on the front side. The embedding depth of the first isolation structure in the semiconductor substrate 10 is shallower than that of the second isolation structure, which is convenient for ensuring the working performance of the photosensitive area and the charge readout area. In addition, a third isolation structure is formed on the back side of the semiconductor substrate. The second isolation structure and the third isolation structure correspond to each other up and down and are connected to each other, so that there is an excellent isolation effect between adjacent pixel areas. Moreover, since the second isolation structure is embedded deeper than the first isolation structure, compared with the method of directly using the first isolation structure to separate the pixel area on the front side and connecting it with the third isolation structure, the embodiment of the present invention connects the third isolation structure to the second isolation structure. The manufacturing difficulty of the third isolation structure is low and it is not easy to etch through the substrate.
[0084] The embodiment of the present invention also relates to a photoelectric sensor, which can be obtained by using the above-mentioned manufacturing method. Fig.6O , the photoelectric sensor comprises:
[0085] A semiconductor substrate 10, wherein the semiconductor substrate 10 has a plurality of pixel regions, each of which is used to form a MOS capacitor and a read transistor that use a common floating gate to realize light sensing;
[0086] A first isolation structure (i.e., isolation medium 103) is embedded on the front side of the semiconductor substrate 10, wherein the first isolation structure separates each pixel region into a photosensitive region and a charge readout region, wherein the photosensitive region is used to construct the MOS capacitor, and the charge readout region is used to construct a read transistor;
[0087] A front pixel separation structure 110 is embedded on the front surface of the semiconductor substrate 10, and the front pixel separation structure 110 is located between adjacent pixel regions; and
[0088] A back pixel separation structure 120 (i.e., a third isolation structure) is embedded on the back side of the semiconductor substrate 10, wherein the back pixel separation structure 120 is located between adjacent pixel areas, and the front pixel separation structure 110 corresponds to the back pixel separation structure 120 up and down and is connected to each other, wherein the embedding depth of the front pixel separation structure 110 in the semiconductor substrate 10 is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate 10.
[0089] In this embodiment, the first isolation structure may adopt shallow trench isolation STI, and the front pixel separation structure 110 is embedded deeper than the first isolation structure, and may adopt deep trench isolation DTI. The etching depth of the back pixel separation structure 120 is set according to the need to connect with the front pixel separation structure 110, and thus may be deep trench isolation DTI or shallow trench isolation STI. The photoelectric sensor may also include a gate stack located on the front side of the semiconductor substrate 10, and the gate stack may refer to the description of the manufacturing method of the photoelectric sensor.
[0090] According to the description of the manufacturing method described in the embodiment of the present invention, the formed photoelectric sensor can ensure the working performance of the photosensitive area and the charge readout area while having excellent isolation effect between adjacent pixel areas and not easily etching through the substrate. Therefore, the crosstalk between adjacent pixels of the photoelectric sensor of the embodiment of the present invention is small, which facilitates the miniaturization of the pixel size and the spacing between pixels, and the device has better quality and reliability.
[0091] It should be noted that the embodiments in this specification are described in a progressive manner, and each part focuses on the differences from the previous part. The same and similar parts between the parts can be referenced to each other.
[0092] The above description is only a description of the preferred embodiment of the present invention, and is not any limitation on the scope of rights of the present invention. Any technical personnel in this field can make possible changes and modifications to the technical solution of the present invention by using the methods and technical contents disclosed above without departing from the spirit and scope of the present invention. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope of the technical solution of the present invention.
Claims
1. A method for manufacturing a photoelectric sensor, characterized in that: include: Providing a semiconductor substrate, the semiconductor substrate having a plurality of pixel regions, each of the pixel regions being used to form a MOS capacitor and a read transistor that use a common floating gate to realize light sensing; A first isolation structure is formed on the front surface of the semiconductor substrate, wherein the first isolation structure separates each pixel region into a photosensitive region and a charge readout region, wherein the photosensitive region is used to manufacture the MOS capacitor, and the charge readout region is used to manufacture a read transistor; forming an embedded second isolation structure on the front surface of the semiconductor substrate, wherein the second isolation structure is located between adjacent pixel regions; as well as, An embedded third isolation structure is formed on the back side of the semiconductor substrate, and the third isolation structure is located between adjacent pixel areas. The third isolation structure corresponds to the second isolation structure up and down and is connected to each other, wherein the embedding depth of the second isolation structure in the semiconductor substrate is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate.
2. The method according to claim 1, characterized in that: The step of forming the first isolation structure includes: forming a pad oxide layer and a first nitride layer in sequence on the front surface of the semiconductor substrate; Etching the first nitride layer, the pad oxide layer, and the semiconductor substrate to form a first trench penetrating the first nitride layer and the pad oxide layer and having a bottom surface located in the semiconductor substrate; Filling the first trench with an isolation dielectric, and using a planarization process to make the upper surface of the isolation dielectric in the first trench flush with the upper surface of the first nitride layer; and, The first nitride layer is removed, and the isolation medium in the first trench is used as the first isolation structure.
3. The method according to claim 2, characterized in that: The step of forming the second isolation structure comprises: forming a second nitride layer on the semiconductor substrate, wherein the second nitride layer covers the pad oxide layer and the first isolation structure, and an upper surface of the second nitride layer is higher than an upper surface of the first isolation structure as a whole; Etching the second nitride layer, the pad oxide layer, and the semiconductor substrate to form a second trench penetrating the second nitride layer and the pad oxide layer and having a bottom surface located in the semiconductor substrate, wherein the depth of the second trench in the semiconductor substrate is more than 1.5 times the depth of the first isolation structure in the semiconductor substrate; Filling the second trench with an isolation dielectric, and using a planarization process to make the upper surface of the isolation dielectric in the second trench flush with the upper surface of the second nitride layer; and, The second nitride layer is removed, and the isolation medium in the second trench is used as the second isolation structure, wherein the upper surface of the second isolation structure is above the first isolation structure.
4. The method according to claim 3, characterized in that: After forming the second isolation structure and before forming the third isolation structure, the manufacturing method further includes: removing the pad oxide layer, and forming a gate oxide material layer and a floating gate material layer on the semiconductor substrate, wherein the gate oxide material layer covers the upper surface of the semiconductor substrate, the floating gate material layer covers the gate oxide material layer and the first isolation structure and the second isolation structure, and the upper surface of the floating gate material layer is entirely located above the second isolation structure; Using a planarization process to remove a portion of the thickness of the floating gate material layer, so that the upper surface of the remaining floating gate material layer is flush with the upper surface of the second isolation structure, and the remaining floating gate material layer continuously covers the photosensitive area and the charge readout area of each pixel area, serving as a floating gate shared by the MOS capacitor and the read transistor; and An inter-gate dielectric material layer and a control gate material layer are sequentially formed on the semiconductor substrate.
5. The method according to claim 4, characterized in that: Before forming the inter-gate dielectric material layer, the manufacturing method further includes: The second isolation structure is etched back so that the upper surface of the second isolation structure is lower than the upper surface of the floating gate, thereby forming a groove between adjacent floating gates, the inter-gate dielectric material layer covers the inner surface of the groove, the control gate material layer covers the inter-gate dielectric material layer and fills the groove, and the second isolation structure after the back etching serves as a front pixel separation structure.
6. The method according to claim 3, characterized in that: The step of forming the third isolation structure comprises: Thinning the semiconductor substrate from the back side; forming a patterned mask layer on the back side of the semiconductor substrate, wherein an opening in the mask layer is formed in a region where the second isolation structure vertically extends toward the back side of the semiconductor substrate; Using the patterned mask layer, etching the semiconductor substrate from the back to form a third trench, wherein the bottom surface of the third trench exposes the second isolation structure; Filling the third trench with an isolation dielectric, and using a planarization process to make a surface of the isolation dielectric in the third trench away from the bottom surface of the third trench flush with a surface of the patterned mask layer; The patterned mask layer is removed, and the isolation medium in the third trench is used as the third isolation structure.
7. The method according to claim 6, characterized in that: The isolation dielectric in the second trench and / or the third trench is formed by an atomic layer deposition process.
8. The method according to claim 6, characterized in that: The isolation dielectric in the second trench and / or the third trench includes a high-k dielectric layer and an insulating layer covering the high-k dielectric layer and having a lower dielectric constant than the high-k dielectric layer.
9. The method according to claim 1, characterized in that: The semiconductor substrate has a plurality of substrate lead-out regions arranged between the plurality of pixel regions, each of the substrate lead-out regions being connected to the substrates of two or more of the pixel regions so as to apply a voltage to the substrates of the pixel regions through the substrate lead-out regions; the first isolation structure defines the range of the substrate lead-out regions.
10. The method according to claim 1, characterized in that: The embedding depth of the first isolation structure in the semiconductor substrate is The embedding depth of the second isolation structure in the semiconductor substrate is 11. A photoelectric sensor, characterized in that: The photoelectric sensor comprises: A semiconductor substrate having a plurality of pixel regions, each of which is used to form a MOS capacitor and a read transistor that use a common floating gate to realize light sensing; A first isolation structure is embedded on the front side of the semiconductor substrate, wherein the first isolation structure separates each pixel region into a photosensitive region and a charge readout region, wherein the photosensitive region is used to construct the MOS capacitor, and the charge readout region is used to construct a read transistor; A front pixel separation structure is embedded on the front side of the semiconductor substrate, wherein the front pixel separation structure is located between adjacent pixel regions; and A third isolation structure is embedded on the back side of the semiconductor substrate, the third isolation structure is located between adjacent pixel areas, and the third isolation structure corresponds to the front pixel separation structure in upper and lower directions and is interconnected, wherein the embedding depth of the front pixel separation structure in the semiconductor substrate is more than 1.5 times the embedding depth of the first isolation structure in the semiconductor substrate.
Citation Information
Patent Citations
Composite dielectric grating metal-oxide-semiconductor field effect transistor (MOSFET) based dual-transistor light-sensitive detector and signal reading method thereof
CN102938409A
Photoelectric conversion device having isolation portions, and imaging system and moving body
CN110137189A
Semiconductor structure and preparation method thereof
CN111029357A
Image sensor and method for manufacturing the same
EP3792973A2
Back side illumination image sensor and method for manufacturing the same
KR1020110079337A