A method for manufacturing a memory
By using a patterned sacrificial layer and a support layer in the memory to define the position of the bit line structure, the problem of morphological defects and over-etching of the bit line conductive layer during the etching process is solved, and the electrical performance of the memory is improved.
Patent Information
- Application Number
- CN202010895429.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-08-31
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-08-31
AI Technical Summary
During the etching process of the bit line structure of the memory, insufficiently vertical sidewalls and over-etching phenomena are prone to occur, causing damage to the bit line conductive layer and affecting conductivity and electrical performance.
Use a patterned sacrificial layer to form a pseudo bit line layer, fill the support layer to define the bit line space, stack the bit line conductive layer and insulating layer in sequence, and finally remove the support layer to form a complete bit line structure to avoid morphological defects and defects caused by etching. Over etching.
The conductive ability of the bit line conductive layer is improved, the electrical performance of the memory is improved, and the morphological defects and over-etching problems of the bit line conductive layer are avoided.
Smart Images

Figure CN114121813B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the semiconductor field, and in particular to a method for manufacturing a memory. Background Art
[0002] The memory is a memory component used to store programs and various data information. It can be divided into read-only memory and random access memory according to the type of use of the memory. The memory usually includes a capacitor and a transistor connected to the capacitor. The capacitor is used to store charges representing the stored information, and the transistor is a switch that controls the flow and release of charges in the capacitor. The bit line conductive layer is part of the bit line structure of the memory, and together with the bit line insulating layer, it serves as the bit line structure of the memory. The method for forming the bit line structure is to deposit the bit line conductive layer and the bit line insulating layer in sequence, and then etch the bit line conductive layer and the bit line insulating layer into separate bit line structures.
[0003] However, when etching the bit line structure, a deeper etching depth is required, and the sidewalls of the etched bit line structure are often not vertical enough, and the bit line conductive layer is over-etched, resulting in damage to the bit line conductive layer and affecting the conductivity of the bit line structure. Summary of the invention
[0004] The purpose of the embodiment of the present invention is to provide a memory manufacturing method, which is beneficial to improving the conductivity of the bit line structure.
[0005] To solve the above problems, an embodiment of the present invention provides a method for manufacturing a memory, including: providing a substrate, forming a sacrificial layer on the substrate; patterning the sacrificial layer, forming a plurality of mutually discrete pseudo bit line layers on the substrate; forming a supporting layer, the supporting layer filling the area between adjacent pseudo bit line layers; removing the pseudo bit line layer to form a bit line space located between adjacent supporting layers; forming a bit line structure, the bit line structure filling the bit line space, and the bit line structure includes a bit line conductive layer and a bit line insulating layer stacked in sequence; removing the supporting layer to form an opening located between adjacent bit line structures.
[0006] In addition, the process steps of forming the bit line structure include: forming a bit line conductive layer in the bit line space, and the top of the bit line conductive layer is lower than the top of the support layer; forming a bit line insulating layer on the top of the bit line conductive layer, and the bit line insulating layer exposes the top of the support layer.
[0007] In addition, the bit line conductive layer includes a bit line contact window and a bit line conductive column stacked in sequence; the process steps for forming the bit line conductive layer include: forming a first conductive layer that fills the bit line space; etching back to remove a portion of the thickness of the first conductive layer, and the remaining first conductive layer serves as the bit line contact window; forming a second conductive layer that fills the bit line space on the bit line contact window; etching back to remove a portion of the thickness of the second conductive layer, and the remaining second conductive layer serves as the bit line conductive column.
[0008] In addition, a wet etching process is used to etch back and remove a portion of the first conductive layer.
[0009] In addition, the process steps for forming the support layer include: forming an initial support layer between adjacent pseudo bit line layers, and the initial support layer is also located on the top of the pseudo bit line layer; flattening the initial support layer, removing the initial support layer above the top of the pseudo bit line layer, and forming the support layer; the bit line conductive layer includes a bit line contact window, and the material of the support layer is the same as the material of the bit line contact window, and the process temperature for forming the initial support layer is greater than the process temperature for forming the bit line contact window.
[0010] In addition, the material of the support layer and the bit line contact window is polysilicon, wherein the material forming the bit line contact window also has doped ions; the process temperature for forming the support layer is 580°C to 620°C, and the process temperature for forming the bit line contact window is 480°C to 520°C.
[0011] In addition, the material of the support layer is different from that of the bit line insulating layer.
[0012] In addition, before forming the supporting layer, the method further includes: forming a protective layer, which covers the sidewalls of the dummy bit line layer and is also located on the substrate between adjacent dummy bit line layers; after removing the supporting layer, the method further includes: removing the protective layer on the substrate between adjacent bit line structures.
[0013] In addition, the process steps of forming the protection layer include: forming a first silicon nitride layer on the substrate covering the sidewalls of the dummy bit line layer and between adjacent dummy bit line layers; forming a silicon oxide layer on the first silicon nitride layer; and forming a second silicon nitride layer on the silicon oxide layer.
[0014] In addition, the sacrificial layer has a single-layer structure.
[0015] Compared with the prior art, the technical solution provided by the embodiment of the present invention has the following advantages:
[0016] A method for manufacturing a memory provided by an embodiment of the present invention first uses a graphic sacrificial layer to form a pseudo bit line layer so as to define the position of the bit line structure; then fills the support layer in the area between the pseudo bit line layers to define the position of the area between the bit line structures; removes the pseudo bit line layer, forms a bit line space between the support layers, and sequentially fills the bit line conductive layer and the bit line insulating layer to form a bit line structure, and finally removes the support layer. The manufacturing method provided by an embodiment of the present invention avoids the problem of morphological defects of the bit line conductive layer that occurs when etching to form the bit line structure, and also avoids over-etching of the bit line conductive layer, improves the damage of the bit line conductive layer, thereby improving the conductivity of the bit line conductive layer and improving the electrical performance of the memory. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] One or more embodiments are exemplarily described by pictures in the corresponding drawings. Unless otherwise stated, the pictures in the drawings are not limited to scale.
[0018] Figure 1 to Figure 17 A schematic cross-sectional structure diagram corresponding to each step of the method for manufacturing a memory provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0019] As can be seen from the background technology, the performance of the memory of the prior art needs to be improved. The memory bit line structure includes a bit line conductive layer and a bit line insulating layer. When forming the bit line structure, a deeper etching depth is often required. Since the etchant has a different selectivity ratio for different structures, a groove is formed in the side wall profile of the bit line structure. After the bit line contact window is formed by etching, further etching is required to remove the bit line contact material remaining between the bit line contact windows to avoid short circuits between multiple adjacent bit line structures. This process also leads to over-etching of the side walls of the bit line contact windows. As the etching proceeds, lateral etching will gradually occur, and the etching will cause morphological defects in the bit line conductive layer. At the same time, the bit line conductive layer will be over-etched, and the bit line conductive layer will be damaged, affecting the electrical performance of the memory.
[0020] In order to solve the above problem, the present invention provides a method for manufacturing a memory, firstly, a pseudo bit line layer is formed by using a graphic sacrificial layer so as to define the position of the bit line structure; then, a support layer is filled in the area between the pseudo bit line layers to define the position of the area between the bit line structures; the pseudo bit line layer is removed, a bit line space is formed between the support layers, and the bit line structure is filled in sequence, and finally the support layer is removed. The manufacturing method provided by the embodiment of the present invention avoids the problem of morphological defects of the bit line conductive layer that occurs when etching to form the bit line structure, and also avoids the situation that the bit line conductive layer will be over-etched, improves the damage of the bit line conductive layer, thereby improving the conductivity of the bit line conductive layer and improving the electrical performance of the memory.
[0021] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the embodiments of the present invention will be described in detail below with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present invention, many technical details are provided to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can be implemented.
[0022] An embodiment of the present invention provides a method for manufacturing a memory. The method for manufacturing the memory provided by the embodiment will be described in detail below with reference to the accompanying drawings. Figure 1-Figure 17 A schematic cross-sectional structure diagram corresponding to each step of the method for manufacturing a memory provided by an embodiment of the present invention.
[0023] refer to Figure 1 , providing a substrate 100 , and forming a sacrificial layer 111 on the substrate 100 .
[0024] Specifically, the substrate 100 has active areas 110 (AA, Active Area), and isolation areas 120 are disposed between the active areas 110 . The isolation areas 120 are used to isolate adjacent active areas 110 .
[0025] In this embodiment, the sacrificial layer 111 is a single-layer structure. In other embodiments, the sacrificial layer may also be a stacked-layer structure.
[0026] The material of the sacrificial layer 111 is silicon dioxide. When etching the same material, the anisotropy in all directions is substantially the same, so over-etching can be effectively avoided. In other embodiments, the material of the sacrificial layer may also be other materials.
[0027] Specifically, the sacrificial layer 111 is formed by chemical vapor deposition at a temperature of 600° C. to 630° C., such as 605° C., 610° C., 615° C., 620° C. or 625° C. In other embodiments, the deposition process may also be physical vapor deposition or atomic layer deposition.
[0028] refer to Figure 2 , patterned sacrificial layer 111 (reference Figure 1 ), a plurality of mutually discrete pseudo bit line layers 101 are formed on the substrate 100.
[0029] The dummy bit line layer 101 defines the position of the bit line structure so as to form the bit line structure later. The dummy bit line layer 101 is located above the active region 110 and in the gap between the isolation regions 120 . The sidewall profile of the dummy bit line layer 101 is smooth and perpendicular to the substrate 100 .
[0030] The process steps after forming the dummy bit line layer 101 include: forming a supporting layer 102 , wherein the supporting layer 102 fills the area between adjacent dummy bit line layers 101 .
[0031] In this embodiment, before forming the support layer 102, the method further includes: Figure 3 , forming a protection layer 105 , the protection layer 105 covers the sidewalls of the dummy bit line layers 101 and is also located on the substrate 100 between adjacent dummy bit line layers 101 .
[0032] The protection layer 105 can protect the bit line conductive layer in the bit line structure formed in the subsequent process steps, and further improve the insulation between the bit line conductive layer and the capacitor contact window formed subsequently during the memory manufacturing process.
[0033] In this embodiment, the process steps for forming the protection layer 105 include: forming a first silicon nitride layer 115 on the substrate 100 covering the side walls of the dummy bit line layer 101 and between adjacent dummy bit line layers 101; forming a silicon oxide layer 135 on the first silicon nitride layer 115; and forming a second silicon nitride layer 125 on the silicon oxide layer 135.
[0034] The process method for forming the first silicon nitride layer 115 and the second silicon nitride layer 125 may be atomic layer deposition, and the reaction gas may be silane, ammonia, etc. The process method for forming the silicon oxide layer 135 may be atomic layer deposition, and the reaction gas may be dipropylaminosilane. In other embodiments, the protective layer may be formed by chemical vapor deposition or physical vapor deposition, and the reaction gas may also be other gases.
[0035] In other embodiments, the protective layer may also be a single-layer structure or a double-layer structure.
[0036] It is understandable that in other embodiments, the protection layer may be formed after the bit line structure is subsequently formed.
[0037] refer to Figure 4 , an initial support layer 112 is formed between adjacent dummy bit line layers 101 , and the initial support layer 112 is also located on top of the dummy bit line layer 101 .
[0038] Specifically, in this embodiment, an initial support layer 112 is formed on the surface of the protection layer 105 .
[0039] refer to Figure 5 , for the initial support layer 112 (reference Figure 4 ) is planarized to remove the initial support layer 112 that is higher than the top of the dummy bit line layer 101, thereby forming a support layer 102.
[0040] It is understandable that the process of removing the initial support layer 112 above the top of the dummy bit line layer 101 can be dry etching, and the etching gas can be selected from sulfur hexafluoride, carbon tetrafluoride, trifluoromethane, oxygen and argon, etc., or a mixture thereof. In other embodiments, other processes can also be used to remove the initial support layer above the top of the dummy bit line layer.
[0041] The material of the support layer 102 is polysilicon, and the process of forming the support layer 102 is a chemical vapor deposition process. The reaction gas may be silane, and the process temperature is 580° C. to 620° C., such as 585° C., 596° C., 600° C. or 610° C.
[0042] refer to Figure 6 , remove the protection layer 105 on the top of the dummy bit line layer 101.
[0043] Because the protection layer 105 is formed before the support layer 102 is formed, and the protection layer 105 covers the side walls and the top of the dummy bit line layer 101, before removing the dummy bit line layer 101, the protection layer 105 on the top of the dummy bit line layer 101 also needs to be removed to expose the dummy bit line layer 101 so as to facilitate the subsequent removal of the dummy bit line layer 101.
[0044] The process for removing the protective layer 105 may be dry etching, and the etching gas may be a mixed gas of sulfur hexafluoride, carbon tetrafluoride, trifluoromethane, oxygen, argon, etc.
[0045] refer to Figure 7 , remove the dummy bit line layer 101 to form a bit line space 106 located between adjacent support layers 102 .
[0046] In this embodiment, the sidewall of the bit line space 106 is a protection layer 105 .
[0047] The process of removing the dummy bit line layer 101 may be wet etching, and the etching liquid of the wet etching is a hydrofluoric acid solution.
[0048] The process steps after removing the dummy bit line layer 101 include: forming a bit line structure, the bit line structure fills the bit line space 106, and the bit line structure includes a bit line conductive layer 103 and a bit line insulating layer 104 stacked in sequence.
[0049] The process steps of forming the bit line structure include: forming a bit line conductive layer 103 in the bit line space 106, and the top of the bit line conductive layer 103 is lower than the top of the support layer 102; forming a bit line insulating layer 104 on the top of the bit line conductive layer 103, and the bit line insulating layer 104 exposes the top of the support layer 102. The steps of forming the bit line structure will be described in detail below with reference to the accompanying drawings.
[0050] refer to Figure 8 , forming a first conductive layer 113 filling the full bit line space 106; Fig. 9 , a portion of the first conductive layer 113 is removed by etching back, and the remaining first conductive layer 113 serves as a bit line contact window 133 .
[0051] In this embodiment, the bit line conductive layer 103 includes a bit line contact window 133 , and the material of the support layer 102 is the same as that of the bit line contact window 133 . The process temperature for forming the initial support layer 112 is higher than the process temperature for forming the bit line contact window 133 .
[0052] In this embodiment, the material of the bit line contact window 133 is polysilicon, wherein the material forming the bit line contact window 133 also has doping ions. The bit line contact window 133 is used to achieve electrical connection between the bit line structure and the active area 110 .
[0053] The process for forming the bit line contact window 133 is a chemical vapor deposition process, the reaction gases are silane and phosphine, and the process temperature is 480° C. to 520° C., such as 485° C., 490° C., 500° C. or 510° C. It can be understood that since the process temperature for forming the above-mentioned support layer 102 is greater than the process temperature for forming the bit line contact window 133, the etching rate of the support layer 102 is much lower than the etching rate of the first conductive layer 113. Therefore, when the first conductive layer 113 is wet-etched using a nitric acid solution of the same concentration, the support layer 102 is almost not affected.
[0054] refer to Fig.10 as well as Fig.11 , a second conductive layer 123 is formed on the bit line contact window 133 to fill the bit line space 106 .
[0055] In addition, a diffusion barrier layer 153 may be formed between the bit line contact window 133 and the bit line conductive pillar 143 . The material of the diffusion barrier layer 153 may be tantalum nitride or titanium nitride.
[0056] refer to Fig.12 , a portion of the second conductive layer 123 is removed by etching back, and the remaining second conductive layer 123 serves as the bit line conductive pillar 143 .
[0057] The material of the bit line conductive pillar 143 includes metal conductive materials such as tungsten, gold or silver.
[0058] refer to Fig.13 , the diffusion barrier layer 153 is etched back.
[0059] It is understandable that before filling the bit line insulating layer 104 , the diffusion barrier layer 153 needs to be etched back.
[0060] In this embodiment, a wet etching process is used to etch back and remove a portion of the first conductive layer 113. According to actual needs, other etching processes can also be used to remove a portion of the first conductive layer 113 to form a bit line contact window 133. The thickness of the first conductive layer 113 removed is determined according to the bit line conductive layer in the bit line structure of the memory.
[0061] In this embodiment, the bit line conductive layer 103 includes a bit line contact window 133 and a bit line conductive pillar 143 which are stacked in sequence.
[0062] refer to Fig.14 and Fig.15 A bit line insulating layer 104 is formed on the top of the bit line conductive layer 103 , and the bit line insulating layer 104 exposes the top of the supporting layer 102 .
[0063] The process steps for forming the bit line insulating layer 104 include: Fig.14, forming a bit line insulating layer 104 on top of the bit line conductive layer 103; referring to Fig.15 , the bit line insulating layer 104 is etched back to expose the top of the support layer 102. The main function of the bit line insulating layer 104 is to insulate the surface of the bit line structure.
[0064] The formed bit line structure includes a bit line conductive layer and a bit line insulating layer stacked in sequence, and the formed bit line conductive layer avoids the morphological defects of the bit line conductive layer formed by etching the bit line structure in the prior art and the over-etching of the bit line conductive layer.
[0065] In addition, the material of the support layer 102 is different from that of the bit line insulating layer 104 .
[0066] In this embodiment, the material of the bit line insulating layer 104 includes silicon nitride. In other embodiments, the material of the bit line insulating layer may also be silicon oxide, silicon oxynitride, or silicon carbon nitride oxide.
[0067] refer to Fig.16 , removing the support layer 102 to form an opening between adjacent bit line structures.
[0068] The process of removing the support layer 102 may be dry etching, and the etching gas may be sulfur hexafluoride, carbon tetrafluoride, chlorine, argon, etc., or a mixture thereof. During the removal of the support layer 102, the protection layer 105 may effectively prevent the bit line conductive layer 103 in the bit line structure from being etched.
[0069] In other embodiments, the process of removing the support layer may also use other processes.
[0070] refer to Fig.17 After removing the support layer 102 , the method further includes: removing the protection layer 105 on the substrate 100 between adjacent bit line structures.
[0071] The protection layer 105 covers the sidewalls of the bit line structure and is also located on the substrate 100 between adjacent bit line structures. Therefore, after removing the support layer 102, the protection layer 105 on the substrate 100 between adjacent bit line structures needs to be removed to expose the substrate 100 and form a discrete bit line structure on the substrate 100.
[0072] The memory manufacturing method provided in this embodiment first forms a pseudo bit line layer without etching defects, defines the position of the bit line structure, and then defines the position of the area between the bit line structures through the support layer, forms a bit line space between the support layers, and sequentially fills the bit line conductive layer and the bit line insulating layer to form the bit line structure, and finally removes the support layer to form a bit line structure without etching defects. The memory manufacturing method provided in this embodiment avoids the problem of morphological defects of the bit line conductive layer when etching to form the bit line structure, and also avoids over-etching of the bit line conductive layer, improves the damage of the bit line conductive layer, improves the conductivity of the bit line conductive layer, and further improves the electrical performance of the memory.
[0073] Those skilled in the art will appreciate that the above embodiments are specific examples of the present invention, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present invention. Any person skilled in the art may make changes and modifications without departing from the spirit and scope of the present invention, and therefore the scope of protection of the present invention shall be subject to the scope defined in the claims.
Claims
1. A method for manufacturing a memory, characterized in that: include: providing a substrate, and forming a sacrificial layer on the substrate; Patterning the sacrificial layer to form a plurality of mutually discrete pseudo bit line layers on the substrate; An initial support layer is formed between adjacent dummy bit line layers, wherein the initial support layer is also located on the top of the dummy bit line layer; the initial support layer is planarized to remove the initial support layer above the top of the dummy bit line layer to form a support layer; the support layer fills the area between adjacent dummy bit line layers; removing the dummy bit line layer to form a bit line space between adjacent support layers; forming a bit line structure, wherein the bit line structure fills the bit line space, and the bit line structure comprises a bit line conductive layer and a bit line insulating layer stacked in sequence; The bit line conductive layer includes a bit line contact window, and the material of the support layer is the same as that of the bit line contact window, and the process temperature for forming the initial support layer is greater than the process temperature for forming the bit line contact window; The supporting layer is removed to form an opening between adjacent bit line structures.
2. The method for manufacturing a memory according to claim 1, characterized in that: The process steps for forming the bit line structure include: forming the bit line conductive layer in the bit line space, and the top of the bit line conductive layer is lower than the top of the supporting layer; forming the bit line insulating layer on the top of the bit line conductive layer, and the bit line insulating layer exposes the top of the supporting layer.
3. The method for manufacturing a memory according to claim 2, characterized in that: The bit line conductive layer includes a bit line contact window and a bit line conductive column stacked in sequence; The process steps for forming the bit line conductive layer include: forming a first conductive layer that fills the bit line space; etching back to remove a portion of the thickness of the first conductive layer, with the remaining first conductive layer serving as the bit line contact window; forming a second conductive layer that fills the bit line space on the bit line contact window; etching back to remove a portion of the thickness of the second conductive layer, with the remaining second conductive layer serving as the bit line conductive column.
4. The method for manufacturing a memory according to claim 3, characterized in that: A wet etching process is adopted to etch back and remove a portion of the thickness of the first conductive layer.
5. The method for manufacturing a memory according to claim 1, characterized in that: The material of the support layer and the bit line contact window is polysilicon, wherein the material forming the bit line contact window also has doped ions; the process temperature for forming the support layer is 580°C to 620°C, and the process temperature for forming the bit line contact window is 480°C to 520°C.
6. The method for manufacturing a memory according to claim 1, characterized in that: A material of the support layer is different from a material of the bit line insulating layer.
7. The method for manufacturing a memory according to claim 1, characterized in that: Before forming the supporting layer, the method further includes: forming a protective layer, the protective layer covers the sidewalls of the pseudo bit line layer and is also located on the substrate between adjacent pseudo bit line layers; after removing the supporting layer, the method further includes: removing the protective layer on the substrate between adjacent bit line structures.
8. The method for manufacturing a memory according to claim 7, characterized in that: The process steps for forming the protection layer include: forming a first silicon nitride layer on the substrate covering the sidewalls of the dummy bit line layer and between adjacent dummy bit line layers; forming a silicon oxide layer on the first silicon nitride layer; and forming a second silicon nitride layer on the silicon oxide layer.
9. The method for manufacturing a memory according to claim 1, characterized in that: The sacrificial layer is a single-layer structure.
Citation Information
Patent Citations
Manufacturing method of semiconductor memory device
CN109244090A
Method of manufacturing semiconductor devices
CN109801918A
Dynamic random access memory and manufacturing method thereof
CN110223982A
Bitline of semiconductor device having stud type capping layer and method for fabricating the same
US20040056247A1
Early Bit Line Air Gap Formation
US20160111326A1