Method for forming semiconductor structure
By forming a second dielectric layer and an isolation structure in the semiconductor structure, and etching to form a third opening between the gate structures, the problem of uneven depth of the conductive layer in the existing technology is solved, and the performance and process of the semiconductor structure are improved. Simplify efficiency.
Patent Information
- Application Number
- CN202010962083.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-14
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-09-14
AI Technical Summary
The manufacturing process of existing semiconductor structures is complex and the performance needs to be improved. Especially in the formation process of local interconnection structures, the depth of the conductive layer is uneven and the resistance is large, which affects device performance.
By forming a second dielectric layer in the second opening and forming an isolation structure in the first opening, etching the first dielectric layer and the second dielectric layer on the source and drain doped regions, a third dielectric layer is formed between the gate structures. The opening uses different etching rates of the second dielectric layer and the isolation structure to simplify the process and improve the uniformity of the conductive layer.
The simplification of the etching process and the uniformity of the conductive layer in the semiconductor structure are achieved, the performance of the semiconductor structure is improved, the process flow is simplified and the production efficiency is improved.
Smart Images

Figure CN114188271B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a method for forming a semiconductor structure. Background Art
[0002] The metal interconnection structure is an indispensable structure in semiconductor devices, which is used to realize the interconnection between active areas, between transistors, or between metal lines of different layers, and complete the transmission and control of signals. Therefore, in the semiconductor manufacturing process, the formation of the metal interconnection structure has a great influence on the performance of semiconductor devices and the semiconductor manufacturing cost. In order to increase the density of devices, the size of semiconductor devices in integrated circuits has been continuously reduced. In order to realize the electrical connection of each semiconductor device, a multi-layer interconnection structure is usually required.
[0003] Generally, in the back-end interconnection process of the semiconductor device manufacturing process, the first metal layer (M1) needs to form an electrical connection with the active device structure (including the source and drain regions and the gate structure region) of the lower layer. Therefore, before forming the first metal layer, it is usually necessary to pre-form a local interconnection structure (Local Interconnect) of the semiconductor device. The local interconnection structure includes: a zeroth metal layer (M0) electrically connected to the source and drain regions of the lower layer, and a zeroth gate metal layer (M0G) electrically connected to the gate structure.
[0004] However, the manufacturing process of the semiconductor structure with the local interconnection structure in the prior art is complicated, and the performance of the formed semiconductor structure needs to be further improved. Summary of the invention
[0005] The technical problem solved by the present invention is to provide a method for forming a semiconductor structure to improve the performance of the semiconductor structure.
[0006] In order to solve the above technical problems, the technical solution of the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate, the substrate comprising an isolation region; forming a plurality of gate structures, source-drain doped regions and a first dielectric layer arranged in parallel, the gate structure being located on the substrate, the plurality of gate structures spanning the isolation region, the source-drain doped regions being located in the substrate on both sides of the gate structure, and the first dielectric layer being located on the sidewalls of the gate structure; removing the gate structure and the first dielectric layer on the isolation region, forming a first opening in the gate structure, the first opening penetrating the gate structure along a direction perpendicular to the extension direction of the gate structure, forming a second opening in the first dielectric layer, the second opening exposing the surface of the source-drain doped regions, and the first opening and the second opening being connected; forming a second dielectric layer in the second opening; forming an isolation structure in the first opening; etching the first dielectric layer and the second dielectric layer on the source-drain doped regions, forming a third opening between the gate structures, the etching rate of the second dielectric layer having a first difference with the etching rate of the first dielectric layer, and the etching rate of the first dielectric layer having a second difference with the etching rate of the isolation structure, and the second difference being greater than the first difference.
[0007] Optionally, a material of the second dielectric layer is different from a material of the isolation structure.
[0008] Optionally, the method for forming the second dielectric layer includes: forming a sacrificial structure in the first opening, the sacrificial structure exposing the second opening; forming a dielectric material layer in the second opening and on the sacrificial structure; planarizing the dielectric material layer until the sacrificial structure is exposed, and forming the second dielectric layer in the second opening.
[0009] Optionally, the sacrificial structure includes a single-layer structure or a multi-layer structure; the material of the single-layer structure includes an amorphous material, and the amorphous material includes amorphous carbon; the multi-layer structure includes an amorphous material layer and an anti-reflection layer located on the amorphous material layer.
[0010] Optionally, the method for forming the sacrificial structure includes: forming a sacrificial structure material layer in the first opening, in the second opening and on the first dielectric layer; forming a patterned photoresist layer on the sacrificial structure material layer, the patterned photoresist layer exposing the sacrificial structure material layer on the second opening; etching the sacrificial structure material layer using the patterned photoresist layer as a mask until the bottom of the second opening is exposed to form the sacrificial structure.
[0011] Optionally, the method for forming the isolation structure includes: forming an isolation material layer in the first opening, on the first dielectric layer and on the second dielectric layer; and planarizing the isolation material layer and the second dielectric layer until the surface of the first dielectric layer is exposed to form the isolation structure.
[0012] Optionally, the material of the isolation structure includes silicon nitride or silicon nitride oxide.
[0013] Optionally, the material of the first dielectric layer includes silicon oxide; and the material of the second dielectric layer includes silicon oxide.
[0014] Optionally, the material of the second dielectric layer is the same as that of the isolation structure.
[0015] Optionally, the method for forming the second dielectric layer and the isolation structure includes: forming an isolation material layer in the first opening, in the second opening and on the first dielectric layer; planarizing the isolation material layer until the first dielectric layer is exposed, forming the second dielectric layer in the second opening, and forming the isolation structure in the first opening.
[0016] Optionally, the method for removing the gate structure and the first dielectric layer on the isolation region includes: forming a first mask layer on the substrate, the first mask layer exposing the surface of the gate structure and the surface of the first dielectric layer on the isolation region; using the first mask layer as a mask to remove the gate structure and the first dielectric layer.
[0017] Optionally, the process of removing the gate structure and the first dielectric layer includes a dry etching process and a wet etching process, or a combination of both.
[0018] Optionally, the substrate further includes an active region, and the isolation region is located between adjacent active regions; and the gate structure spans the active region and the isolation region.
[0019] Optionally, before forming the first dielectric layer, the method further includes: forming a stop layer on the source and drain doped regions, wherein the first dielectric layer is located on the stop layer; and the second opening exposes the stop layer on the surface of the source and drain doped regions.
[0020] Optionally, after etching the first dielectric layer and the second dielectric layer on the source and drain doped regions, the process further includes: removing a stop layer on the surface of the source and drain doped regions until the surface of the source and drain doped regions is exposed; after removing the stop layer, forming a conductive layer in the third opening, wherein the conductive layer is electrically connected to the source and drain doped regions.
[0021] Optionally, during etching of the first dielectric layer and the second dielectric layer, the etching rate of the first dielectric layer by the etching process is greater than the etching rate of the stop layer, and the etching rate of the second dielectric layer by the etching process is greater than the etching rate of the stop layer.
[0022] Optionally, the process of removing the stop layer includes a dry etching process or a wet etching process.
[0023] Optionally, the material of the stop layer includes silicon nitride or silicon oxynitride.
[0024] Optionally, the method for forming the third opening includes: forming a patterned layer on the isolation structure, the first dielectric layer and the second dielectric layer, the patterned layer exposing the first dielectric layer and the second dielectric layer on the source and drain doped regions; etching the first dielectric layer and the second dielectric layer using the patterned layer as a mask until the surface of the source and drain doped regions is exposed, thereby forming a third opening between the gate structures.
[0025] Optionally, the process of etching the first dielectric layer and the second dielectric layer includes a dry etching process.
[0026] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0027] The method for forming a semiconductor structure in the technical solution of the present invention forms a second dielectric layer in a second opening, forms an isolation structure in a first opening, and then etches the first dielectric layer and the second dielectric layer on the source and drain doped regions to form a third opening between gate structures. Since there is a first difference between the etching rate of the second dielectric layer and the etching rate of the first dielectric layer, and there is a second difference between the etching rate of the first dielectric layer and the etching rate of the isolation structure, the second difference is greater than the first difference, so that the process of etching the first dielectric layer and the second dielectric layer is simple, and the conductive layer structure subsequently formed in the third opening is uniform, which is beneficial to improving the performance of the semiconductor structure.
[0028] Furthermore, the material of the isolation structure is different from the material of the second dielectric layer, and the second dielectric layer and the isolation structure can be formed at different times. On the one hand, the material of the second dielectric layer can be selected from easily etched materials, so that the process for etching the first dielectric layer and the second dielectric layer is simple, which is beneficial to improving the performance of the semiconductor structure; on the other hand, the isolation structure can be selected from materials with dense structure and good isolation effect, so that the isolation structure has a better isolation effect on the gate structure.
[0029] Furthermore, the material of the isolation structure is the same as that of the second dielectric layer, so that the isolation structure and the second dielectric layer can be formed in one process, thereby simplifying the process flow and improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figures 1 to 4 is a schematic cross-sectional structure diagram of a semiconductor structure forming process in one embodiment;
[0031] Figures 5 to 16 It is a schematic cross-sectional structure diagram of a semiconductor structure forming process in an embodiment of the present invention. DETAILED DESCRIPTION
[0032] As described in the background art, the performance of the semiconductor structure with a local interconnect structure in the prior art needs to be improved. Now, an analysis and description will be given in conjunction with specific embodiments.
[0033] Figures 1 to 4 It is a schematic cross-sectional structure diagram of a semiconductor structure forming process in one embodiment.
[0034] Please refer to Figure 1 and Figure 2 , Figure 1 for Figure 2 A top view of Figure 2 for Figure 1 A schematic diagram of a cross-sectional structure in the AA' direction, providing a substrate 100; forming a plurality of parallel gate structures 101 on the substrate 100, wherein the sidewalls of the gate structure 101 have sidewalls (not shown), and forming source-drain doped regions 102 in the substrate on both sides of the gate structure 101; forming a stop layer 105 on the surface of the source-drain doped regions 102; forming a dielectric layer 103 on the substrate 100, wherein the dielectric layer 103 is located on the sidewalls of the gate structure 101; removing a portion of the gate structure 103, and forming a first opening (not shown) in the dielectric layer 103, wherein the first opening exposes a portion of the dielectric layer 103 on the source-drain doped regions 102, and the first opening penetrates the gate structure 101 in a direction perpendicular to the extension direction of the gate structure 101; and forming an isolation structure 104 in the first opening.
[0035] Please refer to Figure 3 and Figure 4 , Figure 3 for Figure 4 A top view of Figure 4 for Figure 3 In the cross-sectional structural diagram along the BB′ direction, the dielectric layer 103 and the stop layer 105 on the source-drain doped region 102 are removed to form a second opening 106 between the gate structures 101 , wherein the second opening 106 exposes the surface of the source-drain doped region 102 .
[0036] During the formation of the semiconductor structure, when removing part of the gate structure 101, it is necessary to form a mask layer that exposes part of the gate structure 101. Since the width of the gate structure 101 is relatively small, affected by the exposure accuracy and the overlay accuracy, the formed mask pattern also exposes part of the dielectric layer 103 and the side wall on the source and drain doping area 102. Therefore, when removing the exposed gate structure 101, the removal process also causes certain losses to the exposed dielectric layer 103 and the side wall, so that the isolation structure 104 formed in the first opening is also located on the dielectric layer 103 on the part of the source and drain doping area 102.
[0037] In order to obtain better isolation capability between the gate structures 101, the material of the isolation structure 104 is usually selected from materials with good isolation effect such as dense structure or hard material, and not prone to tunneling and conduction, such as silicon nitride or silicon oxynitride. On the other hand, when forming the second opening 106, it is necessary to first remove the dielectric layer 103 on the surface of the source and drain doping region 102 until the stop layer 105 is exposed, and then remove the stop layer 105 until the surface of the source and drain doping region 102 is exposed. The stop layer 105 is used as an etching stop layer of the dielectric layer 103 and a protective layer of the source and drain doping region 102 to reduce the damage of the source and drain doping region 102 by the etching process. Therefore, the material selected for the stop layer 105 is also a material with a dense structure and a large size compared to silicon oxide etching.
[0038] However, the materials of the stop layer 105 and the isolation structure 104 are difficult to etch due to their dense structure, so the etching rate of the isolation structure 104 in the process of removing the dielectric layer 103 is slow. Therefore, the depth of the second opening 106 formed in the isolation structure 104 is shallow. When a conductive layer electrically connected to the source and drain doped regions 102 is subsequently formed in the second opening 106, the depth of the conductive layer is uneven, which makes the resistance of the conductive layer located on the isolation structure 104 larger, thereby affecting the performance of the semiconductor structure.
[0039] In order to solve the above problems, the technical solution of the present invention provides a method for forming a semiconductor structure, by forming a second dielectric layer in a second opening, forming an isolation structure in a first opening, and then etching the first dielectric layer and the second dielectric layer on the source and drain doped regions to form a third opening between gate structures, wherein the difference between the etching rate of the second dielectric layer and the etching rate of the first dielectric layer is within a preset range, so that the process of etching the first dielectric layer and the second dielectric layer is simple, and the conductive layer structure subsequently formed in the third opening is uniform, which is beneficial to improving the performance of the semiconductor structure.
[0040] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0041] Figures 5 to 16 It is a schematic cross-sectional structure diagram of a semiconductor structure forming process in an embodiment of the present invention.
[0042] Please refer to Figure 5 and Figure 6 , Figure 5 for Figure 6 A top view of Figure 6 for Figure 5 A schematic cross-sectional structure diagram along the section line CC′ direction is provided, wherein a substrate 200 is provided, wherein the substrate 200 comprises an isolation region I, wherein the isolation region I is used to form an isolation structure in a device on the isolation region I subsequently.
[0043] In this embodiment, the substrate 200 further includes an active region II, and the isolation region I is located between adjacent active regions II.
[0044] In this embodiment, the material of the substrate 200 is silicon.
[0045] In other embodiments, the substrate material includes silicon carbide, silicon germanium, a multinary semiconductor material composed of group III-V elements, silicon on insulator (SOI) or germanium on insulator (GOI). Among them, the multinary semiconductor material composed of group III-V elements includes InP, GaAs, GaP, InAs, InSb, InGaAs or InGaAsP.
[0046] Please continue to refer to Figure 5 and Figure 6 , forming a plurality of parallel arranged gate structures 201, source-drain doped regions 203 and a first dielectric layer 205, wherein the gate structure 201 is located on the substrate 200, and the plurality of gate structures 201 span the isolation region I and the active region II, the source-drain doped regions 203 are located in the substrate 200 on both sides of the gate structure 201, and the first dielectric layer 205 is located on the sidewalls of the gate structure 201.
[0047] In this embodiment, the sidewall of the gate structure 201 further has a spacer structure 202 .
[0048] In this embodiment, before forming the first dielectric layer 205 , the method further includes: forming a stop layer 204 on the source-drain doped region 203 , and the first dielectric layer 205 is located on the stop layer 204 .
[0049] The stop layer 204 is used as an etching stop layer for subsequently etching the first dielectric layer 205 on the source-drain doped region 203 , so as to avoid damaging the source-drain doped region 203 when etching directly to the source-drain doped region 203 .
[0050] In this embodiment, the material of the stop layer 204 includes silicon nitride or silicon oxynitride.
[0051] The method for forming the gate structure 201, the sidewall structure 202, the source-drain doped region 203, the stop layer 204 and the first dielectric layer 205 includes: forming a dummy gate structure (not shown) on the substrate 200, wherein the dummy gate structure is arranged in parallel on the substrate; forming the sidewall structure 202 on the sidewall of the dummy gate structure; forming the source-drain doped region 203 in the substrate 200 on both sides of the dummy gate structure; forming the stop layer 204 on the source-drain doped region 203; after forming the stop layer 204, forming the first dielectric layer 205 on the substrate 200, wherein the first dielectric layer 205 is located on the sidewall of the sidewall structure 202; removing the dummy gate structure, forming a gate opening (not shown) in the first dielectric layer 205; and forming the gate structure 201 in the gate opening.
[0052] The gate structure 201 includes a gate dielectric layer (not shown) and a gate layer (not shown) located on the gate dielectric layer. In this embodiment, the gate structure 201 also includes a work function layer (not shown), which is located between the gate dielectric layer and the gate layer.
[0053] The material of the gate dielectric layer includes a high dielectric constant material, the dielectric constant of the high dielectric constant material is greater than 3.9, and the high dielectric constant material includes aluminum oxide or hafnium oxide; the material of the gate layer includes a metal, and the metal includes tungsten; the material of the work function layer includes an N-type work function material or a P-type work function material, the N-type work function material includes titanium aluminum, and the P-type work function material includes titanium nitride or tantalum nitride.
[0054] The material of the spacer structure 202 includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon oxynitride, silicon carbide, silicon carbonitride, and silicon carbonitride. In this embodiment, the material of the spacer structure 202 includes silicon nitride.
[0055] The source-drain doping region 203 has doping ions therein, and the doping ions are of N-type or P-type. The N-type ions include phosphorus ions, arsenic ions or antimony ions. The P-type ions include boron ions, boron fluoride ions or indium ions.
[0056] The material of the first dielectric layer 205 includes a dielectric material, and the dielectric material includes one or more combinations of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. The material of the first dielectric layer 205 includes silicon oxide.
[0057] Please refer to Figure 7 and Figure 8 , Figure 7 for Figure 8 A top view of Figure 8 for Figure 7Schematic diagram of the cross-sectional structure along the section line DD' direction, the gate structure 201 and the first dielectric layer 205 on the isolation region I are removed, and a first opening 206 is formed in the gate structure 201, the first opening 206 penetrates the gate structure 201 along a direction perpendicular to the extension direction of the gate structure 201, and a second opening 207 is formed in the first dielectric layer 205, the second opening 207 exposes the surface of the source-drain doped region 203, and the first opening 206 and the second opening 207 are connected.
[0058] In this embodiment, the second opening 207 exposes the stop layer 204 on the surface of the source / drain doped region 203 .
[0059] The method for removing the gate structure 201 and the first dielectric layer 205 on the isolation region I includes: forming a first mask layer (not shown) on the gate structure 201 and the first dielectric layer 205, wherein the first mask layer exposes the surface of the gate structure 201 and the surface of the first dielectric layer 205 on the isolation region I; and removing the gate structure 201 and the first dielectric layer 205 using the first mask layer as a mask.
[0060] The process of removing the gate structure 201 and the first dielectric layer 205 includes a dry etching process and a wet etching process or a combination of the two.
[0061] In this embodiment, the process of removing the gate structure 201 and the first dielectric layer 205 also removes part or all of the spacer structure 202 .
[0062] In this embodiment, the process of removing the gate structure 201 and the first dielectric layer 205 removes all of the first dielectric layer 205 exposed by the first mask layer, so that the formed second opening 2907 exposes the surface of the stop layer 204 .
[0063] In other embodiments, the process of removing the gate structure and the first dielectric layer removes a portion of the first dielectric layer exposed by the first mask layer.
[0064] Next, a second dielectric layer 210 is formed in the second opening 207. For the process of forming the second dielectric layer 210, please refer to Fig. 9 and Fig.10 .
[0065] Please refer to Fig. 9 , Fig. 9 For Figure 8 Based on the structural diagram of FIG. 2 , a sacrificial structure is formed in the first opening 206 , and the sacrificial structure exposes the second opening 207 .
[0066] The sacrificial structure is used as a mask layer for subsequently forming a second dielectric layer 210 in the second opening 207 .
[0067] The sacrificial structure includes a single-layer structure or a multi-layer structure.
[0068] In this embodiment, the sacrificial structure is a multi-layer structure, and the multi-layer structure includes an amorphous material layer 208 and an anti-reflection layer 209 located on the amorphous material layer 208 .
[0069] The material of the amorphous material layer 208 includes amorphous carbon; the anti-reflection layer 209 includes a thin silicon anti-reflection layer (Si-ARC), an organic bottom anti-reflection layer (organic BARC), a dielectric anti-reflection layer (DARC) or a combination of an organic bottom anti-reflection layer and a dielectric anti-reflection layer.
[0070] In other embodiments, the material of the single-layer structure includes an amorphous material, and the amorphous material includes amorphous carbon.
[0071] The method for forming the sacrificial structure includes: forming a sacrificial structure material layer (not shown) in the first opening 206, in the second opening 207 and on the first dielectric layer 205; forming a patterned photoresist layer (not shown) on the sacrificial structure material layer, wherein the patterned photoresist layer exposes the sacrificial structure material layer on the second opening 207; etching the sacrificial structure material layer using the patterned photoresist layer as a mask until the bottom of the second opening 207 is exposed, thereby forming the sacrificial structure.
[0072] Please refer to Fig.10 , the second dielectric layer 210 is formed in the second opening 207 .
[0073] The method for forming the second dielectric layer 210 includes: forming a dielectric material layer (not shown) in the second opening 207 and on the sacrificial structure; planarizing the dielectric material layer until the sacrificial structure is exposed, and forming the second dielectric layer 210 in the second opening 207 .
[0074] In this embodiment, the height of the second dielectric layer 210 is greater than the height of the first dielectric layer 205. If the height of the second dielectric layer 210 is lower than the height of the first dielectric layer 205, when the isolation structure is subsequently formed in the first opening 206, the isolation structure material layer formed is located on the first dielectric layer 205 and the second dielectric layer 210, and when the isolation structure material layer is planarized until the surface of the first dielectric layer 205 is exposed, the material of the isolation structure on the second dielectric layer 210 is not removed cleanly, so that when the first dielectric layer 205 and the second dielectric layer 210 on the source-drain doped region 203 are subsequently etched, the material of the isolation structure makes the etching depth of the second dielectric layer 210 shallow, and further makes the formed conductive layer uneven, affecting the performance of the semiconductor structure.
[0075] The material of the second dielectric layer 210 includes a dielectric material. In this embodiment, the material of the second dielectric layer 210 includes silicon oxide. The process of forming the second dielectric layer 210 includes a chemical vapor deposition process or an atomic layer deposition process.
[0076] The material of the second dielectric layer 210 and the material of the first dielectric layer 205 have a smaller etching selectivity ratio, so that when the second dielectric layer 210 and the first dielectric layer 205 on the source-drain doped region 203 are subsequently etched, the etching process can simultaneously etch the second dielectric layer 210 and the first dielectric layer 205 until the surface of the stop layer 204 is exposed.
[0077] After forming the second dielectric layer 210 , the sacrificial structure is removed.
[0078] In this embodiment, the process of removing the sacrificial structure includes a dry etching process.
[0079] Please refer to Fig.11 and Fig.12 , Fig.11 for Fig.12 A top view of Fig.12 for Fig.11 The cross-sectional structure diagram along the section line EE′ shows that an isolation structure 211 is formed in the first opening 206 .
[0080] In this embodiment, the material of the second dielectric layer 210 is different from the material of the isolation structure 211 .
[0081] The material of the isolation structure 211 is different from that of the second dielectric layer 210. The second dielectric layer 210 and the isolation structure 211 can be formed at different times. On the one hand, the material of the second dielectric layer 210 can be selected to be a material that is easy to etch, so that the subsequent process of etching the first dielectric layer 205 and the second dielectric layer 210 is simple, which is beneficial to improving the performance of the semiconductor structure. On the other hand, the isolation structure 211 can be selected from a material with a dense structure and good isolation effect, so that the isolation structure 211 has a better isolation effect on the gate structure 201.
[0082] The method for forming the isolation structure 211 includes: forming an isolation material layer (not shown) in the first opening 206 , on the first dielectric layer 205 and on the second dielectric layer 210 ; and planarizing the isolation material layer and the second dielectric layer 210 until the surface of the first dielectric layer 205 is exposed to form the isolation structure 211 .
[0083] The material of the isolation structure 211 includes a dielectric material, and the dielectric material includes a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbonitride, and silicon carbonitride. In this embodiment, the material of the isolation structure 211 includes silicon nitride or silicon oxynitride.
[0084] In other embodiments, the material of the second dielectric layer can be the same as that of the isolation structure. The second dielectric layer and the isolation structure can be formed simultaneously.
[0085] The material of the isolation structure is the same as that of the second dielectric layer, so that the isolation structure and the second dielectric layer can be formed in one process, thereby simplifying the process flow and improving production efficiency.
[0086] The method for forming the second dielectric layer and the isolation structure includes: forming an isolation material layer in the first opening, in the second opening and on the first dielectric layer; planarizing the isolation material layer until the first dielectric layer is exposed, forming the second dielectric layer in the second opening, and forming the isolation structure in the first opening.
[0087] Please refer to Fig.13 and Fig.14 , Fig.13 for Fig.14 A top view of Fig.14 for Fig.13 Schematic diagram of the cross-sectional structure along the section line FF' direction, the first dielectric layer 205 and the second dielectric layer 210 on the source and drain doped regions 203 are etched to form a third opening 212 between the gate structures 201, there is a first difference between the etching rate of the second dielectric layer 210 and the etching rate of the first dielectric layer 205, and there is a second difference between the etching rate of the first dielectric layer 205 and the etching rate of the isolation structure 211, and the second difference is greater than the first difference.
[0088] The method for forming the third opening 212 includes: forming a patterned layer (not shown) on the isolation structure 211, the first dielectric layer 205 and the second dielectric layer 210, wherein the patterned layer exposes the first dielectric layer 205 and the second dielectric layer 210 on the source-drain doped region 203; etching the first dielectric layer 205 and the second dielectric layer 210 using the patterned layer as a mask until the surface of the stop layer 204 is exposed, thereby forming an initial third opening (not shown) between the gate structures 201; and removing the stop layer 204 on the surface of the source-drain doped region 203 until the surface of the source-drain doped region 203 is exposed, thereby forming the third opening 212.
[0089] In the process of etching the first dielectric layer 205 and the second dielectric layer 210, the etching rate of the first dielectric layer 205 by the etching process is greater than the etching rate of the stop layer 204, and the etching rate of the second dielectric layer 210 by the etching process is greater than the etching rate of the stop layer 204. Therefore, the process of etching the first dielectric layer 205 and the second dielectric layer 210 can be stopped on the surface of the stop layer 204, avoiding the situation that the process of etching the first dielectric layer 205 and the second dielectric layer 210 is over-etched and thus damages the source and drain doped regions 203.
[0090] The process of etching the first dielectric layer 205 and the second dielectric layer 210 includes a dry etching process or a wet etching process; the process of removing the stop layer 204 on the surface of the source / drain doped region 203 includes a wet etching process or a dry etching process.
[0091] In this embodiment, the process of etching the first dielectric layer 205 and the second dielectric layer 210 includes a dry etching process; and the process of removing the stop layer 204 on the surface of the source-drain doped region 203 includes a wet etching process.
[0092] Since there is a first difference between the etching rate of the second dielectric layer 210 and the etching rate of the first dielectric layer 205, and there is a second difference between the etching rate of the first dielectric layer 205 and the etching rate of the isolation structure 211, and the second difference is greater than the first difference, the process of etching the first dielectric layer 205 and the second dielectric layer 210 is simple, and the conductive layer structure subsequently formed in the third opening 212 is uniform, which is beneficial to improving the performance of the semiconductor structure.
[0093] Please refer to Fig.15 and Fig.16 , Fig.15 for Fig.16 A top view of Fig.16 for Fig.15 The schematic cross-sectional structure diagram along the section line GG′ shows that after the stop layer 204 is removed, a conductive layer 213 is formed in the third opening 212 , and the conductive layer 213 is electrically connected to the source-drain doped region 203 .
[0094] The material of the conductive layer 213 includes metal, and the metal includes one or more combinations of copper, aluminum, tungsten, nickel, cobalt, and titanium nitride.
[0095] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: providing a substrate, the substrate comprising an isolation region; Forming a plurality of parallelly arranged gate structures, source-drain doped regions and a first dielectric layer, wherein the gate structure is located on a substrate, a plurality of the gate structures span the isolation region, the source-drain doped regions are located in the substrate on both sides of the gate structure, and the first dielectric layer is located on a sidewall of the gate structure; The gate structure and the first dielectric layer on the isolation region are removed to form a first opening in the gate structure, wherein the first opening penetrates the gate structure in a direction perpendicular to the extension direction of the gate structure, and a second opening is formed in the first dielectric layer, wherein the second opening exposes the surface of the source and drain doped regions, and the first opening is connected to the second opening; forming a second dielectric layer in the second opening; forming an isolation structure in the first opening; The first dielectric layer and the second dielectric layer on the source and drain doped regions are etched to form a third opening between the gate structures, an etching rate of the second dielectric layer and an etching rate of the first dielectric layer have a first difference, and an etching rate of the first dielectric layer and an etching rate of the isolation structure have a second difference, and the second difference is greater than the first difference.
2. The method for forming a semiconductor structure according to claim 1, wherein: The material of the second dielectric layer is different from that of the isolation structure.
3. The method for forming a semiconductor structure according to claim 2, wherein: The method for forming the second dielectric layer includes: forming a sacrificial structure in the first opening, the sacrificial structure exposing the second opening; forming a dielectric material layer in the second opening and on the sacrificial structure; planarizing the dielectric material layer until the sacrificial structure is exposed, and forming the second dielectric layer in the second opening.
4. The method for forming a semiconductor structure according to claim 3, wherein: The sacrificial structure includes a single-layer structure or a multi-layer structure; the material of the single-layer structure includes an amorphous material, and the amorphous material includes amorphous carbon; the multi-layer structure includes an amorphous material layer and an anti-reflection layer located on the amorphous material layer.
5. The method for forming a semiconductor structure according to claim 3, wherein: The method for forming the sacrificial structure includes: forming a sacrificial structure material layer in the first opening, in the second opening and on the first dielectric layer; forming a patterned photoresist layer on the sacrificial structure material layer, wherein the patterned photoresist layer exposes the sacrificial structure material layer on the second opening; etching the sacrificial structure material layer using the patterned photoresist layer as a mask until the bottom of the second opening is exposed to form the sacrificial structure.
6. The method for forming a semiconductor structure according to claim 2, wherein: The method for forming the isolation structure comprises: forming an isolation material layer in the first opening, on the first dielectric layer and on the second dielectric layer; and planarizing the isolation material layer and the second dielectric layer until the surface of the first dielectric layer is exposed to form the isolation structure.
7. The method for forming a semiconductor structure according to claim 2, wherein: The material of the isolation structure includes silicon nitride or silicon oxynitride.
8. The method for forming a semiconductor structure according to claim 1, wherein: The material of the first dielectric layer includes silicon oxide; the material of the second dielectric layer includes silicon oxide.
9. The method for forming a semiconductor structure according to claim 1, wherein: The material of the second dielectric layer is the same as that of the isolation structure.
10. The method for forming a semiconductor structure according to claim 9, wherein: The method for forming the second dielectric layer and the isolation structure includes: forming an isolation material layer in the first opening, in the second opening and on the first dielectric layer; planarizing the isolation material layer until the first dielectric layer is exposed, forming the second dielectric layer in the second opening, and forming the isolation structure in the first opening.
11. The method for forming a semiconductor structure according to claim 1, wherein: The method for removing the gate structure and the first dielectric layer on the isolation region comprises: forming a first mask layer on the substrate, wherein the first mask layer exposes the surface of the gate structure and the first dielectric layer on the isolation region; and removing the gate structure and the first dielectric layer using the first mask layer as a mask.
12. The method for forming a semiconductor structure according to claim 11, wherein: The process of removing the gate structure and the first dielectric layer includes a dry etching process and a wet etching process or a combination of the two.
13. The method for forming a semiconductor structure according to claim 1, wherein: The substrate further includes an active region, the isolation region is located between adjacent active regions, and the gate structure spans the active region and the isolation region.
14. The method for forming a semiconductor structure according to claim 1, wherein: Before forming the first dielectric layer, the method further includes: forming a stop layer on the source-drain doped region, wherein the first dielectric layer is located on the stop layer; and the second opening exposes the stop layer on the surface of the source-drain doped region.
15. The method for forming a semiconductor structure according to claim 14, wherein: After etching the first dielectric layer and the second dielectric layer on the source and drain doped regions, the method further includes: removing the stop layer on the surface of the source and drain doped regions until the surface of the source and drain doped regions is exposed; after removing the stop layer, forming a conductive layer in the third opening, wherein the conductive layer is electrically connected to the source and drain doped regions.
16. The method for forming a semiconductor structure according to claim 15, wherein: During etching of the first dielectric layer and the second dielectric layer, the etching rate of the first dielectric layer by the etching process is greater than the etching rate of the stop layer, and the etching rate of the second dielectric layer by the etching process is greater than the etching rate of the stop layer.
17. The method for forming a semiconductor structure according to claim 15, wherein: The process of removing the stop layer includes a dry etching process or a wet etching process.
18. The method for forming a semiconductor structure according to claim 14, wherein: The material of the stop layer includes silicon nitride or silicon nitride oxide.
19. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the third opening includes: forming a patterned layer on the isolation structure, the first dielectric layer and the second dielectric layer, wherein the patterned layer exposes the first dielectric layer and the second dielectric layer on the source and drain doped regions; etching the first dielectric layer and the second dielectric layer using the patterned layer as a mask until the surface of the source and drain doped regions is exposed, thereby forming a third opening between the gate structures.
20. The method for forming a semiconductor structure according to claim 1, wherein: The process of etching the first dielectric layer and the second dielectric layer includes a dry etching process.