A MIM capacitor with a high flatness lower plate and a manufacturing method thereof

By providing a titanium-aluminum alloy suppression layer on the first metal layer of the lower plate of the MIM capacitor and generating a silicon oxide film on the substrate, the problems of high roughness and bulging of the aluminum plate are solved, and the flatness of the MIM capacitor is improved and Breakdown resistance.

CN114388270BActive Publication Date: 2024-12-06SOI MICRO CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210031920.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-12
Publication Date
2024-12-06
Estimated Expiration
2042-01-12

Smart Images

  • Figure CN114388270B_ABST
    Figure CN114388270B_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of MIM capacitors, and discloses a MIM capacitor with a lower plate of high flatness and a manufacturing method thereof. In the manufacturing method of the invention, silicon dioxide generated by the reaction of TEOS and oxygen is deposited on a substrate, so that a high-quality PVD deposition growth starting layer can be provided for a first metal layer, thereby making the generated first metal layer more uniform and stable. In the method of the invention, after the first metal layer, i.e., a first aluminum layer, a third metal layer, i.e., a titanium layer, and a lower cover plate layer are grown by a physical vapor phase method, a dielectric layer is then grown by chemical vapor deposition. In the chemical vapor deposition process, the contact surface of the aluminum layer and the titanium layer reacts to generate an aluminum-titanium alloy, which inhibits the upward migration of atoms in the aluminum layer, thereby avoiding the phenomenon of bulging in the aluminum layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of MIM capacitors, and in particular to a MIM capacitor with a lower plate having high flatness and a manufacturing method thereof. Background Art

[0002] RF circuits have been widely used in SOI, Bulk silicon, GaAs and SiGe. With the increase in the operating frequency and integration of RF circuits, higher requirements are placed on the capacitance accuracy of the capacitor structure and the reliability of the capacitor components. The existing capacitor processes are divided into MOMCAP process and MIMCAP process. The MIMCAP process has better capacitance accuracy and design flexibility due to its proprietary plate mask.

[0003] In the selection of the lower plate material of the MIM capacitor, aluminum metal is often used as the plate metal of the MIM capacitor because of its lower resistance and better Q value. In the MIMCAP process, the flatness of the lower plate of the manufactured MIM capacitor directly affects the breakdown reliability of the capacitor, so controlling the growth quality of the lower plate is the top priority of the entire MIM process. However, when aluminum is selected as the plate material of the MIM capacitor, due to the low thickness of the plate, the plate is very sensitive to the thermal budget, and the lower plate is prone to high roughness or aluminum bulging, which in turn causes the MIM capacitor to fail due to breakdown. Summary of the invention

[0004] In view of the shortcomings of the background technology, the present invention provides a MIM capacitor with a high-flatness lower plate and a manufacturing method thereof. The technical problem to be solved is that the existing MIMCAP process uses aluminum metal as the plate of the MIM capacitor, which will result in high roughness and aluminum bulging, causing the MIM capacitor to fail through breakdown.

[0005] To solve the above technical problems, in a first aspect, the present invention provides a MIM capacitor with a lower electrode plate of high flatness, comprising a placement layer arranged on a substrate, on which a lower electrode plate, a dielectric layer and an upper electrode plate are arranged in sequence from bottom to top, the lower electrode plate comprises a first metal layer, an inhibition layer and a lower cover layer arranged in sequence from bottom to top, the inhibition layer is configured to inhibit the upward migration of atoms of the first metal layer, and the upper electrode plate comprises a second metal layer and an upper cover layer arranged from bottom to top.

[0006] In certain embodiments of the first aspect, the materials of the first metal layer and the second metal layer are both aluminum.

[0007] In certain embodiments of the first aspect, the material of the inhibition layer is titanium aluminum alloy, and the material of the placement layer is silicon oxide.

[0008] In certain embodiments of the first aspect, the material of the dielectric layer is silicon nitride.

[0009] In a second aspect, the present invention provides a method for manufacturing a MIM capacitor with a lower plate having high flatness, comprising the following steps:

[0010] The following steps are involved:

[0011] S1: making a placement layer on a substrate;

[0012] S2: growing a first metal layer on the placement layer;

[0013] S3: forming an inhibition layer on the first metal layer;

[0014] S4: growing a lower cover layer on the inhibition layer;

[0015] S5: growing a dielectric layer on the lower cover layer;

[0016] S6: growing an upper electrode plate on the dielectric layer.

[0017] In a certain embodiment of the second aspect, in step S1, silicon dioxide generated by the reaction of TEOS and oxygen is deposited on a substrate by using a chemical vapor deposition process, thereby manufacturing a silicon oxide film, which is a placement layer.

[0018] In a certain embodiment of the second aspect, physical vapor deposition is used to grow the first metal layer, the lower cover layer, the second metal layer and the upper cover layer in steps S2, S4, S6 and S7, and chemical vapor deposition is used to grow the dielectric layer in step S5.

[0019] In a certain embodiment of the second aspect, a titanium layer is deposited by physical deposition in step S3, the materials of the first metal layer and the second metal layer are aluminum, and in the chemical vapor deposition process in step S5, the contact surface of the titanium layer and the first metal layer reacts to generate a titanium-aluminum alloy layer.

[0020] In certain implementation manner of the second aspect, the following steps are performed after step S7:

[0021] S8: applying photoresist on the upper cover layer to form a photoresist layer, defining the pattern of the actual cover layer of the MIM capacitor on the photoresist layer through a photolithography process, then etching the upper cover layer, the second metal layer and the dielectric layer through an etching process, and transferring the pattern of the actual cover layer defined on the photoresist layer to the upper cover layer, the second metal layer and the dielectric layer;

[0022] S9: Apply photoresist to the area on the lower cover layer that is not covered by the dielectric layer to form a second photoresist layer, define the pattern of the actual lower cover layer of the MIM capacitor on the second photoresist layer through a photolithography process, and then etch the lower cover layer, the inhibition layer and the first metal layer through an etching process, and transfer the pattern of the actual lower cover layer defined on the second photoresist layer to the lower cover layer, the inhibition layer and the dielectric layer.

[0023] In a certain implementation of the second aspect, step S6 is specifically as follows: first, a second metal layer is grown on the dielectric layer, and then an upper cover layer is grown on the second metal layer.

[0024] Compared with the prior art, the present invention has the following beneficial effects: in the process of manufacturing a MIM capacitor on a substrate, after the first metal layer of the lower plate is manufactured, an inhibition layer is set on the first metal layer to prevent atomic migration during the entire manufacturing process of the first metal layer MIM capacitor, thereby avoiding bulging on the first metal layer; in the manufacturing method of the present invention, silicon dioxide generated by the reaction of TEOS with oxygen is deposited on the substrate, thereby providing a high-quality PVD deposition growth starting layer for the first metal layer, thereby making the generated first metal layer more uniform and stable; in the method of the present invention, after the first metal layer, i.e., the first aluminum layer, the titanium layer and the lower cover plate layer, is grown by a physical vapor phase method, then a dielectric layer is grown by chemical vapor deposition, in which the contact surface of the aluminum layer and the titanium layer reacts to generate an aluminum-titanium alloy, which inhibits the upward migration of atoms in the aluminum layer, thereby avoiding bulging on the aluminum layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic diagram of the structure of a MIM capacitor of the present invention;

[0026] Figure 2 is a flow chart of the manufacturing method of the present invention;

[0027] Figure 3 It is a schematic diagram of the structural changes of the MIM capacitor during the manufacturing method of the present invention. DETAILED DESCRIPTION

[0028] The illustrative embodiments of the present application include but are not limited to a MIM capacitor with a lower plate having high flatness and a method for manufacturing the same.

[0029] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The implementations described in the following exemplary embodiments do not represent all implementations consistent with the present application. Instead, they are merely examples of devices and methods consistent with some aspects of the present application as detailed in the appended claims.

[0030] The terms used in this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The singular forms of "a", "said" and "the" used in this application and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings. It should also be understood that the term "and / or" used in this article refers to and includes any or all possible combinations of one or more associated listed items. "Include" or "include" and similar words mean that the elements or objects appearing in front of "include" or "include" cover the elements or objects listed after "include" or "include" and their equivalents, and do not exclude other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, and can include electrical connections, whether direct or indirect.

[0031] It should be understood that although the terms first, second, third, etc. may be used in the present application to describe various information, these information should not be limited to these terms. These terms are only used to distinguish the same type of information from each other. For example, without departing from the scope of the present application, the first information may also be referred to as the second information, and similarly, the second information may also be referred to as the first information. Depending on the context, the word "if" as used herein may be interpreted as "at the time of" or "when" or "in response to determining".

[0032] like Figure 1 As shown, a MIM capacitor with a high-flatness lower plate includes a placement layer arranged on a substrate, on which a lower plate, a dielectric layer and an upper plate are arranged in sequence from bottom to top, and the lower plate includes a first metal layer, an inhibition layer and a lower cover layer arranged in sequence from bottom to top, and the inhibition layer is configured to inhibit the upward migration of atoms in the first metal layer.

[0033] exist Figure 1 In the embodiment, the upper electrode plate includes a second metal layer and an upper cover plate layer arranged from bottom to top.

[0034] The substrate may be a SOI wafer, bulk silicon or other dielectric layers.

[0035] The material of the placement layer is silicon dioxide.

[0036] The materials of the first metal layer and the second metal layer are aluminum, and the material of the inhibition layer is aluminum-titanium alloy.

[0037] In some embodiments, the top plate may be a separate titanium nitride layer, which is replaced by a titanium nitride layer. Figure 1 The second metal layer and the upper cover layer in.

[0038] In this embodiment, every two mutually contacting contact surfaces of the MIM capacitor are arranged to match, that is, the size and shape of the two contact surfaces are the same. In a certain embodiment, every two mutually contacting contact surfaces of the lower plate are arranged to match, every two mutually contacting contact surfaces of the upper plate are arranged to match, the contact areas of the two contact surfaces of the second metal layer and the dielectric layer are arranged to match, the contact area area of ​​the dielectric layer and the upper cover layer is smaller than the top surface area of ​​the upper cover layer, and the contact area area of ​​the bottom surface of the first metal layer and the placement layer is smaller than the top surface area of ​​the placement layer.

[0039] like Figure 2 As shown, a method for manufacturing a MIM capacitor with a lower plate having high flatness comprises the following steps:

[0040] S1: making a placement layer on a substrate;

[0041] Specifically, in step S1, silicon dioxide generated by the reaction of TEOS and oxygen is deposited on the substrate by using a chemical vapor deposition process, thereby forming a silicon dioxide film, which is a placement layer. Figure 3 The substrate is not shown in the schematic diagram of a. When step S1 is actually performed, the substrate may be a SOI wafer, bulk silicon or other dielectric layers that can be used to make MIM capacitors.

[0042] Compared with silicon dioxide generated by reacting silane with oxygen, the silicon atoms in TEOS in the present invention are surrounded by four oxygen atoms instead of four hydrogen atoms. Therefore, the generated deposition layer has less hydrogen, is denser, and has relatively better roughness, which is conducive to the growth of the subsequent first metal layer.

[0043] When actually making the placement layer, a plasma-enhanced chemical vapor process is used at a high temperature of 400 degrees to produce a dense silicon dioxide film at a low deposition rate.

[0044] S2: growing a first metal layer on the placement layer;

[0045] S3: forming an inhibition layer on the first metal layer;

[0046] In this embodiment, an inhibition layer can be directly set to inhibit the atomic migration of the first metal layer, or a third metal layer can be grown on the first metal layer, and then in a subsequent process, the third metal layer is allowed to react with the first metal layer to form an alloy layer, and the atomic migration of the first metal layer is inhibited by the alloy layer. The following steps S4, S5, S6 and S7 are performed on the basis of growing the third metal layer.

[0047] S4: growing a lower cover layer on the third metal layer;

[0048] After executing steps S2, S3 and S4, the generated structural diagram is as follows: Figure 3b. Specifically, in steps S2, S3 and S4, the first metal layer, the third metal layer and the lower cover layer are grown by physical vapor deposition, respectively. In this embodiment, the material of the first metal layer is aluminum, the material of the second metal layer is titanium, and the material of the lower cover layer is titanium nitride. In some implementations, the material of the third metal layer may also be tantalum, and the material of the lower cover layer may also be tantalum nitride.

[0049] S5: growing a dielectric layer on the lower cover layer;

[0050] Specifically, in step S5, a dielectric layer is grown on the lower cover plate by a chemical vapor process. In this embodiment, the material of the dielectric layer is silicon nitride, and the deposition temperature in the chemical vapor process in step S5 is 400 degrees Celsius. Since the material of the first metal layer in this embodiment is aluminum and the material of the third metal layer is titanium, aluminum and titanium will combine to form an aluminum-titanium alloy at 400 degrees Celsius, and the aluminum-titanium alloy can inhibit the upward migration of aluminum atoms. In actual use, the lower part of the third metal layer will react with the first metal layer to form an aluminum-titanium alloy. The inhibition layer of the MIM capacitor manufactured by the method of the present invention includes an aluminum-titanium alloy and a titanium layer in the third metal layer that does not react with aluminum. In a certain embodiment, when the first metal layer is used.

[0051] S6: growing a second metal layer on the dielectric layer;

[0052] S7: growing an upper cover layer on the second metal layer.

[0053] Specifically, step S6 and step S7 grow the second metal layer and the upper cover layer respectively by physical vapor deposition. In this embodiment, the material of the second metal layer is aluminum, and the material of the upper cover layer is titanium nitride. The structural schematic diagram of the MIM capacitor after executing step S7 is shown in FIG. Figure 3 As shown in d.

[0054] In some implementations, after step S5 is performed, a titanium nitride layer may be directly formed on the dielectric layer to replace the second metal layer and the upper cover layer.

[0055] Reference Figure 3 a to Figure 3 d. The contact surfaces of every two adjacent layers of the placement layer, the first metal layer, the third metal layer, the lower cover plate layer, the dielectric layer, the second metal layer and the upper cover plate layer of the MIM capacitor manufactured by the manufacturing method of the present invention are arranged to match, that is, the contact surfaces of the adjacent layers are the same in size and shape. However, in actual use, it may be required that the sizes of the opposite surfaces of the upper plate and the lower plate of the MIM capacitor are different. Therefore, after executing step S7, the following steps can also be performed to make the sizes of the upper plate and the lower plate of the MIM capacitor to the target size.

[0056] S8: Apply photoresist on the upper cover layer to form a photoresist layer, and form a photoresist layer on the photoresist layer through a photolithography process.

[0057] The actual cover layer pattern of the MIM capacitor is defined, and then the upper cover layer, the second metal layer and the dielectric layer are etched by an etching process, and the actual cover layer pattern defined on the photoresist layer is transferred to the upper cover layer, the second metal layer and the dielectric layer; the structural schematic diagram of the MIM capacitor after executing step S8 is as shown in FIG. Figure 3 As shown in e;

[0058] S9: applying photoresist to the area on the lower cover layer not covered by the dielectric layer to form a second photoresist layer, defining the pattern of the actual lower cover layer of the MIM capacitor on the second photoresist layer through a photolithography process, then etching the lower cover layer, the inhibition layer and the first metal layer through an etching process, and transferring the pattern of the actual lower cover layer defined on the second photoresist layer to the lower cover layer, the inhibition layer and the dielectric layer; the structural schematic diagram of the MIM capacitor after executing step S9 is as shown in FIG. Figure 3 f.

[0059] In summary, in the process of manufacturing MIM capacitors on a substrate of the present invention, after the first metal layer of the lower plate is manufactured, an inhibition layer is set on the first metal layer to prevent atomic migration during the entire manufacturing process of the first metal layer MIM capacitor, thereby avoiding bulging on the first metal layer; in the manufacturing method of the present invention, silicon dioxide generated by the reaction of TEOS and oxygen is deposited on the substrate, so that a high-quality PVD deposition growth starting layer can be provided for the first metal layer, thereby making the generated first metal layer more uniform and stable; in the method of the present invention, after the first metal layer, i.e., the first aluminum layer, the third metal layer, i.e., the titanium layer and the lower cover plate layer, are grown by a physical vapor method, and then the dielectric layer is grown by chemical vapor deposition. In the chemical vapor deposition process, the contact surface of the aluminum layer and the titanium layer will react to generate an aluminum-titanium alloy, which will inhibit the upward migration of atoms in the aluminum layer, thereby avoiding bulging on the aluminum layer.

[0060] The above is based on the present invention as an inspiration. Through the above description, relevant staff can make various changes and modifications without departing from the technical idea of ​​this invention. The technical scope of this invention is not limited to the content in the specification, and its technical scope must be determined according to the scope of the claims.

Claims

1. A method for manufacturing a MIM capacitor with a lower plate of high flatness, wherein the MIM capacitor with a lower plate of high flatness comprises a placement layer arranged on a substrate, wherein a lower plate, a dielectric layer and an upper plate are arranged on the placement layer in sequence from bottom to top, wherein the lower plate comprises a first metal layer, an inhibition layer and a lower cover layer arranged in sequence from bottom to top, wherein the inhibition layer is configured to inhibit atoms of the first metal layer from migrating upward; The material of the first metal layer is aluminum, and the material of the inhibition layer is titanium aluminum alloy; the upper electrode plate includes a second metal layer and an upper cover plate layer arranged from bottom to top, the material of the second metal layer is aluminum, and the material of the dielectric layer is silicon nitride; The manufacturing method comprises the following steps: S1: making a placement layer on a substrate; S2: growing a first metal layer on the placement layer; S3: forming an inhibition layer on the first metal layer; S4: growing a lower cover layer on the inhibition layer; S5: growing a dielectric layer on the lower cover layer; S6: growing an upper electrode plate on the dielectric layer; S7: growing an upper cover layer on the second metal layer; S8: applying photoresist on the upper cover layer to form a photoresist layer, defining the pattern of the actual cover layer of the MIM capacitor on the photoresist layer through a photolithography process, then etching the upper cover layer, the second metal layer and the dielectric layer through an etching process, and transferring the pattern of the actual cover layer defined on the photoresist layer to the upper cover layer, the second metal layer and the dielectric layer; S9: applying photoresist to the area on the lower cover layer that is not covered by the dielectric layer to form a second photoresist layer, defining the pattern of the actual lower cover layer of the MIM capacitor on the second photoresist layer by a photolithography process, then etching the lower cover layer, the inhibition layer and the first metal layer by an etching process, and transferring the pattern of the actual lower cover layer defined on the second photoresist layer to the lower cover layer, the inhibition layer and the dielectric layer; In steps S2, S4, S6 and S7, the first metal layer, the lower cover layer, the second metal layer and the upper cover layer are grown by physical vapor deposition, and in step S5, the dielectric layer is grown by chemical vapor deposition; In step S3, a titanium layer is deposited by physical deposition. The materials of the first metal layer and the second metal layer are aluminum. In the chemical vapor deposition process of step S5, the contact surface of the titanium layer and the first metal layer reacts to generate a titanium-aluminum alloy layer. The temperature of the chemical vapor deposition process of step S5 is 400 degrees Celsius.

2. The method for manufacturing a MIM capacitor with a lower plate having high flatness according to claim 1, characterized in that: In step S1, silicon dioxide generated by the reaction of TEOS and oxygen is deposited on a substrate by using a chemical vapor deposition process, thereby manufacturing a silicon oxide film, which is a placement layer.

3. The method for manufacturing a MIM capacitor with a lower plate having high flatness according to claim 2, characterized in that: The specific steps in step S6 are as follows: first, a second metal layer is grown on the dielectric layer, and then an upper cover layer is grown on the second metal layer.

4. The method for manufacturing a MIM capacitor with a lower plate having high flatness according to claim 1, characterized in that: The material of the placement layer is silicon oxide.