Semiconductor device and method for manufacturing the same

By forming trenches between the top metal interconnect structures of the T2Mx type and fabricating MIM capacitor structures, the problem of insufficient insulation layer thickness was solved, and MIM capacitors were successfully formed on the top metal interconnect structure of the T2Mx type, avoiding leakage or short circuit.

CN114429942BActive Publication Date: 2024-11-08SHANGHAI HUAHONG GRACE SEMICON MFG CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210083459.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-13
Publication Date
2024-11-08
Estimated Expiration
2042-01-13

AI Technical Summary

Technical Problem

Existing technologies cannot form MIM capacitors on top metal interconnect structures of the T2Mx type because the insulation layer thickness is insufficient to meet the thickness requirements of MIM capacitors.

Method used

Trenches are formed between the top metal interconnect structures of the T2Mx type, and MIM capacitor structures are fabricated in the trenches, extending upward to the top surface of the dielectric layer. An insulating layer is then covered on the dielectric layer. The height difference between the MIM capacitor structure and the dielectric layer is reduced by forming trenches in the dielectric layer.

Benefits of technology

Without altering the thickness of each film layer in the original metal interconnect structure, a MIM capacitor was successfully formed on the top metal interconnect structure of the T2Mx type, meeting the insulation layer thickness requirements and avoiding leakage or short circuit phenomena.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114429942B_ABST
    Figure CN114429942B_ABST
Patent Text Reader

Abstract

The present invention provides a semiconductor device and a method for manufacturing the same, comprising: a substrate having a dielectric layer on the substrate, a gate structure and a plurality of top-layer metal interconnect structures in the dielectric layer; a groove extending from the top surface of the dielectric layer into the dielectric layer and located between adjacent top-layer metal interconnect structures; a MIM capacitor structure located in the groove and extending upward to a height higher than the top surface of the dielectric layer; and an insulating layer covering the substrate and the MIM capacitor structure. The groove is formed in the dielectric layer, and the MIM capacitor structure is formed in the groove to reduce the height difference between the MIM capacitor structure and the dielectric layer, so that the thickness of the insulating layer can meet the process of preparing the MIM capacitor on the T2Mx type top-layer metal interconnect structure without changing the thickness of each film layer of the original metal interconnect structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor preparation, and in particular to a semiconductor device and a preparation method thereof. Background Art

[0002] Capacitors are often used as electronic passive devices in integrated circuits such as radio frequency and monolithic microwave. Common capacitor components include metal oxide semiconductor (MOS) capacitors, PN junction capacitors, and metal-insulator-metal (MIM) capacitors. Among them, MIM capacitors can provide better frequency and temperature related characteristics in some special applications. In semiconductor preparation, MIM capacitors can be formed in interlayer metal and top metal interconnect structures, which also reduces the complexity of integrated circuit preparation.

[0003] There are three types of semiconductor top metal interconnect structures (Top Metal): T4Mx (the thickness of the insulating layer is four times the thickness of the previous metal interconnect layer), T2Mx (the thickness of the insulating layer is twice the thickness of the previous metal interconnect layer) and UTM. Among them, the thickness of the insulating layer required for forming electrical connectors in the T2Mx type top metal interconnect structure is relatively small, and is smaller than the thickness required for the MIM capacitor process, making it impossible to form a MIM capacitor on the T2Mx type top metal interconnect structure. Summary of the invention

[0004] The object of the present invention is to provide a semiconductor device and a method for manufacturing the same, so as to realize the formation of a MIM capacitor on a top metal interconnect structure of a T2Mx type.

[0005] In order to achieve the above object, the present invention provides a semiconductor device, comprising:

[0006] A substrate having a dielectric layer thereon, wherein the dielectric layer has a gate structure and a plurality of top metal interconnect structures, each of which comprises at least two electrically connected metal interconnect layers;

[0007] A groove extending from the top surface of the dielectric layer into the dielectric layer and located between adjacent top metal interconnect structures;

[0008] A MIM capacitor structure is located in the trench and extends upward to be higher than the top surface of the dielectric layer;

[0009] An insulating layer covers the substrate and the MIM capacitor structure.

[0010] Optionally, an obtuse angle is formed between the side wall of the groove and the bottom of the groove.

[0011] Optionally, the depth of the groove is

[0012] Optionally, there is a gap between the sidewall of the MIM capacitor structure and the sidewall of the trench.

[0013] Optionally, the MIM capacitor structure includes:

[0014] A lower electrode plate, located in the groove and covering a portion of the bottom surface of the groove;

[0015] A dielectric layer covering the upper surface of the lower electrode plate;

[0016] The upper electrode plate is located on the dielectric layer and covers a portion of the dielectric layer.

[0017] Optionally, the semiconductor device further includes:

[0018] The metal wiring layer is located on the insulating layer and is electrically connected to the top metal interconnection structure, the upper electrode plate and the lower electrode plate through a plurality of electrical connectors.

[0019] Optionally, the thickness of the insulating layer is

[0020] Based on the same inventive concept, the present invention also provides a method for preparing a semiconductor device, comprising:

[0021] Providing a substrate, having a dielectric layer on the substrate, and having a gate structure and a plurality of top metal interconnect structures in the dielectric layer, each of the top metal interconnect structures comprising at least two electrically connected metal interconnect layers;

[0022] Etching the dielectric layer to form a groove, wherein the groove extends from the top surface of the dielectric layer into the dielectric layer, and the groove is located between adjacent top-layer metal interconnect structures;

[0023] forming a MIM capacitor structure in the groove, wherein the MIM capacitor structure extends upward to a level higher than the top surface of the dielectric layer;

[0024] An insulating layer is formed on the dielectric layer, wherein the insulating layer covers the MIM capacitor structure and the dielectric layer.

[0025] Optionally, the step of forming the MIM capacitor structure includes:

[0026] forming a stacked layer on the dielectric layer, the stacked layer covering the dielectric layer and the groove, the stacked layer comprising a first metal layer, a dielectric material layer and a second metal layer sequentially stacked on the dielectric layer;

[0027] Etching away the stacked layers on the surface of the dielectric layer and part of the groove, and the remaining first metal layer, the dielectric material layer and the second metal layer respectively constitute the lower plate, the dielectric layer and the upper plate of the MIM capacitor structure;

[0028] The lower electrode plate covers part of the bottom surface of the groove, the dielectric layer covers the upper surface of the lower electrode plate, and the upper electrode plate covers part of the dielectric layer.

[0029] Optionally, after forming the MIM capacitor structure, the method further includes:

[0030] forming the insulating layer on the dielectric layer, wherein the insulating layer fills the groove and covers the dielectric layer and the MIM capacitor structure;

[0031] performing a planarization process on the insulating layer;

[0032] Etching the insulating layer to form an opening in the insulating layer to expose the top metal interconnect structure, the upper electrode plate and the lower electrode plate;

[0033] A metal wiring layer is formed on the insulating layer and an electrical connection member is formed in the opening. The metal wiring layer is electrically connected to the top metal interconnection structure, the upper electrode plate and the lower electrode plate through a plurality of the electrical connections.

[0034] The present invention provides a semiconductor device and a method for manufacturing the same, comprising: a substrate having a dielectric layer on the substrate, a gate structure and a plurality of top-layer metal interconnect structures in the dielectric layer; a groove extending from the top surface of the dielectric layer into the dielectric layer and located between adjacent top-layer metal interconnect structures; a MIM capacitor structure located in the groove and extending upward to a height higher than the top surface of the dielectric layer; and an insulating layer covering the substrate and the MIM capacitor structure. The groove is formed in the dielectric layer, and the MIM capacitor structure is formed in the groove to reduce the height difference between the MIM capacitor structure and the dielectric layer, so that the thickness of the insulating layer can meet the process of preparing the MIM capacitor on the T2Mx type top-layer metal interconnect structure without changing the thickness of each film layer of the original metal interconnect structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 A flow chart of a method for preparing a semiconductor device provided by the present invention;

[0036] Figures 2 to 9 A schematic structural diagram corresponding to corresponding steps of a method for preparing a semiconductor device provided by the present invention;

[0037] The accompanying drawings are as follows:

[0038] 100-substrate; 102-dielectric layer; 104-metal interconnect structure; 108-dielectric barrier layer; 110-groove; 112-oxide layer; 114-first metal layer; 115-lower plate; 117-dielectric layer; 116-dielectric material layer; 118-second metal layer; 120-first etch stop layer; 119-upper plate; 122-second etch stop layer; 124-insulating layer. DETAILED DESCRIPTION

[0039] The specific implementation of the present invention will be described in more detail below in conjunction with the schematic diagram. The advantages and features of the present invention will become clearer based on the following description. It should be noted that the drawings are all in a very simplified form and are not in exact proportions, and are only used to facilitate and clearly assist in explaining the purpose of the embodiments of the present invention.

[0040] Hereinafter, the terms "first", "second", etc. are used to distinguish between similar elements and are not necessarily used to describe a particular order or chronological sequence. It is to be understood that these terms used in this manner are interchangeable where appropriate. Similarly, if the method described herein includes a series of steps, the steps presented herein are not necessarily the only order in which the steps can be performed, and some of the steps described may be omitted and / or other steps not described in the text may be added to the method.

[0041] Fig. 9 A schematic diagram of the structure of a semiconductor device provided in this embodiment, such as Fig. 9 As shown, the semiconductor device includes: a substrate 100, on which a dielectric layer 102 is provided, wherein the dielectric layer 102 has a gate structure and a plurality of top-layer metal interconnect structures 104, wherein each top-layer metal interconnect structure 104 includes at least two electrically connected metal interconnect layers; a groove 110, extending from the top surface of the dielectric layer 102 into the dielectric layer 102, and located between adjacent top-layer metal interconnect structures 104; a MIM capacitor structure, located in the groove 110, and extending upward to be higher than the top surface of the dielectric layer 102; and an insulating layer 124, covering the dielectric layer 102 and the MIM capacitor structure.

[0042] The MIM capacitor structure includes: a lower plate 115 located in the groove 110 and covering a portion of the bottom surface of the groove 110 ; a dielectric layer 117 covering the upper surface of the lower plate 115 ; and an upper plate 119 located on the dielectric layer 117 and covering a portion of the dielectric layer 117 .

[0043] An oxide layer 112 is further included between the MIM capacitor structure and the trench 110. Specifically, the oxide layer 112 covers the dielectric layer 102 and the inner wall of the trench 110, and the MIM capacitor structure is formed on the oxide layer 112. The MIM capacitor structure is insulated from the trench 110. In addition, there is a gap between the sidewall of the MIM capacitor structure and the sidewall of the trench 110 to avoid leakage or short circuit caused by the MIM capacitor structure and the top metal interconnect structure 104 being too close.

[0044] Furthermore, the insulating layer 124 further includes a metal wiring layer (not shown), and the metal wiring layer is electrically connected to the top metal interconnect structure 104, the upper plate 119 and the lower plate 115 through a plurality of electrical connectors penetrating the insulating layer 124. In order to meet the requirements of the T2Mx type top metal interconnect structure for the thickness of the insulating layer 124 for forming the electrical connectors, the thickness of the insulating layer 124 is

[0045] Since the thickness of the MIM capacitor structure and the thickness of the insulating layer 124 required by the process are The thickness of the insulating layer 124 provided by the T2Mx type top metal interconnect structure is not enough to directly form the MIM capacitor structure on the dielectric layer 102. Therefore, the present invention forms the groove 110 in the dielectric layer 102 between adjacent top metal interconnect structures 104, and forms the MIM capacitor structure in the groove 110 to reduce the height difference between the MIM capacitor structure and the dielectric layer 102. Without changing the thickness of the insulating layer 124, the MIM capacitor structure is formed on the T2Mx type top metal interconnect structure. The depth of the groove 110 is

[0046] In addition, an obtuse angle is formed between the side wall of the groove 110 and the bottom of the groove 110, and the angle of the obtuse angle is greater than 100°, so that the side wall angle of the groove 110 is flatter, thereby making the thickness of the film layer subsequently formed on the side wall of the groove 110 more uniform, and also facilitating the subsequent removal of the film layer.

[0047] Figure 1 A flowchart of a method for preparing a semiconductor device provided in this embodiment is shown in FIG. Figure 1 As shown, the present invention provides a method for preparing a semiconductor device, comprising:

[0048] Step S1: providing a substrate, on which a dielectric layer is provided, and in which a gate structure and a plurality of top-layer metal interconnect structures are provided, each of which comprises at least two electrically connected metal interconnect layers;

[0049] Step S2: etching the dielectric layer to form a groove, wherein the groove extends from the top surface of the dielectric layer into the dielectric layer, and the groove is located between adjacent top-layer metal interconnect structures;

[0050] Step S3: forming a MIM capacitor structure in the trench, wherein the MIM capacitor structure extends upward to a level higher than the top surface of the dielectric layer;

[0051] Step S4: forming an insulating layer on the dielectric layer, wherein the insulating layer covers the MIM capacitor structure and the dielectric layer.

[0052] Figures 2 to 9 The following is a schematic diagram of the structure corresponding to the corresponding steps of the method for preparing a semiconductor device provided by the present invention, and is combined with the attached Figures 2 to 9 A method for manufacturing a semiconductor device provided in this embodiment is described in more detail, wherein an optional embodiment of the present invention is illustrated.

[0053] like Figure 2 As shown, a substrate 100 is provided, and a dielectric layer 102 is formed on the substrate 100. The dielectric layer 102 has a gate structure (not shown) and a plurality of top metal interconnect structures 104. Each of the top metal interconnect structures 104 is composed of at least two electrically connected metal interconnect layers.

[0054] In this embodiment, the dielectric layer 102 has a plurality of film layers, but the present invention is not limited thereto.

[0055] A dielectric barrier layer 108 is formed on the dielectric layer 102, and the dielectric barrier layer 108 covers the dielectric layer 102 and the top metal interconnect structure 104. The dielectric barrier layer 108 is made of nitrogen-doped silicon carbide (NDC), and the dielectric barrier layer 108 can prevent the metal material in the top metal interconnect structure 104 from directly contacting other film layers, thereby preventing the diffusion of the metal material; at the same time, the dielectric barrier layer 108 can also serve as an etching stop layer.

[0056] like Figure 3As shown, an alignment mark (AM) layer is formed on the dielectric barrier layer 108, and the alignment mark layer is exposed to form an alignment mark. Then, the dielectric barrier layer 108 and a portion of the dielectric layer 102 between the adjacent top metal interconnect structures 104 are etched using the alignment mark layer as a mask to form a groove 110 extending from the top surface of the dielectric layer 102 to the inside of the dielectric layer 102. The depth of the groove 110 is An obtuse angle is formed between the sidewall of the groove 110 and the bottom of the groove 110 . The obtuse angle is greater than 100°, which improves the thickness uniformity of the film layer formed on the sidewall of the groove 110 and facilitates the subsequent removal of the film layer.

[0057] It should be noted that, by using the alignment mark layer as a mask to etch and form the groove 110, it is possible to avoid adding a new mask, thereby achieving the purpose of reducing process steps and costs.

[0058] like Figure 4 As shown, an oxide layer 112 and a stacked layer are formed on the dielectric barrier layer 108, the oxide layer 112 covers the dielectric barrier layer 108 and the groove 110, the stacked layer covers the oxide layer 112, and the stacked layer includes a first metal layer 114, a dielectric material layer 116, and a second metal layer 118 stacked in sequence on the oxide layer 112.

[0059] The first metal layer 114 may be a stack of metal aluminum, metal titanium and titanium nitride, the dielectric material layer 116 may be made of silicon nitride, and the second metal layer 118 may be made of titanium nitride.

[0060] Furthermore, a first etch stop layer 120 is formed on the stacked layer, and the first etch stop layer 120 covers the stacked layer. The material of the first etch stop layer 120 may be silicon nitride.

[0061] like Figure 5 As shown, the first etch stop layer 120 and the second metal layer 118 are etched to remove the first etch stop layer 120 and the second metal layer 118 on the dielectric layer 102 and part of the groove 110, and the remaining second metal layer 118 forms the upper plate 119 of the MIM capacitor structure.

[0062] In the process of forming the upper electrode plate 119 , in order to completely remove the second metal layer 118 outside the upper electrode plate 119 , over-etching may be performed to remove a portion of the thickness of the dielectric material layer 116 .

[0063] like Figure 6As shown, a second etch stop layer 122 is formed conformally on the dielectric material layer 116, and the second etch stop layer 122 covers the first etch stop layer 120 and the dielectric material layer 116. At this time, the sum of the thickness of the dielectric material layer 116 on the second metal layer 118 and the thickness of the second etch stop layer 122 is greater than The sum of the thickness of the first etch stop layer 120 and the thickness of the second etch stop layer 122 on the upper electrode plate 119 is greater than

[0064] Wherein, the material of the second etch stop layer 122 is silicon nitride.

[0065] like Figure 7 As shown, the second etch stop layer 122, the dielectric material layer 116 and the first metal layer 114 are etched to remove portions of the second etch stop layer 122, the dielectric material layer 116 and the first metal layer 114 on the dielectric layer 102 and in the groove 110. The remaining first metal layer 114 forms the lower plate 115 of the MIM capacitor structure, and the remaining dielectric material layer 116 forms the dielectric layer 117 of the MIM capacitor structure.

[0066] The lower electrode plate 115 is located in the groove 110 and covers a portion of the bottom surface of the groove 110; the dielectric layer 117 covers the upper surface of the lower electrode plate 115; the upper electrode plate 119 is located on the dielectric layer 117 and covers a portion of the dielectric layer 117; the upper electrode plate 119, the lower electrode plate 115 and the dielectric layer 117 constitute the MIM capacitor structure.

[0067] In order to completely etch the second metal layer 118 outside the lower electrode plate 115 , a portion of the oxide layer 112 may be etched to avoid a short circuit between the upper electrode plate 119 and the lower electrode plate 115 due to residual metal.

[0068] like Figure 8 As shown, the insulating layer 124 is formed, the insulating layer 124 covers the oxide layer 112 and fills the remaining portion of the trench 110, and then the insulating layer 124 is planarized to make the upper surface of the insulating layer 124 flat and reduce the thickness of the insulating layer 124. In this embodiment, the thickness of the insulating layer 124 is reduced to The thickness of the insulating layer 124 meets the requirements of the T2Mx type top metal interconnect structure. At this time, the thickness from the bottom surface of the trench 110 to the top surface of the insulating layer 124 is greater than Meet the requirements of MIM capacitor process.

[0069] like Fig. 9As shown, the insulating layer 124 is etched to form an opening in the insulating layer 124 to expose the top metal interconnect structure 104, the upper plate 119 and the lower plate 115. Finally, a metal layer is formed on the insulating layer 124, the metal layer fills the opening to form an electrical connection connected to the top metal interconnect structure 104, the upper plate 119 and the lower plate 115, and the metal layer is etched to form a metal wiring layer (not shown).

[0070] In summary, the present invention provides a semiconductor device and a method for preparing the same, comprising: a substrate 100, wherein the substrate 100 has a dielectric layer 102, wherein the dielectric layer 102 has a gate structure and a plurality of top-layer metal interconnect structures 104, wherein each top-layer metal interconnect structure 104 includes at least two electrically connected metal interconnect layers; a groove 110, extending from the top surface of the dielectric layer 102 into the dielectric layer 102 and located between adjacent top-layer metal interconnect structures 104; a MIM capacitor structure, located in the groove 110 and extending upward to be higher than the top surface of the dielectric layer 102; and an insulating layer 124, covering the substrate 100 and the MIM capacitor structure. The groove 110 is formed in the dielectric layer 102, and the MIM capacitor structure is formed in the groove 1101 to reduce the height difference between the MIM capacitor structure and the dielectric layer 102. Without changing the thickness of each film layer of the original metal interconnect structure, the thickness of the insulating layer can meet the process of preparing the MIM capacitor on the top metal interconnect structure of T2Mx type.

[0071] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any technician in the relevant technical field, without departing from the scope of the technical solution of the present invention, makes any form of equivalent replacement or modification to the technical solution and technical content disclosed in the present invention, which does not depart from the content of the technical solution of the present invention and still falls within the protection scope of the present invention.

Claims

1. A semiconductor device, characterized in that: include: A substrate having a dielectric layer thereon, wherein the dielectric layer has a gate structure and a plurality of top metal interconnect structures, each of which comprises at least two electrically connected metal interconnect layers; A groove extending from the top surface of the dielectric layer into the dielectric layer and located between adjacent top metal interconnect structures; A MIM capacitor structure is located in the trench and extends upward to be higher than the top surface of the dielectric layer, wherein a gap is provided between a sidewall of the MIM capacitor structure and a sidewall of the trench; An insulating layer covers the substrate and the MIM capacitor structure.

2. A semiconductor device according to claim 1, characterized in that: An obtuse angle is formed between the side wall of the groove and the bottom of the groove.

3. A semiconductor device according to claim 1, characterized in that: The depth of the groove is 4. A semiconductor device according to claim 1, characterized in that: The MIM capacitor structure comprises: A lower electrode plate, located in the groove and covering a portion of the bottom surface of the groove; A dielectric layer, located on the lower electrode plate and covering the upper surface of the lower electrode plate; The upper electrode plate is located on the dielectric layer and covers a portion of the dielectric layer.

5. A semiconductor device according to claim 4, characterized in that: Also includes: The metal wiring layer is located on the insulating layer and is electrically connected to the top metal interconnection structure, the upper electrode plate and the lower electrode plate through a plurality of electrical connectors.

6. A semiconductor device according to claim 1, characterized in that: The thickness of the insulating layer is 7. A method for preparing a semiconductor device, characterized in that: include: Providing a substrate, wherein the substrate has a dielectric layer, and the dielectric layer has a gate structure and a plurality of top metal interconnect structures, each of which includes at least two electrically connected metal interconnect layers; Etching the dielectric layer to form a groove, wherein the groove extends from the top surface of the dielectric layer into the dielectric layer, and the groove is located between adjacent top-layer metal interconnect structures; forming a MIM capacitor structure in the trench, wherein the MIM capacitor structure extends upward to a level higher than a top surface of the dielectric layer, wherein a gap exists between a sidewall of the MIM capacitor structure and a sidewall of the trench; An insulating layer is formed on the dielectric layer, wherein the insulating layer covers the MIM capacitor structure and the dielectric layer.

8. A method for preparing a semiconductor device according to claim 7, characterized in that: The steps of forming the MIM capacitor structure include: forming a stacked layer on the dielectric layer, the stacked layer covering the dielectric layer and the groove, the stacked layer comprising a first metal layer, a dielectric material layer and a second metal layer sequentially stacked on the dielectric layer; Etching away a portion of the stacked layers on the surface of the dielectric layer and in the groove, and the remaining first metal layer, the dielectric material layer and the second metal layer respectively constitute the lower plate, the dielectric layer and the upper plate of the MIM capacitor structure; The lower electrode plate covers part of the bottom surface of the groove, the dielectric layer covers the upper surface of the lower electrode plate, and the upper electrode plate covers part of the dielectric layer.

9. A method for preparing a semiconductor device according to claim 8, characterized in that: After forming the MIM capacitor structure, the method further includes: forming the insulating layer on the dielectric layer, wherein the insulating layer fills the groove and covers the dielectric layer and the MIM capacitor structure; performing a planarization process on the insulating layer; Etching the insulating layer to form an opening in the insulating layer to expose the top metal interconnect structure, the upper electrode plate and the lower electrode plate; A metal wiring layer is formed on the insulating layer and an electrical connection is formed in the opening. The metal wiring layer is electrically connected to the top metal interconnection structure, the upper electrode plate and the lower electrode plate through a plurality of the electrical connections.