A method and system for recovering refinery dry gas using metal organic framework materials
The use of metal organic framework materials to separate and recover refinery dry gas into olefin-rich and alkane-rich components, followed by steam cracking and activated carbon adsorption, addresses the inefficiencies of existing technologies, enhancing ethylene yield and reducing energy consumption.
Patent Information
- Application Number
- CN202011153072.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-10-26
AI Technical Summary
Existing methods for recovering refinery dry gas as ethylene raw material face challenges such as high energy consumption, low recovery rates, and inappropriate composition leading to increased energy consumption and cost in ethylene production, particularly due to the limitations of cryogenic separation, pressure swing adsorption, and oil absorption technologies.
A method using metal organic framework materials to separate refinery dry gas into olefin-rich and alkane-rich gases, followed by steam cracking and activated carbon adsorption to produce ethylene and propylene, optimizing the ethylene yield and reducing energy consumption.
The method achieves high recovery rates (>92%) of C2 hydrocarbons, reduces process energy consumption, and expands the ethylene raw material source while improving ethylene cracking yield and product purity.
Smart Images

Figure CN114478167B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of gas separation, and more particularly to a method and system for separating and recovering metal organic framework materials for refinery use. Background Art
[0002] Ethylene is the core of the petrochemical industry, and its output marks the development level of a country's petrochemical industry. In recent years, my country's ethylene production capacity has gradually increased. In 2018, my country's annual ethylene production was 18.41 million tons, ranking second in the world. As ethylene plants become larger and larger, the pressure on raw materials is increasing. Expanding the source of ethylene raw materials and reducing the cost of ethylene are the top priorities for ethylene technology researchers. Dry gas is a co-produced gas in the production process of refining and chemical plants. It has a large output and comes from more than 20 production processes. It is rich in light hydrocarbon resources such as hydrogen, ethylene, ethane, propylene, and propane. Before there was a suitable recovery technology, refinery dry gas was mainly used as fuel and burned, resulting in a huge waste of resources. Recovering components such as carbon two and carbon three in refinery dry gas to replace part of light oil as ethylene raw materials can increase the ethylene yield of the original light weight, while reducing process energy consumption, thereby reducing the production cost of ethylene. Therefore, as a cheap raw material, it is of great significance to develop a technology for separating and recovering refinery dry gas as an ethylene raw material.
[0003] At present, the main technologies for recovering dry gas from refineries include cryogenic separation, pressure swing adsorption and oil absorption. Cryogenic separation, also known as cryogenic distillation, is a low-temperature separation process. Its principle is to utilize the difference in relative volatility of each component in the raw material, condense each component in the dry gas according to the process requirements through gas turbine expansion refrigeration at low temperature, and then separate the various hydrocarbons in it one by one according to their boiling points by distillation. The cryogenic separation process is mature and has a high recovery rate of the target product, but the process has high energy consumption, complex process and large equipment investment. US502971 discloses a low-pressure and low-temperature concentration process for C2 hydrocarbons and heavier hydrocarbons suitable for the recovery of refinery dry gas. This process cancels the traditional high-pressure scheme and replaces it with low-pressure technology, so that the recovery temperature is above the nitric acid resin generation temperature, avoiding potential dangers and maintaining a high olefin yield, but the temperature is still below -100°C, so it still requires a large investment and high energy consumption. Pressure swing adsorption is to use the selectivity, adsorption characteristics and adsorption capacity of the adsorbent for different adsorbents to show differences with pressure changes to achieve the separation of the mixture. The process energy consumption of this method is low, but because the previous pressure swing adsorption technology uses traditional adsorption materials, the separation selectivity is relatively low. To achieve continuous operation, the process needs to switch between 6-10 towers, which makes the technology occupy a large area, difficult to operate, and the recovery rate of the process is low. CN107433107A has improved the process and adopted a two-stage concentration PSA adsorption separation process to make the methane concentration in the C2 enriched product gas lower than 4%, but the separation process is relatively complicated. The oil absorption technology uses the difference in solubility of the absorbent to each component in the mixed gas to achieve the separation of the mixed gas. Generally, the absorbent is first used to absorb C2 and above components, remove methane, hydrogen, nitrogen and other gas components in the dry gas, and then separate the components above C2 by distillation and recover the absorbent. This method is small in scale and low in investment, but the temperature of the intermediate cooling oil absorption separation process is still low, and the recovery rate is usually only about 85%. CN101638584A and CN109553504A developed shallow cooling oil dry gas concentration separation technology. The absorption temperature is higher than -20°C and water can be used as the refrigerant, which greatly reduces the energy consumption of the process. However, the purity and recovery rate of the purified gas of this technology need to be further improved.
[0004] At the same time, in terms of the composition characteristics of dry gas, it can be divided into saturated dry gas and unsaturated dry gas. Among them, the dry gas produced by the atmospheric and vacuum unit, hydrogenation unit and reforming unit is mainly saturated hydrocarbons, and the unsaturated olefin content of the dry gas produced by the catalytic cracking unit and delayed coking unit has increased significantly. In the previous dry gas separation and recovery technology used as ethylene raw material, ethylene-rich gas or ethane-rich gas was obtained by selecting dry gas from different sources and separating and concentrating it. Ethylene-rich gas enters the ethylene separation system to directly obtain ethylene products; ethane-rich gas is sent to the cracking furnace for cracking. However, in actual production, due to the limitations of existing raw gas sources and desulfurization devices, various companies generally have the problem of inappropriate concentration of concentrated gas. For ethylene-rich gas, the ethylene content in the concentrated ethylene-rich gas is currently low, mostly between 25-40%. However, the alkane components in the ethylene-rich gas need to pass through the compressor and separation system before returning to the cracking furnace. The higher alkane content in the olefin-rich gas leads to an increase in the energy consumption of the ethylene unit separation system. Even if the distillation method is used alone for rough separation, propylene refrigeration is still required, and the energy consumption is still high. As for ethane-rich gas, the olefin content in the ethane-rich gas obtained by concentration separation is more than 2%, and some enterprises have reached more than 10%. When the olefin content of the raw gas of the ethylene plant exceeds 2%, it is not suitable to be directly sent to the cracking furnace as ethylene raw material, otherwise it will cause serious coking in the convection section of the cracking furnace, greatly shortening the production cycle. To solve this problem, the current measure is to mix the obtained ethane-rich gas with other saturated light hydrocarbons for cracking, but this has caused an increase in the cost of ethylene raw materials and made it difficult to achieve optimized operation of the cracking furnace.
[0005] Due to the shortcomings of the above methods, developing a new method for separating and recovering refinery dry gas for use as ethylene feedstock, which can expand the source of ethylene feedstock while increasing olefin yield and reducing process energy consumption, is one of the problems to be solved urgently in this field. Summary of the invention
[0006] In order to achieve efficient recycling of refinery dry gas and solve the problems of excessive process energy consumption caused by inappropriate composition when using concentrated gas as ethylene raw material, the present invention provides a method for separating and recycling refinery dry gas using metal organic framework materials. This method processes refinery dry gas to obtain olefin-rich gas and alkane-rich gas at the same time. The alkane-rich gas is used as a raw material for cracking in an industrial cracking furnace, and the olefin-rich gas is separated by activated carbon and sent to an ethylene tower and a propylene tower to obtain olefin products. While expanding the source of ethylene raw materials, the ethylene yield is increased and the energy consumption of the ethylene separation process is reduced. The technology has a high recovery rate, low process energy consumption, and a simple process.
[0007] One of the purposes of the present invention is to provide a method for separating and recovering refinery dry gas using a metal organic framework material, comprising the following steps:
[0008] (1) contacting refinery dry gas with a suspension slurry of metal organic framework material A to obtain a C2 hydrocarbon concentrated gas and a gas phase mixture, wherein the C2 hydrocarbon concentrated gas contains C2 + Component concentration>95v%, C2 hydrocarbon recovery>92%;
[0009] (2) contacting the C2 hydrocarbon enriched gas with a metal organic framework material B to separate the olefin-rich gas and the alkane-rich gas;
[0010] (3) steam cracking the alkane-rich gas;
[0011] (4) The olefin-rich gas is contacted with activated carbon to separate into ethylene-rich gas and propylene-rich gas.
[0012] (5) The ethylene-rich gas and the propylene-rich gas are directly refined to obtain ethylene and propylene products respectively.
[0013] In the method of the present invention, in step (1), the metal organic framework material A is preferably selected from zeolite imidazolate framework structure materials, more preferably at least one selected from ZIF-8, ZIF-11, and ZIF-67;
[0014] The mass content of the metal organic framework material A in the suspension slurry is preferably 20 to 40%, more preferably 25 to 30%;
[0015] The solvent of the suspension slurry is water and an organic solvent; preferably, the molecular diameter of the organic solvent is larger than the window diameter of the metal organic framework material; more preferably, the organic solvent is ethylene glycol;
[0016] The ratio of water to organic solvent is preferably (3:1) to (6:1), more preferably (4:1) to (5:1);
[0017] The temperature at which the refinery dry gas contacts the suspension slurry of the metal organic framework material A is 274-300K, preferably 274-288K; the pressure is 0.1-3Mpa, preferably 0.5-2Mpa; and the gas-liquid volume ratio is 10-150, preferably 30-90.
[0018] Preferably, the step (1) may include the following steps:
[0019] (a) continuously contacting refinery dry gas with a suspension slurry of metal organic framework material A in reverse order to obtain a suspension slurry of C2 hydrocarbons and a gas phase mixture containing hydrogen, methane and nitrogen;
[0020] (b) flash evaporating the C2 hydrocarbon suspension slurry under reduced pressure, and returning the generated gaseous stream to counter-contact with the metal organic framework material A suspension slurry, and back-blowing out the components such as hydrogen that are not easily absorbed and adsorbed in the slurry;
[0021] (c) desorbing the suspended slurry obtained by flash evaporation under reduced pressure to separate it into a C2 hydrocarbon concentrate and a working slurry of the suspended metal organic framework material A;
[0022] (d) The working slurry of the suspended metal organic framework material A is returned to contact with the refinery dry gas for recycling.
[0023] Wherein, in the above steps, the pressure of the reduced pressure flash evaporation is lower than the contact pressure of the refinery dry gas and the suspension slurry of the metal organic framework material A and higher than the desorption pressure, preferably 0.5 to 1.5 MPa;
[0024] The desorption pressure is 0-0.5 MPa.
[0025] In the method of the present invention, in step (2), the metal organic framework material B is preferably at least one selected from FeMOF-74, CoMOF-74, MnMOF-74, and UTSA-280;
[0026] Preferably, the C2 hydrocarbon concentrated gas is separated by pressure swing adsorption by contacting it with a metal organic framework material B; wherein the pressure swing adsorption conditions preferably include: a temperature of 288 to 300 K, an adsorption pressure of 0.5 to 3.0 MPa, and a desorption pressure of 0 to 0.5 MPa.
[0027] In the method of the present invention, in step (3), the alkane-rich gas is used as a cracking furnace raw material for steam cracking.
[0028] In the method of the present invention, in step (3), the steam cracking method may specifically include heating the alkane-rich gas stream to a cracking reaction temperature, mixing with water vapor, and then performing a cracking reaction. The cracking reaction time is 0.05 to 0.6 seconds, preferably 0.05 to 0.5 seconds; the water-oil ratio is 0.2 to 0.8, preferably 0.3 to 0.4; and the cracking temperature is 1053 to 1163 K, preferably 1083 to 1133 K.
[0029] In the method of the present invention, in step (4), the activated carbon is a commercially available product;
[0030] The physical property parameters of the activated carbon are preferably that the specific surface area of the activated carbon is 500 to 1300 m 2 / g, more preferably 650 to 1050 m 2 / g; pore volume 0.2 to 0.9 ml / g, more preferably 0.4 to 0.7 ml / g;
[0031] Preferably, the olefin-rich gas is separated by pressure swing adsorption by contacting with activated carbon; wherein the adsorption conditions preferably include: temperature 288-300K, adsorption pressure 0.1-1.0MPa, and desorption pressure 0-0.5MPa.
[0032] In the method of the present invention, in step (5), the ethylene-rich gas and the propylene-rich gas are respectively refined by distillation towers, and the ethylene tower and the propylene tower are the ethylene distillation tower and the propylene distillation tower in the separation process of a classic ethylene device.
[0033] According to a preferred embodiment of the present invention, the method for recovering refinery dry gas may include the following steps:
[0034] (1) Metal-organic framework material absorption, adsorption, separation and recovery of C2: After desulfurization, the refinery dry gas is compressed and cooled, and then absorbed and adsorbed by metal-organic framework material A to obtain C2 + C2 hydrocarbon concentrate gas with component concentration>95v% and C2 hydrocarbon recovery rate>92% and a gas phase mixture rich in hydrogen, methane and nitrogen.
[0035] (2) Adsorption separation of olefins / alkanes by metal organic framework materials: The C2 hydrocarbon concentrated gas obtained in step (1) is fed into the adsorption separation device of metal organic framework material B to obtain olefin-rich gas and alkane-rich gas.
[0036] (3) Steam cracking of alkane-rich gas: The alkane-rich gas obtained in step (2) is used as an ethylene feedstock and introduced into an industrial cracking furnace to increase the ethylene yield of the ethylene plant.
[0037] (4) Separation of ethylene / propylene by activated carbon adsorption: The olefin-rich gas obtained in step (3) is fed into an activated carbon adsorption separation device to obtain ethylene-rich gas and propylene-rich gas.
[0038] (5) Production of ethylene and propylene: The ethylene-rich gas and propylene-rich gas obtained in step (4) are respectively fed into an ethylene tower and a propylene tower to obtain olefin products.
[0039] The second object of the present invention is to provide a system for recovering refinery dry gas from metal organic framework materials, which is used in the above method, comprising:
[0040] A C2 hydrocarbon enrichment unit configured to receive the refinery dry gas and discharge the C2 hydrocarbon enriched gas and a gas phase mixture;
[0041] an olefin / alkane separation unit configured to receive the C2 hydrocarbon enriched gas and discharge an olefin-rich gas and an alkane-rich gas;
[0042] a cracking unit configured to receive the alkane-rich gas and discharge cracked gas;
[0043] an ethylene / propylene separation unit configured to receive the olefin-rich gas and discharge ethylene-rich gas and propylene-rich gas;
[0044] an ethylene unit configured to receive the ethylene-rich gas and produce an ethylene product;
[0045] A propylene unit is configured to receive the propylene-rich gas and produce a propylene product.
[0046] The system is respectively equipped with pipelines connecting the C2 hydrocarbon concentration unit with the olefin / alkane separation unit, the olefin / alkane separation unit with the cracking unit, the ethylene\propylene separation unit, and the ethylene\propylene separation unit with the ethylene unit and the propylene unit, respectively.
[0047] In the present invention, the C2 hydrocarbon concentration unit includes an absorption adsorption tower, a flash tank and a desorption tower. The middle and lower part of the absorption adsorption tower is provided with a refinery dry gas inlet, and the top is provided with a suspended slurry inlet and a gas phase mixture outlet of the metal organic framework material A. The flash tank is connected to the bottom of the absorption adsorption tower through two pipelines, and the desorption tower is connected to the flash tank. The desorption tower is equipped with a pipeline connected to the absorption adsorption tower to return the working slurry of the suspended metal organic framework material A to the absorption adsorption tower, and a C2 hydrocarbon concentrated gas outlet.
[0048] Furthermore, the C2 hydrocarbon concentration unit may also include a gas booster and a liquid delivery pump. The gas booster is arranged on a pipeline connecting the flash tank and the absorption adsorption tower to return part of the adsorbed gas released from the flash tank to the bottom of the absorption adsorption tower, and the liquid delivery pump is arranged on the pipeline connecting the desorption tower and the absorption adsorption tower.
[0049] In the above C2 hydrocarbon concentration unit, the specific process flow can be shown as follows:
[0050] (i) The desulfurized refinery dry gas is compressed and cooled, and then sent to the middle and lower part of the absorption and adsorption tower, where it is continuously contacted with the working slurry of the suspended metal organic framework material A entering from the top of the absorption and adsorption tower to perform absorption, adsorption and separation, thereby obtaining a suspended slurry rich in C2 hydrocarbons at the bottom of the tower and a gas rich in hydrogen, methane and nitrogen at the top of the tower;
[0051] (ii) the C2 hydrocarbon-rich suspension slurry at the bottom of the tower enters the flash tank at the bottom of the tower for reduced pressure flash evaporation, and the generated gaseous stream returns to the absorption and adsorption tower to contact the working slurry of the suspended metal organic framework material A in reverse order, and back-blowing removes hydrogen and other components in the slurry that are not easily absorbed or adsorbed;
[0052] (iii) the suspended slurry flowing out from the bottom of the flash tank enters a desorption tower, where it is decompressed and desorbed to separate into a C2 hydrocarbon concentrate gas and a working slurry of the suspended metal organic framework material A;
[0053] (iv) The working slurry of the suspended metal organic framework material A from the bottom of the desorption tower is returned to the top of the absorption tower for recycling.
[0054] In the system of the present invention, the olefin / alkane separation unit may include at least two adsorption towers, and a switching operating system is set between the adsorption towers to realize the adsorption and regeneration process. Generally, in the operation of an industrial pressure swing adsorption device, at least one adsorption tower is kept in the adsorption process, and other towers are in the process of equal pressure drop, inversion, equal pressure increase, etc., to ensure efficient gas recovery and adsorbent regeneration of the adsorbent.
[0055] In the system of the present invention, the cracking unit can be a typical tubular high-temperature steam cracking furnace, which includes a convection section, a radiation section, a waste heat boiler, etc.
[0056] In the system of the present invention, the ethylene / propylene separation unit may include at least two adsorption towers, which are provided with a switching operation system between the adsorption towers to realize the adsorption and regeneration process. Generally, in the operation of an industrial pressure swing adsorption device, at least one adsorption tower is kept in the adsorption process, and other towers are in the process of equal pressure drop, reverse, equal pressure increase, etc., to ensure efficient gas recovery and adsorbent regeneration of the adsorbent.
[0057] In the system of the present invention, the ethylene unit and the propylene unit can be selected from the ethylene tower and the propylene tower in the classical ethylene plant.
[0058] The present invention has no particular limitation on the above-mentioned devices, and common devices and equipment in the prior art in the art can be used.
[0059] Compared with the traditional method, the method of the present invention has the advantages of high efficiency, energy saving, economy, etc., and while expanding the source of ethylene devices, it improves the ethylene cracking yield and reduces process energy consumption. BRIEF DESCRIPTION OF THE DRAWINGS
[0060] Figure 1 It is a conceptual flow chart of the industrial application of the present invention for separating and recovering refinery dry gas.
[0061] in, Figure 1 Marking Description:
[0062] 1. C2 hydrocarbon concentration unit absorbed by metal organic framework material A; 2. Olefin / alkane separation unit separated by adsorption by metal organic framework material B; 3. Cracking unit; 4. Ethylene / propylene separation unit separated by adsorption on activated carbon; 5. Ethylene unit; 6. Propylene unit; 7. Raw gas; 8. C2 hydrocarbon concentration gas; 9. Gas phase mixture rich in hydrogen, methane and nitrogen; 10. Alkane-rich gas; 11. Olefin-rich gas; 12. Cracking gas; 13. Ethylene-rich gas; 14. Propylene-rich gas; 15. Ethylene product; 16. Propylene product.
[0063] Figure 1In the process, the raw gas 7 obtained by compressing and cooling the desulfurized refinery dry gas is sent to the C2 hydrocarbon concentration unit 1 absorbed by the metal organic framework material A to obtain a C2 hydrocarbon concentrated gas 8 logistics and a gas phase mixture 9 rich in hydrogen, methane and nitrogen. The C2 hydrocarbon concentration unit adopts the efficient metal organic framework material A absorption and adsorption separation technology to improve the recovery rate of carbon dihydrocarbons and reduce the energy consumption of the process at the same time; then the obtained C2 hydrocarbon concentrated gas 8 logistics (hydrocarbon mixture rich in C2 hydrocarbons) is sent to the olefin / alkane separation unit 2 for adsorption separation by the metal organic framework material B to obtain alkane-rich gas 10 and olefin-rich gas 11; the obtained alkane-rich gas 10 is passed into the cracking unit 3 to obtain cracking gas 12, so as to improve the ethylene yield of the ethylene device. The obtained olefin-rich gas 11 is sent to the ethylene / propylene separation unit 4 for adsorption separation of activated carbon to obtain ethylene-rich gas 13 and propylene-rich gas 14; the obtained ethylene-rich gas 13 is passed into the ethylene tower of the ethylene unit to obtain ethylene product 15; the obtained propylene-rich gas 14 is passed into the propylene tower of the propylene unit to obtain propylene product 16. This avoids the problem that the olefin content in the concentrated gas obtained in the previous dry gas recovery process is low, and the gas returns to the cracking furnace after passing through the compressor and separation system of the ethylene device, which increases the energy consumption of the separation system of the ethylene device. At the same time, part of the olefin products are directly produced through adsorption separation, which reduces energy consumption.
[0064] Figure 2 This is a conceptual flow chart of industrial application of the present invention using a metal organic framework material A suspension slurry to absorb, adsorb and separate a mixed gas.
[0065] in, Figure 2 Marking instructions: 17. Absorption tower; 18. Flash tank; 19. Desorption tower; 20. Gas booster; 21. Liquid delivery pump; 22. Fresh metal organic framework material A suspension slurry.
[0066] The suspension slurry of metal organic framework material A and raw gas 7 are reversely contacted in absorption and adsorption tower 17 for absorption-adsorption separation, and a large amount of C2 + The hydrocarbon suspension slurry is first flashed under reduced pressure in the flash tank 18, and part of the adsorbed gas is released and returned to the bottom of the absorption and adsorption tower 17 through the gas booster 20 to recover some of the hydrogen, methane, nitrogen and other components dissolved and adsorbed in the working liquid. The C2-rich gas flowing out from the bottom of the flash tank 18 + The hydrocarbon suspension slurry enters the desorption tower 19, where it is subjected to reduced pressure desorption, and the desorbed C2 concentrated gas 8 is discharged from the top of the desorption tower. At the same time, the obtained working slurry of the regenerated metal organic framework material A is sent back to the top of the absorption and adsorption tower together with the added fresh metal organic framework material A suspension slurry 22 through the liquid delivery pump 21. DETAILED DESCRIPTION
[0067] The present invention is described in detail below in conjunction with specific embodiments. It is necessary to point out that the following embodiments are only used to further illustrate the present invention and cannot be understood as limiting the scope of protection of the present invention. Some non-essential improvements and adjustments made to the present invention by those skilled in the art based on the contents of the present invention still fall within the scope of protection of the present invention.
[0068] The metal organic framework material and activated carbon in the embodiments of the present invention are commercially available.
[0069] In the present invention, HP6890 gas chromatograph equipped with CHEMSTATION chromatography workstation software is used to analyze the components of raw materials and products.
[0070] In the following examples and comparative examples, the dry gas raw materials are refinery dry gas 1 from a catalytic device and refinery dry gas 2 obtained from a saturated dry gas desulfurization device, and the compositions are shown in Table 1.
[0071] Table 1 Refinery dry gas composition
[0072] composition Refinery dry gas 1 (v%) Refinery dry gas 2 (v%) hydrogen 18.29 35.74 Nitrogen 15.82 3.81 Carbon monoxide 1.98 0 carbon dioxide 0.2 0 Methane 27.69 26.65 Ethylene 14.21 1.39 Ethane 16.27 20.96 Propylene 3.96 0.48 Propane 0.92 7.92 <![CDATA[C4 + ]]> 0.66 3.05
[0073] Example 1
[0074] 1-1. The following method is used to illustrate the method of absorbing, adsorbing, separating and recovering C2 hydrocarbons by the metal organic framework material A of the present invention.
[0075] The experiment was conducted using refinery dry gas 1 as the raw gas. The experimental process is shown in Figure 2 . The working slurry used is a water-ethylene glycol slurry in which ZIF-8 is suspended. The mass fraction of ZIF-8 is 25%, the ratio of water to ethylene glycol is 4:1, and the gas-liquid volume ratio is 45. The theoretical plate number of the absorption adsorption tower is 18, the operating pressure is 1MPa, and the temperature of the circulating working slurry entering the top of the absorption tower is 274.15K. The operating pressure of the flash tank is 0.7MPa, and the operation is adiabatically. The operating pressure of the desorption tower is 0.1MPa. The working slurry and the refinery dry gas are in reverse contact in the absorption adsorption tower 17 for absorption-adsorption separation. A large amount of C2 + The hydrocarbon suspension slurry is first flashed under reduced pressure in the flash tank 18, and part of the adsorbed gas is released and returned to the bottom of the absorption tower by the gas booster 20 to recover some of the hydrogen, methane, nitrogen and other components dissolved and adsorbed in the working liquid. The C2-rich gas flowing out from the bottom of the flash tank + The suspended slurry of hydrocarbons enters the desorption tower 19, where it is decompressed and desorbed. The desorbed C2 concentrated gas 8 is discharged from the top of the desorption tower. At the same time, the regenerated working slurry obtained is sent back to the top of the absorption tower together with the added fresh working slurry through the liquid delivery pump 21. The composition of the obtained desorbed gas is shown in Table 2. The recovery rate of C2 hydrocarbons is 95.73%.
[0076] Table 2 Desorption gas composition
[0077] composition Desorption gas (v%) Methane 3.11 Ethylene 39.42 Ethane 43.95 Propylene 8.27 Propane 3.63 <![CDATA[C4 + ]]> 1.62
[0078] 1-2. The following is used to illustrate the method for separating olefins / alkanes by adsorption of the metal organic framework material B of the present invention. UTSA-280 metal organic framework material is selected as the adsorbent, and a pressure swing adsorption process is adopted. Two adsorption beds filled with adsorbents are used, and the two adsorption beds are operated alternately to ensure that the raw gas can enter continuously. One adsorption bed is in the adsorption step, and the other bed is in the desorption step. The number of theoretical plates of the adsorption tower is 8, the operating temperature is 15°C, the adsorption pressure is 1.5MPa, and the desorption pressure is 0.05MPa. In the adsorption bed in the adsorption step, unsaturated hydrocarbons such as ethylene are easily adsorbed by the adsorbent, and alkane gases such as ethane that are not easily adsorbed are discharged from the top of the tower to obtain an alkane-rich gas flow. After the switching operation depressurizes the gas adsorbed in the bed and desorbs it, an olefin-rich gas flow is obtained. The composition of the obtained olefin-rich gas and alkane-rich gas is shown in Table 3.
[0079] Table 3 Composition of olefin-rich gas and alkane-rich gas
[0080] composition Olefin-rich gas (v%) Alkane-rich gas (v%) Methane 0.00 6.01 Ethylene 80.46 1.12 Ethane 2.15 82.95 Propylene 16.80 0.31 Propane 0.27 6.77 <![CDATA[C4 + ]]> 0.31 2.84
[0081] 1-3. The following is used to illustrate the steam cracking and separation method of the present invention. The separated alkane-rich gas is sent to a steam cracking device for cracking, with a residence time of 0.42s, a water-oil ratio of 0.4, a cracking cross section outlet temperature (COT) of 860°C, and an outlet pressure of 0.0919MPa. Under these process conditions, the yield of the main cracking product is shown in Table 4.
[0082] Table 4 Alkane-rich gas cracking main product yield
[0083] composition Cracking yield (wt%) hydrogen 7.08 Methane 9.84 Ethane 20.88 Ethylene 51.55 Acetylene 0.08 Propane 1.47 Propylene 3.19 Propylene+Propane 0.08 Butadiene 1.62 Other C4 0.49 benzene 0.80 C5~C9(except benzene) 2.92 Ethylene 51.55 Diene 54.74 triene 56.36 High Attachment 64.24
[0084] 1-4. The following is used to illustrate the method for separating ethylene / propylene by adsorption of activated carbon of the present invention. Activated carbon (with a specific surface area of 1015 m 2 / g, pore volume 0.62ml / g) as adsorbent, using pressure swing adsorption process, 2 adsorption beds filled with adsorbent, 2 adsorption beds are operated alternately to ensure that the raw gas can enter continuously, 1 adsorption bed is in the adsorption step, and the other bed is in the desorption step. The operating temperature of the adsorption tower is 25°C, the adsorption pressure is 0.5MPa, and the desorption pressure is 0.05MPa. In the adsorption bed in the adsorption step, propylene, propane and carbon four or above gases are adsorbed by the adsorbent, and ethylene and ethane gases that are not easily adsorbed are discharged from the top of the tower to obtain an ethylene-rich gas flow. After the switching operation to reduce the pressure and desorb the gas adsorbed in the bed, a propylene-rich gas flow is obtained. The composition of the obtained ethylene-rich gas and propylene-rich gas is shown in Table 5.
[0085] Table 5 Composition of ethylene-rich gas and propylene-rich gas
[0086] composition Ethylene-rich gas (v%) Propylene-rich gas (v%) Methane 0.00 0.00 Ethylene 97.40 0.00 Ethane 2.60 0.00 Propylene 0.00 96.67 Propane 0.00 1.55 <![CDATA[C4 + ]]> 0.00 1.78
[0087] 1-5. The ethylene-rich gas and the propylene-rich gas are respectively sent to the ethylene tower and the propylene tower to obtain ethylene and propylene products.
[0088] Example 2
[0089] 2-1. The following method is used to illustrate the method of absorbing, adsorbing, separating and recovering C2 hydrocarbons by the metal organic framework material A of the present invention.
[0090] The experiment was conducted using refinery dry gas 2 as the raw gas. The experimental process is shown in Figure 2 . The working slurry used is a water-ethylene glycol slurry in which ZIF-8 is suspended. The mass fraction of ZIF-8 is 30%, the ratio of water to ethylene glycol is 5:1, and the gas-liquid volume ratio is 68. The theoretical plate number of the absorption adsorption tower is 20, the operating pressure is 2MPa, and the temperature of the circulating working slurry entering the top of the absorption tower is 274.15K. The operating pressure of the flash tank is 0.9MPa, and the operation is adiabatically performed. The operating pressure of the desorption tower is 0.1MPa. The working slurry and the refinery dry gas are in reverse contact in the absorption adsorption tower 17 for absorption-adsorption separation. A large amount of C2 + The hydrocarbon suspension slurry is first flashed under reduced pressure in the flash tank 18, and part of the adsorbed gas is released and returned to the bottom of the absorption tower by the gas booster 20 to recover some of the hydrogen, methane, nitrogen and other components dissolved and adsorbed in the working liquid. The C2-rich gas flowing out from the bottom of the flash tank + The suspended slurry of hydrocarbons enters the desorption tower 19, where it is decompressed and desorbed. The desorbed C2 concentrated gas 6 is discharged from the top of the desorption tower. At the same time, the regenerated working slurry obtained is sent back to the top of the absorption tower together with the added fresh working slurry through the liquid delivery pump 21. The composition of the obtained desorbed gas is shown in Table 6. The olefin content is greater than 2%, which is not suitable for direct use as an ethylene raw material. The recovery rate of C2 hydrocarbons is 96.40%.
[0091] Table 6 Desorption gas composition
[0092] composition Desorption gas (v%) Methane 3.32 Ethylene 4.31 Ethane 65.22 Propylene 1.49 Propane 24.56 <![CDATA[C4 + ]]> 1.10
[0093] 2-2. The following is used to illustrate the method for adsorbing and separating olefins / alkanes by the metal organic framework material B of the present invention. CoMOF-74 metal organic framework material is selected as the adsorbent, and a pressure swing adsorption process is adopted. Two adsorption beds filled with adsorbents are used, and the two adsorption beds are operated alternately, one adsorption bed is in the adsorption step, and the other bed is in the desorption step. The number of theoretical plates of the adsorption tower is 12, the operating temperature is 15°C, the adsorption pressure is 2.0MPa, and the desorption pressure is 0.01MPa. In the adsorption bed in the adsorption step, unsaturated hydrocarbons such as ethylene are easily adsorbed by the adsorbent, and alkane gases such as ethane that are not easily adsorbed are discharged from the top of the tower to obtain an alkane-rich gas flow. After the switching operation depressurizes and desorbs the gas adsorbed in the bed, an olefin-rich gas flow is obtained. The composition of the obtained olefin-rich gas and alkane-rich gas is shown in Table 7.
[0094] Table 7 Composition of olefin-rich gas and alkane-rich gas
[0095] composition Olefin-rich gas (v%) Alkane-rich gas (v%) Methane 0.00 3.55 Ethylene 66.72 0.03 Ethane 7.17 69.20 Propylene 22.99 0.01 Propane 2.34 26.09 <![CDATA[C4 + ]]> 0.78 1.12
[0096] 2-3. The following is used to illustrate the steam cracking and separation method of the present invention.
[0097] The separated alkane-rich gas was sent to the steam cracking unit for cracking, with a residence time of 0.26s, a water-oil ratio of 0.4, a cracking cross section outlet temperature (COT) of 855°C, and an outlet pressure of 0.189MPa. Under these process conditions, the yield of the main cracking product is shown in Table 8.
[0098] Table 8 Alkane-rich gas cracking main product yield
[0099]
[0100]
[0101] 2-4. The following is used to illustrate the method for separating ethylene / propylene by adsorption of activated carbon of the present invention. Activated carbon (with a specific surface area of 1015 m 2 / g, pore volume 0.62ml / g) as adsorbent, using pressure swing adsorption process, 2 adsorption beds filled with adsorbent, 2 adsorption beds are operated alternately to ensure that the raw gas can enter continuously, 1 adsorption bed is in the adsorption step, and the other bed is in the desorption step. The operating temperature of the adsorption tower is 25°C, the adsorption pressure is 0.5MPa, and the desorption pressure is 0.05MPa. In the adsorption bed in the adsorption step, propylene, propane and carbon four or above gases are adsorbed by the adsorbent, and ethylene and ethane gases that are not easily adsorbed are discharged from the top of the tower to obtain an ethylene-rich gas flow. After the switching operation to reduce the pressure and desorb the gas adsorbed in the bed, a propylene-rich gas flow is obtained. The composition of the obtained ethylene-rich gas and propylene-rich gas is shown in Table 9.
[0102] Table 9 Composition of ethylene-rich gas and propylene-rich gas
[0103] composition Ethylene-rich gas (v%) Propylene-rich gas (v%) Methane 0.00 0.00 Ethylene 90.30 0.00 Ethane 9.70 0.00 Propylene 0.00 88.05 Propane 0.00 8.96 <![CDATA[C4 + ]]> 0.00 2.99
[0104] 2-5. The ethylene-rich gas and the propylene-rich gas are respectively sent to the ethylene tower and the propylene tower to obtain ethylene and propylene products.
[0105] Comparative Example 1
[0106] The shallow cold oil absorption process is used to recover the refinery dry gas, and the refinery dry gas 1 is used as the raw gas. The composition of the raw gas is shown in Table 1.
[0107] The raw gas is compressed and cooled before being sent to the absorption tower, where it contacts the countercurrent butane absorbent to absorb the C2 + The absorption liquid in the tower bottom enters the desorption tower for desorption to obtain the recovered C2 + Hydrocarbon fraction. The absorption tower has 40 theoretical plates, the absorption temperature is -10°C, and the absorption pressure is 2.0 MPa. The composition of the obtained C2 fraction gas is shown in Table 10, and the C2 hydrocarbon recovery rate is 92.10%. The obtained C2 hydrocarbon concentrated gas is sent to the cracking gas compressor of the ethylene unit and enters the separation system for separation.
[0108] Table 10C2 fraction product gas composition
[0109] composition C2 fraction gas (v%) Methane 4.43 Ethylene 38.91 Ethane 42.74 Propylene 7.57 Propane 4.60 <![CDATA[C4 + ]]> 1.75
[0110] By comparing Example 1 with Comparative Example 1, it can be seen that the present invention uses a highly efficient metal organic framework material suspension slurry for absorption and adsorption, and the separation efficiency is higher.
[0111] The obtained C2 hydrocarbon concentrated gas is sent to the cracking gas compressor of the ethylene unit and enters the separation system for separation. The concentrated gas contains 38.91% ethylene, 42.74% ethane and 7.57% propane. This alkane component, which is greater than 50%, needs to be sent to the compressor and the ethylene deep cold separation system for separation together with the ethylene component. The obtained ethane and propane gas are then returned to the cracking furnace as cracking raw materials. The total energy consumption of compression and deep cold separation of unit raw materials is 3.95GJ. In the present invention, the energy consumption of obtaining olefin-rich gas and alkane-rich gas by adsorption of metal organic framework materials is only 850MJ / t raw material. The separation energy consumption of the present invention is significantly reduced.
[0112] Comparative Example 2
[0113] Tables 11, 12 and 13 show the physical properties of several naphtha, light naphtha and liquefied gas raw materials and their steam cracking product yields.
[0114] Table 11 Physical properties of atmospheric and vacuum naphtha and light naphtha
[0115]
[0116] Table 12 Composition of atmospheric and vacuum liquefied gas
[0117] raw material Atmospheric and vacuum liquefied gas (wt%) hydrogen 0.00 carbon dioxide 0.16 Carbon monoxide 0.00 Methane 0.26 Ethane 2.64 Ethylene 0.06 Propane 36.28 Propylene 0.08 Isobutane 15.35 n-Butane 39.98 Butene 0.33 n-Pentane 4.86 Isopentane 0.11 Methylcyclopentane 0.11 Cyclopentane + isohexane 0.00 n-Hexane 0.00 Cyclohexane 0.00 Isoheptane 0.00 benzene 0.00
[0118] Table 13 Cracked main product yield
[0119]
[0120] Comparing Comparative Example 2 with Example 1 and Example 2, when the alkane-rich gas obtained by the present invention is subjected to steam cracking, the yields of the main products such as ethylene, dienes, trienes and high value-added products in the cracking products are significantly higher than those of naphtha, light naphtha and liquefied gas raw materials. Therefore, the alkane-rich gas separated and recovered by the present invention can replace naphtha, light naphtha or liquefied gas as an ethylene raw material, while reducing the raw material cost, while increasing the yield of the main products such as ethylene.
Claims
1. A method for recovering refinery dry gas using metal organic framework materials, The following steps are involved: (1) contacting the refinery dry gas with the suspension slurry of the metal organic framework material A to obtain a C2 hydrocarbon concentrated gas and a gas phase mixture, wherein the C2 hydrocarbon concentrated gas contains C2 + Component concentration>95v%, C2 hydrocarbon recovery>92%; (2) contacting the C2 hydrocarbon concentrated gas with a metal organic framework material B to perform pressure swing adsorption separation to obtain olefin-rich gas and alkane-rich gas; (3) steam cracking the alkane-rich gas; (4) contacting the olefin-rich gas with activated carbon to separate into ethylene-rich gas and propylene-rich gas; (5) directly refining the ethylene-rich gas and the propylene-rich gas to obtain ethylene and propylene products respectively; The metal organic framework material A is selected from at least one of ZIF-8, ZIF-11, and ZIF-67; the solvent of the suspension slurry is water and an organic solvent, and the organic solvent is ethylene glycol; the ratio of water to the organic solvent is (3:1) to (6:1); the metal organic framework material B is selected from at least one of CoMOF-74 and UTSA-280; the specific surface area of the activated carbon is 500 to 1300 m 2 / g, pore volume is 0.2~0.9ml / g; The step (1) comprises: (a) continuously contacting refinery dry gas with a suspension slurry of metal organic framework material A in reverse order to obtain a suspension slurry of C2 hydrocarbons and a gaseous mixture containing hydrogen, methane and nitrogen; (b) flashing the suspension slurry of C2 hydrocarbons under reduced pressure, and returning the generated gaseous stream to contact the suspension slurry of metal organic framework material A in reverse order; (c) desorbing the suspension slurry obtained by flashing under reduced pressure to separate it into a C2 hydrocarbon concentrated gas and a working slurry of suspended metal organic framework material A; (d) returning the working slurry of suspended metal organic framework material A to contact with refinery dry gas for recycling; In step (2), the pressure swing adsorption separation conditions include: temperature of 288-300K, adsorption pressure of 1.5-2.0MPa, and desorption pressure of 0-0.5MPa.
2. The method for recovering refinery dry gas according to claim 1, Features: The mass content of the metal organic framework material A in the suspension slurry is 20-40%; and / or, The ratio of water to organic solvent is (4:1) to (5:1).
3. The method for recovering refinery dry gas according to claim 2, Features: The mass content of the metal organic framework material A in the suspension slurry is 25-30%.
4. The method for recovering refinery dry gas according to claim 1, Features: In step (1), the contact temperature is 274-300K; the pressure is 0.1-3Mpa; and the gas-liquid volume ratio is 10-150.
5. The method for recovering refinery dry gas according to claim 4, Features: The contact temperature is 274-288K; the pressure is 0.5-2Mpa; and the gas-liquid volume ratio is 30-90.
6. The method for recovering refinery dry gas according to claim 1, Features: In step (3), the cracking reaction time is 0.05-0.6 s; the water-oil ratio is 0.2-0.8; and the cracking temperature is 1053-1163 K.
7. The method for recovering refinery dry gas according to claim 6, Features: The cracking reaction time is 0.05-0.5s; the water-oil ratio is 0.3-0.4; and the cracking temperature is 1083-1133K.
8. The method for recovering refinery dry gas according to claim 1, Features: In step (4), the specific surface area of the activated carbon is 650 to 1050 m 2 / g; pore volume is 0.4~0.7ml / g.
9. The method for recovering refinery dry gas according to claim 1, Features: In step (4), the olefin-rich gas is separated by pressure swing adsorption by contacting it with activated carbon.
10. The method for recovering refinery dry gas according to claim 9, Features: The adsorption separation conditions include: temperature of 288-300K, adsorption pressure of 0.1-1.0MPa, and desorption pressure of 0-0.5MPa.
11. The method for recovering refinery dry gas according to claim 1, Features: The pressure of the reduced pressure flash evaporation is lower than the pressure at which the refinery dry gas contacts the suspension slurry of the metal organic framework material A and is higher than the pressure of desorption; and / or, The desorption pressure is 0-0.5 MPa.
12. The method for recovering refinery dry gas according to claim 11, Features: The pressure of the reduced pressure flash evaporation is 0.5-1.5 MPa.
Citation Information
Patent Citations
Method for separating catalytic dry gas in refinery by using shallow cold oil absorption method
CN101638584A
Two-stage PSA method for recovering C2+ from refinery dry gas according to concentration
CN107433107A
Method for separating ethane and ethylene in mixed gas
CN103058810A
Refinery mixed dry gas recovery system and recovery method
CN104557384A
Process for separating ethene by catalytic cracking and dry gas adsorption
CN1073422A