A method for preparing similar materials in loose granular formations
By using materials such as giant quartz sand and barite powder, similar materials suitable for loose granular formations are prepared, which solves the error problem of traditional simulation materials in simulating loose granular formations, achieving high similarity and stability, and is suitable for For foundation pit, tunnel excavation and seepage tests.
Patent Information
- Application Number
- CN202210096484.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-26
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-01-26
AI Technical Summary
Similar materials used to simulate loose granular formations in traditional model tests cannot effectively simulate the discrete type, stress transfer and permeability of graded particles, resulting in large errors in test results, and the materials are prone to physical or chemical changes after being immersed in water, resulting in The deviation is serious.
Giant-grained quartz sand is used as the skeleton material, and coarse-grained quartz sand and barite powder are used as gap filling and cementing materials. By adjusting the material ratio and water content, similar materials of suspended dense type, skeleton void type and skeleton dense type are prepared. Meet the characteristics of discontinuity, discreteness and high permeability of the formation, and adjust the performance parameters according to the test type.
It achieves high-similarity simulation of loose granular formations, reduces test errors, improves the reusability and cost-effectiveness of materials, and maintains stability in seepage tests.
Smart Images

Figure CN114487348B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of material model tests, in particular to a method for preparing similar materials of loose granular formations. Background Art
[0002] Model tests can reduce the natural prototypes to be observed, shorten the observation process, and isolate certain factors in the extraction process, making it easier to compare, observe, and discover their cause-and-effect relationships. In recent years, with the increase in the number of tunnels and foundation pits in loose granular formations such as pebbles and sand pebbles, there are more and more problems that need to be studied in loose granular formations, and model tests for loose granular formations are also increasing. Loose granular formations are composed of boulders, pebbles, medium-coarse sand, and soil of different particle sizes. They have special properties such as large permeability, strong discreteness, not easy to deform, poor cementation, and large changes in gradation composition. In traditional model tests, gypsum, PbO powder, bentonite, clay, river sand, iron powder, vaseline, paraffin, water, and other materials are usually used to make relatively homogeneous similar materials as rock formations or soil formations in model tests, and relevant stress and deformation test model tests are carried out.
[0003] These materials are ideal for simulating relatively homogeneous rock formations, clay and loess formations. However, in model tests of tunnels, foundation pits and seepage dewatering in loose granular formations, traditional similar materials have major defects, mainly manifested as follows: (1) They are unable to simulate the discrete type of graded particles in loose granular formations, resulting in errors in the overall deformation and stress transfer of the formations; (2) They are unable to simulate the progressive destruction of loose granular formations in unsupported or weakly supported forms after tunnel or foundation pit excavation; (3) The permeability coefficient of such materials is difficult to meet the similarity ratio requirements in seepage model tests, and the materials are prone to physical or chemical changes after immersion in water, resulting in serious deviations in the test results.
[0004] Therefore, when selecting similar materials to loose granular formations, it is necessary to consider the formation grading composition characteristics and structural performance characteristics to simulate the non-continuity, discreteness, high permeability, weak cementation and other characteristics of this type of formation structure. Only when these conditions are met can reliable test results be obtained. Summary of the invention
[0005] In order to overcome the shortcomings of formation similar materials in traditional model tests in simulating loose granular formations, the present invention provides a loose granular formation similar material and introduces its adjustment method in different tests. It has the characteristics of high similarity, simple preparation, large adjustment range, wide application range and reusability.
[0006] The present invention is achieved through the following technical solutions:
[0007] A similar material of loose granular formation, including coarse-grained material used as a skeleton, coarse-grained material group used as filling and filling gaps, and fine-grained material group used as filling cementation.
[0008] The coarse-grained material is 2-4 mesh quartz sand; the coarse-grained group includes 10-20 mesh quartz sand and 20-40 mesh quartz sand; the fine-grained group includes 150 mesh barite powder and 600 mesh barite powder.
[0009] Preferably, the similar materials include suspended dense formation similar materials, skeleton void type formation similar materials and skeleton void type formation similar materials.
[0010] Preferably, the suspended dense formation similar material includes, by mass percentage, 5% to 10% of 2 to 4 mesh quartz sand, 10% to 20% of 10 to 20 mesh quartz sand, 15% to 25% of 20 to 40 mesh quartz sand, 20% to 30% of 150 mesh barite powder and 25% to 35% of 600 mesh barite powder;
[0011] The skeleton void type stratum similar material includes, by mass percentage, 30% to 40% of 2 to 4 mesh quartz sand, 30% to 40% of 10 to 20 mesh quartz sand, 5% to 15% of 20 to 40 mesh quartz sand, 5% to 15% of 150 mesh barite powder and 5% to 15% of 600 mesh barite powder;
[0012] The skeleton dense formation similar material includes, by mass percentage, 20-30% of 2-4 mesh quartz sand, 20-30% of 10-20 mesh quartz sand, 0.5-5% of 20-40 mesh quartz sand, 20%-30% of 150 mesh barite powder and 20%-30% of 600 mesh barite powder.
[0013] A method for preparing similar materials in loose granular formations, comprising the following steps:
[0014] Step 1, determining similar material types according to the gradation composition of the loose granular formation;
[0015] Step 2: prepare a set amount of mixed dry material sample according to the proportion corresponding to the similar material type, adjust the water content of the mixed dry material sample to make it the same as the water content of the loose granular formation, and obtain the mass percentage of water in the similar material;
[0016] Step 3, determining the geometric similarity ratio between the loose granular formation and the similar material determined in step 1;
[0017] Step 4: set the performance parameters of the similar material according to the test type, compare the performance parameter similarity ratio and geometric similarity ratio of the similar material and the loose granular formation, and adjust the mass percentage of each material in the coarse-grained group or the fine-grained group in the similar material sample according to the comparison result, so that the performance of the similar material reaches the set performance parameters of the similar material, and obtain the mass percentage of each component in the similar material;
[0018] Step 5: Prepare similar materials according to the total amount of similar materials required by the test and in combination with the mass percentage of each component in the similar materials obtained in step 4 and the mass percentage of water.
[0019] Preferably, in step 1, the gradation composition of the loose granular stratum is determined based on the exploration data of the loose granular stratum.
[0020] Preferably, the method for determining the geometric similarity ratio in step 4 is as follows:
[0021] According to the average diameter of the giant particle group in the loose granular formation and the average diameter of the giant particle material in the similar material, the particle size similarity ratio between the loose granular formation and the similar material is calculated, and then the geometric similarity ratio between the loose granular formation and the similar material is determined based on the particle size similarity ratio and economic indicators.
[0022] Preferably, when conducting mechanical and deformation simulation tests, the performance parameters are elastic modulus E and cohesion c.
[0023] Preferably, the elastic modulus E and cohesion c are adjusted as follows:
[0024] The elastic modulus E is adjusted in the following manner: the overall content of the coarse-grained group remains unchanged, and the mass content of the quartz sand of 10 to 20 meshes and the quartz sand of 20 to 40 meshes in the coarse-grained group is adjusted according to a predetermined increase or decrease percentage;
[0025] The method for adjusting the cohesion c is to keep the overall content of the fine-grained group unchanged and adjust the mass content of the 600-mesh barite powder and the 150-mesh barite powder in the fine-grained group according to a predetermined increase or decrease percentage;
[0026] Preferably, when conducting a model test of seepage and precipitation in loose granular formations, the performance parameter is the permeability coefficient k.
[0027] Preferably, the method for adjusting the permeability coefficient is as follows:
[0028] The overall content of the coarse-grained group is kept unchanged, and the mass content of 10-20 mesh quartz sand and 20-40 mesh quartz sand in the coarse-grained group is adjusted according to a predetermined increase or decrease percentage.
[0029] Compared with the prior art, the present invention has the following beneficial technical effects:
[0030] The present invention provides a similar material for loose granular formations. The properties of loose granular formations are quite different from those of rock and soil media, mainly manifested in large porosity, high deformation modulus, large internal friction angle and small cohesion, resulting in surrounding rock deformation mainly caused by the dislocation between particles. The particle grading that satisfies the similarity principle is the key to achieving the simulation effect. Large-particle quartz sand is used as the skeleton material, medium-particle quartz sand is used as the filling material, and small-particle barite powder is used as the cementing material. The characteristics of loose granular formations can be highly restored, and the simulation of the non-continuity, discreteness, high permeability, weak cementation and other characteristics of this type of formation structure can be achieved.
[0031] Furthermore, similar materials are divided into three types according to the gradation composition of the stratum, and the specific component content is given for each material. The composition of the similar material itself is equivalent to a reduction in the diameter of the loose granular stratum. It is naturally similar to the actual stratum in many dimensionless parameters (gravity, porosity, Poisson's ratio), and its similarity coefficient can be achieved to be 1, which makes the similar material have the advantages of high similarity, simple preparation, strong adjustability, low production and use cost, and reusability.
[0032] The present invention also provides a method for preparing similar materials of the above-mentioned loose granular formation. According to different tests, different performance parameters are selected, and the performance parameter similarity ratio and geometric similarity ratio of the similar materials and the loose granular formation are compared. According to the comparison results, the relative content percentage of the internal materials of the coarse-grained group or the fine-grained group in the similar material sample is adjusted to achieve the similarity between the model and the prototype in terms of elastic modulus, cohesion, internal friction angle, permeability coefficient, etc. After determining the final mix ratio of the basic sample, the materials can be batch mixed and tested. The similar material of the loose granular formation has the advantages of high similarity, simple preparation, strong adjustability, low production and use costs, and reusability. It can be used for foundation pit and tunnel excavation destruction tests, formation stress and deformation research tests, and precipitation and permeability tests in such formations, and realizes the simulation of the characteristics of non-continuity, discreteness, high permeability, weak cementation, etc. in such formation structures. Further, the similar material has good water stability, can well achieve the adjustment of water content, and can maintain stability in the seepage process in the seepage test.
[0033] Furthermore, the similar materials can be reused in different tests by using different material ratios, which is low in cost and does not require special mixing processes and mixing equipment during the mixing process. After the ratios of various materials are determined in indoor tests, they can be mixed manually or with a small mixer according to the mass ratio. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1The present invention provides an embodiment of a method for preparing and adjusting loose granular formation similar materials in two common model tests (mechanical and deformation model test and seepage and precipitation model test).
[0035] Figure 2 The change of the arch crown sinking during the tunnel excavation process in the model test provided in the first embodiment of the present invention. DETAILED DESCRIPTION
[0036] The present invention will be further described in detail below in conjunction with the accompanying drawings, which are intended to explain the present invention rather than to limit it.
[0037] A similar material for a loose granular stratum is divided into a suspended dense stratum similar material, a skeleton void stratum similar material and a skeleton dense stratum similar material according to the stratum gradation composition. Considering that the properties of the loose granular stratum are quite different from those of rock and soil media, which are mainly manifested in large porosity, high deformation modulus, large internal friction angle and small cohesion, the deformation of the surrounding rock is mainly caused by the dislocation between particles. The particle gradation satisfying the similarity principle is the key to achieving the simulation effect. Therefore, quartz sand and barite powder of different mesh sizes are used as basic similar materials for the loose granular stratum in each stratum similar material, including giant particles used as a skeleton, coarse particles as filling and interstitial filling, and fine particles as filling and cementation.
[0038] The coarse-grained material is 2-4 mesh quartz sand; the coarse-grained group includes 10-20 mesh quartz sand and 20-40 mesh quartz sand; the fine-grained group includes 150 mesh barite powder and 600 mesh barite powder. The suspended dense formation similar materials, by mass percentage, include 5%-10% 2-4 mesh quartz sand, 10%-20% 10-20 mesh quartz sand, 15%-25% 20-40 mesh quartz sand, 20%-30% 150 mesh barite powder and 25%-35% 600 mesh barite powder.
[0039] Preferably, the suspended dense formation similar material includes, by mass percentage, 10.7% 2-4 mesh quartz sand, 14.8% 10-20 mesh quartz sand, 20.8% 20-40 mesh quartz sand, 25.3% 150 mesh barite powder and 28.4% 600 mesh barite powder.
[0040] Materials similar to skeleton void type formations include, by mass percentage, 30% to 40% of 2-4 mesh quartz sand, 30% to 40% of 10-20 mesh quartz sand, 5% to 15% of 20-40 mesh quartz sand, 5% to 15% of 150 mesh barite powder and 5% to 15% of 600 mesh barite powder.
[0041] Preferably, the skeleton void type formation similar material includes, by mass percentage, 35.7% of 2-4 mesh quartz sand, 34.8% of 10-20 mesh quartz sand, 9.7% of 20-40 mesh quartz sand, 10.5% of 150 mesh barite powder and 9.3% of 600 mesh barite powder.
[0042] Materials similar to skeleton-dense strata include, by mass percentage, 20-30% of 2-4 mesh quartz sand, 20-30% of 10-20 mesh quartz sand, 0.5-5% of 20-40 mesh quartz sand, 20%-30% of 150 mesh barite powder and 20%-30% of 600 mesh barite powder.
[0043] Preferably, the skeleton-dense formation similar material includes, by mass percentage, 25.3% of 2-4 mesh quartz sand, 25.1% of 10-20 mesh quartz sand, 1.2% of 20-40 mesh quartz sand, 24.6% of 150 mesh barite powder and 23.8% of 600 mesh barite powder.
[0044] The weight distribution of the above similar materials is 1.98~2.18g / cm 3 , which can basically achieve the consistency of the gravity of all loose granular formations and satisfy the gravity similarity constant C γ = 1. Secondly, the permeability coefficient distribution of similar materials is 5.2×10 -5 ~2.1×10 -4 , which can basically simulate the permeability of all loose granular formations and satisfy the similarity constant of permeability coefficient C k =Requirement of 5 to 10.
[0045] Table 1 shows the mass percentage content of each material in similar material formulas 1-12 of the present invention.
[0046] Table 1
[0047]
[0048]
[0049] The following is a detailed description of the preparation method of similar materials in the above loose granular formation, including the following steps:
[0050] Step 1: Obtain parameter information of loose granular strata based on the exploration data of loose granular strata.
[0051] Specifically, before the experiment is carried out, based on the stratigraphic exploration data obtained at the engineering site, the information on the grading composition, water content, elastic modulus, cohesion, internal friction angle, and permeability coefficient of loose particles is analyzed to obtain the basic information for preparing similar materials.
[0052] Step 2: Determine the type of similar material according to the grading composition of the loose granular formation, prepare a set amount of mixed dry material sample according to the corresponding ratio of the similar material type, and then adjust the water content of the mixed dry material to make it the same as the water content of the loose granular formation, so as to determine the mass percentage of water in the similar material.
[0053] Specifically, the type of similar material preliminarily determines the mass percentage of quartz sand materials and barite powder of different mesh sizes in the similar materials. For example, if the type of similar material is skeleton void type formation similar material, a mixed dry material sample of predetermined mass is prepared according to the corresponding mass percentage and geometric similarity ratio of each material. In the present embodiment, a total amount of 5 kg of samples is prepared. In the preparation of the samples, the weight of quartz sand materials of different mesh sizes and barite powder of different mesh sizes are strictly weighed on a scale according to the weight content of each material, and the samples are put together and stirred evenly to obtain a uniformly mixed dry material.
[0054] Then add a certain amount of water to the dry material and stir it evenly to form a wet material. Add the wet material to the test mold evenly in 2 to 3 times, and tamp the test mold gradually. After the wet material solidifies, slowly demold the test block. Obtain the moisture content w of the sample through indoor tests, compare its moisture content with the moisture content of the loose granular formation, and repeatedly adjust the amount of water added in the mixed dry material to make the moisture content of the sample the same as that of the loose granular formation. Record the total amount of water added and calculate the mass percentage of water in the entire sample m w / 5.
[0055] The composition of the similar material itself is equivalent to a reduction of the loose granular formation. It is naturally similar to the actual formation in many dimensionless parameters (gravity, porosity, Poisson's ratio), and its similarity coefficient can be 1. According to the similarity ratio relationship, the strain ε, Poisson's ratio μ, and internal friction angle can be obtained. The similarity ratio of dimensionless parameters such as porosity p is equal to the similarity ratio of water content and equal to 1, that is,
[0056] Step 3: Determine the geometric similarity ratio between the loose granular formation and similar materials.
[0057] According to the particle gradation distribution of loose granular strata, the structural form of loose granular strata is clarified, and the average diameter (d) of the giant particle group in the loose granular strata is compared with the average diameter (d) of the giant particle material in similar materials. m ) ratio, and calculate the particle size similarity ratio between loose granular formation and similar materials Then, based on this ratio, the geometric similarity ratio between the loose granular formation and similar materials is determined by comprehensively considering the feasibility and economy of the test. Based on the geometric similarity ratio and the size of the test chamber, determine the total amount of similar materials required for the test.
[0058] Step 4: Select different performance parameters according to the test type, and adjust the relative content percentage of each component in the coarse particle group or fine particle group in the similar material sample according to the performance requirements of the test, so that the performance of the similar material meets the performance requirements of the test.
[0059] Model tests include two categories: mechanical and deformation simulation tests, and model tests of formation seepage and precipitation.
[0060] In mechanical and deformation simulation tests, it is necessary to adjust the elastic modulus E and cohesion c of similar materials.
[0061] In model tests of formation seepage and precipitation, it is necessary to adjust the permeability coefficient k of similar materials.
[0062] The performance adjustment process of similar materials in two simulation tests is described in detail below.
[0063] 1. Adjustment of elastic modulus E and cohesion c of adjacent materials in mechanical and deformation simulation tests. In the model tests of foundation pit and tunnel mechanics and deformation in loose granular strata, the main similarity relationships considered include the following:
[0064] The similarity relationship between stress σ, bulk density γ and geometry L is: σ =C γ C L ;
[0065] The similarity relationship between stress σ, strain ε and elastic modulus E satisfies: C σ =C E C ε ;
[0066] The similarity relationship between cohesion c, geometry L and bulk density γ satisfies: C c =C L C γ
[0067] In general, in the experiment, as long as the elastic modulus and cohesion similarity ratio between the similar material and the loose granular formation are equal to the geometric similarity ratio obtained in step 3, C E =C c =C L (The maximum allowable error is ±0.1), and other similarity ratio relationships can be determined as follows:
[0068] Obtain the initial values of the elastic modulus E and cohesion c of the specimen prepared from similar materials in step 2.
[0069] Specifically, in the model test of the mechanics and deformation of loose granular formations, the initial values of the elastic modulus E and cohesion c of similar samples are obtained through indoor direct shear tests and compression tests, and the obtained elastic modulus and cohesion are compared with the corresponding values of the loose granular formation, respectively, to obtain the corresponding similarity ratio, and then the obtained similarity ratio is compared with the geometric similarity ratio obtained in step 2. If the comparison results are equal, the elastic modulus E and cohesion c of the similar material samples meet the requirements, otherwise they do not meet the requirements.
[0070] When the elastic modulus E of the similar material sample does not meet the requirements, the mass content of 10-20 mesh quartz sand and 20-40 mesh quartz sand in the coarse particle group is adjusted according to the predetermined increase or decrease percentage while keeping the overall content of the coarse particle group unchanged, and the sample of the similar material is re-prepared according to step 2 until the elastic modulus E and cohesion c of the similar sample meet the requirements of the simulation test.
[0071] Specifically, when the elastic modulus E is too small, the mass content of 20-40 mesh quartz sand is increased by 1% by mass, and at the same time, the mass content of 10-20 mesh quartz sand is reduced by 1% by mass. Each time the mass is adjusted, the sample is re-prepared according to the method in step 2 until it meets the simulation test requirements.
[0072] When the elastic modulus E is too large, the mass content of quartz sand of 20 to 40 meshes is reduced by 1% by mass, and at the same time, the mass content of quartz sand of 10 to 20 meshes is increased by 1% by mass.
[0073] When the cohesion c of similar material samples does not meet the requirements, it can be achieved by adjusting the mass content of 600 mesh barite powder and 150 mesh barite powder in the fine particle group while keeping the overall content of the fine particle group unchanged.
[0074] Specifically, when the cohesion c is too small, the mass content of the 600-mesh barite powder is increased by 1% by mass, and at the same time, the mass content of the 150-mesh barite powder is reduced by 1% by mass;
[0075] When the cohesion c is too large, the mass content of the 600-mesh barite powder is reduced by 1% by mass, and at the same time, the mass content of the 150-mesh barite powder is increased by 1% by mass.
[0076] When the performance of similar materials meets the requirements, similar materials required for the simulation test are prepared according to the mass percentage of each material and the required total amount. After the similar materials are prepared, they are packed and sensors are arranged according to the test requirements to carry out the test and study the formation damage characteristics, formation displacement field, stress field change laws and structure stress characteristics.
[0077] 2. Adjustment of permeability coefficients of similar materials in seepage and precipitation model tests.
[0078] In the model test of seepage and precipitation in loose granular strata, the main similarity relationships considered include the following:
[0079] The similarity relationship between flow velocity v and permeability coefficient k is: v =C k ;
[0080] The similarity relationship between seepage rate Q, permeability coefficient k and geometry L is: Q =C L 2 C k ;
[0081] The similarity relationship between the water particle velocity v, permeability coefficient k and porosity p in the pore is:
[0082] C k =C v C p ;
[0083] The similarity relationship between time t, permeability coefficient k, geometry L and porosity p is: t C k =C L C μ .
[0084] In general, in the test, as long as the permeability similarity ratio between the similar material and the loose granular formation is determined to be within the range of 5 to 10, other similarity ratio relationships can be determined, as follows:
[0085] Obtain the initial value of the permeability coefficient k of the sample prepared from similar materials in step 2.
[0086] Specifically, in the model test of mechanics and deformation of loose granular formations, the initial value of the permeability coefficient k of the similar sample is obtained through indoor permeability test, and the obtained permeability coefficient is compared with the corresponding value of the loose granular formation to obtain the permeability coefficient similarity ratio. If the obtained similarity ratio is within the range of 5 to 10, the permeability of the similar material sample meets the requirements, otherwise it does not meet the requirements.
[0087] When the permeability coefficient of the similar material sample does not meet the requirements, keep the overall content of the coarse-grained group unchanged, adjust the mass content of 10-20 mesh quartz sand and 20-40 mesh quartz sand in the coarse-grained group according to the predetermined increase or decrease percentage, and re-prepare the sample of the similar material according to step 2 until the permeability coefficient of the similar sample meets the requirements of the simulation test.
[0088] Specifically, when the permeability coefficient is too large, the mass content of 20-40 mesh quartz sand is increased by 1% by mass, and at the same time, the mass content of 10-20 mesh quartz sand is reduced by 1% by mass. Each time the mass is adjusted, the sample is re-prepared according to the method in step 2 until it meets the simulation test requirements.
[0089] When the permeability coefficient is too small, the mass content of 20-40 mesh quartz sand is reduced by 1% by mass, and at the same time, the mass content of 10-20 mesh quartz sand is increased by 1% by mass.
[0090] After the mass percentage of each part of the similar material is determined, the proportions of quartz sand, barite powder and water of different mesh sizes can be mixed according to the actual total demand. After the materials are prepared, they are packed and the sensors are arranged according to the test requirements. It is found that the similar materials have good water stability and can adjust the water content well. In the seepage test, they can maintain stability during the seepage process. In this way, experiments can be carried out to study the distribution law of structural water pressure, the change law of formation seepage field and the law of formation water inrush and destruction.
[0091] Embodiment 1:
[0092] A similar model test of tunnel excavation without support was carried out for a certain pebble stratum. A total of 200 kg of test materials were required. The preparation and adjustment process of similar materials are shown in the following steps:
[0093] Step 1: According to the survey report of a pebble formation, the gradation composition of the formation material belongs to the skeleton void type, and the density is 2.01g / cm 3 , elastic modulus is 25MPa, internal friction angle is 42.0°, cohesion is 10.02kPa, maximum particle size is 48cm, and moisture content is 5.8%. According to the similar material ratio corresponding to the skeleton void type, the mass percentage of each material in the similar material is preliminarily determined to be: 35.7% 2-4 mesh quartz sand: 34.8% 10-20 mesh quartz sand: 9.7% 20-40 mesh quartz sand: 10.5% 150 mesh barite powder: 9.3% 600 mesh barite powder.
[0094] Step 2: Prepare 5 kg of sample according to the above ratio, and adjust the amount of water added to the sample repeatedly to make the water content of similar samples equal to that of the pebble stratum. The final amount of water added is 0.8 kg, so the mass percentage of water required in the test is
[0095] Step 3: Based on the similarity ratio between the pebble formation and the macrogranular group of similar materials Taking into account the feasibility and economy of the test, the geometric similarity ratio C of this test was finally determined.L = 60. Combined with the size of the test box, the total amount of similar materials required for this test is determined to be 200 kg.
[0096] Step 4: The initial values of cohesion c and elastic modulus E of similar materials obtained through indoor direct shear test and compression test are 0.4MPa and 0.23kPa respectively. Therefore, the elastic modulus similarity ratio between the pebble stratum and the similar material sample can be obtained as follows: Elastic modulus similarity ratio and geometric similarity ratio (C L =60) is -0.04, which meets the requirement.
[0097] The cohesion similarity ratio is The geometric similarity ratio (C L =60) has an error of +0.27, which does not meet the requirement.
[0098] The mass content of 600 mesh barite powder and 150 mesh barite powder in the similar material ratio scheme was adjusted to improve the cohesion of similar samples. Through repeated adjustments, it was finally determined that the mass percentage of 600 mesh barite powder was increased from the original 9.3 to 14.1, and the mass percentage of 150 mesh barite powder was reduced from the original 10.5 to 5.7.
[0099] Therefore, the mass percentage of each material in the similar materials finally determined is: 35.7% 2-4 mesh quartz sand, 34.8% 10-20 mesh quartz sand, 9.7% 20-40 mesh quartz sand, 5.7% 150 mesh barite powder, and 14.1% 600 mesh barite powder.
[0100] Step 5: According to the total amount required for the test, a total of 200 kg of test materials need to be prepared, including 32 kg of water and 168 kg of similar materials. According to the determined content of similar materials, the final required mass of each material is: 59.976 kg of 2-4 mesh quartz sand; 58.464 kg of 10-20 mesh quartz sand; 16.296 kg of 20-40 mesh quartz sand; 9.576 kg of 150 mesh barite powder; 23.688 kg of 600 mesh barite powder.
[0101] After the materials are prepared, they are packed and the sensors are arranged according to the test requirements to carry out the corresponding tests. Figure 2 This is the change of the arch settlement during the tunnel excavation process in this model test. As can be seen from the figure, the settlement of all measuring points has been increasing during the tunnel excavation process, reaching the maximum after the excavation is completed. The arch settlement caused by excavation within 15cm and 25cm before and after the monitoring section accounts for more than 90% of the total settlement. The deformation of the arch surrounding rock during the cavern excavation stage is generally small, which is similar to the deformation law of on-site monitoring.
[0102] The above contents are only for explaining the technical idea of the present invention and cannot be used to limit the protection scope of the present invention. Any changes made on the basis of the technical solution in accordance with the technical idea proposed by the present invention shall fall within the protection scope of the claims of the present invention.
Claims
1. A method for preparing similar materials of loose granular formations, characterized in that: The similar materials include coarse-grained materials used as a framework, coarse-grained materials used as filling interstitial materials, and fine-grained materials used as filling cementation; The coarse-grained material is 2-4 mesh quartz sand; the coarse-grained material group includes 10-20 mesh quartz sand and 20-40 mesh quartz sand; the fine-grained material group includes 150 mesh barite powder and 600 mesh barite powder; The similar materials include suspended dense formation similar materials, skeleton void formation similar materials and skeleton dense formation similar materials; The suspended dense formation similar material includes, by mass percentage, 5% to 10% of 2-4 mesh quartz sand, 10% to 20% of 10-20 mesh quartz sand, 15% to 25% of 20-40 mesh quartz sand, 20% to 30% of 150 mesh barite powder and 25% to 35% of 600 mesh barite powder; The skeleton void type stratum similar material includes, by mass percentage, 30% to 40% of 2 to 4 mesh quartz sand, 30% to 40% of 10 to 20 mesh quartz sand, 5% to 15% of 20 to 40 mesh quartz sand, 5% to 15% of 150 mesh barite powder and 5% to 15% of 600 mesh barite powder; The skeleton dense formation similar material includes, by mass percentage, 20-30% of 2-4 mesh quartz sand, 20-30% of 10-20 mesh quartz sand, 0.5-5% of 20-40 mesh quartz sand, 20%-30% of 150 mesh barite powder and 20%-30% of 600 mesh barite powder; The method for preparing similar materials of the loose granular formation comprises the following steps: Step 1, determining similar material types according to the gradation composition of the loose granular formation; Step 2: prepare a set amount of mixed dry material sample according to the proportion corresponding to the similar material type, adjust the water content of the mixed dry material sample to make it the same as the water content of the loose granular formation, and obtain the mass percentage of water in the similar material; Step 3, determining the geometric similarity ratio between the loose granular formation and the similar material determined in step 1; Step 4: set the performance parameters of the similar material according to the test type, compare the performance parameter similarity ratio and geometric similarity ratio of the similar material and the loose granular formation, and adjust the mass percentage of each material in the coarse-grained group or the fine-grained group in the similar material sample according to the comparison result, so that the performance of the similar material reaches the set performance parameters of the similar material, and obtain the mass percentage of each component in the similar material; According to the average diameter of the giant grain group in the loose granular formation and the average diameter of the giant grain material in the similar material, the particle size similarity ratio between the loose granular formation and the similar material is calculated, and then the geometric similarity ratio between the loose granular formation and the similar material is determined according to the particle size similarity ratio and economic indicators; When conducting mechanical and deformation simulation tests, the performance parameters are elastic modulus E and cohesion c; The adjustment method of the elastic modulus E and the cohesion c is as follows: The elastic modulus E is adjusted in the following manner: the overall content of the coarse-grained group remains unchanged, and the mass content of the quartz sand of 10 to 20 meshes and the quartz sand of 20 to 40 meshes in the coarse-grained group is adjusted according to a predetermined increase or decrease percentage; The method for adjusting the cohesion c is to keep the overall content of the fine-grained group unchanged and adjust the mass content of the 600-mesh barite powder and the 150-mesh barite powder in the fine-grained group according to a predetermined increase or decrease percentage; When conducting a model test of seepage and precipitation in loose granular formations, the performance parameter is the permeability coefficient, and the adjustment method of the permeability coefficient is as follows: A model test of seepage and precipitation in loose granular formations was conducted, the overall content of the coarse-grained group was kept unchanged, and the mass content of 10-20 mesh quartz sand and 20-40 mesh quartz sand in the coarse-grained group was adjusted according to a predetermined increase or decrease percentage; Step 5: Prepare similar materials according to the total amount of similar materials required by the test and in combination with the mass percentage of each component in the similar materials obtained in step 4 and the mass percentage of water.
2. The method for preparing similar materials of loose granular formation according to claim 1, characterized in that: In step 1, the gradation composition of the loose granular stratum is determined based on the exploration data of the loose granular stratum.