An experimental method to study the effect of local failure of tunnel on adjacent structures
By designing pipe sheet making molds and simulating local tunnel failure methods, the strength of tunnel pipe sheets and joints was studied, and the problem of ignoring the strength of tunnel pipe sheets and joints in the existing technology was solved, and effective research on the impact of local tunnel failure was achieved.
Patent Information
- Application Number
- CN202210056674.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-18
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-01-18
AI Technical Summary
When studying the impact of local damage to shield tunnels on adjacent structures, the prior art ignores the strength problems at the tunnel pipe segments and joints, resulting in the inability to effectively study the continuous damage problem of tunnels.
A pipe sheet production method for model tests was designed. The model pipe sheet was made by preparing pipe sheets and casting concrete to simulate local damage to the tunnel, and the wire joint was used to apply high current to simulate joint failure, and the local damage to the tunnel was studied. Structural influence.
The research on the strength of tunnel pipe sheets and joints in tunnel centrifuge tests has been achieved, the method of studying tunnel deformation and failure problems has been broadened, and an effective means to study the impact of local tunnel damage on structure.
Smart Images

Figure CN114592882B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a model test method in underground engineering, and more specifically to a test method for simulating the influence of local damage of a shield tunnel on adjacent structures. Background Art
[0002] Entering the 21st century, my country's urbanization process has accelerated, and the problem of urban ground traffic congestion has become increasingly serious. Due to its small footprint and stable running speed, subway construction has ushered in rapid development. Among them, shield tunnels are widely used in my country's subway tunnel construction due to their small impact on the ground, safety, and high efficiency.
[0003] Shield tunnels are made up of a large number of prefabricated concrete segments, and their joints are relatively weak locations, which are prone to local damage. In shield tunnels, local damage can easily lead to large-scale continuous damage to the tunnel. At present, research on tunnel collapse mainly focuses on the failure mechanism of excavation face instability. There are few studies on the continuous damage of tunnels. Given that the damage problem cannot be studied in actual engineering, the innovation of an effective research method is particularly urgent and important.
[0004] Centrifuge model test is one of the most important methods to study shield tunnel problems. Through the centrifuge, the stress level and stress gradient around the tunnel can be truly restored, and the stress state and changes of structures such as segments in actual tunnel engineering can be truly reflected. By truly restoring the tunnel structure and its environment, important and reliable reference data can be obtained, which is of great significance for studying underground engineering accidents.
[0005] However, current research on tunnel centrifuge tests mostly focuses on tunnel deformation issues, while ignoring the strength issues of tunnel segments and joints. Summary of the invention
[0006] In view of the above-mentioned prior art, the present invention provides a method for manufacturing segments that can be used for model tests and truly restore actual tunnel engineering.
[0007] In order to solve the above technical problems, the present invention proposes a test method for studying the influence of local failure of a tunnel on adjacent structures, comprising the following steps:
[0008] Step 1: Prepare the segment production mold: The segment production mold includes two sets of segment molds corresponding to the standard block segment and the capping block segment; each set of segment molds is composed of 7 modules, and the 7 modules include 2 capping blocks, 1 bottom block, 2 side blocks, 1 concave tenon block and 1 convex tenon block. The 7 molds are all provided with installation positioning mortise or installation positioning tenon, and the bottom block, side block, concave tenon block and convex tenon block are all provided with connector reserved holes, and connector pre-embedded parts are provided between the connector reserved holes of the bottom block and the connector reserved holes of the side block, between the connector reserved holes of the bottom block and the connector reserved holes of the concave tenon block, and between the connector reserved holes of the bottom block and the connector reserved holes of the convex tenon block; after the segment production mold is assembled, grouting holes are reserved;
[0009] Step 2: pouring concrete into the cavity formed inside the mold for making the assembled segments, and then demoulding and curing to obtain a model segment, wherein all the embedded connectors are segment joints, and the embedded connectors are iron wires; assembling the model segments into a complete tunnel model according to the assembly method used in the actual project;
[0010] Step 3: local damage simulation of the model tunnel, including:
[0011] Step 1) After the detection equipment is deployed, the model tunnel is placed at the preset position and the detection equipment is turned on; after the detection data is stable, the soil is filled; during the soil filling process, after each soil thickness of 1 tunnel diameter is filled, the soil surface is scraped flat, and after the detection data are stable again, the soil filling is continued; until the soil thickness above the tunnel is 4 times the tunnel diameter; after the detection data is stable, step 2) is performed;
[0012] Step 2) Start simulating local damage of the tunnel: determine the location and number of failed segment joints in the segment joints, connect the iron wires at the determined locations to the circuit, apply high current to the iron wires at the determined locations through relevant equipment, so that the iron wires heat up and melt, thereby simulating the failure of the segment joints. The test ends when all preset segment joints are destroyed and all monitoring data are finally stable.
[0013] Furthermore, in step 1 of the present invention, each set of segment production molds is assembled into a whole with a cavity inside, and the internal cavity is determined by reducing the size according to the actual segment shape; the seven molds of each set of segment are respectively provided with installation positioning tenons and installation positioning mortise. A release agent is sprayed inside the assembled segment production mold.
[0014] In step 2, the portion of the segment manufacturing mold that contacts the grouting liquid is flat and smooth.
[0015] In step three, the diameter of the iron wire is 0.75 mm, and the applied current is 200 A.
[0016] Compared with the prior art, the present invention has the following beneficial effects:
[0017] The present invention can be used to make a tunnel model for centrifuge testing that truly reflects the strength of tunnel segments and joints. The tunnel model is used to conduct tests, thereby achieving the goal of not only studying tunnel deformation problems, but also studying the strength problems of tunnel segments and joints in tunnel centrifuge test research. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1-1 This is a schematic diagram of the assembly of the standard segment mold;
[0019] Figure 1-2 This is a schematic diagram of the standard segment mold after assembly;
[0020] Figure 2-1 This is the front view of the bottom block (D) of the standard segment mold;
[0021] Figure 2-2 for Figure 2-1 A side view of the bottom block (D) of the standard block segment mold shown;
[0022] Figure 2-3 for Figure 2-1 A top view of the bottom block (D) of the standard block segment mold shown;
[0023] Figure 3-1 This is the front view of the tenon block (A) of the standard segment mold;
[0024] Figure 3-2 for Figure 3-1 A side view of the tenon block (A) of the standard segment mold shown;
[0025] Figure 3-3 for Figure 3-1 A top view of the tenon block (A) of the standard segment mold shown;
[0026] Figure 4-1 It is the front view of the tenon block (T) of the standard segment mold;
[0027] Figure 4-2 for Figure 4-1 A side view of the tenon block (T) of the standard segment mold shown;
[0028] Figure 4-3 for Figure 4-1 A top view of the tenon block (T) of the standard segment mold shown;
[0029] Figure 5-1 This is the front view of the capping block (F) of the standard segment mold;
[0030] Figure 5-2for Figure 5-1 A side view of the capping block (F) of the standard segment mold shown;
[0031] Figure 5-3 for Figure 5-1 A top view of the capping block (F) of the standard segment mold is shown;
[0032] Figure 6-1 This is the front view of the side block (C) of the standard segment mold;
[0033] Figure 6-2 for Figure 6-1 A side view of the side block (C) of the standard block segment mold shown;
[0034] Figure 6-3 for Figure 6-1 A top view of the side block (C) of the standard block segment mold shown;
[0035] Figure 7-1 This is a schematic diagram of the assembly of the capping block segment mold;
[0036] Figure 7-2 This is a schematic diagram of the capping block segment mold after assembly;
[0037] Figure 8-1 It is the front view of the bottom block (D') of the capping segment mold;
[0038] Figure 8-2 for Figure 8-1 A side view of the bottom block (D') of the capping segment mold is shown;
[0039] Figure 8-3 for Figure 8-1 A top view of the bottom block (D') of the capping segment mold is shown;
[0040] Figure 9-1 It is the front view of the tenon block (A') of the capping segment mold;
[0041] Figure 9-2 for Figure 9-1 A side view of the tenon block (A') of the capping segment mold shown;
[0042] Figure 9-3 for Figure 9-1 A top view of the tenon block (A') of the capping block segment mold shown;
[0043] Figure 10-1 It is the front view of the tenon block (T') of the capping block segment mold;
[0044] Figure 10-2 for Figure 10-1 A side view of the tenon block (T') of the capping segment mold shown;
[0045] Figure 10-3for Figure 10-1 A top view of the tenon block (T') of the capping block segment mold shown;
[0046] Figure 11-1 It is the front view of the capping block (F') of the capping block segment mold;
[0047] Figure 11-2 for Figure 11-1 A side view of a capping block (F') of a capping block segment mold is shown;
[0048] Figure 11-3 for Figure 11-1 A top view of a capping block (F') of a capping block segment mold is shown;
[0049] Figure 12-1 It is the front view of the side block (C') of the capping segment mold;
[0050] Figure 12-2 for Figure 12-1 A side view of the side block (C') of the capping segment mold is shown;
[0051] Figure 12-3 for Figure 12-1 A top view of the side block (C') of the capping block segment mold is shown;
[0052] Figure 13-1 It is the front view of the embedded part of the connector (L);
[0053] Figure 13-2 for Figure 13-1 A side view of the embedded connector (L) shown;
[0054] Figure 13-3 for Figure 13-1 A top view of the embedded connector (L) shown;
[0055] Figure 13-4 This is the model connector circuit diagram.
[0056] In the figure:
[0057] 1- The concave / convex tenon block in the bottom block is reserved for installation positioning mortise 2- Binding groove
[0058] 3-Circumferential seam hand hole forming boss 4-Longitudinal seam hand hole forming boss
[0059] 5-Embedded parts installation hole 6-Install the positioning tenon in the concave / convex tenon block
[0060] 7-Reserved mortise for the concave tenon in the concave tenon block 8-Reserved mortise for the convex tenon in the convex tenon block
[0061] 9-Install the positioning tenon 10-Reserve the side block to install the positioning tenon
[0062] 11- Grouting hole A- standard block segment mold tenon block
[0063] C- Side block of standard segment mold D- Bottom block of standard segment mold
[0064] F-Capping block of standard segment mold T-Tongue block of standard segment mold
[0065] A'- the concave and mortise block of the capping segment mold C'- the side block of the capping segment mold
[0066] D'- Bottom block of the capping block segment mold F'- Capping block of the capping block segment mold
[0067] T'- tenon block of capping block segment mold L- embedded part of connector DETAILED DESCRIPTION
[0068] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments, but the following embodiments are by no means intended to limit the present invention in any way.
[0069] The design idea of the test method for studying the influence of local tunnel damage on adjacent structures proposed in the present invention is: mainly including the production of model segments and test implementation methods. Among them, the model segments are made by assembling the designed molds, pouring concrete, and curing. The model tunnel segments are connected by iron wires with diameters determined by similarity ratios. After the test implementation begins, the predetermined joints are made to fail by artificially applying current. This method can artificially control the failure of any part and any number of joints at any time to fully study the influence of local tunnel damage on its adjacent structures. This method not only broadens the methods for studying such accidents, but also provides a research idea for future research.
[0070] The present invention proposes a test method for studying the influence of local failure of a tunnel on adjacent structures, comprising the following steps:
[0071] Step 1: Prepare the segment production mold:
[0072] There are two sets of segment production molds, one is Figure 1-1 and Figure 1-2The standard block segment mold shown is composed of 7 modules, including 2 capping blocks F, 1 bottom block D, 2 side blocks C, 1 tenon block A and 1 convex block T. The 7 molds are all provided with installation positioning mortise or installation positioning tenon. The bottom block D, the side block C, the tenon block A and the convex tenon block T are all provided with connection part reserved holes. The connection part reserved holes of the bottom block and the connection part reserved holes of the side blocks, the connection part reserved holes of the bottom block and the connection part reserved holes of the tenon block, and the connection part reserved holes of the bottom block and the connection part reserved holes of the convex tenon block are all provided with connection part embedded parts L; after the segment manufacturing mold is assembled, a grouting hole 11 is reserved. The 7 modules are assembled into a whole with a cavity inside. The design of the internal cavity is determined according to the actual segment shape and the size is reduced. The 7 molds are respectively provided with installation positioning tenons and installation positioning mortise, which can provide convenience for mold assembly and make the mold assembly more firm.
[0073] Figure 2-1 , Figure 2-2 and Figure 2-3 The structure of the bottom block D of the standard block segment mold is shown, and the concave / convex tenon block of the bottom block D is reserved with an installation positioning mortise 1, and a binding groove 2, a circumferential seam hand hole forming boss 3, a longitudinal seam hand hole forming boss 4 and an embedded part installation hole 5 are reserved; Figure 3-1 , Figure 3-2 and Figure 3-3 The structure of the concave tenon block A of the standard block segment mold is shown, and the concave tenon block A is provided with an embedded part installation hole 5, a positioning tenon 6 for installing the concave / convex tenon block, a concave tenon reserved mortise 7 in the concave tenon block, and a convex tenon reserved mortise 8 in the convex tenon block; Figure 4-1 , Figure 4-2 and Figure 4-3 The structure of the tenon block T of the standard segment mold is shown, and the tenon block T is provided with a bolt embedded part installation hole 5, a positioning tenon 6 installed in the concave / convex tenon block, and a tenon reserved tenon 8 in the tenon block; Figure 5-1 , Figure 5-2 and Figure 5-3 The structure of the capping block F of the standard segment mold is shown. A binding groove 2 is reserved at the top of the capping block F, and a mounting positioning tenon 9 for plugging with the side block C at the lower end is reserved at the bottom of the capping block F; Figure 6-1 , Figure 6-2 and Figure 6-3 The structure of the side block C of the standard block segment mold is shown, and the bottom of the side block C is provided with a binding groove 2, an embedded part installation hole 5 and a reserved installation positioning mortise 10 of the side block. Figure 1-1As shown, the concave tenon block A and the convex tenon block T are respectively located at the front and rear ends of the bottom block D, and the two side blocks C are located at the left and right sides of the bottom block D. The five modules are assembled into a cavity bottom, and the two capping blocks F are respectively installed on the top of the cavity, thereby forming a standard block segment mold with a grouting hole 11 reserved.
[0074] The other set is as follows Figure 7-1 and Figure 7-2 The capping block segment mold shown is also composed of 7 modules, including 2 capping blocks F', 1 bottom block D', 2 side blocks C', 1 concave tenon block A' and 1 convex tenon block T'. The 7 molds are all provided with installation positioning mortise or installation positioning tenon. The bottom block D', the side block C', the concave tenon block A' and the convex tenon block T' are all provided with connection part reserved holes, and connection part embedded parts L are provided between the connection part reserved holes of the bottom block and the connection part reserved holes of the side block, between the connection part reserved holes of the bottom block and the connection part reserved holes of the concave tenon block, and between the connection part reserved holes of the bottom block and the connection part reserved holes of the convex tenon block; after the segment manufacturing mold is assembled, a grouting hole 11 is reserved. Figure 8-1 , Figure 8-2 and Figure 8-3 The structure of the bottom block D' of the capping block segment mold is shown; Figure 9-1 , Figure 9-2 and Figure 9-3 The structure of the tenon block A' of the capping block segment mold is shown; Figure 10-1 , Figure 10-2 and Figure 10-3 The structure of the tenon block T' of the capping block segment mold is shown; Figure 11-1 , Figure 11-2 1-3 show the structure of the capping block F' of the capping block segment mold; Figure 12-1 , Figure 12-2 and Figure 12-3 The structure of the side block C' of the capping block segment mold is shown. Seven modules are assembled into a whole with a cavity inside. The design of the internal cavity is determined according to the shape of the actual segment and the size is reduced. The seven molds are respectively provided with installation positioning tenons and installation positioning mortise. The positional relationship and detailed structure involved in each module for assembly and the design of the shape and size of the inner cavity after assembly are similar to those of the aforementioned standard block segment mold, and will not be repeated here. After the mold is assembled, the connection embedded parts are inserted to reserve the connection holes in the model segment.
[0075] Step 2: pouring concrete into the cavity formed inside the mold for manufacturing the assembled segments, and then demolding and curing to obtain a model segment, wherein all the embedded connectors are segment joints, and the embedded connectors are iron wires; assembling the model segments into a complete tunnel model according to the assembly method used in the actual project, spraying a release agent on the inside of the assembled segment manufacturing mold, and the portion of the segment manufacturing mold in contact with the grouting liquid is flat and smooth to ensure that the surface of the manufactured model segment is smooth.
[0076] Step three, local damage simulation of the model tunnel. The key to the test of the present invention lies in the local damage simulation. The local damage of the tunnel is simulated by joint failure. After the preset joint is destroyed by artificial methods, the internal force value of the structure adjacent to the local damage is monitored to study the impact of local damage on the tunnel. In the present invention, the joints of the pipe segments are connected by iron wire, and the diameter of the iron wire should be determined by the similarity ratio between the bolt diameter in the actual project and the one used in the test. The destruction of the joint in the present invention is achieved by applying a high current to the iron wire at the joint, so that the iron wire heats up and melts. The specific process is as follows:
[0077] Step 1) After the detection equipment is deployed, the model tunnel is placed at the preset position and the detection equipment is turned on; after the detection data is stable, the soil is filled; during the soil filling process, after each soil thickness of 1 tunnel diameter is filled, the soil surface is scraped flat, and after the detection data are stable again, the soil filling is continued; until the soil thickness above the tunnel is 4 times the tunnel diameter; after the detection data is stable, step 2) is performed;
[0078] Step 2) Start simulating local damage of the tunnel: determine the location and number of failed segment joints in the segment joints, thereby simulating local damage to the tunnel; connect the iron wire at the determined location to the circuit, and apply a high current to the iron wire at the determined location through relevant equipment, so that the iron wire heats up and melts, thereby simulating the failure of the segment joint. After all preset segment joints are destroyed and all monitoring data are finally stable, the test ends.
[0079] Example:
[0080] In this embodiment, a test of continuous damage caused by local damage to the tunnel was conducted in a 1g environment and at a depth of 4 times the tunnel diameter. The ratio of the tunnel model size in the embodiment to the actual project size (using the general size of Tianjin subway tunnels) is 1:40. The model tunnel in the embodiment is made of two types of segments, namely, capping segments and standard segments. The arc surface of the standard segment has a central angle of 67.5°, and its mold composition is as follows: Figure 1-1 to Figure 6-3 The arc surface of the capping block segment corresponds to the center angle of the circle at 22.5 degrees, and its mold composition is as follows: Figure 7-1 to Figure 12-3 As shown, Figure 13-1 , Figure 13-2 , Figure 13-3and Figure 13-4 The structure of the embedded connectors in each set of molds of the present invention and the circuit diagram of the model connectors are shown.
[0081] First, determine the total number of tunnel segments based on the required tunnel model length. In this embodiment, the model tunnel consists of 20 rings of segments. Therefore, a total of 20 capping segments and 100 standard segments need to be made. In order to avoid the possibility that the quality of the manufactured segments does not meet the requirements and affects the progress of the experiment, it is determined to make 24 capping segments and 120 standard segments. Therefore, it is necessary to prepare 24 sets of capping segment production molds and 120 sets of standard segment production molds. If there is sufficient time, it can also be produced in batches to save mold costs. After the molds are ready, place the standard segment molds and capping segment molds according to Figure 1-1 , Figure 1-2 and Figure 7-1 and Figure 7-2 Assemble, and do not assemble the remaining capping blocks for the time being. Spray the release agent inside the assembled mold to facilitate the demoulding of the pipe segment. Then, assemble the capping block. Use the binding rope to bind and fix the mold through the binding groove reserved in the mold. After the mold is assembled, inject the prepared concrete slurry into the mold through the grouting hole, and perform sufficient vibration, curing, demolding, curing and other procedures in accordance with regulations to ensure that the strength of the manufactured pipe segment reaches the required standard. During the demolding process, the binding rope should be removed first, and then the molds should be removed in the order of capping block, concave (convex) tenon block, and side block.
[0082] After the segments are manufactured, they are assembled into a complete tunnel model in the same way as in the actual project. Testing tools such as strain gauges are attached to the model tunnel body at the planned monitoring location. The model tunnel segments are connected by wires with a diameter of 0.75 mm.
[0083] In the experiment of this embodiment, the local destruction of the tunnel is controlled by humans, and the local destruction of the tunnel is simulated by the fracture of several joints. Therefore, after the tunnel is assembled, each preset destruction joint is connected to the circuit. The circuit diagram is as follows Figure 13-4 shown.
[0084] After the detection equipment is deployed, place the model tunnel at the preset position and turn on the detection equipment. After the detection data is stable, start filling the soil. It should be noted that after each filling of 1 times the tunnel diameter thickness, the soil surface should be scraped flat, and after the various detection data are stable again, continue filling the soil. This process continues until the thickness of the soil above the tunnel is 4 times the tunnel diameter.
[0085] After the test data is stable, the test preparation phase is completed and the simulation of local tunnel damage can begin. The experimenter should energize the damaged joints in sequence through relevant equipment according to the predetermined joint damage sequence.
[0086] The model tunnel joint of this embodiment is an iron wire with a diameter of 0.75 mm, so the current is set to 200 A. After power is turned on, the iron wire simulating the bolt at the joint will generate heat due to the passage of large current, and then melt. By this means, local damage at the joint can be effectively simulated. After all preset joints are destroyed and the monitoring data are finally stable, the test ends.
[0087] Although the present invention has been described above in conjunction with the accompanying drawings, the present invention is not limited to the above-mentioned specific embodiments, which are merely illustrative rather than restrictive. Under the guidance of the present invention, ordinary technicians in this field can make many modifications without departing from the purpose of the present invention, all of which are within the protection of the present invention.
Claims
1. A test method for studying the effect of local failure of a tunnel on adjacent structures, characterized in that: The following steps are involved: Step 1: Prepare the segment production mold: The segment production mold includes two sets of segment molds corresponding to the standard block segment and the capping block segment; each set of segment molds is composed of 7 modules, and the 7 modules include 2 capping blocks, 1 bottom block, 2 side blocks, 1 concave tenon block and 1 convex tenon block. The 7 molds are all provided with installation positioning mortise or installation positioning tenon, and the bottom block, side block, concave tenon block and convex tenon block are all provided with connector reserved holes, and connector pre-embedded parts are provided between the connector reserved holes of the bottom block and the connector reserved holes of the side block, between the connector reserved holes of the bottom block and the connector reserved holes of the concave tenon block, and between the connector reserved holes of the bottom block and the connector reserved holes of the convex tenon block; after the segment production mold is assembled, grouting holes are reserved; Step 2: pouring concrete into the cavity formed inside the mold for making the assembled segments, and then demoulding and curing to obtain a model segment, wherein all the embedded connectors are segment joints, and the embedded connectors are iron wires; assembling the model segments into a complete tunnel model according to the assembly method used in the actual project; Step 3: local damage simulation of the model tunnel, including: Step 1) After the detection equipment is deployed, the model tunnel is placed at the preset position and the detection equipment is turned on; after the detection data is stable, the soil is filled; during the soil filling process, after each soil thickness of 1 tunnel diameter is filled, the soil surface is scraped flat, and after the detection data are stable again, the soil filling is continued; until the soil thickness above the tunnel is 4 times the tunnel diameter; after the detection data is stable, step 2) is performed; Step 2) Start simulating local damage of the tunnel: determine the location and number of failed segment joints in the segment joints, connect the iron wires at the determined locations to the circuit, apply high current to the iron wires at the determined locations through relevant equipment, so that the iron wires heat up and melt, thereby simulating the failure of the segment joints. The test ends when all preset segment joints are destroyed and all monitoring data are finally stable.
2. The test method for studying the influence of local failure of a tunnel on adjacent structures according to claim 1 is characterized in that: In step one, each set of segment production molds are assembled into a whole with a cavity inside. The internal cavity is determined by reducing the size according to the actual segment shape; the 7 molds of each set of segments are respectively provided with installation positioning tenons and installation positioning mortise.
3. The test method for studying the influence of local failure of a tunnel on adjacent structures according to claim 1 or 2, characterized in that: In step 1, a release agent is sprayed on the inside of the mold for making the assembled pipe segments.
4. The test method for studying the influence of local failure of a tunnel on adjacent structures according to claim 1 is characterized in that: In step 2, the portion of the segment manufacturing mold that contacts the grouting liquid is flat and smooth.
5. The test method for studying the influence of local failure of a tunnel on adjacent structures according to claim 1 is characterized in that: In step three, the diameter of the iron wire is 0.75 mm, and the applied current is 200 A.