Glass article manufacturing device and glass article manufacturing method

Through the suspension support device and vertical adjustment technology, the tilt problem caused by the deformation of the shell of the glass article manufacturing device is solved, ensuring the stability and efficiency of the homogenization process of molten glass.

CN114599614BActive Publication Date: 2024-10-29NIPPON ELECTRIC GLASS CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202080072939.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-07-16
Publication Date
2024-10-29
Estimated Expiration
2040-07-16

AI Technical Summary

Technical Problem

The deformation of the shell of the existing glass article manufacturing device in a high temperature environment causes the stirring tank to tilt, which affects the efficiency and stability of the homogenization treatment of molten glass.

Method used

The original shape of the mixing tank shell is maintained by the suspension support device, the design of the shell is restored by its own weight to prevent tilting, and the correct installation and use of the shell is ensured by adjusting the verticality of the side wall.

Benefits of technology

It effectively prevents the tilt of the stirring tank, ensures the stability of the homogenization process and stirring efficiency of the molten glass, and extends the service life of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114599614B_ABST
    Figure CN114599614B_ABST
Patent Text Reader

Abstract

A glass article manufacturing device (1) comprises a glass melting furnace (2) for generating molten glass, a processing device (6) for performing a predetermined process on the generated molten glass, and a forming device (5) for forming the molten glass subjected to the predetermined process. The processing device (6) comprises a processing tank (13, 15) to which the molten glass is supplied and a housing (12) for holding the processing tank (13, 15), and the housing (12) is suspended and supported.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an apparatus for manufacturing a glass article and a method for manufacturing the same, and more particularly to a technique for performing a predetermined treatment such as homogenization on molten glass between (in the middle of) a molten glass generating step and a forming step. Background Art

[0002] As is well known, when molten glass is transported from a melting furnace to a forming device, a stirring device is provided on the transport path to stir the molten glass supplied to the forming device. The stirring device is formed by arranging a stirrer provided with stirring blades in a cylindrical stirring tank, and by flowing molten glass into the stirring tank and rotating the stirrer around a predetermined axis, the molten glass flowing into the stirring tank can be given a circumferential flow, thereby stirring the molten glass.

[0003] On the other hand, when such a stirring device is used for the purpose of homogenizing molten glass, it is necessary to fully stir not only the molten glass flowing on the central side (rotation center side) of the stirring tank but also the molten glass flowing on the outer side (along the inner wall) of the stirring tank. Although the molten glass flowing on the central side of the stirring tank can be stirred relatively easily by the stirrer, the molten glass flowing along the inner wall flows through the gap inevitably generated between the stirring blades of the stirrer and the inner wall. Therefore, various mechanisms for effectively stirring the molten glass flowing along the inner wall are proposed.

[0004] For example, Patent Document 1 states that by reducing the gap between the outermost diameter of the stirring blade and the inner wall of the stirring tank, specifically by making the rotation diameter of the stirring blade approximately 91% of the inner diameter of the inner wall, the amount of molten glass flowing downstream without contacting the stirring blade is reduced.

[0005] Patent document 2 proposes a technique in which the outer diameter of the stirrer is set to be 0.85 times or more, preferably 0.9 times or more, the inner diameter of the stirring tank in order to prevent the molten glass from passing through the vicinity of the inner wall surface of the molten glass conveying tube (stirring tank).

[0006] Prior art literature

[0007] Patent Literature

[0008] Patent Document 1: Japanese Patent Application Publication No. 2015-124107

[0009] Patent Document 2: Japanese Patent No. 5510446 Summary of the invention

[0010] Problems to be solved by the invention

[0011] Thus, in the agitator of the prior art, by managing the radial clearance between the agitator (stirring blade) and the agitator tank, the agitator efficiency is improved, and then the homogenization is improved. In addition, the agitator is usually assumed to be used in a high temperature environment, and the agitator tank is covered with refractory materials and the agitator tank and the refractory materials are contained in the shell. However, in the case of such a structure, due to various factors such as the large-scale shell, there is a case where the shell is deformed when the agitator is assembled or used. At this time, the shell is installed on the floor surface side, and the agitator and the device (motor) driving the agitator to rotate are installed on the specified parts at a position separated from the floor surface upward. Therefore, in the case of the shell being deformed as described above, the agitator tank in the state of being retained in the shell is tilted along with the deformation of the shell, and the agitator in the state of being installed at a position separated from the floor surface upward maintains the posture before the shell is deformed. As a result, the possibility of a large change in the gap between the outermost diameter part (outermost diameter part of the agitator blade) and the inner surface of the agitator tank is increased. Therefore, it is difficult to stably carry out a good stirring process, and then it is difficult to stably carry out a high-quality homogenization process.

[0012] The above-mentioned problem is not limited to the stirring process (homogenization process), and may occur in other processes in which the molten glass is subjected to a predetermined process in the processing tank, such as a flow rate adjustment process, for example.

[0013] In view of the above circumstances, the technical problem to be solved in this specification is to provide an apparatus for manufacturing a glass article and a method for manufacturing the glass article that can prevent the tilting of a processing tank as much as possible and stably perform good processing on molten glass.

[0014] Solutions to Solve Problems

[0015] The above-mentioned problem is solved by a manufacturing device for glass articles of the present invention. That is, the manufacturing device comprises a glass melting furnace for generating molten glass, a processing device for performing a predetermined processing on the generated molten glass, and a forming device for forming the molten glass subjected to the predetermined processing, and the manufacturing device for glass articles is characterized in that the processing device comprises a processing tank to which the molten glass is supplied and a housing for holding the processing tank, and the housing is suspended and supported.

[0016] Thus, in the manufacturing device of the glass article of the present invention, when the processing device has a shell for holding the processing tank of the molten glass, the shell is suspended and supported. By suspending and supporting the shell constituting the processing device in this way, a force is applied to the shell to restore the original shape of the shell (the shape of the shell when it is a single body) under the action of its own weight. Therefore, even if the shell is deformed during assembly or use, a force is applied to the shell to restore the shape before the deformation, so that the shape before the deformation can be restored or close to it. In addition, when the shell is in the shape of a single body from the beginning of the suspension support, the shape is maintained under the action of its own weight. In summary, according to the manufacturing device of the present invention, the tilting of the processing tank during assembly or use of the processing device can be prevented as much as possible, and the reduction of the processing efficiency or processing capacity caused by the tilting can be prevented. In other words, the molten glass can be stably processed well.

[0017] In addition, in the manufacturing device of the glass article of the present invention, the housing may be rectangular in a top view, and the vertical cross section of the housing may be symmetrical about a vertical line passing through the center of the short side direction of the vertical cross section. It should be noted that the short side direction mentioned in this specification means the direction along one side of the housing that is the short side when the housing is rectangular in a top view. Similarly, the long side direction mentioned in this specification means the direction along the other side of the housing that is the long side.

[0018] In this way, by determining the shape of the shell, the center of gravity of the shell can be set on the plumb line passing through the center of its short side in the design. Therefore, if the shell is in the designed shape from the beginning of assembly (suspension support), its state is maintained during use. Alternatively, when the center line of the shell passing through the center of the short side in the vertical cross section of the shell is tilted relative to the plumb line during assembly, the dead weight of the center line in the direction consistent with the plumb line acts on the shell. Therefore, regardless of the state during assembly, the shell is always in the designed shape, and the tilting of the treatment tank can be prevented more reliably.

[0019] In addition, in the manufacturing device of the glass article of the present invention, the outer shell may have a bottom and a pair of side walls standing upright relative to the bottom, and the verticality of the inner surface of the side wall relative to the upper surface of the bottom is 0.001 or less. It should be noted that the verticality mentioned in this specification means the distance between two ideal planes that can clamp the inner surface of the side wall when the height dimension of the side wall is set to 1. The unit is dimensionless. In addition, the ideal plane mentioned here means a virtual plane perpendicular to the upper surface of the bottom. In the case of defining the verticality as described above, for example, the verticality of 0.001 means that when the height dimension of the side wall is set to 1, the inner surface of the side wall is located between two ideal planes separated by 0.001. Of course, in the case where the parallelism between the inner surface and the outer surface of the side wall is extremely high, in the above definition of verticality, the "inner surface" of the side wall can also be replaced by the "outer surface" of the side wall. Similarly, when the parallelism between the upper surface and the bottom surface (lower surface) of the bottom is extremely high, in the above definition of perpendicularity, the "upper surface" of the bottom may be replaced by the "bottom surface (lower surface)" of the bottom.

[0020] In this way, when the outer shell has a bottom and a pair of side wall portions upright relative to the bottom, for example in a rectangular shape, by determining the verticality of the inner surface of the side wall portion relative to the upper surface of the bottom as described above, it is possible to enjoy a sufficient shape restoration effect or shape maintenance effect brought about by the suspension support.

[0021] In addition, as described above, the manufacturing device of the present invention can prevent the tilting of the processing tank as much as possible and stably perform good processing on the molten glass. Therefore, for example, when the processing tank is a stirring tank, a stirrer is accommodated in the stirring tank, and the molten glass supplied to the stirring tank is stirred by the rotation of the stirrer, that is, when the processing device is a stirring device, the present invention is preferably applied.

[0022] In addition, the above-mentioned problem is also solved by a method for manufacturing a glass article of the present invention. That is, the method for manufacturing a glass article includes a glass generating step of generating molten glass, a processing step of performing a predetermined processing on the generated molten glass, and a forming step of forming the molten glass subjected to the predetermined processing, wherein the processing step includes: a preparation step of preparing a processing device, the processing device having a processing tank to which the molten glass is supplied and a shell for holding the processing tank; and a processing execution step of performing a predetermined processing on the molten glass using the prepared processing device, wherein the shell for holding the processing tank is suspended and supported in the preparation step.

[0023] Thus, in the manufacturing method of the glass article of the present invention, when the processing device has a shell for holding the processing tank of the molten glass, the shell is suspended and supported in the preparation process of the processing device. By supporting the shell constituting the processing device in this way, a force is applied to the shell under the action of its own weight to restore the shell to the shape when the shell is a single body. Therefore, even if the shell is deformed during assembly or use, a force is applied to the shell to restore the shape before the deformation, so that the shape before the deformation can be restored or approximated. In addition, when the shell is in the shape of a single body from the beginning of the suspension support, the shape is maintained under the action of its own weight. In summary, according to the manufacturing method of the glass article of the present invention, the tilting of the processing tank during the use of the processing device can be prevented as much as possible, and the molten glass can be stably and well processed.

[0024] In addition, in the manufacturing method of the glass article of the present invention, the shell may have a bottom and a pair of side walls standing upright relative to the bottom, and in the preparation step, before the shell is suspended and supported, the verticality of the inner surface of the side wall relative to the upper surface of the bottom of the shell is adjusted.

[0025] If the verticality of the inner surface of the side wall relative to the bottom upper surface of the shell is adjusted before the shell is suspended, the verticality can be adjusted in the state of the shell alone. If there is no treatment tank or refractory material, the verticality can be measured on the inside of the shell while the outer side of the shell is held by a predetermined fixture. Therefore, the verticality measurement and the correction of the shell can be easily and repeatedly performed, and the verticality can be adjusted very easily.

[0026] Effects of the Invention

[0027] In summary, according to the present invention, it is possible to prevent the inclination of the treatment tank as much as possible, and to stably and favorably treat the molten glass. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 This is a side view showing the overall structure of a glass article manufacturing apparatus according to one embodiment of the present invention.

[0029] Figure 2 yes Figure 1 An enlarged cross-sectional view of the processing device shown.

[0030] Figure 3 yes Figure 2 AA cross-sectional view of the processing device shown.

[0031] Figure 4 Observed from the direction of arrow B Figure 2 A top view of the processing device shown.

[0032] Figure 5It shows that the Figure 1 The apparatus shown is a flow chart of the process of a method for manufacturing a glass article.

[0033] Fig. 6A It is shown Figure 5 A flow chart showing details of the second processing step is shown.

[0034] Figure 6B It is shown Fig. 6A Flowchart showing details of the preparation process.

[0035] Figure 7 It is used to illustrate Figure 6B A cross-sectional view of the verticality adjustment process is shown.

[0036] Figure 8 It is used to illustrate Figure 6B A cross-sectional view showing the assembly process. DETAILED DESCRIPTION

[0037] The following is based on Figures 1 to 8 First, after describing the outline of the manufacturing apparatus of the glass article of the present invention, the homogenizing apparatus 6 which is the main part of the present invention will be described in detail.

[0038] like Figure 1 As shown, the manufacturing device 1 of the glass article of the present embodiment comprises: a glass melting furnace 2, which is a molten glass generating device and is arranged in the most upstream area; a clarification device 3, which is arranged on the downstream side of the glass melting furnace 2; a viscosity adjustment device 4, which is arranged on the downstream side of the clarification device 3 and mainly adjusts the viscosity of the molten glass; a forming device 5, which is arranged on the downstream side of the viscosity adjustment device 4 and forms the molten glass into a predetermined shape (here, for example, plate glass); and a homogenization device 6, which is arranged on the conveying flow path of the molten glass from the glass melting furnace 2 to the forming device 5. It should be noted that the homogenization device 6 mentioned here is equivalent to the processing device of the present invention.

[0039] The homogenizing device 6 is a device for stirring and mixing the molten glass flowing out of the clarifier 3 to achieve homogenization, and includes a first stirring device 8 connected to the clarifier 3 via a first supply pipe 7a and a second stirring device 9 connected to the first stirring device 8 via a second supply pipe 7b. The second stirring device 9 is connected to the viscosity adjusting device 4 via a third supply pipe 7c.

[0040] The forming device 5 is a device for continuously forming a glass ribbon that becomes a base of plate glass from molten glass, and for example, a device for performing forming based on a float process, a device for performing forming based on a rolling process, a device for performing forming based on an overflow down-draw process, and a device for performing forming based on a slit down-draw process, etc. It should be noted that the forming device 5 may be a device for forming glass articles other than plate glass, and as an example, may be a device for continuously forming a glass tube or a glass rod from molten glass using a Danner process.

[0041] When a plate glass as a glass article is manufactured using the manufacturing apparatus 1 of a glass article having the above-mentioned structure, Figure 5 The steps shown. First, glass raw materials are put into a glass melting furnace 2 to generate molten glass (molten glass generating process S1). Next, after the generated molten glass is clarified by a clarification device 3 (clarification process S2), a prescribed homogenization process is performed on the molten glass by a homogenization device 6 (homogenization process S3). Then, the viscosity of the molten glass subjected to the prescribed homogenization process is adjusted by a viscosity adjustment device 4 (viscosity adjustment process S4). The molten glass having the viscosity adjusted is supplied to a forming device 5, and plate glass is continuously formed from the molten glass (forming process S5). In this way, the manufacture of plate glass is continuously implemented. It should be noted that the homogenization process S3 mentioned here is equivalent to the processing process of the present invention.

[0042] Next, the homogenizing device 6 will be described in detail.

[0043] Figure 2 as well as Figure 3 The cross-sectional views of the homogenizing device 6 of this embodiment are shown respectively. Figure 2 as well as Figure 3 As shown, the homogenizing device 6 includes two stirring devices (first and second stirring devices 8 and 9 ), a refractory material 11 covering the first and second stirring devices 8 and 9 , and a housing 12 accommodating the first and second stirring devices 8 and 9 and the refractory material 11 .

[0044] The first stirring device 8 includes a first stirring tank 13 and a first stirrer 14 accommodated in the first stirring tank 13. The first stirring tank 13 mentioned here corresponds to the treatment tank of the present invention. The second stirring tank 15 described later also corresponds to the treatment tank of the present invention.

[0045] The first stirring tank 13 includes a bottomed cylindrical portion 13a and an upper cover portion 13b that closes the upper opening of the bottomed cylindrical portion 13a. The bottomed cylindrical portion 13a has an upper end (at the Figure 2 The first supply pipe 7a is connected to the first supply pipe 7a, and at its downstream end (at the Figure 2 The lower side in the middle) is connected to the second supply pipe 7b.

[0046] In addition, the first stirrer 14 has a shaft 14a and a plurality of stirring blades 14b installed along the length direction of the shaft 14a. The stirrer 14 is configured to stir the molten glass in the first stirred tank 13 by rotating a plurality of stirring blades 14b around the shaft 14a along with the rotation of the shaft 14a. In the present embodiment, a first motor 14c as a driving device is connected to the upper end of the shaft 14a, and the shaft 14a rotates in a predetermined direction along with the driving of the motor 14c. It is designed that the rotation center of the first stirrer 14 is consistent with the center line of the first stirred tank 13, more accurately, with the center line of the inner circumference of the bottomed cylindrical portion 13a. It should be noted that in the present embodiment, the shaft 14a is installed with four stirring blades 14b, but the number of stirring blades 14b can be appropriately increased or decreased. In addition, the stirring blade 14b can adopt any shape and configuration as long as it can play the stirring effect of the molten glass. Regarding the stirring blade 16b described later, the shape, number of pieces, and configuration are also arbitrary.

[0047] In addition, the second stirring device 9 includes a second agitation tank 15 and a second agitator 16 accommodated in the second agitation tank 15 .

[0048] The second stirring tank 15 includes a bottomed cylindrical portion 15a and an upper cover portion 15b that closes the upper opening of the bottomed cylindrical portion 15a. Figure 2 The upper side of the second supply pipe 7b is connected to the downstream end ( Figure 2 ) is connected to the third supply pipe 7c.

[0049] In addition, the second stirrer 16 has a shaft 16a and a plurality of stirring blades 16b installed along the length direction of the shaft 16a. The stirrer 16 is configured to stir the molten glass in the second stirred tank 15 by rotating the plurality of stirring blades 16b around the shaft 16a as the shaft 16a rotates. In this embodiment, a second motor 16c as a driving device is connected to the upper end of the shaft 16a, and the shaft 16a rotates in a predetermined direction as the motor 16c is driven. It is designed that the rotation center of the second stirrer 16 is consistent with the center line of the inner circumference of the bottomed cylindrical portion 15a of the second stirred tank 15.

[0050] The first and second stirring devices 8 and 9 of the above-mentioned structure are connected to each other and in series via the second supply pipe 7b while being housed in the housing 12. Therefore, the molten glass supplied to the homogenizing device 6 via the first supply pipe 7a is stirred and mixed by the first stirring device 8 and the second stirring device 9 in sequence from the upstream side.

[0051] The refractory 11 can be formed by any refractory, such as electrocast refractory such as high zirconia refractory, AZS refractory, alumina refractory, zirconium refractory, AZS refractory, alumina refractory, mullite refractory, silica refractory and other known refractory materials. High zirconia refractory refers to a refractory containing 80-100% ZrO2 by mass%. In addition, the refractory is not limited to the above-mentioned solid state. For example, it can also be configured to use a fluid amorphous refractory as a part of the refractory 11 and fill it between the shaped refractory and each stirring device 8, 9, between the shaped refractory and each supply pipe 7a, 7b, 7c, or between the shell 12 and the above-mentioned each stirring device 8, 9, between the shell 12 and each supply pipe 7a, 7b, 7c.

[0052] The housing 12 is, for example, Figure 2 as well as Figure 3 As shown, the housing 12 has a bottom 19, two pairs of side walls 20, 21 standing upright relative to the bottom 19, and an upper cover 22. The bottom 19, the side walls 20, 21, and the upper cover 22 are all in a flat plate shape, so the housing 12 is box-shaped as a whole.

[0053] In addition, the housing 12 in this embodiment, as Figure 4 As shown in the figure, when looking down at the housing 12 (when viewed from vertically above), it is in a rectangular shape. In this case, the housing 12 is in a rectangular shape as a whole. In addition, in this case, the arrangement direction of the first and second stirring devices 8 and 9 becomes the long side direction of the housing 12, and the direction orthogonal to the long side direction becomes the short side direction of the housing 12.

[0054] In addition, in this embodiment, if Figure 7 As shown, a first bearing surface 19a as a pressing force bearing portion for bearing a pressing force in a vertically upward direction is provided at the bottom 19 of the housing 12, and a second bearing surface 20a as a pressing force bearing portion for bearing a pressing force in a central side in the short side direction is provided at a pair of side wall portions 20 extending in the long side direction of the housing 12 (hereinafter referred to as the first side wall portion 20. In this case, a pair of side wall portions 21 extending in the short side direction of the housing 12 is hereinafter referred to as the second side wall portion 21.). In addition, in the present embodiment, an internal thread portion 20b (both refer to FIG. 2 ) as a tensile force bearing portion for bearing a tensile force in an outward direction in the short side direction is provided at the first side wall portion 20. Figure 3 ). In this example, Figure 3 As shown, a second bearing surface 20a and an internal thread portion 20b are respectively provided at two locations on the vertical upper side and the vertical lower side of the housing 12, and a second bearing surface 20a and an internal thread portion 20b are respectively provided on the first side wall portion 20 located on both sides in the short side direction.

[0055] In addition, the upper cover 22 of the housing 12 is provided with a fitting hole 22a that can be fitted with each stirring tank 13, 15. Thus, the upper cover 22 can be installed after the refractory 11 and each stirring tank 13, 15 are accommodated in the housing 12. It should be noted that, instead of the fitting hole 22a, a notch larger than each stirring tank 13, 15 can be provided in the upper cover 22, and the illustration is omitted. In this case, each stirring tank 13, 15 is fixed to the upper cover 21 by an arbitrary fixing member.

[0056] In addition, it is desirable that, as in the present embodiment, when the housing 12 is in a rectangular shape in a plan view ( Figure 4 ), Figure 3 The vertical cross section of the housing 12 shown is symmetrical about the vertical line X1 passing through the center of the short side direction thereof. Therefore, it is desirable that, when, for example, the second bearing surface 20a and the internal threaded portion 20b are provided on the first side wall portion 20 located on both sides of the short side direction of the housing 12 as described above, the cross-sectional shape of the first side wall portion 20 including the second bearing surface 20a and the internal threaded portion 20b is the same (symmetrical about the vertical line X1).

[0057] The housing 12 of the above structure, in other words, the homogenizing device 6 having the housing 12 of the above structure is suspended and supported by the suspension support device 23. The suspension support device 23 supports the upper part of the housing 12, thereby being able to suspend and support the housing 12. In this embodiment, as shown in FIG. Figure 3 As shown, the suspension support device 23 has a pair of bases 24 located on both sides of the short side direction of the shell 12 and a beam 25 extending along the short side direction of the shell 12 and connecting the two ends of the short side direction with each base 24. In this case, the shell 12 in a state where the refractory 11 and the first and second stirring devices 8 and 9 are accommodated is suspended and supported by fixing the beam 25 on the upper cover 22 of the shell 12. In this embodiment, three beams 25 are arranged on both sides of the long side direction of the two stirring devices 8 and 9, and the shell 12 is fixed on each beam 25, so as to suspend and support the shell 12. Thus, the shell 12 is supported by a floor surface 28a at the same height level as its upper part. On the other hand, the shell 12 and the floor surface 28b directly below the shell 12 are in a state separated vertically upward by a specified distance.

[0058] In addition, in the present embodiment, the suspension support device 23 further includes a posture adjustment unit 26 for adjusting the posture of the housing 12 during suspension support. The posture adjustment unit 26 is, for example, Figure 3As shown in FIG. 1 , the outer thread portion 27a and the inner thread portion 27b provided on the beam portion 25 and capable of being screwed with the outer thread portion 27a are formed. In addition, the outer thread portion 27a is configured so that the front end (lower end) of the outer thread portion 27a can abut against the base portion 24 by moving the outer thread portion 27a downward vertically while being screwed with the inner thread portion 27b. The combination of the outer thread portion 27a and the inner thread portion 27b is provided at the connection portion where each beam portion 25 is connected to the base portion 24 (see FIG. 1 ). Figure 4 Thus, by moving each external thread portion 27a in the vertical direction, each position in the longitudinal direction of the housing 12 or the vertical position on one side in the lateral direction can be adjusted, and the posture of the housing 12 when suspended can be adjusted.

[0059] Next, the homogenization step S3 using the homogenization device 6 having the above-described configuration will be described in detail.

[0060] like Fig. 6A As shown, the homogenization step S3 includes a preparation step S31 of preparing a homogenization device 6 having a housing 12 having the above-mentioned structure and a stirring step S32 of stirring the molten glass using the prepared homogenization device 6. The stirring step S32 is equivalent to the processing execution step of the present invention. Figure 6B As shown, the preparation step S31 includes a verticality adjustment step S311 of adjusting the predetermined verticality of the shell 12 alone before assembly, an assembly step S312 of assembling the homogenizer 6 by assembling the refractory material 11 and the first and second stirring devices 8 and 9 into the shell 12 in a state in which the verticality adjustment is completed, and an assembly step S313 of assembling the assembled homogenizer 6 at a predetermined position in a suspended support state.

[0061] (S31) Preparation process

[0062] (S311) Verticality Adjustment Process

[0063] In the verticality adjustment step S311, before the homogenizing device 6 having the housing 12 is suspended and supported, the verticality of the inner surface 20c of the first side wall portion 20 relative to the upper surface 19b of the bottom 19 of the housing 12 is adjusted. Figure 7As shown, the above-mentioned vertical adjustment is performed using a restraining clamp 29 that restrains the outer shell 12 from the outside. Here, the restraining clamp 29 has: a first pressing portion that applies a pressing force to the bottom 19 of the outer shell 12 in a vertically upward direction; and a second pressing portion that applies a pressing force to the first side wall portion 20 of the outer shell 12 in a short-side direction. In the present embodiment, the first pressing portion is composed of an external thread portion 30 and an internal thread portion 31 in the restraining clamp 29, which are arranged at a position opposite to the lower surface of the bottom 19 and are screwed together. In addition, the second pressing portion is composed of an external thread portion 32 and an internal thread portion 33 in the restraining clamp 29, which are arranged at a position opposite to the outer surface of the first side wall portion 20 of the outer shell 12 and are screwed together.

[0064] In addition, in the present embodiment, the restraining clamp 29 further includes a tensile force imparting portion, which is composed of a tensile threaded portion 34 provided at a position facing the outer surface of the first side wall portion 20 in the restraining clamp 29, and an internal threaded portion 20b provided at the first side wall portion 20 and capable of being screwed with the tensile threaded portion 34. In this case, the tensile threaded portion 34 is screwed with the internal threaded portion 20b via a cylindrical through hole 35 provided in the restraining clamp 29.

[0065] The verticality of the housing 12 is adjusted by using the restraining fixture 29 of the above structure. Figure 7 As shown, the housing 12 is placed on a predetermined position of the restraining jig 29. Then, the external threaded portion 30 constituting the first pressing portion is rotated to press its front end against the lower surface (first receiving surface 19a) of the bottom 19, and the external threaded portion 32 constituting the second pressing portion is rotated to press its front end against the outer surface (second receiving surface 20a) of the first side wall portion 20, thereby restraining the housing 12. As a result, the housing 12 is restrained and held by the restraining jig 29.

[0066] In this state, the verticality adjustment is performed. Specifically, first, the levelness of the upper surface 19b of the bottom 19 is measured using a level meter. At this time, the levelness is measured by approaching the upper surface 19b from the inner side of the housing 12. And, based on the measured levelness, for example, if Figure 7 In the case shown, the external threaded portion 30 located vertically below the left and right external threaded portions 30 is rotated to push up the bottom 19. By repeating the level measurement and pushing up the bottom 19, the level of the upper surface 19b of the bottom 19 is adjusted to a predetermined accuracy. It should be noted that the level measuring device can adopt any mechanism, for example, various level measuring mechanisms such as a level using a laser, a Y-type level, etc. can be applied.

[0067] In this state where the horizontality of the upper surface 19b of the bottom 19 is improved to a predetermined accuracy, the verticality of the inner surface 20c of the first side wall portion 20 relative to the upper surface 19b of the bottom 19 is adjusted. Specifically, first, a verticality measuring device is brought close to the upper surface 19b of the bottom 19 and the inner surface 20c of the first side wall portion 20 from the inner side of the housing 12 to measure the verticality of the inner surface 20c relative to the upper surface 19b. Then, based on the measured verticality, for example, if Figure 7 In the case shown in the figure, the external thread portion 32 located on the outer side in the short-side direction of the two upper and lower external thread portions 32 is rotated to push the first side wall portion 20 back to the center side in the short-side direction. In addition, when a stretching thread portion 34 as a stretching force applying portion is provided as in the present embodiment, the first side wall portion 20 is pulled back to the outer side in the short-side direction by rotating the stretching thread portion 34. By repeating the measurement of the verticality and the pushing and pulling back of the first side wall portion 20 in this way, the verticality of the inner surface 20c of the first side wall portion 20 relative to the upper surface 19b of the bottom 19 is adjusted to a predetermined accuracy.

[0068] When the target verticality at this time is, for example, 0.001 or less and the height dimension (vertical dimension) of the first side wall portion 20 is 1000 mm, the inner surface 20c of the side wall portion 20 is located between two ideal planes that are parallel to each other and separated by 1.0 mm. When the verticality is preferably 0.0005 or less and the height dimension of the first side wall portion 20 is 1000 mm, the inner surface 20c of the side wall portion 20 is located between two ideal planes that are separated by 0.5 mm. It should be noted that the verticality measuring device can adopt any structure, for example, a non-contact verticality measuring device using a laser, a contact verticality measuring device using a contactor, etc. can be applied.

[0069] (S312) Assembly process

[0070] After the verticality of the housing 12 is adjusted as described above, the homogenizing device 6 having the housing 12 is assembled. Specifically, after the refractory 11 is laid on the upper surface 19b of the bottom 19, the first and second stirring tanks 13 and 15 are arranged at predetermined positions in the long side direction. Then, each stirring tank 13 and 15 is vertically positioned with the outer peripheral surface of each stirring tank 13 and 15 as a reference. At this time, the verticality of the outer peripheral surface relative to the upper surface 19b of the bottom 19 can be adjusted, and the parallelism of the outer peripheral surface relative to the inner surface 20c of the first side wall portion 20 can also be adjusted. Then, the surroundings of each stirring tank 13 and 15 are filled with the refractory 11, and the upper cover portion 22 of the housing 12 is installed. Thus, the first side wall portions 20 located on both sides of the housing 12 in the short side direction are connected to each other via the upper cover portion 22, and the upper portions of the stirring tanks 13 and 15 are fitted into the fitting holes 22a of the upper cover portion 22, thereby fixing the stirring tanks 13 and 15 to the housing 12. As described above, most of the assembly of the homogenizer 6 is completed (see Figure 8 ).

[0071] (S313) Assembly process

[0072] After the upper cover 22 is installed as described above, the constraint of the outer shell 12 by the constraint clamp 29 is released, and the constraint clamp 29 is removed from the outer shell 12. Then, the homogenizer 6 is moved to a predetermined position (assembly position) on the glass article manufacturing device 1 and installed on the suspension support device 23. Specifically, the upper cover 22 of the outer shell 12 is fixed to the beam 25 of the suspension support device 23, so that the homogenizer 6 is assembled in a state where the outer shell 12 is suspended. Finally, the first and second agitators 14 and 16 on which the upper covers 13b and 15b of the stirring tanks 13 and 15 are installed are respectively inserted into the corresponding stirring tanks 13 and 15, and the motors 14c and 16c are fixed at predetermined positions, so that the assembly of the homogenizer 6 is completed ( Figure 3 status shown).

[0073] As described above, in the manufacturing device 1 of the glass article of the present invention and the manufacturing method thereof, it is set to suspend and support the shell 12 holding the stirring tanks 13 and 15. By supporting the shell 12 in this way, a force is applied to the shell 12 under the action of its own weight to restore the shell 12 to its original shape (the shape of the shell 12 when it is a single body). Therefore, even if the shell 12 is deformed during assembly or use, a force is applied to the shell 12 to restore the shape before deformation, so that the shape before deformation can be restored or approached. In addition, when the shell 12 is in the shape of a single body from the beginning of the suspension support, the shape is maintained under the action of its own weight. In summary, according to the manufacturing device 1 of the glass article of the present invention and the manufacturing method thereof, the tilting of the stirring tanks 13 and 15 during assembly or use of the homogenizing device 6 can be prevented as much as possible, and the reduction of the stirring efficiency (homogenization efficiency) or stirring capacity (homogenization capacity) caused by the tilting can be prevented. In other words, a good homogenization treatment can be stably performed on the molten glass.

[0074] In addition, in the present embodiment, the housing 12 has a rectangular shape in a plan view (see Figure 4 ), and the vertical cross section of the housing 12 is symmetrical about the vertical line X1 passing through the center of the short side direction thereof (refer to Figure 3 ). In addition, for this purpose, the verticality of the inner surface 20c of the first side wall portion 20 relative to the upper surface 19b of the bottom 19 constituting the shell 12 is set to be less than 0.001. In this way, by setting the shape of the shell 12, the center of gravity of the shell 12 can be set on the plumb line passing through the center of its short side direction in design. Therefore, if the shell 12 is in the designed shape from the beginning of assembly (suspension support), its state is maintained during use. Alternatively, when the center line of the shell 12 passing through the center of the short side direction in the vertical cross section of the shell 12 is inclined relative to the plumb line X1 during assembly, the dead weight of the center line in the direction consistent with the plumb line X1 acts on the shell 12. Therefore, regardless of the state during assembly, the shell 12 is always in the designed shape. In other words, it enjoys a sufficient shape restoration effect or shape maintenance effect brought by the suspension support, and can more reliably prevent the tilting of each stirring tank 13, 15.

[0075] In addition, in the present embodiment, the verticality of the inner surface 20c of the first side wall portion 20 relative to the upper surface 19b of the bottom 19 of the shell 12 is adjusted before the shell 12 is suspended and supported, so that the verticality can be adjusted in the state of the shell 12 alone. If the stirring tanks 13, 15 and the refractory 11 are not present, it is possible to Figure 7As shown, the verticality is measured on the inner side of the outer shell 12 while the outer side of the outer shell 12 is held (constrained) by a predetermined constraining fixture 29. Therefore, the verticality measurement and the correction of the outer shell 12 can be easily and repeatedly performed, and the verticality adjustment can be performed very easily. In addition, as in the present embodiment, not only a pressing portion (external thread portion 32, internal thread portion 33) but also a tensile force imparting portion (tensile thread portion 34, internal thread portion 20b) is provided, thereby not only being able to push the first side wall portion 20 back toward the center side in the short side direction but also being able to pull it back toward the outer side in the short side direction. Therefore, for example, in the case where a non-negligible warping occurs in the first side wall portion 20, the warping can be eliminated to ensure flatness and the verticality relative to the upper surface 19b of the bottom 19 can be adjusted with high precision.

[0076] It should be noted that, as in this embodiment, the housing 12 is rectangular in a plan view, thereby preventing deformation of the housing 12 in the long side direction. Therefore, only the verticality of the first side wall portions 20 located on both sides of the short side direction relative to the bottom 19 needs to be adjusted, which helps to reduce man-hours.

[0077] As mentioned above, although one embodiment of the present invention has been described, the manufacturing apparatus and the manufacturing method of the glass article of the present invention are not limited to the above-mentioned embodiment, and various forms can be adopted within the scope of the present invention.

[0078] For example, regarding the suspension support method of the shell 12, in the above-mentioned embodiment, it is described that the shell 12 is suspended and supported by fixing the upper cover portion 22 of the shell 12 to the beam portion 25 of the suspension support device 23, but it is of course not limited to this method. For example, the upper end portion of the first side wall portion 20 or the second side wall portion 21 may be fixed to the beam portion 25 by means of a connecting member, thereby suspending and supporting the shell 12, which is omitted in the figure. Alternatively, each stirring tank 13, 15 and the shell 12 may be fixed to each other, and the upper end portion of each stirring tank 13, 15 may be fixed to the beam portion 25, thereby suspending and supporting the shell 12. In short, if it is a component fixed to the shell 12, the shell 12 can be suspended and supported by fixing it to the beam portion 25.

[0079] In addition, in the above-mentioned embodiment, the case where the housing 12 is suspended and supported by fixing the beam portion 25 to the housing 12 is exemplified, but it is of course not limited to this. As long as the base portion 24 that constitutes the suspension support device 23 and is fixed to the floor surface 28a can be connected to the housing 12 (or the component of the homogenizer 6 fixed to the housing 12), the suspension support device 23 can be any structure.

[0080] In addition, regarding the verticality adjustment process S311, in the above-mentioned embodiment, components composed of external thread portions 30, 32 and internal thread portions 31, 33 are exemplified as the first and second pressing portions provided on the constraint clamp 29, but of course it is not limited to this. As long as the first side wall portion 20 can be pressed from the outside in the short side direction to the central side, or the bottom 19 can be pressed toward the vertical upper side, each pressing portion can adopt any structure. In addition, regarding the tensile force applying portion, it is not limited to the illustrated method (tensile thread portion 34 and internal thread portion 20b), and any structure can be adopted. Of course, the position and number of each pressing portion and tensile force applying portion can be appropriately set, and are not limited to the illustrated method.

[0081] In addition, in the above description, the present invention is applied to the homogenization step S3 for stirring molten glass to achieve homogenization and the housing 12 of the homogenization device 6 used in the step S3, but of course the present invention can also be applied to equipment for processes other than the homogenization step S3. For example, the present invention can also be applied to a flow adjustment step for achieving flow adjustment of molten glass by changing the cross-sectional area of ​​the outflow port provided at the lower end by raising and lowering the needle in the processing tank, and the flow adjustment tank used in the process, but the illustration is omitted. Further, the present invention is not limited to the above-mentioned exemplified processing steps, and the present invention can be applied to all processing steps performed using a processing device having an actuator that operates the processing tank in the processing tank.

[0082] In addition, in the above description, the present invention is applied to an apparatus and method for manufacturing plate glass as a glass product, but of course the present invention can also be applied to an apparatus or method for manufacturing glass products other than plate glass, such as other types of glass products such as tube glass and glass fiber.

[0083] Description of Reference Numerals

[0084] 1 Glass object manufacturing device

[0085] 2 Glass melting furnace

[0086] 3. Clarification device

[0087] 4. Viscosity adjustment device

[0088] 5 Forming device

[0089] 6 Homogenization device

[0090] 7a, 7b, 7c Supply pipe

[0091] 8.9 Stirring device

[0092] 11 Refractory

[0093] 12. Housing

[0094] 13, 15 Mixing tank

[0095] 13a, 15a bottomed cylindrical part

[0096] 13b, 15b Upper cover

[0097] 14, 16 Agitator

[0098] 14a, 16a shaft

[0099] 14b, 16b stirring blade

[0100] 14c, 16c motor

[0101] 19 Bottom

[0102] 20, 21 Side wall

[0103] 22 Upper cover

[0104] 23 Suspension support device

[0105] 24 base

[0106] 25 beam

[0107] 26 Posture adjustment unit

[0108] 28a, 28b Floor

[0109] 29 Constraint clamp

[0110] 30, 32 External thread

[0111] 31, 33 Internal thread

[0112] 34 Stretching thread

[0113] 35 Through hole

[0114] S1 Molten glass generation process

[0115] S2 Clarification process

[0116] S3 Homogenization process

[0117] S31 Preparation process

[0118] S311 Verticality Adjustment Process

[0119] S312 Assembly process

[0120] S313 Assembly process

[0121] S32 Mixing process

[0122] S4 Viscosity adjustment process

[0123] S5 Forming process

[0124] X1 plumb line.

Claims

1. A device for manufacturing glass products, comprising a glass melting furnace for generating molten glass, a processing device for performing a predetermined treatment on the generated molten glass, and a forming device for forming the molten glass subjected to the predetermined treatment, The manufacturing device of the glass article is characterized in that: The processing device includes a processing tank to which the molten glass is supplied and a housing for holding the processing tank, wherein the housing is suspended and supported. The housing is rectangular in shape when viewed from above, and The vertical cross section of the housing is symmetrical about a vertical line passing through the center of the short side of the vertical cross section. The treatment tank is a stirred tank in which a stirrer is accommodated. The molten glass supplied to the stirred tank is stirred by the rotation of the stirrer.

2. The manufacturing device for glass articles according to claim 1, wherein: The housing has a bottom and a pair of side walls standing upright relative to the bottom. The verticality of the inner surface of the side wall portion with respect to the upper surface of the bottom portion is 0.001 or less.

3. A method for manufacturing a glass article, comprising a glass generating step of generating molten glass, a processing step of subjecting the generated molten glass to a predetermined processing, and a forming step of forming the molten glass subjected to the predetermined processing, The method for manufacturing the glass article is characterized in that: The processing steps include: A preparation step of preparing a treatment device having a treatment tank to which the molten glass is supplied and a housing for holding the treatment tank; and a treatment execution step of executing the predetermined treatment on the molten glass using the prepared treatment device, In the preparation step, a housing for holding the treatment tank is suspended and supported, the housing is rectangular in a plan view, and a vertical cross section of the housing is symmetrical about a vertical line passing through the center of the short side direction of the vertical cross section. The treatment tank is a stirred tank in which a stirrer is accommodated. The molten glass supplied to the stirred tank is stirred by the rotation of the stirrer.

4. The method for manufacturing a glass article according to claim 3, wherein: The housing has a bottom and a pair of side walls standing upright relative to the bottom. In the preparation step, before the housing is suspended and supported, the verticality of the inner surface of the side wall portion relative to the upper surface of the bottom of the housing is adjusted.

Citation Information

Patent Citations

  • JP1980010446B2

  • Manufacturing method of glass plate, and agitator

    JP2015124107A

  • Molten glass supply apparatus and process for producing glass formed article

    CN102173560A

  • Method for producing glass substrate and device for producing glass substrate

    CN103476716A