Color filter substrate forming method and heating device

By subjecting the initial photoresist layer to low-temperature heating and vibration treatment after the exposure process, the problem of uneven color during the exposure of the liquid crystal display panel was solved, and the uniformity of the photoresist layer thickness and the surface flatness were improved, thus improving the display effect.

CN114690472BActive Publication Date: 2024-11-19INESA (KUNSHAN) DISPLAY MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011639468.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-31
Publication Date
2024-11-19
Estimated Expiration
2040-12-31

AI Technical Summary

Technical Problem

The exposure process of existing liquid crystal display panels is prone to color unevenness, mainly due to the uneven temperature at the contact points during exposure, which leads to differences in the initial photoresist layer thickness.

Method used

After the exposure process, the initial photoresist layer is heated by a low-temperature first treatment, especially the contact area, and the use of a vibration unit is combined to ensure uniform heat distribution and transfer, followed by the development process.

Benefits of technology

It effectively reduces or eliminates the initial photoresist layer thickness difference, improves the surface flatness of the photoresist layer, avoids color unevenness, and improves the image quality of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114690472B_ABST
    Figure CN114690472B_ABST
Patent Text Reader

Abstract

A method for forming a color filter substrate and a heating device, wherein the method for forming a color filter substrate comprises: providing a substrate, the substrate comprising a first surface and a second surface opposite to each other; forming an initial photoresist layer on the first surface; performing an exposure process on the initial photoresist layer; after the exposure process, performing a first treatment on the initial photoresist layer, and the first treatment has a first temperature; after the first treatment, performing development on the initial photoresist layer to remove part of the initial photoresist layer; after the development process, performing a second treatment on the initial photoresist layer to solidify the initial photoresist layer to form a photoresist layer, and the second treatment has a second temperature, and the second temperature is greater than the first temperature. The method can reduce or even avoid the color unevenness problem caused by the contact point during exposure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of display technology, and in particular to a method for forming a color filter substrate and a heating device. Background Art

[0002] Liquid crystal display substrates are currently the most widely used flat panel displays due to their high display quality, low price, and ease of portability. They have gradually become displays with high-resolution color screens that are widely used in various electronic devices such as mobile phones, personal digital assistants (PDAs), digital cameras, computer screens, or laptop screens.

[0003] Most of the LCD panels on the market are backlight LCD panels, which include an LCD substrate and a backlight module. Usually, the LCD substrate is composed of a color filter substrate (CF), a thin film transistor color filter substrate (TFT array substrate), and a liquid crystal layer (LCL) disposed between the two substrates. Photolithography technology is widely used in the display panel industry. With the development of science and technology, large-size glass substrates have higher and higher requirements for photolithography technology, which is related to the quality of the finished display panel.

[0004] However, in the conventional exposure process, the contact points during exposure easily cause color unevenness. Summary of the invention

[0005] The technical problem solved by the present invention is to provide a method for forming a color filter substrate and a heating device to reduce color unevenness.

[0006] In order to solve the above technical problems, the technical solution of the present invention provides a method for forming a color filter substrate, comprising: providing a substrate, the substrate comprising a first surface and a second surface opposite to each other; forming an initial photoresist layer on the first surface; performing an exposure process on the initial photoresist layer; after the exposure process, performing a first treatment on the initial photoresist layer, and the first treatment has a first temperature; after the first treatment, developing the initial photoresist layer to remove a portion of the initial photoresist layer; after the development process, performing a second treatment on the initial photoresist layer to solidify the initial photoresist layer to form a photoresist layer, and the second treatment has a second temperature, and the second temperature is greater than the first temperature.

[0007] Optionally, the initial photoresist layer includes a plurality of contact areas and a plurality of non-contact areas, and the contact areas are located between adjacent non-contact areas; and the first treatment heats the contact areas.

[0008] Optionally, the contact area is in the shape of a regular polygon.

[0009] Optionally, the regular polygon is a regular octagon.

[0010] Optionally, the first temperature ranges from 90 degrees Celsius to 110 degrees Celsius.

[0011] Optionally, the second temperature ranges from 220 degrees Celsius to 250 degrees Celsius.

[0012] Optionally, the processing time range of the first processing is 2 seconds to 5 seconds.

[0013] Optionally, the method for exposing the initial photoresist layer includes: providing an exposure device, the exposure device including: an exposure platform and a plurality of mutually separate support pillars located on the surface of the exposure platform, and the position of each support pillar corresponds to the position of the contact area; placing the second surface on the support pillars; and using the exposure device to illuminate the initial photoresist layer.

[0014] Optionally, the method for performing a first treatment on the initial photoresist layer includes: providing a heating device, the heating device including: a heating disk and a plurality of mutually discrete heating columns located on the surface of the heating disk, and the position of each heating column corresponds to a contact area respectively; placing the second surface on the heating columns; and using the heating device to heat the second surface.

[0015] Optionally, the heating device further includes: a vibration unit for vibrating the heating column; and the method for performing a first treatment on the initial photoresist layer further includes: driving the substrate to vibrate by vibrating the heating column.

[0016] Correspondingly, the technical solution of the present invention further provides a heating device, comprising: a heating plate; and a plurality of mutually separate heating columns located on the surface of the heating plate, wherein the cross-sectional shape of the heating columns is a regular polygon.

[0017] Optionally, the regular polygon is a regular octagon.

[0018] Optionally, it also includes: a vibration unit, used to vibrate the heating column.

[0019] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0020] In the method for forming a color filter substrate provided by the technical solution of the present invention, the initial photoresist layer is subjected to a first treatment after an exposure process and before a development process. Since the first treatment has a first temperature, the first temperature is lower than a second temperature, and the second temperature is the temperature used in the second treatment for curing the initial photoresist layer, the first treatment with a relatively low temperature can make the heated portion of the initial photoresist layer absorb energy to form a high potential field. Since the high potential field tends to transfer to the low potential field, the initial photoresist layer can be locally extended on the first surface of the substrate, thereby reducing or even eliminating the difference in the film thickness of the initial photoresist layer after exposure, so that the surface flatness of the initial photoresist layer is better, thereby reducing or even avoiding the generation of color unevenness.

[0021] Furthermore, after the exposure treatment, the thickness of the contact area of ​​the initial photoresist layer is higher than that of the non-contact area. By performing the first treatment to heat the thicker contact area at a low temperature, the thicker initial photoresist layer can accurately absorb energy to become a high potential field. The film layer of the thicker contact area can quickly extend toward the film layer of the thinner non-contact area, further allowing the thickness of the initial photoresist layer to be balanced quickly, so that the surface flatness of the initial photoresist layer is better, thereby reducing the occurrence of color unevenness.

[0022] Furthermore, by heating the contact area through the first treatment, when the contact area is a regular polygon, especially a regular octagon, it can make the heating uniform and increase the heating area, and there can also be local traction at the angle of the polygon, which is beneficial to uniformly improve the local extension of the initial photoresist layer, so that the flatness of the initial photoresist layer is improved better.

[0023] Furthermore, the processing time of the first treatment ranges from 2 seconds to 5 seconds. The significance of selecting the processing time is that: if the processing time is less than 2 seconds, the first treatment acts on the substrate for too short a time, and thus the effect of heating the initial photoresist layer at a relatively low temperature is weak, and the initial photoresist layer cannot be locally extended; if the processing time is greater than 5 seconds, even if the heating temperature of the initial photoresist layer is relatively low, the initial photoresist layer is easily overheated due to the long time of acting on the substrate, resulting in the solidification of the material of the initial photoresist layer, and the surface thickness uniformity of the initial photoresist layer cannot be improved, and the subsequent development effect of the initial photoresist layer is affected.

[0024] Furthermore, the method for performing a first treatment on the initial photoresist layer also includes: by vibrating the heating column, the substrate in contact with the heating column also locally vibrates, and the vibration can enhance the effect of the heated portion of the initial photoresist layer absorbing energy, thereby quickly becoming a high potential field, and at the same time can accelerate the local extension of the initial photoresist layer on the first surface of the substrate, thereby enhancing the local extension effect of the initial photoresist layer, thereby improving the surface flatness of the initial photoresist layer and reducing the time.

[0025] In the heating device provided by the technical solution of the present invention, when the cross-sectional shape of the heating column is a regular polygon, the regular polygon heating column can provide evenly distributed heat to the object contacting its surface, and the heating area is large. There is a local traction force at the angle of the regular polygon, which makes the effect of raising the potential field better, thereby improving the extension effect of the part of the initial photoresist layer contacting its surface.

[0026] Furthermore, when the cross-section of the heating column is formed as a regular octagon, the regular octagonal heating column can provide evenly distributed heat to the object contacting its surface, and the heating area is large. It can also have local traction at the angle of the regular octagon, which is further beneficial to improve the local extension effect of the initial photoresist layer contacting its surface.

[0027] Furthermore, the heating device also includes: a vibration unit, which can drive the heating column to vibrate, thereby driving the substrate in contact with the surface of the heating column to also locally vibrate, which is beneficial to improving the surface flatness of the initial photoresist layer and reducing the time. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figures 1 to 3 is a schematic structural diagram of each step of a method for forming a color filter substrate in one embodiment;

[0029] Figures 4 to 8 It is a structural schematic diagram of each step of a method for forming a color filter substrate in one embodiment of the present invention. DETAILED DESCRIPTION

[0030] It should be noted that the terms “surface” and “on” in this specification are used to describe relative positional relationships in space and are not limited to direct contact.

[0031] As described in the background art, the performance of the color filter substrate formed by the existing method is poor.

[0032] The following is a detailed description of the reasons why the performance of the color filter substrate is poor, with reference to the accompanying drawings. Figures 1 to 3 The present invention is a structural schematic diagram of each step of a method for forming a color filter substrate.

[0033] Please refer to Figure 1, providing a substrate 100; forming an initial photoresist layer 110 on the substrate 100;

[0034] Please refer to Figure 2 , performing an exposure process on the initial photoresist layer 110 .

[0035] Please refer to Figure 3 After the exposure process, a development process is performed to form the initial photoresist layer 110 into a photoresist layer 120 .

[0036] In the above method, the initial photoresist layer 110 is exposed to light so that the material of the initial photoresist layer 110 in the portion exposed to light reacts, while the material of the initial photoresist layer 110 in the portion not exposed to light does not change. The alkaline solution used in the development process dissolves the reacted material of the initial photoresist layer 110, while the unreacted initial photoresist layer 110 remains to form the photoresist layer 120, thereby forming a desired pattern.

[0037] However, during the exposure process, the substrate 100 needs to be placed on an exposure machine, specifically, the substrate 100 is located on a number of separate support columns 132, and the support columns 132 are located on the surface of the exposure platform 131. The temperature of the substrate 100 that contacts the support columns 132 is different from the temperature of the substrate 100 that does not contact the support columns 131, so that the initial photoresist layer 110 is heated unevenly, so that the thickness of the formed photoresist layer 120 is different, which easily leads to color unevenness.

[0038] In order to solve the technical problem, the embodiment of the present invention provides a method for forming a color filter substrate and a heating device, wherein the method for forming a color filter substrate comprises: performing an exposure process on the initial photoresist layer; after the exposure process, performing a first treatment on the initial photoresist layer, and the first treatment has a first temperature; after the first treatment, developing the initial photoresist layer to remove part of the initial photoresist layer. By performing the first treatment on the initial photoresist layer after the exposure process and before the development process, since the first treatment has a first temperature, and the first temperature is lower than the second temperature, the first treatment with a lower temperature can make the heated part of the initial photoresist layer absorb energy and thus become a high potential field. Since the high potential field tends to transfer to the low potential field, the initial photoresist layer can be locally extended on the first surface of the substrate, thereby reducing or even eliminating the difference in the film thickness of the initial photoresist layer after exposure, so that the surface flatness of the initial photoresist layer is better, thereby reducing or even avoiding the generation of color unevenness.

[0039] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0040] Figures 4 to 8 It is a structural schematic diagram of each step of a method for forming a color filter substrate in one embodiment of the present invention.

[0041] Please refer to Figure 4 , providing a substrate 200, wherein the substrate 200 includes a first surface 201 and a second surface 202 opposite to each other.

[0042] The substrate 200 is made of a transparent material. In this embodiment, the substrate 200 is a glass substrate. In other embodiments, the substrate may also be a plastic substrate.

[0043] Please refer to Figure 5 , an initial photoresist layer 210 is formed on the first surface 201 .

[0044] In this embodiment, the initial photoresist layer 210 includes a plurality of contact regions I and a plurality of non-contact regions II, and the contact regions I are located between adjacent non-contact regions II.

[0045] The method for forming the initial photoresist layer 210 includes: coating a photoresist material on the surface of the substrate 200 by a coating process; and heating the photoresist material to adhere to the surface of the substrate 200 to form the initial photoresist layer 210 .

[0046] The material of the initial photoresist layer 210 includes: photoresist.

[0047] In this embodiment, the initial photoresist layer 210 is a positive photoresist. In the subsequent exposure process, the initial photoresist layer 210 of the illuminated portion reacts, and then in the subsequent development process, it reacts with the developer to be dissolved and removed, while the unilluminated portion does not dissolve in the developer and is retained, thereby forming a pattern on the substrate 200.

[0048] In other embodiments, the initial photoresist layer is a negative photoresist.

[0049] Please refer to Figure 6 , performing an exposure process on the initial photoresist layer 210 .

[0050] The method for exposing the initial photoresist layer 210 includes: providing an exposure device 300, wherein the exposure device 300 includes: an exposure platform 301 and a plurality of mutually separate support pillars 302 located on the surface of the exposure platform 201, and the positions of the support pillars 302 respectively correspond to the positions of the contact areas I; placing the second surface 202 on the support pillars 302; and using the exposure device 300 to illuminate the initial photoresist layer 210.

[0051] It should be noted that, in the exposure process, the substrate 200 needs to be placed on an exposure machine. Specifically, the substrate 200 is located on a number of separate support pillars 302. The temperature of the substrate 200 that contacts the support pillars 302 is different from the temperature of the substrate 200 that does not contact the support pillars 302. This causes the contact area I and the non-contact area II of the initial photoresist layer 210 to be heated unevenly, so that after the exposure process, there is a difference in the thickness of the initial photoresist layer 210, which is specifically manifested as the thickness of the contact area I being greater than the thickness of the non-contact area II.

[0052] Please refer to Figure 7 After the exposure process, the initial photoresist layer 210 is subjected to a first treatment, and the first treatment has a first temperature.

[0053] The first temperature ranges from 90 degrees Celsius to 110 degrees Celsius.

[0054] After the exposure process and before the subsequent development process, the initial photoresist layer 210 is subjected to a first treatment. Since the first treatment has a first temperature, the first temperature is lower than a second temperature, and the second temperature is the temperature used in the second treatment for curing the initial photoresist layer 210, the first treatment with a relatively low temperature can make the heated portion of the initial photoresist layer 210 absorb energy and thus become a high potential field. Since the high potential field tends to transfer to the low potential field, the initial photoresist layer 210 can be locally extended on the first surface 201 of the substrate 200, thereby reducing or even eliminating the difference in the film thickness of the initial photoresist layer 210 after exposure, so that the surface flatness of the initial photoresist layer 210 is better, thereby reducing or even avoiding the generation of color unevenness.

[0055] Specifically, the first treatment heats the contact area I.

[0056] It should be noted that the first treatment directly heats a portion of the second surface 202 of the substrate 200, and the area where the first treatment heats the portion of the second surface 202 of the substrate 200 corresponds to the contact area I. Since the initial photoresist layer 210 is located on the surface of the substrate 200, there is heat conduction during the heating process, thereby achieving the ability to heat the portion of the initial photoresist layer 210 that is in contact with the heated substrate 200, that is, the first treatment heats the contact area I.

[0057] The method for performing a first treatment on the initial photoresist layer 210 includes: providing a heating device 400, wherein the heating device 400 includes: a heating disk 401 and a plurality of mutually separate heating columns 402 located on the surface of the heating disk 401, and the positions of the heating columns 402 correspond to the contact areas I respectively; placing the second surface 202 on the heating columns 402; and heating the second surface 202 using the heating device 400.

[0058] After the exposure treatment, the thickness of the contact area I of the initial photoresist layer 210 is higher than the thickness of the non-contact area II. By performing the first treatment to heat the thicker contact area I at a low temperature, the thicker initial photoresist layer 210 can accurately absorb energy to become a high potential field. The film layer of the thicker contact area I can quickly extend to the film layer of the thinner non-contact area II, further making the thickness of the initial photoresist layer 210 balanced quickly, so that the surface flatness of the initial photoresist layer 210 is better, thereby reducing the occurrence of color unevenness.

[0059] The processing time of the first processing ranges from 2 seconds to 5 seconds.

[0060] The significance of selecting the treatment time is that: if the treatment time is less than 2 seconds, the first treatment acts on the substrate 200 for too short a time, and thus the effect of heating the initial photoresist layer 210 at a relatively low temperature is weak, and the initial photoresist layer 210 cannot be locally extended; if the treatment time is greater than 5 seconds, even if the heating temperature of the initial photoresist layer 210 is relatively low, the initial photoresist layer 210 is easily overheated due to the long action time on the substrate 200, resulting in the material of the initial photoresist layer 210 being solidified, and the surface thickness uniformity of the initial photoresist layer 210 cannot be improved, and the subsequent development effect of the initial photoresist layer 210 is affected.

[0061] The contact area I is in the shape of a regular polygon.

[0062] In this embodiment, the contact area I is in a regular octagonal shape.

[0063] The contact area I is heated by the first treatment. When the contact area I is a regular polygon, especially a regular octagon, it can be heated evenly and the heated area can be increased. There can also be local traction at the angle of the regular polygon, which is beneficial to uniformly improve the local extension of the initial photoresist layer 210, so that the flatness of the initial photoresist layer 210 is better.

[0064] In other embodiments, the shape of the contact area may also be other regular polygons.

[0065] In this embodiment, the heating device 400 further includes: a vibration unit (not shown in the figure) for vibrating the heating column 402 .

[0066] In this embodiment, the method of performing the first treatment on the initial photoresist layer 210 further includes: vibrating the heating column 402 to drive the substrate 200 to vibrate.

[0067] By vibrating the heating column 402, the substrate 200 in contact with the heating column 402 also locally micro-vibrates. The vibration can enhance the effect of the heated portion of the initial photoresist layer 210 absorbing energy, thereby quickly becoming a high potential field. At the same time, it can accelerate the local extension of the initial photoresist layer 210 on the first surface 201 of the substrate 200, thereby enhancing the local extension effect of the initial photoresist layer 210, thereby improving the surface flatness of the initial photoresist layer 210 and reducing the time.

[0068] Please refer to Figure 8 After the first treatment, the initial photoresist layer 210 is developed to remove a portion of the initial photoresist layer 210 .

[0069] In this embodiment, through the development process, the portion of the initial photoresist layer 210 that is illuminated is dissolved and removed, and the portion of the initial photoresist layer 210 that is not illuminated is retained, thereby forming a pattern on the substrate 200 .

[0070] Please continue to refer to Figure 8 After the development process, the initial photoresist layer 210 is subjected to a second treatment to cure the initial photoresist layer 210 to form a photoresist layer 220, and the second treatment has a second temperature, and the second temperature is greater than the first temperature.

[0071] The second temperature ranges from 220 degrees Celsius to 250 degrees Celsius.

[0072] The present invention also provides a heating device 400, please continue to refer to Figure 7 , including: a heating plate 401; and a plurality of mutually separate heating columns 402 located on the surface of the heating plate 401, wherein the cross-sectional shape of the heating columns 402 is a regular polygon.

[0073] When the cross-sectional shape of the heating column 402 is a regular polygon, the regular polygon heating column 402 can provide evenly distributed heat to the object contacting its surface, and the heating area is large. At the same time, there is a local traction force at the angle of the regular polygon, which makes the effect of raising the potential field better, thereby improving the fluidity of the portion of the initial photoresist layer 210 contacting its surface.

[0074] In this embodiment, the regular polygon is a regular octagon.

[0075] When the cross-section of the heating column 402 is formed as a regular octagon, the regular octagonal heating column 402 can provide evenly distributed heat to the object contacting its surface, and the heating area is large. It can also have local traction at the angle of the regular polygon, which is further beneficial to improve the local extension effect of the initial photoresist layer 210 contacting its surface.

[0076] In this embodiment, the heating device further includes: a vibration unit, which is used to make the heating column 402 vibrate.

[0077] The heating device 400 also includes: a vibration unit (not shown in the figure), which can drive the heating column 402 to vibrate, thereby driving the substrate 200 in contact with the surface of the heating column 402 to also locally vibrate, which is beneficial to improving the surface flatness of the initial photoresist layer 210 and reducing the time.

[0078] In other embodiments, the heating device may not include the vibration unit.

[0079] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for forming a color filter substrate, characterized in that: include: Providing a substrate, the substrate comprising a first side and a second side opposite to each other; forming an initial photoresist layer on the first surface; performing an exposure process on the initial photoresist layer; After the exposure process, the initial photoresist layer is subjected to a first treatment, wherein the first treatment has a first temperature; After the first treatment, developing the initial photoresist layer to remove a portion of the initial photoresist layer; After the development process, performing a second treatment on the initial photoresist layer to solidify the initial photoresist layer to form a photoresist layer, wherein the second treatment has a second temperature greater than the first temperature; The initial photoresist layer includes a plurality of contact areas and a plurality of non-contact areas, wherein the contact areas are located between adjacent non-contact areas; the first treatment heats the contact areas; after the exposure process, the thickness of the contact areas on the initial photoresist layer is greater than the thickness of the non-contact areas; The method for exposing the initial photoresist layer comprises: providing an exposure device, the exposure device comprising: an exposure platform and a plurality of mutually separate support pillars located on the surface of the exposure platform, and the position of each support pillar corresponds to the position of the contact area; placing the second surface on the support pillars; and using the exposure device to illuminate the initial photoresist layer.

2. The method for forming a color filter substrate according to claim 1, wherein: The contact area is in the shape of a regular polygon.

3. The method for forming a color filter substrate according to claim 2, wherein: The regular polygon is a regular octagon.

4. The method for forming a color filter substrate according to claim 1, wherein: The first temperature ranges from 90 degrees Celsius to 110 degrees Celsius.

5. The method for forming a color filter substrate according to claim 1, wherein: The second temperature ranges from 220 degrees Celsius to 250 degrees Celsius.

6. The method for forming a color filter substrate according to claim 1, wherein: The processing time of the first processing ranges from 2 seconds to 5 seconds.

7. The method for forming a color filter substrate according to claim 1, wherein: The method for performing a first treatment on the initial photoresist layer includes: providing a heating device, the heating device including: a heating disk and a plurality of mutually separate heating columns located on the surface of the heating disk, and the position of each heating column corresponds to the contact area respectively; placing the second surface on the heating columns; and using the heating device to heat the second surface.

8. The method for forming a color filter substrate according to claim 7, wherein: The heating device further includes: a vibration unit for vibrating the heating column; and the method for performing a first treatment on the initial photoresist layer further includes: driving the substrate to vibrate by vibrating the heating column.