A micromechanical resonator with a coupling structure and a method for preparing the same

By adding a coupling structure to the vibration structure of the micromechanical resonator, the low thermal elastic loss characteristics of the single crystal silicon layer are used to solve the problems of low Q value and poor temperature stability in the prior art, and high Q value and low impedance are achieved Micromechanical resonator design.

CN114866059BActive Publication Date: 2024-11-15WUHAN UNIV
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202210422461.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-21
Publication Date
2024-11-15
Estimated Expiration
2042-04-21

AI Technical Summary

Technical Problem

The Q value of existing micromechanical resonators is low and have poor temperature stability, making it difficult to optimize their energy loss and frequency temperature coefficient at the same time.

Method used

A micromechanical resonator with a coupling structure is designed. By adding a coupling structure to the vibration structure of the resonant oscillator, the low thermal elastic loss characteristics of the single crystal silicon layer are used to adjust the size of the coupling structure for modal coupling, thereby improving Q and reduce the frequency temperature coefficient.

Benefits of technology

It effectively improves the Q value and temperature stability of micromechanical resonators, combines the advantages of capacitive and piezoelectric resonators to realize high Q value and low impedance micromechanical resonators.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114866059B_ABST
    Figure CN114866059B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of microelectronic technology, and discloses a micromechanical resonator with a coupling structure and a preparation method thereof. The micromechanical resonator includes a substrate silicon wafer and a resonator structure layer, the substrate silicon wafer has a cavity structure, the resonator structure layer includes a resonant oscillator and an anchor structure, the resonant oscillator includes a vibration structure and a coupling structure, the vibration structure is a piezoelectric stacked structure, the coupling structure only includes device layer silicon, the number of the coupling structure is one or more, the coupling structure is connected to the vibration structure, and the coupling structure is located outside the vibration structure, the resonant oscillator is connected to the substrate silicon wafer through the anchor structure, and the resonant oscillator and the anchor structure are both suspended above the cavity structure of the substrate silicon wafer. The present invention can improve the Q value and temperature stability of the resonator.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of microelectronic technology, and more specifically, relates to a micromechanical resonator with a coupling structure and a preparation method thereof. Background Art

[0002] In recent years, microelectromechanical systems (MEMS) resonators have received increasing attention and have been increasingly widely used in frequency reference, clock, sensor, and filter fields. MEMS devices have the advantages of small size, light weight, low power consumption, high stability, strong resistance to external interference, and batch manufacturing. MEMS resonators can be mainly divided into capacitive and piezoelectric types. Capacitive micromechanical resonators have a very high quality factor (Q value), but their impedance is very large, which can easily cause circuit impedance mismatch problems. Although the Q value of piezoelectric micromechanical resonators is lower than that of capacitive resonators, their impedance is very low.

[0003] The main performance parameters of MEMS resonators include resonant frequency, quality factor (Q), dynamic impedance, and frequency temperature coefficient. Among them, Q value is the most important performance parameter of MEMS resonators. A high Q value can reduce the dynamic impedance of the resonator, reduce the phase noise of the system, and improve the frequency stability of the oscillator. The energy loss mechanism of the Q value of MEMS resonators mainly consists of five parts: air damping loss (Q air ), thermoelastic loss (Q TED ), material loss (Q material ), anchor loss (Q anchor ) and electrical load losses (Q load ),Right now:

[0004]

[0005] Air damping losses can be reduced by vacuum packaging. Electrical load losses can be reduced by using metals with low resistivity and thicker metal electrodes. Therefore, thermoelastic losses and anchor point losses are the main physical mechanisms for energy loss in micromechanical resonators.

[0006] The frequency temperature coefficient is another key technical parameter of the resonator. The frequency temperature coefficient of a micromechanical resonator that has not been temperature compensated is generally large, so when used as a frequency reference, the micromechanical resonator needs to be temperature compensated. Common temperature compensation methods include passive temperature compensation and active temperature compensation. Passive temperature compensation methods include using heavily doped silicon, adjusting crystal orientation, and depositing silicon oxide. Active temperature compensation is mainly circuit compensation.

[0007] How to optimize the Q value of a micromechanical resonator while improving the temperature stability of the resonator is a technical problem that needs to be solved in this field. Summary of the invention

[0008] The present invention solves the problems of low Q value and poor temperature stability of the micromechanical resonator in the prior art by providing a micromechanical resonator with a coupling structure and a preparation method thereof.

[0009] The present invention provides a micromechanical resonator with a coupling structure, comprising: a substrate silicon wafer and a resonator structure layer; the substrate silicon wafer has a cavity structure; the resonator structure layer comprises a resonant vibrator and an anchor point structure, and the resonant vibrator comprises a vibration structure and a coupling structure;

[0010] The vibration structure is a piezoelectric stacked structure, the coupling structure only includes device layer silicon, the number of the coupling structure is one or more, the coupling structure is connected to the vibration structure, and the coupling structure is located outside the vibration structure;

[0011] The resonant oscillator is connected to the substrate silicon wafer through the anchor structure, and both the resonant oscillator and the anchor structure are suspended above the cavity structure of the substrate silicon wafer.

[0012] Preferably, the operating mode of the micromechanical resonator is one of a width extension mode, a width extension high-order mode, and a square plate extension mode;

[0013] The vibration mode of the vibration structure is a width extension mode or a high-order width extension mode, and the vibration mode of the coupling structure is a radial extension mode.

[0014] Preferably, the piezoelectric stack structure is composed of device layer silicon, piezoelectric film, upper electrode layer and oxide layer from bottom to top, or the piezoelectric stack structure is composed of device layer silicon, dielectric layer, lower electrode layer, piezoelectric film, upper electrode layer and oxide layer from bottom to top.

[0015] Preferably, the material of the piezoelectric film is one of aluminum nitride, zinc oxide or lead zirconate titanate.

[0016] Preferably, the coupling structure is a circular plate structure.

[0017] Preferably, the radius of the coupling structure adopts a specific geometric size, under which the Q value of the micromechanical resonator at the operating frequency is the highest;

[0018] The specific geometric dimensions are selected in the following manner: obtaining the operating frequency information and overall dimension information of the micromechanical resonator, and obtaining the material information and thickness information of each layer in the piezoelectric stack structure; based on the above-obtained information, simulating the coupling structure under different geometric dimensions to obtain the Q value corresponding to the micromechanical resonator; and selecting the geometric dimensions of the coupling structure corresponding to the simulation condition with the highest Q value as the specific geometric dimensions.

[0019] Preferably, the device layer silicon is N-type doped, and the doping concentration is greater than 10 19 cm -1 .

[0020] Preferably, the anchor point structure is located at a vibration node position of the resonant oscillator, the number of the anchor point structures is one or more, and the anchor point structure is a T-shaped beam, an L-shaped beam or a folded beam structure.

[0021] Preferably, the vibration structure is a square plate structure or a circular plate structure.

[0022] On the other hand, the present invention provides a method for preparing the above-mentioned micromechanical resonator with a coupling structure, comprising the following steps:

[0023] Step 1, obtaining an SOI wafer with a cavity structure, wherein the SOI wafer includes a substrate silicon wafer, a buried oxide layer and a device layer silicon from bottom to top;

[0024] Step 2, depositing a piezoelectric film and an upper electrode layer in sequence on the device layer silicon, and performing a patterning process on the upper electrode layer;

[0025] Step 3, depositing an oxide layer on the upper electrode layer;

[0026] Step 4, etching the oxide layer to obtain an upper electrode through hole and expose the upper electrode layer;

[0027] Step 5, etching the oxide layer and the piezoelectric film to expose the device layer silicon;

[0028] Step 6: depositing metal and patterning to form a metal pad;

[0029] Step 7, etching to obtain a vibration structure and a coupling structure;

[0030] Alternatively, include the following steps:

[0031] Step 1, obtaining an SOI wafer with a cavity structure, wherein the SOI wafer includes a substrate silicon wafer, a buried oxide layer and a device layer silicon from bottom to top;

[0032] Step 2, sequentially depositing a dielectric layer and a lower electrode layer on the device layer silicon;

[0033] Step 3, depositing a piezoelectric film and an upper electrode layer on the lower electrode layer in sequence, and performing a patterning process on the upper electrode layer;

[0034] Step 4, depositing an oxide layer on the upper electrode layer;

[0035] Step 5, etching the oxide layer to obtain an upper electrode through hole and expose the upper electrode layer;

[0036] Step 6, etching the oxide layer and the piezoelectric film to expose the lower electrode layer;

[0037] Step 7, etching the oxide layer, the piezoelectric film, the lower electrode layer and the dielectric layer to expose the device layer silicon;

[0038] Step 8: depositing metal and patterning to form a metal pad;

[0039] Step 9: Etching to obtain the vibration structure and the coupling structure.

[0040] One or more technical solutions provided in the present invention have at least the following technical effects or advantages:

[0041] In the invention, by adding a coupling structure to the vibration structure of the resonant oscillator of the micromechanical resonator, the vibration structure and the coupling structure can be modally coupled by adjusting the size of the coupling structure. Since the coupling structure is a single crystal silicon layer, its thermoelastic loss is very small; after adding the coupling structure, the energy stored in the resonator in one vibration cycle increases, while the energy consumed hardly increases, so the thermoelastic loss of the micromechanical resonator is reduced, thereby improving the Q value of the resonator. After adding the coupling structure to the vibration structure of the resonant oscillator, since the frequency temperature coefficient of the vibration mode of the coupling structure is lower than that of the vibration structure of the resonant oscillator, the frequency temperature coefficient of the resonator can be reduced as a whole, thereby improving the temperature stability of the resonator. In the present invention, the vibration structure of the resonant oscillator is a piezoelectric laminated structure, which is a piezoelectric resonator, and the coupling structure of the resonant oscillator is a single crystal silicon layer, which is a capacitive resonator. That is, the present invention combines the advantages of the capacitive micromechanical resonator having a high Q value and the piezoelectric micromechanical resonator having a low impedance, and designs a micromechanical resonator combining a piezoelectric micromechanical resonator and a capacitive micromechanical resonator, which has a high Q value and low impedance. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 A schematic diagram of the three-dimensional structure of a micromechanical resonator when the number of coupling structures provided in Example 1 is 12;

[0043] Figure 2-a to Figure 2-e A top view of a micromechanical resonator with different numbers of coupling structures;

[0044] in: Figure 2-a is a schematic diagram of the structure of a micromechanical resonator when the number of coupling structures is 2; Figure 2-b is a schematic diagram of the structure of a micromechanical resonator when the number of coupling structures is 4; Figure 2-c is a schematic diagram of the structure of a micromechanical resonator when the number of coupling structures is 6; Figure 2-d is a schematic diagram of the structure of a micromechanical resonator when the number of coupling structures is 8; Figure 2-e It is a schematic diagram of the structure of a micromechanical resonator when the number of coupling structures is 12;

[0045] Figure 3 The simulation results of the effect of the number of coupling structures on the Q value of the micromechanical piezoelectric resonator are shown in Figure 2.

[0046] Figure 4 The simulation results of the effect of the number of coupling structures on the frequency shift and temperature stability of the micromechanical resonator are shown in the figure;

[0047] Figure 5-a to Figure 5-g A process flow for preparing a micromechanical resonator with a coupling structure provided in Example 2;

[0048] in: Figure 5-a It is a SOI wafer with a cavity structure; Figure 5-b Depositing a piezoelectric film and an upper electrode layer, and patterning the upper electrode layer; Figure 5-c To deposit an oxide layer; Figure 5-d To etch an upper electrode through hole to expose the upper electrode layer; Figure 5-e To etch the oxide layer and the piezoelectric film to expose the device layer silicon; Figure 5-f Depositing metal and patterning to form metal pads; Figure 5-g To etch the vibration structure and coupling structure of the resonant oscillator.

[0049] Figure 6-a to Figure 6-i A process flow for preparing a micromechanical resonator with a coupling structure provided in Example 3;

[0050] in: Figure 6-a It is a SOI wafer with a cavity structure; Figure 6-b For depositing a dielectric layer and a lower electrode layer; Figure 6-c Depositing a piezoelectric film and an upper electrode layer, and patterning the upper electrode layer; Figure 6-d To deposit an oxide layer; Figure 6-e To etch an upper electrode through hole to expose the upper electrode layer; Figure 6-f To etch the oxide layer and the piezoelectric film to expose the lower electrode layer; Figure 6-g For etching the oxide layer, the piezoelectric film, the lower electrode layer and the dielectric layer; Figure 6-h Depositing metal and patterning to form metal pads; Figure 6-iTo etch the vibration structure and coupling structure of the resonant oscillator.

[0051] Figure 1 And in Figure 2: 1-vibration structure, 2-coupling structure, 3-anchor structure.

[0052] In FIG5 : 51 - substrate silicon wafer, 52 - buried oxide layer, 53 - device layer silicon, 54 - piezoelectric film, 55 - upper electrode layer, 56 - oxide layer, 57 - metal pad.

[0053] In FIG6 : 61 - substrate silicon wafer, 62 - buried oxide layer, 63 - device layer silicon, 64 - piezoelectric film, 65 - upper electrode layer, 66 - oxide layer, 67 - metal pad, 68 - dielectric layer, 69 - lower electrode layer. DETAILED DESCRIPTION

[0054] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0055] Embodiment 1:

[0056] Embodiment 1 provides a micromechanical resonator with a coupling structure, see Figure 1 , including: a substrate silicon wafer and a resonator structure layer; the substrate silicon wafer has a cavity structure; the resonator structure layer includes a resonant oscillator and an anchor structure 3, the resonant oscillator includes a vibration structure 1 and a coupling structure 2; the vibration structure 1 is a piezoelectric stacked structure, the coupling structure 2 only includes device layer silicon, the number of the coupling structures 2 is one or more, the coupling structure 2 is connected to the vibration structure 1, and the coupling structure 2 is located on the outside of the vibration structure 1; the resonant oscillator is connected to the substrate silicon wafer through the anchor structure 3, and the resonant oscillator and the anchor structure 3 are both suspended above the cavity structure of the substrate silicon wafer.

[0057] Among them, the working modes of the micromechanical resonator are width extension mode, width extension high-order mode, square plate extension mode, etc.; the vibration mode of the vibration structure 1 is width extension mode or high-order width extension mode, and the vibration mode of the coupling structure 2 is radial extension mode.

[0058] The piezoelectric stack structure is composed of device layer silicon, piezoelectric film, upper electrode layer and oxide layer from bottom to top, or the piezoelectric stack structure is composed of device layer silicon, dielectric layer, lower electrode layer, piezoelectric film, upper electrode layer and oxide layer from bottom to top.

[0059] The material of the piezoelectric film is one of aluminum nitride, zinc oxide or lead zirconate titanate.

[0060] The coupling structure 2 is a circular plate structure. The radius of the coupling structure 2 adopts a specific geometric dimension, under which the Q value of the micromechanical resonator at the operating frequency is the highest. The specific geometric dimension is selected in the following manner: obtaining the operating frequency information and overall dimension information of the micromechanical resonator, and obtaining the material information and thickness information of each layer in the piezoelectric stacked structure; based on the above-obtained information, simulating the coupling structure 2 under different geometric dimensions to obtain the corresponding Q value of the micromechanical resonator; and selecting the geometric dimension of the coupling structure 2 corresponding to the simulation condition with the highest Q value as the specific geometric dimension.

[0061] The device layer silicon is N-type doped, and the doping concentration is greater than 10 19 cm -1 .

[0062] According to different vibration modes, the anchor structure 3 can be located at the vibration node position of the resonant oscillator. The number of the anchor structure 3 is one or more, and the anchor structure 3 can be a T-beam, an L-beam, a folded beam structure, etc.

[0063] The vibration structure 1 may be a square plate structure, a circular plate structure or other structures.

[0064] The front side of the substrate silicon wafer has a cavity structure, and the position of the cavity structure on the front side of the substrate silicon wafer corresponds to the resonant oscillator and the anchor structure 3. For example, the cavity structure corresponding to the resonant oscillator is a cuboid.

[0065] Embodiment 1 adds a coupling structure to the vibration structure of the resonant oscillator of the micromechanical resonator, and adjusts the size of the coupling structure to allow the vibration structure and the coupling structure to be modally coupled, thereby improving the Q value of the resonator. After adding the coupling structure to the vibration structure of the resonant oscillator, the frequency temperature coefficient can be reduced at the same time, thereby improving the temperature stability of the resonator.

[0066] Figure 1 Shown is a schematic diagram of the three-dimensional structure of a micromechanical resonator when the number of coupling structures is 12. Figure 2-a to Figure 2-e The figure shows a top view of a micromechanical resonator with different numbers of coupling structures, each of which includes a vibration structure 1, a coupling structure 2, and an anchor structure 3. Figure 2-a This is a schematic diagram of the resonator structure when the number of coupling structures is 2. Figure 2-b This is a schematic diagram of the resonator structure when the number of coupling structures is 4. Figure 2-c This is a schematic diagram of the resonator structure when the number of coupling structures is 6. Figure 2-d This is a schematic diagram of the resonator structure when the number of coupling structures is 8. Figure 2-eThe figure is a schematic diagram of the resonator structure when the number of coupling structures is 12. The number of coupling structures is an even number and is symmetrically distributed. The radius of the coupling structure preferably has a specific geometric size. For a micromechanical resonator of a specific frequency, a specific thickness, a specific material and a specific size, the size of the coupling structure is an optimized value. When the size of the coupling structure is a preferred value, the Q value of the resonator is the highest. After adding a coupling structure to the vibration structure of the resonator, the frequency temperature coefficient can be reduced and the temperature stability of the resonator can be improved.

[0067] For example, for <110> The aluminum nitride-single crystal silicon width extension mode micromechanical resonator with a crystal orientation has a single crystal silicon thickness of 40μm, an aluminum nitride thickness of 1μm, an upper electrode molybdenum layer thickness of 0.15μm, and a top oxide thickness of 0.2μm. The length and width of the resonant oscillator are 310μm and 155μm respectively. The coupling structure is a circular plate. When the number of coupling structures is 12, the radius of the circular plate is 91μm. That is, for the micromechanical resonator of the above-mentioned specific frequency, specific thickness, specific material and specific size, the coupling structure is a circular plate. When the number of coupling structures is 12, the radius of the circular plate is 91μm. The Q value of the micromechanical resonator is the largest, and the frequency stability of the micromechanical resonator is better than that of the micromechanical resonator without a coupling structure.

[0068] like Figure 3 As shown in the figure, the Q value of the micromechanical resonator corresponding to different numbers of coupling structures is calculated by finite element simulation when the size of the coupling structure is the optimal value. It can be seen that compared with the micromechanical resonator without a coupling structure, the Q value of the micromechanical resonator can be effectively improved by adding a coupling structure. In addition, as the number of coupling structures increases, the Q of the resonator gradually increases. Figure 4 The figure shows the simulation results of the frequency offset and temperature stability of the resonator under different numbers of coupling structures. It can be seen that as the number of coupling structures increases, the frequency offset of the resonator gradually decreases and the temperature stability gradually improves.

[0069] Two specific embodiments of the preparation method corresponding to the micromechanical resonator with a coupling structure provided in Example 1 are provided below.

[0070] Embodiment 2:

[0071] Embodiment 2 provides a method for preparing a micromechanical resonator with a coupling structure, and the specific steps are as follows:

[0072] (1) A SOI wafer with a cavity structure is provided. The SOI wafer includes, from bottom to top, a substrate silicon wafer 51, a buried oxide layer 52, and a device layer silicon 53. The thickness of the device layer silicon 53 is 40 μm. Figure 5-a ;

[0073] (2) A 1 μm thick piezoelectric film 54 (for example, aluminum nitride AlN) and a 0.2 μm thick upper electrode layer 55 (for example, molybdenum Mo) are sequentially deposited on the SOI wafer, and the upper electrode layer 55 is patterned, see Figure 5-b ;

[0074] (3) Deposit a 0.2 μm thick oxide layer 56, see Figure 5-c ;

[0075] (4) Etching an upper electrode through hole to expose the upper electrode layer 55, see Figure 5-d ;

[0076] (5) Etching the oxide layer 56 and the piezoelectric film 54 to expose the device layer silicon 53, see Figure 5-e ;

[0077] (6) Deposit a 1 μm thick metal (such as aluminum) and pattern it to form a metal pad 57, see Figure 5-f ;

[0078] (7) Etching to obtain the vibration structure and coupling structure of the resonator resonator as described in Example 1, see Figure 5-g .

[0079] Embodiment 2 corresponds to the solution in which the piezoelectric stack structure described in Embodiment 1 comprises, from bottom to top, a device layer silicon, a piezoelectric film, an upper electrode layer and an oxide layer.

[0080] Embodiment 3:

[0081] Embodiment 3 provides a method for preparing a micromechanical resonator with a coupling structure, and the specific steps are as follows:

[0082] (1) A SOI wafer with a cavity structure is provided. The SOI wafer includes, from bottom to top, a substrate silicon wafer 61, a buried oxide layer 62, and a device layer silicon 63. The thickness of the device layer silicon 63 is 40 μm. Figure 6-a ;

[0083] (2) A 1 μm thick dielectric layer 68 (for example, a dielectric layer made of silicon nitride Si3N4) and a 0.2 μm thick lower electrode layer 69 (for example, molybdenum Mo) are sequentially deposited on the SOI wafer, see Figure 6-b ;

[0084] (3) A 1 μm thick piezoelectric film 64 (e.g., aluminum nitride AlN) and a 0.2 μm thick upper electrode layer 65 (e.g., molybdenum Mo) are sequentially deposited on the SOI wafer, and the upper electrode layer 65 is patterned. Figure 6-c ;

[0085] (4) Deposit a 0.2 μm thick oxide layer 66, see Figure 6-d ;

[0086] (5) Etching an upper electrode through hole to expose the upper electrode layer 65, see Figure 6-e ;

[0087] (6) Etching the oxide layer 66 and the piezoelectric film 64 to expose the lower electrode layer 69, see Figure 6-f ;

[0088] (7) Etching the oxide layer 66, the piezoelectric film 64, the lower electrode layer 69 and the dielectric layer 68, see Figure 6-g ;

[0089] (8) Deposit a 1 μm thick metal (such as aluminum) and pattern it to form a metal pad 67, see Figure 6-h ;

[0090] (9) Etching to obtain the vibration structure and coupling structure of the resonator resonator as described in Example 1, see Figure 6-i .

[0091] Embodiment 3 corresponds to the solution in which the piezoelectric stack structure described in Embodiment 1 includes, from bottom to top, a device layer silicon, a dielectric layer, a lower electrode layer, a piezoelectric film, an upper electrode layer and an oxide layer.

[0092] A micromechanical resonator with a coupling structure and a method for manufacturing the same provided by an embodiment of the present invention include at least the following technical effects:

[0093] The present invention optimizes the design of the resonant oscillator of the micromechanical resonator and adds a coupling structure, which can effectively improve the Q value of the micromechanical resonator and reduce the frequency temperature coefficient. In addition, for a micromechanical resonator of a specific frequency, when the size of the coupling structure is an optimal value, the Q value of the resonator is the highest. As the number of coupling structures increases, the Q value of the resonator gradually increases, and the frequency temperature coefficient gradually decreases.

[0094] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to examples, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.

Claims

1. A micromechanical resonator with a coupling structure, characterized in that: include: Substrate silicon wafer and resonator structure layer; The substrate silicon wafer has a cavity structure; the resonator structure layer includes a resonant vibrator and an anchor point structure, and the resonant vibrator includes a vibration structure and a coupling structure; The vibration structure is a piezoelectric stacked structure, the coupling structure only includes device layer silicon, the number of the coupling structure is one or more, the coupling structure is connected to the vibration structure, and the coupling structure is located outside the vibration structure; The resonant oscillator is connected to the substrate silicon wafer through the anchor structure, and the resonant oscillator and the anchor structure are both suspended above the cavity structure of the substrate silicon wafer; The piezoelectric stack structure is composed of a device layer silicon, a piezoelectric film, an upper electrode layer and an oxide layer from bottom to top, or the piezoelectric stack structure is composed of a device layer silicon, a dielectric layer, a lower electrode layer, a piezoelectric film, an upper electrode layer and an oxide layer from bottom to top; The coupling structure is a circular plate structure; the radius of the coupling structure adopts a specific geometric dimension, under which the Q value of the micromechanical resonator at the operating frequency is the highest; the specific geometric dimension is selected in the following manner: obtaining the operating frequency information and overall dimension information of the micromechanical resonator, and obtaining the material information and thickness information of each layer in the piezoelectric stack structure; based on the above-obtained information, simulating the coupling structure under different geometric dimensions to obtain the corresponding Q value of the micromechanical resonator; and selecting the geometric dimension of the coupling structure corresponding to the simulation condition with the highest Q value as the specific geometric dimension.

2. The micromechanical resonator with a coupling structure according to claim 1, characterized in that: The working mode of the micromechanical resonator is one of a width extension mode, a width extension high-order mode, and a square plate extension mode; The vibration mode of the vibration structure is a width extension mode or a high-order width extension mode, and the vibration mode of the coupling structure is a radial extension mode.

3. The micromechanical resonator with a coupling structure according to claim 1, characterized in that: The material of the piezoelectric film is one of aluminum nitride, zinc oxide or lead zirconate titanate.

4. The micromechanical resonator with a coupling structure according to claim 1, characterized in that: The device layer silicon is N-type doped, and the doping concentration is greater than 10 19 cm -1 .

5. The micromechanical resonator with a coupling structure according to claim 1, characterized in that: The anchor point structure is located at the vibration node position of the resonant oscillator, the number of the anchor point structure is one or more, and the anchor point structure is a T-shaped beam, an L-shaped beam or a folded beam structure.

6. The micromechanical resonator with a coupling structure according to claim 1, characterized in that: The vibration structure is a square plate structure or a circular plate structure.

7. A method for preparing a micromechanical resonator with a coupling structure as claimed in any one of claims 1 to 6, characterized in that: The following steps are involved: Step 1, obtaining an SOI wafer with a cavity structure, wherein the SOI wafer includes a substrate silicon wafer, a buried oxide layer and a device layer silicon from bottom to top; Step 2, depositing a piezoelectric film and an upper electrode layer in sequence on the device layer silicon, and performing a patterning process on the upper electrode layer; Step 3, depositing an oxide layer on the upper electrode layer; Step 4, etching the oxide layer to obtain an upper electrode through hole and expose the upper electrode layer; Step 5, etching the oxide layer and the piezoelectric film to expose the device layer silicon; Step 6: depositing metal and patterning to form a metal pad; Step 7, etching to obtain a vibration structure and a coupling structure; Alternatively, include the following steps: Step 1, obtaining an SOI wafer with a cavity structure, wherein the SOI wafer includes a substrate silicon wafer, a buried oxide layer and a device layer silicon from bottom to top; Step 2, sequentially depositing a dielectric layer and a lower electrode layer on the device layer silicon; Step 3, depositing a piezoelectric film and an upper electrode layer on the lower electrode layer in sequence, and performing a patterning process on the upper electrode layer; Step 4, depositing an oxide layer on the upper electrode layer; Step 5, etching the oxide layer to obtain an upper electrode through hole and expose the upper electrode layer; Step 6, etching the oxide layer and the piezoelectric film to expose the lower electrode layer; Step 7, etching the oxide layer, the piezoelectric film, the lower electrode layer and the dielectric layer to expose the device layer silicon; Step 8: depositing metal and patterning to form a metal pad; Step 9: Etching to obtain the vibration structure and the coupling structure.

Citation Information

Patent Citations

  • Micromechanical resonator

    CN102868384A

  • Micromechanical resonator

    CN110289823A

  • Method for measuring microwave dielectric properties of high-loss material by adopting electric field symmetrical structure

    CN111157802A

  • Micromechanical resonator with anchor point auxiliary structure and preparation method thereof

    CN112751544A

  • Micromechanical resonator and preparation method thereof

    CN114124025A