A multilayer circuit board and its preparation process and application
Through dry process, the built-in circuit layer is constructed on the insulating resin layer, which solves the problems of environmental pollution and line layer side corrosion in the preparation of printed circuit boards, improves the conductivity and welding performance, and realizes environmentally friendly and efficient multi-layer circuits Plate preparation.
Patent Information
- Application Number
- CN202210677429.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-15
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-06-15
AI Technical Summary
The use of a large amount of chemical agents in the existing printed circuit board (PCB) preparation process leads to environmental pollution, and the circuit layer is easily eroded by side, and the large dielectric constant of the solder resist layer leads to slowing signal transmission and increasing loss.
Using dry process instead of traditional wet process, laser processing is used to build grooves on the insulating resin layer and fill conductive paste to form an embedded circuit layer, avoid the use of chemical potions and solder resist ink, and improve the flatness and conductivity of the circuit layer. performance.
It realizes the preparation of green and environmentally friendly multi-layer circuit boards, reduces side corrosion and dielectric losses, and improves the conductivity, welding performance and resistance to extreme environments.
Smart Images

Figure CN114867195B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of printed circuit boards, and in particular relates to a multilayer circuit board and a preparation process and application thereof. Background Art
[0002] With the advent of the 5G era, the industry has put forward higher requirements for the miniaturization, high integration, stability and reliability of signal transmission of electronic products. As the electrical connection carrier of electronic products, the manufacturing technology and interconnection technology of printed circuit boards (PCBs) are constantly improving.
[0003] CN108055784A discloses a method for making a circuit board. The method includes using a positive film process to make inner and / or outer circuits, and the positive film process includes the following steps: (1) forming a circuit pattern on the circuit board through film pasting, exposure and development processes in sequence; (2) copper plating is added to the circuit pattern on the circuit board to form an electroplated copper layer; (3) then chemical nickel plating is performed to deposit a nickel layer on the surface of the electroplated copper layer; (4) film stripping and etching processes are performed in sequence to etch out the circuit on the circuit board. This technical solution changes the traditional tin plating after electroplating copper to nickel plating. After the outer layer circuit pattern is copper plated, a nickel layer with uniform thickness is deposited through the nickel plating process, thereby avoiding the deviation of the protective layer thickness (tin thickness) caused by the special distribution of the pattern. However, a large amount of chemical solution is required for surface treatment in the copper plating process, which leads to the discharge of industrial wastewater and seriously pollutes the environment.
[0004] CN105208777A discloses a method for manufacturing a circuit board with metallized back-drilled holes. The manufacturing method includes the following steps: S1, coating a circuit board with a copper layer on the surface and back-drilled holes with a dry film, exposing and developing the required copper circuit and back-drilled holes; S2, copper plating in the back-drilled holes and on the exposed copper circuits, plating the copper to the required copper layer thickness, and then tin plating to the required tin layer thickness; S3, removing the dry film on the surface of the circuit board to expose the surface copper in the dry film area; S4, covering the mouth of the back-drilled holes with an anti-etching film; S5, etching away the surface copper in the dry film area corresponding to the surface of the circuit board; S6, removing the anti-etching film covering the mouth of the back-drilled holes; S7, removing the tin layer in the back-drilled holes of the circuit board and on the surface of the exposed copper circuit. Although this technical solution improves the electroplating quality by adding a back-drilled hole capping process for the circuit board, a large amount of industrial wastewater will be discharged during the electroplating process, seriously polluting the environment.
[0005] CN101400212A discloses a method for making a local high-frequency circuit printed circuit board by a semi-additive method. The method comprises the following steps: (1) embedding a Rogers sheet in an area on an ordinary sheet that requires high-frequency characteristics; (2) mixing and pressing with another ordinary sheet; (3) grinding and smoothing the joint between the Rogers sheet and the ordinary sheet; (4) depositing copper and electroplating on the surface of the Rogers and ordinary sheets to form a flat copper foil. This technical solution presses the high-frequency material Rogers sheet into the area that requires high-frequency characteristics by an embedded pressing method, and then plates a layer of copper on the common surface of Rogers and ordinary FR-4 by a semi-additive method for wiring to achieve effective connection of electrical signals. However, the circuit layer protrudes outside the insulating layer and is easily eroded by side corrosion.
[0006] From the above content, it can be seen that there are some problems in the existing PCB preparation process that cannot be ignored. For example, the copper electroplating and copper plating processes in the preparation of circuit boards require the use of a large amount of chemical solutions for surface treatment, which leads to the discharge of industrial wastewater and serious environmental pollution. In addition, in the process of preparing circuit boards by the additive method or semi-additive method, the circuit layer protrudes outside the insulating resin layer and is therefore easily eroded by side corrosion. At the same time, in order to ensure flatness, ink or the like is required to form a solder mask layer, but the solder mask layer has a large dielectric constant, which will slow down signal transmission and increase losses.
[0007] Therefore, how to provide a circuit layer preparation process that can replace the traditional wet method for preparing circuit boards, avoid the use of chemical solutions, and thus achieve green environmental protection; at the same time, reduce the side corrosion of the circuit, avoid the use of solder mask ink, and reduce the loss during transmission has become a technical problem that needs to be solved urgently. Summary of the invention
[0008] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a multilayer circuit board and its preparation process and application. In the present invention, by designing the structure of the multilayer circuit board and preparing the circuit layer by a dry process instead of a traditional wet process, the prepared multilayer circuit board has good conductivity, solderability and flatness.
[0009] To achieve this object, the present invention adopts the following technical solutions:
[0010] In a first aspect, the present invention provides a multilayer circuit board, the multilayer circuit board comprising a first metal layer, a first multilayer composite layer, a core layer, and a second metal layer stacked in sequence;
[0011] The multilayer circuit board comprises a through hole / blind hole, wherein the through hole / blind hole penetrates the first multilayer composite layer or the through hole / blind hole penetrates the first multilayer composite layer and the core layer;
[0012] The through hole / blind hole is filled with conductive paste;
[0013] The first multi-layer composite layer consists of at least 3 composite layers;
[0014] The composite layer comprises an insulating resin layer and a circuit layer which are bonded to each other.
[0015] In the present invention, the requirements of the use conditions can be met through the design of the multi-layer circuit board structure and further through the design of the multi-layer circuit layer. At the same time, through the design of the first metal layer and the second metal layer, the multi-layer circuit board can have a lower contact resistance, further having good electrical conductivity, while improving the welding performance, corrosion resistance and extreme environment resistance of the multi-layer circuit board.
[0016] It should be noted that in the first multi-layer composite layer between the first metal layer and the core layer of the present invention, the side of the insulating resin layer away from the circuit layer in each composite layer is close to the core layer, and the side of the circuit layer away from the insulating resin layer is close to the first metal layer.
[0017] The following are preferred technical solutions of the present invention, but are not intended to limit the technical solutions provided by the present invention. Through the following preferred technical solutions, the objectives and beneficial effects of the present invention can be better achieved and realized.
[0018] As a preferred technical solution of the present invention, the circuit layer is embedded in a side of the insulating resin layer away from the core layer.
[0019] Preferably, a side of the circuit layer away from the core layer is flush with a side of the insulating resin layer away from the core layer.
[0020] Preferably, at least one composite layer is provided between the core layer and the second metal layer.
[0021] In the composite layer between the second metal layer and the core layer, a side of the insulating resin layer away from the circuit layer is close to the core layer, and a side of the circuit layer away from the insulating resin layer is close to the second metal layer.
[0022] It should be noted that if at least one composite layer is provided between the core layer and the second metal layer, the through hole / blind hole in the multilayer circuit board penetrates the composite layer between the core layer and / or the second metal layer.
[0023] It should also be noted that if two or more composite layers are disposed between the core layer and the second metal layer, the multiple composite layers between the core layer and the second metal layer are recorded as second multi-layer composite layers.
[0024] Preferably, the number of composite layers in the multilayer circuit board is 5 to 50 layers, for example, it can be 5 layers, 10 layers, 15 layers, 20 layers, 25 layers, 30 layers, 35 layers, 40 layers, 45 layers or 50 layers.
[0025] As a preferred technical solution of the present invention, the core layer is selected from any one of a ceramic substrate, a BT resin substrate, a polyester substrate or a polyimide substrate.
[0026] Preferably, the thermal expansion coefficient of the core layer is less than 40 ppm·K -1 , for example, it can be 20ppm·K -1 、22ppm·K -1 、24ppm·K -1 、26ppm·K -1 、28ppm·K -1 、30ppm·K -1 、32ppm·K -1 、36ppm·K -1 or 39ppm·K -1 wait.
[0027] Preferably, the thickness of the core layer is 10-1000 μm, for example, 10 μm, 50 μm, 100 μm, 200 μm, 400 μm, 600 μm, 800 μm or 1000 μm.
[0028] Preferably, the dielectric loss of the core layer is 0.003-0.1, for example, it may be 0.003, 0.005, 0.01, 0.02, 0.03, 0.04, 0.05, 0.06, 0.07, 0.08, 0.09 or 0.1.
[0029] As a preferred technical solution of the present invention, the thermal expansion coefficient of the insulating resin layer is less than 40ppm·K -1 , for example, it can be 20ppm·K -1 、22ppm·K -1 、24ppm·K -1 、26ppm·K -1 、28ppm·K -1 、30ppm·K -1 、32ppm·K -1 、36ppm·K -1 or 39ppm·K -1 wait.
[0030] Preferably, the thickness of the insulating resin layer is 10-100 μm, for example, 10 μm, 20 μm, 30 μm, 40 μm, 50 μm, 60 μm, 70 μm, 80 μm, 90 μm or 100 μm.
[0031] Preferably, the dielectric loss of the insulating resin layer is 0.003-0.1, for example, it may be 0.003, 0.005, 0.01, 0.02, 0.03, 0.04, 0.05, 0.06, 0.07, 0.08, 0.09 or 0.1.
[0032] In the present invention, by selecting insulating resin layers and core layers with specific thermal expansion coefficient ranges, the two layers have relatively close thermal expansion coefficients, thereby avoiding the occurrence of deformation, warping and unusable problems of the multilayer circuit board due to excessive difference in thermal expansion coefficients between the two layers.
[0033] In the present invention, the insulating resin layer can be selected from any one of an insulating film and an insulating dielectric film. For example, the insulating dielectric film can be prepared according to CN110591591A, and the insulating film can be prepared according to CN113088039A, CN113831875A, CN114181652A or CN114231221A. Materials with similar properties to the above-mentioned insulating films and insulating dielectric films can also be used, such as NBF films produced in China, film products of Ajinomoto of Japan, film products of Sekisui Chemical of Japan, film products of Taiyo Ink of Japan, etc.
[0034] As a preferred technical solution of the present invention, the circuit layer is prepared from conductive paste B.
[0035] Preferably, the conductive paste A and the conductive paste B are each independently selected from any one or a combination of at least two of a silver-containing conductive paste, a copper-containing conductive paste or a gold-containing conductive paste.
[0036] Preferably, the thickness of the first metal layer and the second metal layer are independently selected from 0.5 to 5 μm, for example, 0.5 μm, 1 μm, 2 μm, 3 μm, 4 μm or 5 μm.
[0037] In a second aspect, the present invention provides a process for preparing a multilayer circuit board as described in the first aspect, wherein the process comprises the following steps:
[0038] (1) laminating an insulating resin layer on either side of the core layer, and forming through holes / blind holes and grooves on the side of the insulating resin layer away from the core layer by laser processing;
[0039] (2) filling the through hole / blind hole and the groove obtained in step (1) with conductive paste A and conductive paste B respectively, and sintering at low temperature to form a through hole / blind hole filled with conductive paste A and a composite layer;
[0040] (3) laminating another insulating adhesive film layer on the side of the composite layer obtained in step (2) away from the core layer, forming through holes / blind holes and grooves on the side of the insulating resin layer away from the core layer by laser processing, and filling the through holes / blind holes and grooves with conductive paste A and conductive paste B respectively, and sintering at low temperature to form through holes / blind holes filled with conductive paste A and composite layers;
[0041] (4) repeating step (3) to obtain through holes / blind holes filled with conductive paste A and a first multi-layer composite layer;
[0042] (5) Forming a first metal layer and a second metal layer on a side of the first multi-layer composite layer away from the core layer and on a side of the core layer away from the first multi-layer composite layer, respectively, to obtain the multi-layer circuit board.
[0043] It should be noted that in step (2), after the conductive paste B is filled in the groove formed in step (1), a circuit layer is formed after low-temperature sintering, and the circuit layer is embedded in the side of the insulating resin layer away from the core layer, together forming a composite layer.
[0044] It should also be noted that the position of the through hole / blind hole formed by laser drilling in step (3) is the same as the position of the through hole / blind hole formed by laser drilling in step (1).
[0045] The present invention constructs a groove pattern on the insulating resin layer through laser processing, and adds conductive paste B for sintering to obtain a circuit layer. The circuit layer is prepared by a dry process instead of a traditional wet process. The conductive paste B is used to replace copper plating, which can avoid the use of a large amount of chemical solutions in the wet process, thereby achieving green environmental protection. In addition, the circuit layer of the present invention is completely buried in the insulating resin layer, which can effectively reduce the side corrosion phenomenon. At the same time, the complete coating of the insulating resin layer can avoid the use of solder mask ink, effectively reduce dielectric loss, and thus reduce the loss during transmission.
[0046] As a preferred technical solution of the present invention, the pressing temperature in step (1) is 100-150°C, for example, it can be 100°C, 105°C, 110°C, 115°C, 120°C, 125°C, 130°C, 135°C, 140°C, 145°C or 150°C, etc.
[0047] Preferably, the pressing pressure in step (1) is 0.1-10 MPa, for example, it can be 0.1 MPa, 0.2 MPa, 0.5 MPa, 1 MPa, 2 MPa, 3 MPa, 4 MPa, 5 MPa, 6 MPa, 7 MPa, 8 MPa, 9 MPa or 10 MPa.
[0048] Preferably, step (2) further includes a post-processing step after filling the conductive paste.
[0049] Preferably, the post-treatment method is: removing excess conductive paste A and conductive paste B on the surface of the insulating resin layer by a brushing process.
[0050] Preferably, the temperature of the low-temperature sintering in step (2) is 120-150°C, for example, it can be 120°C, 125°C, 130°C, 135°C, 140°C, 145°C or 150°C.
[0051] Preferably, the low-temperature sintering time in step (2) is 30 to 60 min, for example, 30 min, 35 min, 40 min, 45 min, 50 min, 55 min or 60 min.
[0052] As a preferred technical solution of the present invention, the pressing temperature in step (3) is 100-150°C, for example, it can be 100°C, 105°C, 110°C, 115°C, 120°C, 125°C, 130°C, 135°C, 140°C, 145°C or 150°C, etc.
[0053] Preferably, the pressing pressure in step (3) is 0.1-10 MPa, for example, it can be 0.1 MPa, 0.2 MPa, 0.5 MPa, 1 MPa, 2 MPa, 3 MPa, 4 MPa, 5 MPa, 6 MPa, 7 MPa, 8 MPa, 9 MPa or 10 MPa.
[0054] Preferably, the temperature of the low-temperature sintering in step (3) is 120-150°C, for example, it can be 120°C, 125°C, 130°C, 135°C, 140°C, 145°C or 150°C.
[0055] Preferably, the low-temperature sintering time in step (3) is 30 to 60 min, for example, 30 min, 35 min, 40 min, 45 min, 50 min, 55 min or 60 min.
[0056] As a preferred technical solution of the present invention, the preparation methods of the first metal layer and the second metal layer in step (5) are independently selected from electroplating thick gold or chemical nickel palladium gold.
[0057] Preferably, a pre-treatment step is further included before forming the second metal layer.
[0058] Preferably, the pretreatment method is: through laser processing, a through hole / blind hole is formed on the side of the core layer away from the first multi-layer composite layer, the conductive paste A is filled into the through hole / blind hole, and low-temperature sintering is performed to form a through hole / blind hole filled with conductive paste A in the core layer.
[0059] It should be noted that the positions of through holes / blind holes formed by laser drilling in the pretreatment, the positions of through holes / blind holes formed by laser drilling in step (1), and the positions of through holes / blind holes formed by laser drilling in step (3) are the same (hereinafter the same). After the pretreatment step, through holes / blind holes penetrating the first multi-layer composite layer and the core layer can be formed in the multi-layer circuit board provided by the present invention; if the pretreatment step is not performed, the through holes / blind holes penetrate the first multi-layer composite layer.
[0060] In the present invention, if no composite layer is provided between the core layer and the second metal layer in the multilayer circuit board, the preparation process of the multilayer circuit board comprises the following steps:
[0061] (1) Under the conditions of 100-150° C. and 0.1-10 MPa, an insulating resin layer is pressed on either side of a core layer, and through holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer by laser processing;
[0062] (2) filling the through holes / blind holes and grooves obtained in step (1) with conductive paste A and conductive paste B respectively, removing excess conductive paste A and conductive paste B on the surface of the insulating resin layer by a brushing process, and sintering at a low temperature of 120 to 150° C. for 30 to 60 minutes to form through holes / blind holes filled with conductive paste A and a composite layer;
[0063] (3) Under the conditions of 100-150° C. and 0.1-10 MPa, another insulating adhesive film layer is pressed onto the side of the composite layer obtained in step (2) away from the core layer, through holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer by laser processing, and conductive paste A and conductive paste B are respectively filled into the through holes / blind holes and grooves, and excess conductive paste A and conductive paste B on the surface of the insulating resin layer are removed by a brushing process, and low-temperature sintering is performed at 120-150° C. for 30-60 min to form through holes / blind holes filled with conductive paste A and a composite layer;
[0064] (4) repeating step (3) to obtain through holes / blind holes filled with conductive paste A and a first multi-layer composite layer;
[0065] (5) forming a first metal layer on a side of the first multi-layer composite layer away from the core layer by electroplating thick gold or chemical nickel-palladium-gold;
[0066] The multi-layer circuit board is obtained by forming a second metal layer on the side of the core layer away from the first multi-layer composite layer through electroplating thick gold or chemical nickel-palladium-gold.
[0067] Through the above preparation process, the through hole / blind hole in the multi-layer circuit board prepared penetrates the first multi-layer composite layer; if the through hole / blind hole is required to penetrate the first multi-layer composite layer and the core layer, step (5) is replaced by step (5′):
[0068] Step (5′) forming a first metal layer on a side of the first multi-layer composite layer away from the core layer by electroplating thick gold or chemical nickel-palladium-gold;
[0069] Through laser processing, a through hole / blind hole is formed on the side of the core layer away from the first multi-layer composite layer, and conductive paste A is filled into the through hole / blind hole. Low-temperature sintering is performed to form a through hole / blind hole filled with conductive paste A in the core layer, and then thick gold or chemical nickel-palladium-gold is electroplated to form a second metal layer on the side of the core layer away from the first multi-layer composite layer to obtain the multi-layer circuit board.
[0070] It should be noted that in step (1) and step (3), laser processing only forms through holes / blind holes in the insulating resin layer; and in step (5′), laser processing forms through holes / blind holes in the core layer.
[0071] In the present invention, if at least one composite layer is provided between the core layer and the second metal layer in the multilayer circuit board, the preparation process of the multilayer circuit board comprises the following steps:
[0072] (S1) Under the conditions of 100-150° C. and 0.1-10 MPa, an insulating resin layer is pressed on one side of the core layer, through laser processing, through holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer, and conductive paste A and conductive paste B are filled therein, respectively, and excess conductive paste A and conductive paste B on the surface of the insulating resin layer are removed by a brushing process, and low-temperature sintering is performed at 120-150° C. for 30-60 minutes to form through holes / blind holes filled with conductive paste A and a composite layer;
[0073] (S2) Under the conditions of 100-150° C. and 0.1-10 MPa, an insulating resin layer is similarly pressed on the other side of the core layer, through-holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer by laser processing, and conductive paste A and conductive paste B are respectively filled therein, and excess conductive paste A and conductive paste B on the surface of the insulating resin layer are removed by a brushing process, and low-temperature sintering is performed at 120-150° C. for 30-60 min to form through-holes / blind holes filled with conductive paste A and a composite layer on the other side of the core layer;
[0074] (S3) Under the conditions of 100-150° C. and 0.1-10 MPa, an insulating film layer is pressed on the side of one of the composite layers obtained in step (2) away from the core layer, through holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer by laser processing, and conductive paste A and conductive paste B are filled into the through holes / blind holes and grooves, excess conductive paste A and conductive paste B on the surface of the insulating resin layer are removed by a brushing process, and low-temperature sintering is performed at 120-150° C. for 30-60 min to form through holes / blind holes filled with conductive paste A and composite layers;
[0075] (S4) Under the conditions of 100-150° C. and 0.1-10 MPa, an insulating film layer is pressed on the side of the other composite layer obtained in step (2) away from the core layer, through holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer by laser processing, and conductive paste A and conductive paste B are filled into the through holes / blind holes and grooves, excess conductive paste A and conductive paste B on the surface of the insulating resin layer are removed by a brushing process, and low-temperature sintering is performed at 120-150° C. for 30-60 min to form through holes / blind holes filled with conductive paste A and composite layers;
[0076] (S5) repeating step (S3) to obtain through holes / blind holes filled with conductive paste A and a first multi-layer composite layer, and optionally repeating step (S4) to obtain through holes / blind holes filled with conductive paste A and a second multi-layer composite layer;
[0077] (S6) forming a first metal layer and a second metal layer on a side of the first multi-layer composite layer away from the core layer and a side of the second multi-layer composite layer away from the core layer respectively by electroplating thick gold or chemical nickel palladium gold to obtain the multi-layer circuit board.
[0078] Through the above preparation process, the through hole / blind hole in the multi-layer circuit board prepared penetrates the first multi-layer composite layer and the second multi-layer composite layer; if the through hole / blind hole is required to penetrate the first multi-layer composite layer, the second multi-layer composite layer and the core layer, step (S2) is replaced by the following step (S2′):
[0079] (S2′) Under the conditions of 100-150°C and 0.1-10MPa, an insulating resin layer is also pressed on the other side of the core layer. Through laser processing, through holes / blind holes and grooves are formed on the side of the insulating resin layer away from the core layer. During the laser processing, through holes / blind holes are formed in the core layer and the insulating resin layer at the same time. Conductive paste A and conductive paste B are filled into the through holes / blind holes and grooves respectively. The excess conductive paste A and conductive paste B on the surface of the insulating resin layer are removed by a brushing process. The composite layer is sintered at 120-150°C for 30-60min to form a core layer filled with conductive paste A, through holes / blind holes filled with conductive paste A, and a composite layer filled with conductive paste B.
[0080] In a third aspect, the present invention provides an application of the multilayer circuit board as described in the first aspect in a PCB.
[0081] Compared with the prior art, the present invention has the following beneficial effects:
[0082] (1) The present invention constructs a groove pattern on the insulating resin layer through laser processing, and adds a conductive paste B for low-temperature sintering to obtain a circuit layer. The circuit layer is prepared by a dry process instead of a traditional wet process. The conductive paste is used to replace copper plating, which can avoid the use of a large amount of chemical solutions in the wet process, thereby achieving green environmental protection.
[0083] (2) The circuit layer of the composite layer in the present invention is completely buried in the insulating resin layer, which can effectively reduce the side erosion phenomenon. At the same time, the complete covering of the insulating resin layer can avoid the use of solder mask ink, effectively reduce dielectric loss, and thus reduce the loss during signal transmission.
[0084] (3) The first metal layer and the second metal layer formed by electroplating thick gold or chemical nickel-palladium-gold have a low contact resistance, and the prepared multilayer circuit board has good electrical conductivity and a low dielectric loss of 0.011 to 0.013; at the same time, the prepared multilayer circuit board has excellent welding performance, high corrosion resistance and resistance to extreme environments.
[0085] (4) The multilayer circuit board prepared by the present invention has a smooth appearance, no warping, and a small thermal expansion coefficient of 19 to 22 ppm·K by selecting the materials of the core layer and the insulating resin layer. -1 . BRIEF DESCRIPTION OF THE DRAWINGS
[0086] Figure 1 is a schematic diagram of the cross-sectional structure of a multilayer circuit board at a through hole / blind hole provided by Embodiment 1 of the present invention;
[0087] Figure 2 is a schematic diagram of the preparation process of step (S1) of Example 1 of the present invention;
[0088] Figure 3 is a schematic diagram of the cross-sectional structure of the circuit board prepared in step (S2) of Example 1 of the present invention at the through hole / blind hole;
[0089] Figure 4 is a schematic diagram of the cross-sectional structure of the circuit board prepared in step (S3) of Example 1 of the present invention at the through hole / blind hole;
[0090] Figure 5 is a schematic diagram of the cross-sectional structure of the circuit board prepared in step (S4) of Example 1 of the present invention at the through hole / blind hole;
[0091] Figure 6 is a schematic diagram of the cross-sectional structure of the circuit board prepared in step (S5) of Example 1 of the present invention at the through hole / blind hole;
[0092] Among them, 1-first metal layer, 2-first multi-layer composite layer, 3-core layer, 4-second metal layer, 5-through hole / blind hole, 6-second multi-layer composite layer, 21-composite layer, 211-insulating resin layer, 212-circuit layer, 7-groove, 8-conductive paste. DETAILED DESCRIPTION
[0093] The technical solution of the present invention is further described below in conjunction with the accompanying drawings and through specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0094] The sources of some components in the following examples and comparative examples are as follows:
[0095] Ceramic substrate: Rogers Company, USA, ROGERS 4350, ROGERS4003;
[0096] BT resin substrate: Mitsubishi Gas Chemical, HL832NSF LCA;
[0097] Insulating film (1): prepared according to CN113088039A;
[0098] Insulating adhesive film (2): prepared according to CN114231221A;
[0099] Insulating film (3): prepared according to CN114181652A;
[0100] Silver-containing conductive paste: Dupont, USA, LT133;
[0101] Copper-containing conductive paste: prepared according to CN106605270A;
[0102] Gold-containing conductive paste: prepared according to CN109087723A.
[0103] Example 1
[0104] This embodiment provides a multi-layer circuit board and a preparation process thereof. The structural schematic diagram of the multi-layer circuit board is as follows: Figure 1 As shown, it includes a first metal layer 1, a first multi-layer composite layer 2, a core layer 3, a second multi-layer composite layer 6 and a second metal layer 4 which are stacked in sequence;
[0105] The multi-layer circuit board includes a through hole / blind hole 5, the through hole / blind hole 5 penetrates the first multi-layer composite layer 2 and the second multi-layer composite layer 6, and the through hole / blind hole 5 is filled with a copper-containing conductive paste;
[0106] The first multi-layer composite layer 2 is composed of three composite layers 21, and the second multi-layer composite layer 6 is composed of three composite layers 21;
[0107] The composite layer 21 includes an insulating resin layer 211 and a circuit layer 212, wherein the circuit layer 212 is embedded in a side of the insulating resin layer 211 away from the core layer 3, and the side of the circuit layer 212 away from the core layer 3 is flush with the side of the insulating resin layer 211 away from the core layer 3, and the circuit layer 212 is prepared from a copper-containing conductive paste;
[0108] The core layer 3 is a ceramic substrate (ROGERS 4350) with a thickness of 250 μm; the insulating resin layer 211 is an insulating adhesive film (1) with a thickness of 40 μm.
[0109] The preparation process of the above-mentioned multilayer circuit board is as follows:
[0110] (S1) Under the conditions of 100° C. and 10 MPa, an insulating film (1) is pressed on one side of a ceramic substrate (ROGERS 4350), and through-holes / blind holes 5 and grooves 7 are formed on the side of the insulating film (1) away from the ceramic substrate (ROGERS 4350) by laser processing, and copper-containing conductive paste is filled therein, and excess copper-containing conductive paste on the surface of the insulating resin layer is removed by a grinding and brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through-holes / blind holes 5 filled with copper-containing conductive paste and a composite layer 21 (the schematic diagram of its preparation process is shown in FIG. Figure 2 shown);
[0111] (S2) Under the conditions of 100° C. and 10 MPa, an insulating film (1) is similarly pressed on the other side of the ceramic substrate (ROGERS 4350), and through-holes / blind holes 5 and grooves 7 are formed on the side of the insulating film (1) away from the ceramic substrate (ROGERS 4350) by laser processing, and copper-containing conductive paste is filled therein, and excess copper-containing conductive paste on the surface of the insulating resin layer is removed by a grinding process, and low-temperature sintering is performed at 150° C. for 30 minutes, and through-holes / blind holes 5 filled with copper-containing conductive paste and a composite layer 21 (such as Figure 3 shown);
[0112] (S3) Under the conditions of 100° C. and 10 MPa, an insulating film (1) is pressed onto the side of one of the composite layers 21 obtained in step (2) away from the ceramic substrate (ROGERS 4350), through-holes / blind holes 5 and grooves 7 are formed on the side of the insulating film (1) away from the ceramic substrate (ROGERS 4350) by laser processing, and copper-containing conductive paste is filled into the through-holes / blind holes 5 and the grooves 7, and excess copper-containing conductive paste on the surface of the insulating film (1) is removed by a brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through-holes / blind holes 5 and composite layers 21 (such as Figure 4 shown);
[0113] (S4) Under the conditions of 100° C. and 10 MPa, an insulating film (1) is pressed onto the side of another composite layer 21 obtained in step (2) away from the ceramic substrate (ROGERS 4350), through-holes / blind holes 5 and grooves 7 are formed on the side of the insulating film (1) away from the ceramic substrate (ROGERS 4350) by laser processing, and copper-containing conductive paste is filled into the through-holes / blind holes 5 and the grooves 7, and excess copper-containing conductive paste on the surface of the insulating film (1) is removed by a brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through-holes / blind holes 5 and composite layers 21 (such as Figure 5 shown);
[0114] (S5) Repeat step (S3) to obtain a through hole / blind hole 5 filled with a copper-containing conductive paste and a first multilayer composite layer 2, and repeat step (S4) to obtain a through hole / blind hole filled with a copper-containing conductive paste and a second multilayer composite layer 6 (such as Figure 6 shown);
[0115] (S6) By electroplating thick gold, a first metal layer 1 with a thickness of 5 μm and a second metal layer 4 with a thickness of 5 μm are respectively formed on the side of the first multi-layer composite layer 2 away from the ceramic substrate (ROGERS 4350) and the side of the second multi-layer composite layer 6 away from the ceramic substrate (ROGERS 4350), thereby obtaining the multi-layer circuit board.
[0116] Example 2
[0117] This embodiment provides a multi-layer circuit board and a preparation process thereof, wherein the multi-layer circuit board comprises a first metal layer, a first multi-layer composite layer, a core layer, a second multi-layer composite layer and a second metal layer which are sequentially stacked;
[0118] The multi-layer circuit board comprises a through hole / blind hole, wherein the through hole / blind hole penetrates the first multi-layer composite layer and the second multi-layer composite layer, and the through hole / blind hole is filled with a silver-containing conductive paste;
[0119] The first multi-layer composite layer consists of 25 composite layers, and the second multi-layer composite layer consists of 25 composite layers;
[0120] The composite layer comprises an insulating resin layer and a circuit layer, wherein the circuit layer is embedded in a side of the insulating resin layer away from the core layer, and the side of the circuit layer away from the core layer is flush with the side of the insulating resin layer away from the core layer, and the circuit layer is prepared from a silver-containing conductive paste;
[0121] The core layer is a BT resin substrate with a thickness of 700 μm; the insulating resin layer is an insulating adhesive film (3) with a thickness of 100 μm.
[0122] The preparation process of the above-mentioned multilayer circuit board is as follows:
[0123] (S1) Under the conditions of 150° C. and 0.1 MPa, an insulating adhesive film (3) is pressed onto one side of a BT resin substrate, through laser processing is used to form through holes / blind holes and grooves on the side of the insulating adhesive film (3) away from the BT resin substrate, silver-containing conductive paste is filled into the grooves, excess silver-containing conductive paste on the surface of the insulating resin layer is removed by a grinding and brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through holes / blind holes filled with silver-containing conductive paste and a composite layer;
[0124] (S2) at 150° C. and 0.1 MPa, an insulating adhesive film (3) is similarly pressed on the other side of the BT resin substrate, through-holes / blind holes and grooves are formed on the side of the insulating adhesive film (3) away from the BT resin substrate by laser processing, and silver-containing conductive paste is filled therein, and excess silver-containing conductive paste on the surface of the insulating resin layer is removed by a brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through-holes / blind holes filled with silver-containing conductive paste and a composite layer on the other side of the BT resin substrate;
[0125] (S3) Under the conditions of 150° C. and 0.1 MPa, an insulating adhesive film (3) is pressed onto the side of one of the composite layers obtained in step (2) away from the BT resin substrate, through-holes / blind holes and grooves are formed on the side of the insulating adhesive film (3) away from the BT resin substrate by laser processing, and silver-containing conductive paste is filled into the through-holes / blind holes and grooves, excess silver-containing conductive paste on the surface of the insulating adhesive film (3) is removed by a brushing process, and low-temperature sintering is performed at 120° C. for 60 minutes to form through-holes / blind holes and composite layers filled with silver-containing conductive paste;
[0126] (S4) Under the conditions of 150° C. and 0.1 MPa, an insulating adhesive film (3) is pressed onto the side of the other composite layer obtained in step (2) away from the BT resin substrate, through-holes / blind holes and grooves are formed on the side of the insulating adhesive film (3) away from the BT resin substrate by laser processing, and silver-containing conductive paste is filled into the through-holes / blind holes and grooves, and excess silver-containing conductive paste on the surface of the insulating adhesive film (3) is removed by a brushing process, and low-temperature sintering is performed at 120° C. for 60 minutes to form through-holes / blind holes and composite layers filled with silver-containing conductive paste;
[0127] (S5) repeating step (S3) to obtain through holes / blind holes filled with silver-containing conductive paste and a first multi-layer composite layer, and repeating step (S4) to obtain through holes / blind holes filled with silver-containing conductive paste and a second multi-layer composite layer;
[0128] (S6) A first metal layer with a thickness of 5 μm and a second metal layer with a thickness of 5 μm are formed on a side of the first multi-layer composite layer away from the BT resin substrate and a side of the second multi-layer composite layer away from the BT resin substrate, respectively, by chemical nickel-palladium-gold to obtain the multi-layer circuit board.
[0129] Example 3
[0130] This embodiment provides a multi-layer circuit board and a preparation process thereof, wherein the multi-layer circuit board comprises a first metal layer, a first multi-layer composite layer, a core layer, a second multi-layer composite layer and a second metal layer which are sequentially stacked;
[0131] The multi-layer circuit board comprises a through hole / blind hole, wherein the through hole / blind hole penetrates the first multi-layer composite layer and the second multi-layer composite layer, and the through hole / blind hole is filled with a gold-containing conductive paste;
[0132] The first multi-layer composite layer consists of 5 composite layers, and the second multi-layer composite layer consists of 5 composite layers;
[0133] The composite layer includes an insulating resin layer and a circuit layer, wherein the circuit layer is embedded in a side of the insulating resin layer away from the core layer, and the side of the circuit layer away from the core layer is flush with the side of the insulating resin layer away from the core layer, and the circuit layer is prepared from a gold-containing conductive paste;
[0134] The core layer is a ceramic substrate (ROGERS4003) with a thickness of 1000 μm; the insulating resin layer is an insulating film (2) with a thickness of 100 μm.
[0135] The preparation process of the above-mentioned multilayer circuit board is as follows:
[0136] (S1) Under the conditions of 120° C. and 1 MPa, an insulating film (2) is pressed on one side of a ceramic substrate (ROGERS4003), through-holes / blind holes and grooves are formed on the side of the insulating film (2) away from the ceramic substrate (ROGERS4003) by laser processing, and gold-containing conductive paste is filled therein, and excess gold-containing conductive paste on the surface of the insulating resin layer is removed by a brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through-holes / blind holes filled with gold-containing conductive paste and a composite layer;
[0137] (S2) at 120° C. and 1 MPa, an insulating film (2) is similarly pressed on the other side of the ceramic substrate (ROGERS4003), through-holes / blind holes and grooves are formed on the side of the insulating film (2) away from the ceramic substrate (ROGERS4003) by laser processing, and gold-containing conductive paste is filled therein, and excess gold-containing conductive paste on the surface of the insulating resin layer is removed by a grinding and brushing process, and low-temperature sintering is performed at 150° C. for 30 minutes to form through-holes / blind holes filled with gold-containing conductive paste and a composite layer on the other side of the ceramic substrate (ROGERS4003);
[0138] (S3) Under the conditions of 120° C. and 1 MPa, an insulating film (2) is pressed onto the side of one of the composite layers obtained in step (2) away from the ceramic substrate (ROGERS4003), through-holes / blind holes and grooves are formed on the side of the insulating film (2) away from the ceramic substrate (ROGERS4003) by laser processing, and the through-holes / blind holes and grooves are filled with gold-containing conductive paste, and excess gold-containing conductive paste on the surface of the insulating film (2) is removed by a brushing process, and low-temperature sintering is performed at 130° C. for 40 minutes to form through-holes / blind holes and composite layers filled with gold-containing conductive paste;
[0139] (S4) Under the conditions of 120° C. and 1 MPa, an insulating film (2) is pressed onto the side of another composite layer obtained in step (2) away from the ceramic substrate (ROGERS4003), through-holes / blind holes and grooves are formed on the side of the insulating film (3) away from the ceramic substrate (ROGERS4003) by laser processing, and the through-holes / blind holes and grooves are filled with gold-containing conductive paste, and the excess gold-containing conductive paste on the surface of the insulating film (2) is removed by a brushing process, and low-temperature sintering is performed at 130° C. for 40 minutes to form through-holes / blind holes and a composite layer filled with the gold-containing conductive paste;
[0140] (S5) repeating step (S3) to obtain through holes / blind holes filled with gold-containing conductive paste and a first multi-layer composite layer, and repeating step (S4) to obtain through holes / blind holes filled with gold-containing conductive paste and a second multi-layer composite layer;
[0141] (S6) By electroplating thick gold, a first metal layer with a thickness of 3 μm and a second metal layer with a thickness of 3 μm are respectively formed on the side of the first multi-layer composite layer away from the ceramic substrate (ROGERS4003) and the side of the second multi-layer composite layer away from the ceramic substrate (ROGERS4003), thereby obtaining the multi-layer circuit board.
[0142] Example 4
[0143] This embodiment provides a multi-layer circuit board and a preparation process thereof, wherein the multi-layer circuit board comprises a first metal layer, a first multi-layer composite layer, a core layer and a second metal layer which are sequentially stacked;
[0144] The multi-layer circuit board comprises a through hole / blind hole, wherein the through hole / blind hole penetrates the first multi-layer composite layer, and the through hole / blind hole is filled with a gold-containing conductive paste;
[0145] The first multi-layer composite layer consists of 10 composite layers;
[0146] The composite layer includes an insulating resin layer and a circuit layer, wherein the circuit layer is embedded in a side of the insulating resin layer away from the core layer, and the side of the circuit layer away from the core layer is flush with the side of the insulating resin layer away from the core layer, and the circuit layer is prepared from a gold-containing conductive paste;
[0147] The core layer is a ceramic substrate (ROGERS4003) with a thickness of 1000 μm; the insulating resin layer is an insulating film (2) with a thickness of 10 μm.
[0148] The preparation process of the above-mentioned multilayer circuit board is as follows:
[0149] (1) Under the conditions of 110° C. and 5 MPa, an insulating adhesive film (2) is pressed onto either side of a ceramic substrate, and through holes / blind holes and grooves are formed on the side of the insulating adhesive film (2) away from the ceramic substrate by laser processing;
[0150] (2) filling the through holes / blind holes and grooves obtained in step (1) with a gold-containing conductive paste, removing excess gold-containing conductive paste on the surface of the insulating film (2) by a grinding and brushing process, and sintering at a low temperature of 130° C. for 40 minutes to form through holes / blind holes filled with the gold-containing conductive paste and a composite layer;
[0151] (3) Under the conditions of 110° C. and 5 MPa, another insulating film (2) is pressed onto the side of the composite layer obtained in step (2) away from the ceramic substrate, through-holes / blind holes and grooves are formed on the side of the insulating film (2) away from the ceramic substrate by laser processing, and the through-holes / blind holes and grooves are filled with gold-containing conductive paste, and the excess gold-containing conductive paste on the surface of the insulating film (2) is removed by a brushing process, and low-temperature sintering is performed at 130° C. for 40 minutes to form through-holes / blind holes and composite layers filled with gold-containing conductive paste;
[0152] (4) repeating step (3) to obtain a through hole / blind hole filled with a gold-containing conductive paste and a first multi-layer composite layer;
[0153] (5) forming a first metal layer with a thickness of 3 μm on a side of the first multi-layer composite layer away from the ceramic substrate by electroplating thick gold;
[0154] A second metal layer with a thickness of 3 μm is formed on the side of the ceramic substrate away from the first multi-layer composite layer by electroplating thick gold, thereby obtaining the multi-layer circuit board.
[0155] Comparative Example 1
[0156] This comparative example provides a multilayer circuit board and a preparation process thereof, wherein the multilayer circuit board comprises a first metal layer, a solder resist layer, a first multilayer composite layer, a core layer and a second metal layer which are sequentially stacked;
[0157] The core layer is a ceramic substrate (ROGERS 4350) with a thickness of 250 μm;
[0158] The first multi-layer composite layer comprises 10 composite layers;
[0159] The composite layer comprises an insulating resin layer and a circuit layer arranged on one side surface of the insulating resin layer. The insulating resin layer is an insulating adhesive film (2) having a thickness of 40 μm.
[0160] (1) Under the conditions of 110° C. and 5 MPa, an insulating film (2) is pressed onto either side of a ceramic substrate (ROGERS 4350), and a through hole / blind hole is formed on the side of the insulating film (2) away from the ceramic substrate (ROGERS 4350) by laser processing;
[0161] (2) by a semi-additive method, drill desmearing, chemical copper plating, pattern transfer, blind hole filling under pattern electroplating, film stripping, and flash etching are sequentially performed to obtain a circuit layer on the side of the insulating layer film (2) away from the core layer, thereby obtaining a composite layer;
[0162] (3) Under the conditions of 110° C. and 5 MPa, another insulating adhesive film (2) is pressed onto the side of the composite layer obtained in step (2) away from the ceramic substrate (ROGERS 4350), and through holes / blind holes are formed on the side of the insulating adhesive film (2) away from the ceramic substrate (ROGERS 4350) by laser processing, and another composite layer is obtained by a semi-additive method;
[0163] (4) repeating step (3) to obtain a first multi-layer composite layer;
[0164] (5) forming a welding layer on the side of the first multi-layer composite layer away from the ceramic substrate (ROGERS 4350) by coating a solder resist ink (LE-600, Okura Fujita Co., Ltd.);
[0165] (6) forming a first metal layer with a thickness of 0.3 μm on a side of the first multi-layer composite layer away from the ceramic substrate (ROGERS 4350) by electroplating thin gold;
[0166] A second metal layer with a thickness of 0.3 μm was formed on a side of the ceramic substrate (ROGERS 4350) away from the first multi-layer composite layer by electroplating thin gold to obtain the multi-layer circuit board.
[0167] The performance of the multilayer circuit boards provided in the above embodiments and comparative examples was tested, and the testing method was as follows:
[0168] Dielectric loss: The multilayer circuit board was cut into 2mm×80mm test pieces (3 pieces). The dielectric loss of each test piece was measured by the cavity resonance perturbation method at a measurement frequency of 5.8GHz and a measurement temperature of 23°C using the "HP8362B" of Agilent Technologies Co., Ltd., and the average value of the 3 test pieces was calculated.
[0169] Thermal expansion coefficient: The multilayer circuit board was cut into test pieces with a width of about 6 mm and a length of about 15 mm. A thermal mechanical analysis was performed using a thermomechanical analyzer (Mettler Toledo "TMA SDTA2+") under the conditions of a preload force of 0.02 N, a temperature rise range of 25°C to 260°C, and a heating rate of 10°C / min to obtain the thermal expansion coefficient in the range of 25°C to 150°C.
[0170] Appearance evaluation: Observe whether the prepared multilayer circuit board is intact, cracked, or warped.
[0171] Solderability test: Solderability test is carried out according to the standard "IPC J-STD-003B".
[0172] The performance test results of the multilayer circuit boards provided in the above embodiments and comparative examples are shown in Table 1 below:
[0173] Table 1
[0174]
[0175] As can be seen from the contents of Table 1, the present invention further constructs a groove pattern on the insulating resin layer by laser processing through the design of the multilayer circuit board structure and the selection of materials, and adds a conductive paste for low-temperature sintering to obtain a circuit layer, and prepares the circuit layer through a dry process. The prepared multilayer circuit board has a low dielectric loss of 0.011-0.013, and the prepared multilayer circuit board has excellent welding performance. At the same time, the prepared multilayer circuit board has a smooth appearance without warping, and its thermal expansion coefficient is small, which is 19-22ppm·K. -1 .
[0176] If a wet process is used to prepare a multilayer circuit board (Comparative Example 1), a large amount of chemical solutions will be used in the process of preparing the multilayer circuit board, which is not environmentally friendly. In addition, since the circuit layer is attached to the surface of the insulating resin layer, it is easily eroded by the side. At the same time, in order to ensure flatness, ink or the like is required to form a solder mask layer. However, the solder mask layer has a large dielectric constant, which will cause signal transmission to slow down. The performance of the multilayer circuit board prepared in this way is poor.
[0177] The applicant declares that the present invention illustrates the detailed structural features and detailed process flow of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned detailed structural features and detailed process flow, that is, it does not mean that the present invention must rely on the above-mentioned detailed structural features and detailed process flow to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
Claims
1. A multilayer circuit board, It is characterized in that The multi-layer circuit board comprises a first metal layer, a first multi-layer composite layer, a core layer and a second metal layer which are sequentially stacked; The multilayer circuit board comprises a through hole / blind hole, wherein the through hole / blind hole penetrates the first multilayer composite layer or the through hole / blind hole penetrates the first multilayer composite layer and the core layer; The through hole / blind hole is filled with conductive paste A; The first multi-layer composite layer consists of at least 3 composite layers; The composite layer includes an insulating resin layer and a circuit layer bonded to each other; The multilayer circuit board is prepared by the following method, which comprises the following steps: (1) laminating an insulating resin layer on either side of the core layer, and forming through holes / blind holes and grooves on the side of the insulating resin layer away from the core layer by laser processing; (2) filling the through hole / blind hole and the groove obtained in step (1) with conductive paste A and conductive paste B respectively, and sintering at low temperature to form a through hole / blind hole filled with conductive paste A and a composite layer; (3) laminating another insulating adhesive film layer on the side of the composite layer obtained in step (2) away from the core layer, forming through holes / blind holes and grooves on the side of the insulating resin layer away from the core layer by laser processing, and filling the through holes / blind holes and grooves with conductive paste A and conductive paste B respectively, and sintering at low temperature to form through holes / blind holes filled with conductive paste A and composite layers; (4) repeating step (3) to obtain through holes / blind holes filled with conductive paste A and a first multi-layer composite layer; (5) forming a first metal layer on a side of the first multi-layer composite layer away from the core layer; Forming a second metal layer on a side of the core layer away from the first multi-layer composite layer to obtain the multi-layer circuit board; The temperature of the low temperature sintering in step (2) is 120-150° C. The low-temperature sintering time in step (2) is 30 to 60 minutes.
2. The multilayer circuit board according to claim 1, It is characterized in that The circuit layer is embedded in a side of the insulating resin layer away from the core layer.
3. The multilayer circuit board according to claim 2, It is characterized in that The side of the circuit layer away from the core layer is flush with the side of the insulating resin layer away from the core layer.
4. The multilayer circuit board according to claim 1, It is characterized in that At least one composite layer is arranged between the core layer and the second metal layer.
5. The multilayer circuit board according to claim 1, It is characterized in that The number of composite layers in the multi-layer circuit board is 5 to 50.
6. The multilayer circuit board according to claim 1, It is characterized in that The core layer is selected from any one of a ceramic substrate, a BT resin substrate, a polyester substrate or a polyimide substrate.
7. The multilayer circuit board according to claim 1, It is characterized in that The thermal expansion coefficient of the core layer is less than 40 ppm·K -1 .
8. The multilayer circuit board according to claim 1, It is characterized in that The thickness of the core layer is 10 to 1000 μm.
9. The multilayer circuit board according to claim 1, It is characterized in that The dielectric loss of the core layer is 0.003 to 0.
1.
10. The multilayer circuit board according to claim 1, It is characterized in that The thermal expansion coefficient of the insulating resin layer is less than 40 ppm·K -1 .
11. The multilayer circuit board according to claim 1, It is characterized in that The thickness of the insulating resin layer is 10-100 μm.
12. The multilayer circuit board according to claim 1, It is characterized in that The dielectric loss of the insulating resin layer is 0.003 to 0.
1.
13. The multilayer wiring board according to claim 1, It is characterized in that The circuit layer is prepared from conductive paste B.
14. The multilayer wiring board according to claim 13, It is characterized in that The conductive paste A and the conductive paste B are each independently selected from any one of a silver-containing conductive paste and a gold-containing conductive paste or a combination of at least two thereof.
15. The multilayer wiring board according to claim 1, It is characterized in that The thickness of the first metal layer and the second metal layer are each independently selected from 0.5 to 5 μm.
16. A process for preparing a multilayer circuit board according to any one of claims 1 to 15, It is characterized in that The preparation process comprises the following steps: (1) laminating an insulating resin layer on either side of the core layer, and forming through holes / blind holes and grooves on the side of the insulating resin layer away from the core layer by laser processing; (2) filling the through hole / blind hole and the groove obtained in step (1) with conductive paste A and conductive paste B respectively, and sintering at low temperature to form a through hole / blind hole filled with conductive paste A and a composite layer; (3) laminating another insulating adhesive film layer on the side of the composite layer obtained in step (2) away from the core layer, forming through holes / blind holes and grooves on the side of the insulating resin layer away from the core layer by laser processing, and filling the through holes / blind holes and grooves with conductive paste A and conductive paste B respectively, and sintering at low temperature to form through holes / blind holes filled with conductive paste A and composite layers; (4) repeating step (3) to obtain through holes / blind holes filled with conductive paste A and a first multi-layer composite layer; (5) forming a first metal layer on a side of the first multi-layer composite layer away from the core layer; Forming a second metal layer on a side of the core layer away from the first multi-layer composite layer to obtain the multi-layer circuit board; The temperature of the low temperature sintering in step (2) is 120-150° C. The low-temperature sintering time in step (2) is 30 to 60 minutes.
17. The preparation process according to claim 16, It is characterized in that The pressing temperature in step (1) is 100-150°C.
18. The preparation process according to claim 16, It is characterized in that The pressing pressure in step (1) is 0.1 to 10 MPa.
19. The preparation process according to claim 16, It is characterized in that Step (2) also includes a post-processing step after filling the conductive paste.
20. The preparation process according to claim 19, It is characterized in that The post-treatment method is: removing the excess conductive paste A and conductive paste B on the surface of the insulating resin layer by a brushing process.
21. The preparation process according to claim 16, It is characterized in that The pressing temperature in step (3) is 100-150°C.
22. The preparation process according to claim 16, It is characterized in that The pressing pressure in step (3) is 0.1 to 10 MPa.
23. The preparation process according to claim 16, It is characterized in that The temperature of the low-temperature sintering in step (3) is 120-150°C.
24. The preparation process according to claim 16, It is characterized in that The low-temperature sintering time in step (3) is 30 to 60 minutes.
25. The preparation process according to claim 16, It is characterized in that In step (5), the preparation methods of the first metal layer and the second metal layer are independently selected from electroplating thick gold or chemical nickel palladium gold.
26. The preparation process according to claim 16, It is characterized in that The method further includes a pre-treatment step before forming the second metal layer.
27. The preparation process according to claim 26, It is characterized in that The pretreatment method is: through laser processing, a through hole / blind hole is formed on the side of the core layer away from the first multi-layer composite layer, the conductive paste A is filled into the through hole / blind hole, and low-temperature sintering is performed to form a through hole / blind hole filled with the conductive paste A in the core layer.
28. Use of the multilayer circuit board according to any one of claims 1 to 15 in a PCB.