Cigar moisturizing bag and preparation method thereof
By using bentonite and other materials in cigar moisturizing packages to form a gel core structure in which composite moisturizing materials crosslinked with polyvinyl alcohol and hydroxyethyl cellulose, and covering the porous cross-linking network, the existing cigar moisturizing packages have a short service life. The problem has achieved long-term stable maintenance of cigar moisture and improved suction comfort.
Patent Information
- Application Number
- CN202210433622.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-04-24
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-04-24
AI Technical Summary
The existing cigar moisturizing bag has a short service life and cannot effectively maintain the moisture stability of the cigar under different environmental conditions, resulting in a decrease in quality and a reduction in suction comfort.
Ultrasonic treatment is carried out using bentonite, acrylic acid, N,N-methylenebisacrylamide and potassium persulfate to form a composite moisturizing material, and cross-link it with polyvinyl alcohol and hydroxyethyl cellulose to form a gel core structure, and then add it Sodium alginate forms hydrogel beads, coated with porous crosslinking network structure, and prepares a cigar moisturizing package with high stability.
It significantly improves the service life and stability of the cigar moisturizing bag, extends the storage time of the cigar, reduces the impact of changes in environmental conditions on the cigar quality, and ensures comfort during the suction process.
Smart Images

Figure HDA0003611987330000011 
Figure HDA0003611987330000012
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cigar moisturizing, and in particular to a cigar moisturizing bag and a preparation method thereof. Background Art
[0002] Cigar is a natural tobacco product made from dried, fermented and aged tobacco leaves. The production process is to combine the cigar core and the cigar wrapper to make a cigar bundle, then shape it, and finally add the cigar wrapper. The packaged cigars must be identified for quality and then stored in an environment with ideal humidity. After hundreds of years of development, cigars are currently showing a trend of continuous recovery and booming development in my country, and the consumer market is quite large, but the storage environment of domestic cigars is not taken seriously, which affects their quality.
[0003] During the storage process, cigars are highly sensitive to the surrounding environment. Environmental changes directly affect the moisture content of cigars. When the humidity is low, the cigar wrapper is prone to cracking, which is mainly manifested in greater irritation and obvious dryness when smoking, which can easily cause phlegm in the smoker's mouth, thereby reducing the comfort of smoking cigarettes. In the maintenance and preservation of cigars, using professional equipment to provide professional maintenance for cigars is a very effective method, but the high investment in professional maintenance equipment is beyond the reach of ordinary people.
[0004] Moisturizing packs are a common auxiliary material for product protection. They mainly use the chemical or physical adsorption properties of some substances to reduce or increase the humidity value in the product packaging to extend the shelf life of the product and ensure product quality. Common moisturizing packs mainly refer to moisture-absorbing and water-locking carriers combined with a certain amount of pure water, and are packaged with packaging materials with certain moisture permeability properties. Common raw materials include high-molecular polyacrylates, modified starch, complex polysaccharides, etc., but the service life is short and the product limitations are significant. Summary of the invention
[0005] The purpose of the present invention is to solve the shortcomings of the prior art and to propose a cigar moisturizing bag and a preparation method thereof.
[0006] A method for preparing a cigar moisturizing bag comprises the following steps:
[0007] S1. Add sodium hydroxide solution to acrylic acid, stir at 30-40°C for 10-20min, add bentonite and ultrasonically treat for 1-2h, the ultrasonic frequency is 5-12kHz, add N,N-methylenebisacrylamide and stir, add potassium persulfate and continue stirring, heat to 80-90°C under nitrogen protection and stir for 1-2h, filter, wash, dry and crush to obtain a composite moisturizing material;
[0008] S2. A composite moisturizing material, polyvinyl alcohol and hydroxyethyl cellulose are reacted, wherein the carboxyl group and the hydroxyl group are cross-linked by hydrogen bonds to form a gel core structure, and then calcium chloride and sodium alginate are reacted to form hydrogel beads; after washing, freeze-drying is performed, water is added to a water content of 80-90%, and packaging is performed to obtain a cigar moisturizing bag.
[0009] Preferably, in S1, the concentration of the sodium hydroxide solution is 0.5-1.5 mol / L, and the mass ratio of acrylic acid, sodium hydroxide solution, bentonite, N,N-methylenebisacrylamide, and potassium persulfate is 5-15:40-80:10-20:0.1-1:0.01-0.1.
[0010] Preferably, in S1, the bentonite is 200 mesh.
[0011] Preferably, in S1, the filtration is followed by washing with water for 2-4 times.
[0012] Preferably, S2 is prepared by the following specific steps: adding the composite moisturizing material and polyvinyl alcohol into water and stirring for 1-2 hours, then adding hydroxyethyl cellulose under stirring, stirring at 50-70°C for 10-30 minutes, adding calcium chloride and glucono-δ-lactone, continuing to stir for 10-30 minutes, adding sodium alginate solution dropwise thereto under high-speed stirring, standing for 1-2 hours to obtain hydrogel beads; after washing, freeze-drying, adding water to a water content of 80-90%, and packaging to obtain cigar moisturizing bags.
[0013] Preferably, in S2, the mass ratio of the composite moisturizing material, polyvinyl alcohol and hydroxyethyl cellulose is 15-35:5-10:1-5.
[0014] Preferably, in S2, the concentration of the sodium alginate solution is 1-2 mol / L, and the mass ratio of the composite moisturizing material, calcium chloride, glucono-δ-lactone, and the sodium alginate solution is 15-35:0.1-1:1-2:5-15.
[0015] Preferably, in S2, the specific washing operation is as follows: rinse with distilled water 2-4 times.
[0016] A cigar moisturizing bag is prepared by adopting the preparation method of the cigar moisturizing bag.
[0017] The technical effects of the present invention are as follows:
[0018] Bentonite has a strong hygroscopicity and can absorb water equivalent to 20 times its own volume and expand to 30 times. The present invention introduces bentonite into the acrylic polymer, and the system is in a colloidal state, which not only improves the water absorption performance, but also stabilizes the product structure;
[0019] The present invention further compounded the composite moisturizing material with polyvinyl alcohol and hydroxyethyl cellulose, wherein the carboxyl group and the hydroxyl group were cross-linked by hydrogen bonds to form a gel core structure, and then calcium chloride was added thereto. The calcium ions had a high affinity with the gel core structure, and were attached to and coated outside the gel core structure. Then, a sodium alginate solution was dripped thereto, and a network structure was further formed outside the gel core structure by combining with the calcium ions.
[0020] Specifically, sodium alginate reacts with calcium chloride to quickly form a dense network structure shell. At the same time, sodium alginate penetrates into the gel core structure and can further produce hydrogen bond cross-linking with the gel core structure formed by the composite moisturizing material, polyvinyl alcohol, and hydroxyethyl cellulose to construct a stable core-shell interface.
[0021] The cigar moisturizing bag obtained by the present invention has good structural stability, not only has excellent moisturizing properties, but also can maintain long-term stability during use. By compounding and cross-linking the composite moisturizing material with polyvinyl alcohol and hydroxyethyl cellulose to form a gel core structure, and then coating a layer of porous cross-linked network structure, the long-term moisturizing effect of the composite moisturizing material can be maintained, further expanding the storage environment range of cigars over a long period of time, reducing the irreparable loss of cigars caused by changes in environmental conditions, and can play an important role in the maintenance of cigars. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 The graph shows the change of moisture content of cigars over time in Example 5 and Comparative Examples 1-2 under simulated storage conditions.
[0023] Figure 2 The graph is a graph showing the change in moisture content of cigars over time for Example 5 and Comparative Examples 1-2 when simulating the situation of consumers using cigars. DETAILED DESCRIPTION
[0024] The present invention will be further explained below in conjunction with specific embodiments.
[0025] Example 1
[0026] A method for preparing a cigar moisturizing bag comprises the following steps:
[0027] S1. Add 40 kg of 0.5 mol / L sodium hydroxide solution to 5 kg of acrylic acid, stir at 30 ° C for 10 min, add 10 kg of bentonite sieved through a 200 mesh sieve, ultrasonically treat for 1 h, the ultrasonic frequency is 5 kHz, add 0.1 kg of N, N-methylenebisacrylamide, stir at a speed of 100 r / min for 10 min, add 0.01 kg of potassium persulfate, continue stirring for 5 min, heat to 80 ° C under nitrogen protection, stir for 1 h, filter, wash with water twice, dry, and crush to obtain a composite moisturizing material;
[0028] S2. Add 15kg of composite moisturizing material and 5kg of polyvinyl alcohol into 50kg of water and stir for 1h. Then add 1kg of hydroxyethyl cellulose under stirring, stir at 50℃ for 10min at a stirring speed of 200r / min, add 0.1kg of calcium chloride and 1kg of glucono-δ-lactone, continue stirring for 10min, add 5kg of 1mol / L sodium alginate solution dropwise under high-speed stirring, let stand for 1h to obtain hydrogel beads; rinse with distilled water twice, freeze-dry, add water to a water content of 80%, and package to obtain cigar moisturizing bags.
[0029] Example 2
[0030] A method for preparing a cigar moisturizing bag comprises the following steps:
[0031] S1. Add 80 kg of 1.5 mol / L sodium hydroxide solution to 15 kg of acrylic acid, stir at 40 ° C for 20 min, add 20 kg of bentonite sieved through a 200-mesh sieve, ultrasonically treat for 2 h, the ultrasonic frequency is 12 kHz, add 1 kg of N, N-methylenebisacrylamide, stir at a speed of 400 r / min for 20 min, add 0.1 kg of potassium persulfate, continue stirring for 15 min, heat to 90 ° C under nitrogen protection, stir for 2 h, filter, wash with water 4 times, dry, and crush to obtain a composite moisturizing material;
[0032] S2. Add 35kg of composite moisturizing material and 10kg of polyvinyl alcohol into 100kg of water and stir for 2h. Then add 5kg of hydroxyethyl cellulose under stirring, stir at 70℃ for 30min at a stirring speed of 400r / min, add 1kg of calcium chloride and 2kg of glucono-δ-lactone, continue stirring for 30min, add 15kg of 2mol / L sodium alginate solution dropwise under high-speed stirring, let stand for 2h to obtain hydrogel beads; rinse with distilled water 4 times, freeze-dry, add water to a water content of 90%, and package to obtain cigar moisturizing bags.
[0033] Example 3
[0034] A method for preparing a cigar moisturizing bag comprises the following steps:
[0035] S1. Add 70 kg of 0.8 mol / L sodium hydroxide solution to 8 kg of acrylic acid, stir at 37 ° C for 13 min, add 18 kg of bentonite passed through a 200 mesh sieve, ultrasonically treat for 1.3 h, the ultrasonic frequency is 10 kHz, add 0.2 kg of N, N-methylenebisacrylamide, stir at a speed of 300 r / min for 13 min, add 0.08 kg of potassium persulfate, continue stirring for 8 min, heat to 88 ° C under nitrogen protection, stir for 1.3 h, filter, wash with water 3 times, dry, and crush to obtain a composite moisturizing material;
[0036] S2. Add 30kg of composite moisturizing material and 6kg of polyvinyl alcohol into 90kg of water and stir for 1.3h. Then, add 4kg of hydroxyethyl cellulose under stirring, stir at 55℃ for 25min at a stirring speed of 250r / min, add 0.7kg of calcium chloride and 1.3kg of glucono-δ-lactone, continue stirring for 25min, add 8kg of 1.7mol / L sodium alginate solution dropwise under high-speed stirring, let stand for 1.2h to obtain hydrogel beads; rinse with distilled water 3 times, freeze-dry, add water to a water content of 88%, and package to obtain cigar moisturizing bags.
[0037] Example 4
[0038] A method for preparing a cigar moisturizing bag comprises the following steps:
[0039] S1. Add 50 kg of 1.2 mol / L sodium hydroxide solution to 12 kg of acrylic acid, stir at 33 ° C for 17 min, add 12 kg of bentonite sieved through a 200-mesh sieve, ultrasonically treat for 1.7 h, the ultrasonic frequency is 6 kHz, add 0.8 kg of N, N-methylenebisacrylamide, stir at a speed of 200 r / min for 17 min, add 0.02 kg of potassium persulfate, continue stirring for 12 min, heat to 82 ° C under nitrogen protection, stir for 1.7 h, filter, wash with water 3 times, dry, and crush to obtain a composite moisturizing material;
[0040] S2. Add 20kg of composite moisturizing material and 8kg of polyvinyl alcohol into 60kg of water and stir for 1.7h. Then, add 2kg of hydroxyethyl cellulose under stirring, stir at 65℃ for 15min at a stirring speed of 350r / min, add 0.3kg of calcium chloride and 1.7kg of glucono-δ-lactone, continue stirring for 15min, add 12kg of 1.3mol / L sodium alginate solution dropwise under high-speed stirring, let stand for 1.8h to obtain hydrogel beads; rinse with distilled water 3 times, freeze-dry, add water to a water content of 82%, and package to obtain cigar moisturizing bags.
[0041] Example 5
[0042] A method for preparing a cigar moisturizing bag comprises the following steps:
[0043] S1. Add 60 kg of 1 mol / L sodium hydroxide solution to 10 kg of acrylic acid, stir at 35 °C for 15 min, add 15 kg of bentonite sieved through a 200-mesh sieve, ultrasonically treat for 1.5 h at a frequency of 9 kHz, add 0.5 kg of N,N-methylenebisacrylamide, stir at 260 r / min for 15 min, add 0.05 kg of potassium persulfate, continue stirring for 10 min, heat to 85 °C under nitrogen protection, stir for 1.5 h, filter, wash with water 3 times, dry, and crush to obtain a composite moisturizing material;
[0044] S2. Add 25kg of composite moisturizing material and 7kg of polyvinyl alcohol into 75kg of water and stir for 1.5h. Then add 3kg of hydroxyethyl cellulose under stirring, stir at 60℃ for 20min at a stirring speed of 300r / min, add 0.5kg of calcium chloride and 1.5kg of glucono-δ-lactone, continue stirring for 20min, add 10kg of 1.5mol / L sodium alginate solution dropwise under high-speed stirring, let stand for 1.5h to obtain hydrogel beads; rinse with distilled water 3 times, freeze-dry, add water to a water content of 85%, and package to obtain cigar moisturizing bags.
[0045] Comparative Example 1
[0046] A preparation method of a cigar moisturizing bag comprises the following steps: adding 60 kg of 1 mol / L sodium hydroxide solution into 10 kg of acrylic acid, stirring at 35°C for 15 minutes, adding 15 kg of bentonite sieved through a 200-mesh sieve, ultrasonically treating for 1.5 hours at an ultrasonic frequency of 9 kHz, adding 0.5 kg of N,N-methylenebisacrylamide, stirring at a speed of 260 r / min for 15 minutes, adding 0.05 kg of potassium persulfate, continuing to stir for 10 minutes, heating to 85°C under nitrogen protection and stirring for 1.5 hours, filtering, washing with water for 3 times, drying, crushing, adding water to a water content of 85%, and packaging to obtain a cigar moisturizing bag.
[0047] Comparative Example 2
[0048] A method for preparing a cigar moisturizing bag comprises the following steps:
[0049] S1. Add 60 kg of 1 mol / L sodium hydroxide solution to 10 kg of acrylic acid, stir at 35 °C for 15 min, add 15 kg of bentonite sieved through a 200-mesh sieve, ultrasonically treat for 1.5 h at a frequency of 9 kHz, add 0.5 kg of N,N-methylenebisacrylamide, stir at 260 r / min for 15 min, add 0.05 kg of potassium persulfate, continue stirring for 10 min, heat to 85 °C under nitrogen protection, stir for 1.5 h, filter, wash with water 3 times, dry, and crush to obtain a composite moisturizing material;
[0050] S2. Add 25 kg of composite moisturizing material and 7 kg of polyvinyl alcohol into 75 kg of water and stir for 1.5 h. Then add 3 kg of hydroxyethyl cellulose under stirring. Stir at 60 ° C for 20 min at a stirring speed of 300 r / min. Freeze-dry, add water to a moisture content of 85%, and package to obtain a cigar moisturizing bag.
[0051] The cigar moisturizing bags obtained in Example 5 and Comparative Examples 1-2 were respectively packaged together with cigars, and then sealed with ordinary small box packaging paper and then plastic-sealed for outer packaging. Storage experiments were carried out at a temperature of 25° C. and a humidity of 50-60%, and the oven weighing method was used for testing.
[0052] 1. Simulate the storage situation, that is, the moisture changes of cigars in the cigar boxes when they are fully packaged during storage in the warehouse. Figure 1 As shown, within 12 weeks, the water content of cigars continued to decrease with time, but the water content of cigars in Example 5 group was always higher than 12%, which prevented the cigars from overheating during the smoking process and affected the smoke and taste of the cigars.
[0053] The applicant believes that this is because the cigar moisturizing bag obtained by the present invention forms a gel core structure by compounding and cross-linking the composite moisturizing material with PVA and hydroxyethyl cellulose, and then coating it with a layer of porous cross-linked network structure, which can maintain a long-term moisturizing effect.
[0054] 2. Simulate the situation of consumers using cigars. That is, after consumers tear off the plastic seal of the outer packaging of the cigar box, they still keep the box sealed and monitor the moisture changes of the cigars in the box within 72 hours.
[0055] like Figure 2 As shown, within 72 hours, the moisture content of the cigars continued to decrease with time, but the moisture content of the cigars in the Example 5 group was still the highest, and the moisture reduction rate of the Comparative Example 1-2 group was significantly higher than that of the Example 5 group. It is confirmed that even if the plastic seal is removed, the cigar moisturizing bag obtained by the present invention can still effectively maintain the moisture content of the cigars, avoiding the discomfort caused to consumers by the excessive loss of moisture in the cigars during the smoking process.
[0056] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for preparing a cigar moisturizing bag, characterized in that: The steps include: S1. Add sodium hydroxide solution to acrylic acid, stir at 30-40°C for 10-20min, add bentonite and ultrasonically treat for 1-2h, the ultrasonic frequency is 5-12kHz, add N,N-methylenebisacrylamide and stir, add potassium persulfate and continue stirring, heat to 80-90°C under nitrogen protection and stir for 1-2h, filter, wash, dry and crush to obtain a composite moisturizing material; S2. Add the composite moisturizing material and polyvinyl alcohol into water and stir for 1-2 hours. Then add hydroxyethyl cellulose under stirring, stir at 50-70°C for 10-30 minutes, add calcium chloride and glucono-δ-lactone, continue stirring for 10-30 minutes, add sodium alginate solution dropwise under high-speed stirring, let stand for 1-2 hours to obtain hydrogel beads; wash and freeze-dry, add water to a water content of 80-90%, and package to obtain cigar moisturizing bags.
2. The method for preparing the cigar moisturizing bag according to claim 1, characterized in that: In S1, the concentration of the sodium hydroxide solution is 0.5-1.5 mol / L, and the mass ratio of acrylic acid, sodium hydroxide solution, bentonite, N,N-methylenebisacrylamide, and potassium persulfate is 5-15:40-80:10-20:0.1-1:0.01-0.
1.
3. The method for preparing the cigar moisturizing bag according to claim 1, characterized in that: In S1, the bentonite is 200 mesh.
4. The method for preparing the cigar moisturizing bag according to claim 1, characterized in that: In S1, after filtering, wash with water 2-4 times.
5. The method for preparing the cigar moisturizing bag according to claim 1, characterized in that: In S2, the mass ratio of the composite moisturizing material, polyvinyl alcohol and hydroxyethyl cellulose is 15-35:5-10:1-5.
6. The method for preparing the cigar moisturizing bag according to claim 1, characterized in that: In S2, the concentration of the sodium alginate solution is 1-2 mol / L, and the mass ratio of the composite moisturizing material, calcium chloride, glucono-δ-lactone, and the sodium alginate solution is 15-35:0.1-1:1-2:5-15.
7. The method for preparing the cigar moisturizing bag according to claim 1, characterized in that: In S2, the specific washing operation is as follows: rinse with distilled water 2-4 times.
8. A cigar moisturizing bag, characterized in that: The cigar moisturizing bag is prepared by the preparation method of any one of claims 1 to 7.