A solvent-free coating process

Through solvent-free coating process and composite cooling device, environmental pollution and fire hazards caused by gasoline use in the production of traditional Chinese medicine rubber paste are solved, low-cost and efficient plaster production are achieved, and market competitiveness is enhanced.

CN114948729BActive Publication Date: 2024-11-26CHONGQING PEIDU PHARMA
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202210774867.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-01
Publication Date
2024-11-26
Estimated Expiration
2042-07-01

AI Technical Summary

Technical Problem

The large amount of gasoline used in the existing traditional Chinese medicine rubber paste production process leads to environmental pollution, fire hazards and high production costs, and is affected by the shortage of gasoline, making market competition difficult.

Method used

The solvent-free coating process is adopted to produce plasters through ingredients, spice, glue refining, rough refining, plate separation, glue coating and composite cooling devices, avoid the use of gasoline, mint, camphor, borneol, salicylic acid, Vegetable oil and liquid paraffin are volatile ingredients combined with oven and composite cooling device for softening and cooling treatment.

Benefits of technology

It realizes efficient production of solvent-free plasters, reduces costs, avoids environmental pollution and fire hazards, reduces investment in gasoline volatile treatment equipment, and improves production efficiency and market competitiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114948729B_ABST
    Figure CN114948729B_ABST
Patent Text Reader

Abstract

The invention discloses a solvent-free coating process, comprising: step 1: batching; volatile components are configured according to the product varieties, wherein the volatile components are menthol, camphor, borneol, salicylic acid, vegetable oil, liquid paraffin, and liquefied; step 2: foaming rubber; after the rubber is cut into pieces, it is pressed into thin sheets or silk screens by a rubber mixer, static electricity is removed, and it is added to the liquefied material of step 1, stirred and mixed, and soaked; step 3: rubber refining; step 4: rough refining; step 5: refining; step 6: plate separation; step 7: glue coating; step 8: slicing and packaging. No need to add gasoline, no environmental pollution, no need to dry in a drying oven, and no fire hazard.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of plaster coating, and in particular to a solvent-free coating process. Background Art

[0002] The production of Chinese medicine rubber plasters is still mostly produced by the solvent method, which requires the use of a large amount of gasoline, which not only causes environmental pollution during the production process, but also has safety hazards such as fire. Due to the influence of international crude oil production, gasoline is in short supply. Therefore, the price remains high. Relatively speaking, the production cost of enterprises has increased, while the market price of finished products has remained unchanged, which puts enterprises in a very unfavorable situation in the market competition. Summary of the invention

[0003] The present invention aims to solve the technical problems existing in the prior art, and particularly innovatively proposes a solvent-free coating process, which does not require the addition of gasoline, does not cause environmental pollution, does not require drying in a drying oven, and does not have a fire hazard.

[0004] In order to achieve the above-mentioned object of the present invention, the present invention provides a solvent-free coating process, comprising:

[0005] Step 1: preparing ingredients; preparing volatile components, wherein the volatile components are menthol, camphor, borneol, salicylic acid, vegetable oil and liquid paraffin, and then liquefying them;

[0006] Step 2: Foaming rubber: After the rubber is cut into pieces, it is pressed into thin sheets or meshes by a rubber mixer, and static electricity is removed. Then, it is added to the liquefied material in step 1, stirred and mixed, and soaked;

[0007] Step 3: Rubber refining: Press the soaked rubber into thin sheets with an open mill, then put it into a honey mill, add lead powder or zinc oxide, rosin particles or tinfoil resin, Chinese medicine extract and oil according to the prescription for mixing; mix it until a small amount of visible rubber particles remain in the paste, control the temperature of the honey refining room below 60°C, take it out and put it aside for use;

[0008] Step 4: Rough refining: put the honey-refined material into a rubber mixer for rough refining. The rough refining is to make sure that no rubber particles are visible to the naked eye. After the rough refining is completed, take it out and set aside for later use.

[0009] Step 5: Refining: Put the material obtained in step 4 into a rubber mixer for refining;

[0010] Step 6: Divide into plates; put the refined material into a rubber mixer and divide it into plates, and spread it on the plates with a thickness not exceeding 8 mm for later use;

[0011] Step 7: Glue application;

[0012] 7-1 Place the material obtained in step 6 in an oven and heat to soften it;

[0013] 7-2: Coating; putting the softened material on the material storage tank of the coater, and heating the coating material storage plate and the scraper of the coater; preventing the material from hardening again,

[0014] 7-3: Coating;

[0015] 7-4: After coating, the silicone paper is cooled through a composite cooling device and laminated with a cover layer material, cut into a specified width and wound up;

[0016] Step 8: Slicing and packaging.

[0017] In the above solution: In step 2, during soaking, turn it over twice in the middle, and the soaking time is more than 24 hours.

[0018] In the above solution: The preparation method of the rosin particles is as follows: heat and melt the rosin, continuously stir during heating, pass through a 100-mesh sieve to remove impurities, let the rosin liquid filtered from impurities cool, break it into pieces, and pass through a 20-40 mesh sieve for standby.

[0019] In the above solution: The coater includes a sizing device for rubber material and a positioning coating device. The sizing device for rubber material includes a lower coating roller and an upper coating roller located above the lower coating roller. In front of the lower coating roller, there is a coating material storage plate with a front high and rear low shape. A glue storage tank is arranged on the coating material storage plate. The side wall of the glue storage tank on the side close to the lower coating roller leans against the roller surface of the lower coating roller. On the left and right sides of the glue storage tank, there are glue baffle plates respectively. The glue baffle plates extend upward to the upper side of the roller surface of the upper coating roller. The back of the coating material storage plate is provided with heating wires to heat the material in the glue storage tank through the heating wires; a stirring mechanism is arranged in the glue storage tank.

[0020] In the above solution: The stirring mechanism includes two "C"-shaped stirring blades. The closed ends of the two stirring blades are respectively connected to the rotating shafts of the rotating motors installed on the left and right side frames, and the rotating shafts pass through the corresponding side glue baffle plates. The open ends of the two stirring blades face each other, and one leg of any one stirring blade is located between the two legs of the other stirring blade.

[0021] In the above solution: The oven is a hot air circulation type drum drying oven. The heating temperature of the paste is 60-65 degrees. The oven temperature is: 90-100 degrees in summer and 100-110 degrees in winter. The heating time is: 30-60 minutes.

[0022] In the above solution: The composite cooling device includes a cold water rotating cylinder extending left and right. A pressing roller is arranged above the rear of the cold water rotating cylinder. A wrap angle adjusting roller is arranged below the cold water rotating cylinder. After the silicone paper bypasses the cold water rotating cylinder, the pressing roller and the wrap angle adjusting roller in sequence, it passes out of the box body;

[0023] The cold water drum comprises an outer drum and an inner drum which are coaxially arranged. The left and right ends of the outer drum and the inner drum are sealed by sealing plates, so that a closed cavity is formed between the outer drum and the inner drum. The cavity is filled with hot water for heat exchange. A chilled water pipe is sheathed in the inner drum, and heat is exchanged with the hot water for heat exchange in the cavity through the chilled water pipe.

[0024] A circle of limit baffles is provided on the outer wall of the outer cylinder near both ends thereof, the silicone paper and the pressing roller are both located between the limit baffles, and a circle of teeth is provided on the portion outside the limit baffle to form a gear; a support frame is provided at the bottom of the outer cylinder, and the support frame is provided with driving gears meshing with the teeth on both sides of the corresponding limit baffles at intervals in front and back, and the driving gears are equipped with a rotating motor, and a plurality of support plates for stirring the hot water are fixed on the inner wall of the outer cylinder along its circumference, and the support plates rotate while the outer cylinder rotates, thereby stirring the hot water in the outer cylinder.

[0025] In the above solution: a heat-conducting layer is provided on the inner side of the inner cylinder.

[0026] In the above scheme: in step 4-2, the temperature range of the coating plate in summer is 75-80°C, and the temperature range in winter is 80-85°C.

[0027] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are: it can provide a method for coating and spreading a solvent-free plaster, without the need to add gasoline, reducing costs, without the need for drying in a drying tunnel, and without fire hazards. During the coating process, no pollution to the working environment will be generated due to gasoline volatilization, thus protecting the environment and reducing pollution. At the same time, it can also save investment in gasoline volatilization treatment equipment, further saving costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:

[0029] Figure 1 It is a schematic structural diagram of a coating machine and a composite cooling device of the present invention;

[0030] Figure 2 It is a schematic diagram of the structure of the coating machine;

[0031] Figure 3 It is a top view of the coating machine;

[0032] Figure 4 is a schematic diagram of a composite cooling device;

[0033] Figure 5 It is a front view of the cooling drum. DETAILED DESCRIPTION

[0034] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0035] like Figure 1-Figure 5 As shown, a solvent-free coating process comprises:

[0036] Step 1: ingredients; volatile ingredients are prepared according to the product type, wherein the volatile ingredients are menthol, camphor, borneol, salicylic acid, vegetable oil, and liquid paraffin, and liquefied; the menthol, borneol, and camphor are fully dissolved and evenly mixed with methyl salicylate and liquid paraffin by utilizing the co-melting characteristics of the menthol, borneol, and camphor.

[0037] Step 2: Rubber foaming: After the rubber is cut into pieces, it is pressed into thin sheets or screens by a rubber mixer, and static electricity is removed. It is spread out to cool in summer and soaked in the liquefied material of step 1 while it is hot in winter. Stir and mix, soak it to make it fully mixed with the liquid, turn it over twice in the middle, and soak it for 24 hours.

[0038] Step 3: Rubber refining: Press the soaked rubber into thin sheets with an open mill, then put it into a honey mill, add lead powder or zinc oxide, rosin particles or tinfoil resin, Chinese medicine extract and oil according to the prescription for mixing; mix it until a small amount of visible rubber particles remain in the paste, control the temperature of the honey refining room below 60°C, take it out and put it aside for use;

[0039] The preparation of rosin particles is as follows: heating and melting the rosin, stirring continuously during heating, then passing through a 100-mesh sieve to remove impurities, cooling the rosin liquid from which impurities have been filtered out, crushing it, and passing through a 20-40 mesh sieve to form rosin particles.

[0040] Step 4: Rough refining: put the honey-refined material into a rubber mixer for rough refining. The rough refining is to the extent that no rubber particles can be seen in the paste with the naked eye. After rough refining, take it out and set it aside for later use.

[0041] Step 5: Refining: Put the material obtained in step 4 into a rubber mixer for refining. The refining is carried out until the paste has good viscosity and elasticity.

[0042] Step 6: Divide into plates; put the refined material into a rubber mixer and divide it into plates, spread it on the plates with a thickness not exceeding 8mm, and set aside.

[0043] Step 7: Glue

[0044] 7-1: Put the material obtained in step 6 into an oven and heat it to soften it; the oven adopts a hot air circulation blast drying oven, the paste heating temperature is 60-65 degrees (the actual temperature inside the paste), the oven temperature is: 90-100 degrees in summer, 100-110 degrees in winter, and the heating time is: 30-60 minutes.

[0045] 7-2: Coating; put the softened material into the coating machine's trough, and heat the coating plate and scraper of the coating machine to prevent the material from hardening again.

[0046] 7-3: coating;

[0047] 7-4: After coating, the silicone paper is cooled by a composite cooling device and the composite cover material is cut into a specified width and rolled up by a slitting and winding device.

[0048] Step 8: Slice and package.

[0049] Coating system used in the present invention

[0050] It includes a glue applying device, a positioning coating device, a composite cooling device, a composite unwinding device c, a composite cloth feeding device d and a cutting and rewinding device e.

[0051] The coating machine mentioned above includes a glue coating device and a positioning coating device, wherein the positioning coating device includes a lower positioning rod, an adjustment sleeve, a return spring, a pressure coating steel belt, an upper positioning rod and a turning frame, which is the same as the technical solution disclosed in the patent document with publication number CN113798115B. The composite unwinding device c, the composite cloth feeding device d and the cutting and winding device are also the same as the solution disclosed in CN113798115B.

[0052] The difference is that since we use a solvent-free coating process, there is no need to add gasoline, so we have eliminated the drying oven.

[0053] Similar to the glue gluing device disclosed in the patent document CN113798115B, the glue gluing device of the present invention also includes a glue coating lower roller 4 and a glue coating upper roller 3 located above the glue coating lower roller 4, a coating material holding plate 1 which is higher in front and lower in the back is arranged in front of the glue coating lower roller 4, a glue containing groove 1b is arranged on the coating material holding plate 1, a side wall of the glue containing groove 1b close to the lower glue coating roller 4 is leaned against the roller surface of the lower glue coating roller 4, glue baffle plates 3 are respectively arranged on the left and right sides of the glue containing groove 1b, and the glue baffle plates 3 extend upward to the upper side of the roller surface of the glue coating upper roller.

[0054] The difference is that a heating wire 1a is provided on the back of the coating material holding plate 1, and the material on the coating material holding plate 1 is heated by the heating wire 1a; and a stirring mechanism for stirring the material is provided above the coating material holding plate 1.

[0055] Among them, the stirring mechanism includes two "C"-shaped stirring blades 5. The sealing ends of the two stirring blades 5 are respectively connected to the rotating shafts of the rotating motors 5b installed on the left and right side frames, and the rotating shafts pass through the rubber blocking plates 3 on the corresponding sides. The open ends of the two stirring blades 5 face each other, and one leg 5a of any one stirring blade 5 is located between the two legs 5a of the other stirring blade 5.

[0056] The composite cooling device is also the same as that disclosed in CN113798115B, and also includes a rotating cooling cylinder. A pressing roller 12 is provided above the rear of the cylinder, and a wrap angle adjusting roller 11 is provided below it. The silicone paper a bypasses the cold water rotating cylinder, the pressing roller 12, and the wrap angle adjusting roller 11 in sequence, and then passes out of the box body 7. The central axis of the roller shaft of the wrap angle adjusting roller 11 is located on the left side of the central axis of the roller shaft of the cold water rotating cylinder, so that the wrap angle of the silicone paper on the cold water rotating cylinder is greater than 180°. Preferably, the position where the central axis of the roller shaft of the wrap angle adjusting roller 11 deviates from the central axis of the roller shaft of the cold water rotating cylinder satisfies that the wrap angle of the silicone paper on the cold water rotating cylinder is 240°, that is, the coverage area of the silicone paper on the cold water rotating cylinder is large, so the cooling effect is good.

[0057] Among them, the wrap angle adjusting roller 11 is equipped with a composite unwinding device c for unwinding the bi-elastic fabric. Preferably, the composite unwinding device c is equipped with an unwinding automatic deviation correction device. This is prior art and will not be elaborated.

[0058] The composite fabric feeding device d is used to send the bi-elastic fabric b to the pressing roller 12, and includes a feeding roller, a tension-free roller, etc. This is prior art and will not be elaborated here.

[0059] Among them, the cooling cylinder disclosed in CN113798115B is a hollow cooling water roller. Different from this, in order to improve the cooling efficiency, we have improved the hollow cooling water roller and changed it to a cold water rotating cylinder extending left and right. The cold water rotating cylinder includes an outer cylinder 9a and an inner cylinder 9b arranged coaxially. The left and right ends of the outer cylinder 9a and the inner cylinder 9b are sealed by sealing plates, so that a closed cavity is formed between the outer cylinder 9a and the inner cylinder 9b, and the cavity is filled with heat exchange water. A refrigeration water pipe 10 is sleeved inside the inner cylinder 9b, and heat exchange is carried out between the refrigeration water pipe 10 and the heat exchange water in the cavity. Preferably, a heat conduction layer is provided on the inner side of the inner cylinder 9b to facilitate heat conduction. The refrigeration water pipe 10 is communicated with an external cold water supply system.

[0060] A circle of limit baffles 9d are provided on the outer wall of the outer cylinder 9a near both ends thereof, the silicone paper a and the pressing roller 12 are both located between the limit baffles 9d, and a circle of teeth are provided outside the limit baffles 9d to form a gear. A support frame is provided at the bottom of the outer cylinder 9a, and the support frame is provided with teeth on both sides of the corresponding limit baffles 9d, and driving gears 13 meshing therewith are arranged at intervals in front and back on the support frame, and the driving gears 13 are equipped with a rotating motor, and the outer cylinder 9a is driven to rotate through the driving gears 13. A number of support plates 9c for stirring the hot water are fixed on the inner wall of the outer cylinder 9a along its circumference, and the support plates 9c rotate while the outer cylinder 9a rotates, thereby stirring the hot water in the outer cylinder 9a.

[0061] During operation, the refined material is placed in an oven for heating and softening after being separated into plates. The softened material is transported to the glue tank on the coating plate 1 by a delivery pump, and glue baffles 2 are arranged on both sides. The glue baffles 2 extend upward to the upper side of the coating roller 3 to prevent the glue from leaking. The electric heating wire 1a on the back of the coating plate 1 can heat the material on the coating plate 1, and stir it through the stirring blade 5 to fully heat the material.

[0062] The silicone paper a enters from the lower side of the glue coating lower roller 4, and first passes through between the glue coating lower roller 4 and the glue coating upper roller 3. Then adjust the tension rod 15 to make the pressure coating steel belt 13 tightly attached to the silicone paper a. The part of the pressure coating steel belt 13 attached to the silicone paper a will not be coated with glue during gluing, and becomes a reserved easy-to-tear edge.

[0063] The material is squeezed out through the gap between the lower glue roller 4 and the upper glue roller 3 to form a plaster of a certain thickness attached to the silicone paper a, thereby completing the coating.

[0064] After coating, the silicone paper a is transferred to the composite cooling device and cooled by the cooling drum. The biaxial stretch fabric b is sent to the laminating roller 12 through the composite unwinding device c and the composite fabric feeding device d. The silicone paper a passes between the cold water drum and the laminating roller 12 to be laminated with the biaxial stretch fabric b, and is cooled by the wrap angle adjustment roller 11 while being pressed against the surface of the cooling drum.

[0065] When liquid cooling is performed, the outer cylinder 9a of the cooling drum is driven to rotate by the driving gears 13 on the front and rear sides. At the same time, when the outer cylinder 9a rotates, the hot water in the cavity between the outer cylinder 9a and the inner cylinder 9b is stirred by the support plate 9c to make the water temperature uniform, which is convenient for heat exchange with the water temperature of the freezing water pipe 10, thereby improving the cooling effect.

[0066] The composite silicone paper a coming out of the wrap angle adjustment roller 11 is transported to the cutting and winding device e through the automatic deviation correction device. The automatic deviation correction device adopts the existing mechanism, and the cutting and winding device also has the existing structure, and the specific structure is not shown in the figure.

[0067] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.

Claims

1. A solvent-free coating process, characterized in that: Including: Step 1: Ingredients preparation; Prepare volatile components, which are menthol, camphor, borneol, salicylic acid, vegetable oil and liquid paraffin, and then liquefy them. Step 2: Soaking the rubber; After cutting the rubber into pieces, press it into thin sheets or wire meshes by a rubber mill, remove static electricity, add it to the liquefied material in Step 1, stir and mix, and soak it. In Step 2, during soaking, turn it over twice in the middle, and the soaking time is more than 24 hours. Step 3: Rubber refining; Press the soaked rubber into thin sheets by an open mill, then put it into a kneader, and add lithopone or zinc oxide, rosin particles or terpene resin, Chinese medicine extract and grease according to the prescription for kneading; Knead until there are a small amount of visible rubber particles remaining in the paste, control the temperature of the kneading chamber below 60°C, take it out and set it aside for later use. Step 4: Rough refining; Place the kneaded material in a rubber mill for rough refining until no rubber particles can be seen with the naked eye in the paste, take it out after rough refining and set it aside for later use. Step 5: Fine refining; Put the material obtained in Step 4 into a rubber mill for fine refining. Step 6: Dividing into plates; Put the material obtained by fine refining into a rubber mill for dividing into plates, and lay it flat in the plate with a thickness not exceeding 8 mm, and set it aside for later use. Step 7: Coating; 7-1 Heat the material obtained in Step 6 in an oven to soften it. 7-2: Coating; Put the softened material on the material storage tank of the coater, and heat the coating material storage plate and the scraper of the coater; Avoid the material from hardening again. 7-3: Coating; 7-4: After coating, the silicone paper is cooled through a composite cooling device and laminated with a cover layer material, cut into a specified width and wound up. Step 8: Slicing and packaging; The coater includes a rubber material coating device and a positioning coating device. The rubber material coating device includes a lower coating roller (4) and an upper coating roller (3) located above the lower coating roller (4). In front of the lower coating roller (4), there is a coating material storage plate (1) with a front high and rear low shape. There is a glue storage tank (1b) on the coating material storage plate (1). The side wall of the glue storage tank (1b) close to the lower coating roller (4) leans against the roller surface of the lower coating roller (4). There are baffle plates on the left and right sides of the glue storage tank (1b), and the baffle plates extend upward to the upper side of the roller surface of the upper coating roller. There is a heating wire (1a) on the back of the coating material storage plate (1) to heat the material in the glue storage tank (1b); Above the coating material storage plate (1), there is a stirring mechanism for stirring the material. The stirring mechanism includes two "匚"-shaped stirring blades (5). The closed ends of the two stirring blades (5) are respectively connected to the rotating shafts of the rotating motors (5b) installed on the left and right side frames, and the rotating shafts pass through the corresponding baffle plates. The open ends of the two stirring blades (5) face each other, and one leg (5a) of any one stirring blade is located between the two legs (5a) of the other stirring blade. The composite cooling device comprises a cold water drum extending left and right, a pressing roller (12) is provided at the upper rear of the cold water drum, and an angle adjustment roller (11) is provided at the lower part of the cold water drum, and the silicone paper (a) passes through the cold water drum, the pressing roller (12) and the angle adjustment roller (11) in sequence and then passes out of the box body (7); The cold water drum comprises an outer drum (9a) and an inner drum (9b) which are coaxially arranged, and the left and right ends of the outer drum (9a) and the inner drum (9b) are sealed by sealing plates, so that a closed cavity is formed between the outer drum (9a) and the inner drum (9b), and the cavity is filled with hot water for heat exchange; the inner drum (9b) is sheathed with a chilled water pipe (10), and heat is exchanged with the hot water for heat exchange in the cavity through the chilled water pipe (10); A circle of limit baffles (9d) are provided on the outer wall of the outer cylinder (9a) near both ends thereof, the silicone paper (a) and the laminating roller (12) are both located between the limit baffles (9d), and a circle of teeth are provided on the outer portion of the limit baffles (9d) to form a gear; a support frame is provided at the bottom of the outer cylinder (9a), and driving gears (13) meshing with the teeth on both sides of the corresponding limit baffles (9d) are arranged at intervals in front and back on the support frame, and the driving gears (13) are equipped with a rotating motor; a plurality of support plates (9c) for stirring the hot water are fixed on the inner wall of the outer cylinder (9a) along its circumference, and the support plates (9c) rotate while the outer cylinder (9a) rotates, thereby stirring the hot water in the outer cylinder (9a).

2. A solvent-free coating process according to claim 1, characterized in that: The preparation method of the rosin particles is as follows: heating and melting the rosin, stirring continuously during heating, then passing through a 100-mesh sieve to remove impurities, cooling the rosin liquid from which the impurities have been filtered out, crushing it, passing through a 20-40 mesh sieve to obtain the rosin particles for later use.

3. The solvent-free coating process according to claim 1, characterized in that: The oven is a hot air circulation blast drying oven, the paste heating temperature is 60-65 degrees, the oven temperature is: 90-100 degrees in summer, 100-110 degrees in winter, and the heating time is: 30-60 minutes.

4. A solvent-free coating process according to claim 1, characterized in that: A heat-conducting layer is provided on the inner side of the inner cylinder (9b).

5. The solvent-free coating process according to claim 1, characterized in that: In step 4-2, the temperature of the coating plate (1) is in the range of 75-80°C in summer and in the range of 80-85°C in winter.

Citation Information

Patent Citations

  • A topical plaster positioning coating composite cooling system

    CN113798115B

  • Dustproof production method for rubber paste

    CN102727383A

  • Base material for adhesive plaster production through hot-press method, and adhesive plaster preparation method utilizing base material

    CN104873480A

  • Ointment capable of removing dampness and relieving pain and preparation method of ointment

    CN104906544A

  • Production process of Zushima joint analgesic plaster