A method for preparing a low temperature resistant, aging resistant and explosion-proof gas pipe
By installing a protective layer of foam, aging-resistant aging agent and metal spring microfilaments on the outside of the stainless steel pipe, the problem of aging of gas pipelines under low temperature and ultraviolet light is solved, and a high-performance, easy-to-operate and safe gas pipeline design is achieved.
Patent Information
- Application Number
- CN202210587239.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-05-26
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-05-26
AI Technical Summary
Existing gas pipelines are prone to aging and rupture under low temperature and ultraviolet rays. The existing multi-layer structures are complex in operation and low durability during installation and use, and have poor performance.
A protective layer is provided on the outside of the stainless steel pipe, including foam, aging-resistant agent, plasticizer and micro-scale metal spring microfilaments. A single-layer structure is formed through a heat shrink coating process to improve anti-freeze, anti-aging and explosion-proof performance.
It significantly improves the anti-freeze, anti-aging and explosion-proof performance of gas pipelines, has high structural strength, is simple to operate, is easy to industrial production, and reduces the damage to the surrounding environment by material breakage and debris in low temperature environments.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention relates to the field of pipelines, and in particular to a method for preparing a low-temperature-resistant, aging-resistant and explosion-proof gas pipe. Background Art
[0002] Gas pipelines are pipelines that transport natural gas from mining sites or processing plants to urban gas distribution centers or industrial enterprise users. They have the advantages of low transportation cost, small land occupation, fast construction, large oil and gas transportation volume, high safety performance, low transportation loss, no three wastes, low risk of leakage, low environmental pollution, small impact of bad weather, small equipment maintenance, easy management, and easy remote centralized monitoring. The types and functions of gas pipelines in the prior art are diverse. For example, publication number CN214305734U discloses a gas pipeline with antifreeze and anticorrosion functions, including a pipeline body, both left and right ports of the pipeline body are equipped with connectors, multiple screw holes are evenly opened inside the connectors, and screws are screwed inside the screw holes. A base is installed below the pipeline body, and a support plate is connected above the base. A groove is provided in the middle of the upper wall of the support plate, and the groove is adapted to the pipeline body. A buffer protective layer is provided on the upper wall of the inner cavity of the support plate, and the outer surface of the buffer protective layer contacts the outer surface of the lower wall of the pipeline body, and is in the first antifreeze layer. Under the joint action of the second antifreeze layer and the corrosion-resistant layer, the pipeline body has the functions of antifreeze and anti-corrosion. Under the action of the leak-proof gasket, multiple pipeline bodies are not prone to leakage after being connected by three connecting heads. Under the action of the buffering protection layer, the pipeline body and the support plate are not easily damaged under severe high vibration.
[0003] Another example is publication number CN210462175U, which discloses an insulated and antifreeze gas pipeline, which provides a gas pipeline with good thermal insulation effect, good antifreeze effect and simple structure. The key points of its technical solution are that it also includes an insulation mechanism coated outside the outer sheath, and the insulation mechanism includes a first insulation layer coated outside the outer sheath, a second insulation layer coated outside the outer sheath, and a connecting component that sequentially connects the first insulation layer and the second insulation layer. Limit blocks are provided on the contact surface between the first insulation layer and the outer sheath, and on the contact surface between the second insulation layer and the outer sheath. The outer sheath is provided with an outer ring groove that matches the limit block, which is suitable for the field of gas pipeline technology.
[0004] Another example is publication number CN214368520U, which discloses a pipeline antifreeze structure, including a pipeline body, a positioning tube fixedly provided at the middle position of the top of the pipeline body, a positioning plate fixedly provided at the top of the positioning tube, a motor fixedly provided at the top of the positioning plate, a rotating shaft fixedly provided at the output end of the motor through the positioning plate, a first gear fixedly provided at the bottom end of the rotating shaft, a rotating shaft fixedly provided through the output end of the motor through the positioning plate, a first gear fixedly provided at the bottom end of the rotating shaft, an outer wall of the first gear meshes with an outer wall of the second gear, so that the second gear drives two screw rods to rotate and connect, and the top ends of the two sliders are convenient for movement through the card groove and the card strip, thereby preventing the liquid inside the pipeline body from freezing, which not only makes the pipeline antifreeze efficiency higher and facilitates the internal liquid transportation efficiency, but also protects the pipeline body and improves the service life of the pipeline.
[0005] The applicant found that when the gas pipeline is connected to the user end from the underground transmission section, one end of the gas pipeline needs to be connected from the gas pipeline buried deep underground. This section of the gas pipeline will be exposed to the external environment and will easily age after being exposed to ultraviolet light for a long time. When the ambient temperature is low, the gas pipeline will rupture and cause leakage. The prior art will add a multi-layer structure to this section of the pipeline to increase the safety of this section of the gas pipeline, but the prior art also has the following problems: the multi-layer structure is complicated to install and use, and each layer of the structure only has one of the properties of aging resistance, low temperature resistance, and structural strength. At the same time, the multi-layer composite structure has low durability and poor performance when used in a complex environment. Summary of the invention
[0006] In order to overcome the problems of the prior art adopting a multi-layer structure, complicated operation during installation and use, single function of each layer of the structure, low durability and poor performance when used in a complex environment, a low-temperature resistant, aging-resistant and explosion-proof gas pipe and a preparation method thereof are provided. By arranging a low-temperature resistant, aging-resistant and high-strength protective layer on the outside of the stainless steel pipe, the anti-freeze, anti-aging and explosion-proof performance of the gas pipeline is significantly improved. The preparation method of the present application has a simple process and is easy to industrialize.
[0007] The specific technical scheme of the present invention is:
[0008] A low-temperature-resistant, aging-resistant and explosion-proof gas pipe comprises a stainless steel pipe and a protective layer sleeved on the outside of the stainless steel pipe, wherein the protective layer comprises a foam, an aging-resistant agent, a plasticizer and spring microfilaments in a mass ratio of 10-30:0.2-0.5:0.3-0.7:3-5.
[0009] The present application provides a low-temperature-resistant, aging-resistant and explosion-proof gas pipe. A protective layer is arranged on the outside of the stainless steel pipe, which significantly improves the anti-freeze, aging-resistant and explosion-proof performance of the gas pipe. The protective layer material includes a foam, an anti-aging agent, a plasticizer and a spring microfilament. The anti-aging agent is added to enhance the anti-ultraviolet performance of the protective layer, reduce the corrosion of ultraviolet rays to the material, and reduce the aging rate of the material. The addition of a plasticizer increases the cold resistance of the protective layer. The plasticizer used in the present application is a cold-resistant plasticizer, which can enhance the toughness of the protective layer. At the same time, the chemical bonds formed by the cold-resistant plasticizer and the foam will not break due to low temperature. The structural strength is higher in a low-temperature environment, and the aging resistance is enhanced. The structural strength of the protective layer can be significantly enhanced by adding spring microfilaments. The spring microfilaments used in the present application are micron-level metal springs, which have a certain stress load. When the protective layer receives external stress, it can act as a buffer to buffer the external stress. When the protective layer is in a cold environment, the protective layer material itself will shrink. At this time, the spring microwires inside the protective layer can resist the shrinkage force generated by the material, support the material structure, and prevent the protective layer from breaking. In addition, the spring microwires can also act as reinforcing ribs inside the protective layer. When the protective layer is subjected to pressure from the inside to the outside, the spring microwires can enhance the connection between the protective layer materials. When the pressure is in the stress load range of the spring microwires, the spring microwires themselves can buffer the received pressure to ensure the structural safety of the protective layer material. When the pressure exceeds the stress load range of the spring microwires, the spring microwires can also act as connectors to connect the material structures together to reduce the degree of material breakage. When an explosion occurs, the damage to the surrounding environment by material fragments is reduced, thereby enhancing safety.
[0010] Preferably, the foam is selected from any one or more of polyvinyl chloride, polyethylene and polyurethane.
[0011] Preferably, the spring microwire is selected from any one or more of stainless steel, aluminum alloy and copper alloy.
[0012] Preferably, the anti-aging agent is selected from any one or more of UV-531, UV-326, UV-741 and JW-791.
[0013] Preferably, the plasticizer is selected from any one or more of dioctyl adipate, dioctyl sebacate, dioctyl terephthalate and epoxidized soybean oil.
[0014] Preferably, the spring microwire has a wire diameter of 5-100 μm and a length of 300-500 μm.
[0015] Preferably, the preparation steps of the spring microwire are as follows:
[0016] (1) Rough wire drawing: The stainless steel raw wire is rough-drawn to make stainless steel rough wire, the wire diameter of the stainless steel rough wire is 5 mm, and the stainless steel rough wire is annealed once after wire drawing, the annealing temperature is 300~1050℃, and the annealing rate is 5m / s;
[0017] (2) Medium wire drawing: The stainless steel coarse wire in step (1) is subjected to secondary wire drawing to form a stainless steel medium wire, wherein the wire diameter of the stainless steel medium wire is 1 mm. After wire drawing, the stainless steel medium wire is subjected to secondary annealing, wherein the annealing temperature is 300-1050° C. and the annealing rate is 5 m / s;
[0018] (3) Micro wire drawing: The stainless steel medium wire in step (2) is drawn three times to form a stainless steel micro wire, the wire diameter of the stainless steel micro wire is 0.15 mm, and the stainless steel micro wire is annealed three times after drawing, the annealing temperature is 300-1050°C, and the annealing rate is 5 m / s;
[0019] (4) Four-time wire drawing: The stainless steel microwire in step (3) is drawn four times to form a spring microwire. After drawing, the spring microwire is annealed four times at an annealing temperature of 300-1000°C and an annealing time of 10 min.
[0020] A method for preparing a low-temperature resistant, aging resistant and explosion-proof gas pipe comprises the following steps:
[0021] a) preparing spring microwires;
[0022] b) preparing the protective layer: mixing the foam, the anti-aging agent, the plasticizer and the spring microfilaments at a mixing speed of 1000 to 2000 rpm, and then extruding the mixture and blowing it into a tube, and rapidly cooling and shaping it to form the protective layer;
[0023] c) Heat shrink wrapping: The protective layer is put on the outside of the stainless steel pipe, and the protective layer is heated to shrink and fit the outer wall of the stainless steel pipe to make a low-temperature, aging-resistant and explosion-proof gas pipe.
[0024] The present application also provides a method for preparing a low-temperature-resistant, aging-resistant and explosion-proof gas pipe, which adopts a heat shrink coating processing method to sleeve a protective layer on a stainless steel pipe. During processing, the protective layer in a highly elastic state is quickly cooled to enter a glass state, at which time the shape of the protective layer is fixed. When in use, the protective layer is transformed into a glass state by heating, at which time the protective layer will shrink in volume and complete the heat shrink coating. The assembly of this process is simple and easy to operate, and it is easy to industrialize.
[0025] Preferably, the heating temperature in step c) is 80-120°C.
[0026] Compared with the prior art, this application has the following technical effects:
[0027] (1) This application adopts a single-layer protective layer, which has a simple structure and high anti-freeze, anti-aging and explosion-proof performance;
[0028] (2) The preparation method of the present application is simple and easy to operate and can be easily industrialized;
[0029] (3) The spring microwires of the present application can be used as a buffer to buffer external stress. When the protective layer is in a cold environment, the protective layer material itself will shrink. At this time, the spring microwires inside the protective layer can resist the shrinkage force generated by the material, support the material structure, and prevent the protective layer from breaking;
[0030] (4) The spring microwire of the present application can also act as a reinforcing rib inside the protective layer, which can connect the material structure together, reduce the degree of material breakage, and when an explosion occurs, reduce the damage of material fragments to the surrounding environment, thereby enhancing safety. DETAILED DESCRIPTION
[0031] The present invention will be further described below in conjunction with the embodiments.
[0032] Embodiment 1:
[0033] A low-temperature-resistant, aging-resistant and explosion-proof gas pipe comprises a stainless steel pipe and a protective layer sleeved on the outside of the stainless steel pipe, the protective layer comprising a foam body, an aging-resistant agent, a plasticizer and spring microfilaments in a mass ratio of 18:0.3:0.4:4; the foam body is polyvinyl chloride, and the spring microfilaments are stainless steel; the aging-resistant agent is selected from UV-531; the plasticizer is dioctyl adipate; the wire diameter of the spring microfilament is 5-100 μm, and the length is 300-500 μm.
[0034] The preparation steps of spring microwire are as follows:
[0035] (1) Rough wire drawing: Use a wire drawing machine to rough draw the stainless steel raw wire into stainless steel rough wire, the wire diameter of the stainless steel rough wire is 5 mm, and after wire drawing, the stainless steel rough wire is annealed once, the annealing temperature is 1000 ° C, and the annealing rate is 5 m / s;
[0036] (2) Medium wire drawing: The stainless steel rough wire in step (1) is subjected to secondary wire drawing to form a stainless steel medium wire, wherein the wire diameter of the stainless steel medium wire is 1 mm. After wire drawing, the stainless steel medium wire is subjected to secondary annealing, wherein the annealing temperature is 1000° C. and the annealing rate is 5 m / s;
[0037] (3) Micro-wire drawing: The stainless steel medium wire in step (2) is drawn three times to form a stainless steel micro-wire, wherein the wire diameter of the stainless steel micro-wire is 0.15 mm. After drawing, the stainless steel micro-wire is annealed three times, wherein the annealing temperature is 1000° C. and the annealing rate is 5 m / s;
[0038] (4) Four-time wire drawing: The stainless steel microwire in step (3) is drawn four times to form a spring microwire. After drawing, the spring microwire is annealed four times at an annealing temperature of 975° C. and an annealing time of 10 min.
[0039] A method for preparing a low-temperature resistant, aging resistant and explosion-proof gas pipe comprises the following steps:
[0040] a) preparing spring microwires;
[0041] b) preparing the protective layer: mixing the foam, the anti-aging agent, the plasticizer and the spring microfilaments at a mixing speed of 500-700 r / min for 60-90 min, extruding the mixture after mixing evenly and blow-molding it into a tube, and rapidly cooling and shaping it to form the protective layer;
[0042] c) Heat shrink wrapping: put the protective layer on the outside of the stainless steel pipe, heat it to shrink the protective layer and make it fit the outer wall of the stainless steel pipe to make a low-temperature, aging-resistant and explosion-proof gas pipe. The heating temperature is 80°C.
[0043] Embodiment 2:
[0044] Compared with Example 1, the protective layer includes a foam, an anti-aging agent, a plasticizer and spring microfilaments in a mass ratio of 15:0.8:0.5:5. The foam is polyvinyl chloride, the spring microfilaments are stainless steel, the aging agent is UV-531; the plasticizer is dioctyl sebacate; the wire diameter of the spring microfilament is 50 μm and the length is 400 μm; the other conditions are the same as those in Example 1.
[0045] Embodiment 3:
[0046] Compared with Example 1, the protective layer includes a foam, an anti-aging agent, a plasticizer and spring microfilaments in a mass ratio of 25:0.4:0.6:6.5, the foam is polyethylene, the spring microfilaments are stainless steel, the aging agent is UV-741; the plasticizer is dioctyl terephthalate; the wire diameter of the spring microfilament is 80 μm and the length is 350 μm; the other conditions are the same as those in Example 1.
[0047] Embodiment 4:
[0048] Compared with Example 1, the protective layer includes a foam, an anti-aging agent, a plasticizer and spring microfilaments in a mass ratio of 22:0.9:0.3:5, the foam is polyethylene, the spring microfilaments are stainless steel, the aging agent is UV-326; the plasticizer is epoxy soybean oil; the wire diameter of the spring microfilament is 100 μm and the length is 300 μm; the other conditions are the same as those in Example 1.
[0049] Embodiment 5:
[0050] Compared with Example 1, the protective layer includes a foam, an anti-aging agent, a plasticizer and spring microfilaments in a mass ratio of 17:0.6:0.45:7, the foam is polyurethane, the spring microfilaments are stainless steel, the aging agent is JW-791; the plasticizer is dioctyl adipate; the wire diameter of the spring microfilament is 30μm, and the length is 500μm; the other conditions are the same as those in Example 1.
[0051] Embodiment 6:
[0052] Compared with Example 1, the protective layer includes a foam, an anti-aging agent, a plasticizer and spring microfilaments in a mass ratio of 22:0.9:0.3:5, the foam is polyurethane, the spring microfilaments are stainless steel, the aging agent is UV-326; the plasticizer is epoxy soybean oil; the wire diameter of the spring microfilament is 100 μm, and the length is 300 μm; the other conditions are the same as those in Example 1. .
[0053] Example 7
[0054] Compared with Example 1, the spring microwire is made of aluminum alloy; the wire diameter of the spring microwire is 100 μm and the length is 400 μm.
[0055] The preparation steps of spring microwire are as follows:
[0056] (1) Rough wire drawing: A wire drawing machine is used to rough draw the aluminum alloy raw wire into aluminum alloy rough wire. The wire diameter of the aluminum alloy rough wire is 5 mm. After wire drawing, the aluminum alloy rough wire is annealed once. The annealing temperature is 340 ° C and the annealing rate is 5 m / s.
[0057] (2) Wire drawing: The aluminum alloy raw wire in step (1) is subjected to secondary wire drawing to form a stainless steel medium wire, wherein the diameter of the aluminum alloy medium wire is 1 mm. After wire drawing, the aluminum alloy medium wire is subjected to secondary annealing, wherein the annealing temperature is 340° C. and the annealing rate is 5 m / s;
[0058] (3) Micro-wire drawing: The aluminum alloy medium wire in step (2) is wire-drawn three times to form aluminum alloy micro-wires, wherein the wire diameter of the aluminum alloy micro-wires is 0.15 mm. After wire drawing, the aluminum alloy micro-wires are annealed three times, wherein the annealing temperature is 340° C. and the annealing rate is 5 m / s.
[0059] (4) Four-time wire drawing: The aluminum alloy microwire in step (3) is drawn four times to form a spring microwire. After drawing, the spring microwire is annealed four times at an annealing temperature of 340° C. and an annealing time of 10 min.
[0060] The remaining conditions are the same as those in Example 1.
[0061] Example 8
[0062] Compared with Example 1, the spring microwire is made of brass; the wire diameter of the spring microwire is 50 μm, and the length is 500 μm.
[0063] The preparation steps of spring microwire are as follows:
[0064] (1) Rough wire drawing: Use a wire drawing machine to rough draw the brass raw wire into brass rough wire. The wire diameter of the brass rough wire is 5 mm. After wire drawing, the stainless steel rough wire is annealed once. The annealing temperature is 600 ° C and the annealing rate is 5 m / s.
[0065] (2) Medium wire drawing: The brass rough wire in step (1) is subjected to secondary wire drawing to form a brass medium wire, wherein the wire diameter of the brass medium wire is 1 mm. After wire drawing, the brass medium wire is subjected to secondary annealing, wherein the annealing temperature is 600° C. and the annealing rate is 5 m / s;
[0066] (3) Micro-wire drawing: The brass medium wire in step (2) is drawn three times to form a brass micro-wire, the wire diameter of the brass micro-wire is 0.15 mm, and after drawing, the brass micro-wire is annealed three times, the annealing temperature is 600° C., and the annealing rate is 5 m / s;
[0067] (4) Four-time wire drawing: The stainless steel microwire in step (3) is drawn four times to form a spring microwire. After drawing, the spring microwire is annealed four times at an annealing temperature of 620° C. and an annealing time of 10 min.
[0068] The remaining conditions are the same as those in Example 1.
[0069] Comparative Example 1
[0070] A low-temperature-resistant, aging-resistant and explosion-proof gas pipeline comprises a stainless steel pipe and a protective layer sleeved on the outside of the stainless steel pipe, wherein the protective layer comprises a protective layer, a low-temperature-resistant layer and an aging-resistant layer; the protective layer is stainless steel, the low-temperature-resistant layer is a low-temperature-resistant polyurethane foam, and the aging-resistant layer is an anti-ultraviolet polyethylene foam.
[0071] The protective layer of the gas pipeline made in the above-mentioned embodiment and comparative example was tested, and the thickness of the protective layer was 5 mm.
[0072] Weather resistance test: Test its weather resistance in a special environment with an ambient temperature of -40°C and continuous irradiation with ultraviolet light (290nm~400nm), and record the cracking time of the gas pipeline protective layer.
[0073] Pressure limit test: Seal both ends of the protection, continuously pressurize the protective layer, and test the pressure limit of the protective layer.
[0074] Performance testing: The above-mentioned embodiment was tested using a tensile testing machine to test the tensile strength and elongation at break of the protective layer.
[0075] Table 1 Test results
[0076]
[0077] Compared with the control example, the cracking rate of the embodiment in a cold environment with continuous ultraviolet irradiation is significantly reduced, and the pressure limit, tensile strength and elongation at break of the embodiment are significantly increased. The results show that the application provides a low-temperature, aging-resistant and explosion-proof gas pipe with high cold resistance, aging resistance and structural strength, and the gas pipeline process of the application is simple, easy to produce and convenient to install and operate.
[0078] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent transformation made to the above embodiment based on the technical essence of the present invention still falls within the protection scope of the technical solution of the present invention.
Claims
1. A method for preparing a low temperature resistant, aging resistant and explosion-proof gas pipe, characterized in that: The following steps are involved: a) Preparation of spring microwires, The preparation steps of the spring microwire are as follows: (1) Rough wire drawing: The stainless steel raw wire is rough-drawn to make stainless steel rough wire, the wire diameter of the stainless steel rough wire is 5 mm, and the stainless steel rough wire is annealed once after wire drawing, the annealing temperature is 300~1050℃, and the annealing rate is 5m / s; (2) Medium wire drawing: The stainless steel coarse wire in step (1) is subjected to secondary wire drawing to form a stainless steel medium wire, wherein the wire diameter of the stainless steel medium wire is 1 mm. After wire drawing, the stainless steel medium wire is subjected to secondary annealing, wherein the annealing temperature is 300-1050° C. and the annealing rate is 5 m / s; (3) Micro wire drawing: The stainless steel medium wire in step (2) is drawn three times to form a stainless steel micro wire, the wire diameter of the stainless steel micro wire is 0.15 mm, and the stainless steel micro wire is annealed three times after drawing, the annealing temperature is 300-1050°C, and the annealing rate is 5 m / s; (4) Four-time wire drawing: The stainless steel microwire in step (3) is drawn four times to form a spring microwire. After drawing, the spring microwire is annealed four times at an annealing temperature of 300-1000°C and an annealing time of 10 min. b) preparing the protective layer: mixing the foam, the anti-aging agent, the plasticizer and the spring microfilaments, extruding the mixture after mixing evenly and blow-molding it into a tube, and rapidly cooling and shaping it to form the protective layer; c) Heat shrink wrapping: The protective layer is placed on the outside of the stainless steel pipe, and the protective layer is heated to shrink and fit the outer wall of the stainless steel pipe to make a low-temperature resistant, aging-resistant and explosion-proof gas pipe; The low-temperature-resistant, aging-resistant and explosion-proof gas pipe comprises a stainless steel pipe and a protective layer sleeved on the outside of the stainless steel pipe, wherein the protective layer comprises the following components in mass proportions: 10-25 foaming body: 0.2-1.2 anti-aging agent: 0.3-0.7 plasticizer: 3-8 spring microfilaments, wherein the wire diameter of the spring microfilament is 5-100 μm and the length is 300-500 μm.
2. The preparation method according to claim 1, characterized in that: The foam is selected from one or more of polyvinyl chloride, polyethylene and polyurethane.
3. The preparation method according to claim 1, characterized in that: The anti-aging agent is selected from one or more of UV-531, UV-326, UV-741 and JW-791.
4. The preparation method according to claim 1, characterized in that: The plasticizer is selected from one or more of dioctyl adipate, dioctyl sebacate, dioctyl terephthalate and epoxidized soybean oil.
5. The preparation method according to claim 1, characterized in that: The heating temperature in c) is 80-120°C.
6. The preparation method according to claim 1, characterized in that: The mixing speed in b) is 500-700 r / min.
7. The preparation method according to claim 1, characterized in that: The mixing time in b) is 60 to 90 minutes.