Method for manufacturing semiconductor device
By forming a carbon protective layer on the bit line structure of the semiconductor device and etching the layer, the problem of damage to the bit line structure when forming the storage node contact hole is solved, and the dimensional accuracy and yield of the semiconductor device are improved.
Patent Information
- Application Number
- CN202110334039.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-03-29
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-03-29
AI Technical Summary
During the manufacturing process of semiconductor devices, the top of the bit line structure in the prior art is easily etched away when forming the storage node contact hole, resulting in dimensional deviation and reducing the yield of the semiconductor device.
By forming a carbon protective layer on the bit line structure, using a plasma carbon source to deposit onto the top surface of the bit line structure, and etching the carbon protective layer without directly etching the bit line structure, the integrity of the bit line structure is ensured.
Damage to the bit line structure is effectively avoided, the dimensional accuracy and yield of the semiconductor device are ensured, and the reliability of the manufacturing process is improved.
Smart Images

Figure CN115148672B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a method for manufacturing a semiconductor device. Background Art
[0002] In the semiconductor device manufacturing process, after a bit line structure is formed through deposition and etching processes, a storage node contact hole is further formed on the semiconductor substrate corresponding to the bit line contact hole between the bit line structures, so as to form a storage node contact plug in the storage node contact hole to further form a capacitor structure.
[0003] In the prior art, a storage node contact hole is generally etched on a semiconductor substrate through an etching process, but at the same time the top of the bit line structure is also etched away, that is, after the storage node contact hole is formed, the top of the bit line structure is consumed and the size deviates, resulting in a reduced yield of the entire semiconductor device.
[0004] The above information disclosed in this Background section is only for enhancement of understanding of the background of the invention and therefore it may contain information that does not form the prior art that is already known to a person of ordinary skill in the art. Summary of the invention
[0005] A main purpose of the present invention is to provide a method for manufacturing a semiconductor device, which can effectively prevent the bit line structure from being etched during the process of forming a storage node contact hole, so that the bit line structure remains intact and the yield of the semiconductor device is improved.
[0006] In order to achieve the above-mentioned purpose, the present invention provides a method for manufacturing a semiconductor device, comprising: forming a plurality of spaced bit line structures on a substrate of the semiconductor device, wherein the plurality of bit line structures extend along a first direction; forming a sacrificial layer between the plurality of bit line structures; placing the semiconductor device in a reaction chamber of an etching device; releasing a carbon source gas into the reaction chamber, and providing an alternating electric field to dissociate the carbon source gas to generate a plasma carbon source; controlling the plasma carbon source to be deposited on the top surface of the bit line structure to form a carbon protective layer; etching the sacrificial layer and a portion of the substrate to form a storage node contact hole; and removing the carbon protective layer.
[0007] According to an exemplary embodiment of the present invention, releasing the carbon source gas into the reaction chamber and providing an alternating electric field to dissociate the carbon source gas to generate a plasma carbon source includes: controlling the dissociation power of the alternating electric field to be 1000-1500W and the dissociation frequency to be 10-20MHz.
[0008] According to an exemplary embodiment of the present invention, the vacuum pressure in the reaction chamber is controlled to be 20-40 mtorr, and the temperature is controlled to be 30° C.-40° C.
[0009] According to an exemplary embodiment of the present invention, controlling the plasma carbon source to be deposited onto the top surface of the bit line structure includes: controlling the longitudinal bias power of the alternating electric field to be 0-10 W and the longitudinal bias frequency to be 500 KHz-5 MHz.
[0010] According to an exemplary embodiment of the present invention, the vacuum pressure in the reaction chamber is controlled to be 5-20 mtorr, and the temperature is controlled to be 30° C.-40° C.
[0011] According to an exemplary embodiment of the present invention, the thickness of the carbon protective layer is 2-40 nm.
[0012] According to an exemplary embodiment of the present invention, the carbon source gas is at least one of CH4, C2H6 and C4H8.
[0013] According to an exemplary embodiment of the present invention, the sacrificial layer and a portion of the substrate are etched using a dry etching process to form the storage node contact hole.
[0014] According to an exemplary embodiment of the present invention, the carbon protection layer is removed by using a plasma process, an ashing process or a wet etching process.
[0015] According to an exemplary embodiment of the present invention, forming a sacrificial layer between the plurality of bit line structures comprises: filling an initial sacrificial layer between the plurality of bit line structures; forming spaced photoresist patterns on the initial sacrificial layer, each of the photoresist patterns extending along a second direction, the second direction intersecting the first direction; using the photoresist pattern as a mask, etching a portion of the initial sacrificial layer to form a blind hole until the bottom of the blind hole exposes the substrate; forming a spacer layer to fill the blind hole; removing the photoresist pattern, and the remaining initial sacrificial layer is the sacrificial layer.
[0016] According to an exemplary embodiment of the present invention, the sacrificial layer is silicon nitride, silicon oxide or silicon oxynitride.
[0017] According to an exemplary embodiment of the present invention, the spacer layer is silicon nitride or silicon oxynitride.
[0018] According to an exemplary embodiment of the present invention, the method further includes: forming a storage node contact plug in the storage node contact hole.
[0019] According to an exemplary embodiment of the present invention, the storage node contact plug is metal silicide, polysilicon, metal oxynitride or metal.
[0020] According to an exemplary embodiment of the present invention, a data storage element is formed on the storage node contact plug.
[0021] It can be seen from the above technical solution that the present invention has at least one of the following advantages and positive effects:
[0022] In the manufacturing method of the semiconductor device provided by the present invention, a carbon source gas is dissociated to generate a plasma carbon source, and the plasma carbon source is controlled to be deposited on the top of the bit line structure to form a carbon protective layer. When etching is performed, the carbon protective layer will be etched for the bit line structure, and the top of the bit line structure will not be directly etched. After the etching is completed, the bit line structure is not damaged and the size will not deviate, thereby ensuring the dimensional accuracy of the semiconductor device and improving the yield of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The above and other features and advantages of the present invention will become more apparent by describing in detail exemplary embodiments thereof with reference to the attached drawings.
[0024] Figure 1 is a flow chart of a method for manufacturing a semiconductor device in an exemplary embodiment of the present invention;
[0025] Figures 2 to 3 A schematic diagram of forming a bit line structure of a semiconductor device in an exemplary embodiment of the present invention;
[0026] Figure 4 A top view of a sacrificial layer formed in a semiconductor device in an exemplary embodiment of the present invention;
[0027] Figure 5 for Figure 4 Schematic diagram of the cross section along AA;
[0028] Figure 6 A top view of a spacer layer formed in a semiconductor device in an exemplary embodiment of the present invention;
[0029] Figure 7 for Figure 6 Schematic diagram of the cross section along BB;
[0030] Figure 8 A schematic diagram of a semiconductor device for dissociating and generating a plasma carbon source in an exemplary embodiment of the present invention;
[0031] Fig. 9 A schematic diagram of a semiconductor device in which a plasma carbon source is deposited onto a bit line structure in an exemplary embodiment of the present invention;
[0032] Fig.10 is a schematic diagram of a semiconductor device in which a carbon protective layer is formed in an exemplary embodiment of the present invention;
[0033] Fig.11 A schematic diagram of etching a sacrificial layer and removing a carbon protective layer in an exemplary embodiment of the present invention;
[0034] Fig.12 A top view of a semiconductor device after forming a storage node contact hole and removing a carbon layer in an exemplary embodiment of the present invention;
[0035] Fig.13 for Fig.12 Schematic diagram of the cross section along CC line;
[0036] Fig.14 A top view of a semiconductor device for forming a storage node contact plug in an exemplary embodiment of the present invention;
[0037] Fig.15 for Fig.14 Schematic diagram of the cross section along DD.
[0038] Description of reference numerals:
[0039] 1. Substrate; 2. Shallow trench isolation; 3. Insulating layer; 4. Bit line structure; 41. Bit line spindle structure; 411. Bit line contact plug; 412. Bit line; 413. Insulating cap layer; 42. Spacer layer; 421. First spacer layer; 422. Second spacer layer; 5. Sacrificial layer; 51. Initial sacrificial layer; 6. Spacer layer; 7. Carbon protective layer; 8. Storage node contact plug; H1. Storage node contact hole; H2. Bit line node plug hole; G. Carbon source gas; C. Plasma carbon source; F1. First direction; F2. Second direction. DETAILED DESCRIPTION
[0040] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided so that the present invention will be comprehensive and complete and fully convey the concepts of the example embodiments to those skilled in the art. The same reference numerals in the figures represent the same or similar structures, and thus their detailed description will be omitted.
[0041] In the following description of different exemplary embodiments of the present disclosure, reference is made to the accompanying drawings, which form a part of the present disclosure and in which different exemplary structures that can implement multiple aspects of the present disclosure are shown by way of example. It should be understood that other specific schemes of components, structures, exemplary devices, systems and steps can be used, and structural and functional modifications can be made without departing from the scope of the present disclosure. Moreover, although the terms "above", "between", "within", etc. may be used in this specification to describe different exemplary features and elements of the present disclosure, these terms are used herein only for convenience, such as according to the direction of the examples in the accompanying drawings. Nothing in this specification should be construed as requiring a specific three-dimensional direction of the structure to fall within the scope of the present disclosure. In addition, the terms "first", "second", etc. in the claims are used only as marks and are not numerical limitations on their objects.
[0042] The flowcharts shown in the accompanying drawings are only exemplary and do not necessarily include all the contents and operations / steps, nor must they be executed in the order described. For example, some operations / steps can be decomposed, and some operations / steps can be combined or partially combined, so the actual execution order may change according to actual conditions.
[0043] In addition, in the description of the present invention, “plurality” means at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0044] Please refer to Figures 1 to 15 ,in, Figure 1 A flowchart showing a method for manufacturing a semiconductor device according to an embodiment of the present invention is shown. Figures 2 to 15 Schematic diagram showing a semiconductor device in different manufacturing stages according to an embodiment of the present invention. Figures 1 to 15 As shown, the method for manufacturing a semiconductor device of the present invention comprises:
[0045] Step S200: forming a plurality of spaced-apart bit line structures 4 on a substrate 1 of a semiconductor device, wherein the plurality of bit line structures extend along a first direction F1.
[0046] Step S400: forming a sacrificial layer 5 between a plurality of bit line structures.
[0047] Step S600: placing a semiconductor device in a reaction chamber of an etching device.
[0048] Step S800: releasing a carbon source gas G into a reaction chamber and providing an alternating electric field to dissociate the carbon source gas G into a plasma carbon source C.
[0049] Step S1000 : controlling the plasma carbon source C to be deposited onto the top surface of the bit line structure to form a carbon protection layer 7 .
[0050] Step S1200: etching the sacrificial layer 5 and a portion of the substrate to form a storage node contact hole.
[0051] Step S1400: removing the carbon protective layer 7.
[0052] In the manufacturing method of the semiconductor device provided by the present invention, a carbon source gas is dissociated to generate a plasma carbon source C, and the plasma carbon source C is controlled to be deposited on the top of the bit line structure 4 to form a carbon protection layer 7. When etching is performed, the carbon protection layer 7 will be etched for the bit line structure 4, and the top of the bit line structure 4 will not be directly etched. After the etching is completed, the bit line structure 4 is not damaged and the size will not deviate, thereby ensuring the dimensional accuracy of the semiconductor device and improving the yield of the semiconductor device.
[0053] The following is a detailed description of the method for manufacturing the semiconductor device of the present invention.
[0054] Step S200: forming a plurality of spaced bit line structures on a substrate of a semiconductor device, wherein the plurality of bit line structures extend along a first direction F1.
[0055] The semiconductor device may be a wafer, which is not particularly limited here. Figure 2 and Figure 3 , which shows a schematic diagram of the structure of a semiconductor device. The semiconductor device includes a semiconductor substrate 1, on which a shallow trench isolation 2 is formed, and an active region is provided between the shallow trench isolations 2. The semiconductor substrate 1 is also provided with a word line structure (not shown in the figure) and a bit line structure 4, which are arranged at different heights of the substrate 1, and the word line structure and the bit line structure 4 are both connected to the active region. The word line structure may include a high dielectric constant dielectric layer, a polysilicon layer, a work function layer, and a word line metal layer.
[0056] In one embodiment, the material of the substrate 1 of the semiconductor device of the embodiment of the present invention can be silicon, silicon carbide, silicon nitride, silicon on insulator, stacked silicon on insulator, stacked silicon germanium on insulator, silicon germanium on insulator or germanium on insulator, etc.
[0057] like Figures 1 to 3 As shown, step S200: forming a plurality of spaced bit line structures on a substrate of a semiconductor device, wherein the plurality of bit line structures extend along a first direction F1, may specifically include:
[0058] Step S201 : forming a plurality of bit line node plug holes H2 on a substrate 1 .
[0059] Specifically, Figure 2As shown, an insulating layer 3 is first formed on the semiconductor substrate 1, and is patterned using a mask pattern as an etching mask to form a plurality of openings. Then, the substrate 1 in the openings is etched through an etching process to form a plurality of bit line node plug holes H2. The bit line node plug holes H2 are at least partially located in the active area of the substrate 1. The bit line node plug holes H2 are used to form bit line contact plugs 411 and bit lines 412, so that the bit lines 412 are connected to the active area.
[0060] Step S202: forming a bit line contact plug 411 in each bit line node plug hole H2.
[0061] Specifically, a bit line contact plug 411 may be formed in each bit line node plug hole H2 by a deposition method. In some embodiments, an atomic layer deposition process or a chemical vapor deposition process may be used to deposit and form the bit line contact plug 411. The bit line contact plug 411 may be metal silicide, polysilicon, metal nitride or metal, which is not particularly limited here.
[0062] Step S203 : forming a bit line 412 on the top of each bit line contact plug 411 .
[0063] Specifically, Figure 2 As shown, a bit line 412 can be formed on each bit line contact plug 411 by a deposition method. In some embodiments, the bit line 412 can be formed by deposition using an atomic layer deposition process or a chemical vapor deposition process. The bit line 412 can be a metal. The bit line contact plug 411 and the bit line 412 can also be made of the same material, and the two are formed by the same deposition step, which is not particularly limited here.
[0064] Step S204 : forming an insulating capping layer 413 on the top of each bit line 412 , so that the bit line contact plug 411 , the bit line 412 and the insulating capping layer 413 form a bit line mandrel structure 41 .
[0065] Specifically, an insulating capping layer 413 may be formed on each bit line 412 by a deposition method. In some embodiments, the insulating capping layer 413 may be formed by deposition using an atomic layer deposition process or a chemical vapor deposition process. The insulating capping layer 413 may be silicon nitride or silicon oxynitride, which is not particularly limited herein. The insulating capping layer 413 insulates the top of the bit line 412 and plays a protective role.
[0066] Step S205 : forming a spacer layer 42 on the top and sidewalls of the bit line mandrel structure 41 .
[0067] Specifically, Figure 3As shown, an insulating spacer layer 42 can be conformally formed on the top and sidewalls of the bit line mandrel structure 41 by a deposition method to form a bit line structure 4. In some embodiments, the spacer layer 42 can be deposited by an atomic layer deposition process or a chemical vapor deposition process. Of course, in the actual operation process, the spacer layer 42 will also be deposited on the substrate 1 between the bit line structures 4 (not shown in the figure), and it will be removed by an etching process. The spacer layer 42 can be silicon nitride, silicon oxide, or silicon oxynitride.
[0068] Further references Figure 3 , the spacer layer 42 may include a first spacer layer 421 and a second spacer layer 422. The first spacer layer 421 is conformally deposited on the top and sidewall of the bit line mandrel structure 41 through the above-mentioned deposition process, and then the second spacer layer 422 is conformally formed on the first spacer layer 421. Among them, the first spacer layer 421 may be silicon dioxide (SiO2), and the second spacer layer may be silicon nitride (Si3N4). Of course, the spacer layer 42 may also have three layers, four layers or more layers. By setting the spacer layer 42 as multiple layers, the spacer layer 42 formed during the deposition process is more uniform and has a more precise size. At the same time, if a single spacer layer 42 is set, when the thickness of the spacer layer 42 is relatively thick and the deposition is uneven, stress is easily generated inside the spacer layer 42, thereby affecting the stability of the performance of the semiconductor device. Setting multiple spacer layers 42 can avoid stress and improve the stability of the semiconductor device. Of course, if a thinner spacer layer 42 is formed, a single spacer layer 42 may also be set. Regarding the number of spacer layers 42 , those skilled in the art can set it according to actual conditions, and no special limitation is made here.
[0069] By providing an insulating cap layer 413 and a spacer layer 42 on the top and sidewalls of the bit line 412 , the bit line 412 is protected, parasitic capacitance is reduced, and leakage is prevented.
[0070] Step S400: forming a sacrificial layer 5 between a plurality of bit line structures. Specifically comprising:
[0071] Step S401: Filling an initial sacrificial layer 51 between a plurality of bit line structures, such as Figure 4 and Figure 5 shown.
[0072] Step S402: forming photoresist patterns (not shown) arranged at intervals on the initial sacrificial layer 51, each photoresist pattern extending along the second direction F2.
[0073] The second direction F2 intersects with the first direction F1 , that is, the second direction F2 may have an angle with the first direction F1 , and the angle may be 90° or an acute angle, which is not particularly limited here.
[0074] Step S403: using the photoresist pattern as a mask, etching a portion of the initial sacrificial layer 51 to form a blind hole, until the bottom of the blind hole exposes the substrate.
[0075] Step S404: forming a spacer layer 6 and filling the blind hole, such as Figure 6 and Figure 7 shown.
[0076] Specifically, the blind hole is filled with a spacer layer 6 by a deposition method. The spacer layer 6 may be made of silicon nitride or silicon oxynitride. In one embodiment, the spacer layer 6 may be higher than the bit line structure, that is, the spacer layer 6 may be deposited on the top of the bit line structure in addition to being filled in the blind hole, so as to avoid damaging the top surface of the bit line structure in subsequent processes, and the spacer layer 6 on the top may be removed together with the sacrificial layer 5.
[0077] Step S405 : removing the photoresist pattern, and the remaining initial sacrificial layer 51 is the sacrificial layer 5 .
[0078] The initial sacrificial layer 51 is made of the same material as the sacrificial layer 5 , which may be silicon nitride, silicon oxide or silicon oxynitride, which is not particularly limited here.
[0079] Step S600: placing a semiconductor device in a reaction chamber of an etching device.
[0080] Specifically, the semiconductor device formed with the bit line structure 4 and the sacrificial layer 5 is placed in a reaction chamber of an etching device. The etching device is provided with a reaction chamber inside, which can accommodate the semiconductor device and process the semiconductor device. The etching device is a dry etching device, for example, the device can be a plasma etching device.
[0081] Step S800: releasing carbon source gas G into the reaction chamber and providing an alternating electric field to dissociate the carbon source gas G into a plasma carbon source C, such as Figure 8 shown.
[0082] The carbon source gas G may be at least one of CH4, C2H6 and C4H8. Figure 8 As shown, the carbon source gas G can be dissociated in an alternating electric field to generate a carbon-containing plasma. In one embodiment, the carbon source gas G is CH4, and its chain reaction is as follows:
[0083] CH4→CH 3● +H
[0084] CH4→CH 2● +2H
[0085] CH4→CH ● +3H
[0086] CH4→C ● +4H
[0087] During the dissociation process, the dissociation power of the alternating electric field is controlled to be 1000-1500 W, for example, the dissociation power can be 1200 W, 1300 W or 1400 W, and the dissociation frequency is 10-20 MHz, for example, 12 MHz, 15 MHz, 18 MHz, which is not specifically limited here. By controlling the above parameters of the alternating electric field, the carbon source gas G can be plasma-dissociated to form a plasma carbon source C.
[0088] Furthermore, during the dissociation process, the vacuum pressure in the reaction chamber can be controlled to 20-40 mtorr, for example, 25 mtorr, 30 mtorr or 35 mtorr, and the temperature can be controlled to 30°C-40°C. There is no special limitation here. Under the above conditions, CH4 can be rapidly dissociated into plasma carbon source C.
[0089] Step S1000 : controlling the plasma carbon source C to be deposited onto the top surface of the bit line structure 4 to form a carbon protection layer 7 .
[0090] Specifically, Fig. 9 and Fig.10 As shown, after the plasma carbon source C is generated, the plasma carbon source C floats in the reaction chamber. In order to control the plasma carbon source C to be deposited orderly on the top surface of the bit line structure, the longitudinal bias power of the alternating electric field can be controlled to be 0 to 10 W, for example, 2 W, 5 W, or 8 W, and the longitudinal bias frequency is 500 KHz to 5 MHz, for example, 800 KHz, 2 MHz or 4 MHz, and no special limitation is made here.
[0091] Furthermore, the vacuum pressure in the reaction chamber can be controlled to be 5-20 mtorr, for example, 8 mtorr, 10 mtorr, 15 mtorr or 18 mtorr, while maintaining the temperature at 30° C. to 40° C. The above adjustment is beneficial for the plasma carbon source C to be deposited on the top of the bit line structure 4 .
[0092] Furthermore, the thickness of the carbon protective layer 7 can be 2 to 40 nm, specifically, 10 nm, 20 nm or 30 nm. By controlling the thickness of the carbon protective layer 7 within this range, the carbon protective layer 7 can be removed to the greatest extent in the next etching step without damaging the top of the bit line structure 4.
[0093] Step S1200: etching the sacrificial layer 5 and a portion of the substrate to form a storage node contact hole.
[0094] Specifically, Figures 11 to 13 As shown, the semiconductor device is etched using a dry etching process, first the sacrificial layer 5 is etched, and after the substrate is exposed, etching is continued to a certain depth to form a storage node contact hole. It should be noted that Fig.13 for Fig.12 The cross-sectional view along CC is to clearly show that the sacrificial layer 5 is removed and the storage node contact hole H1 is formed. Fig.13 The spacer layer 6 is omitted.
[0095] The dry etching may be plasma etching, and the etching gas used in the plasma process may be chlorine gas. By controlling the amount of the etching gas, the etching degree may be controlled, that is, the storage node contact hole H1 of a desired depth may be formed.
[0096] In the above etching process, by controlling the etching conditions, the carbon protective layer 7 is also etched to remove the carbon protective layer 7, and the bit line structure 4 is not further etched, so that the size of the semiconductor device is more accurate and the top of the bit line structure 4 is exposed. Of course, the etching conditions can also be controlled to remove only part of the carbon protective layer 7 or not remove the carbon protective layer 7 during the process of etching to form the storage node contact hole, and then remove the carbon protective layer 7 through other processes after the etching is completed.
[0097] Furthermore, the carbon protection layer 7 may be removed by a plasma process, an ashing process or a wet etching process.
[0098] Specifically, the parameters in the plasma process, the ashing process or the wet etching process can be controlled to improve the selectivity of carbon, thereby removing the carbon protective layer 7 alone without damaging other parts of the semiconductor device. In some embodiments, the plasma process can be implemented by supplying at least one of H2, N2H2, O2 or CO at a plasma power of 300 to 800 W at a temperature of 200 to 400° C. and a pressure of 3-8 Torr. In some embodiments, the ashing process can be implemented by supplying a gas that produces hydrogen or oxygen radicals at 200 to 400° C. The gas that can produce hydrogen or oxygen radicals can be NH3, H2, N2O, O2 or CO, which is not specifically limited here. In some embodiments, the wet etching process can remove the carbon protective layer 7 using concentrated sulfuric acid plus hydrogen peroxide.
[0099] The above process can completely remove the residual carbon protection layer 7, so that the top of the bit line structure 4 is exposed, thereby ensuring the dimensional accuracy of the semiconductor device and avoiding the introduction of impurities, thereby ensuring the stability of the performance of the semiconductor device.
[0100] Furthermore, the method for manufacturing a semiconductor device of the present invention further includes step S1400: forming a storage node contact plug 8 in the storage node contact hole H1.
[0101] Specifically, Fig.14 and Fig.15As shown, a storage node contact plug 8 can be formed in the storage node contact hole H1 by a deposition method. The storage node contact plug 8 can be a metal silicide, polysilicon, metal nitride or metal, which is not specifically limited here. In addition, since the bit line 412 is covered with a spacer, the electrical insulation between the bit line 412 and the storage node contact plug 8 can be improved to avoid electrical interference or leakage current between the two.
[0102] Furthermore, the method for manufacturing a semiconductor device of the present invention further includes step S1600 : forming a data storage element on the storage node contact plug 8 .
[0103] Specifically, in some embodiments, the data storage element may include a capacitor of a lower electrode, a dielectric and an upper electrode, so that the semiconductor device can be used as a dynamic random access memory (DRAM) device. In some embodiments, the data storage element forms a dielectric layer on the side wall of the lower electrode, and forms an upper electrode layer on the dielectric layer. The dielectric layer is selected as a high-K dielectric to increase the capacitance value of the capacitor per unit area. The material of the dielectric layer may include: ZrO x , HfO x 、ZrTiO x 、RuO x , SbO x 、AlO x The dielectric layer may also include multiple layers stacked with different materials. The material of the upper electrode layer may be the same as that of the lower electrode layer, and may include at least one of metal nitride and metal silicide species, such as titanium nitride, titanium silicide, nickel silicide, etc. The above-mentioned dielectric layer and the upper electrode layer may be formed by atomic layer deposition process or chemical vapor deposition process.
[0104] In summary, in the manufacturing method of the semiconductor device provided by the present invention, the carbon source gas G is dissociated to generate a plasma carbon source C, and the plasma carbon source C is controlled to be deposited on the top of the bit line structure 4 to form a carbon protective layer 7. When etching is performed, the carbon protective layer 7 will be etched for the bit line structure 4, and the top of the bit line structure 4 will not be directly etched. After the etching is completed, the bit line structure 4 is not damaged and the size will not deviate, thereby ensuring the dimensional accuracy of the semiconductor device and improving the yield of the semiconductor device.
[0105] It should be understood that the present invention is not limited in its application to the detailed structure and arrangement of the components proposed in this specification. The present invention can have other embodiments and can be implemented and executed in a variety of ways. The aforementioned variations and modifications fall within the scope of the present invention. It should be understood that the present invention disclosed and defined in this specification extends to all alternative combinations of two or more individual features mentioned or evident in the text and / or the drawings. All these different combinations constitute multiple alternative aspects of the present invention. The embodiments described in this specification illustrate the best mode known for implementing the present invention and will enable those skilled in the art to utilize the present invention.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: include: forming a plurality of spaced-apart bit line structures on a substrate of a semiconductor device, the plurality of bit line structures extending along a first direction; forming a sacrificial layer between the plurality of bit line structures; Placing the semiconductor device in a reaction chamber of an etching device; releasing a carbon source gas into a reaction chamber and providing an alternating electric field to dissociate the carbon source gas to generate a plasma carbon source; Controlling the plasma carbon source to be deposited onto the top surface of the bit line structure to form a carbon protection layer; Etching the sacrificial layer and a portion of the substrate to form a storage node contact hole; removing the carbon protective layer; Wherein, controlling the plasma carbon source to be deposited onto the top surface of the bit line structure comprises: The longitudinal bias power of the alternating electric field is controlled to be 0-10W, and the longitudinal bias frequency is controlled to be 500KHz-5MHz.
2. The method for manufacturing a semiconductor device according to claim 1, wherein: The step of releasing the carbon source gas into the reaction chamber and providing an alternating electric field to dissociate the carbon source gas to generate a plasma carbon source comprises: The dissociation power of the alternating electric field is controlled to be 1000-1500 W, and the dissociation frequency is controlled to be 10-20 MHz.
3. The method for manufacturing a semiconductor device according to claim 2, wherein: The vacuum pressure in the reaction chamber is controlled to be 20-40 mtorr and the temperature is controlled to be 30° C.-40° C.
4. The method for manufacturing a semiconductor device according to claim 1, wherein: The vacuum pressure in the reaction chamber is controlled to be 5-20 mtorr and the temperature is controlled to be 30° C.-40° C.
5. The method for manufacturing a semiconductor device according to claim 1, wherein: The thickness of the carbon protective layer is 2-40 nm.
6. The method for manufacturing a semiconductor device according to claim 1, wherein: The carbon source gas is at least one of CH4, C2H6 and C4H8.
7. The method for manufacturing a semiconductor device according to claim 1, wherein: The sacrificial layer and a portion of the substrate are etched using a dry etching process to form the storage node contact hole.
8. The method for manufacturing a semiconductor device according to claim 1, wherein: The carbon protection layer is removed by using a plasma process, an ashing process or a wet etching process.
9. The method for manufacturing a semiconductor device according to claim 1, wherein: Forming a sacrificial layer between the plurality of bit line structures comprises: filling an initial sacrificial layer between the plurality of bit line structures; forming spaced photoresist patterns on the initial sacrificial layer, each of the photoresist patterns extending along a second direction, the second direction intersecting the first direction; Using the photoresist pattern as a mask, etching a portion of the initial sacrificial layer to form a blind hole, until the bottom of the blind hole exposes the substrate; forming a spacer layer to fill the blind hole; The photoresist pattern is removed, and the remaining initial sacrificial layer is the sacrificial layer.
10. The method for manufacturing a semiconductor device according to claim 9, wherein: The sacrificial layer is silicon nitride, silicon oxide or silicon oxynitride.
11. The method for manufacturing a semiconductor device according to claim 9, wherein: The spacer layer is silicon nitride or silicon nitride oxide.
12. The method for manufacturing a semiconductor device according to claim 1, wherein: Also includes: A storage node contact plug is formed in the storage node contact hole.
13. The method for manufacturing a semiconductor device according to claim 12, wherein: The storage node contact plug is made of metal silicide, polysilicon, metal nitride oxide or metal.
14. The method for manufacturing a semiconductor device according to claim 12, wherein: A data storage element is formed on the storage node contact plug.