A non-destructive separation method for lithium-ion battery electrode diffusion process
Through the voltage increment matching relationship and AC impedance model of virtual three electrodes, the solid phase diffusion time of lithium-ion batteries is separated by the basis transformation method, solving the problem of lossless separation of electrode diffusion kinetics, and achieving high reliability of electrode diffusion polarization online Monitoring, suitable for electric vehicle power batteries.
Patent Information
- Application Number
- CN202210714553.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-23
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-06-23
AI Technical Summary
The existing lithium-ion battery management system is difficult to perform lossless separation of electrode diffusion kinetics, especially in low-temperature environments, and battery aging and capacity decay are difficult to effectively analyze.
The SOC points are selected through the voltage increment matching relationship of the virtual three electrodes, combined with the AC impedance test and diffusion impedance model, and the solid phase diffusion time of the electrode is separated by the basis transformation method to achieve lossless separation of electrode diffusion polarization.
This method achieves high reliability of electrode diffusion polarization and easy to achieve lossless separation online. It is suitable for electric vehicle power batteries, and can accurately analyze the contribution rate of electrode diffusion polarization, improving the battery's performance monitoring and management capabilities.
Smart Images

Figure CN115166553B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of lithium ion battery diagnosis, in particular to a method for lossless separation of lithium ion battery electrode diffusion process. Background Art
[0002] In recent years, the large-scale development of electric vehicles is of great significance to achieving the goal of "carbon peak and neutrality". Highly integrated and reliable lithium-ion batteries are the key carriers for energy conservation and consumption reduction. With the continuous aging of the battery and its application in low-temperature environments, the capacity and power performance of the battery show an accelerated linear decline. The root cause is often due to the accelerated loss of the battery's interface and diffusion kinetics polarization. Diffusion kinetics is a concentrated expression of the loss of essential properties such as electrode active material and diffusion coefficient. The increased solid-phase diffusion coefficient of the negative electrode and the severe fracture of the positive electrode material loss are the dominant factors for the increase in battery diffusion impedance under low temperature and deep aging, respectively. However, how to non-destructively separate the diffusion kinetics of the electrode at the battery level to achieve quantitative analysis of the contribution rate of electrode diffusion polarization loss is a very important technical issue.
[0003] Most of the existing battery management systems are separation methods for the thermodynamic properties of lithium-ion battery electrodes, while the lossless separation methods for electrode kinetics are still immature, especially the lossless separation technology for electrode diffusion kinetics is relatively scarce. Summary of the invention
[0004] In view of the defects existing in the prior art, the purpose of the present invention is to provide a method for lossless separation of lithium-ion battery electrode diffusion process, which has simple steps, is easy to implement online, and has high reliability, and is suitable for lossless separation of electrode diffusion polarization of electric vehicle power batteries.
[0005] In order to achieve the above purpose, the technical solution adopted by the present invention is:
[0006] A method for lossless separation of lithium ion battery electrode diffusion process, comprising the following steps:
[0007] S1: Select the separable SOC point based on the voltage increment matching relationship between the lithium-ion battery electrode and the full battery;
[0008] S2: Identify the solid phase diffusion time of the battery based on AC impedance test and diffusion impedance model;
[0009] S3: The basis transformation method is used to separate the solid-phase diffusion time of the electrode at the separable SOC point, and the voltage increment of the electrode is combined to achieve lossless separation of the electrode diffusion polarization.
[0010] Furthermore, the step S1 comprises the following steps:
[0011] S11: Assemble the positive and negative half-cells with the pole pieces of the sample battery, perform constant current charge and discharge tests on the half-cells and the sample battery at a charge rate of 0.05-0.2C, and record the current and voltage data of the experimental process;
[0012] S12: Calculate the equilibrium potential of the virtual three electrodes according to the current and voltage data in step S11, thereby constructing the equilibrium potential OCV of the virtual three electrodes i And the voltage increment DV i The matching relationship between them is used to obtain the initial lithium insertion position SOC of the electrode. init,i and the maximum available capacity Q max,i ;
[0013] S13: According to the matching relationship between the equilibrium potential and the voltage increment of the virtual three electrodes determined in step S12, two SOC points are selected, wherein the SOC values of the selected SOC points are less than 40%, the negative electrode voltage increment DV values of the selected SOC points are not equal, and the adjacent SOC intervals of the selected SOC points are not greater than 10%;
[0014] Furthermore, the step S2 comprises the following steps:
[0015] S21: Performing an AC impedance EIS test on the sample battery at the two SOC points selected in step S2 with an amplitude of no more than 10 mV and a frequency range of 10 kHz to 10 mHz;
[0016] S22: Fitting the equivalent impedance model of the EIS test in step S21 to identify the solid phase diffusion internal resistance of the battery, and fc and the maximum available capacity Q max,fc To calculate the solid phase diffusion time of the battery.
[0017] Furthermore, step S3 includes the following steps:
[0018] S31: At any SOC point, the solid-phase diffusion resistance of the battery is the linear superposition of the solid-phase diffusion resistance of the electrodes. The solid-phase diffusion resistance at each electrode is the product of the voltage increment and the solid-phase diffusion time. Based on this, the incremental voltage of the electrode and the whole battery is used as the linear space V 2 and V 1 The solid phase diffusion time of the electrode is taken as the coordinate under the linear space basis vector, and the solid phase diffusion time of the electrode is calculated at adjacent SOC points;
[0019] S32: Calculate the electrode solid phase diffusion internal resistance based on the electrode incremental voltage and the electrode solid phase diffusion time separated in step S31.
[0020] Furthermore, the equivalent impedance model in step S22 is: using resistors and inductors in parallel to simulate high-frequency impedance; using resistors and constant phase elements in parallel to simulate the impedance of charge transfer in the mid-frequency band; using the solid-phase diffusion impedance expression of spherical particles to simulate the solid-phase diffusion impedance, and using resistors and capacitors in parallel to simulate the liquid-phase diffusion impedance.
[0021] The non-destructive separation method of the lithium-ion battery electrode diffusion process described in the present invention uses the matching relationship of the incremental voltage of the virtual three electrodes to determine the feasible SOC point, obtains AC impedance data at the feasible SOC point, and identifies the solid phase diffusion time of the battery through impedance test data and diffusion impedance model; according to the basis transformation theory, the voltage increment of two SOC points and the solid phase diffusion time of the battery are used to achieve non-destructive separation of electrode diffusion time and internal resistance. The method has simple steps, is easy to implement online, and has high reliability. It is suitable for non-destructive separation of electrode diffusion polarization of electric vehicle power batteries. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The present invention has the following accompanying drawings:
[0023] Figure 1 A relationship diagram between the equilibrium potential and the voltage increment of the virtual three electrodes of the present invention;
[0024] Figure 2 Flow chart of the electrode diffusion polarization lossless separation method of the present invention;
[0025] Figure 3 Schematic diagram of basis transformation theory of the present invention;
[0026] Figure 4 Result diagram of lossless separation of electrode solid-phase diffusion internal resistance of the present invention. DETAILED DESCRIPTION
[0027] The present invention is further described in detail below in conjunction with the accompanying drawings.
[0028] In the embodiment, a soft-pack lithium-ion power battery of the NMC111 system is taken as an example, and its rated voltage is 3.65V and the nominal capacity is 8.5Ah. The experimental equipment used is: Biologic electrochemical workstation with Tianjin Tester SPX-150BX temperature control box. This embodiment does not limit the present invention.
[0029] The electrode diffusion polarization lossless separation method of the present invention is as follows Figure 2 As shown, the specific steps include:
[0030] The first step is to assemble button-type positive and negative half-cells with the pole pieces of the sample battery, and perform 0.05-0.2C constant current charge and discharge tests on the half-cells and sample batteries, and record the current data of the experimental process I=[I 1 ,I 2 ,…,IN ] T , voltage data U=[U 1 ,U 2 ,…,U N ] T , where N is the number of data samples.
[0031] The second step is to calculate the equilibrium potential of the virtual three electrodes according to the charge and discharge data in step one, thereby constructing a matching relationship between the equilibrium potential and the voltage increment of the virtual three electrodes, and obtaining the initial lithium insertion position SOC of the electrode. init,i and the maximum available capacity Q i :
[0032]
[0033] The voltage increment of the virtual three electrodes is shown as follows:
[0034] DV fc (SOC) = DV ca (SOC)-DV an (SOC) (2)
[0035] Where OCV i ,DV i ,SOC i They respectively represent the equilibrium potential, voltage increment and state of charge of the virtual three electrodes; simu and mear respectively represent the simulation and test results, RMSE represents the root mean square error; init represents initial, ca represents cathode, an represents anode, and fc represents battery.
[0036] The third step is based on Figure 1 The voltage increment DV matching relationship shown in the figure selects two SOC points below 40%, and the selected SOC points must meet the following two conditions:
[0037] First, to ensure the non-singularity of the transition matrix in the basis transformation, the voltage increment DV values of the virtual three electrodes at adjacent SOCs should be unequal; second, to ensure that the electrode solid phase diffusion time has a small difference, the interval of adjacent SOCs should not be greater than 10%.
[0038] The fourth step is to fit the EIS test of the sample battery and the equivalent impedance model at two selected adjacent SOC points to identify the solid phase diffusion internal resistance parameters. The high-frequency inductive reactance and the medium-frequency interface impedance are fitted using the equivalent impedance models of R / / L and R / / Q, respectively. The low-frequency diffusion impedance consists of two parts: solid phase and liquid phase diffusion impedance. The specific impedance expression is:
[0039]
[0040] Where τs represents the solid phase diffusion time, α s represents fractional order, R d Represents the internal resistance of ion diffusion, R e represents the liquid phase diffusion resistance, τ e represents the liquid phase diffusion time.
[0041] In order to further derive the relationship between the solid-phase diffusion internal resistance of the electrode and the full battery, the specific expression of the reduced-order solid-phase diffusion internal resistance is:
[0042]
[0043] Where R s,i represents the solid phase diffusion internal resistance, ω represents the angular frequency, represents the constant coefficient.
[0044] The fifth step is to establish the solid-phase diffusion internal resistance relationship between the electrode and the full battery. The specific expression is:
[0045]
[0046] Since the fractional order is generally between 0.3 and 0.8, in order to eliminate the influence of the fractional order on the diffusion impedance, the order is fixed to 0.5 without losing accuracy. In addition, the fractional order also directly affects the solid phase diffusion time, but this is not the true relaxation time. is the concentrated solid-phase diffusion relaxation time.
[0047] At any SOC point, the solid phase diffusion internal resistance of the battery is the linear superposition of the solid phase diffusion internal resistance of the electrode. The solid phase diffusion internal resistance at each electrode is the product of the voltage increment and the solid phase diffusion time, that is:
[0048]
[0049] Where DV i,j and are the voltage increment and solid diffusion time constant, i and j are a certain electrode and SOC point respectively.
[0050] Step 6: Figure 3 As shown, the electrode increment voltage is the linear space V 2 The basis vectors and the voltage increment DV of the full battery is linear space V 1 The basis vectors Under a certain SOC, build and The coordinates of the basis vectors satisfy the following relationship:
[0051]
[0052] According to the small difference of electrode solid phase diffusion time under small SOC changes, the relationship between the solid phase diffusion internal resistance of the electrode and the battery is constructed at two adjacent SOC points, as shown in the matrix operation of the following formula:
[0053]
[0054] In the formula It should be a non-singular matrix, and formula (8) is valid. In the third step, two standards are used to select the SOC point, which is a key condition for constructing a non-singular coefficient matrix. The comparison results of the positive and negative electrode solid phase diffusion time separated by the technology described in the invention content and the true value are listed in Table 1. The true value involved in the present invention is the result identified by the EIS test of the three-electrode battery made in the laboratory, and the effectiveness of the invention technology is verified at 25°C, 10°C and 0°C.
[0055] Table 1 Solid phase diffusion time results based on base transformation and three-electrode experimental separation
[0056]
[0057] Step 7: Calculate the solid phase diffusion internal resistance of the electrode according to the electrode voltage increment matched in step 2, the electrode solid phase diffusion time separated in step 6 and formula (5), as follows: Figure 4 As shown; according to the process described in the content of the invention, the electrode solid-phase diffusion polarization parameters are basically consistent with the true values obtained by the three electrodes, indicating that the content involved in the present invention is very effective in reconstructing the temperature dependence of diffusion impedance.
[0058] The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.
Claims
1. A method for lossless separation of lithium ion battery electrode diffusion process, characterized in that: The steps include: S1: Select a separable SOC point based on the voltage increment matching relationship between the lithium-ion battery electrode and the full battery; S2: Establish a diffusion impedance model based on AC impedance test to identify the solid phase diffusion time of the battery; S3: The solid phase diffusion time of the separation electrode is separated at the separable SOC point by using the basis transformation method, and the voltage increment of the electrode is combined to achieve lossless separation of the electrode diffusion polarization; The step S1 comprises the following steps: S11: Assemble the positive and negative electrode half-cells with the pole pieces of the sample battery, perform constant current charge and discharge tests on the half-cells and the sample battery at a charge rate of 0.05-0.2C, and record the current and voltage data of the experimental process; S12: Calculate the equilibrium potential of the virtual three electrodes according to the current and voltage data in step S11, thereby constructing the equilibrium potential OCV of the virtual three electrodes i And the voltage increment DV i The matching relationship between them is used to obtain the initial lithium insertion position SOC of the electrode. init,i and the maximum available capacity Q max,i ; S13: According to the matching relationship between the equilibrium potential and the voltage increment of the virtual three electrodes determined in step S12, two SOC points are selected, wherein the SOC values of the selected SOC points are less than 40%, the negative electrode voltage increment DV values of the selected SOC points are not equal, and the adjacent SOC intervals of the selected SOC points are not greater than 10%; The step S2 comprises the following steps: S21: Performing an AC impedance EIS test on the sample battery at the two SOC points selected in step S2 with an amplitude of no more than 10 mV and a frequency range of 10 kHz to 10 mHz; S22: Fitting the equivalent impedance model of the EIS test in step S21 to identify the solid phase diffusion internal resistance of the battery, and fc and the maximum available capacity Q max,fc To calculate the solid phase diffusion time of the battery; The step S3 comprises the following steps: S31: At any SOC point, the solid-phase diffusion internal resistance of the battery is the linear superposition of the solid-phase diffusion internal resistance of the electrode, and the solid-phase diffusion internal resistance at each electrode is the product of the voltage increment and the solid-phase diffusion time; accordingly, the incremental voltage of the electrode and the full battery is used as the basis vector of the linear space V2 and V1, and the solid-phase diffusion time of the electrode is used as the coordinate under the basis vector of the linear space, and the solid-phase diffusion time of the electrode is calculated at adjacent SOC points; S32: Calculating the electrode solid phase diffusion internal resistance according to the electrode incremental voltage and the electrode solid phase diffusion time separated in step S31; The equivalent impedance model in step S22 is: using resistors and inductors in parallel to simulate high-frequency impedance; using resistors and constant phase elements in parallel to simulate the impedance of charge transfer in the mid-frequency band; using the solid-phase diffusion impedance expression of spherical particles to simulate solid-phase diffusion impedance, and using resistors and capacitors in parallel to simulate liquid-phase diffusion impedance.