A reverse pull-out shotcrete bonding strength testing device and method

Through the reverse pull-out test device and the threaded connection of the rod hanging ring and the locking nut, the direct measurement of the bond strength of the shotcrete throughout the entire age is achieved, which solves the problem of the inability to test the bond strength in the plastic stage in the existing technology. problems, improving the test success rate and the reusability of the device.

CN115235987BActive Publication Date: 2024-10-01BEIJING JIAOTONG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210794258.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-07
Publication Date
2024-10-01
Estimated Expiration
2042-07-07

AI Technical Summary

Technical Problem

The existing shotcrete bond strength testing method is mainly suitable for hardened concrete and cannot test the bond strength of concrete in the early plastic stage, and may damage the bonding surface and reduce the test success rate.

Method used

A reverse pull-out shotcrete bond strength test device is used, including a hanging ring with a rod, a locking nut, a stopper and a bond strength pull-out instrument. The reverse pull is achieved by reserving holes in the rock slab and using threaded connections. Pull out to avoid damage to the bonding surface and directly measure the bonding strength.

Benefits of technology

It has achieved an effective test of the bond strength of shotcrete throughout its life, is suitable for rock slabs of different thicknesses, has a high test success rate, is easy to install and disassemble, and the device can be used repeatedly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115235987B_ABST
    Figure CN115235987B_ABST
Patent Text Reader

Abstract

The present application discloses a reverse pull-out shotcrete bonding strength test device and method, and relates to the technical field of concrete bonding strength test. It can realize effective testing of the bonding strength of shotcrete at all ages in the laboratory, and can meet the test requirements of rock slabs of different thicknesses. It also has the advantages of high test success rate, convenient installation and disassembly, and can be reused repeatedly. The testing device includes a rod hanging ring, a locking nut, a blocking member and a bonding strength puller; the annular portion of the rod hanging ring is connected to the bonding strength puller, the screw portion is connected to the locking nut, and its end face is provided with an internal threaded hole; the blocking member includes a blocking piece and a connecting screw; the connecting screw is fastened in the internal threaded hole; the blocking piece is located at the bonding surface between the shotcrete to be tested and the rock slab; the screw portion passes through the reserved hole on the rock slab and is connected to the connecting screw; the rock slab is clamped between the blocking piece and the locking nut of the blocking member. The present application also discloses a reverse pull-out shotcrete bonding strength test method.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of concrete bond strength testing, and in particular to a reverse pull-out type shotcrete bond strength testing device and method. Background Art

[0002] At present, the main test method for the bond strength of shotcrete is the forward pull-out method (direct pulling of concrete), which generally includes core pulling, reserved hole specimen pulling and shotcrete large plate splitting pulling method.

[0003] Among them, the core pulling method uses a small drill with a diamond drill bit to drill perpendicular to the shotcrete layer and penetrate more than 20mm into the rock slab to form a cylindrical core sample with a bonding surface between the shotcrete and the rock slab. Then, the concrete core sample is clamped and clamped with a ferrule and a puller is installed. Then, a pulling force is slowly applied to the ferrule until the core sample is destroyed along the bonding surface between the shotcrete and the rock slab. The disadvantage of this method is that it is only applicable to hardened concrete and cannot be used for concrete in the early plastic stage. In addition, the core drilling may cause damage to the bonding surface, reducing the success rate of the test.

[0004] The reserved hole specimen pulling method is to pre-embed a steel tie rod in the center of the specimen with a diameter of 200-500mm and a height of about 100mm, and bond it with epoxy resin mortar. Its pull-out resistance must be greater than the bonding force between the shotcrete and the rock slab. After the concrete at the specimen site is sprayed, a 50mm wide groove is immediately dug along the specimen contour with a spatula to completely separate the specimen from the surrounding shotcrete, with only the bottom surface bonded to the rock slab. After the shotcrete reaches the design age, a puller is used to apply tension to the tie rod to cause the specimen to fail along its bonding surface with the rock slab. The disadvantage of this method is that since its failure mode is a mixture of bonding failure and tensile failure, it can only indirectly measure the bonding strength between the shotcrete and the rock, and cannot directly measure the bonding strength value.

[0005] The large-plate splitting method is to place a rock plate with a thickness of more than 50 mm selected from the construction site in a wooden formwork of an open large-plate spraying of 450mm×350mm×120mm, wet the surface of the rock plate with water, spray concrete into the large-plate formwork according to the actual spraying conditions, and cure for 7 days under the same conditions as the actual structure. Use the cutting method to process a cubic specimen with a side length of 100mm (where the thickness of the rock and concrete is about 50mm each), and cure to the design age. At the bonding surface of the concrete and the rock plate, the splitting method is used to measure the bonding strength between the concrete and the rock block. The disadvantages of this method are: it is difficult to ensure that the interface between the concrete and the rock is on a vertical plane, the specimen is difficult to accurately process, and it cannot meet the test requirements. At the same time, it is only applicable to hardened concrete. Summary of the invention

[0006] The embodiments of the present application provide a reverse pull-out shotcrete bonding strength testing device and method, which can realize effective testing of the bonding strength of shotcrete at all ages in laboratory tests, and can meet the testing requirements of rock slabs of different thicknesses. It also has the advantages of high test success rate, easy installation and disassembly, and repeated use.

[0007] To achieve the above-mentioned purpose, on the one hand, an embodiment of the present application provides a reverse pull-out type shotcrete bonding strength testing device, comprising a rod hanging ring, a locking nut, a blocking member and a bonding strength puller; the rod hanging ring comprises a circular ring portion and a screw portion; the circular ring portion is connected to the bonding strength puller; the screw portion comprises a threaded section and a bare rod section; the threaded section is arranged close to the circular ring portion and is connected to the locking nut; an internal threaded hole is arranged in the bare rod section; the blocking member comprises a fixed blocking piece and a connecting screw; the connecting screw can be fastened in the internal threaded hole of the bare rod section; the blocking member of the blocking member is located at the bonding surface between the shotcrete to be tested and the rock slab; the circular ring portion of the rod hanging ring is located on the side of the rock slab away from the shotcrete to be tested; the screw portion of the rod hanging ring is connected to the connecting screw of the blocking member after passing through the reserved hole on the rock slab; the rock slab is clamped between the blocking member and the locking nut.

[0008] Furthermore, the rod hanging ring and the blocking member are both made of high-speed steel.

[0009] Furthermore, the blocking piece and the connecting screw are connected by a welding process.

[0010] Furthermore, a gasket is sleeved on the screw portion with the rod hanging ring; the rock plate is clamped between the blocking piece of the blocking member and the gasket.

[0011] Furthermore, the baffle is a rectangular plate; the length×width of the baffle=25mm×10mm; the diameter of the connecting screw is 3mm; and the diameter of the screw portion is 5mm.

[0012] Furthermore, the inner diameter of the annular portion is 25 mm.

[0013] On the other hand, an embodiment of the present application further provides a measurement method based on the above-mentioned reverse pull-out shotcrete bonding strength testing device, comprising the following steps:

[0014] Process a reserved hole on the rock slab; put the locking nut on the screw part of the rod hanging ring; pass the screw part of the rod hanging ring through the reserved hole on the rock slab and connect it with the connecting screw of the blocking member; pull the rod hanging ring in the opposite direction of the insertion direction of the rod hanging ring until the blocking piece of the blocking member is close to the rock slab; adjust the locking nut and tighten it so that the rock slab is clamped between the blocking piece of the blocking member and the locking nut; spray or pour concrete on the side of the rock slab close to the blocking piece to complete the preparation of the sprayed concrete bond strength test block; connect the bond strength puller to the circular ring part of the rod hanging ring, and pull until the bond strength test is completed.

[0015] Compared with the prior art, this application has the following beneficial effects:

[0016] 1. The embodiment of the present application is different from the traditional method of pulling the concrete to be tested to measure the bonding strength. The bonding strength between the concrete to be tested and the rock slab is measured by pulling the rock slab in the reverse direction, which solves the problem that the bonding strength of shotcrete cannot be tested in the plastic stage.

[0017] 2. The rod hanging ring in the reverse pull-out shotcrete bonding strength testing device of the embodiment of the present application is connected to the locking nut and the blocking member by threads. By simply tightening (loosening) the nut, one person can easily install and disassemble the device, which is very convenient and can save labor costs.

[0018] 3. In the embodiment of the present application, the rod hanging ring is fastened to the blocking member before spraying or pouring concrete, thereby avoiding damage to the bonding interface.

[0019] 4. The embodiment of the present application can directly measure the bonding strength value, and the test piece is easy to make and has strong operability.

[0020] 5. The embodiments of the present application can be reused to save costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figure 1 This is a schematic diagram of the structure of a reverse pull-out shotcrete bonding strength testing device according to an embodiment of the present application;

[0023] Figure 2 for Figure 1 A partial enlarged view of point Ⅰ in the middle;

[0024] Figure 3This is a schematic diagram of the connection structure of the rod hanging ring, the locking nut and the blocking member in the reverse pull-out shotcrete bonding strength testing device according to the embodiment of the present application;

[0025] Figure 4 This is a front view of a blocking member in a reverse pull-out type shotcrete bonding strength testing device according to an embodiment of the present application;

[0026] Figure 5 A side view of a blocking member in a reverse pull-out shotcrete bonding strength testing device according to an embodiment of the present application;

[0027] Figure 6 A top view of a blocking member in a reverse pull-out shotcrete bonding strength testing device according to an embodiment of the present application;

[0028] Figure 7 This is a diagram of the installation process of the reverse pull-out shotcrete bonding strength testing device according to an embodiment of the present application;

[0029] Figure 8 This is a diagram of the disassembly process of the reverse pull-out shotcrete bonding strength testing device according to an embodiment of the present application. DETAILED DESCRIPTION

[0030] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0031] In the description of the present application, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0032] In the description of the present application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0033] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise specified, "plurality" means two or more.

[0034] The embodiment of the present application combines the hard texture of the rock slab with the processed high-speed steel to invent a reverse pull-out bonding strength test device. This test device is fastened to the rock slab through the reserved holes of the rock slab and can meet the test requirements of rock slabs of different thicknesses. It achieves the goals of strong applicability (applicable to concrete of all ages), high test success rate (reverse pulling will not damage the bonding surface), convenient installation and disassembly of the device, and repeated use of the device.

[0035] Reference Figures 1 to 3 An embodiment of the present application provides a reverse pull-out shotcrete bonding strength testing device, comprising a rod hanging ring 1, a locking nut 2, a gasket 3, a blocking member 4 and a bonding strength pulling instrument 5.

[0036] Among them, refer to Figure 3 , the rod hanging ring 1 includes a circular ring portion 11 and a screw portion 12. The inner diameter of the circular ring portion 11 is 25mm, and the bonding strength puller 5 is connected thereto. That is, the hook of the bonding strength puller 5 is hung on the circular ring portion 11. The bonding strength puller 5 is a prior art, and its structure is not described in detail here. The diameter of the screw portion 12 is 5mm. The screw portion 12 includes a threaded section 121 and a bare rod section 122. The threaded section 121 is arranged close to the circular ring portion 11, and a locking nut 2 and a gasket 3 are sleeved thereon. An internal threaded hole 123 is provided at the end of the bare rod section 122. The depth of the internal threaded hole 123 is 10mm.

[0037] Reference Figures 4 to 6 The blocking member 4 includes a blocking piece 41 and a connecting screw 42. The blocking piece 41 and the connecting screw 42 can be integrally formed or welded together. The blocking piece 41 is a rectangular plate. The length × width of the blocking piece 41 = 25 mm × 10 mm. The diameter of the connecting screw 42 is 3 mm, and its size is compatible with the size of the internal threaded hole 123 of the screw portion 12. Figure 2 , the connecting screw 42 can be fastened in the internal threaded hole 123 of the polished rod segment 122 .

[0038] Reference Figure 1 and Figure 2, the shotcrete 6 to be tested is located on the left side of the rock plate 7. The baffle 41 of the blocking member 4 is located at the bonding surface between the shotcrete 6 to be tested and the rock plate 7, and the annular portion 11 of the rod hanging ring 1 is located on the right side of the rock plate 7. The connecting screw portion 12 of the rod hanging ring 1 passes through the reserved hole 10 on the rock plate 7 and is connected to the connecting screw 42 of the blocking member 4. The gasket 3 is located on the left side of the locking nut 2. After the locking nut 2 is tightened, the rock plate 7 is clamped between the baffle 41 of the blocking member 4 and the gasket 3.

[0039] The rod hanging ring 1 and the blocking member 4 are both made of high-speed steel, so that the rod hanging ring 1 and the blocking member 4 have high hardness, high toughness, high wear resistance and excellent bending strength. Specifically, the rod hanging ring 1 and the blocking member 4 can both be made of W18Cr4V.

[0040] Reference Figure 7 On the other hand, an embodiment of the present application further provides a measurement method based on the above-mentioned reverse pull-out shotcrete bonding strength testing device, comprising the following steps:

[0041] S1. A reserved hole 10 is processed on the rock plate 7. The diameter of the reserved hole 10 is slightly larger than the diameter of the screw rod portion 12, for example, it can be 6 mm.

[0042] S2. Put the locking nut 2 and the gasket 3 on the connecting screw part 12 of the rod hanging ring 1, so that the gasket 3 is located on the left side of the locking nut 2, and then pass the connecting screw part 12 of the rod hanging ring 1 through the reserved hole 10 on the rock plate 7, and screw the connecting screw 42 of the blocking member 4 into the internal threaded hole 123 at the end of the connecting screw part 12.

[0043] S3. Pull the rod hanging ring 1 in the opposite direction (right side) to the insertion direction of the rod hanging ring 1 until the blocking piece 41 of the blocking member 4 is in close contact with the rock plate 7.

[0044] S4. Adjust and tighten the locking nut 2 so that the rock plate 7 is clamped between the blocking piece 41 of the blocking member 4 and the locking nut 2 to ensure that the entire device is free of shaking.

[0045] S5. Spray or pour concrete 6 on the left side of the rock slab 7 to complete the preparation of the sprayed concrete bonding strength test block.

[0046] S6. Connect the bonding strength pulling instrument 5 to the annular portion 11 of the rod hanging ring 1, and perform pulling until the bonding strength test is completed.

[0047] Reference Figure 1 and Figure 2It should be noted that, in order to facilitate the processing of the reserved holes 10 on the rock slab 7, before pouring concrete, you can first take a large rock slab, cut a small rock block 8 of the size required for the test on the rock slab 7, and pre-drill a hole in the center of the cut small rock block 8. Install the rod hanging ring 1 and the blocking piece 4 through the pre-drilled hole and fasten them with the locking nut 2. Then, put the small rock block 8 with the rod hanging ring 1 and the blocking piece 4 installed and fixed back to the original cutting position of the large rock slab 7, and pour concrete 6 on the rock surface on one side of the blocking piece 41 to cover the entire large rock slab (including the small rock block 8). It should be noted that before the small rock block 8 is put back in place, it needs to be covered with 1mm thick high-viscosity foam 9 all around (to prevent concrete from filling the gap and affecting the measurement results). The molding state of the test block is as follows Figure 1 As shown, a bonding strength puller 5 is then connected to the annular portion 1 with a rod hanging ring 1, and the bonding strength of the concrete plasticity and the bonding strength of the entire hardening stage can be conveniently tested by reversely pulling the hanging ring through the bonding strength puller.

[0048] Reference Figure 8 After the test is completed, the disassembly process of the reverse pull-out shotcrete bonding strength testing device of the embodiment of the present application is as follows:

[0049] S7. After the test is completed, the bonding strength puller 5 is removed. At this time, the shotcrete 6 and the rock slab 7 have been separated, but the rod hanging ring 1 and the blocking member 4 are still in the state of clamping the rock slab 7.

[0050] S8. Loosen the locking nut 2 on the rod hanging ring 1 to ensure that the rod hanging ring 1 can be moved forward and backward.

[0051] S9, loosen the blocking member 4 to separate it from the rod hanging ring 1, and then pull out the rod hanging ring 1.

[0052] The above are only specific implementations of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.

Claims

1. A reverse pull-out shotcrete bonding strength test device, It is characterized in that It comprises a rod hanging ring, a locking nut, a blocking member and a bonding strength puller; the rod hanging ring comprises a circular ring portion and a screw portion; the circular ring portion is connected to the bonding strength puller; the screw portion comprises a threaded section and a polished rod section; the threaded section is arranged close to the circular ring portion and is connected to the locking nut; an internal threaded hole is arranged in the polished rod section; the blocking member comprises a fixedly connected blocking piece and a connecting screw; the connecting screw can be fastened in the internal threaded hole of the polished rod section; The blocking piece of the blocking member is located at the bonding surface between the tested shotcrete and the rock slab; the annular portion of the rod hanging ring is located on the side of the rock slab away from the tested shotcrete; the screw portion of the rod hanging ring passes through the reserved hole on the rock slab and is connected to the connecting screw of the blocking member; the rock slab is clamped between the blocking piece of the blocking member and the locking nut; The reverse pull-out shotcrete bonding strength testing device is implemented by the following method: Process reserved holes on the rock plate; Put the locking nut on the screw part with the rod hanging ring; and connect the screw part with the rod hanging ring through the reserved hole on the rock plate and then connect it to the connecting screw of the blocking member; Pull the rod hanging ring in the opposite direction of the insertion direction of the rod hanging ring until the blocking piece of the blocking member is close to the rock plate; Adjust the locking nut and tighten it so that the rock plate is clamped between the blocking piece and the locking nut of the blocking member; Spray or pour concrete on the side of the rock slab close to the baffle to complete the preparation of the sprayed concrete bond strength test block; Connect the bond strength puller to the circular ring with a rod hanging ring and pull until the bond strength test is completed.

2. The reverse pull-out shotcrete bonding strength testing device according to claim 1, It is characterized in that The rod hanging ring and the blocking member are both made of high-speed steel.

3. The reverse pull-out shotcrete bonding strength testing device according to claim 1, It is characterized in that The baffle and the connecting screw are connected by a welding process.

4. The reverse pull-out shotcrete bonding strength testing device according to claim 1, It is characterized in that A gasket is also sleeved on the screw portion with the rod hanging ring; the rock plate is clamped between the blocking piece of the blocking member and the gasket.

5. The reverse pull-out shotcrete bonding strength testing device according to claim 1, It is characterized in that The baffle is a rectangular plate; the length×width of the baffle is 25mm×10mm; the diameter of the connecting screw is 3mm; and the diameter of the screw part is 5mm.

6. The reverse pull-out shotcrete bonding strength testing device according to claim 1, It is characterized in that The inner diameter of the annular portion is 25 mm.