A polyamide film and its manufacturing process
By applying and heating the polyamide solution on aluminum foil and applying heat insulation coating in the polyamide film manufacturing process, the problem of polyamide film becoming soft or melting at high temperatures is solved, and its heat resistance and heat insulation are improved.
Patent Information
- Application Number
- CN202211010073.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-23
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2042-08-23
AI Technical Summary
The existing polyamide films tend to soften or melt under high temperature conditions, losing their preservation effect.
The polyamide solution is prepared by mixing fixed polyamide and water, and then applied on aluminum foil to heat it to solidify, then apply heat insulation coating, separate the solidified polyamide solution through a bevel cutter and peel it off , cutting edges, winding, pickling, washing, washing and drying to produce a polyamide film with higher heat resistance.
It improves the heat resistance and heat insulation of the polyamide film and extends its service life under high temperature conditions.
Smart Images

Figure CN115351962B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of polyamide films, and more particularly to a polyamide film and a manufacturing process thereof. Background Art
[0002] Film is a thin, soft, transparent sheet made of plastic, adhesive, rubber or other materials. The most common film on the market is polyamide film. Polyamide film is made of nylon resin and can be manufactured by T-type film forming method, T-die biaxial stretch film forming method and air blowing expansion method. Resin raw materials with higher viscosity should be used. Commercially available commercial films are mainly nylon and nylon films. Nylon film has the characteristics of high strength, good oxygen barrier and good transparency. Its industrial use is mainly as vacuum bag film for molding, and its civilian use is mainly as food packaging film.
[0003] However, the outer surface of the polyamide film processed by the existing technology does not have the property of being resistant to high temperatures. When using this polyamide film, the polyamide film may soften or melt due to high temperatures. If the polyamide film softens or melts, the preservation effect of the polyamide film will be lost. Summary of the invention
[0004] The purpose of the present invention is to provide a polyamide film and a manufacturing process thereof, wherein the polyamide film with higher heat resistance can be processed by the process.
[0005] The purpose of the present invention is achieved through the following technical solutions:
[0006] A polyamide film manufacturing process, the process comprising the following steps:
[0007] Step 1, adding fixed polyamide and water into a hot melt machine in proportion to prepare a polyamide solution;
[0008] Step 2: Add the polyamide solution into the liquid storage cavity, then pass the aluminum foil through the polyamide solution, and apply the polyamide solution to the lower surface of the aluminum foil;
[0009] Step 3, heating the aluminum foil to solidify the polyamide solution on the lower surface of the aluminum foil, applying the heat-insulating coating to the lower surface of the aluminum foil after solidification, and then separating the solidified polyamide solution from the lower surface of the aluminum foil with an inclined knife;
[0010] Step 4: The polyamide film is manufactured by peeling, trimming, rolling, pickling, washing and drying.
[0011] Preferably, the manufacturing device includes a liquid storage chamber and four limiting rollers rotatably connected to the liquid storage chamber, aluminum foil is transmission-connected between the four limiting rollers, a bevel dividing knife is fixedly connected to the liquid storage chamber, and a smearing component is fixedly connected to the liquid storage chamber.
[0012] Preferably, the smearing component includes a transverse sliding cavity fixedly connected to the liquid storage cavity and a supporting wall plate slidably connected in the transverse sliding cavity, an oblique sliding plate is fixedly connected to the supporting wall plate, an smearing roller is rotatably connected to the upper part of the oblique sliding plate, a transverse moving screw is rotatably connected to the upper part of the liquid storage cavity, and the transverse moving screw is connected to the supporting wall plate by threads.
[0013] Preferably, the manufacturing device further comprises a storage barrel and a contact cone cavity, the storage barrel is fixedly connected to the supporting wall plate, the contact cone cavity is fixedly connected to the storage barrel, and the coating roller contacts the contact cone cavity.
[0014] Preferably, the manufacturing device further comprises two wedge scrapers, which are respectively fixedly connected to two sides of the liquid storage chamber, and the inner surface of the aluminum foil is in contact with the two wedge scrapers.
[0015] Preferably, the manufacturing device also includes four limit slides, a lifting curved cavity and a discharge pipe, the four limit slides are respectively fixedly connected at the four corners of the liquid storage cavity, the lifting curved cavity is slidably connected to the four limit slides, the lifting curved cavity is slidably connected in the liquid storage cavity, the discharge pipe is fixedly connected below the lifting curved cavity, and the liquid storage cavity is slidably connected to the discharge pipe.
[0016] Preferably, the manufacturing device further comprises two telescopic rods, both of which are fixedly connected to the liquid storage chamber, and the lifting and lowering curved chamber is fixedly connected to the two telescopic rods.
[0017] Preferably, the manufacturing device also includes two reduction motors II, two stirring shafts and two groups of multiple stirring plates, the two reduction motors II are respectively fixedly connected to the two sides below the lifting and lowering chamber, the two stirring shafts are respectively fixedly connected to the output shafts of the two reduction motors II, and the two groups of multiple stirring plates are respectively fixedly connected to the two stirring shafts.
[0018] Preferably, the manufacturing device also includes an inclined slide, a hollow storage cavity and a cleaning sponge, the inclined slide is fixedly connected to the liquid storage cavity, the hollow storage cavity is rotatably connected to the inclined slide, the cleaning sponge is adhered to the hollow storage cavity, and the outer surface of the aluminum foil is in contact with the cleaning sponge.
[0019] Preferably, the polyamide film produced by the polyamide film manufacturing process has a heat-insulating coating applied on its outer surface. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The present invention is further described in detail below with reference to the accompanying drawings and specific implementation methods.
[0021] Figure 1 It is a schematic flow diagram of a polyamide film and a manufacturing process thereof of the present invention;
[0022] Figure 2 It is a schematic diagram of the overall structure of the manufacturing device of the present invention;
[0023] Figure 3 It is a partial structural schematic diagram of the entire manufacturing device of the present invention;
[0024] Figure 4 It is a schematic diagram of the cross-sectional structure of the entire part of the manufacturing device of the present invention;
[0025] Figure 5 It is a schematic diagram of the structure of four limiting rollers and aluminum foil of the present invention;
[0026] Figure 6 It is a structural schematic diagram of an embodiment of driving a polyamide solution to move upward;
[0027] Figure 7 is a structural schematic diagram of an embodiment of applying a heat-insulating coating to a polyamide solution;
[0028] Figure 8 is a schematic diagram of a cross-sectional structure of an embodiment of applying a heat-insulating coating to a polyamide solution;
[0029] Fig. 9 It is a structural schematic diagram of an embodiment of cleaning aluminum foil;
[0030] Fig.10 It is a schematic diagram of the cross-sectional structure of an embodiment of cleaning aluminum foil. DETAILED DESCRIPTION
[0031] The present invention will be further described in detail below in conjunction with the accompanying drawings.
[0032] The following is combined with Figure 1 Detailed description, a polyamide film manufacturing process, the process comprises the following steps:
[0033] Step 1, adding fixed polyamide and water into a hot melt machine in proportion to prepare a polyamide solution;
[0034] Step 2: Add the polyamide solution into the liquid storage cavity, then pass the aluminum foil through the polyamide solution, and apply the polyamide solution to the lower surface of the aluminum foil;
[0035] Step 3, heating the aluminum foil to solidify the polyamide solution on the lower surface of the aluminum foil, applying the heat-insulating coating to the lower surface of the aluminum foil after solidification, and then separating the solidified polyamide solution from the lower surface of the aluminum foil with an inclined knife;
[0036] Step 4: The polyamide film is manufactured by peeling, trimming, rolling, pickling, washing and drying.
[0037] Furthermore, when the outer surface of the polyamide film is coated with a heat-insulating coating, the polyamide film will have better heat-insulating properties, further enhancing the heat resistance of the polyamide film.
[0038] The following is combined with Figure 2-5 7-8 describe in detail, the manufacturing device includes a liquid storage chamber 101, four limiting rollers 102, an aluminum foil 103, a bevel knife 104 and a smearing component, the liquid storage chamber 101 is connected to four limiting rollers 102 by shaft rotation, the aluminum foil 103 is transmission-connected between the four limiting rollers 102, the bevel knife 104 is fixedly connected to the liquid storage chamber 101 by welding, and the smearing component is connected to the liquid storage chamber 101.
[0039] Furthermore, the liquid storage chamber 101 plays a role of storage and can provide storage space for the polyamide solution, and the four limiting rollers 102 can provide support space for the aluminum foil 103, so that the aluminum foil 103 can be stably stretched between the four limiting rollers 102. The front ends of the four limiting rollers 102 are fixedly connected to the transmission sprockets. The liquid storage chamber 101 is rotatably connected to the main rotating sprocket and the reduction motor. The reduction motor is fixedly connected to the main rotating sprocket, and the main rotating sprocket is connected to the four transmission sprockets through a transmission chain. After the reduction motor is started, the main rotating sprocket can be driven to rotate, and the rotation The main rotating sprocket will drive the four transmission sprockets to rotate, and the rotating four transmission sprockets will drive the four limiting rollers 102 to rotate in the same direction, and the four limiting rollers 102 rotating in the same direction will drive the aluminum foil 103 to rotate counterclockwise. When the aluminum foil 103 rotates, the aluminum foil 103 will contact the polyamide solution in the liquid storage chamber 101, and the polyamide solution will stick to the lower surface of the aluminum foil 103. The limiting roller 102 at the right end has a heating function. When the polyamide solution sticking to the lower surface of the aluminum foil 103 contacts the limiting roller at the right end, the aluminum foil 103 will be heated. When the polyamide solution contacts the aluminum foil 103, the polyamide solution will be dried and solidified on the aluminum foil 103. The inclined blade 104 is located directly above the upper limiting roller 102. The inclined blade 104 contacts the aluminum foil 103. The thermal insulation coating can be applied to the lower surface of the aluminum foil by using the smearing member to store the polyamide solution in the liquid storage chamber 101. Then, the four limiting rollers 102 are rotated to drive the aluminum foil 103 to rotate. The rotating aluminum foil 103 will contact the polyamide solution in the liquid storage chamber 101, and the polyamide solution will stick to the aluminum foil 103. To the lower surface of the aluminum foil 103, the aluminum foil 103 is then heated by the limiting roller 102 located at the right end to allow the polyamide solution to solidify on the aluminum foil 103, and finally the thermal insulation coating is applied to the solidified polyamide solution by using the smearing component. When the polyamide solution that is adhered to the thermal insulation coating and solidified contacts with the bevel dividing knife 104, the bevel dividing knife 104 will contact the polyamide solution that is adhered to the thermal insulation coating and solidified, and remove the polyamide solution that is adhered to the thermal insulation coating and solidified from the aluminum foil 103, thereby completing the separation of the polyamide solution that is adhered to the thermal insulation coating and solidified.
[0040] The following is combined with Figure 2-4 As described in detail in 7-8, the smearing component includes a transverse sliding cavity 201, a supporting wall plate 202, an oblique sliding plate 203, a smearing roller 204 and a transverse screw 205. The transverse sliding cavity 201 is fixedly connected to the liquid storage cavity 101 by welding, the supporting wall plate 202 is slidingly connected in the transverse sliding cavity 201 through a cavity, the oblique sliding plate 203 is fixedly connected to the supporting wall plate 202 by welding, the smearing roller 204 is rotatably connected to the oblique sliding plate 203 through a bearing seat, the transverse screw 205 is rotatably connected to the liquid storage cavity 101 through a bearing hole, and the supporting wall plate 202 and the transverse screw 205 are connected by threaded transmission.
[0041] Furthermore, the transverse sliding cavity 201 can provide a sliding space for the supporting wall plate 202, and the supporting wall plate 202 can provide a fixed space for the oblique sliding plate 203, and the oblique sliding plate 203 can provide a rotating space for the coating roller 204. The coating roller 204 is adhered with a heat-insulating coating and contacts with the polyamide solution solidified on the aluminum foil 103, so as to apply the heat-insulating coating to the polyamide solution solidified on the aluminum foil 103, and the distances between the oblique sliding plate 203 and the coating roller 204 and the aluminum foil 103 are equal. After rotating the transverse moving screw 205, the supporting wall plate 202 can be driven to slide in the transverse sliding cavity 201, thereby changing the position of the supporting wall plate 202. The position of the supporting wall panel 202 is different, and the distance between the oblique sliding plate 203 and the coating roller 204 and the aluminum foil 103 will also change. The oblique sliding plate 203 can be used to contact the polyamide solution adhering to the aluminum foil 103, and the polyamide solution can be scraped off, thereby further changing the thickness of the polyamide solution adhering to the aluminum foil 103, thereby changing the thickness of the processed polyamide film, and the scraped polyamide solution will be dried by the limiting roller 102 at the right end to allow the polyamide solution to solidify. The solidified polyamide solution will contact the coating roller 204 to apply the thermal insulation coating to the solidified polyamide solution.
[0042] According to the instruction manual Figure 2 , 7 As described in detail in FIG. 8 , the manufacturing device further includes a storage barrel 301 and a contact cone cavity 302 . The storage barrel 301 is fixedly connected to the supporting wall plate 202 by welding. The contact cone cavity 302 is fixedly connected to the storage barrel 301 by welding. The coating roller 204 contacts the contact cone cavity 302 .
[0043] Furthermore, thermal insulation coating is stored in the storage barrel 301, and the thermal insulation coating in the storage barrel 301 will enter the contact cone cavity 302, and a valve is provided on the contact cone cavity 302. After the valve is opened, the thermal insulation coating will enter the contact cone cavity 302 and be smeared on the coating roller 204. At this time, when the coating roller 204 contacts the solidified polyamide solution, the thermal insulation coating will be smeared on the solidified polyamide solution. When a large amount of thermal insulation coating is stuck to the coating roller 204, the thermal insulation coating will directly fall onto the inclined sliding plate 203, so as to prevent the thermal insulation coating from falling into the liquid storage cavity 101 and affecting the quality of the polyamide solution in the liquid storage cavity 101.
[0044] According to the instruction manual Figure 2-5 In detail, the manufacturing device further includes two wedge scrapers 401 , which are fixedly connected to two sides of the liquid storage chamber 101 by welding, and the inner surface of the aluminum foil 103 is in contact with the two wedge scrapers 401 .
[0045] Furthermore, when the aluminum foil 103 moves in the liquid storage chamber 101, the upper and lower surfaces of the aluminum foil 103 will be stuck with the polyamide solution, and the polyamide solution stuck to the inner surface of the aluminum foil 103 is useless, so it is necessary to use a wedge scraper 401 to scrape the polyamide solution stuck to the inner surface of the aluminum foil 103 to ensure that there is no residual polyamide solution on the inner surface of the aluminum foil 103, and use another wedge scraper 401 to scrape the inner surface of the aluminum foil 103 to ensure that the clean aluminum foil 103 enters the liquid storage chamber 101 again.
[0046] According to the instruction manual Figure 2-4 6 is described in detail, the manufacturing device also includes four limit slides 501, a lifting curved cavity 502 and a discharge pipe 504, the four limit slides 501 are respectively fixedly connected at the four corners of the liquid storage cavity 101 by welding, the lifting curved cavity 502 and the four limit slides 501 are slidably connected through a plurality of circular holes, the lifting curved cavity 502 is slidably connected in the liquid storage cavity 101, the discharge pipe 504 is fixedly connected below the lifting curved cavity 502 by welding, and the liquid storage cavity 101 and the discharge pipe 504 are slidably connected through circular holes.
[0047] Furthermore, the four limiting slides 501 can provide sliding space for the lifting curved cavity 502, and limit the lifting curved cavity 502 so that the lifting curved cavity 502 can only slide up and down. When the polyamide solution enters the liquid storage cavity 101, it will fall on the lifting curved cavity 502. The lifting and lowering of the lifting curved cavity 502 can drive the polyamide solution to rise and fall, thereby playing a feeding role. When the polyamide solution in the liquid storage cavity 101 is consumed, the lifting curved cavity 502 will slowly move upward to allow the aluminum foil 103 to contact the polyamide solution at all times until there is no polyamide solution on the lifting curved cavity 502. A valve is provided on the discharge pipe 504 to control whether there is a flow of polyamide solution in the discharge pipe 504, and the polyamide solution on the lifting curved cavity 502 can be discharged through the discharge pipe 504 to achieve the recycling and reuse of the remaining polyamide solution.
[0048] According to the instruction manual Figure 2-4 6, the manufacturing device further comprises two telescopic rods 503, both of which are fixedly connected to the liquid storage chamber 101 via flange plates, and the lifting and lowering chamber 502 is fixedly connected to the two telescopic rods 503 via flange plates.
[0049] Furthermore, when the polyamide solution in the liquid storage chamber 101 is consumed, the two telescopic rods 503 will be activated, thereby driving the lifting and lowering curved chamber 502 to move slowly upward, ensuring that the aluminum foil 103 can always be in contact with the polyamide solution.
[0050] According to the instruction manual Figure 2-46 is described in detail, the manufacturing device also includes two reduction motors II601, two stirring shafts 602 and two groups of multiple stirring plates 603, the two reduction motors II601 are respectively fixedly connected to the two sides below the lifting and lowering chamber 502 through flange plates, the two stirring shafts 602 are respectively fixedly connected to the output shafts of the two reduction motors II601 through couplings, and the two groups of multiple stirring plates 603 are respectively fixedly connected to the two stirring shafts 602 by welding.
[0051] Furthermore, when the aluminum foil 103 moves in the liquid storage chamber 101, the two reduction motors II601 will also be started. The started two reduction motors II601 will drive the two stirring shafts 602 to rotate, and the rotating two stirring shafts 602 will drive the two groups of multiple stirring plates 603 to rotate. The two groups of multiple stirring plates 603 both have a heating function. When the two groups of multiple stirring plates 603 rotate, the polyamide solution on the lifting and lowering cavity 502 will be heated and stirred to ensure that the polyamide solution on the lifting and lowering cavity 502 will not solidify.
[0052] According to the instruction manual Figure 2 , 9 10 is described in detail, the manufacturing device also includes an inclined slide 701, a hollow storage chamber 702 and a cleaning sponge 703, the inclined slide 701 is fixedly connected to the liquid storage chamber 101 by welding, the hollow storage chamber 702 is rotatably connected to the inclined slide 701 by a hollow shaft, the cleaning sponge 703 is adhered to the hollow storage chamber 702 by multiple screws, and the outer surface of the aluminum foil 103 is in contact with the cleaning sponge 703.
[0053] Furthermore, the inclined slide plate 701 can provide a rotating space for the hollow storage chamber 702. The hollow storage chamber 702 is designed as a hollow structure, and a plurality of circular holes are arranged on the top thereof. Both ends of the hollow storage chamber 702 are fixedly connected with round tubes, and the two round tubes are rotatably connected to the inclined slide plate 701. Water is added into the hollow storage chamber 702 through the two round tubes, and the water entering the hollow storage chamber 702 will be discharged through the plurality of circular holes on the top and adhere to the cleaning sponge 703. At this time, the cleaning sponge 703 will be in a wet state. At this time, when the aluminum foil 103 rotates, it will contact with the wet cleaning sponge 703, and the wet cleaning sponge 703 can be cleaned by the aluminum foil 103. The moistened cleaning sponge 703 can be in contact with the aluminum foil 103 to achieve contact with the outer surface of the aluminum foil 103, ensuring that the outer surface of the aluminum foil 103 is in a clean state, which is convenient for the outer surface of the aluminum foil 103 to adhere the polyamide solution again. If the outer surface of the aluminum foil 103 is not clean, the effect of the aluminum foil 103 adhering to the polyamide solution may be reduced, and finally the quality of the polyamide film may be affected. When excess water from the cleaning sponge 703 flows down, it will also fall onto the inclined slide 701, and finally flow down through the inclined slide 701, preventing water from entering the liquid storage chamber 101. If water enters the liquid storage chamber 101, it may affect the quality of the polyamide film.
Claims
1. A polyamide film manufacturing process, characterized in that: The process includes the following steps: Step 1, adding fixed polyamide and water into a hot melt machine in proportion to prepare a polyamide solution; Step 2: Add the polyamide solution into the liquid storage cavity, then pass the aluminum foil through the polyamide solution, and apply the polyamide solution to the lower surface of the aluminum foil; Step 3, heating the aluminum foil to solidify the polyamide solution on the lower surface of the aluminum foil, applying the heat-insulating coating to the lower surface of the aluminum foil after solidification, and then separating the solidified polyamide solution from the lower surface of the aluminum foil with an inclined knife; Step 4: After peeling, trimming, rolling, pickling, washing and drying, the polyamide film can be manufactured; The above-mentioned manufacturing process also requires the use of a manufacturing device, which comprises a liquid storage chamber (101) and four limiting rollers (102) rotatably connected to the liquid storage chamber (101), an aluminum foil (103) is transmission-connected between the four limiting rollers (102), an inclined dividing knife (104) is fixedly connected to the liquid storage chamber (101), and a smearing component is connected to the liquid storage chamber (101); The smearing member comprises a transverse sliding cavity (201) fixedly connected to the liquid storage cavity (101) and a supporting wall plate (202) slidably connected in the transverse sliding cavity (201); an obliquely retracted sliding plate (203) is fixedly connected to the supporting wall plate (202); an smearing roller (204) is rotatably connected to the upper part of the obliquely retracted sliding plate (203); a transversely moving screw (205) is rotatably connected to the upper part of the liquid storage cavity (101); and the transversely moving screw (205) is connected to the supporting wall plate (202) by threads; Two wedge scrapers (401) are fixedly connected in the liquid storage chamber (101), and the two wedge scrapers (401) are in contact with the inner surface of the aluminum foil (103).
2. A polyamide film manufacturing process according to claim 1, characterized in that: The supporting wall plate (202) is fixedly connected to a storage barrel (301), the storage barrel (301) is fixedly connected to a contact cone cavity (302), and the contact cone cavity (302) is in contact with the coating roller (204).
3. A polyamide film manufacturing process according to claim 1, characterized in that: The liquid storage chamber (101) is fixedly connected to four limiting slides (501), and a lifting curved chamber (502) is slidably connected to the four limiting slides (501). The lifting curved chamber (502) is slidably connected in the liquid storage chamber (101), and a discharge pipe (504) is fixedly connected to the lifting curved chamber (502), and the discharge pipe (504) is slidably connected to the liquid storage chamber (101).
4. A polyamide film manufacturing process according to claim 3, characterized in that: Two telescopic rods (503) are fixedly connected to the liquid storage chamber (101), and the two telescopic rods (503) are both fixedly connected to the lifting and lowering chamber (502).
5. A polyamide film manufacturing process according to claim 4, characterized in that: The lifting and lowering curved chamber (502) is fixedly connected to two reduction motors II (601), the output shafts of the two reduction motors II (601) are fixedly connected to stirring shafts (602), and the two stirring shafts (602) are fixedly connected to a plurality of stirring plates (603).
6. A polyamide film manufacturing process according to claim 1, characterized in that: The liquid storage cavity (101) is fixedly connected to an inclined slide plate (701), a hollow storage cavity (702) is rotatably connected to the inclined slide plate (701), a cleaning sponge (703) is adhered to the hollow storage cavity (702), and the cleaning sponge (703) is in contact with the outer surface of the aluminum foil (103).
7. The polyamide film produced by the polyamide film manufacturing process according to claim 1, characterized in that: The outer surface of the polyamide film is coated with a heat-insulating coating.