Preparation method and application of immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters

Through a mixed ceria composite material loaded with gold nanoparticles and a sandwich electrochemiluminescence immunosensor with gold and silver nanoclusters, combined with triethylamine co-reactant, the existing detection methods have solved the low sensitivity and complicated steps. , achieving high sensitivity and rapid detection of neuron-specific enolases, is suitable for early screening and chemotherapy monitoring of small cell lung cancer.

CN115356384BInactive Publication Date: 2024-11-29SHANDONG UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211044223.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-30
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing neuron-specific enolase detection methods have problems such as radiocontamination, low sensitivity, long detection cycle and cumbersome steps, making it difficult to achieve fast and accurate detection.

Method used

Using mixed ceria composites loaded with gold nanoparticles as substrates, combined with gold and silver nanoclusters as luminescent materials and neuron-specific enolase detection antibodies, sandwich electrochemiluminescence immunity is prepared using layer-by-layer self-assembly technology. The sensor enhances the electrochemiluminescence intensity through the aggregation-induced luminescence characteristics, and accelerates the generation of excited states with triethylamine as a co-reaction promoter.

Benefits of technology

It realizes high sensitivity and rapid detection of neuron-specific enolases, with a wide detection range, low lower detection limit, simple operation, good reproducibility and selectivity, and is suitable for early screening and chemotherapy monitoring of small cell lung cancer.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention belongs to the field of immunoassay and biosensor technology, and provides a preparation method and application of an immunosensor based on gold-silver nanocluster aggregation-induced luminescence. Specifically, gold-silver nanocluster is used as a luminescent material, and the doping of silver not only increases the aggregation of metal clusters, but also inhibits the free rotation of organic ligands to reduce non-radiative transitions, effectively enhancing the intensity of electrochemiluminescence signals. Mixed-valence cerium dioxide loaded with gold nanoparticles is used as a co-reaction promoter to promote the generation of more strongly oxidizing triethylamine free radicals to accelerate the generation of excited states of gold-silver nanocluster, thereby further improving the efficiency of electrochemiluminescence; at the same time, its larger specific surface area can fix more antibodies. According to the difference in the intensity of the electrochemiluminescence signal of the test object with different concentrations, the detection of neuron-specific enolase is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for preparing an immunosensor for gold-silver nanocluster aggregation-induced luminescence. Specifically, a sandwich-type electrochemiluminescent immunosensor for detecting neuron-specific enolase is prepared by using a mixed-valence cerium dioxide composite material loaded with gold nanoparticles as a substrate, using gold-silver nanocluster as a luminescent material to label a neuron-specific enolase detection antibody, and using triethylamine as a co-reactant, belonging to the field of new functional materials and biosensor detection technology. Background Art

[0002] Neuron-specific enolase (NSE) is one of the most commonly used serum tumor biomarkers in clinical diagnosis. It is mainly present in neural tissue and neuroendocrine tissue. It is usually used for early screening of small cell lung cancer, and its critical value is about 16 ~ 25 ng / mL. Lung cancer is the most common malignant tumor in the world, which has serious harm to human life and health. Small cell lung cancer accounts for 13 ~ 20% of lung cancer. It shows symptoms of metastasis to lymph nodes or distant sites in the early stage, and is the most invasive type of lung cancer. Seven out of ten patients are in the advanced stage when diagnosed. Early detection and early treatment of small cell lung cancer can prolong the survival time of one-quarter of patients. The concentration of neuron-specific enolase is significantly increased in the blood of patients with small cell lung cancer, and its sensitivity is as high as 81.2% compared with other tumor markers. The serum level of neuron-specific enolase is related to tumor progression and is considered to be a reliable detection marker during chemotherapy. Therefore, rapid and accurate detection of neuron-specific enolase is of great significance for the clinical diagnosis and treatment of related cancers and diseases.

[0003] There are many clinical detection methods for neuron-specific enolase antigen, such as enzyme-linked immunosorbent assay, radioimmunoassay, chemiluminescence immunoassay, etc. However, the above methods have the disadvantages of radioactive pollution, low sensitivity, long detection cycle, and complicated steps. Electrochemiluminescence sensor is a new analytical method that combines chemiluminescence technology with electrochemical technology. Therefore, it has the controllability of chemiluminescence technology and the sensitivity of electrochemical technology. Compared with traditional analytical methods, the electrochemiluminescence immunosensor used in the present invention has the advantages of high sensitivity, good selectivity, simple structure, easy operation, easy miniaturization, fast response, low background signal, etc. Therefore, the present invention prepares an immunosensor based on gold and silver nanoclusters with aggregation-induced luminescence characteristics, and realizes the detection of neuron-specific enolase.

[0004] In the present invention, Ag is used as a bridge connector between Au-sulfate motifs, which not only increases the aggregation of metal clusters, but also inhibits the free rotation of organic ligands to reduce non-radiative transitions. Its aggregation-induced luminescence characteristics are used to effectively enhance the electrochemiluminescence intensity, and obtain highly luminescent gold-silver nanoclusters. Mixed-valence cerium dioxide loaded with gold nanoparticles is used as a substrate, which has good electrical conductivity and a large surface area to fix more antibodies; at the same time, as a co-reaction promoter, it can promote the generation of more strongly oxidizing triethylamine free radicals to accelerate the generation of excited states of gold-silver nanoclusters. The present invention uses layer-by-layer self-assembly technology to prepare an immunosensor based on aggregation-induced luminescence of gold-silver nanoclusters, realizes quantitative detection of neuron-specific enolase, has the advantages of wide detection range, low detection limit, high sensitivity, simple operation, fast detection speed, etc., and has good reproducibility, stability and selectivity. The research on constructing this electrochemiluminescence immunosensor is of great significance for the detection of neuron-specific enolase. Summary of the invention

[0005] One of the purposes of the present invention is to use gold and silver nanoclusters with aggregation-induced emission characteristics as luminescent materials, and the luminescent materials show excellent electroluminescent properties.

[0006] The second purpose of the present invention is to synthesize mixed-valence cerium dioxide loaded with gold nanoparticles with a large specific surface area as a substrate, which has good electrical conductivity and a large surface area to fix more antibodies; at the same time, as a co-reaction promoter, it can promote the generation of more strongly oxidizing triethylamine free radicals to accelerate the generation of excited states of gold and silver nanoclusters, thereby doubling the electrochemiluminescence efficiency.

[0007] The third purpose of the present invention is to use a mixed-valence cerium dioxide composite material loaded with gold nanoparticles as a substrate and gold-silver nanoclusters as neuron-specific enolase detection antibody markers to construct an enzyme-free, rapid and ultra-sensitive sandwich electrochemiluminescence immunosensor, thereby achieving the purpose of sensitive detection of neuron-specific enolase.

[0008] The technical solution of the present invention is as follows:

[0009] 1. A method for preparing an immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters, comprising the following steps:

[0010] (1) Polish a glassy carbon electrode with a diameter of 3.0 to 5.0 mm into a mirror surface using alumina polishing powder and clean it by ultrasonic cleaning in anhydrous ethanol;

[0011] (2) Take 6.0 μL of 0.3 ~ 3.0 mg / mL of the mixed-valence ceria composite dispersion loaded with gold nanoparticles and drop it onto the electrode surface, dry it at room temperature, rinse the electrode surface with ultrapure water, and dry it at room temperature;

[0012] (3) Continue to add 6 µL of 5.0 ~ 15.0 µg / mL neuron-specific enolase capture antibody to the electrode surface and dry in a 4°C refrigerator;

[0013] (4) Continue to add 3.0 μL of 0.8 ~ 1.2 mg / mL bovine serum albumin solution to the electrode surface to block nonspecific active sites on the electrode surface, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0014] (5) Add 6.0 µL of a series of different concentrations of neuron-specific enolase antigen solutions ranging from 0.0001 to 40 ng / mL, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0015] (6) Finally, 6 μL of a 0.3-3.0 mg / mL gold-silver nanocluster-labeled neuron-specific enolase detection antibody solution was dropped onto the electrode and incubated at room temperature for 1 hour. The solution was then washed with ultrapure water to prepare an immunosensor based on gold-silver nanocluster aggregation-induced luminescence, which was then stored in a refrigerator at 4°C for future use.

[0016] 2. The mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles is prepared by the following steps:

[0017] (1) Preparation of mixed valence cerium dioxide

[0018] 4 mL of 0.2 mol / L cerium nitrate solution was added to 26 mL of 1 mmol / L sodium phosphate solution, stirred for 5 minutes, transferred to a polytetrafluoroethylene autoclave and heated to 100-200°C for 12-20 hours, then washed three times with ultrapure water and ethanol in sequence, dried in a 60°C vacuum drying oven for 12 hours, programmed to rise to 400-600°C and calcined for 4-8 hours, with the heating rate controlled at 5-10°C / min, to obtain mixed-valence cerium dioxide;

[0019] (2) Preparation of gold nanoparticle solution

[0020] 1 mL of 0.01 mol / L chloroauric acid solution and 1 mL of 0.01 mol / L trisodium citrate solution were added to 18 mL of ultrapure water in sequence under stirring, and after stirring for 5 to 15 minutes, 1 mL of 0.1 mol / L freshly prepared sodium tetrahydroborate solution was added, and the mixture was kept in an ice water bath for 10 to 30 minutes, and then stirred at room temperature for 30 minutes, and allowed to stand for 12 hours to obtain a gold nanoparticle solution;

[0021] (3) Preparation of mixed-valence cerium dioxide composite dispersion loaded with gold nanoparticles

[0022] 10.5 to 105 mg of the mixed-valence cerium dioxide prepared above was added to 21 mL of the gold nanoparticle solution prepared above, and stirred for 1 to 5 h to obtain a mixed-valence cerium dioxide composite material solution loaded with gold nanoparticles. After centrifugal washing with ultrapure water and ethanol, respectively, the solution was vacuum dried at 60°C for 12 h to obtain a mixed-valence cerium dioxide composite material loaded with gold nanoparticles. 0.5 to 5 mg of the mixed-valence cerium dioxide composite material loaded with gold nanoparticles prepared above was added to 1 mL of ultrapure water, and ultrasonicated for 30 min to obtain a mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles.

[0023] 3. The preparation steps of the gold-silver nanocluster labeled neuron-specific enolase detection antibody solution are as follows:

[0024] (1) Preparation of gold and silver nanoclusters

[0025] 4 mL of 5 ~ 15 mmol / L chloroauric acid solution and 1 mL of 2 ~ 10 mmol / L silver nitrate solution were added to 5 mL of freshly prepared 5 ~ 15 mmol / L glutathione GSH solution, 10 μL of 1 ~ 5 mol / L sodium hydroxide solution was added dropwise to dissolve the precipitate, the mixed solution was heated at 70 ~ 95°C for 4 ~ 24 h with gentle stirring, cooled to room temperature, dialyzed for purification for 24 h, then washed with a water / acetonitrile mixed solution with a volume ratio of 1:3, dried at 60°C for 12 h, and the gold-silver nanoclusters were obtained, which were stored in a refrigerator at 4°C for later use;

[0026] (2) Preparation of gold-silver nanocluster labeled neuron-specific enolase detection antibody solution

[0027] 1 ~ 5 mol / L 1-ethyl-3-dimethylaminopropylcarbodiimide and 0.1 ~ 1 mol / L N-hydroxysuccinimide were mixed with 1 mL of the gold-silver nanoclusters prepared above, incubated at 4°C for 5 ~ 10 hours, centrifuged at 12000 rpm to separate the above solution, added with 100 ~ 500 μL of neuron-specific enolase detection antibody solution, and shaken at room temperature for 10 ~ 40 minutes to obtain a neuron-specific enolase detection antibody solution labeled with gold-silver nanoclusters.

[0028] 4. For the detection of neuron-specific enolase, the steps are as follows:

[0029] (1) The test was carried out using an electrochemical workstation with a three-electrode system. The Ag / AgCl electrode was used as the reference electrode, the platinum wire electrode was used as the auxiliary electrode, the prepared immunosensor based on gold-silver nanocluster aggregation-induced luminescence was used as the working electrode, the high voltage of the photomultiplier tube was set to 500 V, the scanning potential was 0 ~ 1.2 V, and the scanning rate was 0.1 V / s;

[0030] (2) In 10 mL of phosphate buffer solution containing 100 mmol / L triethylamine at pH 7.38, the electrochemiluminescence signal intensity generated by the antigen at different concentrations was detected by the electrochemiluminescence system, and a working curve was drawn;

[0031] (3) replacing the neuron-specific enolase antigen solution with the test sample solution for testing;

[0032] (4) Use the working curve method to calculate the concentration of neuron-specific enolase in the sample to be tested.

[0033] Beneficial results of the present invention

[0034] (1) The present invention successfully synthesized gold-silver nanoclusters with aggregation-induced emission properties. The material preparation method is simple. By doping with silver elements, not only the free rotation of glutathione organic ligands is reduced, but also the gold nanoclusters can be connected to increase their aggregation, thereby reducing the non-radiative energy transition in the energy relaxation of excited-state gold nanoclusters, improving the luminescence intensity, and solving the problem of low electrochemiluminescence signal.

[0035] (2) The mixed-valence ceria loaded with gold nanoparticles in the present invention serves as a substrate, has good electrical conductivity, and a large surface area to fix more antibodies. At the same time, gold-nitrogen bonds can be formed between the gold nanoparticles and the antibodies, making the antibodies more firmly immobilized. In addition, the use of a cross-linking agent is omitted, which reduces the number of steps and avoids the influence of the poor conductivity of the cross-linking agent. At the same time, the mixed-valence ceria loaded with gold nanoparticles serves as a co-reaction promoter, which can promote the generation of more strongly oxidizing triethylamine free radicals to accelerate the generation of excited states of gold-silver nanoclusters, thereby enhancing the electrochemiluminescence efficiency, so that during the neuron-specific enolase test, the signal change value increases, thereby improving the sensitivity of the detection.

[0036] (3) The immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters prepared by the present invention has a linear range of 0.1 pg / mL to 40 ng / mL for neuron-specific enolase and a detection limit of 0.033 pg / mL. It has a short response time, a wide linear range, a low detection limit, good stability and reproducibility, and can achieve simple, fast, highly sensitive and specific detection. DETAILED DESCRIPTION

[0037] (The present invention is now further described through specific implementation methods, but is not limited thereto)

[0038] Example 1. A method for preparing an immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters, comprising the following steps:

[0039] (1) Polish a glassy carbon electrode with a diameter of 3.0 mm into a mirror surface using alumina polishing powder and clean it by ultrasonic cleaning in anhydrous ethanol;

[0040] (2) Take 6.0 μL of 3.0 mg / mL of mixed-valence ceria composite dispersion loaded with gold nanoparticles and drop it onto the electrode surface, dry it at room temperature, rinse the electrode surface with ultrapure water, and dry it at room temperature;

[0041] (3) Continue to add 6 µL, 15.0 µg / mL neuron-specific enolase capture antibody to the electrode surface and dry in a 4°C refrigerator;

[0042] (4) Continue to add 3.0 μL of 1.2 mg / mL bovine serum albumin solution to the electrode surface to block nonspecific active sites on the electrode surface, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0043] (5) Add 6.0 µL of a series of different concentrations of neuron-specific enolase antigen solutions ranging from 0.0001 to 40 ng / mL, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0044] (6) Finally, 6 μL of 3.0 mg / mL gold-silver nanocluster-labeled neuron-specific enolase detection antibody solution was dropped onto the electrode and incubated at room temperature for 1 hour. The solution was then washed with ultrapure water to prepare an immunosensor based on aggregation-induced luminescence of gold-silver nanocluster clusters. The immunosensor was stored in a refrigerator at 4°C for future use.

[0045] Example 2. A method for preparing an immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters, comprising the following steps:

[0046] (1) Polish a glassy carbon electrode with a diameter of 4.0 mm into a mirror surface using alumina polishing powder and clean it by ultrasonic cleaning in anhydrous ethanol;

[0047] (2) Take 6.0 μL of 1.0 mg / mL of the mixed-valence ceria composite dispersion loaded with gold nanoparticles and drop it onto the electrode surface, dry it at room temperature, rinse the electrode surface with ultrapure water, and dry it at room temperature;

[0048] (3) Continue to add 6 µL, 10.0 µg / mL neuron-specific enolase capture antibody to the electrode surface and dry in a 4°C refrigerator;

[0049] (4) Continue to add 3.0 μL of 1.0 mg / mL bovine serum albumin solution to the electrode surface to block nonspecific active sites on the electrode surface, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0050] (5) Add 6.0 µL of a series of different concentrations of neuron-specific enolase antigen solutions ranging from 0.0001 to 40 ng / mL, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0051] (6) Finally, 6 μL of 1.5 mg / mL gold-silver nanocluster-labeled neuron-specific enolase detection antibody solution was dropped onto the electrode and incubated at room temperature for 1 hour. The solution was then washed with ultrapure water to prepare an immunosensor based on aggregation-induced luminescence of gold-silver nanocluster clusters. The immunosensor was stored in a refrigerator at 4°C for future use.

[0052] Example 3. A method for preparing an immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters, comprising the following steps:

[0053] (1) Polish a glassy carbon electrode with a diameter of 5.0 mm into a mirror surface using alumina polishing powder and clean it by ultrasonic cleaning in anhydrous ethanol;

[0054] (2) Take 6.0 μL of 0.3 mg / mL of the mixed-valence ceria composite dispersion loaded with gold nanoparticles and drop it onto the electrode surface, dry it at room temperature, rinse the electrode surface with ultrapure water, and dry it at room temperature;

[0055] (3) Continue to add 6 µL, 5.0 µg / mL neuron-specific enolase capture antibody to the electrode surface and dry in a 4°C refrigerator;

[0056] (4) Continue to add 3.0 μL of 0.8 mg / mL bovine serum albumin solution to the electrode surface to block the nonspecific active sites on the electrode surface, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry it in a refrigerator at 4°C;

[0057] (5) Add 6.0 µL of a series of different concentrations of neuron-specific enolase antigen solutions ranging from 0.0001 to 40 ng / mL, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator;

[0058] (6) Finally, 6 μL of 0.3 mg / mL gold-silver nanocluster-labeled neuron-specific enolase detection antibody solution was dropped onto the electrode and incubated at room temperature for 1 hour. The solution was then washed with ultrapure water to prepare an immunosensor based on gold-silver nanocluster aggregation-induced luminescence, which was then stored in a refrigerator at 4°C for future use.

[0059] Example 4. The mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles is prepared in the following steps:

[0060] (1) Preparation of mixed valence cerium dioxide

[0061] 4 mL of 0.2 mol / L cerium nitrate solution was added to 26 mL of 1 mmol / L sodium phosphate solution, stirred for 5 minutes, transferred to a polytetrafluoroethylene autoclave and heated to 100°C for 20 hours, then washed three times with ultrapure water and ethanol in sequence, dried in a 60°C vacuum drying oven for 12 hours, programmed to 400°C and calcined for 8 hours at a heating rate of 5°C / min to obtain mixed-valence cerium dioxide;

[0062] (2) Preparation of gold nanoparticle solution

[0063] 1 mL of 0.01 mol / L chloroauric acid solution and 1 mL of 0.01 mol / L trisodium citrate solution were added to 18 mL of ultrapure water in sequence under stirring. After stirring for 5 minutes, 1 mL of 0.1 mol / L freshly prepared sodium tetrahydroborate solution was added, and the mixture was kept in an ice-water bath for 10 minutes, and then stirred at room temperature for 30 minutes and allowed to stand for 12 hours to obtain a gold nanoparticle solution.

[0064] (3) Preparation of mixed-valence cerium dioxide composite dispersion loaded with gold nanoparticles

[0065] The 10.5 mg mixed-valence cerium dioxide prepared above was added to the 21 mL gold nanoparticle solution prepared above, and stirred for 5 h to obtain a mixed-valence cerium dioxide composite material solution loaded with gold nanoparticles. After centrifugal washing with ultrapure water and ethanol respectively, it was vacuum dried at 60°C for 12 h to obtain a mixed-valence cerium dioxide composite material loaded with gold nanoparticles. 0.5 mg of the mixed-valence cerium dioxide composite material loaded with gold nanoparticles prepared above was added to 1 mL ultrapure water and ultrasonicated for 30 min to obtain a mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles.

[0066] Example 5. The mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles is prepared in the following steps:

[0067] (1) Preparation of mixed valence cerium dioxide

[0068] 4 mL of 0.2 mol / L cerium nitrate solution was added to 26 mL of 1 mmol / L sodium phosphate solution, stirred for 5 minutes, transferred to a polytetrafluoroethylene autoclave and heated to 150°C for 16 hours, then washed three times with ultrapure water and ethanol in sequence, dried in a 60°C vacuum drying oven for 12 hours, programmed to 500°C and calcined for 6 hours at a heating rate of 7°C / min to obtain mixed-valence cerium dioxide;

[0069] (2) Preparation of gold nanoparticle solution

[0070] 1 mL of 0.01 mol / L chloroauric acid solution and 1 mL of 0.01 mol / L trisodium citrate solution were added to 18 mL of ultrapure water respectively under stirring, and after stirring for 10 minutes, 1 mL of 0.1 mol / L freshly prepared sodium tetrahydroborate solution was added, and the mixture was kept in an ice water bath for 20 minutes, and then stirred at room temperature for 30 minutes, and allowed to stand for 12 hours to obtain a gold nanoparticle solution;

[0071] (3) Preparation of mixed-valence cerium dioxide composite dispersion loaded with gold nanoparticles

[0072] The 50 mg mixed-valence cerium dioxide prepared above was added to the 21 mL gold nanoparticle solution prepared above, and stirred for 3 h to obtain a mixed-valence cerium dioxide composite material solution loaded with gold nanoparticles. After centrifugal washing with ultrapure water and ethanol respectively, it was vacuum dried at 60°C for 12 h to obtain a mixed-valence cerium dioxide composite material loaded with gold nanoparticles. 3 mg of the mixed-valence cerium dioxide composite material loaded with gold nanoparticles prepared above was added to 1 mL ultrapure water and ultrasonicated for 30 min to obtain a mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles.

[0073] Example 6. The mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles is prepared in the following steps:

[0074] (1) Preparation of mixed valence cerium dioxide

[0075] 4 mL of 0.2 mol / L cerium nitrate solution was added to 26 mL of 1 mmol / L sodium phosphate solution, stirred for 5 minutes, transferred to a polytetrafluoroethylene autoclave and heated to 200°C for 12 hours, then washed three times with ultrapure water and ethanol in sequence, dried in a 60°C vacuum drying oven for 12 hours, programmed to 600°C and calcined for 4 hours at a heating rate of 10°C / min to obtain mixed valence cerium dioxide;

[0076] (2) Preparation of gold nanoparticle solution

[0077] 1 mL of 0.01 mol / L chloroauric acid solution and 1 mL of 0.01 mol / L trisodium citrate solution were added to 18 mL of ultrapure water in sequence under stirring. After stirring for 5 minutes, 1 mL of 0.1 mol / L freshly prepared sodium tetrahydroborate solution was added, and the mixture was kept in an ice-water bath for 10 minutes, and then stirred at room temperature for 30 minutes and allowed to stand for 12 hours to obtain a gold nanoparticle solution.

[0078] (3) Preparation of mixed-valence cerium dioxide composite dispersion loaded with gold nanoparticles

[0079] 105 mg of the mixed-valence cerium dioxide prepared above was added to 21 mL of the gold nanoparticle solution prepared above, and stirred for 1 h to obtain a mixed-valence cerium dioxide composite material solution loaded with gold nanoparticles. After centrifugal washing with ultrapure water and ethanol respectively, it was vacuum dried at 60°C for 12 h to obtain a mixed-valence cerium dioxide composite material loaded with gold nanoparticles. 5 mg of the mixed-valence cerium dioxide composite material loaded with gold nanoparticles prepared above was added to 1 mL of ultrapure water and ultrasonicated for 30 min to obtain a mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles.

[0080] Example 7. The preparation steps of the gold-silver nanocluster labeled neuron-specific enolase detection antibody solution are as follows:

[0081] (1) Preparation of gold and silver nanoclusters

[0082] 4 mL of 5 mmol / L chloroauric acid solution and 1 mL of 2 mmol / L silver nitrate solution were added to 5 mL of freshly prepared 5 mmol / L glutathione GSH solution, 10 μL of 1 mol / L sodium hydroxide solution was added dropwise to dissolve the precipitate, the mixed solution was heated at 70°C with gentle stirring for 24 h, cooled to room temperature, dialyzed for purification for 24 h, then washed with a water / acetonitrile mixed solution with a volume ratio of 1:3, dried at 60°C for 12 h, and the gold-silver nanoclusters were obtained, which were stored in a refrigerator at 4°C for later use;

[0083] (2) Preparation of gold-silver nanocluster labeled neuron-specific enolase detection antibody solution

[0084] 1 mol / L 1-ethyl-3-dimethylaminopropylcarbodiimide and 0.1 mol / L N-hydroxysuccinimide were mixed with 1 mL of the gold-silver nanoclusters prepared above, incubated at 4°C for 5 hours, centrifuged at 12000 rpm, the above solution was separated, 100 μL of neuron-specific enolase detection antibody solution was added, and shaken at room temperature for 10 minutes to obtain a neuron-specific enolase detection antibody solution labeled with gold-silver nanoclusters.

[0085] Example 8. The preparation steps of the gold-silver nanocluster labeled neuron-specific enolase detection antibody solution are as follows:

[0086] (1) Preparation of gold and silver nanoclusters

[0087] 4 mL of 10 mmol / L chloroauric acid solution and 1 mL of 6 mmol / L silver nitrate solution were added to 5 mL of freshly prepared 8 mmol / L glutathione GSH solution, and 10 μL of 3 mol / L sodium hydroxide solution was added dropwise to dissolve the precipitate. The mixed solution was heated at 80°C for 12 h with gentle stirring, cooled to room temperature, dialyzed and purified for 24 h, and then washed with a water / acetonitrile mixed solution with a volume ratio of 1:3, and dried at 60°C for 12 h to obtain gold and silver nanoclusters, which were stored in a refrigerator at 4°C for later use;

[0088] (2) Preparation of gold-silver nanocluster labeled neuron-specific enolase detection antibody solution

[0089] 3 mol / L 1-ethyl-3-dimethylaminopropylcarbodiimide and 0.5 mol / L N-hydroxysuccinimide were mixed with 1 mL of the gold-silver nanoclusters prepared above, incubated at 4°C for 7 hours, centrifuged at 12000 rpm, the above solution was separated, 300 μL of neuron-specific enolase detection antibody solution was added, and shaken at room temperature for 25 minutes to obtain a neuron-specific enolase detection antibody solution labeled with gold-silver nanoclusters.

[0090] Example 9. The preparation steps of the gold-silver nanocluster labeled neuron-specific enolase detection antibody solution are as follows:

[0091] (1) Preparation of gold and silver nanoclusters

[0092] 4 mL of 15 mmol / L chloroauric acid solution and 1 mL of 10 mmol / L silver nitrate solution were added to 5 mL of freshly prepared 15 mmol / L glutathione GSH solution, 10 μL of 5 mol / L sodium hydroxide solution was added dropwise to dissolve the precipitate, the mixed solution was heated at 95°C for 4 h with gentle stirring, cooled to room temperature, dialyzed for purification for 24 h, then washed with a water / acetonitrile mixed solution with a volume ratio of 1:3, dried at 60°C for 12 h, and the gold-silver nanoclusters were obtained, which were stored in a refrigerator at 4°C for later use;

[0093] (2) Preparation of gold-silver nanocluster labeled neuron-specific enolase detection antibody solution

[0094] 5 mol / L 1-ethyl-3-dimethylaminopropylcarbodiimide and 1 mol / L N-hydroxysuccinimide were mixed with 1 mL of the gold-silver nanoclusters prepared above, incubated at 4°C for 10 hours, centrifuged at 12000 rpm, the above solution was separated, 500 μL of neuron-specific enolase detection antibody solution was added, and shaken at room temperature for 40 minutes to obtain a neuron-specific enolase detection antibody solution labeled with gold-silver nanoclusters.

[0095] Example 10. For the detection of neuron-specific enolase, the steps are as follows:

[0096] (1) The test was carried out using an electrochemical workstation with a three-electrode system. The Ag / AgCl electrode was used as the reference electrode, the platinum wire electrode was used as the auxiliary electrode, the prepared immunosensor based on gold-silver nanocluster aggregation-induced luminescence was used as the working electrode, the high voltage of the photomultiplier tube was set to 500 V, the scanning potential was 0 ~ 1.2 V, and the scanning rate was 0.1 V / s;

[0097] (2) In 10 mL of phosphate buffer solution containing 100 mmol / L triethylamine at pH 7.38, the electrochemiluminescence signal intensity generated by the antigen at different concentrations was detected by the electrochemiluminescence system, and a working curve was drawn;

[0098] (3) replacing the neuron-specific enolase antigen solution with the test sample solution for testing;

[0099] (4) Using the working curve method, the concentration of neuron-specific enolase antigen was obtained;

[0100] (5) Based on the linear relationship between the obtained luminescence intensity and the concentration of neuron-specific alcoholase antigen, a working curve was drawn with a linear range of 0.1 pg / mL to 40 ng / mL and a detection limit of 0.033 pg / mL.

Claims

1. A method for preparing an immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters, characterized in that: The following steps are involved: (1) A glassy carbon electrode with a diameter of 3.0 to 5.0 mm was polished into a mirror surface with aluminum oxide polishing powder and ultrasonically cleaned in anhydrous ethanol; (2) taking 6.0 μL of 0.3-3.0 mg / mL of a mixed-valence cerium dioxide composite dispersion loaded with gold nanoparticles and dropping it onto the electrode surface, drying it at room temperature, rinsing the electrode surface with ultrapure water, and drying it at room temperature; (3) Continue to add 6 μL of 5.0-15.0 μg / mL neuron-specific enolase capture antibody to the electrode surface and dry in a 4°C refrigerator; (4) Continue to add 3.0 μL of 0.8-1.2 mg / mL bovine serum albumin solution to the electrode surface to block nonspecific active sites on the electrode surface, rinse the electrode surface with pH 7.38 phosphate buffer, and dry in a 4°C refrigerator; (5) Add 6.0 μL of a series of neuron-specific enolase antigen solutions with different concentrations ranging from 0.0001 to 40 ng / mL, rinse the electrode surface with pH = 7.38 phosphate buffer, and dry in a 4°C refrigerator; (6) Finally, 6 μL of a 0.3-3.0 mg / mL gold-silver nanocluster-labeled neuron-specific enolase detection antibody solution was dropped onto the electrode, incubated at room temperature for 1 hour, and washed with ultrapure water to prepare an immunosensor based on gold-silver nanocluster aggregation-induced luminescence, which was stored in a refrigerator at 4°C for future use.

2. The method for preparing an immunosensor based on aggregation-induced luminescence of gold and silver nanoclusters according to claim 1, wherein the preparation of the mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles is characterized in that: Here are the steps: (1) Preparation of mixed valence cerium dioxide 4 mL of 0.2 mol / L cerium nitrate solution was added to 26 mL of 1 mmol / L sodium phosphate solution, stirred for 5 minutes, transferred to a polytetrafluoroethylene autoclave and heated to 100-200°C for 12-20 hours, then washed three times with ultrapure water and ethanol in sequence, dried in a 60°C vacuum drying oven for 12 hours, programmed to heat to 400-600°C and calcined for 4-8 hours, with the heating rate controlled at 5-10°C / min, to obtain mixed valence cerium dioxide; (2) Preparation of gold nanoparticle solution 1 mL of 0.01 mol / L chloroauric acid solution and 1 mL of 0.01 mol / L trisodium citrate solution were added to 18 mL of ultrapure water in sequence under stirring, and after stirring for 5 to 15 minutes, 1 mL of 0.1 mol / L freshly prepared sodium tetrahydroborate solution was added, and the mixture was kept in an ice water bath for 10 to 30 minutes, and then stirred at room temperature for 30 minutes, and allowed to stand for 12 hours to obtain a gold nanoparticle solution; (3) Preparation of mixed-valence cerium dioxide composite dispersion loaded with gold nanoparticles The 10.5-105 mg mixed-valence cerium dioxide prepared above was added to the 21 mL gold nanoparticle solution prepared above, and stirred for 1-5 h to obtain a mixed-valence cerium dioxide composite material solution loaded with gold nanoparticles. The solution was centrifuged and washed with ultrapure water and ethanol respectively, and then vacuum dried at 60°C for 12 h to obtain a mixed-valence cerium dioxide composite material loaded with gold nanoparticles. The 0.5-5 mg mixed-valence cerium dioxide composite material loaded with gold nanoparticles prepared above was added to 1 mL ultrapure water, and ultrasonicated for 30 min to obtain a mixed-valence cerium dioxide composite material dispersion loaded with gold nanoparticles.

3. The preparation method based on aggregation-induced luminescence of gold and silver nanoclusters as claimed in claim 1, wherein the preparation of the gold and silver nanoclusters labeled neuron-specific enolase detection antibody solution is characterized in that: Here are the steps: (1) Preparation of gold and silver nanoclusters 4 mL of 5-15 mmol / L chloroauric acid solution and 1 mL of 2-10 mmol / L silver nitrate solution were added to 5 mL of freshly prepared 5-15 mmol / L glutathione GSH solution, 10 μL of 1-5 mol / L sodium hydroxide solution was added dropwise to dissolve the precipitate, the mixed solution was heated at 70-95°C with gentle stirring for 4-24 h, cooled to room temperature, dialyzed and purified for 24 h, then washed with a water / acetonitrile mixed solution with a volume ratio of 1:3, dried at 60°C for 12 h, and gold-silver nanoclusters were obtained, which were stored in a refrigerator at 4°C for later use; (2) Preparation of gold-silver nanocluster labeled neuron-specific enolase detection antibody solution 1-5 mol / L 1-ethyl-3-dimethylaminopropylcarbodiimide and 0.1-1 mol / L N-hydroxysuccinimide were mixed with 1 mL of the gold-silver nanoclusters prepared above, incubated at 4°C for 5-10 hours, centrifuged at 12000 rpm, the above solution was separated, 100-500 μL of neuron-specific enolase detection antibody solution was added, and shaken at room temperature for 10-40 minutes to obtain a neuron-specific enolase detection antibody solution labeled with gold-silver nanoclusters.

4. A detection method for a sensor prepared by the preparation method according to claim 1, characterized in that: For the detection of neuron-specific enolase, the steps are as follows: (1) The test was performed using an electrochemical workstation with a three-electrode system, with an Ag / AgCl electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, the prepared immunosensor based on gold-silver nanocluster aggregation-induced luminescence as the working electrode, the high voltage of the photomultiplier tube set to 500 V, the scanning potential of 0-1.2 V, and the scanning rate of 0.1 V / s; (2) In 10 mL of phosphate buffer solution containing 100 mmol / L triethylamine at pH 7.38, the electrochemiluminescence signal intensity generated by the antigen at different concentrations is detected by an electrochemiluminescence system, and a working curve is drawn; (3) replacing the neuron-specific enolase antigen solution with the test sample solution for testing; (4) Using the working curve method, the concentration of neuron-specific enolase in the sample to be tested is calculated.