Stress migration test structure and stress migration test method

By designing a stress migration test structure for the lower and upper via connection layers with different line widths, the stress migration failure in the bottom and conductive plugs can be tested simultaneously, solving the problem of incomplete evaluation in the prior art and improving the improvement of the problem of improving the The integrity of reliability assessment is achieved.

CN115377069BActive Publication Date: 2024-11-12WUHAN XINXIN SEMICON MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211159646.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-22
Publication Date
2024-11-12
Estimated Expiration
2042-09-22

AI Technical Summary

Technical Problem

The existing stress migration test structures cannot simultaneously test stress migration failures in the bottom of the conductive plug and in the conductive plug, resulting in incomplete assessment of the reliability of the metal interconnect structure.

Method used

A stress migration test structure was designed, including a lower through-hole connection layer and an upper through-hole connection layer. The bottom and top of the conductive plug are connected to the lower and upper connecting layers respectively. The lower voltage and current test pads are respectively connected to the lower through-holes. The connection layer end is connected, the upper voltage and current test pads are connected to the upper through-hole connection layer respectively. The line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer. By measuring the change of resistance value, the stress migration failure is judged. .

Benefits of technology

Simultaneous testing of stress migration failures in the bottom and in the conductive plug is achieved, improving the integrity of the assessment of the reliability of metal interconnect structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115377069B_ABST
    Figure CN115377069B_ABST
Patent Text Reader

Abstract

The present invention provides a stress migration test structure and a stress migration test method, wherein the stress migration test structure comprises at least one test structure, wherein the test structure comprises: a lower through-hole connection layer; an upper through-hole connection layer, located above the lower through-hole connection layer; a conductive plug, wherein the bottom and the top of the conductive plug are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer, and the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer; a lower voltage test pad and a lower current test pad, respectively connected to the two ends of the lower through-hole connection layer; an upper voltage test pad and an upper current test pad, respectively connected to the two ends of the upper through-hole connection layer. The technical solution of the present invention can simultaneously test stress migration failures in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability assessment more complete.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a stress migration test structure and a stress migration test method. Background Art

[0002] Stress migration (SM) is one of the important test items for evaluating the reliability of metal interconnect structures in semiconductor processes. Stress migration is a physical phenomenon in which stress is formed between materials due to the different thermal expansion coefficients of various materials at high temperatures, causing small gaps between grains in the metal interconnect structure to gather to the place where stress is concentrated to form voids. Stress migration leads to increased resistance, and the voids formed by stress migration will cause the metal interconnect structure to break when reaching a certain level.

[0003] like Figure 1a and Figure 1b As shown, the metal interconnection structure includes a first metal layer, a second metal layer and a conductive plug 13 connecting the first metal layer and the second metal layer, the first metal layer and the second metal layer are located in different layers, the first metal layer includes a first through-hole connection layer 11 and a first current test terminal F1 and a first voltage test terminal S1 connected to the first through-hole connection layer 11, the second metal layer includes a second through-hole connection layer 12 and a second current test terminal F2 and a second voltage test terminal S2 connected to the second through-hole connection layer 12, the top and bottom of the conductive plug 13 are respectively connected to the second through-hole connection layer 12 and the first through-hole connection layer 11, the first through-hole connection layer 11 and the second through-hole connection layer 12 have the same line width, wherein the cross-section of the first through-hole connection layer 11 and the second through-hole connection layer 12 can be a rectangle or a square, and the length of the short side of the rectangle and the side length of the square are the line width. Among them, during the stress release process, when the line width of the metal interconnection structure is large (the line width of the first through-hole connection layer 11 is also large), voids are most likely to form in the first through-hole connection layer 11 at the bottom of the conductive plug 13, and the larger the line width of the metal interconnection structure, the more obvious the stress migration, and the larger the void in the first through-hole connection layer 11; as the feature size of the semiconductor process continues to shrink, the line width of the metal interconnection structure continues to decrease (the line width of the second through-hole connection layer 12 also decreases), and voids will also form in the conductive plug 13, and under high-temperature baking, stress migration causes the void to further increase.

[0004] but, Figure 1a and Figure 1b The metal interconnect structure shown as a stress test structure cannot simultaneously test stress failures in the first via connection layer 11 at the bottom of the conductive plug 13 and in the conductive plug 13 , resulting in incomplete reliability evaluation.

[0005] Therefore, it is necessary to improve the stress migration test structure and the stress migration test method to solve the above problems. Summary of the invention

[0006] The purpose of the present invention is to provide a stress migration test structure and a stress migration test method, which can simultaneously test the stress migration failure in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability evaluation more complete.

[0007] To achieve the above object, the present invention provides a stress migration test structure, including at least one test structure, wherein the test structure includes:

[0008] The lower through-hole connection layer;

[0009] An upper through-hole connection layer, located above the lower through-hole connection layer;

[0010] A conductive plug, wherein the bottom and the top of the conductive plug are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer, and the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer;

[0011] A lower voltage test pad and a lower current test pad are respectively connected to two ends of the lower through-hole connection layer;

[0012] The upper voltage test pad and the upper current test pad are respectively connected to the two ends of the upper through-hole connection layer.

[0013] Optionally, when the stress migration test structure includes at least two test structures, the lower through-hole connection layers in two adjacent test structures are connected, and two adjacent lower through-hole connection layers are connected to the same lower voltage test pad or the lower current test pad.

[0014] Optionally, when the stress migration test structure includes at least two test structures, all of the lower through-hole connection layers have the same extension direction, and at least two of the upper through-hole connection layers have different extension directions.

[0015] Optionally, all the lower through-hole connection layers extend in a first direction, at least one of the upper through-hole connection layers extends in the first direction, at least one of the upper through-hole connection layers extends in a second direction, and the first direction is perpendicular to the second direction.

[0016] Optionally, the line width of the lower through-hole connection layer is 8 to 12 times the line width of the upper through-hole connection layer.

[0017] Optionally, the test structure also includes a plurality of connecting metal wires, and the lower voltage test pad, the lower current test pad and the lower through-hole connection layer, the upper voltage test pad, the upper current test pad and the upper through-hole connection layer, and adjacent lower through-hole connection layers are all connected by the connecting metal wires.

[0018] The present invention also provides a stress migration testing method, comprising:

[0019] Providing a test sample comprising the stress migration test structure;

[0020] Testing the resistance value of the stress migration test structure before and after baking to obtain the resistance offset value before and after baking;

[0021] It is determined whether the resistance offset value exceeds a set specification.

[0022] Optionally, the step of obtaining the resistance offset value before and after baking includes:

[0023] Connecting the lower voltage test pad to a first voltage, the lower current test pad to a current, and the upper current test pad to a low voltage, so as to measure the voltage of the upper voltage test pad as a second voltage, and dividing the difference between the first voltage and the second voltage by the current to obtain an initial resistance value;

[0024] baking the test sample;

[0025] Connecting the lower voltage test pad to the first voltage, the lower current test pad to the current, and the upper current test pad to a low voltage, so as to measure the voltage of the upper voltage test pad as a third voltage, and dividing the difference between the first voltage and the third voltage by the current to obtain a test resistance value;

[0026] A change of the test resistance value based on the initial resistance value is calculated to obtain the resistance shift value.

[0027] Optionally, the step of obtaining the resistance offset value before and after baking includes:

[0028] Connecting the lower current test pad to a first current, connecting the upper current test pad to a second current, measuring the voltage of the lower voltage test pad as a first voltage and the voltage of the upper voltage test pad as a second voltage, and dividing the difference between the first voltage and the second voltage by the difference between the first current and the second current to obtain an initial resistance value;

[0029] baking the test sample;

[0030] Connecting the lower current test pad to the first current, connecting the upper current test pad to the second current, measuring the voltage of the lower voltage test pad as a third voltage and the voltage of the upper voltage test pad as a fourth voltage, and dividing the difference between the third voltage and the fourth voltage by the difference between the first current and the second current to obtain a test resistance value;

[0031] A change of the test resistance value based on the initial resistance value is calculated to obtain the resistance shift value.

[0032] Optionally, when the stress migration test structure includes at least two test structures, the resistance values ​​of different test structures before and after baking are tested in sequence to obtain the resistance offset values ​​of different test structures.

[0033] Optionally, when the stress migration test structure includes at least two test structures, and at least two of the upper through-hole connection layers have different extension directions, the resistance offset value exceeds the process abnormality in the vertical direction of the extension direction of the upper through-hole connection layer in the test structure corresponding to the set specification.

[0034] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0035] 1. The stress migration test structure of the present invention comprises at least one test structure, which comprises: a lower through-hole connection layer; an upper through-hole connection layer, located above the lower through-hole connection layer; a conductive plug, the bottom and top of which are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer, and the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer; a lower voltage test pad and a lower current test pad, respectively connected to the two ends of the lower through-hole connection layer; an upper voltage test pad and an upper current test pad, respectively connected to the two ends of the upper through-hole connection layer. The stress migration test structure provided by the present invention can simultaneously test stress migration failures in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability assessment more complete.

[0036] 2. The stress migration test method of the present invention comprises: providing a test sample including the stress migration test structure; testing the resistance value of the stress migration test structure before and after baking to obtain the resistance offset value before and after baking; and judging whether the resistance offset value exceeds the set specification. The stress migration test method provided by the present invention can simultaneously test the stress migration failure in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability assessment more complete. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1ais a schematic top view of a stress migration test structure;

[0038] Figure 1b yes Figure 1a A schematic cross-sectional view of the stress migration test structure along AA' is shown;

[0039] Figure 2a is a schematic top view of a stress migration test structure according to an embodiment of the present invention;

[0040] Figure 2b yes Figure 2a The schematic cross-sectional view of the stress migration test structure along BB' is shown;

[0041] Figure 3a is a schematic top view of a stress migration test structure according to another embodiment of the present invention;

[0042] Figure 3b yes Figure 3a A schematic cross-sectional view of the stress migration test structure along CC' is shown;

[0043] Figure 4 FIG. 4 is a flow chart of a stress migration testing method according to an embodiment of the present invention.

[0044] Among them, Figure 1a to Figure 4 The reference numerals are described as follows:

[0045] 11-first through-hole connection layer; 12-second through-hole connection layer; 13-conductive plug; 211-lower through-hole connection layer; 221-upper through-hole connection layer; 231-conductive plug; 241-lower current test pad; 242-upper current test pad; 251-lower voltage test pad; 252-upper voltage test pad; 261-first connection metal wire; 262-second connection metal wire; 311-first lower through-hole connection layer; 312-second lower through-hole connection layer; 321-first Upper through-hole connection layer; 322-second upper through-hole connection layer; 331-first conductive plug; 332-second conductive plug; 341-first lower current test pad; 342-first upper current test pad; 343-second lower current test pad; 344-second upper current test pad; 351-first lower voltage test pad; 352-first upper voltage test pad; 353-second upper voltage test pad; 361-first connecting metal wire; 362-second connecting metal wire. DETAILED DESCRIPTION

[0046] In order to make the purpose, advantages and features of the present invention clearer, the stress migration test structure and stress migration test method proposed in the present invention are further described in detail below. It should be noted that the drawings are all in a very simplified form and are not in precise proportions, which are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0047] An embodiment of the present invention provides a stress migration test structure, comprising at least one test structure, wherein the test structure comprises: a lower through-hole connection layer; an upper through-hole connection layer, located above the lower through-hole connection layer; a conductive plug, wherein the bottom and top of the conductive plug are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer, and the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer; a lower voltage test pad and a lower current test pad, respectively connected to the two ends of the lower through-hole connection layer; and an upper voltage test pad and an upper current test pad, respectively connected to the two ends of the upper through-hole connection layer.

[0048] See below Figure 2a to Figure 2b and Figure 3a to Figure 3b The stress migration test structure provided in this embodiment is described in detail.

[0049] The stress migration test structure includes at least one test structure, each of which includes a lower through-hole connection layer, an upper through-hole connection layer, a conductive plug, a lower voltage test pad, a lower current test pad, an upper voltage test pad and an upper current test pad.

[0050] In each of the test structures, the upper through-hole connection layer is located above the lower through-hole connection layer, and the bottom and top of the conductive plug are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer; the lower voltage test pad and the lower current test pad are respectively connected to the two ends of the lower through-hole connection layer; the upper voltage test pad and the upper current test pad are respectively connected to the two ends of the upper through-hole connection layer.

[0051] The stress migration test structure can be located in the cutting path of the wafer, and the cutting path is located at the periphery of the chip area. After cutting along the cutting path, the chip can be obtained. The stress migration test structure does not occupy the area of ​​the chip area to avoid affecting the wiring design of the chip area, thereby avoiding affecting the performance of the chip and increasing the production cost.

[0052] The wafer may include a substrate and a dielectric layer formed on the substrate, the lower through-hole connection layer, the upper through-hole connection layer and the conductive plug may be located in the dielectric layer, and the lower voltage test pad, the lower current test pad, the upper voltage test pad and the upper current test pad may all be located on the surface of the dielectric layer, so that the probe on the test machine can be used to contact the lower voltage test pad, the lower current test pad, the upper voltage test pad and the upper current test pad for testing. It should be noted that Figure 2a to Figure 2b and Figure 3a to Figure 3b The substrate and dielectric layer are not shown.

[0053] In the following embodiments, when the stress migration test structure includes at least two test structures, all of the lower through-hole connection layers can be located on the same layer, all of the upper through-hole connection layers can be located on the same layer above the lower through-hole connection layers, and all of the conductive plugs can be located together in the same dielectric layer or in at least two dielectric layers.

[0054] When the stress migration test structure includes at least two test structures, the two lower through-hole connection layers in the two adjacent test structures are connected, and the adjacent ends of the two lower through-hole connection layers in the two adjacent test structures are connected to the same lower voltage test pad or the lower current test pad, that is, the adjacent ends of the two lower through-hole connection layers in the two adjacent test structures share the same lower voltage test pad or the lower current test pad, so that while meeting the test requirements, the composition of the stress migration test structure can be simplified and space can be saved. Wherein, if the adjacent ends of the two lower through-hole connection layers in the two adjacent test structures are connected to the same lower voltage test pad, the other ends of the two lower through-hole connection layers in the two adjacent test structures that are far away are respectively connected to different lower current test pads; if the adjacent ends of the two lower through-hole connection layers in the two adjacent test structures are connected to the same lower current test pad, the other ends of the two lower through-hole connection layers in the two adjacent test structures that are far away are respectively connected to different lower voltage test pads.

[0055] The test structure further includes a plurality of connecting metal wires, and the lower voltage test pad and the lower current test pad are connected to the lower through-hole connection layer, the upper voltage test pad and the upper current test pad are connected to the upper through-hole connection layer, and the adjacent lower through-hole connection layers are connected by the connecting metal wires. It should be noted that the extension length and extension path of the connecting metal wires are not limited.

[0056] The line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer, and the projection of the upper through-hole connection layer in the direction perpendicular to the substrate may be partially or completely located within the range of the lower through-hole connection layer. Preferably, the line width of the lower through-hole connection layer is 8 to 12 times the line width of the upper through-hole connection layer. The line width of the upper through-hole connection layer may preferably be 50 nm to 100 nm, but other values ​​may also be selected according to process requirements.

[0057] Preferably, the cross-sectional shape of the lower through-hole connection layer and the upper through-hole connection layer is a rectangle, in which case the line widths of the lower through-hole connection layer and the upper through-hole connection layer are respectively the lengths of the short sides of the corresponding rectangles, and the long sides of the rectangles are the extension directions of the lower through-hole connection layer and the upper through-hole connection layer. It should be noted that, in other embodiments, the shape of the lower through-hole connection layer and the upper through-hole connection layer may be a square, in which case the line widths of the lower through-hole connection layer and the upper through-hole connection layer are respectively the side lengths of the corresponding squares.

[0058] And, preferably, the line width of the connecting metal line is equal to the line width of the upper through-hole connecting layer.

[0059] If the lower through-hole connection layer has a large line width, stress migration can easily lead to the formation of voids in the lower through-hole connection layer at the bottom of the conductive plug, thereby increasing resistance.

[0060] When forming the conductive plug and the upper through-hole connection layer, a through-hole exposing part of the surface of the lower through-hole connection layer can be formed in the dielectric layer, and a groove connected to the through-hole can be formed on the top of the through-hole, and then a seed layer is deposited on the inner surface of the through-hole and the groove by a physical vapor deposition process, and a metal is continuously grown on the surface of the seed layer by an electrochemical plating process to fill the through-hole and the groove, thereby forming the conductive plug in the through-hole and the upper through-hole connection layer in the groove. If the width of the groove is very small, the diameter of the through-hole is also very small, and the depth of the through-hole itself is deep, part of the side wall of the through-hole cannot be deposited on the seed layer, so that the area where the seed layer is not deposited cannot be electroplated with metal, thereby forming a void in the conductive plug. Therefore, if the upper through-hole connection layer has a very small line width, a void will be formed in the conductive plug, and stress migration will further increase the void, thereby increasing resistance.

[0061] Therefore, in this embodiment, the line width of the lower through-hole connection layer is designed to be larger than the line width of the upper through-hole connection layer, so that the lower through-hole connection layer at the bottom of the conductive plug can have a large line width, while the upper through-hole connection layer at the top of the conductive plug can have a very small line width, thereby making it possible to simultaneously test the stress migration failure in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability evaluation more complete.

[0062] Preferably, when the stress migration test structure includes at least two of the test structures, all of the lower through-hole connection layers have the same extension direction, and at least two of the upper through-hole connection layers have different extension directions, so that the direction source of the process causing the stress migration failure can be determined based on the extension direction of the upper through-hole connection layer in the test structure where the stress migration failure occurs, thereby quickly clarifying the adjustment direction of the process and the machine.

[0063] Wherein, the extension direction of all the lower through-hole connection layers may be the first direction, the extension direction of at least one of the upper through-hole connection layers may be the first direction, the extension direction of at least one of the upper through-hole connection layers may be the second direction, and the first direction is perpendicular to the second direction. In other embodiments, the angle between the extension direction of all the lower through-hole connection layers and the extension direction of at least one of the upper through-hole connection layers may be 45°, etc.

[0064] For example, if the extension direction of the upper through-hole connection layer in the test structure that has stress failure is the first direction, the process parameters on the process machine regarding the second direction (i.e., the direction perpendicular to the first direction) can be adjusted (for example, adjusting the power and other parameters of the etching machine or deposition machine in the second direction).

[0065] In addition, when it is tested that stress migration failure occurs in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, the stress test structure can be further sliced ​​to confirm whether the failure position is located in the lower through-hole connection layer at the bottom of the conductive plug or in the conductive plug.

[0066] Below Figure 2a to Figure 2b The illustrated embodiment provides a detailed description of the stress migration test structure, which includes one test structure.

[0067] The test structure includes a lower through-hole connection layer 211, an upper through-hole connection layer 221, a conductive plug 231, a lower current test pad 241, a lower voltage test pad 251, an upper current test pad 242 and an upper voltage test pad 252. The bottom and top of the conductive plug 231 are respectively connected to the lower through-hole connection layer 211 and the upper through-hole connection layer 221, the lower voltage test pad 251 and the lower current test pad 241 are respectively connected to the two ends of the lower through-hole connection layer 211, and the upper voltage test pad 252 and the upper current test pad 242 are respectively connected to the two ends of the upper through-hole connection layer 221.

[0068] The test structure also includes multiple first connecting metal wires 261 and multiple second connecting metal wires 262. The lower layer voltage test pad 251 and the lower layer current test pad 241 are connected to the lower layer through-hole connection layer 211 through the first connecting metal wires 261; the upper layer voltage test pad 252 and the upper layer current test pad 242 are connected to the upper layer through-hole connection layer 221 through the second connecting metal wires 262.

[0069] In this embodiment, the cross-sectional shapes of the lower through-hole connection layer 211 and the upper through-hole connection layer 221 are both rectangles, the long side of the rectangle is the extension direction, the extension direction of the lower through-hole connection layer 211 is the X direction, the extension direction of the upper through-hole connection layer 221 is the Y direction, and the X direction is perpendicular to the Y direction; the line width of the lower through-hole connection layer 211 is the length of the short side of the rectangle (that is, the length of the lower through-hole connection layer 211 in the Y direction), the line width of the upper through-hole connection layer 221 is the length of the short side of the rectangle (that is, the length of the upper through-hole connection layer 221 in the X direction), and the line width of the lower through-hole connection layer 211 is greater than the line width of the upper through-hole connection layer 221.

[0070] When the lower through-hole connection layer 211 has a large line width, stress migration can easily lead to the formation of voids in the lower through-hole connection layer 211 at the bottom of the conductive plug 231, thereby increasing resistance; when the upper through-hole connection layer 221 has a small line width, voids will be formed in the conductive plug 231, and stress migration will further increase the voids, thereby increasing resistance. Therefore, in this embodiment, by designing the line width of the lower through-hole connection layer 211 to be larger than the line width of the upper through-hole connection layer 221, the lower through-hole connection layer 211 at the bottom of the conductive plug 231 can have a large line width, while the upper through-hole connection layer 221 at the top of the conductive plug 231 can have a small line width, thereby enabling the stress migration failures in the lower through-hole connection layer 211 at the bottom of the conductive plug 231 and in the conductive plug 231 to be tested simultaneously, thereby making the reliability evaluation more complete.

[0071] In addition, if Figure 3a to Figure 3b In the illustrated embodiment, the stress migration test structure includes two test structures. It should be noted that, for ease of description, the two lower through-hole connection layers, the two upper through-hole connection layers, the two conductive plugs, the two lower current test pads, the two upper current test pads and the two upper voltage test pads in the two test structures are all named differently and labeled differently.

[0072] exist Figure 3a to Figure 3bIn one embodiment, one of the test structures comprises a first lower through-hole connection layer 311, a first upper through-hole connection layer 321, a first conductive plug 331, a first lower current test pad 341, a first lower voltage test pad 351, a first upper current test pad 342 and a first upper voltage test pad 352, the bottom and top of the first conductive plug 331 are respectively connected to the first lower through-hole connection layer 311 and the first upper through-hole connection layer 321, the first lower voltage test pad 351 and the first lower current test pad 341 are respectively connected to the two ends of the first lower through-hole connection layer 311, the first upper voltage test pad 352 and the first upper current test pad 342 are respectively connected to the two ends of the first upper through-hole connection layer 321; the other test structure comprises a second lower through-hole connection layer 312, a second upper through-hole connection layer 322, a second conductive plug 332, a second A lower layer current test pad 343, a first lower layer voltage test pad 351, a second upper layer current test pad 344 and a second upper layer voltage test pad 353, the bottom and top of the second conductive plug 332 are respectively connected to the second lower layer through-hole connection layer 312 and the second upper layer through-hole connection layer 322, the first lower layer voltage test pad 351 and the second lower layer current test pad 343 are respectively connected to the two ends of the second lower layer through-hole connection layer 312, the second upper layer voltage test pad 353 and the second upper layer current test pad 344 are respectively connected to the two ends of the second upper layer through-hole connection layer 322; the first lower layer through-hole connection layer 311 and the second lower layer through-hole connection layer 312 in the two test structures are connected, and the end close to the first lower layer through-hole connection layer 311 and the second lower layer through-hole connection layer 312 in the two test structures is connected to the same first lower layer voltage test pad 351.

[0073] The test structure also includes multiple first connecting metal wires 361 and multiple second connecting metal wires 362, and the first lower layer voltage test pad 351 and the first lower layer current test pad 341 are connected to the first lower layer through-hole connection layer 311, the first lower layer voltage test pad 351 and the second lower layer current test pad 343 are connected to the second lower layer through-hole connection layer 312, and the first lower layer through-hole connection layer 311 and the second lower layer through-hole connection layer 312 are all connected through the first connecting metal wires 361; the first upper layer voltage test pad 352 and the first upper layer current test pad 342 are connected to the first upper layer through-hole connection layer 321, and the second upper layer voltage test pad 353 and the second upper layer current test pad 344 are connected to the second upper layer through-hole connection layer 322.

[0074] The cross-sectional shapes of the first lower through-hole connection layer 311, the first upper through-hole connection layer 321, the second lower through-hole connection layer 312 and the second upper through-hole connection layer 322 are all rectangular; the long side of the rectangle is the extension direction, the extension direction of the first lower through-hole connection layer 311, the second lower through-hole connection layer 312 and the second upper through-hole connection layer 322 is the X direction, the extension direction of the first upper through-hole connection layer 321 is the Y direction, and the X direction is perpendicular to the Y direction. straight; the length of the short side of the rectangle is the line width, the length of the first lower through-hole connection layer 311, the second lower through-hole connection layer 312 and the second upper through-hole connection layer 322 in the Y direction is the line width, the length of the first upper through-hole connection layer 321 in the X direction is the line width, the line width of the first lower through-hole connection layer 311 is greater than the line width of the first upper through-hole connection layer 321, and the line width of the second lower through-hole connection layer 312 is greater than the line width of the second upper through-hole connection layer 322.

[0075] and Figure 2a to Figure 2b The embodiment shown is similar, in Figure 3a to Figure 3b In the illustrated embodiment, by designing the line width of the first lower through-hole connection layer 311 to be larger than the line width of the first upper through-hole connection layer 321, stress migration failures in the first lower through-hole connection layer 311 at the bottom of the first conductive plug 331 and in the first conductive plug 331 can be tested simultaneously; and by designing the line width of the second lower through-hole connection layer 312 to be larger than the line width of the second upper through-hole connection layer 322, stress migration failures in the second lower through-hole connection layer 312 at the bottom of the second conductive plug 332 and in the second conductive plug 332 can be tested simultaneously.

[0076] And, in Figure 3a to Figure 3bIn the embodiment shown, since the extension direction of the first upper through-hole connection layer 321 is the Y direction, the length of the groove corresponding to the first upper through-hole connection layer 321 in the Y direction (i.e., the length of the long side of the rectangular first upper through-hole connection layer 321) is very long and the length in the X direction (i.e., the length of the short side of the rectangular first upper through-hole connection layer 321) is very short, resulting in that when the seed crystal is deposited in the through hole at the bottom of the groove (i.e., the through hole corresponding to the first conductive plug 331), the seed crystal is easily deposited in the through hole along the Y direction, but the seed crystal is difficult to be deposited in the through hole along the X direction, which leads to the through hole in the X direction. The amount of seed crystals on the through hole is too small or even no seed crystals are deposited on part of the sidewalls of the through hole in the X direction, which leads to the risk of defects in the structure filled in the first conductive plug 331 or even direct voids, which leads to stress migration failure in the first conductive plug 331 when performing the stress migration test; similarly, since the extension direction of the second upper through hole connection layer 322 is the X direction, the seed crystals are easily deposited in the through hole corresponding to the second conductive plug 332 along the X direction, but the seed crystals are difficult to be deposited in the through hole along the Y direction, which leads to stress migration failure in the second conductive plug 332 when performing the stress migration test. Therefore, if the test shows that there is stress migration failure in the first conductive plug 331, the process and machine in the X direction need to be adjusted; if the test shows that there is stress migration failure in the second conductive plug 332, the process and machine in the Y direction need to be adjusted.

[0077] Taking the adjustment of the process and machine in the X direction as an example, specifically, the deposition power when depositing the seed crystal in the X direction can be adjusted, and the deposition time can be adjusted to improve the effect of depositing the seed crystal in the X direction; or, when etching to form the groove corresponding to the first upper through-hole connection layer 321, the morphology of the etched groove can be adjusted (for example, the opening width of the groove in the X direction is increased); or, when etching to form the through hole corresponding to the first conductive plug 331, the morphology of the etched through hole can be adjusted (the opening width of the through hole in the X direction is increased). Through the above adjustment, the amount of seed crystal deposited in the through hole in the X direction is increased, thereby avoiding the risk of defects in the structure filled in the first conductive plug 331, and further avoiding stress migration failure in the first conductive plug 331 when performing the stress migration test.

[0078] In summary, the present invention provides a stress migration test structure, including at least one test structure, the test structure including: a lower through-hole connection layer; an upper through-hole connection layer, located above the lower through-hole connection layer; a conductive plug, the bottom and top of the conductive plug are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer, the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer; a lower voltage test pad and a lower current test pad, respectively connected to the two ends of the lower through-hole connection layer; an upper voltage test pad and an upper current test pad, respectively connected to the two ends of the upper through-hole connection layer. The stress migration test structure provided by the present invention can simultaneously test stress migration failures in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability assessment more complete.

[0079] Based on the same inventive concept, an embodiment of the present invention provides a stress migration test method, see Figure 4 ,from Figure 4 It can be seen that the stress migration test method includes:

[0080] Step S1, providing a test sample including the stress migration test structure;

[0081] Step S2, testing the resistance value of the stress migration test structure before and after baking to obtain the resistance offset value before and after baking;

[0082] Step S3, determining whether the resistance offset value exceeds a set specification.

[0083] The electromigration testing method provided in this embodiment is described in detail below.

[0084] According to step S1, a test sample including the stress migration test structure of the present invention is provided.

[0085] The stress migration test structure can be referred to the detailed description of the stress migration test structure of the present invention, which will not be described in detail here.

[0086] According to step S2, the resistance value of the stress migration test structure before and after baking is tested to obtain the resistance offset value before and after baking.

[0087] Wherein, the method for obtaining the resistance offset value before and after baking may include: first, connecting the lower voltage test pad to a first voltage, the lower current test pad to a current, and the upper current test pad to a low voltage, so as to measure the voltage of the upper voltage test pad as a second voltage, and dividing the difference between the first voltage and the second voltage by the current to obtain an initial resistance value; then, baking the test sample; then, connecting the lower voltage test pad to the first voltage, the lower current test pad to the current, and the upper current test pad to the low voltage, so as to measure the voltage of the upper voltage test pad as a third voltage, and dividing the difference between the first voltage and the third voltage by the current to obtain a test resistance value; then, calculating the change of the test resistance value based on the initial resistance value to obtain the resistance offset value. Wherein, the low voltage connected to the upper current test pad may be grounded.

[0088] Alternatively, the method for obtaining the resistance offset value before and after baking may include: first, connecting the lower current test pad to a first current, connecting the upper current test pad to a second current, measuring the voltage of the lower voltage test pad as a first voltage and the voltage of the upper voltage test pad as a second voltage, dividing the difference between the first voltage and the second voltage by the difference between the first current and the second current to obtain an initial resistance value; then, baking the test sample; then, connecting the lower current test pad to the first current, connecting the upper current test pad to the second current, measuring the voltage of the lower voltage test pad as a third voltage and the voltage of the upper voltage test pad as a fourth voltage, dividing the difference between the third voltage and the fourth voltage by the difference between the first current and the second current to obtain a test resistance value; then, calculating the change of the test resistance value based on the initial resistance value to obtain the resistance offset value. Among them, the first current is greater than the second current, at this time, the measured first voltage is greater than the second voltage, and the third voltage is greater than the fourth voltage; or, the first current is less than the second current, at this time, the measured first voltage is less than the second voltage, and the third voltage is less than the fourth voltage.

[0089] In the above-mentioned method for obtaining the resistance offset value before and after baking, the former method uses a single-ended current supply method (i.e., current is input only through the lower current test pad) to obtain the initial resistance value and the test resistance value, and the latter method uses a double-ended current supply method (i.e., current is input to both the lower current test pad and the upper current test pad) to obtain the initial resistance value and the test resistance value. Compared with the single-ended current supply method, which causes a small amount of current to be shunted to the outside of the test structure, the double-ended current supply method directly uses the current difference input at both ends as the current of the test structure itself, which makes the calculation of the initial resistance value and the test resistance value more accurate.

[0090] When the test sample is baked, the baking temperature may be 175° C. to 225° C., and the baking time may be 168 h, 500 h, or 1000 h, etc.

[0091] Furthermore, when the stress migration test structure includes at least two test structures, the resistance values ​​of different test structures before and after baking are tested in sequence to obtain the resistance offset values ​​of different test structures.

[0092] Among them, the test before and after baking Figure 2a to Figure 2b The resistance value of the stress migration test structure shown in the figure, to obtain the resistance offset value before and after baking, can include the following steps: first, connecting the lower voltage test pad 251 to a first voltage, the lower current test pad 241 to a current, and the upper current test pad 242 to a low voltage, so as to measure the voltage of the upper voltage test pad 252 as a second voltage, and divide the difference between the first voltage and the second voltage by the current to obtain an initial resistance value; then, baking the test sample; then, connecting the lower voltage test pad 251 to the first voltage, the lower current test pad 241 to the current, and the upper current test pad 242 to the low voltage, so as to measure the voltage of the upper voltage test pad 252 as a third voltage, and divide the difference between the first voltage and the third voltage by the current to obtain a test resistance value; then, calculating the change of the test resistance value based on the initial resistance value to obtain the resistance offset value of the test structure.

[0093] Alternatively, test before and after baking Figure 2a to Figure 2bThe resistance value of the stress migration test structure shown in the figure, to obtain the resistance offset value before and after baking, can include: first, connecting the lower current test pad 241 to the first current, connecting the upper current test pad 242 to the second current, and measuring the voltage of the lower voltage test pad 251 as the first voltage and the voltage of the upper voltage test pad 252 as the second voltage, dividing the difference between the first voltage and the second voltage by the difference between the first current and the second current to obtain the initial resistance value; then, baking the test sample; then, connecting the lower current test pad 241 to the first current, connecting the upper current test pad 242 to the second current, and measuring the voltage of the lower voltage test pad 251 as the third voltage and the voltage of the upper voltage test pad 252 as the fourth voltage, dividing the difference between the third voltage and the fourth voltage by the difference between the first current and the second current to obtain the test resistance value; then, calculating the change of the test resistance value based on the initial resistance value to obtain the resistance offset value of the test structure.

[0094] Among them, Figure 3a to Figure 3bTaking the stress migration test structure shown as an example, the steps of obtaining the resistance offset values ​​of different test structures may include: first, connecting the first lower voltage test pad 351 to a first voltage V1, the first lower current test pad 341 to a current I1, and the first upper current test pad 342 to a low voltage to measure the voltage of the first upper voltage test pad 352 as a second voltage V11, and dividing the difference between the first voltage V1 and the second voltage V11 by the current I1 to obtain a first initial resistance value; and connecting the first lower voltage test pad 351 to a first voltage V1, the second lower current test pad 343 to a current I1, and the second upper current test pad 344 to a low voltage to measure the voltage of the second upper voltage test pad 353 as a second voltage V12, and dividing the difference between the first voltage V1 and the second voltage V12 by the current I1 to obtain a second initial resistance value; then, baking the test sample; then, connecting the first lower voltage test pad 351 to the first voltage V1, and connecting the first lower current test pad 343 to the current I1, and connecting the second upper current test pad 344 to a low voltage to measure the voltage of the second upper voltage test pad 353 as a second voltage V12, and dividing the difference between the first voltage V1 and the second voltage V12 by the current I1 to obtain a second initial resistance value. voltage V1, the first lower current test pad 341 is connected to the current I1, and the first upper current test pad 342 is connected to the low voltage to measure the voltage of the first upper voltage test pad 352 as the third voltage V13, and the difference between the first voltage V1 and the third voltage V13 is divided by the current I1 to obtain a first test resistance value; and, the first lower voltage test pad 351 is connected to the first voltage V1, the second lower current test pad 343 is connected to the current I1, and the second upper current test pad 344 is connected to the low voltage to measure the voltage of the second upper voltage test pad 353 as the third voltage V14, and the difference between the first voltage V1 and the third voltage V14 is divided by the current I1 to obtain a second test resistance value; then, the change of the first test resistance value based on the first initial resistance value is calculated to obtain a first resistance offset value of one of the test structures, and the change of the second test resistance value based on the second initial resistance value is calculated to obtain a second resistance offset value of another test structure.

[0095] Alternatively, the step of obtaining the resistance offset value of the different test structures may include: first, connecting the first lower current test pad 341 to the first current I21, connecting the first upper current test pad 342 to the second current I22, and measuring the voltage of the first lower voltage test pad 351 as the first voltage V21 and the voltage of the first upper voltage test pad 352 as the second voltage V22, dividing the difference between the first voltage V21 and the second voltage V22 by the difference between the first current I21 and the second current I22 to obtain a first initial resistance value; and The lower current test pad 343 is connected to the first current I21, the second upper current test pad 344 is connected to the second current I22, and the voltage of the first lower voltage test pad 351 is measured as the first voltage V23 and the voltage of the second upper voltage test pad 353 is measured as the second voltage V24, and the difference between the first voltage V23 and the second voltage V24 is divided by the difference between the first current I21 and the second current I22 to obtain a second initial resistance value; then, the test sample is baked; then, the first lower current test pad 341 is connected to the first current I21, the first ... An upper current test pad 342 is connected to the second current I22, and the voltage of the first lower voltage test pad 351 is measured as the third voltage V31 and the voltage of the first upper voltage test pad 352 is measured as the fourth voltage V32, and the difference between the third voltage V31 and the fourth voltage V32 is divided by the difference between the first current I21 and the second current I22 to obtain a first test resistance value; and the second lower current test pad 343 is connected to the first current I21, the second upper current test pad 344 is connected to the second current I22, and the first lower current is measured. The voltage of the pressure test pad 351 is used as the third voltage V33 and the voltage of the second upper voltage test pad 353 is used as the fourth voltage V34, and the difference between the third voltage V33 and the fourth voltage V34 is divided by the difference between the first current I21 and the second current I22 to obtain a second test resistance value; then, the change of the first test resistance value based on the first initial resistance value is calculated to obtain a first resistance offset value of one of the test structures, and the change of the second test resistance value based on the second initial resistance value is calculated to obtain a second resistance offset value of another test structure.

[0096] According to step S3, it is determined whether the resistance offset value exceeds a set specification to determine whether the stress migration test structure has stress migration failure. If the resistance offset value exceeds the set specification, the stress migration test structure has stress migration failure.

[0097] Among them, since in the stress migration test structure, the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer, the lower through-hole connection layer at the bottom of the conductive plug can have a large line width, while the upper through-hole connection layer at the top of the conductive plug can have a very small line width, thereby making it possible to simultaneously test whether there is stress migration failure in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability evaluation more complete.

[0098] The set specification may be defined according to an industry testing standard, and the set specification may be, for example, 10%.

[0099] Furthermore, when the stress migration test structure includes at least two test structures, all of the lower through-hole connection layers have the same extension direction, and at least two of the upper through-hole connection layers have different extension directions. Then, the resistance offset value exceeds the process abnormality in the vertical direction of the extension direction of the upper through-hole connection layer in the test structure corresponding to the set specification, so that the direction source of the process causing the stress migration failure can be determined based on the extension direction of the upper through-hole connection layer in the test structure where the stress migration failure occurs, thereby quickly clarifying the adjustment direction of the process and the machine.

[0100] by Figure 3a to Figure 3b Taking the stress migration test structure shown as an example, the extension direction of the first lower through-hole connection layer 311 and the second lower through-hole connection layer 312 are both in the X direction, the extension direction of the first upper through-hole connection layer 321 is in the Y direction, and the extension direction of the second upper through-hole connection layer 322 is in the X direction, and the X direction is perpendicular to the Y direction. It should be noted that the line width and other characteristics of the first lower through-hole connection layer 311 and the second lower through-hole connection layer 312 are the same. Then, if only the first resistance offset value or the second resistance offset value exceeds the set specification, the first lower through-hole connection layer 311 and the second lower through-hole connection layer 312 do not have stress migration failure, and the stress migration failure occurs in the first conductive plug 331 or the second conductive plug 332.

[0101] Among them, since the extension direction of the first upper through-hole connection layer 321 is the Y direction, the length of the groove corresponding to the first upper through-hole connection layer 321 in the Y direction (that is, the length of the long side of the rectangular first upper through-hole connection layer 321) is very long and the length in the X direction (that is, the length of the short side of the rectangular first upper through-hole connection layer 321) is very short, resulting in that when the seed crystal is deposited in the through hole at the bottom of the groove (that is, the through hole corresponding to the first conductive plug 331), the seed crystal is easily deposited in the through hole along the Y direction, but the seed crystal is difficult to be deposited in the through hole along the X direction, which leads to the seed crystal in the through hole in the X direction. The amount of seed crystals is too small or even the seed crystals are not deposited on part of the side walls of the through-hole in the X direction, resulting in the risk of defects in the structure filled in the first conductive plug 331 or even direct voids, which leads to stress migration failure in the first conductive plug 331 when performing the stress migration test; similarly, since the extension direction of the second upper through-hole connecting layer 322 is the X direction, the seed crystals are easily deposited in the through-holes corresponding to the second conductive plugs 332 along the X direction, but it is difficult for the seed crystals to be deposited in the through-holes along the Y direction, resulting in stress migration failure in the second conductive plug 332 when performing the stress migration test.

[0102] Therefore, if the first resistance offset value exceeds the set specification and the second resistance offset value does not exceed the set specification, it means that stress migration failure exists in the first conductive plug 331, and the process and machine in the X direction need to be adjusted; if the second resistance offset value exceeds the set specification and the first resistance offset value does not exceed the set specification, it means that stress migration failure exists in the second conductive plug 332, and the process and machine in the Y direction need to be adjusted.

[0103] Taking the adjustment of the process and machine in the X direction as an example, specifically, the deposition power when depositing the seed crystal in the X direction can be adjusted, and the deposition time can be adjusted to improve the effect of depositing the seed crystal in the X direction; or, when etching to form the groove corresponding to the first upper through-hole connection layer 321, the morphology of the etched groove can be adjusted (for example, the opening width of the groove in the X direction is increased); or, when etching to form the through hole corresponding to the first conductive plug 331, the morphology of the etched through hole can be adjusted (the opening width of the through hole in the X direction is increased). Through the above adjustment, the amount of seed crystal deposited in the through hole in the X direction is increased, thereby avoiding the risk of defects in the structure filled in the first conductive plug 331, and further avoiding stress migration failure in the first conductive plug 331 when performing the stress migration test.

[0104] In addition, when the stress migration test structure includes only one test structure, or when the stress migration test structure includes at least two test structures and the measured resistance offset values ​​all exceed the set specifications, the stress test structure can continue to be sliced ​​to confirm whether the failure position is located in the lower through-hole connection layer at the bottom of the conductive plug or in the conductive plug.

[0105] In summary, the present invention provides a stress migration test method, comprising: providing a test sample including the stress migration test structure; testing the resistance value of the stress migration test structure before and after baking to obtain the resistance offset value before and after baking; and judging whether the resistance offset value exceeds the set specification. The stress migration test method provided by the present invention can simultaneously test the stress migration failure in the lower through-hole connection layer at the bottom of the conductive plug and in the conductive plug, thereby making the reliability evaluation more complete.

[0106] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.

Claims

1. A stress migration test structure, characterized in that: The method comprises at least two test structures, wherein the test structure comprises: The lower through-hole connection layer; An upper through-hole connection layer, located above the lower through-hole connection layer; A conductive plug, wherein the bottom and the top of the conductive plug are respectively connected to the lower through-hole connection layer and the upper through-hole connection layer, and the line width of the lower through-hole connection layer is greater than the line width of the upper through-hole connection layer; A lower voltage test pad and a lower current test pad are respectively connected to two ends of the lower through-hole connection layer; An upper voltage test pad and an upper current test pad are respectively connected to two ends of the upper through-hole connection layer; Wherein, all the lower through-hole connection layers have the same extension direction, and at least two of the upper through-hole connection layers have different extension directions.

2. The stress migration test structure according to claim 1, characterized in that: The lower through-hole connection layers in two adjacent test structures are connected to each other, and two adjacent lower through-hole connection layers are connected to the same lower voltage test pad or the lower current test pad.

3. The stress migration test structure according to claim 1, characterized in that: All the lower through-hole connection layers extend in a first direction, at least one upper through-hole connection layer extends in a first direction, at least one upper through-hole connection layer extends in a second direction, and the first direction is perpendicular to the second direction.

4. The stress migration test structure according to claim 1, characterized in that: The line width of the lower through-hole connection layer is 8 to 12 times the line width of the upper through-hole connection layer.

5. The stress migration test structure according to claim 1, characterized in that: The test structure also includes a plurality of connecting metal wires, and the lower voltage test pad, the lower current test pad and the lower through-hole connection layer, the upper voltage test pad, the upper current test pad and the upper through-hole connection layer, and adjacent lower through-hole connection layers are all connected by the connecting metal wires.

6. A stress migration test method, characterized in that: include: Providing a test sample comprising the stress migration test structure as claimed in any one of claims 1 to 5; Testing the resistance value of the stress migration test structure before and after baking to obtain the resistance offset value before and after baking; It is determined whether the resistance offset value exceeds a set specification.

7. The stress migration testing method according to claim 6, characterized in that: The step of obtaining the resistance offset value before and after baking comprises: Connecting the lower voltage test pad to a first voltage, the lower current test pad to a current, and the upper current test pad to a low voltage, so as to measure the voltage of the upper voltage test pad as a second voltage, and dividing the difference between the first voltage and the second voltage by the current to obtain an initial resistance value; baking the test sample; Connecting the lower voltage test pad to the first voltage, the lower current test pad to the current, and the upper current test pad to a low voltage, so as to measure the voltage of the upper voltage test pad as a third voltage, and dividing the difference between the first voltage and the third voltage by the current to obtain a test resistance value; A change of the test resistance value based on the initial resistance value is calculated to obtain the resistance shift value.

8. The stress migration testing method according to claim 6, wherein: The step of obtaining the resistance offset value before and after baking comprises: Connecting the lower current test pad to a first current, connecting the upper current test pad to a second current, measuring the voltage of the lower voltage test pad as a first voltage and the voltage of the upper voltage test pad as a second voltage, and dividing the difference between the first voltage and the second voltage by the difference between the first current and the second current to obtain an initial resistance value; baking the test sample; Connecting the lower current test pad to the first current, connecting the upper current test pad to the second current, measuring the voltage of the lower voltage test pad as a third voltage and the voltage of the upper voltage test pad as a fourth voltage, and dividing the difference between the third voltage and the fourth voltage by the difference between the first current and the second current to obtain a test resistance value; A change of the test resistance value based on the initial resistance value is calculated to obtain the resistance shift value.

9. The stress migration testing method according to claim 6, characterized in that: The resistance values ​​of the different test structures before and after baking are tested in sequence to obtain the resistance offset values ​​of the different test structures.

10. The stress migration testing method according to claim 6, characterized in that: The resistance offset value exceeds the set specification corresponding to a process abnormality in a direction perpendicular to an extension direction of the upper through-hole connection layer in the test structure.