Method for providing reactive cementitious component or concrete admixture
By reprocessing the carbonaceous pile and extracting the calcined rock, and using the calcined clay as a cement component or concrete admixture, the problem of CO2 emissions and resource consumption in cement production is solved, and environmentally friendly and resource-saving cement production is achieved, which is suitable for global cement demand. growth.
Patent Information
- Application Number
- CN202180047953.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-04-28
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-04-28
AI Technical Summary
The existing cement production process has high CO2 emissions and high resource consumption, making it difficult to meet the growing global demand for cement. At the same time, a more environmentally friendly and resource-saving method is needed to produce the main components of cement.
By reprocessing the carbonaceous pile, the calcined rock is extracted and refined, and the calcined clay is used as a cement component or concrete admixture to replace traditional cement clinker and reduce energy consumption and CO2 emissions.
Significantly reduces CO2 emissions and energy input in cement production, while providing an environmentally friendly, sustainable cement alternative suitable for areas with high cement demand, especially in developing countries.
Smart Images

Figure CN115803303B_ABST
Abstract
Description
[0001] The present invention relates to a process for producing cement or concrete.
[0002] Global evolution in terms of population growth, increasing urbanization and economic progress is increasing the demand for new buildings and infrastructure and therefore the demand for concrete. Even now, concrete is the second most common substance used by humans based on mass, after water. Although concrete has less than 150 kgCO2, eq / t concrete has low specific CO2 emissions, but due to the amount used, it is responsible for 5-8% of anthropogenic CO2 emissions.
[0003] A large part of the emissions from concrete comes from the production of cement clinker, the main component of cement. To produce cement clinker, a mixture of lime-containing rock and clay is ground and then calcined; in the course of the process, the lime present in the raw meal releases carbon dioxide (CO2) and is converted into quicklime (CaO). Later in the course of the combustion process, the raw meal, which has been deacidified by elimination of CO2, is sintered to give various calcium silicate phases as well as calcium aluminate and calcium aluminoferrite. A correspondingly complex and energy-intensive device and a corresponding method for producing cement clinker are known, for example, from DE 10 2013 006 236.
[0004] In modern cement plants, cement is produced in a continuous process in a dry process from mainly natural raw materials. The raw materials (limestone, clay, optionally sand and iron ore) are usually obtained in quarries, pre-crushed in crushers and transported to the cement plant. In tubular mills and alternatively other fine mills, the raw materials are ground together and dried simultaneously to obtain the so-called raw meal, which is then fired in a rotary kiln at a temperature of about 1450°C to obtain clinker, which is then cooled in a cooler to a temperature below 200°C. The resulting gray-brown particles are then ground in ball mills and alternatively other fine mills with gypsum or anhydrite to obtain the finished cement. By adding different admixtures, such as slag sand, pozzolana, fly ash and limestone, cements with different chemical and physical properties can be produced.
[0005] Cement is a so-called hydraulic binder. "Hydraulic" substances are those that harden and are stable both in air and in water. Cement reacts with water to form insoluble stable compounds. These compounds, calcium silicate hydrates, form fine needle-shaped crystals that interlock with each other and thus lead to the high strength of cement boards. These properties mean that cement is a binder that meets the high demands in the construction industry.
[0006] The cement industry must therefore significantly reduce its associated emissions and at the same time cope with the growing demand for cement from the global economy.
[0007] The object of the present invention is therefore to at least partially solve the problems mentioned with respect to the prior art. In particular, a method for obtaining further main components of cement in a more environmentally friendly and / or resource-saving manner should be proposed. In addition, materials should be proposed as concrete admixtures in concrete production, with which the cement content of concrete can be reduced. In particular, a method for obtaining and providing binder-containing components for producing cement or concrete should be provided.
[0008] These objects are achieved by a method and a use according to any of the independent claims. Advantageous embodiments are given in the dependent claims. It should be pointed out that the features mentioned in the claims can be combined with each other in any technically feasible way and provide further embodiments. The present description, in particular in conjunction with the drawings, illustrates the invention and gives further advantageous embodiments of the invention.
[0009] This is contributed to by providing a method for providing a reactive cement component or concrete admixture, the method comprising at least the following steps:
[0010] a) reprocessing of carbonaceous piles comprising at least coal and clay-containing rock;
[0011] b) extracting at least calcined rock;
[0012] c) production of fine-grained calcined rock;
[0013] d) To provide fine-grained calcined rock for use as cement component or concrete admixture.
[0014] The above steps can be performed in the specified order, but this is not absolutely necessary. In particular, it is possible that the steps overlap each other at least partially in time, are performed at different locations with a time delay and / or are repeated with different frequencies.
[0015] In step a), the carbonaceous heap is reprocessed. In this case, such a heap contains at least coal and clay-containing rock. In particular, the coal is hard coal. Rock is here in particular understood to mean a (solid) natural material consisting mainly or even at least essentially of mineral components. The rock contains a significant proportion of clay. Most preferably, the heap is a deposit of material mined from a hard coal mine. In this regard, "reprocessing" in particular includes at least partial removal, re-sorting, re-stratification, movement and / or replacement of coal, rock and / or foreign material in the heap, in particular after the heap has been in existence for a long time (without reprocessing). Coal and / or rock are optionally present in the heap with a particle size of up to 100 mm [millimeters].
[0016] The method is particularly useful for heaps containing hard coal, calcined and uncalcined clay. The average proportion of hard coal may be as high as 15%. Calcined clay is an "autogenous" calcined clay formed by the burnout of coal. This is usually or especially carried out by spontaneous combustion of the coal in the heap under suitable environmental conditions. Due to local spontaneous combustion, which optionally occurs repeatedly over time, it is possible to adjust to dryness and a temperature in the range of 350-800° C. in some parts of the heap for a longer period of time, which leads to calcination of the rock, especially the clay.
[0017] Since the particle size is somewhat coarse, it may be advisable to subject at least part of the components of the heap to a preliminary comminution, for example to a particle size of about 30 to 40 mm. This process may be carried out before and / or during step b).
[0018] In step b), at least a portion of the calcined rock present in the heap is extracted. It is possible to selectively extract only the calcined rock from the heap in practice. However, it is conventional practice to separate a portion having all the components of the heap and then identify and separate the calcined rock therefrom. In particular, means and / or devices are provided and used for identifying and extracting (independently and / or automatically) exactly the calcined rock from the components of the heap.
[0019] In order to subsequently add the calcined rock to the cement, in step c), the fineness of the calcined rock is adjusted. In particular, a fine-grained fraction of calcined rock, in particular clay, is produced and / or separated (with or without a preliminary grinding step). This can already be carried out during conditioning or immediately after extraction from the heap, but it is also the case that, alternatively or cumulatively, the calcined rock fraction extracted from the heap is first processed (for example dried and / or ground) before carrying out step c). "Fine" in this context refers in particular to a particle size of the calcined rock of less than 5 mm [millimeters], in particular less than 2 mm or even less than 1 mm. Calcined rock with a particle size of less than 200 μm [micrometers] or even less than 125 μm can be provided as a binder component in cement.
[0020] According to step d), fine-grained calcined rock is provided for use as a cement component or concrete admixture. This may mean that this calcined rock is sent directly to the production process of cement. However, in many cases, cement production is carried out at another location, so the obtained calcined rock is transported there and processed at a later point in time.
[0021] Calcined rock comprises especially calcined clay.
[0022] During the calcination of clay, it loses, inter alia, surface and structural water. The consequence of this water loss is optionally the formation of x-ray-amorphous meta-ton minerals. Upon further heating (500-1250° C.), the melting of the meta-ton minerals forms aluminosilicate glass or optionally also mullite or cristobalite, wherein a high content of mullite and cristobalite is undesirable in the present case. These properties can be taken into account during the (selective) extraction of calcined clay from fuel piles.
[0023] Step b) may include at least one of the following methods:
[0024] - Gravity sorting
[0025] - Sensor sorting.
[0026] The above method can be used in particular for separating or selecting the components of the heap. For this purpose, it can be provided that the components are provided with a particle size suitable for the method, ie in particular they are pre-comminuted to a particle size of at most 50 mm.
[0027] Gravimetric sorting or density sorting includes, in particular, determining the mass of the components of the pile, for example by means of so-called weighing. In particular, this can include sensory determination of the specific gravity of heavy and light materials and separation of these components by means of sensor signals.
[0028] Sensor sorting is preferably carried out using a sensor that generates an image and / or generates a film, in particular a camera. This can be an optical sensor. Sensors that work in the near infrared region can also be used.
[0029] Step b) and / or step c) may include at least one of the following methods:
[0030] - Electrostatic separation
[0031] - Magnetic separation.
[0032] The above method can be used in particular for separating or selecting the components of the pile or the extracted calcined rock. For this purpose, it can be proposed to provide the components with a particle size suitable for the method, ie in particular to pre-crush and / or grind them to a particle size of at most 5 mm.
[0033] In electrostatic separation, component particle sizes of up to 2 mm are preferred. For this purpose, a separator with a high voltage system, a spray electrode and a precipitation electrode and a cleaning system can be used. The air stream carrying particles or containing components / foreign materials can be ionized therein by means of the spray electrode subjected to a high negative voltage. The particles become negatively charged and accumulate at the positively charged precipitation electrode. The particles thus separated can be removed from the separator with a cleaning system.
[0034] When magnetic separation is used, the iron content of the rock to be separated should be greater than 1.5% by weight and the particle size should be a maximum of 5 mm. In the simplest case, the material runs on a conveyor belt under the magnets. The magnetic rock, in particular calcined clay with the indicated iron content, is then attracted by the magnets and thereby separated from the non-magnetic material.
[0035] After step b), at least part of the rock may be conditioned, wherein it is at least partially comminuted or dried.
[0036] "Conditioning" in this context refers in particular to adjusting the properties of the (calcined) rock so that at least the subsequent processes or process steps can be carried out in the most efficient manner possible. This can include, for example, adjustment to a predetermined particle size by means of crushing, grinding, etc., and / or adjustment of the temperature and / or adjustment of the density or distribution in a certain volume or over a certain area, and / or adjustment of the moisture content. For this purpose, temperature treatments of up to about 120° C. can be included.
[0037] The fine or powdery part of the calcined rock can be mixed with other fractions of the cement composition in particular. In the case of calcined clay, it can at least partially replace the clinker and / or fly ash fractions of conventional cement compositions in particular. Alternatively, it can be used as a concrete admixture. In particular, the properties of the calcined rock have been adjusted for these alternative purposes by the method proposed here.
[0038] It is believed that the use of calcined clay as a reactive additive for cement and / or concrete production is becoming increasingly important. The reason is that the calcination of clay takes place at significantly lower temperatures than the formation of clinker from limestone. In this particular case, calcination has already taken place, so that the CO2 balance is much more favorable than in the case of artificially calcined clay.
[0039] With ongoing reprocessing and the continued lack of new coal-fired power plants and declining demand for pig iron, the availability of suitable fly ash and blast furnace slag has decreased.
[0040] As coal is separated into an ash-poor product (fuel) and an ash-rich product (tailings), an ash-rich fraction is obtained, which is usually backfilled into old mine sites or landfilled in heaps. Due to the residual carbon content therein, many tailings heaps have spontaneously ignited and burned or burned in an uncontrolled manner. The thermal processes within the heaps convert part of the incorporated mine waste into clinker or calcine it, so that a considerable amount of such heaps consists of burnt clays. These calcined clays are very similar to the admixtures of Portland cement clinker in terms of mineralogy and chemistry. In addition, these calcined rocks are more CO2 neutral than limestone and Portland cement clinker made therefrom, because the thermal treatment is almost complete.
[0041] In the course of remediation measures, tailings piles are increasingly being fixed, moved and regenerated. The method described here makes it possible to utilize a high proportion of this material (> 50%) in an environmentally friendly, sustainable and economically viable manner. A marketable raw material is formed from the material to be landfilled. This reduces the proportion of new landfills, the area required and the transportation costs, as well as the CO2 emissions generated during transportation.
[0042] Furthermore, the method can also be used to separate unburned coal residues in addition to the calcined rock and to use them as fossil fuel.
[0043] By means of the method, other uncalcined components or rocks can also be separated and sent for further processing. For example, these rocks can be used as road building materials or recycled building materials.
[0044] Burnt clays from hard coal deposits or from tailings heaps obtained by the proposed method can therefore make a considerable contribution to obtaining cement substitutes SCM (English: Supplementary Cementing Materials), since these clays are already converted into clinker and no temperature treatment is required at all.
[0045] It has been possible to show that, after fine grinding to cement fineness (> 5000 Blaine), the "autogenous" calcined tailings selectively processed by this method are comparable or even superior in quality to industrial calcined clay or the hard coal fly ash currently used. The composite cements thus obtained therefore have excellent potential for comprehensive use in the adhesives industry.
[0046] The solution proposed here significantly reduces CO2 emissions in cement production and reduces the necessary energy input. In addition, many developing countries with high cement demand lack high-quality raw materials for producing adhesives. The cement substitute obtained by this method can make a valuable contribution to the raw material supply. It is known from China and India that large tailings piles are burning there and even hard coal deposits have spontaneously combusted. Here, the potential for using this method is huge.
[0047] In another aspect, the use of calcined clay obtained from a carbon-containing pile for adjusting the hydraulic properties of a cementitious composition or a concrete composition is proposed.
[0048] Preferably, the use is such that the calcined clay is used as a replacement for cement clinker and / or fly ash and / or other artificial or natural pozzolanic admixtures.
[0049] Furthermore, the use of calcined clay obtained from a carbon-containing pile for producing a cement composition or a concrete composition with reduced emissions or reduced energy consumption is proposed.
[0050] Calcined clay can be used in fractions of up to 25% or even up to 40% of the cement composition without having to suffer significant disadvantages in terms of concrete strength compared with cement compositions made from pure clinker.
[0051] Thus, high energy "autogenous" calcined clays can replace the expensive and energy intensively produced clinker comprising conventional cement compositions.
[0052] The present invention and the technical field are explained below by means of the accompanying drawings, which disclose particularly preferred embodiments, but the present invention is not limited to these. The accompanying drawings show in schematic form:
[0053] Figure 1 : An overview of heap remediation using an integrated approach to providing reactive cementitious components or concrete admixtures, and
[0054] Figure 2 : Used to provide an overview of the bulk handling of reactive cementitious ingredients or concrete admixtures.
[0055] Figure 1 First, a heap is shown at the top, which is the starting point of the method. Below is shown a possible progression of the method. Starting from a heap containing coal, rock and possibly foreign material, first there is reprocessing according to step a). As a result, three parts can be defined: the contaminated part, which should be sent to landfill, and the (calcined and uncalcined) tailings, which can be subjected to further parts of the method; in particular, the calcined components or the rock are extracted (step b)). These tailings are then further classified, sorted and extracted or further diversified according to step c). As a result, a part of the calcined rock is then discharged as a binder component (step d)). In addition, components that are not suitable for cement / concrete can be used as road building materials, and the beneficiated coal is used as a fossil fuel.
[0056] Figure 2 Displayable Figure 1 The differentiated operating process in steps b) and c) of . Accordingly, for tailings, (repeated) sorting of foreign materials can be implemented, wherein landfill material is discharged. The remaining part can then be (optionally repeatedly) gently comminuted, temperature treated and / or dried, and optionally thereafter (always repeatedly) classified to identify / verify the suitability of the current properties of the components or rocks for downstream processes, and optionally further adjust them. The fine or powdery part can be identified, sorted and allocated to the intended end use, for example, by means of electrostatic separation and / or magnetic separation. Further fine-grained fractions can be identified, sorted and allocated to the intended end use, for example (in addition) by means of density sorting. The coarse-grained part can also be evaluated by density sorting, optionally with the use of sensor sorting, and then these are also identified, sorted and allocated to the intended end use.
Claims
1. A method for providing a reactive cementitious component or a concrete admixture, comprising at least the following steps: a) reprocessing a carbonaceous pile comprising at least coal and a clay-containing rock, wherein the clay-containing rock comprises autogenous calcined clay formed by burnout of the coal; b) extracting at least a portion of the calcined rock present in the carbonaceous pile; c) producing fine-grained calcined rock; d) Providing fine-grained calcined rock for use as a cement component or concrete admixture.
2. The method according to claim 1, wherein step b) comprises at least one of the following methods: - Gravity sorting -Sensor sorting.
3. The method according to any one of the preceding claims, wherein at least step b) or step c) comprises at least one of the following methods: -Electrostatic separation -Magnetic separation.
4. The method according to claim 1, wherein after step b), at least a portion of the rock is conditioned by at least partially crushing it or drying it.
5. A process according to claim 3, wherein the separated portion of calcined rock obtained in step c) is mixed with other fractions of the cement composition in step d).
6. Use of calcined clay obtained from a carbon-containing pile for adjusting the hydraulic properties of a cement composition or a concrete composition, wherein the calcined clay is autogenous calcined clay formed by the combustion of coal.
7. The use according to claim 6, wherein the calcined clay is used as a substitute for cement clinker, fly ash or other artificial pozzolanic or natural pozzolanic admixtures.
8. Use of calcined clay obtained from a carbon-containing pile for producing a cement composition or a concrete composition with reduced emissions, wherein the calcined clay is autogenous calcined clay formed by the combustion of coal.
Citation Information
Patent Citations
Method for producing a pozzolanic or latent-hydraulic cement clinker substitute
CN105793209A
Method for producing cement clinker substitute which is made primarily of calcined clay
CN108349804A
Activated clays from oil contaminated drill cuttings
US7481878B1