Stable emulsified system containing oil bead composition
By using emulsifiers containing PEG and polyglycerol groups, the recrystallization of dodecanol is prevented, and the problem of unstable oil-coagulated beads in the emulsification system is solved, and the long-term stability of oil-coagulated beads and the product effect is improved. .
Patent Information
- Application Number
- CN202211676063.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-26
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-12-26
AI Technical Summary
The existing oil-coagulated beads are unstable in the emulsifier system containing emulsifiers, resulting in whitening color, smaller size and reduced quantity of oil-coagulated beads, mainly due to the recrystallization and migration of dodecanol.
Using an emulsifier containing PEG and polyglycerol groups, a stable oil-coagulant bead composition is formed by adjusting the type and proportion of the emulsifier and adding it to the emulsified matrix to prevent the recrystallization and migration of dodecanol. Ensure the stability of oil beads in the system.
It significantly improves the long-term stability of oil-coagulated beads in the emulsification system, avoids the problems of color changes and quantity reduction, and ensures the stability and effect of the product.
Smart Images

Figure CN115844769B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of cosmetics, and in particular to a stable emulsified system containing an oil gel bead composition. Background Art
[0002] With the development of cosmetic formulation technology, the dosage forms of skin care cosmetics with added particles are becoming more and more popular among consumers. These particles can add more active ingredients and bring fun to consumers, bringing new development directions to cosmetics. The particles in these products can be divided into two categories: 1. Cellulose-wrapped particles, such as vitamin C particles added to hand cream, which use cellulose to wrap vitamin C to maintain its stability, break during the application process, and release nutrients; 2. Oily particles, such as the wrapped oily particles added to the micro-essence series of Chanel, Dior, etc. These particles provide the product with a very high-end appearance and have the effect of moisturizing the skin.
[0003] However, the above two kinds of particles have limitations in use:
[0004] 1) Cellulose-coated particles: Cellulose is hard and difficult to break quickly during application, resulting in a poor consumer experience. In addition, the content of active ingredients encapsulated in it is very low, resulting in weak efficacy of the particles themselves.
[0005] 2) Oily particles. The oily particles currently used in the market are all prepared by raw material suppliers. The preparation process of these particles is very complicated and the technology is not yet mature, resulting in high costs and difficulty in large-scale use in products. In addition, the particles prepared by this process are relatively soft and need to be stored in a liquid with a thickening suspension system to ensure the uniformity of the particles. When used, the entire suspension system mixed with oily particles is added to the finished product, which is difficult to operate. In addition, due to the introduction of thickeners, the skin feel is poor and it is difficult to achieve the expected effect.
[0006] For example, Chinese patent application CN201711457925 discloses a matrix composition containing suspended particles. It successfully produces oily particles using conventional cosmetic production equipment and raw materials, and studies the effects of thickener types and the proportion of oil phase components on the stability and hardness of the oily particles.
[0007] However, in actual application, the oil beads prepared by this patented method are difficult to be applied to the emulsification system containing emulsifiers. Studies have found that after the emulsification formula containing oil beads is stored at 25°C for 1 month and 48°C for 2 weeks, the oil beads in the formula have instability problems such as whitening, smaller oil droplet size, and reduced number. Further research has found that this instability is caused by the change of the component docosanol in the oil beads. The oil beads are composed of docosanol and liquid oil. When the temperature exceeds 70°C, they are liquid oil beads. During the preparation process, the temperature is gradually reduced from 70°C to room temperature, and the docosanol in the liquid oil droplets gradually crystallizes and solidifies, eventually forming oil beads. When the oil beads are prepared and added to a matrix containing certain emulsifiers, the docosanol in the oil beads will be affected by the emulsifier and recrystallize. The docosanol gradually migrates to the interface and even migrates to the water phase, eventually causing the oil beads to turn white, decrease in number, or even disappear.
[0008] Therefore, the art still needs to find a suitable technology to improve the stability of oil beads in the emulsified system. The present invention adopts a one-step method to prepare oil beads, and adds them to an emulsified matrix containing an emulsifier, and by adjusting the type of emulsifier in the emulsified matrix, the oil beads can be stably present in the system. Summary of the invention
[0009] In one aspect, the present invention provides a stable emulsified system containing an oil bead composition, comprising:
[0010] (1) an emulsified base; and
[0011] (2) oil bead composition,
[0012] The emulsified matrix comprises an aqueous phase and an oil phase, the aqueous phase comprises an emulsifier, and the oil phase comprises oil, wherein the emulsifier is an emulsifier containing PEG and polyglycerol groups,
[0013] Wherein, the oil bead composition comprises:
[0014] (i) an aqueous matrix; and
[0015] (ii) oil beads dispersed in the aqueous matrix;
[0016] Wherein, the aqueous matrix comprises a thickener,
[0017] Wherein, the oil gel beads contain one or more moisturizers, and the moisturizers include C 16 -C 24 of saturated fatty alcohols.
[0018] In a preferred embodiment, the emulsifier containing PEG and polyglycerol groups is selected from: polyglycerol-10 laurate, polyglycerol-10 stearate, polyglycerol-10 oleate, polyglycerol-6 oleate, polyglycerol-6 isostearate, polyglycerol-8 stearate, Tween 20, Tween 60, Tween 80 or a combination thereof. In a preferred embodiment, the emulsifying system contains 0.1-1% by weight of the emulsifier. In a preferred embodiment, the thickener in the oil gel bead composition is a polyacrylate thickener, more preferably an acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer. In a preferred embodiment, the C 16 -C 24 The saturated fatty alcohol is behenyl alcohol. In a preferred embodiment, the oil beads further comprise one or more other moisturizers selected from the group consisting of white oil, olive oil, sunflower oil, squalane or a combination thereof.
[0019] In another aspect, the present invention provides a method for preparing the stable emulsified system, comprising:
[0020] (i) preparing an oil bead composition, comprising:
[0021] (1a) dispersing a thickener uniformly in water to form an aqueous phase 1;
[0022] (1b) mixing one or more moisturizers to a homogeneous liquid to form an oil phase 1; and
[0023] (1c) adding the oil phase 1 to the water phase 1 to form the desired oil bead composition;
[0024] (ii) preparing an emulsified base, comprising:
[0025] (2a) dissolving an emulsifier and optionally a thickener in the aqueous phase to form aqueous phase 2;
[0026] (2b) heating the oil until it becomes transparent to form oil phase 2; and
[0027] (2c) adding the oil phase 2 to the water phase 2 to form the desired emulsified matrix;
[0028] (iii) adding the oil bead composition of step (i) to the emulsified base of step (ii) to obtain the desired emulsified system.
[0029] In a preferred embodiment, the method further comprises adjusting the pH value to between 5 and 7 after step (iii).
[0030] In yet another aspect, the present invention provides a formulation comprising the stable emulsified system of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 A photograph showing the Oil Droplet Stability Index.
[0032] Figure 2 The DSC curve of Example 1 is shown. DETAILED DESCRIPTION
[0033] By using emulsifiers containing different functional groups, we can find out the emulsifier that can prevent the recrystallization of docosanol, so that docosanol is not easy to recrystallize and migrate in the system, stabilize the oil droplets containing docosanol, and make it stably exist in the emulsified system containing the emulsifier.
[0034] The present invention unexpectedly found that in the emulsified system, the type of emulsifier has a great influence on the long-term stability of the oil droplets. Emulsifiers containing PEG and polyglycerol groups will weaken the recrystallization of docosanol and enhance its stability. Other types of emulsifiers, especially anionic emulsifiers, will adsorb docosanol to form crystals in the water phase, resulting in recrystallization of docosanol in independent oil droplets, or even precipitation, and the entire system is destroyed, resulting in the oil droplets turning white in color, decreasing in number, or even disappearing.
[0035] Specifically, the present invention studies emulsifiers such as polyglyceryl-10 laurate, polyglyceryl-10 stearate, polyglyceryl-10 oleate, polyglyceryl-6 oleate, polyglyceryl-6 isostearate, polyglyceryl-8 stearate, Tween 20, Tween 60, and Tween 80, which have a good effect on stabilizing oil droplets.
[0036] Oil bead composition
[0037] The present invention relates to an oil gel bead composition, which comprises an aqueous matrix and oil gel beads dispersed in the aqueous matrix.
[0038] In some examples of the present invention, the aqueous matrix is solid or semisolid. In one or more examples, the aqueous matrix is a gel. In some specific examples, the matrix is a hydrogel. In one or more examples, the aqueous matrix comprises a thickener. In one or more examples, the thickener can be a natural (e.g., polysaccharide, etc.) or synthetic (e.g., polyacrylate, polyacrylamide, etc.) thickener. In one or more specific examples, the thickener is selected from TR-1, U21, U30, carbomer 980, AVC, ZEN, Sepigel 305, Sepiplus 400, gellan gum, or a combination of two or more thereof. In one or more preferred examples, the thickener is selected from TR-1, U21, U30, carbomer 980, AVC, ZEN, or a combination of two or more thereof. In a specific embodiment, the thickener is acrylic acid (ester) class / C10-30 alkyl alcohol acrylate crosslinked polymer.
[0039] In some embodiments of the present invention, the oil beads contain one or more moisturizers. In one or more embodiments, the oil beads contain alcohol and / or lipid moisturizers. In one or more embodiments, the oil beads contain C16-C24 saturated fatty alcohols. In some preferred embodiments, the oil beads contain behenyl alcohol.
[0040] In one or more examples, the oil condensation beads also include one or more other wetting agents. In some instantiations, the one or more other wetting agents can be selected from the grease containing the alkyl chain structure. In some instantiations, the one or more other wetting agents can be selected from: 16 / 18 alcohol, white oil, olive oil, sunflower oil, squalane, jojoba esters, shea butter, silicone oil, or two or more combinations thereof. In some instantiations, the one or more other wetting agents are preferably selected from: white oil, olive oil, sunflower oil, squalane, or two or more combinations thereof.
[0041] In some examples of the present invention, the oil beads contain a combination of C16-C24 saturated fatty alcohol and other moisturizers. In a specific example, the oil beads contain a combination of behenyl alcohol and other moisturizers.
[0042] In one or more embodiments, the weight ratio of C16-C24 saturated fatty alcohol to other moisturizers in the oil gel beads is 0.1-1. In a preferred embodiment, the weight ratio of C16-C24 saturated fatty alcohol to other moisturizers in the oil gel beads is 0.1-0.2.
[0043] In some examples of the present invention, the oil bead composition comprises 1-10 wt % of oil bead.
[0044] In some examples of the present invention, the oil gel beads may also include one or more efficacy additives. In other examples, one or more other moisturizers in the oil gel beads are partially replaced by one or more efficacy additives. In one or more examples, the mass of the efficacy additive does not exceed the mass of the moisturizer contained in the oil gel beads. In some exemplary examples, the mass of the efficacy additive does not exceed 95%, 90%, 85% or 80% of the mass of the moisturizer contained in the oil gel beads. In some examples, the one or more efficacy additives are oil-soluble efficacy additives. In one or more examples, the efficacy additives may be beauty additives (e.g., skin beautifying additives, hair beautifying additives), pharmaceutical additives, food additives, or a combination of two or more thereof. Examples of the efficacy additives may include (but are not limited to): oil-soluble licorice, vitamin C tetraisopalmitate, vitamin E acetate, bisabolol, grape extract compound oil, tea seed oil, turmeric root extract, resveratrol, rhodiola rosea oil, safflower seed oil, ganoderma lucidum extract, Xinminshu, methyl salicylate, colorless lycopene, or any combination of two or more thereof.
[0045] Stable emulsified system comprising oil bead composition
[0046] The present invention provides a stable emulsified system comprising an oil gel bead composition. The emulsified system comprises an emulsified base and the oil gel bead composition.
[0047] In some examples of the present invention, the emulsified base comprises an aqueous phase and an oil phase.
[0048] In some instances, the aqueous phase comprises an emulsifier. In one or more instances of the present invention, the emulsifier is an emulsifier containing PEG and polyglycerol groups. The present invention is based on the following unexpected discovery that emulsifiers containing PEG and polyglycerol groups can weaken the recrystallization of saturated fatty alcohol moisturizers (e.g., behenyl alcohol) and enhance their stability. Therefore, selecting this type of emulsifier in the emulsification system can obtain a stable emulsification system containing an oil gel bead composition. In some instances of the present invention, the emulsifier is selected from: polyglyceryl-10 laurate, polyglyceryl-10 stearate, polyglyceryl-10 oleate, polyglyceryl-6 oleate, polyglyceryl-6 isostearate, polyglyceryl-8 stearate, Tween 20, Tween 60, Tween 80 or a combination thereof. In some instances, the aqueous phase comprises a thickener. In one or more instances of the present invention, the thickener is polyacrylate cross-linked polymer-6.
[0049] In some examples of the present invention, the oil phase comprises oil. In one or more examples of the present invention, the oil comprises dimethicone, triethylhexanoin, or a combination thereof.
[0050] In some examples of the present invention, the emulsifying system comprises 1-5 wt % of an oil phase. In a specific example, the emulsifying system comprises 1 wt % of polydimethylsiloxane and 2 wt % of triethylhexanoin.
[0051] In some embodiments of the present invention, the emulsified system comprises 10-50 wt % of the oil bead composition. In a preferred embodiment, the emulsified system comprises 20-40 wt % of the oil bead composition. In a most preferred embodiment, the emulsified system comprises 30-35 wt % of the oil bead composition.
[0052] In one specific example of the present invention, the emulsifying system comprises 0.4 wt % of behenyl alcohol and 2.5 wt % of squalane.
[0053] In some examples of the present invention, the emulsified system comprises 0.1-1 wt % of an emulsifier. In one or more examples, the emulsified system comprises 0.5 wt % of an emulsifier.
[0054] In some examples of the present invention, the emulsifying system comprises, by weight, a combination of 0.2% to 0.3% polyglyceryl-10 laurate, 0.2% to 0.3% polyglyceryl-10 stearate, 0.2% to 0.3% polyglyceryl-10 oleate, 0.2% to 0.3% polyglyceryl-6 oleate, 0.2% to 0.3% polyglyceryl-6 isostearate, and 0.2% to 0.3% polyglyceryl-8 stearate.
[0055] In some examples of the present invention, the emulsifying system comprises, by weight, a combination of 0.1% to 0.2% polyglyceryl-10 laurate, 0.1% to 0.2% polyglyceryl-10 stearate, 0.1% to 0.2% polyglyceryl-10 oleate, 0.1% to 0.2% polyglyceryl-6 oleate, 0.1% to 0.2% polyglyceryl-6 isostearate, and 0.1% to 0.2% polyglyceryl-8 stearate.
[0056] In some examples of the present invention, the emulsifying system comprises, by weight, a combination of 0.1% to 0.2% polyglyceryl-10 laurate, 0.1% to 0.2% polyglyceryl-10 stearate, 0.1% to 0.2% polyglyceryl-10 oleate, 0.1% to 0.2% polyglyceryl-6 oleate, 0.1% to 0.2% polyglyceryl-6 isostearate, and 0.1% to 0.2% polyglyceryl-8 stearate.
[0057] In some examples of the present invention, the emulsifying system comprises, by weight, 0.1%-0.5% Tween 20, 0.1%-0.5% Tween 60, 0.1%-0.5% Tween 80, or a combination of any two.
[0058] Preparation method of emulsified system
[0059] The present invention provides a method for preparing an emulsified system, comprising:
[0060] (i) preparing an oil bead composition;
[0061] (ii) preparing an emulsified base;
[0062] (iii) adding the oil bead composition of step (i) to the emulsified base of step (ii) to obtain the desired emulsified system.
[0063] In some embodiments of the present invention, the present invention provides a method for preparing an oil bead composition, comprising:
[0064] (1a) dispersing a thickener uniformly in water to form an aqueous phase 1;
[0065] (1b) mixing one or more moisturizers to a homogeneous liquid to form an oil phase 1; and
[0066] (1c) Add the above oil phase 1 to the above water phase 1 to form the desired oil drop composition.
[0067] In one or more embodiments, in step (1a), the thickener dispersed in water is heated to a temperature higher than 70°C, for example, 72°C, 75°C, 78°C, 80°C, 82°C, 85°C, or a range formed by any two of the above values as endpoints. In some specific embodiments, the water used in step (1a) is purified water, distilled water, preferably deionized water. In some embodiments, the dispersion in step (1a) is carried out by stirring or shaking.
[0068] In one or more examples, the mixing in step (1b) is carried out at a temperature higher than 70°C, for example, 72°C, 75°C, 78°C, 80°C, 82°C, 85°C, or a range formed by any two of the above values as endpoints. In some examples, the one or more moisturizers include alcohols and / or lipid moisturizers. In some examples, the one or more moisturizers include saturated fatty alcohols of C16-C24. In some preferred examples, the one or more moisturizers include behenyl alcohol. In some examples, one or more other moisturizers are also used. In some specific examples, the one or more other moisturizers can be selected from: hexadecyl alcohol, white oil, olive oil, sunflower oil, squalane, jojoba esters, shea butter, silicone oil, or a combination of two or more thereof. In some preferred examples, the one or more other moisturizers are selected from: white oil, olive oil, sunflower oil, squalane, or a combination of two or more thereof. In some examples, the mixing in step (1b) is carried out in a stirring or oscillating manner.
[0069] In one or more functional examples, one or more efficacy additives are further added in step (1b) and mixed with the one or more moisturizers to form an oil phase. In some examples, one or more efficacy additives are added to partially replace one or more other moisturizers in the oil phase. In one or more examples, the mass of the efficacy additive does not exceed the mass of the moisturizer contained in the oil phase. In some exemplary examples, the mass of the efficacy additive does not exceed 95%, 90%, 85% or 80% of the mass of the moisturizer contained in the oil phase. In some examples, the one or more efficacy additives are oil-soluble efficacy additives. In one or more embodiments, the efficacy additives can be beauty additives (e.g., skin care additives, hair care additives), pharmaceutical additives, food additives, or a combination of two or more thereof. Examples of the efficacy additives may include (but are not limited to): oil-soluble licorice, vitamin C tetraisopalmitate, vitamin E acetate, bisabolol, grape extract compound oil, tea seed oil, turmeric root extract, resveratrol, rhodiola rosea oil, safflower seed oil, ganoderma lucidum extract, Xinminshu, methyl salicylate, colorless lycopene, or a combination of any two or more thereof.
[0070] In one or more examples, step (1c) includes adding the oil phase to the water phase and stirring to obtain a dispersion. In one or more examples, the stirring is carried out at a speed of 200 to 600 RPM, for example, at a speed of 250 to 550 RPM, 300 to 500 RPM, or 350 to 450 RPM. In one or more examples, the stirring lasts for more than 5 minutes, for example, more than 8 minutes, more than 10 minutes. In one or more examples, the stirring in step (1c) is carried out at a temperature higher than 70°C, for example, 72°C, 75°C, 78°C, 80°C, 82°C, 85°C, or a range formed by any two of the above numerical values as endpoints. In one or more examples, step (1c) also includes cooling the dispersion to room temperature. In some examples, the dispersion obtained as described above is allowed to stand and cool to room temperature. In one or more examples, the dispersion is allowed to stand and cool until a solid or semi-solid matrix in which oil droplets are dispersed is obtained. In one or more examples, the dispersion is placed in a corresponding container (eg, a container having a desired shape or a desired composition), and then cooled to obtain a solid or semi-solid matrix with the oil droplets dispersed therein.
[0071] In some embodiments of the present invention, the present invention provides a method for preparing an emulsified matrix, comprising:
[0072] (2a) dissolving an emulsifier and a thickener in the aqueous phase to form an aqueous phase 2;
[0073] (2b) heating the oil until it becomes transparent to form oil phase 2; and
[0074] (2c) Add the oil phase 2 to the water phase 2 to form the desired emulsified base.
[0075] In one or more embodiments, step (2a) is performed at a temperature equal to or greater than 70°C, for example, 72°C, 75°C, 78°C, 80°C, 82°C, 85°C, or a range formed by any two of the above values as endpoints. In some specific embodiments, the water used in step (2a) is purified water, distilled water, preferably deionized water. In some embodiments, step (2a) is performed in a stirring or oscillating manner.
[0076] In one or more examples, step (2b) is performed at a temperature equal to or higher than 70° C., for example, 72° C., 75° C., 78° C., 80° C., 82° C., 85° C., or a range formed by any two of the above values as endpoints. In some examples, step (2b) is performed in a stirring or shaking manner.
[0077] In one or more examples, step (2c) includes adding the oil phase 2 to the water phase 2 under homogenization conditions. In one or more examples, the homogenization conditions last for equal to or greater than 5 minutes, for example, equal to or greater than 8 minutes, equal to or greater than 10 minutes. In one or more examples, step (2c) also includes cooling to room temperature to form an emulsified matrix.
[0078] In some embodiments of the present invention, the prepared oil bead composition is added to the prepared emulsified matrix to obtain the desired emulsified system. In one or more preferred embodiments, the method for preparing an emulsified system of the present invention further comprises: after adding the oil bead composition to the emulsified matrix, adjusting the pH. In some embodiments, tromethamine is used to adjust the pH value of the emulsified system. In some embodiments, the pH value of the emulsified system is adjusted to between 5 and 7.
[0079] Preparations containing emulsifying systems
[0080] The present invention provides a preparation comprising the above-mentioned emulsifying system. In some examples, the preparation may be a cosmetic preparation (e.g., a skin beautifying preparation, a hair beautifying preparation), a pharmaceutical preparation, a food preparation, or a combination of two or more thereof. In one or more examples, the preparation may be in a semisolid or solid form. In one or more examples, the preparation may also include other additives, such as, but not limited to, pigments, flavoring agents, spices, etc.
[0081] Use of emulsified systems comprising oil bead compositions
[0082] The present invention also provides the use of the above-mentioned matrix composition containing suspended oil beads in cosmetic products, medicines and / or foods.
[0083] Example
[0084] The present invention will be further described below in conjunction with specific embodiments. It should be understood that these embodiments are only used to illustrate the present invention and are not intended to limit the scope of the present invention. Those skilled in the art may make appropriate modifications and changes to the present invention, and these modifications and changes are within the scope of the present invention.
[0085] Unless otherwise specified, percentages and parts are calculated by weight. Unless otherwise defined, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. In addition, any methods and materials similar or equivalent to those described herein can be applied to the methods of the present invention. The preferred implementation methods and materials described herein are for demonstration purposes only.
[0086] Experimental Materials
[0087] The raw materials and sources used in the present invention are as follows:
[0088]
[0089]
[0090] Experimental Instruments
[0091] The following instruments are mainly used in the following embodiments of the present invention: 1. Stationary stirrer IKA RW20;
[0092] 2. Constant temperature water bath, model HWS 28, manufactured by Shanghai Yiheng Scientific Instrument Co., Ltd.;
[0093] 3. Weighing balance METTLER TOLEDO PL602-S;
[0094] 4.DSC differential thermal analyzer
[0095] 5. Brookfield RVDV-C Viscometer
[0096] 6. Wet film preparation device, 1 micron height
[0097] Experimental process
[0098] The oil condensate composition can be prepared by the following process:
[0099] The thickener is uniformly dispersed in water, and then heated to a temperature higher than 70° C. to form an aqueous phase 1;
[0100] Mixing one or more moisturizers at a temperature above 70°C to a homogeneous liquid to form an oil phase 1;
[0101] Add the oil phase 1 to the water phase 1, continue stirring to obtain a uniform dispersion, and cool to room temperature with stirring.
[0102] The preparation process of the matrix containing emulsifier is as follows:
[0103] dissolving an emulsifier and a thickener etc. in the water phase at 70° C. to form a water phase 2;
[0104] Heat the oil to 70°C until it becomes transparent to form oil phase 2;
[0105] The oil phase 2 was added to the water phase 2 under homogenizing conditions, homogenized for 10 minutes, and cooled to room temperature to form an emulsified matrix.
[0106] The preparation process of the cream containing oil beads is as follows:
[0107] The oil bead composition is added to the emulsified base, and after mixing evenly, tromethamine is added and stirred evenly.
[0108] Examples 1-6
[0109]
[0110]
[0111] Example 1: Sample preparation
[0112] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol tri(ethylhexanoate), mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.5 mass parts of polyglycerol-10 laurate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 and use as water phase 2; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0113] Example 2: Sample preparation
[0114] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol tri(ethylhexanoate), mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.5 mass parts of polyglycerol-10 stearate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 and use as water phase 2; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0115] Example 3: Sample preparation
[0116] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol tri(ethylhexanoate), mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.5 mass parts of polyglycerol-10 oleate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for later use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0117] Example 4: Sample preparation
[0118] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol Oil tri(ethylhexanoate), mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.5 mass parts of polyglycerol-6 oleate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature as mixed phase 2 for later use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0119] Example 5: Sample preparation
[0120] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol tri(ethylhexanoate), mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.5 mass parts of polyglycerol-6 isostearate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 and use as water phase 2; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0121] Example 6: Sample preparation
[0122] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol tri(ethylhexanoate), mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.5 mass parts of polyglycerol-8 stearate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 and use as water phase 2; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0123] Comparative ratio: 1-6
[0124]
[0125]
[0126] Comparative Example 1: Sample Preparation
[0127] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol Oil tri(ethylhexanoate), mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.5 mass parts of sucrose polystearate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature as mixed phase 2 for later use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0128] Comparative Example 2: Sample Preparation
[0129] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of Glyceryl tri(ethylhexanoate), mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.5 parts by mass of sucrose laurate and 0.5 parts by mass of polyacrylate cross-linked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for later use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0130] Comparative Example 3: Sample Preparation
[0131] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of tri(ethyl)glycerol; PEG-20 methyl glucose sesquistearate and 0.5 parts by mass of polyacrylate cross-linked polymer-6 are weighed, and the mixture is added with 60 parts by mass of deionized water, and the mixture is heated to 70°C and dispersed evenly as aqueous phase 2 for later use. The oil phase 2 is added to aqueous phase 2 under homogenization, and the mixture is kept homogenized for 10 minutes, and cooled to room temperature as mixed phase 2 for later use. The mixed phase 2 is added to the mixed phase 1 under stirring, and stirred for 2 minutes until the oil droplets are evenly dispersed. After dissolving 0.2 parts by mass of tromethamine, the mixture is added to the mixture of mixed phases 1+2, stirred for 10 minutes, and discharged.
[0132] Comparative Example 4: Sample Preparation
[0133] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) ) ester, mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.5 mass parts of cetearyl glucoside and cetearyl alcohol PL68 / 50, 0.5 mass parts of polyacrylate crosslinked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature as mixed phase 2 for later use, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0134] Comparative Example 5: Sample Preparation
[0135] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol tri(ethylhexanoate), mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.5 mass parts of sodium methyl stearoyl taurate, 0.5 mass parts of polyacrylate crosslinked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 and use as water phase 2; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0136] Comparative Example 6: Sample Preparation
[0137] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glycerol Oil tri(ethylhexanoate), mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.5 mass parts of potassium cetyl phosphate, 0.5 mass parts of polyacrylate crosslinked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for later use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0138] Test Example 1: Viscosity test, oil drop film stability test, DSC thermal differential analysis test
[0139] Viscosity test: Use Brookfield RVDV-C viscosity tester to test the viscosity change of the sample after placing it for stability, and calculate the viscosity change ratio. If the viscosity increases significantly, it proves that docosanol migrates to the water phase and recrystallizes in the water phase, increasing the viscosity of the continuous phase. After comparison with the oil droplet sample, it is found that when the viscosity increases by <10%, the shape and color stability of the oil droplets are good, which is judged as "√"; when the viscosity increases by >10%, the shape of the oil droplets is poor, which is judged as "×".
[0140] Oil droplet film drawing stability test: Take 2g of sample, put it in the film drawing mold, and draw it down on the black paper card at a uniform speed to form a film with a thickness of 1mm. After 48 hours, the moisture of the cream evaporates and becomes a transparent phase. The oil droplets are evenly distributed on the black paper. Observe the number and color of oil droplets on a fixed area to evaluate the stability of the oil droplets in the system. The more oil droplets in the same area and the bluer the color, the better the stability of the system. The stability evaluation standards are set as follows:
[0141] Oil droplet stability index 5: The number of oil droplets decreases by <10%, and the oil droplets are blue;
[0142] Oil droplet stability index 4: 10% < The number of oil droplets decreases by <20%, and the oil droplets are blue;
[0143] Oil droplet stability index 3: The number of oil droplets is reduced by <30%, and the oil droplets are white;
[0144] Oil droplet stability index 2: The number of oil droplets is reduced by <50%, and the oil droplets are white;
[0145] Oil droplet stability index 1: The number of oil droplets is reduced by <70%, and the oil droplets are white;
[0146] Oil droplet stability index 0: There are basically no oil droplets visible to the naked eye.
[0147] Figure 1 A photograph showing the Oil Droplet Stability Index.
[0148] A stability index of 3 or above is considered acceptable.
[0149] Oil droplet DSC test:
[0150] Take 20g of sample, put it on a sieve, rinse with deionized water for 5 minutes, screen out the oil droplets, put it in an oven for 24 hours to dry, take 0.01g of dried oil droplets for DSC testing, and set the temperature as: from 25°C, increase the temperature to 100°C at 15°C / min, and then cool down to 25°C at 10°C / min. Analyze the change in phase transition temperature after the stability of the oil droplets. Compare the DSC cooling crystallization peak of the sample just prepared and the position change of the crystallization peak after the sample was placed at 48°C for 2 weeks. If the temperature difference of the crystallization peak is less than 10°C, it indirectly proves that the crystallization of docosin has changed little and the oil droplets are relatively stable, marked with "о". If the change is greater than 10°C, it means that the crystallization and position of docosin in the oil bead structure have changed, which indirectly reflects that the stability of the oil bead has deteriorated and is rated as "△". Figure 2 As shown in the DSC curve of , the DSC crystallization peak position of Example 1 hardly changed, the change was less than 10°C, and was evaluated as "о".
[0151] Table 1
[0152]
[0153] From the results of Examples 1-6, it was found that the type of emulsifier had a great influence on the state stability of the oil droplets, the system viscosity and the crystallization state of the oil droplets. Polyglycerol ester emulsifiers such as polyglycerol-10 laurate, polyglycerol-10 stearate, and polyglycerol-10 oleate could effectively reduce the recrystallization of behenyl alcohol, had good morphological stability, and the viscosity increase was less than 10%, indicating that polyglycerol emulsifiers had a good effect in stabilizing the oil droplets.
[0154] From the results of Comparative Examples 1-6, it was found that the structures of anionic, glycoside, and sucrose emulsifiers were easier to interact with docosanol, enhancing the crystallization of docosanol. From the DSC results, it was found that the crystallization change of the anionic emulsifier was particularly large, exceeding 15 degrees Celsius, and the viscosity increased by more than 20%, demonstrating that it had a great influence on the recrystallization of docosanol. Docosanol interacted with the anionic emulsifier, migrated from the oil droplets to the water phase, and interacted with the emulsifier to form small crystals, thereby significantly increasing the viscosity.
[0155] Embodiment 7-12
[0156]
[0157]
[0158] Embodiments 13-18
[0159]
[0160]
[0161] Embodiment 19-24
[0162]
[0163]
[0164] Example 7: Sample preparation
[0165] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) , mix evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.2 mass parts of polyglycerol-10 laurate, 0.3 mass parts of polyglycerol-10 stearate, and 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and standby use as mixed phase 2, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0166] Example 8: Sample preparation
[0167] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), Mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.2 parts by mass of polyglycerol-10 stearate and 0.3 parts by mass of polyglycerol-10 oleate, 0.5 parts by mass of polyacrylate cross-linked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for use; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0168] Example 9: Sample preparation
[0169] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) , mix evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.2 parts by mass of polyglycerol-10 oleate and 0.3 parts by mass of polyglycerol-6 oleate, 0.5 parts by mass of polyacrylate cross-linked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature as mixed phase 2 for standby use, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0170] Example 10: Sample preparation
[0171] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) , mix evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.2 parts by mass of polyglycerol-6 oleate and 0.3 parts by mass of polyglycerol-6 isostearate, 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenous conditions, keep homogenizing for 10 minutes, cool to room temperature as mixed phase 2 for standby use, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0172] Example 11: Sample preparation
[0173] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), Mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.2 parts by mass of polyglycerol-6 isostearate and 0.3 parts by mass of polyglycerol-8 stearate, 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for use; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0174] Example 12: Sample preparation
[0175] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), Mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.2 parts by mass of polyglycerol-8 stearate and 0.3 parts by mass of polyglycerol-10 laurate, 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0176] Example 13: Sample preparation
[0177] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid and use them as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse them evenly and heat them to 70°C for later use as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature for later use as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, and heat to 70 ℃ transparent as oil phase 2 for standby; weigh 0.2 mass parts of polyglycerol-10 laurate, 0.2 mass parts of polyglycerol-10 stearate, 0.1 mass parts of polyglycerol-10 oleate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70 ℃ and disperse evenly as water phase 2 for standby; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenization for 10 minutes, cool to room temperature and use as mixed phase 2 for standby; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0178] Example 14: Sample preparation
[0179] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid and use them as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse them evenly and heat them to 70°C for later use as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature for later use as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.1 parts by mass of polyglycerol-6 oleate, 0.2 parts by mass of polyglycerol-10 stearate, 0.2 parts by mass of polyglycerol-10 oleate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for standby use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0180] Example 15: Sample preparation
[0181] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid and use them as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse them evenly and heat them to 70°C for later use as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature for later use as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.1 parts by mass of polyglycerol-6 isostearate, 0.2 parts by mass of polyglycerol-6 oleate, 0.2 parts by mass of polyglycerol-10 oleate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for standby use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0182] Example 16: Sample preparation
[0183] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid and use them as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse them evenly and heat them to 70°C for later use as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature for later use as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.1 parts by mass of polyglycerol-6 isostearate, 0.2 parts by mass of polyglycerol-6 oleate, 0.1 parts by mass of polyglycerol-8 stearate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for standby use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0184] Example 17: Sample preparation
[0185] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid and use them as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse them evenly and heat them to 70°C for later use as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature for later use as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, and heat to 70 ℃ transparent as oil phase 2 for standby; weigh 0.2 mass parts of polyglycerol-6 isostearate, 0.1 mass parts of polyglycerol-10 laurate, 0.2 mass parts of polyglycerol-8 stearate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70 ℃ and disperse evenly as water phase 2 for standby; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenization for 10 minutes, cool to room temperature and use as mixed phase 2 for standby; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0186] Example 18: Sample preparation
[0187] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid and use them as oil phase 1 for later use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse them evenly and heat them to 70°C for later use as water phase 1 for later use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature for later use as mixed phase 1 for later use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, and heat to 70 ℃ transparent as oil phase 2 for standby; weigh 0.2 mass parts of polyglycerol-10 laurate, 0.1 mass parts of polyglycerol-10 stearate, 0.2 mass parts of polyglycerol-8 stearate, 0.5 mass parts of polyacrylate cross-linked polymer-6, add 60 mass parts of deionized water, heat to 70 ℃ and disperse evenly as water phase 2 for standby; add oil phase 2 to water phase 2 under homogenization conditions, keep homogenization for 10 minutes, cool to room temperature and use as mixed phase 2 for standby; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0188] Example 19: Sample preparation
[0189] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as oil Phase 2 is set aside; weigh 0.2 parts by mass of polyglycerol-10 laurate, 0.1 parts by mass of polyglycerol-10 stearate, 0.1 parts by mass of polyglycerol-10 oleate, 0.1 parts by mass of polyglycerol-6 oleate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and set aside as mixed phase 2, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0190] Example 20: Sample preparation
[0191] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as The oil phase 2 is set aside; 0.2 parts by mass of polyglycerol-10 stearate and 0.1 parts by mass of polyglycerol-10 oleate, 0.1 parts by mass of polyglycerol-6 oleate, 0.1 parts by mass of polyglycerol-6 isostearate, and 0.5 parts by mass of polyacrylate cross-linked polymer-6 are weighed, 60 parts by mass of deionized water are added, and the mixture is heated to 70°C and dispersed evenly as the water phase 2 for standby use; the oil phase 2 is added to the water phase 2 under homogenization conditions, and the homogenization is maintained for 10 minutes, and the mixture is cooled to room temperature and set aside as the mixed phase 2; the mixed phase 2 is added to the mixed phase 1 under stirring conditions, and stirred for 2 minutes until the oil droplets are evenly dispersed; after dissolving 0.2 parts by mass of tromethamine, the mixture is added to the mixture of the mixed phases 1+2, stirred for 10 minutes, and discharged.
[0192] Example 21: Sample preparation
[0193] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as The oil phase 2 is set aside; 0.2 parts by mass of polyglycerol-10 oleate, 0.1 parts by mass of polyglycerol-6 oleate, 0.1 parts by mass of polyglycerol-6 isostearate, 0.1 parts by mass of polyglycerol-8 stearate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6 are weighed, and 60 parts by mass of deionized water are added, and the mixture is heated to 70°C and dispersed evenly as the water phase 2 for use; the oil phase 2 is added to the water phase 2 under homogenization conditions, and the homogenization is maintained for 10 minutes, and the mixture is cooled to room temperature and set aside as the mixed phase 2; the mixed phase 2 is added to the mixed phase 1 under stirring conditions, and stirred for 2 minutes until the oil droplets are evenly dispersed; after dissolving 0.2 parts by mass of tromethamine, the mixture is added to the mixture of the mixed phases 1+2, stirred for 10 minutes, and discharged.
[0194] Example 22: Sample preparation
[0195] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as oil Phase 2 is set aside; weigh 0.2 parts by mass of polyglycerol-6 oleate, 0.1 parts by mass of polyglycerol-6 isostearate, 0.1 parts by mass of polyglycerol-8 stearate, 0.1 parts by mass of polyglycerol-10 laurate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and set aside as mixed phase 2, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0196] Example 23: Sample preparation
[0197] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent and obtain oil phase 2 for standby; weigh 0.2 parts by mass of polyglycerol-6 isostearate, 0.1 parts by mass of polyglycerol-8 stearate, 0.1 parts by mass of polyglycerol-10 laurate, 0.1 parts by mass of polyglycerol-10 stearate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for standby, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0198] Example 24: Sample preparation
[0199] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 70°C until transparent as oil Phase 2 is set aside; weigh 0.2 parts by mass of polyglycerol-8 stearate, 0.1 parts by mass of polyglycerol-10 laurate, 0.1 parts by mass of polyglycerol-10 stearate, 0.1 parts by mass of polyglycerol-10 oleate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenization conditions, keep homogenizing for 10 minutes, cool to room temperature and set aside as mixed phase 2, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0200] Comparative Examples 7-12
[0201]
[0202]
[0203] Comparative Example 7: Sample Preparation
[0204] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) ) ester, mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.2 parts by mass of sucrose polystearate, 0.3 parts by mass of sucrose laurate, and 0.5 parts by mass of polyacrylate cross-linked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for later use, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0205] Comparative Example 8: Sample Preparation
[0206] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them at 70°C to a transparent liquid as oil phase 1 for standby; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes, rotate at 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix Mix evenly, heat to 70°C until transparent and use as oil phase 2; weigh 0.2 parts by mass of sucrose laurate, 0.3 parts by mass of PEG-20 methyl glucose sesquistearate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for use; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for use; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0207] Comparative Example 9: Sample Preparation
[0208] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is obtained as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and then cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix them evenly, heat to 7 0℃ transparent as oil phase 2 for standby use; weigh 0.2 mass parts of PEG-20 methyl glucose sesquistearate, 0.3 mass parts of cetearyl glucoside and cetearyl alcohol PL68 / 50, 0.5 mass parts of polyacrylate crosslinked polymer-6, add 60 mass parts of deionized water, heat to 70℃ and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenization conditions, keep homogenization for 10 minutes, cool to room temperature as mixed phase 2 for standby use, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 mass parts of tromethamine, add to the mixture of mixed phase 1+2, stir for 10 minutes, and discharge.
[0209] Comparative Example 10: Sample Preparation
[0210] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until a transparent liquid is used as oil phase 1 for standby; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes, the speed is 400RPM, after stirring to form oil droplets, cool to room temperature as mixed phase 1 for standby; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate), mix evenly, add Heat to 70°C until transparent and set aside as oil phase 2; weigh 0.3 parts by mass of sodium methyl stearoyl taurate, 0.2 parts by mass of cetearyl glucoside and cetearyl alcohol PL68 / 50, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 and set aside; add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and set aside as mixed phase 2; add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0211] Comparative Example 11: Sample Preparation
[0212] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) , mix evenly, heat to 70°C until transparent as oil phase 2 for standby use; weigh 0.2 parts by mass of sodium methyl stearoyl taurate, 0.3 parts by mass of potassium cetyl phosphate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for standby use, add oil phase 2 to water phase 2 under homogenous conditions, keep homogenizing for 10 minutes, cool to room temperature and standby use as mixed phase 2, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0213] Comparative Example 12: Sample Preparation
[0214] Weigh 0.4 parts by mass of behenyl alcohol and 2.5 parts by mass of squalane, 0.00006 parts by mass of CI61650, mix them evenly at 70°C until they become a transparent liquid as oil phase 1 for standby use; weigh 30.00 parts by mass of deionized water, add 0.40 parts by mass of acrylic acid (ester) / C10-30 alkyl acrylate crosslinked polymer, disperse evenly and heat to 70°C as water phase 1 for standby use; add oil phase 1 to water phase 1 under stirring, keep stirring for 10 minutes at a speed of 400RPM, stir to form oil droplets, and cool to room temperature as mixed phase 1 for standby use; weigh 1 part by mass of polydimethylsiloxane and 2 parts by mass of glyceryl tri(ethylhexanoate) ) ester, mix evenly, heat to 70°C until transparent as oil phase 2 for later use; weigh 0.3 parts by mass of sucrose polystearate, 0.2 parts by mass of potassium cetyl phosphate, and 0.5 parts by mass of polyacrylate crosslinked polymer-6, add 60 parts by mass of deionized water, heat to 70°C and disperse evenly as water phase 2 for later use, add oil phase 2 to water phase 2 under homogenizing conditions, keep homogenizing for 10 minutes, cool to room temperature and use as mixed phase 2 for later use, add mixed phase 2 to mixed phase 1 under stirring conditions, stir for 2 minutes until the oil droplets are evenly dispersed, dissolve 0.2 parts by mass of tromethamine, add to the mixture of mixed phases 1+2, stir for 10 minutes, and discharge.
[0215] Test Example 2: Viscosity test, oil drop film stability test, DSC thermal differential analysis test
[0216] Viscosity test: Use Brookfield RVDV-C viscosity tester to test the viscosity change of the sample after placing it for stability, and calculate the viscosity change ratio. If the viscosity increases significantly, it proves that docosanol migrates to the water phase and recrystallizes in the water phase, increasing the viscosity of the continuous phase. After comparison with the oil droplet sample, it is found that when the viscosity increases by <10%, the shape and color stability of the oil droplets are good, which is judged as "√"; when the viscosity increases by >10%, the shape of the oil droplets is poor, which is judged as "×".
[0217] Oil droplet film drawing stability test: Take 2g of sample, put it in the film drawing mold, and draw it down on the black paper card at a uniform speed to form a film with a thickness of 1mm. After 48 hours, the moisture of the cream evaporates and becomes a transparent phase. The oil droplets are evenly distributed on the black paper. Observe the number and color of oil droplets on a fixed area to evaluate the stability of the oil droplets in the system. The more oil droplets in the same area and the bluer the color, the better the stability of the system. The stability evaluation standards are set as follows:
[0218] Oil droplet stability index 5: The number of oil droplets decreases by <10%, and the oil droplets are blue;
[0219] Oil droplet stability index 4: 10% < The number of oil droplets decreases < 20%, and the oil droplets are blue;
[0220] Oil droplet stability index 3: The number of oil droplets is reduced by <30%, and the oil droplets are white;
[0221] Oil droplet stability index 2: The number of oil droplets is reduced by <50%, and the oil droplets are white;
[0222] Oil droplet stability index 1: The number of oil droplets is reduced by <70%, and the oil droplets are white;
[0223] Oil droplet stability index 0: There are basically no oil droplets visible to the naked eye.
[0224] A stability index of 3 or above is considered acceptable.
[0225] Oil droplet DSC test: Take 20g sample, put it in a sieve, rinse it with deionized water for 5 minutes, sieve out the oil droplets, put it in an oven for 24h to dry, take 0.01g of dried oil droplets for DSC test, the temperature is set as: from 25℃, increase the temperature to 100℃ at 15℃ / min, and then cool it to 25℃ at 10℃ / min, analyze the change of phase transition temperature after the oil droplets are placed for stability, and compare the DSC cooling crystallization peak when the sample is just prepared and the position change of the crystallization peak after the sample is placed at 48℃ for 2 weeks. If the crystallization peak temperature difference is less than 10℃, it proves that the crystallization of docosin has little change and the oil droplets are relatively stable, marked "о"; if the change is greater than 10℃, it means that the crystallization and position of docosin in the oil bead structure have changed, which reflects the poor stability of the oil bead, rated as "△".
[0226] Table 2
[0227]
[0228] It was found from Examples 7-24 that 0.2% to 0.3% of polyglyceryl-10 laurate, 0.2% to 0.3% of polyglyceryl-10 stearate, 0.2% to 0.3% of polyglyceryl-10 oleate, 0.2% to 0.3% of polyglyceryl-6 oleate, 0.2% to 0.3% of polyglyceryl-6 isostearate, and 0.2% to 0.3% of polyglyceryl-8 stearate, when combined in pairs, form a compound emulsifier, which has a good effect on stabilizing oil droplets.
[0229] Polyglyceryl-10 laurate 0.1%-0.2%, polyglyceryl-10 stearate 0.1%-0.2%, polyglyceryl-10 oleate 0.1%-0.2%, polyglyceryl-6 oleate 0.1%-0.2%, polyglyceryl-6 isostearate 0.1%-0.2%, polyglyceryl-8 stearate 0.1%-0.2%, wherein every three emulsifiers are combined to form a compound emulsifier, which has a better effect on stabilizing oil droplets.
[0230] Polyglyceryl-10 laurate 0.1%-0.2%, polyglyceryl-10 stearate 0.1%-0.2%, polyglyceryl-10 oleate 0.1%-0.2%, polyglyceryl-6 oleate 0.1%-0.2%, polyglyceryl-6 isostearate 0.1%-0.2%, polyglyceryl-8 stearate 0.1%-0.2%, wherein every four emulsifiers are combined to form a compound emulsifier, which has a better effect on stabilizing oil droplets.
[0231] It was found from Comparative Examples 7-12 that 0.2%-0.3% sucrose polystearate, 0.2%-0.3% sucrose laurate, 0.2%-0.3% PEG-20 methyl glucose sesquistearate, 0.2%-0.3% cetearyl glucoside and cetearyl alcohol PL68 / 50, 0.2%-0.3% sodium methyl stearoyl taurate, and 0.2%-0.3% potassium cetyl phosphate, where two emulsifiers are combined and added to the matrix to form a corresponding emulsification system matrix, and then the prepared oil droplets are added to the matrix, and it is found that the stability of the oil droplets in the emulsification system does not pass, the oil droplets become smaller, or even disappear, confirming that sucrose and anionic emulsifiers have a negative effect on the stability of the system.
[0232] Examples 25-30
[0233]
[0234]
[0235] Examples 31-36
[0236]
[0237]
[0238] Test Example 3: Viscosity test, oil drop film stability test, DSC thermal differential analysis test
[0239] Viscosity test: Use Brookfield RVDV-C viscosity tester to test the viscosity change of the sample after placing it for stability, and calculate the viscosity change ratio. If the viscosity increases significantly, it proves that docosanol migrates to the water phase and recrystallizes in the water phase, increasing the viscosity of the continuous phase. After comparison with the oil droplet sample, it is found that when the viscosity increases by <10%, the shape and color stability of the oil droplets are good, which is judged as "√"; when the viscosity increases by >10%, the shape of the oil droplets is poor, which is judged as "×".
[0240] Oil droplet film drawing stability test: Take 2g of sample, put it in the film drawing mold, and draw it down on the black paper card at a uniform speed to form a film with a thickness of 1mm. After 48 hours, the moisture of the cream evaporates and becomes a transparent phase. The oil droplets are evenly distributed on the black paper. Observe the number and color of oil droplets on a fixed area to evaluate the stability of the oil droplets in the system. The more oil droplets in the same area and the bluer the color, the better the stability of the system. The stability evaluation standards are set as follows:
[0241] Oil droplet stability index 5: The number of oil droplets decreases by <10%, and the oil droplets are blue;
[0242] Oil droplet stability index 4: 10% < The number of oil droplets decreases < 20%, and the oil droplets are blue;
[0243] Oil droplet stability index 3: The number of oil droplets is reduced by <30%, and the oil droplets are white;
[0244] Oil droplet stability index 2: The number of oil droplets is reduced by <50%, and the oil droplets are white;
[0245] Oil droplet stability index 1: The number of oil droplets is reduced by <70%, and the oil droplets are white;
[0246] Oil droplet stability index 0: There are basically no oil droplets visible to the naked eye.
[0247] A stability index of 3 or above is considered acceptable.
[0248] Oil droplet DSC test: Take 20g sample, put it in a sieve, rinse it with deionized water for 5 minutes, sieve out the oil droplets, put it in an oven for 24h to dry, take 0.01g of dried oil droplets for DSC test, the temperature is set as: from 25℃, increase the temperature to 100℃ at 15℃ / min, and then cool it to 25℃ at 10℃ / min, analyze the change of phase transition temperature after the oil droplets are placed for stability, and compare the DSC cooling crystallization peak when the sample is just prepared and the position change of the crystallization peak after the sample is placed at 48℃ for 2 weeks. If the crystallization peak temperature difference is less than 10℃, it proves that the crystallization of docosin has little change and the oil droplets are relatively stable, marked "о"; if the change is greater than 10℃, it means that the crystallization and position of docosin in the oil bead structure have changed, which reflects the poor stability of the oil bead, rated as "△".
[0249] Table 3
[0250]
[0251] From the test results of Examples 25-36, it was found that Tween 20 0.1%-0.5%, Tween 60 0.1%-0.5%, and Tween 80 0.1%-0.5%, when used alone or in combination of two to prepare a matrix, could stabilize the oil droplets added to the matrix, prevent the docosanol in the oil droplets from recrystallizing, and prevent the oil droplets from turning white or disappearing.
[0252] The preparations of Examples 1 to 36 are used for the preparation of a skin external preparation. The skin external preparation is preferably a cosmetic composition, such as an essence, a cream, etc. The weight percentage of the mixture in the skin external preparation is 1%-100% (w / w). The preferred weight percentage is 20%-100% (w / w). The more preferred weight percentage is 30%-90% (w / w). The most preferred weight percentage is 50%-90% (w / w).
[0253] The following are examples of specific applications of the preparations in external skin preparations, and the formulations and preparation methods of these preparations. In the following tables, "-" means no addition.
[0254] Example 37: Preparation of facial cream
[0255]
[0256] Example 38: Preparation of emulsion
[0257]
[0258]
[0259] Example 39: Preparation of gel
[0260]
[0261] Example 40: Preparation of Essence
[0262]
[0263] Example 41: Preparation of facial mask
[0264]
[0265]
[0266] Example 42: Preparation of eye cream
[0267]
[0268] It should be understood that after reading the above teachings of the present invention, those skilled in the art may make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the claims attached to this application.
Claims
1. A stable emulsified system containing an oil bead composition, comprising: (1) an emulsified base; and (2) Oil bead composition, in, The emulsified matrix comprises an aqueous phase and an oil phase, wherein the aqueous phase comprises an emulsifier and a thickener, wherein the thickener in the aqueous phase is polyacrylate cross-linked polymer-6, and the oil phase comprises oil, wherein the oil is selected from polydimethylsiloxane, triethylhexanoin or a combination thereof, wherein the emulsifier is selected from polyglyceryl-10 laurate, polyglyceryl-10 stearate, polyglyceryl-10 oleate, polyglyceryl-6 oleate, polyglyceryl-6 isostearate, polyglyceryl-8 stearate, Tween 20, Tween 60, Tween 80 or a combination thereof, Wherein, the oil bead composition comprises: (i) an aqueous matrix; and (ii) oil beads dispersed in the aqueous matrix; Wherein, the aqueous matrix contains a thickener, and the thickener in the aqueous matrix is an acrylic acid (ester) / C10-30 alkyl acrylate cross-linked polymer, The oil beads contain one or more moisturizers, and the moisturizer contains behenyl alcohol.
2. The stable emulsified system according to claim 1, in, The emulsified system contains 0.1-1 wt % of an emulsifier.
3. The stable emulsified system according to claim 1, in, The emulsifying system comprises a combination of 0.2-0.3 wt % of polyglyceryl-10 laurate, 0.2-0.3 wt % of polyglyceryl-10 stearate, 0.2-0.3 wt % of polyglyceryl-10 oleate, 0.2-0.3 wt % of polyglyceryl-6 oleate, 0.2-0.3 wt % of polyglyceryl-6 isostearate, and 0.2-0.3 wt % of polyglyceryl-8 stearate.
4. The stable emulsified system according to claim 1, in, The emulsifying system comprises a combination of 0.1-0.2 wt % of polyglyceryl-10 laurate, 0.1-0.2 wt % of polyglyceryl-10 stearate, 0.1-0.2 wt % of polyglyceryl-10 oleate, 0.1-0.2 wt % of polyglyceryl-6 oleate, 0.1-0.2 wt % of polyglyceryl-6 isostearate, and 0.1-0.2 wt % of polyglyceryl-8 stearate.
5. The stable emulsified system according to claim 1, in, The emulsifying system comprises a combination of 0.1-0.2 wt % of polyglyceryl-10 laurate, 0.1-0.2 wt % of polyglyceryl-10 stearate, 0.1-0.2 wt % of polyglyceryl-10 oleate, 0.1-0.2 wt % of polyglyceryl-6 oleate, 0.1-0.2 wt % of polyglyceryl-6 isostearate, and 0.1-0.2 wt % of polyglyceryl-8 stearate.
6. The stable emulsified system according to claim 1, in, The emulsification system comprises 0.1-0.5 wt % of Tween 20, 0.1-0.5 wt % of Tween 60, or 0.1-0.5 wt % of Tween 80, or a combination of any two of them.
7. The stable emulsified system according to claim 1, in, The oil beads may further comprise one or more other moisturizers selected from the group consisting of white oil, olive oil, sunflower oil, squalane, or a combination thereof.
8. A method for preparing a stable emulsified system as claimed in any one of claims 1 to 7, wherein include: (i) preparing an oil bead composition, comprising: (1a) uniformly dispersing acrylic acid (esters) / C10-30 alkyl acrylate cross-linked polymer in water to form an aqueous phase 1; (1b) mixing one or more humectants into a homogeneous liquid to form an oil phase 1; and (1c) adding the oil phase 1 to the water phase 1 to form the desired oil bead composition; (ii) preparing an emulsified base, comprising: (2a) dissolving an emulsifier and polyacrylate cross-linked polymer-6 in an aqueous phase to form an aqueous phase 2; (2b) heating the oil until it becomes transparent to form oil phase 2; and (2c) adding the oil phase 2 to the water phase 2 to form the desired emulsified matrix; (iii) adding the oil bead composition of step (i) into the emulsified base of step (ii) to obtain the desired emulsified system.
9. The method according to claim 8, in, The method further comprises adjusting the pH value to between 5 and 7 after step (iii).
10. A formulation comprising the stable emulsified system according to any one of claims 1 to 7.