A method for treating the filtrate of desulfurization of kiln flue gas in the zinc oxide production industry
Through the combined treatment of calcium sulfide, calcium dihydrogen phosphate and potassium metaaluminate, the problem of removing heavy metals and chloride ions in the kiln flue gas desulfurization filtrate in the sub-zinc oxide production industry is solved, and the recycling of the filtrate and the elimination of slag are achieved. Recycling hazardous waste into resources improves gypsum quality and desulfurization efficiency while reducing treatment costs and equipment maintenance requirements.
Patent Information
- Application Number
- CN202211650309.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-21
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-12-21
AI Technical Summary
Existing technology has accumulated heavy metals, chloride ions and other impurities in the treatment of kiln flue gas desulfurization filtrate in the sub-zinc oxide production industry, resulting in reduced desulfurization efficiency, poor gypsum quality and difficulty in sewage treatment. In addition, the existing method has high equipment costs and maintenance requirements. Harsh and difficult to achieve harmless recycling of resources.
Calcium sulfide agent is used to remove heavy metal impurities, calcium dihydrogen phosphate is used to adjust the pH value to co-precipitate impurities, and potassium metaaluminate and oxidizing gas treatment are combined to remove chloride ions, forming a reusable double salt slag, reducing the use of agents and lowering costs. Equipment Requirements.
It achieves the effective reduction of various ions, ensures that the filtrate can be recycled, avoids wastewater discharge, produces harmless resource residue, ensures that flue gas emission standards are met and the quality of gypsum is excellent, and the operation and maintenance costs of process equipment are reduced.
Smart Images

Figure CN115849627B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fume treatment in metallurgy, and in particular to a method for treating fume desulfurization filtrate in a kiln in the zinc oxide production industry. Background Art
[0002] Due to the increasing scarcity of zinc mineral resources, solid waste resource recycling is a must. Nowadays, the proportion of industrial zinc-containing solid wastes such as various industrial zinc-containing waste slags, blast furnace dust, etc. using pyrometallurgical kiln volatilization to produce secondary zinc oxide is increasing, and it has even become the main process in China. However, the components of zinc-containing solid wastes are often complex, inevitably containing sulfides, heavy metals, ammonia nitrogen, etc., and then a large amount of sulfur oxides are produced during the kiln calcination reaction. In order to protect the environment and make the emission indicators meet the standards, whether the desulfurization system is efficient, reliable and stable is the premise for the continued survival and development of the enterprise. The existing desulfurization process is mainly based on wet desulfurization with lime or limestone. The process is to absorb sulfur oxides in the desulfurization tower with lime slurry or limestone slurry, and the generated calcium sulfite is oxidized into calcium sulfate by blowing air. When the specific gravity of the slurry in the desulfurization tower reaches a certain value, it is discharged and filtered to obtain by-product desulfurization gypsum and desulfurization filtrate. The desulfurization filtrate is generally used in a short-term cycle. When the chlorine, magnesium, sodium, potassium, ammonium and metal elements in the desulfurization filtrate are enriched and accumulated to a certain extent, the desulfurization efficiency will be reduced, the amount of lime or limestone will increase greatly, and the desulfurization gypsum will be too viscous to be dehydrated, resulting in ultra-high water content and other drawbacks that seriously affect production operations. The filtrate has to be replaced with tap water and discharged to the sewage station for treatment. The desulfurization filtrate has complex components, high salinity, high ammonia nitrogen, and many types of heavy metals. It not only greatly increases the treatment burden of the sewage system, but also wastes a lot of resources.
[0003] At present, researchers have conducted a lot of research and development on the treatment methods of desulfurization filtrate, mainly including chemical precipitation purification method, chemical pretreatment-nanofiltration-electrodialysis / membrane dialysis-evaporation crystallization combined treatment method, concentration-incineration method, etc. For example, the Chinese invention patent, announcement number CN106007046B, provides a desulfurization wastewater hardness ion resource pretreatment process. This technical solution first sends the desulfurization wastewater into a pre-coagulation sedimentation unit, adds a flocculant for coagulation, and then removes the suspended matter and SO in the desulfurization wastewater. 4 2- and F - Then, sodium hydroxide, lime and polymer flocculant are added to remove Mg. 2+ Magnesium hydroxide is generated, and aluminum chloride and lime are added to remove Ca 2+ Etc. to generate calcium aluminate, add carbonate to generate calcium carbonate and remove the remaining Ca 2+, calcium carbonate is recovered as a desulfurizing agent; although this invention can effectively remove various hardness ions, impurities such as chloride ions and ammonium ions in the desulfurization filtrate are not removed, and the addition of a large amount of sodium salt will cause the sodium ions in the system solution to continue to enrich and accumulate, resulting in subsequent process problems.
[0004] The Chinese invention patent, with the announcement number CN106430786B, provides a method for treating desulfurization wastewater, firstly using flocculation precipitation treatment, and then pre-treating the obtained clear liquid with alkali metal carbonate to obtain calcium carbonate precipitation and softened desulfurization wastewater; the softened desulfurization wastewater is subjected to nanofiltration treatment to obtain sulfate-rich water and sulfate-poor water, and the sulfate-rich water is returned and mixed with the softened desulfurization wastewater and then subjected to nanofiltration treatment; the sulfate-poor water is subjected to reverse osmosis treatment to obtain a first chlorine-rich concentrated water and a first fresh water; the first chlorine-rich concentrated water is subjected to electrodialysis treatment, A second chlorine-rich concentrated water and a second fresh water are obtained; the second chlorine-rich concentrated water is subjected to an evaporation and crystallization treatment to obtain chloride salt and a third fresh water; the method of the invention can effectively treat the wastewater after flue gas desulfurization generated by coal-fired power plants, etc., but the produced slag is not classified and precipitated step by step, so that the produced slag contains highly toxic heavy metals such as lead, cadmium, and mercury, which has great harm to the environment and the relevant resources are not fully recovered. Secondly, the nanofiltration and membrane treatment system process requirements are strict, the membrane is easy to clog, the service life is not long, the treatment process route is long, and the initial investment and operation costs are large.
[0005] The Chinese invention patent, with the announcement number CN113511754B, proposes a method for treating desulfurized wastewater, firstly flotation treatment of the desulfurized wastewater; flocculation and sedimentation of the supernatant after flotation treatment; two-stage dechlorination treatment of the supernatant after flocculation and sedimentation; Freund's salt method is used for dechlorination treatment; the invention treats the heavy metal ions, fluoride ions and chloride ions in the flue gas desulfurization wastewater from the copper-containing sludge pyrometallurgical treatment in an integrated manner, but the impurities cannot be classified and recovered in sequence, and the waste residue produced pollutes the environment and is difficult to treat. In addition, this method will continuously introduce sodium ions, which is only suitable for alkaline desulfurization, and will cause many process problems for lime / limestone desulfurization. Therefore, it is urgent to develop a method for treating the flue gas desulfurization filtrate of the secondary zinc oxide production industry. Summary of the invention
[0006] In view of the above-mentioned deficiencies, the present invention provides a method for treating the flue gas desulfurization filtrate of the secondary zinc oxide production industry kiln, which is a method for treating the flue gas desulfurization filtrate of the secondary zinc oxide production industry kiln, and ... 2+ , Pb 2+ 、Ni 2+ 、Cd 2+ NH + 4 Mg 2+ , Cl - 、SO 2-4 The method effectively removes ions and forms reusable valuable filter residues, so that the filtrate can be recycled without discharging wastewater, and the produced slag can be harmlessly recycled, ensuring that the flue gas emission meets the standards and produces high-quality gypsum products, avoiding the difficulty of dehydrating gypsum slag and affecting the operation of the desulfurization system.
[0007] The technical process of the present invention is described as follows:
[0008] The main components of flue gas desulfurization filtrate in zinc oxide production industry are Zn 2+ , Pb 2+ 、Ni 2+ 、Cd 2+ NH + 4 Mg 2+ , K + 、Na + , Cl - 、SO 2- 4 Plasma, firstly, calcium sulfide is added to remove heavy metals such as zinc, lead, and cadmium in the desulfurization filtrate in the form of sulfide precipitation, and the heavy metal sulfide slag produced is returned to the production line for recycling. The advantage of this step is that it not only recovers valuable resources but also ensures that the slag produced in the subsequent filtrate treatment process does not contain heavy metals, thereby avoiding the restriction that it cannot be used in the agricultural field. The reaction formulas involved are mainly:
[0009]
[0010] Where M = Zn 2+ , Pb 2+ 、Ni 2+ 、Cd 2+ Heavy metal ions such as
[0011] Removal of Zn 2+ , Pb 2+ 、Ni 2+ 、Cd 2+ The first filtrate after heavy metal ions also contains a large amount of NH 4 + Mg 2+ 、SO 2- 4 , Cl - ions, based on the NH 4 + Mg 2+ 、SO 2- 4 ion molar content by adding a certain amount of calcium dihydrogen phosphate to make SO 2- 4 NH 4+ Mg 2+ and PO 3- 4 The molar contents of the four ions are controlled within a certain ratio range, the temperature is controlled between 20°C and 40°C, and the pH value is gradually adjusted to four steps of 1.5-2.5, 7-8, 8-9, and 9-11 with calcium hydroxide. Each pH step is kept for 30min-60min. After completion, the impurities ammonium ions, magnesium ions, phosphate ions, and sulfate ions generate complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain secondary filtrate and complex slag. The complex slag is ammonium sulfate calcium magnesium complex salt crystals, which can be used as a multi-element slow-release fertilizer as a raw material and auxiliary material and widely used in various agricultural compound fertilizer products; it should be particularly noted that the technical scheme of this step is different from the existing scheme. First, calcium sulfate precipitation is generated and filtered to remove sulfate, and then the filtrate is removed in the form of struvite by adding an agent. There are essential differences between the ammonium ion and magnesium ion methods. First of all, this scheme belongs to the "one-pot method". Sulfate, ammonium ions, magnesium ions and phosphate are co-precipitated and removed in the same reaction tank. To achieve this goal, first, calcium dihydrogen phosphate and sulfate are converted into nano calcium sulfate crystals under pH = 1.5-2.5, and then the pH value is quickly adjusted to 7-8, so that the generated calcium hydrogen phosphate and magnesium hydrogen phosphate wrap the calcium sulfate particles, and then the pH is continued to be adjusted to 8-9 with calcium hydroxide, so that ammonium ions are combined through chemical adsorption to produce ammonium calcium phosphate and ammonium magnesium phosphate mixed crystals, and finally the pH value is raised to 9-10.5 again to remove residual phosphate and stabilize the ammonium calcium magnesium sulfate double salt crystals. This method for preparing ammonium calcium magnesium sulfate double salt crystal double salt slag also has a certain synergistic removal of K + 、Na + The effect of ions is chemical adsorption or combining with sulfur phosphoric acid complex salt to produce eutectic precipitation. The reactions involved are mainly:
[0012]
[0013] Where M' = NH 4 + , K + 、Na + Plasma;
[0014] Remove NH by the above steps 4 + Mg 2+ ,PO 3- 4 The secondary filtrate obtained after plasma treatment still contains Cl which affects the desulfurization production operation. - Ionic impurities; Existing technology for removing Cl -The methods for removing ions generally adopt nanofiltration, electrodialysis, diffusion dialysis and other combined methods or lime aluminum salt precipitation method. Among them, nanofiltration, electrodialysis, diffusion dialysis and other combined methods have the defects of high investment cost, high technical requirements for operation and maintenance, and short life of equipment system. The lime aluminum salt precipitation method has low raw material prices and low process equipment requirements. It is one of the methods suitable for industrial application. The lime aluminum salt precipitation method is to add excess calcium salt and aluminum salt to the chlorine-containing solution. At a certain reaction temperature and stirring speed, calcium ions and aluminum ions react with chloride ions to generate Ca 2 Al 2 Cl 2 (OH) 12 Precipitation ultimately achieves efficient removal of chloride ions, and the main reactions involved are as follows:
[0015]
[0016] From the above reaction equations (1), (4), (5) and (6), it can be seen that when sodium aluminate is added in excess or too quickly, or as the reaction proceeds, excessive OH will be introduced or generated. - , while OH - The presence of a large amount of makes the reaction unfavorable to the formation of Ca 2 Al 2 Cl 2 (OH) 12 direction, thus affecting Cl - The removal of the reagents results in a waste of reagents (usually requiring the input of n(CaO):n(NaAlO 2 ):n(Cl - ) is above 6:4:1); in order to solve the above problems, this scheme uses potassium aluminate as the aluminum source, and the potassium ions introduced by potassium aluminate are more easily chemically adsorbed by the ammonium calcium magnesium sulfate complex salt crystals generated in the solution system and removed, and the addition time of potassium aluminate is controlled in such a way that the OH in the reaction system - The content is controlled within a moderate range. In addition, calcium sulfide is used to replace lime, and calcium sulfide solid is hydrolyzed in the solution to generate Ca(HO) 2 and H 2 The characteristics of S, on the one hand, provide the Ca(HO) required for chlorine precipitation 2 On the other hand, H 2 S can neutralize the excess OH produced during the reaction - Of course, in order to avoid H 2 S neutralizes OH - The generated Na 2 S was continuously enriched in the reaction solution system, affecting the reaction chain. Ozone gas was introduced to remove Na 2 S oxidation, ensuring that the entire reaction process is in the process of generating Ca 2 Al2 Cl 2 (OH) 12 The favorable conditions involved are mainly:
[0017]
[0018] Where M" = K + 、Na + ion;
[0019] The above steps are used to remove Cl - The filtrate after ionization is the purified liquid, which is returned to the desulfurization system for pulping and recycling. Although the purified liquid contains a small amount of potassium and sodium ions, it does not affect the operation of the desulfurization system. Potassium and sodium are synergistically reduced while removing phosphate, magnesium ions, ammonium and sulfate by the aforementioned ammonium calcium magnesium thiophosphate double salt crystal method, so the content of potassium and sodium can be maintained in balance.
[0020] Compared with the existing technology, this technical method has a fundamental breakthrough. The reagents and treatment processes used have not been reported before, and the amount of reagents used is greatly reduced (only n(CaS):n(KAlO 2 ):n(Cl - )3-4.5:1.5-2.5:1 is sufficient).
[0021] The purpose of the present invention is achieved through the following technical solutions:
[0022] A method for treating a flue gas desulfurization filtrate of a kiln in a zinc oxide production industry, comprising the following steps:
[0023] 1) The desulfurized gypsum slurry of the kiln flue gas of the secondary zinc oxide production industry is extracted from the desulfurization tower, and the desulfurized gypsum and desulfurized filtrate A are obtained by filtration through a vacuum belt conveyor. The desulfurized filtrate A is sent to the reaction tank 1. Under stirring, a sufficient amount of calcium sulfide is added according to the total content of zinc, lead and cadmium in the filtrate to remove heavy metal impurities such as zinc, lead and cadmium. After precipitation reaction for 30min-60min, the slag B and filtrate C mainly containing zinc sulfide, lead sulfide, cadmium sulfide and calcium sulfate are obtained. The slag B is returned to the secondary zinc oxide production section for recycling and treatment;
[0024] 2) The filtrate C is sent to the reaction tank 2. Under stirring, a certain amount of calcium dihydrogen phosphate is added according to the molar content of ammonium ions, magnesium ions and sulfate ions in the filtrate C, so that the molar content of ammonium ions, magnesium ions, sulfate ions and phosphate ions is controlled within a certain ratio range, the temperature is controlled between 20°C and 40°C, and the pH value is gradually adjusted to four steps of 1.5-2.5, 7-8, 8-9 and 9-11 with calcium hydroxide. Each pH step is kept for 30min-60min. After completion, the impurities ammonium ions, magnesium ions, phosphate ions and sulfate ions form a complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain filtrate E and complex salt slag D. The complex salt slag D is ammonium calcium magnesium sulfate phosphate complex salt crystals, which are rich in plant nutrients such as sulfur, phosphorus, magnesium, nitrogen, potassium and calcium. As a multi-element slow-release fertilizer raw material, it is widely used in various agricultural compound fertilizer products;
[0025] The relationship between the amount of calcium dihydrogen phosphate added and the molar content ratio of ammonium ions, magnesium ions and sulfate radicals in the filtrate C is: The sum of the molar content of ammonium ions and the molar content of magnesium ions is marked as K 1 , the molar content of sulfate is marked as K 2 The molar amount of calcium dihydrogen phosphate added is marked as K 3 ;
[0026] When K 1 ≤K 2 When the amount of calcium dihydrogen phosphate added is K 3 =1.1K 2 ;
[0027] When K 2 <K 1 ≤2K 2 When the amount of calcium dihydrogen phosphate added is K 3 =0.7(K 1 +K 2 );
[0028] When K 1 >2K 2 When the amount of calcium dihydrogen phosphate added is K 3 =0.6K 1 ;
[0029] 3) The filtrate E is sent to the reaction tank 3, and calcium sulfide is added according to the chloride ion content in the filtrate E. The amount of calcium sulfide added is 3.0-4.5 times the molar content of chloride ions in the filtrate E. The reaction temperature is controlled at 20°C-40°C. Sodium aluminate is added under stirring, and the amount of potassium aluminate added is 1.5-2.5 times the molar content of chloride ions in the filtrate E. The addition time of sodium aluminate is controlled at 1.0h-1.5h. The timing starts from the beginning of the addition of sodium aluminate. After 30 minutes of reaction, oxidizing gas is blown in. The aeration reaction is carried out for 2.0h-3.0h. Impurity chloride ions and aluminum calcium are removed by co-precipitation. The slurry is sent to a vacuum belt conveyor for filtration to obtain aluminum calcium slag and filtrate F. The aluminum calcium slag is used as a building material auxiliary material, and the filtrate F is the purified liquid returned to the desulfurization system for pulping and recycling.
[0030] In the present invention:
[0031] In step 1), a sufficient amount of calcium sulfate is added, preferably, the ratio of the amount of calcium sulfide added to the total molar content of zinc, lead and cadmium in the desulfurization filtrate is 1.05-1.5:1.
[0032] The calcium sulfide described in step 1) can be replaced by ammonium sulfide. The ammonium introduced after the replacement is removed together with the original ammonium ions during the treatment process in step 2). However, calcium sulfide is cheap, and the introduced calcium ions will form precipitation with sulfate ions. In addition, for the desulfurization system, calcium ions are not "impurities", so calcium sulfide is preferred.
[0033] The oxidizing gas in step 3) refers to a mixed gas composed of ozone and air prepared by an ozone generator using air as the gas source, and the aeration flow rate per liter of filtrate is 2L / min;
[0034] The reaction pool 1, reaction pool 2 and reaction pool 3 should not be understood as special or single-use equipment. For example, under conditions of low production load or intermittent production, when reaction pool 1 is empty, i.e., without material, it can be used as reaction pool 3. Similarly, reaction pool 2 can be used as reaction pool 1.
[0035] Compared with the prior art, the present invention has the following advantages:
[0036] 1. The method for treating the flue gas desulfurization filtrate in the secondary zinc oxide production industry of the present invention can remove various ions Zn that affect the flue gas desulfurization efficiency and gypsum quality. 2+ , Pb 2+ 、Ni 2+ 、Cd 2+ NH + 4 Mg 2+ , Cl - 、SO 2- 4The filtrate after effective reduction and removal of impurity ions can be recycled without discharging wastewater. The slag produced can be harmlessly recycled, ensuring that the flue gas emission meets the standards and produces high-quality gypsum products, avoiding the difficulty in dehydrating gypsum slag and affecting desulfurization production.
[0037] 2. The method for treating the flue gas desulfurization filtrate in the secondary zinc oxide production industry described in the present invention has a simple process, low reagent cost, and the required process equipment is easy to operate and maintain. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 The present invention is a process flow chart of a method for treating a flue gas desulfurization filtrate from a kiln in the zinc oxide production industry. DETAILED DESCRIPTION
[0039] In combination with the description of the above technical solution and the process flow chart, the technical solution is described in detail, clearly and completely through embodiments below, but the described embodiments are only some representative examples of the solution of the present invention and cannot be understood as limiting the solution of the present invention. Example
[0040] A method for treating a flue gas desulfurization filtrate of a kiln in a zinc oxide production industry, comprising the following steps:
[0041] 1) The desulfurized gypsum slurry is extracted from the desulfurization tower, and the desulfurized gypsum and desulfurized filtrate A are obtained by vacuum belt conveyor filtration. The desulfurized filtrate A is sent to the reaction tank 1. The main components of the desulfurized filtrate A are sampled and tested as shown in Table 1. Under stirring, according to the test results of the filtrate in Table 1, it is calculated that the total molar content of zinc, lead, cadmium and nickel is about 0.0145 mol / L. Calcium sulfide is added in an amount of 0.0152 mol / L to remove heavy metal impurities such as zinc, lead, cadmium and cadmium. At this time, the ratio of the amount of calcium sulfide added to the total molar content of zinc, lead, cadmium and nickel in the desulfurized filtrate A is 1.05:1. After 60 minutes of precipitation reaction, the slag B and filtrate C mainly composed of zinc sulfide, lead sulfide, cadmium sulfide and calcium sulfate are obtained. The slag B is returned to the secondary zinc oxide production section for recycling and treatment. The test results of the filtrate C after heavy metal removal are shown in Table 1;
[0042] 2) The filtrate C is sent to the reaction tank 2, and under stirring, the NH 4 + Mg 2+ 、SO 2- 4 The molar content of ions is known as NH 4 + Mg 2+ The sum of the contents of K 1 is 1.6096 mol / L, SO 2-4 Molar content of ions K 2 is 1.1011 mol / L, at this time K 2 <K 1 ≤2K 2 Therefore, the amount of calcium dihydrogen phosphate added is K 3 =0.7(K 1 +K 2 ) is added, that is, the amount of calcium dihydrogen phosphate added K 3 The pH value is 1.8975 mol / L, the temperature is controlled between 20℃-40℃, and the pH value is adjusted to four steps of 1.5-2.5, 7-8, 8-9, and 9-11 by calcium hydroxide. Each pH step is kept for 60 minutes. After completion, the impurities ammonium ions, magnesium ions, phosphate and sulfate ions form a complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain filtrate E and complex salt slag D. The test results of filtrate E are shown in Table 1. Complex salt slag D is ammonium thiophosphate calcium magnesium complex salt crystals, which are rich in plant nutrients such as sulfur, phosphorus, magnesium, nitrogen, potassium and calcium, and can be used as a multi-element slow-release fertilizer as a raw material and auxiliary material and widely used in various agricultural compound fertilizer products;
[0043] 3) The filtrate E is sent to the reaction tank 3, and the Cl content in the filtrate E is - The molar content of ions is 0.2327 mol / L, according to Cl - away from SO 2- 4 Calcium sulfide was added at 3.0 times the molar content of the sulfide, that is, the amount of calcium sulfide added was 0.6980 mol / L, the reaction temperature was controlled at 20℃-40℃, and the Cl - Potassium aluminate is added at 1.5 times the molar content of the ions, that is, the amount of potassium aluminate added is 0.3490 mol / L. The addition time of potassium aluminate is controlled to complete the feeding within 1.5 hours. The timing starts from the beginning of the addition of potassium aluminate. After 30 minutes of reaction, a mixed oxidizing gas composed of ozone and air prepared by an ozone generator with air as the gas source is blown in. The aeration flow rate per liter of filtrate is 2 L / min. The aeration reaction is carried out for 3.0 hours. Impurity chloride ions and aluminum calcium are removed by co-precipitation. The slurry is sent to a vacuum belt conveyor for filtration to obtain aluminum calcium slag and filtrate F. The detection results of filtrate F are shown in Table 1. The aluminum calcium slag is used as an auxiliary material for building materials, and the filtrate F is the purified liquid returned to the desulfurization system for pulping and recycling.
[0044]
[0045] Embodiment 2:
[0046] The method for preparing high-chloride zinc sulfate suitable for high-quality trace element premix feed comprises the following steps:
[0047] 1) The desulfurized gypsum slurry is extracted from the desulfurization tower, and the desulfurized gypsum and desulfurized filtrate A are obtained by vacuum belt conveyor filtration. The desulfurized filtrate A is sent to the reaction tank 1. The main components of the desulfurized filtrate A are sampled and tested as shown in Table 2. Under stirring, according to the test results of the filtrate in Table 2, it is calculated that the total molar content of zinc, lead, cadmium and nickel is about 0.0070 mol / L. Calcium sulfide is added in an amount of 0.0084 mol / L to remove heavy metal impurities such as zinc, lead, cadmium and cadmium. At this time, the ratio of the amount of calcium sulfide added to the total molar content of zinc, lead, cadmium and nickel in the desulfurized filtrate A is 1.2:1. After 30 minutes of precipitation reaction, it is pumped to the vacuum belt conveyor for filtration to obtain slag B and filtrate C mainly composed of zinc sulfide, lead sulfide, cadmium sulfide and calcium sulfate. The slag B is returned to the secondary zinc oxide production section for recycling and treatment. The test results of the filtrate C after heavy metal removal are shown in Table 2;
[0048] 2) Send the filtrate C into the reaction tank 2, and under stirring, according to the NH 4 + Mg 2+ 、SO 2- 4 The molar content of ions is known as NH 4 + Mg 2+ The sum of the contents of K 1 is 1.6942 mol / L, SO 2- 4 Molar content of ions K 2 is 0.8449 mol / L, at this time K 1 >2K 2 Therefore, the amount of calcium dihydrogen phosphate added is K 3 =0.6K 1 Add, that is, add the amount of monocalcium phosphate K 3 The pH value is 1.0165 mol / L, the temperature is controlled between 20℃-40℃, and the pH value is adjusted to 1.5-2.5, 7-8, 8-9, and 9-11 by calcium hydroxide. Each pH step is kept for 60 minutes. After completion, the impurities ammonium ions, magnesium ions, phosphate and sulfate ions form a complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain filtrate E and complex salt slag D. The test results of filtrate E are shown in Table 2. Complex salt slag D is ammonium thiophosphate calcium magnesium complex salt crystals, which are rich in plant nutrients such as sulfur, phosphorus, magnesium, nitrogen, potassium and calcium, and can be used as a multi-element slow-release fertilizer as a raw material and auxiliary material and widely used in various agricultural compound fertilizer products;
[0049] 3) The filtrate E is sent to the reaction tank 3, and the Cl content in the filtrate E is - The molar content of ions is 0.2409 mol / L, according to Cl - away from SO 2- 4Calcium sulfide was added at 4.5 times the molar content of the sulfide, that is, the amount of calcium sulfide added was 1.0838 mol / L, the reaction temperature was controlled at 20℃-40℃, and the Cl - Potassium aluminate was added at 2.5 times the molar content of the ions, that is, the amount of potassium aluminate added was 0.6021 mol / L, and the addition time of potassium aluminate was controlled to complete the feeding within 1.0 h. The timing was started from the beginning of the addition of potassium aluminate. After 30 minutes of reaction, a mixed oxidizing gas composed of ozone and air prepared by an ozone generator with air as the gas source was blown in. The aeration flow rate per liter of filtrate was 2 L / min, and the aeration reaction was carried out for 2.0 h. Impurity chloride ions and aluminum calcium were removed by co-precipitation, and the slurry was sent to a vacuum belt conveyor for filtration to obtain aluminum calcium slag and filtrate F. The test results of filtrate F are shown in Table 2. The aluminum calcium slag is used as an auxiliary material for building materials, and the filtrate F is the purified liquid returned to the desulfurization system for pulping and recycling.
[0050]
[0051] Embodiment 3:
[0052] The method for preparing high-chloride zinc sulfate suitable for high-quality trace element premix feed comprises the following steps:
[0053] 1) The desulfurized gypsum slurry is extracted from the desulfurization tower, and the desulfurized gypsum and desulfurized filtrate A are obtained by vacuum belt conveyor filtration. The desulfurized filtrate A is sent to the reaction tank 1. The main components of the desulfurized filtrate A are sampled and tested as shown in Table 3. Under stirring, according to the test results of the filtrate in Table 3, it is calculated that the total molar content of zinc, lead, cadmium and nickel is about 0.0079 mol / L. Calcium sulfide is added in an amount of 0.0118 mol / L to remove heavy metal impurities such as zinc, lead, cadmium and cadmium. At this time, the ratio of the amount of calcium sulfide added to the total molar content of zinc, lead, cadmium and nickel in the desulfurized filtrate A is 1.5:1. After 45 minutes of precipitation reaction, it is pumped to the vacuum belt conveyor for filtration to obtain slag B and filtrate C mainly composed of zinc sulfide, lead sulfide, cadmium sulfide and calcium sulfate. The slag B is returned to the secondary zinc oxide production section for recycling and treatment. The test results of the filtrate C after heavy metal removal are shown in Table 3;
[0054] 2) Send the filtrate C into the reaction tank 2, and under stirring, according to the NH 4 + Mg 2+ 、SO 2- 4 The molar content of ions is known as NH 4 + Mg 2+ The sum of the contents of K 1 is 1.1953 mol / L, SO 2- 4 Molar content of ions K 2 is 0.9253 mol / L, at this time K2 <K 1 ≤2K 2 Therefore, the amount of calcium dihydrogen phosphate added is K 3 =0.7(K 1 +K 2 ) is added, that is, the amount of calcium dihydrogen phosphate added K 3 The pH value is 1.4844 mol / L, the temperature is controlled between 20℃-40℃, and the pH value is adjusted to 1.5-2.5, 7-8, 8-9, and 9-11 by calcium hydroxide. Each pH step is kept for 45 minutes. After completion, the impurities ammonium ions, magnesium ions, phosphate and sulfate ions form a complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain filtrate E and complex salt slag D. The test results of filtrate E are shown in Table 3. Complex salt slag D is ammonium sulfate phosphate calcium magnesium complex salt crystals, which are rich in plant nutrients such as sulfur, phosphorus, magnesium, nitrogen, potassium and calcium. It can be used as a multi-element slow-release fertilizer as a raw material and auxiliary material and is widely used in various agricultural compound fertilizer products;
[0055] 3) The filtrate E is sent to the reaction tank 3, and the Cl content in the filtrate E is - The molar content of ions is 0.4944 mol / L, according to Cl - away from SO 2- 4 Calcium sulfide was added at 3.5 times the molar content of the sulfide, that is, the amount of calcium sulfide added was 1.7303 mol / L, the reaction temperature was controlled at 20℃-40℃, and the Cl - Potassium aluminate was added at 2.0 times the molar content of the ions, that is, the amount of potassium aluminate added was 0.9887 mol / L. The addition time of potassium aluminate was controlled to complete the feeding within 1.2 h. The timing was started from the beginning of the addition of potassium aluminate. After 30 minutes of reaction, a mixed oxidizing gas composed of ozone and air prepared by an ozone generator with air as the gas source was blown in. The aeration flow rate per liter of filtrate was 2 L / min. The aeration reaction was carried out for 2.5 hours. Impurity chloride ions and aluminum calcium were removed by co-precipitation. The slurry was sent to a vacuum belt conveyor for filtration to obtain aluminum calcium slag and filtrate F. The test results of filtrate F are shown in Table 3. The aluminum calcium slag is used as an auxiliary material for building materials, and the filtrate F is the purified liquid returned to the desulfurization system for pulping and recycling.
[0056]
[0057] Embodiment 4:
[0058] A method for treating a flue gas desulfurization filtrate of a kiln in a zinc oxide production industry, comprising the following steps:
[0059] 1) The desulfurized gypsum slurry is extracted from the desulfurization tower, and the desulfurized gypsum and desulfurized filtrate A are obtained by vacuum belt conveyor filtration. The desulfurized filtrate A is sent to the reaction tank 1. The main components of the desulfurized filtrate A are sampled and tested as shown in Table 4. Under stirring, according to the test results of the filtrate in Table 4, it is calculated that the total molar content of zinc, lead, cadmium and nickel is about 0.0099 mol / L. Calcium sulfide is added in an amount of 0.0129 mol / L to remove heavy metal impurities such as zinc, lead, cadmium and cadmium. At this time, the ratio of the amount of calcium sulfide added to the total molar content of zinc, lead, cadmium and nickel in the desulfurized filtrate A is 1.3:1. After 30 minutes of precipitation reaction, it is pumped to the vacuum belt conveyor for filtration to obtain slag B and filtrate C mainly composed of zinc sulfide, lead sulfide, cadmium sulfide and calcium sulfate. The slag B is returned to the secondary zinc oxide production section for recycling and treatment. The test results of the filtrate C after heavy metal removal are shown in Table 4;
[0060] 2) The filtrate C is sent to the reaction tank 2, and under stirring, the NH 4 + Mg 2+ 、SO 2- 4 The molar content of ions is known as NH 4 + Mg 2+ The sum of the contents of K 1 is 1.1087mol / L, SO 2- 4 Molar content of ions K 2 is 1.1705mol / L, at this time K 1 <K 2 Therefore, the amount of calcium dihydrogen phosphate added is K 3 =1.1K 2 Add, that is, add the amount of monocalcium phosphate K 3 The pH value is 1.2876 mol / L, the temperature is controlled between 20℃-40℃, and the pH value is adjusted to 1.5-2.5, 7-8, 8-9, and 9-11 by calcium hydroxide. Each pH step is kept for 30 minutes. After completion, the impurities ammonium ions, magnesium ions, phosphate and sulfate ions form a complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain filtrate E and complex salt slag D. The test results of filtrate E are shown in Table 4. Complex salt slag D is ammonium thiophosphate calcium magnesium complex salt crystals, which are rich in plant nutrients such as sulfur, phosphorus, magnesium, nitrogen, potassium and calcium. It can be used as a multi-element slow-release fertilizer as a raw material and auxiliary material and is widely used in various agricultural compound fertilizer products;
[0061] 3) The filtrate E is sent to the reaction tank 3, and the Cl content in the filtrate E is - The molar content of ions is 0.4068 mol / L, according to Cl - away from SO 2- 4Calcium sulfide was added at 4.0 times the molar content of the sulfide, that is, the amount of calcium sulfide added was 1.6270 mol / L, the reaction temperature was controlled at 20℃-40℃, and the Cl - Potassium aluminate was added at 2.0 times the molar content of the ions, that is, the amount of potassium aluminate added was 0.7322 mol / L. The addition time of potassium aluminate was controlled to complete the feeding within 1.5 h. The timing was started from the beginning of the addition of potassium aluminate. After 30 minutes of reaction, a mixed oxidizing gas composed of ozone and air prepared by an ozone generator with air as the gas source was blown in. The aeration flow rate per liter of filtrate was 2 L / min. The aeration reaction was carried out for 3.0 h. Impurity chloride ions and aluminum calcium were removed by co-precipitation. The slurry was sent to a vacuum belt conveyor for filtration to obtain aluminum calcium slag and filtrate F. The test results of filtrate F are shown in Table 4. The aluminum calcium slag was used as an auxiliary material for building materials, and the filtrate F was the purified liquid returned to the desulfurization system for pulping and recycling.
[0062]
[0063] The above description is only a preferred embodiment of the present invention. It should be pointed out that, for ordinary technicians in this field, without departing from the creative concept of the present invention, several improvements and changes can be made, which all belong to the protection scope of the present invention.
Claims
1. A method for treating the filtrate of flue gas desulfurization in the secondary zinc oxide production industry, characterized in that: The steps include: 1) The desulfurized gypsum slurry of the kiln flue gas of the secondary zinc oxide production industry is extracted from the desulfurization tower, and the desulfurized gypsum and desulfurized filtrate A are obtained by filtration through a vacuum belt conveyor. The desulfurized filtrate A is sent to the reaction tank 1. Under stirring, sufficient calcium sulfide is added according to the total content of zinc, lead and cadmium in the filtrate to remove heavy metal impurities of zinc, lead and cadmium. After precipitation reaction for 30min-60min, the slag B and filtrate C mainly containing zinc sulfide, lead sulfide, cadmium sulfide and calcium sulfate are obtained. The slag B is returned to the secondary zinc oxide production section for recycling and treatment; 2) The filtrate C is sent to the reaction tank 2. Under stirring, a certain amount of calcium dihydrogen phosphate is added according to the molar content of ammonium ions, magnesium ions and sulfate ions in the filtrate C, so that the molar content of ammonium ions, magnesium ions, sulfate ions and phosphate ions is controlled within a certain ratio range, the temperature is controlled between 20°C and 40°C, and the pH value is gradually adjusted to four steps of 1.5-2.5, 7-8, 8-9 and 9-11 with calcium hydroxide. Each pH step is kept for 30min-60min. After completion, the impurities ammonium ions, magnesium ions, phosphate ions and sulfate ions generate complex salt co-precipitation mixed slag, and the slurry is sent to a vacuum belt conveyor for filtration to obtain filtrate E and complex salt slag D. The complex salt slag D is ammonium calcium magnesium sulfate phosphate complex salt crystals, which are rich in sulfur, phosphorus, magnesium, nitrogen, potassium and calcium plant nutrients and can be used as a multi-element slow-release fertilizer raw material; The relationship between the amount of calcium dihydrogen phosphate added and the molar content ratio of ammonium ions, magnesium ions and sulfate in the filtrate C is as follows: the sum of the molar content of ammonium ions and the molar content of magnesium ions is marked as K1, the molar content of sulfate is marked as K2, and the molar amount of calcium dihydrogen phosphate added is marked as K3; When K1≤K2, the amount of calcium dihydrogen phosphate added is K3=1.1K2; When K2<K1≤2K2, the amount of calcium dihydrogen phosphate added is K3=0.7(K1+K2); When K1>2K2, the amount of calcium dihydrogen phosphate added is K3=0.6K1; 3) The filtrate E is sent to the reaction tank 3, and calcium sulfide is added according to the chloride ion content in the filtrate E. The amount of calcium sulfide added is 3.0-4.5 times the molar content of chloride ions in the filtrate E. The reaction temperature is controlled at 20°C-40°C. Sodium aluminate is added under stirring, and the amount of potassium aluminate added is 1.5-2.5 times the molar content of chloride ions in the filtrate E. The addition time of sodium aluminate is controlled at 1.0h-1.5h. The timing starts from the beginning of the addition of sodium aluminate. After 30 minutes of reaction, oxidizing gas is blown in. The aeration reaction is carried out for 2.0h-3.0h. Impurity chloride ions and aluminum calcium are removed by co-precipitation. The slurry is sent to a vacuum belt conveyor for filtration to obtain aluminum calcium slag and filtrate F. The aluminum calcium slag is used as a building material auxiliary material, and the filtrate F is the purified liquid returned to the desulfurization system for pulping and recycling.
2. The method for treating the flue gas desulfurization filtrate of the secondary zinc oxide production industry according to claim 1, characterized in that: The adding of sufficient amount of calcium sulfate in step 1) means that the ratio of the amount of calcium sulfide added to the total molar content of zinc, lead and cadmium in the desulfurization filtrate is 1.05-1.5:
1.
3. The method for treating the flue gas desulfurization filtrate of the secondary zinc oxide production industry according to claim 1, characterized in that: The oxidizing gas described in step 3) refers to a mixed gas composed of ozone and air prepared by an ozone generator using air as the gas source, and the aeration flow rate per liter of filtrate is 2L / min.
Citation Information
Patent Citations
A pretreatment process for the resource utilization of hardness ions in desulfurization wastewater
CN106007046B
A method and apparatus for treating desulfurization wastewater
CN106430786B
A method for treating desulfurization wastewater
CN113511754B
Efficient low rank coal gasification, combustion, and processing systems and methods
AU2010249327B2
Catalytic converter for converting reactants of a gas mixture
CA2115723A1