Preparation and application method of high temperature and high pressure resistant foam slow acid solution

By adding nano SiO2 and foam stabilizer to the foam acid solution, a foam slow acid solution that is resistant to high temperature and high pressure is formed, which solves the problem of poor stability of existing foam acid solution in high temperature and high pressure environments, and achieves the extension of foam half-life and improve construction results.

CN116004217BActive Publication Date: 2024-11-22HANZHONG JUZHIDAYUAN HUANNENG TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211529919.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-30
Publication Date
2024-11-22
Estimated Expiration
2042-11-30

AI Technical Summary

Technical Problem

The existing foam acid solution has poor stability in high temperature and high pressure environments, and the foam half-life is short, which affects the construction effect of acidification and fracturing.

Method used

0.5 wt% to 0.8% foaming agent, 0.1 wt% to 0.3 wt% nano SiO2 and 0.05 wt% to 0.1 wt% foaming agent were prepared in 20% HCl solution, and the high temperature resistance was formed by stirring by a stirrer. High pressure foam slow acid solution, the foam stabilizer is a mixture of polyacrylamide, cellulose, polyvinyl alcohol, and polyethylene glycol, nano SiO2 is a mixture of different particle sizes, and the foaming agent is a cationic and nonionic surfactant compound system of agent.

Benefits of technology

The foam half-life reaches 12 minutes at 140°C and does not change much with the increase of pressure, which significantly improves the stability of the foam and reduces the core dissolution rate. It is suitable for deep well development.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116004217B_ABST
    Figure CN116004217B_ABST
Patent Text Reader

Abstract

The invention discloses a method for preparing a foam retarded acid solution resistant to high temperature and high pressure and an application method thereof. A foam retarded acid solution resistant to high temperature and high pressure comprises 0.5wt% to 0.8wt% of a foaming agent, 0.1wt% to 0.3wt% of nano-SiO2, 0.05wt% to 0.1wt% of a foam stabilizer, and the rest is a 20% by mass HCl solution, with the total weight of the foam retarded acid solution being 100%. The preparation process is to sequentially add a foaming agent, nano-SiO2, and a foam stabilizer to a 20% by mass HCl solution, and stir with a stirrer to obtain the foam retarded acid solution. The high temperature and high pressure resistant foam retarded acid solution of the present invention can still achieve a foam half-life of 12 minutes at 140°C, and with the increase of pressure, the foam half-life does not change much, the stability is good, and the solution is particularly suitable for deep well development; the high temperature and high pressure resistant foam retarded acid solution of the present invention adopts nano-SiO2 in combination with a foaming agent and a foam stabilizer, which plays a synergistic role, making the foam retarded acid solution more widely applicable and having good foam stability under high temperature and high pressure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of oilfield chemical additives, and more specifically, relates to a preparation method of a high-temperature and high-pressure resistant foam retarding acid solution and an application method thereof. Background Art

[0002] Foam is a multiphase dispersion system in which gas is dispersed in liquid, where gas is the dispersed phase (discontinuous phase) and liquid is the dispersion medium (continuous phase). In the process of preparing foam, bubbles in liquid tend to form a bubble aggregate on the liquid surface due to density difference, in which gas is separated by a liquid film composed of a small amount of liquid - foam. The foamability of foam refers to the ease of foam generation and the amount of foam generated; the stability of foam refers to the durability (lifespan) of the generated foam, that is, the ease of defoaming.

[0003] The stability of foam can be measured by the foam drainage rate or the foam half-life. Obviously, the more stable the foam is, the slower the drainage rate is and the longer the half-life is. The foam half-life is the time required for the volume of liquid discharged from the foam to be half of the total liquid volume when the foam is not drained.

[0004] Let V0: the volume of liquid in the foam (i.e. the volume of foaming liquid);

[0005] V t : The volume of liquid discharged by the foam at time t;

[0006] V0-V t : The volume of liquid removed from the foam, which decreases with time.

[0007] The instantaneous discharge speed is: -d(V0-V t ) / d=K(V0-V t )n or dV / dt=K(V0-V t )n where n is called the drainage series and K is called the proportional constant, which is related to factors such as temperature, liquid density, liquid viscosity, foam height, gravity, etc.

[0008] In recent years, with the gradual maturity of acid fracturing technology, it has become an indispensable and important means for the exploration and development of oil and gas. Foam acid has become an important component of the acid fracturing process because of its advantages of high viscosity, high return rate and low filtration loss. Conventional foam acid systems only use a single foaming agent. Although the foaming property is good, the foam is less stable under the influence of factors such as high temperature and high pressure in the actual formation environment, resulting in a short foam half-life, which seriously reduces the retarding performance of the foam acid and ultimately affects the construction effect. Therefore, the development of a foam retarding acid system that is resistant to high temperature and high pressure is of great significance to acid fracturing. Summary of the invention

[0009] In view of the above defects or improvement needs of the prior art, the present invention provides a foam retarded acid liquid with a foam half-life of 12 minutes at 140°C, and with little change in the foam half-life as the pressure increases, and has good stability. The foam retarded acid liquid is particularly suitable for high temperature and high pressure resistant foam in deep well development.

[0010] According to one aspect of the present invention, a high temperature and high pressure resistant foam retarded acid solution is provided, which comprises the following components, calculated by mass percentage, with the total weight of the foam retarded acid solution being 100%:

[0011] 0.5 wt% to 0.8 wt% of a foaming agent;

[0012] 0.1wt% to 0.3wt% of nano-SiO2;

[0013] 0.05wt% to 0.1wt% of a foam stabilizer;

[0014] The rest is HCl solution with a mass fraction of 20%;

[0015] The foam stabilizer is a mixture of polyacrylamide and one or two of cellulose, polyvinyl alcohol, polyethylene glycol and polyvinyl butyral in a mass ratio of (15-45):(4-10).

[0016] Furthermore, the nano-SiO2 is a mixture of two SiO2 with different particle sizes ranging from 50nm to 500nm prepared in a mass ratio of (20-50):(3-10).

[0017] Furthermore, the foaming agent is a composite foaming system prepared by a cationic surfactant and a non-ionic surfactant in a mass ratio of (35-45):(10-20).

[0018] Further, the cationic surfactant is one of octadecyl ammonium chloride, hexadecyl trimethyl ammonium chloride, tetradecyl dimethyl pyridinium bromide and quinoline benzyl ammonium chloride;

[0019] The nonionic surfactant is one of lauryl alcohol polyoxyethylene ether, hexadecyl polyoxyethylene ether and nonylphenol polyoxyethylene ether.

[0020] According to a second aspect of the present invention, a method for preparing a high-temperature and high-pressure resistant foam-retarded acid solution is provided, comprising the following preparation process: 0.5wt% to 0.8wt% of a foaming agent, 0.1wt% to 0.3wt% of nano-SiO2, and 0.05wt% to 0.1wt% of a foam stabilizer are sequentially added to a 20wt% HCl solution, and stirred with a stirrer to obtain the foam-retarded acid solution.

[0021] Furthermore, the rotation speed of the agitator is 7500-8500 r / min.

[0022] Furthermore, the stirring time after adding the foaming agent is 3 to 5 minutes.

[0023] According to a third aspect of the present invention, there is provided an application of a high temperature and high pressure resistant foam-retarded acid solution, which comprises the foam-retarded acid solution as described above, and the foam-retarded acid solution is used for oilfield chemical additive production enhancement operations.

[0024] In general, the above technical solutions conceived by the present invention can achieve the following beneficial effects compared with the prior art:

[0025] 1. The foam stabilizer in the high temperature and high pressure resistant foam retarding acid solution of the present invention makes the liquid film thicker, and the silicon dioxide particles make the foam denser. The foam stabilizer component used in the present invention is a polymer, and the molecular chain is a relatively long macromolecule. The hydrophobic functional group causes the surfactant to aggregate, and after aggregation, a composite micelle is formed. The composite micelle is cross-linked with other polymers to form a composite network structure. The foaming agent and the foam stabilizer act synergistically to make the liquid film more stable;

[0026] 2. The high temperature and high pressure resistant foam slow acid solution of the present invention can still have a foam half-life of 12 minutes at 140°C, and with the increase of pressure, the foam half-life does not change much, has good stability, and is particularly suitable for deep well development;

[0027] 3. The high temperature and high pressure resistant foam retarding acid solution of the present invention adopts nano-SiO2 in combination with a foaming agent and a foam stabilizer, which plays a synergistic role, making the foam retarding acid solution more widely applicable and having good foam stability under high temperature and high pressure;

[0028] 4. The average dissolution rate of the high temperature and high pressure resistant foam slow acid solution of the present invention is 1.148×10 - 3 mg / (cm 2 ·s) of 20% HCl base solution, the average core dissolution rate of the homemade foam slow acid solution was reduced to 7.142×10 -5 mg / (cm 2 ·s), which is reduced by two orders of magnitude and the slowdown rate reaches 93.7%. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 This is a test diagram of foam half-life of a high temperature and high pressure resistant foam retarder acid solution at different temperatures according to an embodiment of the present invention;

[0030] Figure 2 This is a test diagram of the foam half-life of a high temperature and high pressure resistant foam retarder acid solution under different pressures according to an embodiment of the present invention. DETAILED DESCRIPTION

[0031] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0032] According to one aspect of the present invention, a high temperature and high pressure resistant foam retarded acid solution is provided, which comprises the following components, calculated by mass percentage, with the total weight of the foam retarded acid solution being 100%:

[0033] 0.5 wt% to 0.8 wt% of a foaming agent;

[0034] 0.1wt% to 0.3wt% of nano-SiO2;

[0035] 0.05wt% to 0.1wt% of a foam stabilizer;

[0036] The rest is HCl solution with a mass fraction of 20%;

[0037] The foam stabilizer is a mixture of polyacrylamide and one or two of cellulose, polyvinyl alcohol, polyethylene glycol and polyvinyl butyral in a mass ratio of (15-45):(4-10).

[0038] The nano-SiO2 is a mixture of two SiO2 particles with different particle sizes ranging from 50nm to 500nm in a mass ratio of (20-50):(3-10).

[0039] The foaming agent is a composite foaming system prepared by a cationic surfactant and a nonionic surfactant in a mass ratio of (35-45):(10-20).

[0040] The cationic surfactant is one of octadecyl ammonium chloride, hexadecyl trimethyl ammonium chloride, tetradecyl dimethyl pyridinium bromide and quinoline benzyl ammonium chloride;

[0041] The nonionic surfactant is one of lauryl alcohol polyoxyethylene ether, hexadecyl polyoxyethylene ether and nonylphenol polyoxyethylene ether.

[0042] According to a second aspect of the present invention, a method for preparing a high temperature and high pressure resistant foam retarded acid solution is provided, comprising the following preparation process:

[0043] 0.5wt%-0.8wt% of a foaming agent, 0.1wt%-0.3wt% of nano-SiO2, and 0.05wt%-0.1wt% of a foam stabilizer are sequentially added into a 20wt% HCl solution, and stirred with a stirrer to obtain the foam slow-speed acid solution.

[0044] The rotating speed of the stirrer is 7500-8500 r / min.

[0045] The stirring time after adding the foaming agent is 3 to 5 minutes.

[0046] According to a third aspect of the present invention, there is provided an application of a high temperature and high pressure resistant foam-retarded acid solution, which comprises the foam-retarded acid solution as described above, and the foam-retarded acid solution is used for oilfield chemical additive production enhancement operations.

[0047] Embodiment 1:

[0048] A high temperature and high pressure resistant foam retarding acid solution, which comprises, based on the total weight of the foam retarding acid solution being 100%, 0.51wt% of octadecyl ammonium chloride, 0.09wt% of lauryl alcohol polyoxyethylene ether, 0.15wt% of SiO2 with a particle size of 50nm, 0.05wt% of SiO2 with a particle size of 100nm, 0.06wt% of polyacrylamide, 0.02wt% of polyvinyl alcohol and 99.12wt% of HCl solution with a mass fraction of 20%.

[0049] 0.03 polyacrylamide and 0.03 cellulose

[0050] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0051] 0.51wt% octadecyl ammonium chloride, 0.09wt% lauryl alcohol polyoxyethylene ether, 0.15wt% SiO2 with a particle size of 50nm, 0.05wt% SiO2 with a particle size of 100nm, 0.06wt% polyacrylamide, and 0.02wt% polyvinyl alcohol are added to 99.12wt% 20% HCl solution, and stirred at a speed of 8000r / min for 3min.

[0052] Example 2

[0053] A high temperature and high pressure resistant foam retarding acid solution, which comprises, based on the total weight of the foam retarding acid solution being 100%, 0.33wt% of octadecyl ammonium chloride, 0.17% of lauryl alcohol polyoxyethylene ether, 0.25wt% of SiO2 with a particle size of 100nm, 0.05wt% of SiO2 with a particle size of 200nm, 0.08wt% of polyacrylamide (TH-16005), 0.02wt% of polyethylene glycol and 99.1wt% of a 20% HCl solution.

[0054] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0055] 0.5wt% octadecyl ammonium chloride, 0.25wt% SiO2 with a particle size of 100nm, 0.05wt% SiO2 with a particle size of 200nm, 0.08wt% polyacrylamide (TH-16005), and 0.02wt% polyethylene glycol were added to 99.1wt% 20% HCl solution and stirred at 8000r / min for 3min.

[0056] Example 3

[0057] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0058] 0.53wt% hexadecyltrimethylammonium chloride, 0.17wt% hexadecyl polyoxyethylene ether, 0.20wt% SiO2 with a particle size of 200nm, 0.05wt% SiO2 with a particle size of 500nm, 0.08wt% polyacrylamide (TH-16010) and 98.97wt% HCl solution with a mass fraction of 20%.

[0059] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0060] 0.53wt% hexadecyltrimethylammonium chloride, 0.17wt% hexadecyl polyoxyethylene ether, 0.20wt% SiO2 with a particle size of 200nm, 0.05wt% SiO2 with a particle size of 500nm, and 0.08wt% polyacrylamide (TH-16010) were added to 98.97wt% HCl solution with a mass fraction of 20%, and stirred at a speed of 8000r / min for 3min.

[0061] Embodiment 4:

[0062] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0063] 0.48wt% tetradecyl-dimethylpyridinium bromide, 0.17wt% nonylphenol polyoxyethylene ether, 0.15wt% SiO2 with a particle size of 50nm, 0.05wt% SiO2 with a particle size of 200nm, 0.06wt% polyacrylamide, 0.04wt% polyvinyl alcohol and 99.05wt% HCl solution with a mass fraction of 20%.

[0064] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0065] 0.48wt% of tetradecyl-dimethylpyridinium bromide, 0.17wt% of nonylphenol polyoxyethylene ether, 0.15wt% of SiO2 with a particle size of 50nm, 0.05wt% of SiO2 with a particle size of 200nm, 0.06wt% of polyacrylamide, and 0.04wt% of polyvinyl alcohol were added to 99.05wt% of 20% HCl solution and stirred at 8000r / min for 3min.

[0066] Embodiment 5:

[0067] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0068] 0.6wt% tetradecyl-dimethylpyridinium bromide, 0.15wt% hexadecyl polyoxyethylene ether, 0.20wt% SiO2 with a particle size of 100nm, 0.05wt% SiO2 with a particle size of 500nm, 0.05wt% polyacrylamide (TH-16010), 0.04wt% polyvinyl butyral and 98.91wt% 20% HCl solution.

[0069] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0070] 0.6wt% of tetradecyl-dimethylpyridinium bromide, 0.15wt% of hexadecyl polyoxyethylene ether, 0.20wt% of SiO2 with a particle size of 100nm, 0.05wt% of SiO2 with a particle size of 500nm, 0.05wt% of polyacrylamide (TH-16010), and 0.04wt% of polyvinyl butyral are added to 98.91wt% of 20% HCl solution, and stirred at 8000r / min for 3min to obtain a high temperature and high pressure resistant foam slow acid solution.

[0071] Embodiment 6:

[0072] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0073] 0.47wt% hexadecyltrimethylammonium chloride, 0.13wt% lauryl alcohol polyoxyethylene ether, 0.12wt% SiO2 with a particle size of 50nm, 0.08wt% SiO2 with a particle size of 200nm, 0.05wt% polyacrylamide, 0.03wt% cellulose and 99.12wt% HCl solution with a mass fraction of 20%.

[0074] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0075] 0.47wt% hexadecyltrimethylammonium chloride, 0.13wt% lauryl alcohol polyoxyethylene ether, 0.12wt% SiO2 with a particle size of 50nm, 0.08wt% SiO2 with a particle size of 200nm, 0.05wt% polyacrylamide, and 0.03wt% cellulose are added into a 99.12wt% HCl solution with a mass fraction of 20%, and stirred for 4 minutes at 8500r / min to obtain a high temperature and high pressure resistant foam retarded acid solution.

[0076] Embodiment 7:

[0077] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0078] 0.67wt% quinoline benzyl ammonium chloride, 0.13wt% lauryl alcohol polyoxyethylene ether, 0.12wt% SiO2 with a particle size of 50nm, 0.06wt% SiO2 with a particle size of 200nm, 0.05wt% cellulose and 98.97wt% HCl solution with a mass fraction of 20%.

[0079] A foam retarded acid solution resistant to high temperature and high pressure is prepared by the following method:

[0080] 0.67wt% quinoline benzyl ammonium chloride, 0.13wt% lauryl alcohol polyoxyethylene ether, 0.12wt% SiO2 with a particle size of 50nm, 0.06wt% SiO2 with a particle size of 200nm, and 0.05wt% cellulose are added to 98.97wt% HCl solution with a mass fraction of 20%, and stirred at 7500r / min for 5min to obtain a high temperature and high pressure resistant foam slow acid solution.

[0081] Embodiment 8:

[0082] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0083] 0.8wt% foaming agent, the foaming agent is quinoline benzyl ammonium chloride and lauryl alcohol polyoxyethylene ether in a mass ratio of 35:20; 0.18wt% SiO2, wherein the ratio of SiO2 with a particle size of 50nm and SiO2 with a particle size of 200nm is 50:3; 0.05wt% foam stabilizer, the foam stabilizer is polyacrylamide and cellulose in a mass ratio of 15:10; and 98.97wt% HCl solution with a mass fraction of 20%.

[0084] Embodiment 9:

[0085] A high temperature and high pressure resistant foam retarded acid solution, based on the total weight of the foam retarded acid solution as 100%, comprising:

[0086] 0.8wt% foaming agent, the foaming agent is quinoline benzyl ammonium chloride and lauryl alcohol polyoxyethylene ether in a mass ratio of 45:10; 0.18wt% SiO2, wherein the ratio of SiO2 with a particle size of 50nm and SiO2 with a particle size of 200nm is 50:3; 0.05wt% foam stabilizer, the foam stabilizer is polyacrylamide and cellulose in a mass ratio of 45:4; and 98.97wt% HCl solution with a mass fraction of 20%.

[0087] Performance Test:

[0088] 1. Foam half-life test

[0089] Pour the prepared foam retarding acid solution into a 1L measuring cylinder, start a stopwatch at the same time, and record the time when the foam volume decays to half of the initial foam volume. The test results are shown in Table 1.

[0090] Table 1 Foam half-life determination table of different embodiments

[0091] Experimental content Example 1 Example 2 Example 3 Example 4 Example 5 Example 6 Bubble half-life / s 1436.85 1365.87 1602.61 1565.81 1468.04 1512.66

[0092] It can be seen from Table 1 that the foam retarding acid solution has a foam half-life greater than 20 min at a dosage of 0.5-0.8%. The foam retarding acid solution prepared in Example 3 has the best foam half-life measurement result. The following high temperature and high pressure resistance tests are all for Example 3.

[0093] 2. Foam temperature resistance test

[0094] Please refer to Figure 1 The foam slow acid solution prepared in Example 3 was poured into the foam fluid sand carrying capacity evaluation device, the temperature was set, and the foam half-life at different temperatures was tested. The test results are shown in Table 2.

[0095] Table 2 Foam half-life determination table at different temperatures

[0096] Experimental content 90℃ 100℃ 110℃ 120℃ 130℃ 140℃ Bubble half-life / s 1179.93 1102.45 1021.51 968.52 847.65 723.43

[0097] It can be seen from Table 2 that with the continuous increase of temperature, the foam half-life gradually decreases, but it is still greater than 12 minutes at 140°C, and the high temperature resistance is excellent.

[0098] 3. Foam pressure resistance test

[0099] Please refer to Figure 1 The foam slow acid solution prepared in Example 3 was poured into the foam fluid sand carrying capacity evaluation device, and the high-temperature autoclave was pressed with nitrogen to test the foam half-life under different pressures. The test results are shown in Table 3.

[0100] Table 3 Foam half-life determination table under different pressures

[0101] Experimental content 2Mpa 4Mpa 6Mpa 8Mpa 10Mpa 12Mpa Bubble half-life / s 1598.37 1521.65 1468.10 1432.76 1398.52 1341.78

[0102] It can be seen from Table 3 that with the continuous increase of pressure, the foam half-life changes little and the pressure resistance performance is excellent.

[0103] 4. Retarding performance test

[0104] The foam slow-rate acid solution prepared in Example 3 was poured into a GGSD71 high-temperature and high-pressure corrosion tester to measure the core acid-rock reaction rate at 90°C and 12MPa, and the average acid-rock reaction rate was calculated. And the slowing rate K, the calculation formula is as follows:

[0105] Acid-rock reaction rate unit: mg / (cm 2 ·s)

[0106]

[0107] Where Δm is the dissolved mass of the rock sample (g); S is the total surface area of ​​the rock sample (cm 2 );Δt is the reaction time (s).

[0108] (b) Average acid-rock reaction rate Unit: mg / (cm 2 ·s)

[0109]

[0110] Where n is the number of trials.

[0111] (c) Slowdown rate

[0112]

[0113] Where, K is the slowing rate (%); is the average acid-rock reaction rate of the full acid solution (mg / (cm 2 ·s)); is the average acid-rock reaction rate of the blank acid solution (mg / (cm 2 ·s)).

[0114] The specific test results are shown in Table 4.

[0115] Table 4 Example 3 Acid-rock reaction rate determination

[0116]

[0117] It can be seen from Table 4 that compared with the average core dissolution rate of 1.148×10 -3 mg / (cm 2 ·s) of 20% HCl base solution, the average core dissolution rate of the laboratory-made foam slow acid solution was reduced to 7.142×10-5 mg / (cm 2 ·s), which is reduced by two orders of magnitude and the slowdown rate reaches 93.7%.

[0118] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A foam retarded acid solution resistant to high temperature and high pressure, characterized in that: Calculated by weight percentage, the total weight of the foam retarded acid solution is 100%, and includes the following components: 0.5 wt% to 0.8 wt% of a foaming agent; 0.1wt% to 0.3wt% of nano-SiO2; 0.05wt% to 0.1wt% of a foam stabilizer; The rest is HCl solution with a mass fraction of 20%; The foam stabilizer is a mixture of polyacrylamide and one or two of cellulose, polyvinyl alcohol, polyethylene glycol, and polyvinyl butyral in a mass ratio of (15-45):(4-10); The nano-SiO2 is a mixture of two SiO2 particles with different particle sizes of 50nm-500nm in a mass ratio of (20-50):(3-10); The foaming agent is a composite foaming system prepared by a cationic surfactant and a nonionic surfactant in a mass ratio of (35-45): (10-20); The cationic surfactant is one of octadecyl ammonium chloride, hexadecyl trimethyl ammonium chloride, tetradecyl dimethyl pyridinium bromide and quinoline benzyl ammonium chloride; The nonionic surfactant is one of lauryl alcohol polyoxyethylene ether, hexadecyl polyoxyethylene ether and nonylphenol polyoxyethylene ether.

2. The method for preparing a high temperature and high pressure resistant foam slow acid solution according to claim 1, characterized in that: The preparation process includes the following: 0.5wt% to 0.8wt% of a foaming agent, 0.1wt% to 0.3wt% of nano-SiO2, and 0.05wt% to 0.1wt% of a foam stabilizer are sequentially added to a 20wt% HCl solution, and stirred with a stirrer to obtain the foam slow-speed acid solution.

3. The method for preparing a high temperature and high pressure resistant foam retarded acid solution according to claim 2, characterized in that: The rotating speed of the stirrer is 7500-8500 r / min.

4. The method for preparing a high temperature and high pressure resistant foam retarded acid solution according to claim 2, characterized in that: The stirring time after adding the foaming agent is 3 to 5 minutes.

5. An application of a high temperature and high pressure resistant foam-retarded acid solution, comprising the foam-retarded acid solution as claimed in claim 1, wherein the foam-retarded acid solution is used for oilfield chemical additive production enhancement operations.