A method for catalytically producing hydrogen and simultaneously producing light olefins

Through the catalytic decomposition reaction of hydrocarbon raw materials in the fluidization reactor and the catalyst regeneration cycle, the high cost and environmental protection problems in the existing hydrogen production technology are solved, the production of high-efficiency hydrogen and low-carbon olefins is achieved, and energy utilization and Carbon capture.

CN116004274BActive Publication Date: 2024-12-06CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111229710.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-22
Publication Date
2024-12-06
Estimated Expiration
2041-10-22

AI Technical Summary

Technical Problem

Among the existing hydrogen production technologies, natural gas reforming hydrogen production and coal hydrogen production have high costs, environmental protection problems and high energy consumption, which is difficult to meet the demand for growth in hydrogen demand and low-carbon olefin production.

Method used

Hydrocarbon raw materials and water vapor are used to carry out catalytic decomposition reaction in the fluidization reactor, combined with the catalyst regeneration cycle, hydrogen and low-carbon olefins are separated, and flue gas resource utilization is optimized through low-temperature incomplete regeneration technology.

Benefits of technology

It reduces the energy consumption of the hydrogen production process, reduces the cost of natural gas, achieves efficient production of hydrogen and low-carbon olefins, alleviates the tension in the energy structure, and reduces carbon emissions through carbon capture.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116004274B_ABST
    Figure CN116004274B_ABST
Patent Text Reader

Abstract

A method for catalytically producing hydrogen and simultaneously producing low-carbon olefins, wherein a hydrocarbon raw material is mixed with water vapor, introduced into a fluidized reactor to contact with a catalyst and undergo a catalytic decomposition reaction to obtain a reactant stream and a carbon-bearing catalyst; the reaction oil and gas obtained by the catalytic decomposition reaction and the deactivated catalyst are subjected to gas-solid separation; the reaction oil and gas are separated to obtain products including hydrogen, CO, CO2, low-carbon olefins and other hydrocarbons; the deactivated catalyst is sent to a regenerator for regeneration, and after the deactivated catalyst is regenerated by burning, it is returned to the fluidized reactor for recycling, and the regenerated flue gas is separated to obtain CO and CO2. The method of the present invention converts low-value hydrocarbon raw materials into hydrogen and low-carbon olefins, realizes the high-value utilization of petroleum resources, and at the same time realizes CO2 enrichment, which is beneficial to carbon recovery and utilization.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for producing hydrogen and light olefins. Background Art

[0002] Hydrogen energy is an ideal new energy source. As a green energy with abundant reserves, high calorific value, high energy density and diverse sources, hydrogen energy is known as the "ultimate energy" of the 21st century. Hydrogen is produced through clean energy such as wind and light, and hydrogen is combined with fuel cells to generate electricity, thus forming a hydrogen energy industry ecosystem, which will help accelerate the construction of a clean and low-carbon hydrogen energy supply system.

[0003] There are three relatively mature technical routes for the main hydrogen production methods, namely, hydrogen production from fossil energy such as coal and natural gas reforming, hydrogen production from high-temperature decomposition and reforming of chemical raw materials represented by alcohol cracking hydrogen production technology, and hydrogen production from water electrolysis. Technical routes such as photolysis of water and biomass gasification hydrogen production are still in the experimental and development stage. It is difficult to make breakthroughs in related technologies and has not yet met the needs of large-scale hydrogen production. At present, domestic natural gas reforming hydrogen production and high-temperature cracking hydrogen production are mainly used in large-scale hydrogen production industry. The raw gas in the natural gas hydrogen production process is also fuel gas and does not need to be transported, but the investment in natural gas hydrogen production is relatively high and is suitable for large-scale industrial production. The general hydrogen production scale is 5000m 3 / h or more, it is more economical to choose the natural gas hydrogen production process. In addition, natural gas raw materials account for more than 70% of the cost of hydrogen production, and the price of natural gas is an important factor in determining the price of hydrogen. Coal gasification hydrogen production is the first choice for industrial large-scale hydrogen production, and it is also the mainstream fossil energy hydrogen production method in my country. This hydrogen production process converts coal into synthesis gas (CO, CH4, H2, CO2, N2, etc.) through gasification technology, and then separates and treats it through water-gas shift to extract high-purity hydrogen. It is the raw material for preparing synthetic ammonia, methanol, liquid fuel, natural gas and other products, and is widely used in petrochemical, steel and other fields. The coal-to-hydrogen technology route is mature and efficient, and can be produced on a large scale and stably, but the power consumption of coal-to-hydrogen fuel is higher than that of natural gas hydrogen production, and the system steam and electricity requirements are high, and enterprises need matching boilers. In addition, environmental protection issues are prominent, the existing urban refineries have harsh environmental requirements, and coal transportation is subject to many factors, which also limits the application of this technology in modern refineries.

[0004] With the development of oil refining technology, especially the trend of heavy / inferior crude oil and the improvement of oil product quality, the hydrogenation process has been more widely used, which has greatly promoted the demand for hydrogen. According to statistics, the annual growth rate of global refinery hydrogen demand exceeds 4%. Hydrogen from refineries mainly comes from by-products of process units, refinery gas recovery, and existing refinery hydrogen production units. It is difficult for refineries to produce hydrogen by themselves to meet the future growth demand for hydrogen. Therefore, it is necessary to explore more flexible and feasible hydrogen supply strategies. Low-carbon olefins represented by ethylene and propylene are the most basic raw materials for the chemical industry, and the demand has been increasing. Faced with the contradiction of serious overcapacity of refining capacity, unreasonable oil product structure, and insufficient chemical production capacity, especially high-end production capacity to meet market needs, the transformation of oil refining enterprises from "fuel type" to "chemical type" is already a general trend. If flexible hydrogen production technology can be developed to produce low-carbon olefins, it will undoubtedly have good economic and social benefits. Summary of the invention

[0005] The object of the present invention is to provide a method for catalytically producing hydrogen and simultaneously producing light olefins.

[0006] The method for producing hydrogen and simultaneously producing light olefins from hydrocarbon raw materials provided by the present invention comprises the following steps:

[0007] (1) mixing a hydrocarbon feedstock with water vapor, introducing the mixture into a fluidized bed reactor to contact the mixture with a regenerated catalyst and undergo a catalytic decomposition reaction to obtain a reactant stream and a deactivated catalyst;

[0008] (2) separating the reaction oil and gas obtained from the catalytic decomposition reaction and the deactivated catalyst;

[0009] (3) further separating the separated reaction oil and gas into products including hydrogen, carbon monoxide, carbon dioxide, light olefins and other hydrocarbon products;

[0010] (4) The deactivated catalyst is sent to a regenerator for regeneration. After the deactivated catalyst is regenerated by burning, it is returned to the fluidized bed reactor for recycling. The regenerated flue gas enters a separation unit to separate carbon monoxide and carbon dioxide.

[0011] The hydrocarbons are selected from one or more mixtures of petroleum hydrocarbons, mineral oils and synthetic oils. The petroleum hydrocarbons are gaseous hydrocarbons, gasoline, diesel, vacuum wax oil, atmospheric residue oil, vacuum wax oil mixed with part of vacuum residue oil or hydrocarbon oil obtained by secondary processing; mineral oil is selected from one or more mixtures of coal liquefaction oil, oil sand oil and shale oil; synthetic oil is a distillate oil obtained by Fischer-Tropsch synthesis of coal, natural gas or asphalt. The hydrocarbon oil obtained by secondary processing is selected from one or more of coker gasoline, catalytic diesel, hydrogenated diesel, coker diesel, coker wax oil, deasphalted oil and furfural refined raffinate oil.

[0012] Based on the dry weight of the catalyst, the catalyst includes 5%-65% natural minerals, 10%-60% oxides, 10%-60% zeolites and 0.1%-30% metal active components. The zeolite includes medium-pore zeolite and optional large-pore zeolite, the medium-pore zeolite is ZSM series zeolite and / or ZRP zeolite, and the large-pore zeolite is selected from one or more of rare earth Y, rare earth hydrogen Y, ultra-stable Y and high silicon Y. The medium-pore zeolite accounts for 5-100% by weight of the total weight of the zeolite, preferably 20-50% by weight. The content of the metal active component is 0.1%-30% by weight, preferably 0.5-20% by weight. The metal active component is selected from one or more compounds of transition metal elements, preferably one or more of nickel, cobalt, iron, tungsten, molybdenum, manganese, copper, zirconium and chromium.

[0013] The reaction temperature of the fluidized reactor is 450-800°C, preferably 550-700°C, the reaction time is 0.1-10 seconds, preferably 1-8 seconds, the weight ratio of the catalyst to the hydrocarbon feedstock is 5-100, preferably 20-50, and the weight ratio of water vapor to the hydrocarbon feedstock is 0.1-20, preferably 1-10.

[0014] The fluidized reactor is selected from one or a combination of a riser reactor, a fast bed and a dense phase fluidized bed. The fluidized reactor comprises a pre-lifting section and a fluidized reactor of at least one reaction zone from bottom to top, and the number of the reaction zones is preferably 2-8, more preferably 2-3.

[0015] The oxygen concentration in the oxygen-containing gas at the bottom of the regenerator is 22-100 volume % and preferably 25-80 volume %.

[0016] The regeneration operation conditions are: temperature of 550-700°C, preferably 600-650°C; gas superficial velocity of 0.2-1.2 m / s, preferably 0.4-0.8 m / s; average residence time of deactivated catalyst of 1-10 minutes, preferably 2-6 minutes.

[0017] The volume ratio of CO / CO2 in the regeneration flue gas is 0.2-2.0, preferably 0.8-1.5.

[0018] The separated gas obtained from the regenerated flue gas and the separation unit is rich in carbon monoxide, which can be used as a raw material for water-gas shift to further produce hydrogen and carbon dioxide; it can also be sent to a carbon monoxide boiler to recover the waste heat of the flue gas to produce high-quality steam.

[0019] The present invention uses hydrocarbon raw materials as raw materials, which not only reduces the raw material cost of natural gas hydrogen production, but also helps to ease the tight supply situation in my country's natural gas market, which is of strategic significance to the stable development of my country's energy structure.

[0020] The present invention adopts a fluidized reactor to produce hydrogen, and the catalyst circulates between the reactor and the regenerator, which not only achieves the regeneration of the deactivated catalyst, but also transfers a large amount of heat for the reaction, greatly reducing the energy required for the hydrogen production process and achieving process economy.

[0021] The present invention preferably adopts low-temperature incomplete regeneration technology, and the CO / CO2 ratio in the regenerated flue gas is high, which can provide cheap raw gas for the water-gas shift process and realize the optimal utilization of resources. It can also recover the waste heat of the flue gas to produce hot water or high-quality steam for supply to other devices, which can play the role of a public engineering island, realize the rational utilization of energy in the refinery, and improve the process economy.

[0022] The oxygen-containing gas used for regenerating the deactivated catalyst in the hydrogen production process of the present invention is preferably oxygen-rich gas, which greatly increases the concentration of CO2 in the flue gas, can achieve large-scale production of CO2, and then reduce carbon emissions through capture, utilization, and storage technology, thereby achieving the production of blue hydrogen.

[0023] The present invention adopts a catalytic conversion method to convert hydrocarbon raw materials into hydrogen and produce low-carbon olefins as by-products, with a high hydrogen yield. The present invention not only realizes the high-value utilization of hydrocarbon raw materials and meets the market demand for low-carbon olefins, but also enriches the CO2 generated in the process, which not only brings hydrogen energy, but also facilitates carbon capture, and can bring greater economic and social benefits to the petrochemical industry. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 A process flow chart of a specific implementation method of producing hydrogen from hydrocarbon feedstocks in a fluidized bed and simultaneously producing light olefins provided by the present invention. DETAILED DESCRIPTION

[0025] A method for producing hydrogen from hydrocarbon raw materials and simultaneously producing light olefins, the method comprising the following steps:

[0026] After the hydrocarbon feedstock is mixed with water vapor, it is introduced into a fluidized reactor to contact with the regenerated catalyst and undergo a catalytic decomposition reaction;

[0027] separating the reaction products and the deactivated catalyst obtained from the catalytic decomposition reaction, and separating the reaction products into hydrogen, carbon monoxide, carbon dioxide, light olefins and other hydrocarbon products;

[0028] The deactivated catalyst is sent to a regenerator for low-temperature incomplete regeneration. After being regenerated by burning, the deactivated catalyst is returned to the fluidized bed reactor for recycling. The regenerated flue gas enters a separation unit to separate carbon monoxide and carbon dioxide.

[0029] The carbon monoxide obtained from the regenerated flue gas and the separation unit can be used as a raw material for water-gas shift to further produce hydrogen and carbon dioxide; it can also be sent to a carbon monoxide boiler to recover flue gas waste heat to generate high-pressure steam.

[0030] The hydrocarbon raw material is various animal and plant oils rich in hydrocarbons, and the hydrocarbon is selected from one or more mixtures of petroleum hydrocarbons, mineral oils and synthetic oils. Petroleum hydrocarbons are well known to those skilled in the art, for example, it can be a petroleum distillate obtained by a primary processing device, and can be selected from one or more mixed oils such as gasoline, diesel, vacuum wax oil, atmospheric residue oil, vacuum residue oil, or a distillate obtained by a secondary processing device, and can be selected from one or more of coker gasoline, catalytic diesel, hydrogenated diesel, coker diesel, coker wax oil, deasphalted oil, furfural refined raffinate oil. Mineral oil is selected from one or more mixtures of coal liquefaction oil, oil sand oil and shale oil. Synthetic oil is a distillate obtained from coal, natural gas or asphalt through Fischer-Tropsch synthesis.

[0031] The catalyst comprises the following components by weight percentage:

[0032] A) 5%-65% natural minerals,

[0033] B) 10%-60% oxide,

[0034] C) 10% to 60% of zeolite, and

[0035] D) 0.1%-30% metal active component.

[0036] The method provided by the present invention can be carried out in various existing fluidized reactors, wherein the fluidized reactor is selected from one or a combination of a turbulent bed, a fast bed and a dilute phase transport bed. The fluidized reactor includes a pre-lifting section and at least one reaction zone fluidized reactor from bottom to top. In order to allow the crude oil to react fully and according to different quality requirements of the target product, the reaction zones can be 2-8, preferably 2-3.

[0037] The conditions of the catalytic decomposition reaction include: the reaction temperature of the fluidized reactor is 450-800°C, preferably 550-700°C, the reaction time is 0.1-10 seconds, preferably 1-8 seconds, the weight ratio of the catalyst to the hydrocarbon feedstock is 5-100, preferably 20-50; the weight ratio of water vapor to the hydrocarbon feedstock is 0.1-20, preferably 1-10.

[0038] According to the method provided by the present invention, the deactivated catalyst is generally first separated from the reaction oil and gas to obtain the deactivated catalyst and the reaction oil and gas, and then the obtained reaction oil and gas are separated into hydrogen, CO2, CO, gaseous hydrocarbons and liquid hydrocarbons and other fractions through a subsequent separation unit, and the gaseous hydrocarbons are further separated by a gas separation device to obtain hydrocarbon components such as ethylene and propylene. The method for separating hydrogen, ethylene, propylene, etc. from the reaction products is similar to the conventional technical method in the field, and the present invention is not limited to this and is not described in detail herein.

[0039] In the method provided by the present invention, the CO obtained in the separation unit can be sent to the water-gas shift unit to further react with water vapor to obtain hydrogen and enriched CO2. The water-gas shift of CO and water vapor adopts the existing technology well known to those skilled in the art.

[0040] In the method provided by the present invention, preferably the deactivated catalyst enters the stripping section under the action of gravity, the hydrocarbon products adsorbed on the deactivated catalyst are stripped by water vapor, and the deactivated catalyst after stripping enters the regenerator.

[0041] The deactivated catalyst can be regenerated in a conventional regenerator, and a single regenerator or multiple regenerators can be used. During the regeneration process, an oxygen-containing gas is generally introduced from the bottom of the regenerator. After the oxygen-containing gas is introduced into the regenerator, the deactivated catalyst contacts with oxygen and burns and regenerates. The flue gas generated after the catalyst burns and regenerates is separated into gas and solid at the top of the regenerator, and the flue gas enters the water-gas shift unit. The oxygen-containing gas used for regenerating the deactivated catalyst is preferably an oxygen-rich gas. The oxygen concentration in the oxygen-containing gas at the bottom of the regenerator is 22-100% by volume, preferably 25%-80% by volume.

[0042] In the method provided by the present invention, low-temperature incomplete regeneration is preferred, and the operating conditions are: temperature is 550-700°C, preferably 600-650°C; gas superficial linear velocity is 0.2-1.2 m / s, preferably 0.4-0.8 m / s, and the average residence time of the deactivated catalyst is 1-10 minutes, preferably 2-6 minutes.

[0043] In the method provided by the present invention, the volume ratio of CO / CO2 in the regeneration flue gas is 0.2-2.0, preferably 0.8-1.5.

[0044] In the method provided by the present invention, the natural minerals in the catalyst are selected from one or more of kaolin, halloysite, montmorillonite, diatomite, attapulgite, sepiolite, halloysite, hydrotalcite, bentonite and rectorite, and the content of natural minerals on a dry basis is 5% to 65% by weight, preferably 15% to 60% by weight; the oxide is one or more of silicon oxide, aluminum oxide, zirconium oxide, titanium oxide, and amorphous silicon aluminum, and the content of the oxide is 10% to 60% by weight, preferably 10% to 30% by weight, and more preferably 12% to 28% by weight, based on the total amount of the catalyst and in terms of oxide weight percentage. The zeolite includes a medium-pore zeolite and an optional large-pore zeolite, and the large-pore zeolite is selected from one or more of rare earth Y, rare earth hydrogen Y, ultrastable Y and high silicon Y. The medium-pore zeolite is a ZSM series zeolite and / or a ZRP zeolite, and the medium-pore zeolite accounts for 5-100% by weight of the total weight of the zeolite, preferably 20-50% by weight.

[0045] Based on the weight of the catalyst, the metal active component content is 0.1%-30% by weight, preferably 0.5-20% by weight. The metal active component is selected from one or more compounds of transition metal elements, preferably one or more of nickel, cobalt, iron, tungsten, molybdenum, manganese, copper, zirconium and chromium.

[0046] In the method provided by the present invention, the catalyst preparation method adopts the preparation method of conventional catalytic cracking catalyst, which is a preparation method well known to those skilled in the art. The metal can be loaded on the catalyst by impregnation method or slurry method, preferably impregnation method, which are well known to those skilled in the art.

[0047] The accompanying drawings are used to provide further understanding of the present disclosure and constitute a part of the specification. They are used to explain the present disclosure together with the following detailed description, but do not constitute a limitation of the present disclosure.

[0048] like Figure 1 As shown, the regenerated catalyst from the regeneration inclined tube 7 enters the fluidized reactor 1, accelerates upward along the reactor, and the hydrocarbon feedstock is mixed with the water vapor from the pipeline 6 through the pipeline 5, and then injected into the fluidized reactor 1 to contact with the regenerated catalyst. The hydrocarbon feedstock undergoes a catalytic reaction on the hot catalyst and accelerates upward. After the generated reaction product and the deactivated deactivated catalyst are separated, the reaction product enters the separation unit 3 through the pipeline 8 and is separated into hydrogen 9, carbon dioxide 10, carbon monoxide 15, and hydrocarbon products 11. The hydrocarbon products can be further separated to obtain light olefins such as ethylene, propylene and butene, and the remaining other hydrocarbon products can be further converted by partial or full refining. The separated carbon monoxide can be used as a water gas shift feedstock, and the light olefins can be further separated to obtain ethylene.

[0049] The deactivated catalyst enters the regenerator 2 through the inclined tube 12, and the coke on the deactivated catalyst is burned off to regenerate the deactivated catalyst. The regenerated flue gas enters the separation unit 3 through the flue gas pipeline 14, and carbon monoxide 15 and carbon dioxide 10 are separated. The regenerated catalyst is circulated to the bottom of the fluidized reactor 1 through the regeneration pipeline 7.

[0050] The present invention will be further described in the following examples, but the present invention is not limited thereto.

[0051] The raw materials used in the examples and comparative examples are all catalytic diesel, and the properties are shown in Table 1. The catalyst used in the comparative example is an industrial catalyst, the trade name is DMMC-1, and the properties are shown in Table 2.

[0052] The catalyst preparation method used in the examples is briefly described as follows:

[0053] 1) 75.4 kg of kaolin (solid content 71.6 wt%) was slurried with 250 kg of decationized water, and then 54.8 kg of pseudo-boehmite (solid content 63 wt%) was added, and the pH was adjusted to 2-4 with hydrochloric acid, and stirred evenly. The mixture was allowed to stand and age at 60-70°C for 1 hour, maintaining the pH at 2-4, and the temperature was lowered to below 60°C. 41.5 kg of aluminum sol (Al2O3 content of 21.7 wt%) was added, and stirred for 40 minutes to obtain a mixed slurry.

[0054] 2) ZRP-1 (22 kg on dry basis) and DASY zeolite (22.5 kg on dry basis) were added to the obtained mixed slurry, stirred evenly, spray dried to form, washed with diammonium phosphate solution (phosphorus content of 1 wt%) to remove free Na+, and calcined to obtain a molecular sieve catalyst sample.

[0055] 3) 3 kg of Ni(NO3)2 was dissolved in 5.5 kg of water to prepare a Ni(NO3)2·6H2O aqueous solution, 10 kg of the molecular sieve catalyst sample was immersed in the Ni(NO3)2·6H2O aqueous solution, and the obtained mixture was dried at 180°C for 4 hours and calcined at 600°C for 2 hours. After repeated immersion, drying and calcination, the content of Ni loaded on the catalyst sample reached 15%, and the catalyst A of the embodiment was obtained.

[0056] Example 1

[0057] according to Figure 1The catalytic decomposition reaction test of catalytic diesel was carried out on the riser reactor. The catalytic diesel entered the lower part of the riser reactor, contacted with the hot regenerated catalyst and underwent catalytic decomposition reaction. The reaction products and the deactivated catalyst entered the closed cyclone separator from the reactor outlet. The reaction products and the deactivated catalyst were quickly separated. The reaction products were separated into cracked gas and liquid according to the distillation range in the separation system.

[0058] The deactivated catalyst enters the stripping section under the action of gravity, and the hydrocarbon products adsorbed on the deactivated catalyst are stripped by water vapor. The deactivated catalyst after stripping enters the regenerator and contacts with oxygen-rich air for regeneration; the regenerated catalyst is then returned to the riser reactor for recycling. The operating conditions and product distribution are listed in Table 3.

[0059] From the results in Table 3, it can be seen that the hydrogen yield is as high as 17.46%, the ethylene yield is 2.27%, the propylene yield is 5.76%, the CO yield in the reaction product is 29.11%, and the CO2 yield is 26.16%. The CO concentration in the regeneration flue gas is 7.17% by volume, and the CO2 concentration is 25.08% by volume.

[0060] Comparative Example 1

[0061] The test was carried out on a medium-sized device of a riser, the catalytic diesel feedstock was the same as in Example 1, and the catalyst was DMMC-1.

[0062] The catalytic diesel enters the riser reactor and contacts the hot DMMC-1 catalyst to undergo a catalytic decomposition reaction. The reaction products and the deactivated catalyst enter the closed cyclone separator from the reactor outlet. The reaction products and the deactivated catalyst are quickly separated. The reaction products are separated into gas and liquid products according to the distillation range in the separation system.

[0063] The deactivated catalyst enters the stripping section under the action of gravity, and the hydrocarbon products adsorbed on the deactivated catalyst are stripped out by water vapor. The deactivated catalyst after stripping enters the regenerator and is regenerated by contact with air; the regenerated catalyst is then returned to the riser reactor for recycling; the operating conditions and product distribution are listed in Table 3.

[0064] From the results in Table 3, it can be seen that the hydrogen yield is 1.35%, the ethylene yield is 3.01%, the propylene yield is 9.35%, and the CO and CO2 yields in the reaction products are low. No CO was detected in the regeneration flue gas, the CO2 concentration was 15.01% by volume, and the O2 concentration was 3.55% by volume.

[0065] The preferred embodiments of the present invention are described in detail above. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, a variety of simple modifications can be made to the technical solution of the present invention, and these simple modifications all belong to the protection scope of the present invention.

[0066] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present invention will not further describe various possible combinations.

[0067] In addition, various embodiments of the present invention may be arbitrarily combined, and as long as they do not violate the concept of the present invention, they should also be regarded as the content of the present invention.

[0068] Table 1

[0069] project Catalytic diesel <![CDATA[Density (20 °C) / (kg / m 3 )]]> 948.9 <![CDATA[Kinematic viscosity (20 °C) / (mm 2 / s)]]> 3.754 Total acid value / (mg KOH / g) <0.05 Freezing point / ℃ -27 Closed cup flash point / ℃ 66 Distillation range / ℃ Initial distillation point 197.9 5% 220.4 10% 228.4 50% 262.5 70% 283.1 90% 308.6 95% 319.5 Final distillation point 329.9

[0070] Table 2

[0071] Example 1 Comparative Example 1 Catalyst A Industrial catalyst DMMC-1 Physical properties <![CDATA[Specific surface area, m 2 / g]]> 118 106 <![CDATA[Specific surface area of molecular sieve, m 2 / g]]> 30 42 <![CDATA[Pore volume, cm 3 / g]]> 0.126 0.13 Sieve composition, weight % 0~40 microns 22.7 30.9 0~80 microns 64.4 75.0 0~105 microns 87.1 89.1 0~149 microns 97.9 98.4 Average particle size / micron 55.0 55.6 Micro-anti-activity, % 50 65 Metal content, % Ni 14.5 0.06

[0072] Table 3

[0073] Example 1 Comparative Example 1 Riser reaction conditions Reaction temperature, °C 650 650 Reaction time, seconds 2 2 Weight ratio of catalyst to catalytic diesel 20 20 Water to oil weight ratio 0.2 0.2 Regeneration conditions Regeneration temperature, °C 650 680 Oxygen concentration in regeneration air, volume % 50 21 Gas superficial velocity, m / s 0.8 0.8 Average stay time, minutes 4.5 4.5 Product distribution, weight % CO 29.11 0.23 <![CDATA[CO2]]> 26.16 0.9 <![CDATA[H2]]> 17.46 1.35 Ethylene 2.27 3.01 Propylene 5.76 9.35 Other gaseous hydrocarbons 11.63 29.02 Liquid hydrocarbons 2.54 46.51 Coke 5.07 9.63 total 100.00 100.00 Regeneration flue gas composition, volume % CO 7.17 0 <![CDATA[CO2]]> 25.08 15.01 <![CDATA[N2]]> 67.75 81.44 <![CDATA[O2]]> 0 3.55

Claims

1. A method for catalytically producing hydrogen and light olefins, comprising the following steps: (1) After mixing a hydrocarbon feedstock with water vapor, the feedstock is introduced into a fluidized reactor to contact with a regenerated catalyst and perform a catalytic decomposition reaction. The reaction temperature of the fluidized reactor is 450-800° C., the reaction time is 0.1-10 seconds, the weight ratio of the catalyst to the hydrocarbon feedstock is 5-100, and the weight ratio of the water vapor to the hydrocarbon feedstock is 0.1-20, to obtain a reactant stream and a deactivated catalyst, wherein the hydrocarbon feedstock is catalytic diesel, the dry weight of the catalyst is the basis, and the catalyst comprises 5%-65% of natural minerals, 10%-60% of oxides, and 10%- 60% zeolite and 0.1%-30% metal active components, the natural minerals are selected from one or more of kaolin, halloysite, montmorillonite, diatomite, attapulgite, sepiolite, halloysite, hydrotalcite, bentonite and rectorite, the oxides are one or more of silicon oxide, aluminum oxide, zirconium oxide, titanium oxide, amorphous silicon aluminum, the zeolite includes medium-pore zeolite and large-pore zeolite, the medium-pore zeolite is ZSM series zeolite and / or ZRP zeolite, the large-pore zeolite is one or more selected from rare earth Y, rare earth hydrogen Y, ultrastable Y and high silicon Y; (2) Separating the reaction oil and gas obtained from the catalytic decomposition reaction and the deactivated catalyst; (3) further separating the separated reaction oil and gas into products including hydrogen, carbon monoxide, carbon dioxide, light olefins and other hydrocarbon products; (4) The deactivated catalyst is sent to a regenerator for regeneration. The regeneration operating conditions are as follows: temperature of 550-700°C; gas superficial velocity of 0.2-1.2 m / s; average residence time of the deactivated catalyst of 1-10 minutes; oxygen concentration of the oxygen-containing gas at the bottom of the regenerator of 22-100% by volume; after incomplete regeneration by burning, the deactivated catalyst is returned to the fluidized bed reactor for recycling; the regenerated flue gas enters a separation unit to separate carbon monoxide and carbon dioxide; the CO / CO2 volume ratio in the regenerated flue gas is 0.2-2.

0.

2. The method according to claim 1, characterized in that: The content of the metal active component is 0.1%-30% by weight, and the metal active component is selected from one or more compounds of transition metal elements.

3. The method according to claim 1, characterized in that The content of the metal active component is 0.5-20% by weight, and the metal active component is selected from one or more of nickel, cobalt, iron, tungsten, molybdenum, manganese, copper, zirconium and chromium.

4. The method according to claim 1, characterized in that: The reaction conditions of the fluidized bed reactor are: reaction temperature of 550-700°C, reaction time of 1-8 seconds, weight ratio of catalyst to hydrocarbon feedstock of 20-50; weight ratio of water vapor to hydrocarbon feedstock of 1-10.

5. The method according to claim 1, characterized in that The fluidized reactor is selected from one or a combination of a riser reactor, a fast bed and a dense phase fluidized bed.

6. The method according to claim 1, characterized in that The fluidized reactor comprises, from bottom to top, a pre-lifting section and at least one reaction zone.

7. The method according to claim 6, characterized in that The number of the reaction zones is 2-8.

8. The method according to claim 6, characterized in that The number of the reaction zones is 2-3.

9. The method according to claim 1, characterized in that: The oxygen concentration in the oxygen-containing gas at the bottom of the regenerator is 25-80% by volume.

10. The method according to claim 1, characterized in that The regeneration operation conditions are: temperature of 600-650° C.; gas superficial linear velocity of 0.4-0.8 m / s; and average residence time of the deactivated catalyst of 2-6 minutes.

11. The method according to claim 1, characterized in that: The volume ratio of CO / CO2 in the regeneration flue gas is 0.8-1.5.