An organic sulfide absorbent and a method for treating sulfur-containing organic waste gas
Through the absorbent composed of choline chloride, organic carboxylic acid and basic amino acid, combined with the synergistic effect of hydrogen bonding and basic amino acid, the problem of non-recyclable absorbent and environmental harm in the existing technology is solved, achieving high efficiency and environmental protection. The absorption and recycling of organic sulfides significantly improves the absorption effect and stability.
Patent Information
- Application Number
- CN202111263256.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-28
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-10-28
AI Technical Summary
When dealing with sulfur-containing organic waste gas in the existing technology, the preparation method of the absorbent is complicated, the absorbent cannot be recycled and reused, and the commonly used non-green solvents cause harm to the environment, and the absorption effect is not good for other organic sulfides.
Using choline chloride, organic carboxylic acid and basic amino acid as the main components of the absorbent, by building the synergistic effect of hydrogen bonds and basic amino acids, an efficient and environmentally friendly organic sulfide absorbent is prepared for Treat sulfur-containing organic waste gas and realize the recycling of absorbent through decompression regeneration.
It achieves efficient absorption of organic sulfides, has good absorption performance, high stability, low absorption cost, the absorbent can be recycled, and is environmentally friendly.
Smart Images

Figure DEST_PATH_IMAGE001
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of air pollution control, and specifically relates to an organic sulfide absorbent and a method for treating sulfur-containing organic waste gas thereof. Background Art
[0002] Organic sulfides such as mercaptans and sulfides usually come from waste gases discharged from chemical plants and sewage treatment plants. These compounds are in high concentrations and are accompanied by an unpleasant odor. They have a strong irritating effect on the upper respiratory tract and eyes, and may cause anorexia, shortness of breath, nausea, vomiting, etc. At high concentrations, they can cause spasms and paralysis of the nervous system, and even endanger life and health.
[0003] At present, the treatment and control technologies for sulfur-containing compounds include high-temperature thermal oxidation, wet chemical washing, adsorption, absorption and biofiltration. Although these methods have their own advantages, they have high operating costs or produce a large amount of waste that requires further treatment. The absorption method has a simple process flow, stable operation and low operating costs, and can selectively adsorb organic sulfides to separate them and achieve removal effects. For specific absorption equipment, obtaining efficient and green absorbents is the key problem to solve the bottleneck of this technology.
[0004] CN108822908A discloses a natural gas organic sulfur removal agent and a preparation method thereof, characterized in that the absorbent comprises a composite amine liquid, a desulfurization enhancer, a defoamer, an antioxidant and a preservative. The preparation method of the organic sulfur removal agent comprises: (1) mixing hindered amine, methyldiethanolamine and water in a proportion to prepare a composite amine liquid; (2) adding ammonium chloride to ethanolamine in a proportion, stirring at 40-60°C for 0.5-2 hours to obtain a desulfurization enhancer; (3) adding a desulfurization enhancer, a defoamer, an antioxidant and a preservative in a proportion to the composite amine solution; (4) stirring at room temperature for 2-6 hours to obtain a natural gas organic sulfur removal agent. The prepared natural gas organic sulfur desulfurization agent has the advantages of large acid gas load, low sulfur content in purified gas, stable solvent performance, and no corrosion to equipment. However, the preparation method of the removal agent is complicated, and the absorbent cannot be recovered and reused.
[0005] CN107684803A discloses an organic amine absorbent for removing acidic substances in gas streams. By adding a compound containing a nitrogen cyclic group as a catalyst in the organic amine absorbent, the acidic substances in the gas stream, including organic sulfur, are removed, and carbonyl sulfide and mercaptan in the raw gas can be removed at the same time. However, the organic amine solution of this technology has a good absorption response to carbonyl sulfide and mercaptan as an absorbent, but has a poor absorption effect on other organic sulfides, and is a non-green solvent, which will cause certain harm to the environment. Summary of the invention
[0006] In view of the shortcomings of the prior art, the object of the present invention is to provide an organic sulfide absorbent and a method for treating sulfur-containing organic waste gas. The absorbent provided by the present invention has the advantages of good absorption performance, high stability, environmental friendliness, and recyclability. It is applied to the treatment of sulfur-containing organic waste gas, has mild absorption conditions, is easy to desorb, and has low absorption cost.
[0007] On one hand, the present invention provides an organic sulfide absorbent, which mainly comprises choline chloride, an organic carboxylic acid and a basic amino acid, wherein the molar ratio of choline chloride to the organic carboxylic acid is 1:1-1:10, preferably 1:2-1:6, and the mass of the basic amino acid accounts for 1%-15% of the total mass of choline chloride and the organic carboxylic acid, preferably 5%-10%.
[0008] In the present invention, the organic carboxylic acid is an aliphatic organic carboxylic acid, specifically at least one of citric acid, lactic acid, malonic acid and malic acid, preferably citric acid.
[0009] In the present invention, the basic amino acid is at least one of lysine, arginine and histidine, preferably lysine.
[0010] The second aspect of the present invention provides a method for preparing the above-mentioned organic sulfide absorbent, comprising the following contents: mixing choline chloride and organic carboxylic acid in proportion, heating and stirring until they become a uniform liquid; then adding alkaline amino acid, heating and stirring until they become a uniform liquid, and cooling to obtain the organic sulfide absorbent.
[0011] In the above preparation method, the molar ratio of choline chloride to organic carboxylic acid is 1:1 to 1:10, preferably 1:2 to 1:6. The organic carboxylic acid is an aliphatic organic carboxylic acid, specifically at least one of citric acid, lactic acid, malonic acid and malic acid, preferably citric acid.
[0012] In the above preparation method, the basic amino acid is at least one of lysine, arginine and histidine, preferably lysine.
[0013] In the above preparation method, the heating temperature is 60-100°C, the stirring speed is 100-200 r / min, and the stirring time is 1-2h. The cooling is generally cooling to room temperature.
[0014] The third aspect of the present invention provides a method for treating sulfur-containing organic waste gas using the above-mentioned organic sulfide absorbent, wherein the sulfur-containing waste gas is contacted with the organic sulfide absorbent, and the absorbent includes choline chloride, an organic carboxylic acid and a basic amino acid, wherein the molar ratio of choline chloride to the organic carboxylic acid is 1:1 to 1:10, preferably 1:2 to 1:6, and the mass of the basic amino acid accounts for 1% to 15% of the total mass of choline chloride and the organic carboxylic acid, preferably 5% to 10%.
[0015] In the method of the present invention, the sulfur-containing organic waste gas is mainly organic waste gas containing organic sulfides, wherein the organic sulfide can be at least one of methyl mercaptan, ethyl mercaptan, methyl sulfide, propyl mercaptan, isopropyl mercaptan, thiophene and the like.
[0016] In the method of the present invention, the contact conditions between the sulfur-containing organic waste gas and the absorbent are: temperature of 15-30°C, pressure of 0.1-0.3MPa, liquid-gas ratio of 3-5 L / m 3 .
[0017] In the method of the present invention, the organic carboxylic acid is an aliphatic organic carboxylic acid, specifically at least one of citric acid, lactic acid, malonic acid and malic acid, preferably citric acid.
[0018] In the method of the present invention, the basic amino acid is at least one of lysine, arginine and histidine, preferably lysine.
[0019] In the method of the present invention, regeneration is performed after absorption equilibrium is reached, and a reduced pressure regeneration method is adopted, and the pressure is 10kPa to 0.1MPa. Further, regeneration is preferably performed in a N2 atmosphere, and the regenerated absorbent is recycled.
[0020] Compared with the prior art, the present invention has the following beneficial effects:
[0021] (1) The organic sulfide absorbent of the present invention has good selective absorption capacity for organic sulfides by selecting specific components and proportions, and has the advantages of good absorption effect, high stability, low volatility, easy regeneration, etc. In addition, the raw material source is abundant and easy to synthesize, and it is an efficient and environmentally friendly organic sulfide absorbent.
[0022] (2) The method of the present invention first mixes choline chloride and carboxylic acid solvents, and by constructing hydrogen bonds, has good selective absorption of organic sulfides, and then synergistically acts with basic amino acids to further enhance its absorption capacity for organic sulfides, ultimately achieving efficient absorption of organic sulfides by the absorbent.
[0023] (3) The absorbent of the present invention is used for treating waste gas containing organic sulfides, and has the advantages of good absorption performance and environmental friendliness. Moreover, after absorption equilibrium, the rich absorbent can be efficiently desorbed by decompression, and the regenerated absorbent can be recycled and has good stability in use. DETAILED DESCRIPTION
[0024] The organic sulfide absorbent of the present invention and the method and effect thereof for treating sulfur-containing organic waste gas are further described below in conjunction with specific examples. The examples are implemented based on the technical solution of the present invention, and detailed implementation methods and specific operation processes are given, but the protection scope of the present invention is not limited to the following examples.
[0025] The experimental methods in the following examples, unless otherwise specified, are all conventional methods in the art. The experimental materials used in the following examples, unless otherwise specified, were purchased from conventional biochemical reagent stores.
[0026] Example 1
[0027] Preparation of absorbent: choline chloride and citric acid are added to a reactor in a molar ratio of 1:6, and stirred at 100°C and 200 r / min for 1 hour to obtain a uniform liquid; then lysine is added in an amount of 6% of the total mass of choline chloride-citric acid, and stirred at 80°C and 150 r / min for 1 hour, and then cooled to room temperature to obtain an absorbent.
[0028] The above absorbent is used to treat waste gas containing methyl mercaptan: the waste gas and the absorbent are absorbed in the absorption tower, the absorption temperature is controlled to be 30°C, the absorption pressure is 0.2MPa, and the liquid-gas ratio is 5L / m 3 After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 343 mg of methyl mercaptan was absorbed per gram of absorbent.
[0029] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.01 MPa and a desorption time of 30 min. The regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After being recycled for 5 times, it was found through testing and calculation that 309 mg of methyl mercaptan was absorbed per gram of absorbent.
[0030] Example 2
[0031] Preparation of absorbent: choline chloride and citric acid are added to a reactor in a molar ratio of 1:4, stirred at 80°C and 100 r / min for 1 hour, cooled to room temperature, and a uniform liquid is obtained; lysine is then added so that 6% of the total mass of choline chloride-citric acid is added, stirred at 80°C and 200 r / min for 1 hour, cooled to room temperature, and an absorbent is obtained.
[0032] The above absorbent is used to treat waste gas containing methyl mercaptan: the waste gas and the absorbent are absorbed in the absorption tower, and the absorption temperature is controlled to be 25°C, the absorption pressure is 0.3MPa, and the liquid-gas ratio is 4L / m 3 After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 302 mg of methyl mercaptan was absorbed per gram of absorbent.
[0033] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 10 kPa for 30 minutes. After 10 absorption and desorption cycles, the regenerated absorbent was used to absorb methyl mercaptan-containing gas under the same operating conditions. After 5 cycles, the methyl mercaptan absorbed by each gram of absorbent was 281 mg, according to detection and calculation.
[0034] Example 3
[0035] Preparation of absorbent: choline chloride and citric acid are added to a reactor in a molar ratio of 1:2, and stirred at 60°C and 150 r / min for 1 hour to obtain a uniform liquid; then lysine is added in an amount of 6% of the total mass of choline chloride-citric acid, and stirred at 80°C and 200 r / min for 1 hour, and then cooled to room temperature to obtain an absorbent.
[0036] The above absorbent is used to treat waste gas containing methyl mercaptan: the waste gas and the absorbent are absorbed in the absorption tower, the absorption temperature is controlled to be 30°C, the absorption pressure is 0.3MPa, and the liquid-gas ratio is 4L / m 3 After the absorption reached equilibrium, the weight before and after absorption was measured by weight method, and it was calculated that 275 mg of methyl mercaptan was absorbed per gram of absorbent.
[0037] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.03 MPa for 1 hour. After 10 absorption and desorption cycles, the regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After 5 cycles, the methyl mercaptan absorbed by each gram of absorbent was 258 mg, according to detection and calculation.
[0038] Example 4
[0039] The same as Example 1, except that histidine was used instead of lysine in the preparation of the absorbent. After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 307 mg of methyl mercaptan was absorbed per gram of the absorbent.
[0040] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.01 MPa and a desorption time of 30 min. The regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After being recycled for 5 times, it was found through testing and calculation that 283 mg of methyl mercaptan was absorbed per gram of absorbent.
[0041] Example 5
[0042] The same as Example 1, except that arginine was used instead of lysine in the preparation of the absorbent. After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 309 mg of methyl mercaptan was absorbed per gram of the absorbent.
[0043] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.01 MPa and a desorption time of 30 min. The regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After being recycled for 5 times, it was found through testing and calculation that 287 mg of methyl mercaptan was absorbed per gram of absorbent.
[0044] Example 6
[0045] The same as Example 1, except that lactic acid was used instead of citric acid in the preparation of the absorbent. After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 288 mg of methyl mercaptan was absorbed per gram of absorbent.
[0046] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.01 MPa and a desorption time of 30 min. The regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After being recycled for 5 times, it was found through testing and calculation that 267 mg of methyl mercaptan was absorbed per gram of absorbent.
[0047] Example 7
[0048] The same as Example 1, except that malonic acid was used instead of citric acid in the preparation of the absorbent. After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 285 mg of methyl mercaptan was absorbed per gram of absorbent.
[0049] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.01 MPa and a desorption time of 30 min. The regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After being recycled for 5 times, it was found through testing and calculation that 260 mg of methyl mercaptan was absorbed per gram of absorbent.
[0050] Example 8
[0051] The same as Example 1, except that malic acid was used instead of citric acid in the preparation of the absorbent. After the absorption reached equilibrium, the weight before and after absorption was measured by gravimetric method, and it was calculated that 294 mg of methyl mercaptan was absorbed per gram of absorbent.
[0052] The rich absorbent at absorption equilibrium was regenerated under reduced pressure at a pressure of 0.01 MPa and a desorption time of 30 min. The regenerated absorbent was used for the absorption of methyl mercaptan-containing gas under the same operating conditions. After being recycled for 5 times, it was found through testing and calculation that 269 mg of methyl mercaptan was absorbed per gram of absorbent.
[0053] Example 9
[0054] The organic sulfide absorbents prepared in Examples 1 and 4-8 were used to absorb different types of organic sulfides, and the absorption effects are shown in Table 1. The absorption conditions were the same as in Example 1.
[0055] Table 1 Absorption effect of different absorbents (unit: mg / g absorbent)
[0056]
[0057] Example 10
[0058] The sulfide concentration in the organic sulfur waste gas discharged from a wastewater treatment station in an oil and gas field is 4233 mg / m 3 , which contains organic sulfides such as hydrogen sulfide, methyl mercaptan, and methyl sulfide, with a concentration of 2132 mg / m 3 The absorbent of Example 1 was used for absorption. The sulfide concentration after absorption was 2236 mg / m 3 , the concentration of organic sulfide is 311 mg / m 3 More than 85% of organic sulfides were absorbed, and the absorption rate of other sulfides was less than 10%.
[0059] Comparative Example 1
[0060] The same as Example 1, except that: in the preparation process of the absorbent, citric acid was not used, and only choline chloride and lysine were contained. After the absorption reached equilibrium, the methyl mercaptan absorbed by each gram of absorbent was 206 mg after detection and calculation. The rich absorbent at the absorption equilibrium was regenerated under reduced pressure, and after being recycled for 5 times, the methyl mercaptan absorbed by each gram of absorbent was 164 mg.
[0061] Comparative Example 2
[0062] The same as Example 1, except that: in the preparation process of the absorbent, choline chloride was not used, and only citric acid and lysine were contained. After the absorption reached equilibrium, it was detected and calculated that 58 mg of methyl mercaptan was absorbed per gram of absorbent. The rich absorbent at absorption equilibrium was regenerated under reduced pressure, and after 5 cycles, 46 mg of methyl mercaptan was absorbed per gram of absorbent.
[0063] Comparative Example 3
[0064] The same as Example 1, except that: in the preparation process of the absorbent, lysine was not used, and only choline chloride and citric acid were contained. After the absorption reached equilibrium, it was detected and calculated that 145 mg of methyl mercaptan was absorbed per gram of absorbent. The rich absorbent at absorption equilibrium was regenerated under reduced pressure, and after 5 cycles, 129 mg of methyl mercaptan was absorbed per gram of absorbent.
[0065] Comparative Example 4
[0066] The same as Example 1, except that benzoic acid was used instead of citric acid during the preparation of the absorbent. After the absorption reached equilibrium, the amount of methyl mercaptan absorbed by each gram of absorbent was 233 mg after detection and calculation. The rich absorbent at the absorption equilibrium was regenerated under reduced pressure, and after 5 cycles, the amount of methyl mercaptan absorbed by each gram of absorbent was 209 mg. In addition, benzoic acid has a strong pungent odor and is not an environmentally friendly green solvent.
[0067] Comparative Example 5
[0068] The same as Example 1, except that proline was used instead of lysine during the preparation of the absorbent. After the absorption reached equilibrium, the amount of methyl mercaptan absorbed by each gram of absorbent was 154 mg after detection and calculation. The rich absorbent at the absorption equilibrium was regenerated under reduced pressure, and after 5 cycles, the amount of methyl mercaptan absorbed by each gram of absorbent was 124 mg. Since proline contains an imino group and is a non-basic amino acid, the absorption effect is poor.
[0069] Comparative Example 6
[0070] The same as Example 1, except that glutamic acid was used instead of lysine in the absorbent preparation process. After the absorption reached equilibrium, the amount of methyl mercaptan absorbed by each gram of absorbent was 123 mg after detection and calculation. The rich absorbent at the absorption equilibrium was regenerated under reduced pressure, and after 5 cycles, the amount of methyl mercaptan absorbed by each gram of absorbent was 110 mg. Since glutamic acid is an acidic amino acid, the absorption effect is not good.
[0071] Comparative Example 7
[0072] The same as Example 1, except that: in the process of treating the waste gas, the absorbent is used to absorb hydrogen sulfide. After the absorption reaches equilibrium, it is detected and calculated that the hydrogen sulfide absorbed by each gram of absorbent is 92 mg. The rich absorbent at the absorption equilibrium is regenerated under reduced pressure, and after being recycled for 5 times, the hydrogen sulfide absorbed by each gram of absorbent is 73 mg.
Claims
1. An organic sulfide absorbent, characterized in that The invention comprises choline chloride, organic carboxylic acid and basic amino acid, wherein the molar ratio of choline chloride to organic carboxylic acid is 1:1-1:10, and the mass of basic amino acid accounts for 1%-15% of the total mass of choline chloride and organic carboxylic acid; the organic carboxylic acid is aliphatic organic carboxylic acid, and the basic amino acid is at least one of lysine, arginine and histidine; the preparation method comprises the following steps: mixing choline chloride and organic carboxylic acid in proportion, heating and stirring until the mixture becomes a uniform liquid; then adding basic amino acid, heating and stirring until the mixture becomes a uniform liquid, and cooling to obtain organic sulfide absorbent.
2. The absorbent according to claim 1, characterized in that: The molar ratio of choline chloride to organic carboxylic acid is 1:2-1:6, and the mass of the basic amino acid accounts for 5%-10% of the total mass of choline chloride and organic carboxylic acid.
3. The absorbent according to claim 1 or 2, characterized in that: The organic carboxylic acid is at least one of citric acid, lactic acid, malonic acid and malic acid.
4. The absorbent according to claim 3, characterized in that: The organic carboxylic acid is citric acid.
5. The absorbent according to claim 1 or 2, characterized in that: The basic amino acid is lysine.
6. The absorbent according to claim 1, characterized in that: The heating temperature is 60-100° C., the stirring speed is 100-200 r / min, and the stirring time is 1-2 h.
7. A method for treating sulfur-containing organic waste gas, characterized in that the organic sulfide absorbent according to any one of claims 1 to 6 is used to contact the sulfur-containing organic waste gas with the organic sulfide absorbent.
8. The method according to claim 7, characterized in that: The sulfur-containing organic waste gas is mainly organic waste gas containing organic sulfide, wherein the organic sulfide is at least one of methyl mercaptan, ethyl mercaptan, methyl sulfide, propyl mercaptan, isopropyl mercaptan and thiophene.
9. The method according to claim 7, characterized in that: The contact conditions between the sulfur-containing organic waste gas and the absorbent are: temperature of 15-30°C, pressure of 0.1-0.3MPa, liquid-gas ratio of 3-5 L / m 3 .
10. The method according to claim 7, characterized in that: After absorption equilibrium is reached, regeneration is carried out using a reduced pressure regeneration method with a pressure of 10 kPa to 0.1 MPa.
11. The method according to claim 10, characterized in that: Regeneration is carried out in a N2 atmosphere, and the regenerated absorbent is recycled.