A method for low-pressure pretreatment of coal tar raw materials

Through low-pressure pretreatment method, combined with centrifugal separation, filtration and hydrogen reaction, the existing coal tar pretreatment problems are solved, and the metal and ash content is efficiently reduced, the process is simplified, and the device operation cycle is extended. And meet environmental protection requirements.

CN116064157BActive Publication Date: 2024-12-06CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111273191.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-29
Publication Date
2024-12-06
Estimated Expiration
2041-10-29

AI Technical Summary

Technical Problem

The existing coal tar pretreatment methods are inefficient, resource utilization is not high, and the introduction of water causes environmental pollution, making it difficult to meet environmental protection requirements, especially when treating coal tar with high metal, high ash and high asphaltene content, the catalyst is deactivated. Fast, the device operation cycle is short.

Method used

Using low-pressure pretreatment method, the metal and ash are effectively reduced by mixing coal tar with organic compound solvent, followed by filtration and centrifugation, combined with the pretreatment reaction in contact with the pretreatment agent under temporary hydrogen conditions. Avoid the introduction of water and simplify the process flow.

Benefits of technology

It effectively reduces the metal and ash content in coal tar, simplifies the process flow, reduces investment and operation costs, avoids environmental pollution, extends the operation cycle of the device, and meets environmental protection requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116064157B_ABST
    Figure CN116064157B_ABST
Patent Text Reader

Abstract

The present disclosure relates to a method for pretreating coal tar raw materials, which comprises: S1, mixing the coal tar raw materials with an organic compound solvent and centrifuging to obtain a first solid phase material and a second liquid phase material; S2, filtering the second liquid phase material to obtain a second liquid phase material and a third liquid phase material, wherein the solid content of the second liquid phase material is higher than that of the third liquid phase material; S3, mixing the second liquid phase material with solvent oil and returning to step S1 for centrifugal separation; S4, contacting the third liquid phase material with a pretreatment agent under hydrogen conditions for pretreatment reaction, and performing gas-liquid separation on the obtained pretreatment reaction product. The method disclosed in the present disclosure is simple, easy to operate, and has low investment cost, and can more effectively reduce the metal and ash content in the pretreated coal tar.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of coal tar processing, and in particular to a method for low-pressure pretreatment of coal tar raw materials. Background Art

[0002] In recent years, my country's demand for petroleum products has been increasing. However, petroleum is a non-renewable energy source and is facing a crisis of depletion. In contrast, China's coal reserves are relatively abundant. Therefore, making alternative liquid fuels from coal has become a basic direction of coal processing and utilization.

[0003] With the development of coal chemical industry, the output of coal tar is increasing, and the clean and efficient use of coal tar is becoming more and more important. At present, the main utilization of coal tar is deep processing to extract chemical products or hydrogenation to produce clean fuel. In recent years, the number of fixed-bed coal tar hydrogenation units in China has increased. Although fixed-bed hydrogenation units have the characteristics of simple operation and small investment, when processing coal tar raw materials with high metal, high ash and high asphaltene content, the pressure drop of the catalyst bed increases rapidly, the heat exchanger is coked and blocked, and the asphaltene is deposited on the catalyst, causing the catalyst to deactivate quickly. The unit is forced to shut down, the start-up time of the unit is shortened, and the economic benefits of the enterprise are seriously affected.

[0004] Therefore, in order to extend the operating cycle of the coal tar hydrogenation unit, the coal tar raw materials need to be pretreated to remove metals and ash and realize the hydrogenation conversion of asphaltene, and then carry out fixed-bed hydrogenation to produce clean fuel, which can greatly extend the operating cycle of the unit.

[0005] At present, the pretreatment of coal tar in China mainly adopts centrifugal separation, sedimentation separation, solvent extraction, electric field purification and filtration separation. These methods have the disadvantages of poor pretreatment effect, low efficiency and low utilization rate of coal tar resources.

[0006] CN106701157A discloses a method for demetallizing high-temperature coal tar. Although the method uses solvent oil dilution, adds alcohol substances and uses a demetallization reactor to pre-treat the high-temperature coal tar to remove metals, water is introduced during the implementation process. The treated water is phenol water, which contains high levels of phenols, ammonia nitrogen, etc., which is difficult to process and does not meet environmental protection requirements.

[0007] CN105713658B discloses a pretreatment process for low-temperature coal tar. The coal tar raw material is pretreated through sedimentation separation, primary electric desalination and secondary electric desalination. The process is complicated and the operation cost is high. In addition, water is introduced during the implementation process, and there is also the problem of difficult treatment of phenol water.

[0008] CN101012385A discloses a method for pretreating coal tar, which utilizes distillate oil and aromatic hydrocarbons to perform two-stage extraction on coal tar to remove ash and asphaltene, etc. Although the solvent extraction separation method has a good purification effect, it uses a large amount of solvent, has a complex process, and has high operating costs. Summary of the invention

[0009] The purpose of the present invention is to provide a method for low-pressure pretreatment of coal tar raw materials, which is simple, easy to operate, and has low investment costs, and can more effectively reduce the metal and ash contents in the pretreated coal tar.

[0010] In order to achieve the above-mentioned purpose, the present disclosure provides a method for pretreating coal tar raw materials, which comprises: S1, mixing the coal tar raw materials with an organic compound solvent and then centrifuging to obtain a first solid phase material and a first liquid phase material; S2, filtering the first liquid phase material to obtain a second liquid phase material and a third liquid phase material, wherein the second liquid phase material has a higher solid content than the third liquid phase material; S3, mixing the second liquid phase material with solvent oil and then returning to step S1 to perform the centrifugal separation; S4, contacting the third liquid phase material with a pretreatment agent under hydrogen conditions to perform a pretreatment reaction, and performing gas-liquid separation on the obtained pretreatment reaction product.

[0011] Optionally, in step S1, the volume ratio of the organic compound solvent to the coal tar raw material is (0.005-0.5):1, preferably (0.01-0.3):1;

[0012] In step S3, the volume ratio of the solvent oil to the second liquid phase material is (0.05-2):1, preferably (0.1-1.5):1.

[0013] Optionally, in step S2, the filtering conditions include: a temperature of 80-250° C. and a pressure of 0.1-1.0 MPa, preferably, the temperature is 100-230° C. and the pressure is 0.3-0.6 MPa;

[0014] Based on the total weight of the first liquid phase material, the amount of the second liquid phase material is 3-30 weight %, preferably 5-20 weight %.

[0015] Optionally, in step S4, after the third liquid phase material is contacted with a first pretreatment agent for a first reaction, the obtained first reaction product is contacted with a second pretreatment agent for a second reaction to obtain the pretreatment reaction product;

[0016] The active components in the first pretreatment agent and the second pretreatment agent are each independently a metal of Group VIB and / or a metal of Group VIII.

[0017] Optionally, in step S4, the conditions of the first reaction include: hydrogen partial pressure of 0.5-3.5 MPa, reaction temperature of 120-300°C, hydrogen-oil volume ratio of 10-500 Nm 3 / m 3 , the volume space velocity of raw material liquid is 0.2-2h -1 ;

[0018] Preferably, the hydrogen partial pressure is 1-3 MPa, the reaction temperature is 180-280°C, and the hydrogen-to-oil volume ratio is 30-300 Nm 3 / m 3 The raw material liquid volume space velocity is 0.3-1.5h -1 ;

[0019] The conditions of the second reaction include: hydrogen partial pressure of 0.5-3.5 MPa, reaction temperature of 160-340°C, hydrogen-to-oil volume ratio of 10-500 Nm 3 / m 3 , the volume space velocity of raw material liquid is 0.15-1.5h -1 ;

[0020] Preferably, the hydrogen partial pressure is 1-3 MPa, the reaction temperature is 200-320°C, and the hydrogen-oil volume ratio is 30-300 Nm 3 / m 3 The raw material liquid has a volume space velocity of 0.2-1h -1 .

[0021] Optionally, the first pretreatment agent includes pretreatment agent I, pretreatment agent II, pretreatment agent III and pretreatment agent IV arranged in sequence from upstream to downstream; the second pretreatment agent includes pretreatment agent IV, pretreatment agent V and pretreatment agent VI arranged in sequence from upstream to downstream;

[0022] The average diameter of the pretreatment agent I is 15-17 mm, and the carrier is silicon oxide or aluminum oxide;

[0023] The average diameter of the pretreatment agent II is 9-11 mm, and based on the total weight of the pretreatment agent II, it contains 0.05-0.2 wt % of nickel oxide, 0.5-1.0 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide;

[0024] The average diameter of the pretreatment agent III is 5.6-6.5 mm, and based on the total weight of the pretreatment agent III, it contains 0.1-0.5 wt % of nickel oxide, 0.5-2.5 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide;

[0025] The average diameter of the pretreatment agent IV is 2.5-3.5 mm, and based on the total weight of the pretreatment agent IV, it contains 0.1-1 wt % of nickel oxide, 1-5.5 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide;

[0026] The pretreatment agent V has an average diameter of 1-1.2 mm and contains 0.5-1.5 wt % of nickel oxide, 1.5-6.5 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide, based on the total weight of the pretreatment agent V;

[0027] The average diameter of the pretreatment agent VI is 1-1.2 mm. Based on the total weight of the pretreatment agent VI, the pretreatment agent VI contains 1-3 wt % of nickel oxide, 5-8 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide.

[0028] Optionally, relative to 100 volumes of the pretreatment agent IV used in the second reaction, in the first reaction, the amount of the pretreatment agent I is 10-40 volumes, the amount of the pretreatment agent II is 10-40 volumes, the amount of the pretreatment agent III is 20-60 volumes, and the amount of the pretreatment agent IV is 20-60 volumes;

[0029] In the second reaction, the amount of the pretreatment agent V is 40-80 volumes, and the amount of the pretreatment agent VI is 40-80 volumes.

[0030] Optionally, the organic compound solvent includes one or more of C5-C9 hydrocarbons, C1-C4 alcohols, inorganic acids, organic acids, organic amines and quaternary ammonium salts;

[0031] Preferably, the organic compound solvent includes one or more of n-pentane, n-hexane, n-heptane, benzene, toluene, xylene, methanol, ethanol, formic acid, acetic acid, oxalic acid, phosphoric acid, citric acid, tartaric acid, pyruvic acid, ethanolamine, quaternary ammonium salt and polyethylene glycol;

[0032] The solvent oil includes one or more of naphtha, kerosene, diesel, tail oil, light oil, phenol oil, wash oil, naphthalene oil and anthracene oil.

[0033] Optionally, in step S1, a centrifugal separation device is used for the centrifugal separation, and the centrifugal separation device is selected from a horizontal screw centrifuge and / or a disc centrifuge; the conditions for the centrifugal separation include: an operating temperature of 50-120°C and a rotation speed of 3000-8000 rpm.

[0034] Optionally, in step S2, a filtering device is used for the filtering, and a filter element of the filtering device is selected from one of a stainless steel sintered wire mesh, a stainless steel sintered powder, a ceramic membrane and a flexible filter cloth.

[0035] Optionally, the coal tar raw material includes one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar, or a mixture of one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar with anthracene oil and / or wash oil.

[0036] Through the above technical solution, the method disclosed in the present invention has the following advantages:

[0037] (1) More effectively reduce the metal and ash content in pretreated coal tar;

[0038] (2) It has the advantages of low investment, simple process flow, simple operation and low operating cost;

[0039] (3) No water is introduced, thus avoiding the environmental pollution caused by the difficulty in treating phenol water and meeting environmental protection requirements.

[0040] Other features and advantages of the present disclosure will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] The accompanying drawings are used to provide a further understanding of the present disclosure and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present disclosure but do not constitute a limitation of the present disclosure. In the accompanying drawings:

[0042] Figure 1 It is a schematic flow diagram of the method for low-pressure pretreatment of coal tar feedstock provided in the present disclosure.

[0043] Description of Reference Numerals

[0044] 1. Coal tar raw material 2. Organic compound solvent 3. Mixing tank

[0045] 4. Solvent oil 5. First solid-liquid separator 6. First solid phase material

[0046] 7. Second solid-liquid separator 8. Hydrogen-containing gas 9. First pretreatment tank

[0047] 10. Second pretreatment tank 11. Gas-liquid separation tank 12. Gas

[0048] 13. Pretreatment product tank DETAILED DESCRIPTION

[0049] The specific implementation of the present disclosure is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described herein is only used to illustrate and explain the present disclosure, and is not used to limit the present disclosure.

[0050] The present disclosure provides a method for pretreating a coal tar raw material, which comprises: S1, mixing the coal tar raw material with an organic compound solvent and then centrifuging to obtain a first solid phase material and a first liquid phase material; S2, filtering the first liquid phase material to obtain a second liquid phase material and a third liquid phase material, wherein the second liquid phase material has a higher solid content than the third liquid phase material; S3, mixing the second liquid phase material with solvent oil and then returning to step S1 to perform the centrifugal separation; S4, contacting the third liquid phase material with a pretreatment agent under hydrogen conditions to perform a pretreatment reaction, and performing gas-liquid separation on the obtained pretreatment reaction product.

[0051] The method disclosed in the present invention adopts a process operation of centrifugal separation combined with filtration in the pretreatment of coal tar raw materials, and uses organic compound solvents and solvent oil to assist separation in the two steps of centrifugal separation and filtration, respectively, which can more effectively reduce the metal and ash content in the pretreated coal tar.

[0052] In a specific embodiment of the present disclosure, the content of organic impurities in the third liquid phase material is not more than 0.015% by weight, preferably not more than 0.01% by weight, and the content of organic impurities in the second liquid phase material is not less than 1% by weight, preferably not less than 1.5% by weight.

[0053] In a specific embodiment of the present disclosure, in step S1, the volume ratio of the organic compound solvent to the coal tar raw material is (0.005-0.5): 1, preferably (0.01-0.3): 1. According to the present disclosure, the temperature for mixing the coal tar raw material and the solvent in step S1 is not specifically limited, for example, it can be 50-75°C.

[0054] In a specific embodiment of the present disclosure, in step S2, the filtering conditions include: a temperature of 80-250° C. and a pressure of 0.1-1.0 MPa, preferably, a temperature of 100-230° C. and a pressure of 0.3-0.6 MPa. Wherein, based on the total weight of the first liquid phase material, the amount of the second liquid phase material is 3-30% by weight, preferably 5-20% by weight, and more preferably 8-15% by weight.

[0055] In a specific embodiment of the present disclosure, in step S3, the volume ratio of the solvent oil to the second liquid phase material is (0.05-2): 1, preferably (0.1-1.5): 1. According to the present disclosure, the temperature for mixing the second liquid phase material with the solvent oil in step S3 is not specifically limited, for example, it can be 50-100°C.

[0056] In a specific embodiment of the present disclosure, in step S4, after the third liquid phase material is contacted with a first pretreatment agent for a first reaction, the first reaction product is contacted with a second pretreatment agent for a second reaction to obtain the pretreatment reaction product; the active components in the first pretreatment agent and the second pretreatment agent are each independently a Group VIB metal and / or a Group VIII metal.

[0057] In a preferred embodiment of the present disclosure, in step S4, the conditions of the first reaction include: a hydrogen partial pressure of 0.5-3.5 MPa, a reaction temperature of 120-300°C, a hydrogen-to-oil volume ratio of 10-500 Nm 3 / m 3 , the volume space velocity of raw material liquid is 0.2-2h -1 Preferably, the hydrogen partial pressure is 1-3MPa, the reaction temperature is 180-280°C, and the hydrogen-to-oil volume ratio is 30-300Nm 3 / m 3 The raw material liquid volume space velocity is 0.3-1.5h -1 ;

[0058] The conditions of the second reaction include: hydrogen partial pressure of 0.5-3.5 MPa, reaction temperature of 160-340°C, hydrogen-to-oil volume ratio of 10-500 Nm 3 / m 3 , the volume space velocity of raw material liquid is 0.15-1.5h -1 Preferably, the hydrogen partial pressure is 1-3MPa, the reaction temperature is 200-320°C, and the hydrogen-oil volume ratio is 30-300Nm 3 / m 3 The raw material liquid has a volume space velocity of 0.2-1h -1 .

[0059] In a specific embodiment of the present disclosure, the first pretreatment agent includes pretreatment agent I, pretreatment agent II, pretreatment agent III and pretreatment agent IV arranged in sequence from upstream to downstream; the second pretreatment agent includes pretreatment agent IV, pretreatment agent V and pretreatment agent VI arranged in sequence from upstream to downstream;

[0060] The average diameter of the pretreatment agent I is 15-17 mm, and the carrier is silicon oxide or aluminum oxide; the average diameter of the pretreatment agent II is 9-11 mm, and based on the total weight of the pretreatment agent II, it contains 0.05-0.2 wt% of nickel oxide, 0.5-1.0 wt% of molybdenum oxide, and the balance of silicon oxide or aluminum oxide; the average diameter of the pretreatment agent III is 5.6-6.5 mm, and based on the total weight of the pretreatment agent III, it contains 0.1-0.5 wt% of nickel oxide, 0.5-2.5 wt% of molybdenum oxide, and the balance of silicon oxide or aluminum oxide; the average diameter of the pretreatment agent IV is 2.5-3. The average diameter of the pretreatment agent V is 1-1.2 mm, and based on the total weight of the pretreatment agent V, it contains 0.5-1.5 wt% of nickel oxide, 1.5-6.5 wt% of molybdenum oxide, and the balance is silicon oxide or aluminum oxide. The average diameter of the pretreatment agent VI is 1-1.2 mm, and based on the total weight of the pretreatment agent VI, it contains 1-3 wt% of nickel oxide, 5-8 wt% of molybdenum oxide, and the balance is silicon oxide or aluminum oxide.

[0061] In a specific embodiment of the present disclosure, relative to 100 volumes of the pretreatment agent IV used in the second reaction, in the first reaction, the amount of the pretreatment agent I is 10-40 volumes, the amount of the pretreatment agent II is 10-40 volumes, the amount of the pretreatment agent III is 20-60 volumes, and the amount of the pretreatment agent IV is 20-60 volumes; in the second reaction, the amount of the pretreatment agent V is 40-80 volumes, and the amount of the pretreatment agent VI is 40-80 volumes.

[0062] In a specific embodiment of the present disclosure, the organic compound solvent includes one or more of C5-C9 hydrocarbons, C1-C4 alcohols, inorganic acids, organic acids, organic amines and quaternary ammonium salts; preferably, the organic compound solvent includes one or more of n-pentane, n-hexane, n-heptane, benzene, toluene, xylene, methanol, ethanol, formic acid, acetic acid, oxalic acid, phosphoric acid, citric acid, tartaric acid, pyruvic acid, ethanolamine, quaternary ammonium salts and polyethylene glycol.

[0063] In a specific embodiment of the present disclosure, the solvent oil may be one or more of a hydrogenated product oil, a cut fraction oil of a coal tar raw material, and the solvent oil. The hydrogenated product oil may be obtained by hydrogenating one or more of a petroleum-based raw material, a coal tar raw material, and a Fischer-Tropsch synthetic oil, for example, may include one or more of naphtha, kerosene, diesel, and tail oil, and the cut fraction oil of the coal tar raw material may include one or more of light oil, phenol oil, wash oil, naphthalene oil, and anthracene oil.

[0064] In a specific embodiment of the present disclosure, in step S1, a centrifugal separation device is used to perform the centrifugal separation, and the centrifugal separation device is selected from a horizontal screw centrifuge and / or a disc centrifuge; the conditions for the centrifugal separation may include: an operating temperature of 50-120°C and a rotation speed of 3000-8000 rpm.

[0065] In a specific embodiment of the present disclosure, in step S2, a filtering device is used for the filtration, and the filtering device can be any device that can have a filtering effect, and the filter element of the filtering device can be selected from one of stainless steel sintered wire mesh, stainless steel sintered powder, ceramic membrane and flexible filter cloth.

[0066] According to the present disclosure, coal tar is well known to those skilled in the art, and refers to coal tar produced by coal pyrolysis or coal gasification or other processes. The coal tar raw material may include low-temperature coal tar produced in the coal gasification process, or may be one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar produced in coal pyrolysis or coking process (including low-temperature pyrolysis, medium-temperature pyrolysis and high-temperature coking process), or a mixture of one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar with anthracene oil and / or wash oil.

[0067] According to the present disclosure, the distillation range of the low-temperature coal tar can be 50-450°C; the distillation range of the medium-low temperature coal tar can be 50-550°C; the distillation range of the medium-temperature coal tar can be 50-600°C; the distillation range of the high-temperature coal tar can be 50-650°C.

[0068] like Figure 1 As shown, in a preferred embodiment of the present disclosure, the low-pressure pretreatment of coal tar raw material is carried out by a method comprising the following steps:

[0069] S1, the coal tar raw material 1 to be pretreated and the organic compound solvent 2 are introduced into a mixing tank 3 for mixing, and then introduced into a first solid-liquid separator 5 for centrifugal separation of solid residue and liquid to obtain a first solid phase material 6 and a second liquid phase material;

[0070] S2, introducing the second liquid phase material into the second solid-liquid separator 7 for filtration to obtain a second liquid phase material and a third liquid phase material, wherein the solid content of the second liquid phase material is higher than that of the third liquid phase material;

[0071] S3, mixing the second liquid phase material with solvent oil 4 and returning to the first solid-liquid separator 5 in step S1 to further centrifuge the solid residue and liquid stream;

[0072] S4. The third liquid phase material is mixed with the hydrogen-containing gas 8 and then enters the first pretreatment tank 9 and the second pretreatment tank 10 in sequence to contact with the pretreatment agent for pretreatment reaction. The pretreatment reaction product is introduced into the gas-liquid separation tank 11 for gas-liquid separation. The separated gas 12 is used as fuel gas, and the separated liquid flow is the pretreated product, which then enters the pretreatment product tank 13. The pretreated product is used as the raw material for the subsequent fixed bed hydrogenation device.

[0073] In a specific embodiment of the present disclosure, the first pretreatment tank and the second pretreatment tank can be independently selected from an upflow operation mode or a downflow operation mode.

[0074] In a specific embodiment of the present disclosure, the number of the first pretreatment tank and the number of the second pretreatment tank may be more than two, and the first pretreatment tank and the second pretreatment tank are arranged in series.

[0075] In a specific embodiment of the present disclosure, when the pressure drop of the first pretreatment tank reaches 0.5-0.7MPa, the first pretreatment tank can be cut out of the system and the reaction flow from the first pretreatment tank to the second pretreatment tank is operated. At this time, the cut-out first pretreatment tank is cleaned and the pretreatment agent is replaced. After the pretreatment agent of the first pretreatment tank is replaced, the reaction flow is improved to the first pretreatment tank and operated in series with the second pretreatment tank. When the pressure drop of the second pretreatment tank reaches 0.5-0.7MPa, the flow from the first pretreatment tank is improved to the gas-liquid separator, and the second pretreatment tank is cut out of the system for cleaning and replacement of the pretreatment agent. After the pretreatment agent of the second pretreatment tank is replaced, the flow from the first pretreatment tank is improved to the second pretreatment tank.

[0076] The present disclosure is further illustrated below by way of examples, but the present disclosure is not limited thereby.

[0077] In the following examples, unless otherwise specified, all the raw materials used are commercially available. The properties of the coal tar raw materials to be pretreated used below are shown in Table 1.

[0078] In Examples 1-6, along the direction of the reactant flow, the first pretreatment agents in the first pretreatment tank are pretreatment agent I, pretreatment agent II, pretreatment agent III and pretreatment agent IV; the second pretreatment agents in the second pretreatment tank are pretreatment agent IV, pretreatment agent V and pretreatment agent VI.

[0079] Among them, pretreatment agent I is a porous cylindrical pretreatment agent with a carrier of silicon oxide or aluminum oxide and a diameter of 15-17 mm; pretreatment agent II is a honeycomb cylindrical pretreatment agent with a diameter of 9-11 mm, and its composition is 0.15% by weight of nickel oxide, 0.8% by weight of molybdenum oxide, and the balance is silicon oxide or aluminum oxide; pretreatment agent III is a Raschig ring with a diameter of 5.6-6.5 mm, and its composition is 0.3% by weight of nickel oxide, 1.5% by weight of molybdenum oxide, and the balance is silicon oxide or aluminum oxide; pretreatment agent IV It is in the shape of a Raschig ring with a diameter of 2.5-3.5 mm, and its composition is 0.5% by weight of nickel oxide, 2.5% by weight of molybdenum oxide, and the balance is silicon oxide or aluminum oxide; pretreatment agent V is in the shape of a clover with a diameter of 1-1.2 mm, and its composition is 1.0% by weight of nickel oxide, 3.5% by weight of molybdenum oxide, and the balance is silicon oxide or aluminum oxide; pretreatment agent VI is in the shape of a butterfly with a diameter of 1.0-1.2 mm, and its composition is 2.0% by weight of nickel oxide, 6.0% by weight of molybdenum oxide, and the balance is silicon oxide or aluminum oxide.

[0080] In the following examples, unless otherwise specified, based on the pretreatment agent IV in the second pretreatment tank, the filling volume of the pretreatment agent I in the first pretreatment tank is 20 volume %, the filling volume of the pretreatment agent II is 20 volume %, the filling volume of the pretreatment agent III is 35 volume %, and the filling volume of the pretreatment agent IV is 35 volume %. The filling volume of the pretreatment agent V in the second pretreatment tank is 60 volume %, and the filling volume of the pretreatment agent VI is 60 volume %.

[0081] Example 1

[0082] S1, using the coal tar to be pretreated as a raw material, and mixing n-heptane with the raw material in a mixing tank at a volume ratio of 0.15:1, and then entering the first solid-liquid separator for centrifugal separation of solid residue and liquid to obtain a first solid phase material and a first liquid phase material;

[0083] S2, introducing the first liquid phase material into a second solid-liquid separator and filtering at 160° C. and 0.4 MPa to obtain a second liquid phase material and a third liquid phase material, wherein the solid content of the second liquid phase material is higher than that of the third liquid phase material, and the amount of the second liquid phase material is 10% by weight based on the total weight of the first liquid phase material;

[0084] S3, mixing the second liquid phase material separated by the second solid-liquid separator with the hydrogenated tail oil and introducing the mixture into the first solid-liquid separator for further solid-liquid centrifugal separation, wherein the volume ratio of the hydrogenated tail oil to the second liquid phase material is 1:1;

[0085] S4. The third liquid phase material separated by the second solid-liquid separator is mixed with the hydrogen-containing gas and enters the first pretreatment tank and the second pretreatment tank in turn to contact with the pretreatment agent for pretreatment reaction. The logistics coming out of the pretreatment tank enters the gas-liquid separation tank for gas-liquid separation. The separated gas is used as fuel gas, and the separated liquid logistics is the pretreated product, which then enters the pretreatment product tank. The pretreatment product is suitable as a raw material for the subsequent coal tar hydrogenation unit.

[0086] The specific operating conditions of the pretreatment tank are shown in Table 2, and the properties of the pretreated coal tar are shown in Table 3.

[0087] Example 2

[0088] S1, using the coal tar to be pretreated as a raw material, and mixing xylene with the raw material in a mixing tank at a volume ratio of 0.05:1, and then entering the first solid-liquid separator for centrifugal separation of solid residue and liquid to obtain a first solid phase material and a first liquid phase material;

[0089] S2, introducing the first liquid phase material into a second solid-liquid separator for filtration at 100° C. and 0.45 MPa to obtain a second liquid phase material and a third liquid phase material, wherein the solid content of the second liquid phase material is higher than that of the third liquid phase material, and the amount of the second liquid phase material is 8% by weight based on the total weight of the first liquid phase material;

[0090] S3, mixing the second liquid phase material separated by the second solid-liquid separator with the light oil and introducing the mixture into the first solid-liquid separator for further solid-liquid centrifugal separation, wherein the volume ratio of the light oil to the second liquid phase material is 0.2:1;

[0091] S4. The third liquid phase material separated by the second solid-liquid separator is mixed with the hydrogen-containing gas and enters the first pretreatment tank and the second pretreatment tank in turn to contact with the pretreatment agent for pretreatment reaction. The logistics coming out of the pretreatment tank enters the gas-liquid separation tank for gas-liquid separation. The separated gas is used as fuel gas, and the separated liquid logistics is the pretreated product, which then enters the pretreatment product tank. The pretreatment product is suitable as a raw material for the subsequent coal tar hydrogenation unit.

[0092] The specific operating conditions of the pretreatment tank are shown in Table 2, and the properties of the pretreated coal tar are shown in Table 3.

[0093] Example 3

[0094] S1, using the coal tar to be pretreated as a raw material, and mixing ethanol with the raw material in a mixing tank at a volume ratio of 0.3:1, and then entering the first solid-liquid separator for centrifugal separation of solid residue and liquid to obtain a first solid phase material and a first liquid phase material;

[0095] S2, introducing the first liquid phase material into a second solid-liquid separator for filtration at 230° C. and 0.35 MPa to obtain a second liquid phase material and a third liquid phase material, wherein the solid content of the second liquid phase material is higher than that of the third liquid phase material, and the amount of the second liquid phase material is 15% by weight based on the total weight of the first liquid phase material;

[0096] S3, mixing the second liquid phase material separated by the second solid-liquid separator with the wash oil and introducing the mixture into the first solid-liquid separator for further solid-liquid centrifugal separation, wherein the volume ratio of the wash oil to the second liquid phase material is 1.5:1;

[0097] S4. The third liquid phase material separated by the second solid-liquid separator is mixed with the hydrogen-containing gas and enters the first pretreatment tank and the second pretreatment tank in turn to contact with the pretreatment agent for pretreatment reaction. The logistics coming out of the pretreatment tank enters the gas-liquid separation tank for gas-liquid separation. The separated gas is used as fuel gas, and the separated liquid logistics is the pretreated product, which then enters the pretreatment product tank. The pretreatment product is suitable as a raw material for the subsequent coal tar hydrogenation unit.

[0098] The specific operating conditions of the pretreatment tank are shown in Table 2, and the properties of the pretreated coal tar are shown in Table 3.

[0099] Example 4

[0100] The coal tar raw material was pretreated in the same manner as in Example 1, except that in step S1, the volume ratio of n-heptane to the coal tar to be pretreated was 0.4:1.

[0101] Example 5

[0102] The coal tar raw material was pretreated in the same manner as in Example 1, except that in step S2, the filtration temperature was 90° C. and 0.2 MPa, and the amount of the second liquid phase material obtained was 30% by weight based on the total weight of the first liquid phase material.

[0103] Example 6

[0104] The coal tar feedstock was pretreated in the same manner as in Example 1, except that in step S3, the volume ratio of the hydrogenated tail oil to the second liquid phase material was 0.08:1.

[0105] Example 7

[0106] The coal tar raw material is pretreated in the same manner as in Example 1, except that in step S4, the third liquid phase material separated by the second solid-liquid separator is mixed with the hydrogen-containing gas and then enters only the first pretreatment tank to contact the pretreatment agent in the first pretreatment tank for pretreatment reaction.

[0107] Comparative Example 1

[0108] Compared with Example 1, the difference is that the second solid-liquid separator is not set in Example 1, and the first liquid phase material from the first solid-liquid separator is mixed with the hydrogen-containing gas and directly enters the first pretreatment tank and the second pretreatment tank to contact the pretreatment agent for reaction.

[0109] The specific operating conditions of the pretreatment tank are shown in Table 2, and the properties of the pretreated coal tar are shown in Table 3.

[0110] Table 1

[0111]

[0112]

[0113] Table 2

[0114]

[0115] Table 3

[0116]

[0117] It can be seen from the above that the method disclosed in the present invention can more effectively reduce the metal and ash contents in pretreated coal tar.

[0118] The preferred embodiments of the present disclosure are described in detail above in conjunction with the accompanying drawings; however, the present disclosure is not limited to the specific details in the above embodiments. Within the technical concept of the present disclosure, a variety of simple modifications can be made to the technical solution of the present disclosure, and these simple modifications all fall within the protection scope of the present disclosure.

[0119] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present disclosure will not further describe various possible combinations.

[0120] In addition, various embodiments of the present disclosure may be arbitrarily combined, and as long as they do not violate the concept of the present disclosure, they should also be regarded as the contents disclosed by the present disclosure.

Claims

1. A method for pretreating coal tar raw materials, wherein: The method includes: S1, mixing the coal tar raw material and the organic compound solvent and then centrifuging to obtain a first solid phase material and a first liquid phase material; The volume ratio of the organic compound solvent to the coal tar raw material is (0.005-0.5):1; the organic compound solvent includes one or more of C5-C9 hydrocarbons, C1-C4 alcohols, organic acids, ethanolamines and polyethylene glycols; S2, filtering the first liquid phase material to obtain a second liquid phase material and a third liquid phase material, wherein the second liquid phase material has a higher solid content than the third liquid phase material; The filtering conditions include: a temperature of 80-250° C. and a pressure of 0.1-1.0 MPa; the amount of the second liquid phase material is 3-30% by weight based on the total weight of the first liquid phase material; and a filtering device is used for the filtering, wherein the filter element of the filtering device is selected from one of a stainless steel sintered wire mesh, a stainless steel sintered powder, a ceramic membrane and a flexible filter cloth; S3, mixing the second liquid phase material with solvent oil and returning to step S1 for the centrifugal separation; Wherein, the volume ratio of the solvent oil to the second liquid phase material is (0.05-2):1; The solvent oil is a hydrogenated product oil and / or a cut fraction oil of a coal tar raw material, wherein the hydrogenated product oil is obtained by hydrogenating one or more of a petroleum-based raw material, a coal tar raw material and a Fischer-Tropsch synthetic oil, and includes one or more of naphtha, kerosene, diesel and tail oil, and the cut fraction oil of the coal tar raw material includes one or more of light oil, phenol oil, wash oil, naphthalene oil and anthracene oil; S4. Under hydrogen conditions, the third liquid phase material is brought into contact with a pretreatment agent to perform a pretreatment reaction, and the obtained pretreatment reaction product is subjected to gas-liquid separation.

2. The method according to claim 1, wherein: In step S1, the volume ratio of the organic compound solvent to the coal tar raw material is (0.01-0.3): 1; In step S3, the volume ratio of the solvent oil to the second liquid phase material is (0.1-1.5):

1.

3. The method according to claim 1, wherein: In step S2, the filtering conditions include: the temperature is 100-230°C, and the pressure is 0.3-0.6MPa; Based on the total weight of the first liquid phase material, the amount of the second liquid phase material is 5-20 weight %.

4. The method according to claim 1, wherein: In step S4, after the third liquid phase material is contacted with the first pretreatment agent for a first reaction, the obtained first reaction product is contacted with the second pretreatment agent for a second reaction to obtain the pretreatment reaction product; The active components in the first pretreatment agent and the second pretreatment agent are each independently a metal of Group VIB and / or a metal of Group VIII.

5. The method according to claim 4, wherein: In step S4, the conditions of the first reaction include: hydrogen partial pressure of 0.5-3.5 MPa, reaction temperature of 120-300°C, hydrogen-to-oil volume ratio of 10-500 Nm 3 / m 3 , the volume space velocity of raw material liquid is 0.2-2h -1 ; The conditions of the second reaction include: hydrogen partial pressure of 0.5-3.5 MPa, reaction temperature of 160-340°C, hydrogen-to-oil volume ratio of 10-500 Nm 3 / m 3 , the volume space velocity of raw material liquid is 0.15-1.5h -1 .

6. The method according to claim 5, wherein: In step S4, the conditions of the first reaction include: the hydrogen partial pressure is 1-3 MPa, the reaction temperature is 180-280°C, the hydrogen-to-oil volume ratio is 30-300 Nm 3 / m 3 The raw material liquid volume space velocity is 0.3-1.5h -1 ; The conditions of the second reaction include: the hydrogen partial pressure is 1-3 MPa, the reaction temperature is 200-320°C, the hydrogen-oil volume ratio is 30-300 Nm 3 / m 3 The raw material liquid has a volume space velocity of 0.2-1h -1 .

7. The method according to claim 4, wherein: The first pretreatment agent includes pretreatment agent I, pretreatment agent II, pretreatment agent III and pretreatment agent IV arranged in sequence from upstream to downstream; the second pretreatment agent includes pretreatment agent IV, pretreatment agent V and pretreatment agent VI arranged in sequence from upstream to downstream; The average diameter of the pretreatment agent I is 15-17 mm, and the carrier is silicon oxide or aluminum oxide; The average diameter of the pretreatment agent II is 9-11 mm, and based on the total weight of the pretreatment agent II, it contains 0.05-0.2 wt % of nickel oxide, 0.5-1.0 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide; The average diameter of the pretreatment agent III is 5.6-6.5 mm, and based on the total weight of the pretreatment agent III, it contains 0.1-0.5 wt % of nickel oxide, 0.5-2.5 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide; The average diameter of the pretreatment agent IV is 2.5-3.5 mm, and based on the total weight of the pretreatment agent IV, it contains 0.1-1 wt % of nickel oxide, 1-5.5 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide; The pretreatment agent V has an average diameter of 1-1.2 mm and contains 0.5-1.5 wt % of nickel oxide, 1.5-6.5 wt % of molybdenum oxide, and the remainder of silicon oxide or aluminum oxide, based on the total weight of the pretreatment agent V; The average diameter of the pretreatment agent VI is 1-1.2 mm. Based on the total weight of the pretreatment agent VI, the pretreatment agent VI contains 1-3 wt % of nickel oxide, 5-8 wt % of molybdenum oxide, and the balance of silicon oxide or aluminum oxide.

8. The method according to claim 7, wherein: Relative to 100 volumes of the pretreatment agent IV used in the second reaction, in the first reaction, the amount of the pretreatment agent I is 10-40 volumes, the amount of the pretreatment agent II is 10-40 volumes, the amount of the pretreatment agent III is 20-60 volumes, and the amount of the pretreatment agent IV is 20-60 volumes; In the second reaction, the amount of the pretreatment agent V is 40-80 volumes, and the amount of the pretreatment agent VI is 40-80 volumes.

9. The method according to claim 1, wherein: The organic compound solvent includes one or more of n-pentane, n-hexane, n-heptane, benzene, toluene, xylene, methanol, ethanol, formic acid, acetic acid, oxalic acid, citric acid, tartaric acid, pyruvic acid, ethanolamine and polyethylene glycol.

10. The method according to claim 1, wherein: In step S1, the centrifugal separation is performed using a centrifugal separation device, and the centrifugal separation device is selected from a horizontal screw centrifuge and / or a disc centrifuge; The conditions for the centrifugal separation include: an operating temperature of 50-120° C. and a rotation speed of 3000-8000 rpm.

11. The method according to claim 1, wherein: The coal tar raw material includes one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar, or a mixture of one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar with anthracene oil and / or washing oil.