A corrosion-resistant fiber cement board carbonization reactor and manufacturing method

By using concrete cast carbonization reactor shell and spraying inorganic coating, the problem of rust in traditional metal carbonization reactors is solved, the strength and durability of the carbonization reactor of fiber cement boards is improved, the maintenance cost is reduced, and the maintenance cost is achieved High-efficiency carbonization of carbon mineralized fiber cement boards.

CN116217171BActive Publication Date: 2024-11-05WUHAN UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310194723.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-02-28
Publication Date
2024-11-05
Estimated Expiration
2043-02-28

AI Technical Summary

Technical Problem

Traditional metal carbonization reactors are prone to rust in high humidity and heat environments, affecting the strength and appearance of fiber cement boards, and are costly and have a long maintenance cycle.

Method used

The carbonization reactor shell is cast with concrete slurry and sprayed with inorganic coating on its inner surface. It uses ultra-high performance concrete and organic synthetic PVA fiber reinforced materials, combined with calcium silicate ore powder and styrene butadiene emulsion to form corrosion resistance carbonization reactor.

Benefits of technology

It effectively avoids rust problems, improves the strength and durability of the carbonization reactor, reduces maintenance costs, and meets the atmospheric carbonization needs of carbon mineralized fiber cement boards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116217171B_ABST
    Figure CN116217171B_ABST
Patent Text Reader

Abstract

The present invention relates to a corrosion-resistant fiber cement board carbonization reactor and a manufacturing method, comprising a carbonization reactor shell and a coating arranged on the inner side wall of the carbonization reactor shell; the carbonization reactor shell is made by casting concrete slurry; the raw materials of the concrete slurry include a first cementitious component, fine aggregate, water, a first water reducer and a reinforcing material in a mass ratio of (950-1100): (1100-1200): (20-30): (15-20); the raw materials of the coating include a second cementitious component, water, a second water reducer and an organic admixture. The present invention casts the carbonization reactor shell with concrete slurry, and then attaches a coating to form a corrosion-resistant fiber cement board carbonization reactor, thereby avoiding the corrosion of traditional metal carbonization reactors in a high-humidity and hot environment, and the coating can improve the impermeability and density of concrete, and increase the strength, durability and service life of the carbonization reactor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of building materials, and in particular to a carbonization reactor for a corrosion-resistant fiber cement board and a manufacturing method thereof. Background Art

[0002] With the rapid advancement of urbanization and industrialization, industrial waste gas generated in various fields has caused the concentration of carbon dioxide in the air to reach a historical high. How to reasonably control the emission and utilization of carbon dioxide has become an urgent problem to be solved. Carbon mineralization technology for building materials is an effective way to absorb and utilize carbon dioxide. Carbon mineralized fiber cement board is a new type of board. Its carbonization curing process can not only provide the strength source of the board, but also fix a large amount of carbon dioxide, which is energy-saving and environmentally friendly.

[0003] However, due to the different carbonization curing conditions, the carbonization curing process of fiber cement board also exposes many problems. Among them, the carbonization curing of carbon mineralized fiber cement board needs to be carried out in a carbonization reactor. The material of the carbonization reactor is usually metal, but the high humidity and heat environment during the carbonization process makes the traditional metal carbonization reactor very easy to rust even with anti-rust measures. While destroying the carbonization reactor, it also pollutes the fiber cement board products, seriously affecting the strength and appearance of the board. In addition, the cost of the metal carbonization reactor is expensive, and the subsequent rust removal, maintenance and repair cycle is long, which seriously affects the continuity of production. Summary of the invention

[0004] The purpose of the present invention is to overcome the above technical deficiencies, provide a corrosion-resistant fiber cement board carbonization reactor and a manufacturing method, and solve the technical problems of high cost and easy corrosion of metal carbonization reactors in the prior art.

[0005] In order to achieve the above technical purpose, the technical solution of the present invention provides a corrosion-resistant fiber cement board carbonization reactor:

[0006] It includes a carbonization reactor shell and a coating arranged on the inner side wall of the carbonization reactor shell;

[0007] The carbonization reactor shell is formed by casting concrete slurry; the raw materials of the concrete slurry include a first cementitious component, fine aggregate, water, a first water reducing agent and a reinforcing material in a mass ratio of (950-1100): (1100-1200): (20-30): (15-20);

[0008] The raw materials of the coating include a second gelling component, water, a second water reducing agent and an organic admixture.

[0009] Furthermore, the first cementitious component includes cement, mineral powder and silica fume in a mass ratio of (450-500):(400-450):(100-150); the fine aggregate includes one or more of quartz sand and river sand; the reinforcing material is PVA fiber; the cement strength grade is PⅡ52.5, the mineral powder grade is S105, and the silica fume particle size is 0.1-0.3μm; the water-cement mass ratio in the concrete slurry is 0.16-0.19.

[0010] Furthermore, the mass ratio of the second gelling component, water, the second water reducing agent and the organic admixture is (64-68):(26-30):(2-2.5):(3-5); the first water reducing agent and the second water reducing agent are both polycarboxylate water reducing agents; the second gelling component is calcium silicate mineral powder; and the organic admixture is styrene-butadiene emulsion.

[0011] Furthermore, the thickness of the carbonization reactor shell is 50 mm to 100 mm, and the thickness of the coating is 1 to 2 mm.

[0012] Furthermore, the carbonization reactor shell includes a bottom plate, two side walls, a reactor top and a movable door plate. The bottom plate, the side walls and the reactor top are connected to form a chamber with openings at both ends. The movable door plate is used to close the opening of the chamber.

[0013] Further, the chamber includes a rectangular kettle body at the lower side and a triangular kettle top at the upper side;

[0014] The bottom plate includes an arc-shaped ground and guiding inclined surfaces at two ends of the arc-shaped ground, and the guiding inclined surfaces are located outside the opening of the chamber;

[0015] The arc-shaped floor is a floor that is high in the middle and low on both sides, and the two lower sides are parallel to each other and connected to the bottom of the side wall; the two lower sides of the arc-shaped floor are provided with drainage channels with valves.

[0016] Furthermore, the angle between the tangent line at the lowest point of the arc-shaped ground along the arc direction and the horizontal plane is 3° to 5°; the angle between the guiding slope and the horizontal plane is 5° to 10°.

[0017] Furthermore, a plurality of vent valves are arranged on the side wall of the carbonization reactor shell, and a vent valve is arranged on the top of the reactor; a temperature control device, a humidity control device, a CO2 concentration detector and a pressure control device are arranged on the carbonization reactor shell.

[0018] The technical solution of the manufacturing method of the above-mentioned corrosion-resistant fiber cement board carbonization reactor is: comprising the following steps:

[0019] (1) uniformly mixing the first cementitious component and fine aggregate to obtain a solid phase mixture; mixing the solid phase mixture with water, a first water reducing agent and a reinforcing material to obtain a concrete slurry, and demolding after casting to obtain a carbonization reactor shell;

[0020] (2) The second gelling component, water, the second water reducing agent and the organic admixture are mixed uniformly to obtain a coating slurry; the coating slurry is sprayed on the inner surface of the carbonization reactor shell, and the carbonization reactor shell is cured to obtain a corrosion-resistant fiber cement board carbonization reactor.

[0021] Furthermore, the curing conditions are: temperature 35-42°C, CO2 volume concentration above 90%; and curing time above 3 days.

[0022] Compared with the prior art, the beneficial effects of the present invention include:

[0023] The present invention casts the carbonization reactor shell with concrete slurry, and then attaches a coating to the inner surface of the carbonization reactor shell, together forming a rust-resistant fiber cement board carbonization reactor with high strength, and effectively avoiding the rust of traditional metal carbonization reactors in high humidity and heat environments; at the same time, the subsequent fiber cement board carbonization curing process can not only make the coating more dense, but also carbonize the concrete surface after multiple and long-term carbonization to make it denser, and its airtightness is sufficient to meet the normal pressure carbonization process of the carbon mineralized fiber cement board, and effectively increase the strength, durability and service life of the carbonization reactor. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a structural schematic diagram of the carbonization reactor of the present invention;

[0025] Figure 2 for Figure 1 The front view of the carbonization reactor;

[0026] Figure 3 for Figure 1 A top view of the carbonization reactor in FIG.

[0027] Figure 4 for Figure 1 Schematic diagram of the structure of the bottom plate of the carbonization reactor. DETAILED DESCRIPTION

[0028] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0029] The present invention provides a corrosion-resistant fiber cement board carbonization reactor and a manufacturing method thereof to solve the problem that a traditional metal carbonization reactor is prone to corrosion. The manufacturing method of the present invention comprises the following steps:

[0030] (1) The first cementitious component and fine aggregate are mixed uniformly to obtain a solid phase mixture; the first cementitious component includes cement, mineral powder and silica fume; the fine aggregate includes one or more of quartz sand and river sand; the solid phase mixture is mixed with water and a first water reducing agent to obtain a concrete slurry, and then an organic fiber reinforcement material is added, and the ultra-high performance concrete slurry is obtained by uniformly stirring, and the slurry is cast, demolded, and cured to obtain a corrosion-resistant fiber cement board carbonization reactor shell.

[0031] (2) The second gelling component, water, the second water reducing agent and the organic admixture are mixed uniformly to obtain a coating slurry; the coating slurry is sprayed on the inner surface of the shell of the corrosion-resistant fiber cement board carbonization reactor, and the corrosion-resistant fiber cement board carbonization reactor is obtained after curing.

[0032] Preferably, the reinforcing material is organic synthetic PVA fiber; the mass ratio of the ultra-high performance concrete raw materials is cement: mineral powder: silica fume: fine aggregate: water reducer: reinforcing material = (450-500): (400-450): (100-150): (1100-1200): (20-30): (15-20), the water-cement mass ratio is 0.16-0.19, and the fiber volume fraction is 1%-2%; the cement strength grade is PⅡ52.5, the grade of the mineral powder is S105, the silica fume particle size is 0.1-0.3μm, the PVA fiber length is 9mm, and the first water reducer is a polycarboxylate water reducer.

[0033] The mass ratio of the coating slurry is the second gelling component: water: the second water reducing agent: the organic admixture = (64-68): (26-30): (2-2.5): (3-5), the second water reducing agent is a polycarboxylic acid water reducing agent, the organic admixture is a styrene-butadiene emulsion, and the preferred solid content is 40% to 50%.

[0034] Preferably, the second gelling component is calcium silicate mineral powder.

[0035] In the present invention, the calcium silicate ore powder preferably includes one or more of γ-type dicalcium silicate (γ-C2S), tricalcium disilicate (C3S2) and monocalcium silicate (CS).

[0036] In the present invention, the average particle size of the calcium silicate ore powder is preferably less than 20 μm.

[0037] The present invention has no special limitation on the mixing, stirring, casting and demoulding of ultra-high performance concrete, and the processes well known in the art can be followed. The present invention has no special limitation on the coating mixing process, and the slurry can be mixed evenly according to the processes well known in the art. In an embodiment of the present invention, the slurry is stirred in a stirring device, and the stirring time is preferably 5 to 15 minutes to mix the slurry evenly. The present invention has no special limitation on the stirring rate, and the slurry can be mixed evenly according to the processes well known in the art.

[0038] In the present invention, the caliber of the spray gun used for spraying is preferably 1 to 3 mm, more preferably 2 mm, and the spraying distance is preferably 20 to 30 cm, more preferably 25 cm.

[0039] In the present invention, the coating is sprayed before the carbonization reactor is used and cured together with the fiber cement board; if cured separately, it only takes one day at room temperature because the coating is relatively thin. The present invention provides a corrosion-resistant fiber cement board carbonization reactor prepared by the above manufacturing method.

[0040] See also Figure 1 The carbonization reactor shell of the present invention comprises a bottom plate 1, two side walls 2 and a reactor top 3. The bottom plate 1, the side walls 2 and the reactor top 3 are connected to form a chamber with openings at both ends, that is, the two ends of the carbonization reactor shell are connected in the transverse direction, which is convenient for feeding and discharging. For the convenience of description, the direction from feeding to discharging is defined as the transverse direction, but it is not a limitation of the present invention.

[0041] It is understandable that, in the actual process of curing the cement board, in order to improve the curing effect, the two ends of the chamber can be sealed by setting a movable door plate; the movable door plate is more flexible to use, so there is no restriction on its material.

[0042] Preferably, the thickness of the carbonization reactor shell is 50 mm to 100 mm, and the thickness of the coating is 1 to 2 mm, more preferably 1.5 mm.

[0043] Preferably, the top 3 of the carbonization reactor shell is a triangular top, and the lower side wall 2 forms a rectangular reactor body; the angle of the triangular top is 90° to 120°.

[0044] Preferably, see Figure 2 and Figure 3 The side walls 2 of the carbonization reactor shell are provided with ventilation valves 4 at the top and bottom, and the top 3 of the reactor is provided with an air release valve 5.

[0045] More preferably, two vent valves 4 are provided and one deflation valve 5 is provided.

[0046] Preferably, a temperature sensor, a hygrometer, a CO2 concentration detector and a pressure gauge are provided on the inner wall of the carbonization reactor shell; the temperature sensor, the hygrometer, the CO2 concentration detector and the pressure gauge are electrically connected to a controller, the controller is connected to a display, the display is used to display the real-time temperature, humidity, CO2 concentration and pressure in the reactor, and the temperature, humidity, CO2 concentration and pressure in the reactor are adjusted by controlling the closing and opening of the ventilation valve 4 and the air release valve 5.

[0047] It is understandable that the temperature and humidity in the kettle as well as the CO2 concentration and pressure can be adjusted by manually controlling the closing and opening of the ventilation valve 4 and the air release valve 5; or the controller and the relay can be connected, and the relays are independently connected to the ventilation valve 4 and the air release valve 5 to realize intelligent control.

[0048] Preferably, see Figure 4 In the transverse direction, the bottom plate 1 of the carbonization reactor shell includes guiding slopes 101 at both ends and an arc-shaped ground 102 in the middle. The arc-shaped ground 102 is a ground with a high middle and low sides in the longitudinal direction, and the angle between the tangent line of the lowest point on both sides along the arc direction and the horizontal plane is 3° to 5°. The angle between the guiding slope 101 and the horizontal plane is 5° to 10°, which is convenient for feeding and discharging.

[0049] Preferably, drainage channels 103 with valves are provided on both sides of the arc-shaped floor 102 of the carbonization reactor shell in the longitudinal direction.

[0050] The fiber cement board carbonization reactor of the present invention uses ultra-high performance concrete as the reactor body, and the inner surface of the reactor body is coated, which together constitute a rust-resistant fiber cement board carbonization reactor. The reactor uses ultra-high performance concrete as the matrix and organic synthetic PVA fiber instead of steel fiber as the reinforcing material, which avoids the rust of traditional metal carbonization reactors in high humidity and heat environment. Adding mineral powder and silica fume to the concrete mix design can improve the fluidity of concrete, reduce the heat of cement hydration, increase the later strength, improve the internal structure of concrete, and improve the impermeability and corrosion resistance. The particle size of silica fume is small, which can fill the pores between cement particles, making the cement mortar and the hardened product more compact.

[0051] The inner surface of the carbonization reactor of the fiber cement board of the present invention is coated, which can improve the anti-seepage performance and density of the ultra-high performance concrete, and can improve the durability and service life of the carbonization reactor; the inorganic coating uses raw materials rich in calcium silicate mineral phase as a gelling component and styrene-butadiene emulsion as an adhesive. Firstly, the inorganic coating has good bonding performance with the ultra-high performance concrete reactor body, and the calcium silicate mineral phase has good carbonization activity, which can promote the carbonization reaction in the carbon dioxide curing atmosphere, making the surface denser, which can improve the bonding performance and anti-seepage ability with concrete, and enhance the durability of concrete; secondly, the styrene-butadiene emulsion has good heat resistance and is not easy to decompose in the carbonization exothermic environment.

[0052] In addition, the carbonization process can not only make the coating denser, but also carbonize the surface of ultra-high performance concrete after multiple and long-term carbonization, making it denser. Its airtightness is sufficient to meet the normal pressure carbonization process of carbon mineralized fiber cement board, and can improve its strength and durability.

[0053] The upper part of the reactor shell of the present invention is a triangular reactor top, and the lower part is a rectangular reactor body. The triangular reactor top allows the water generated during the carbonization process to slide freely along the wall to the ground without dripping on the fiber cement board to affect the uniformity of carbonization. Two ventilation valves are arranged on the upper and lower side walls of the reactor shell, and a vent valve is arranged on the top of the reactor. The internal air can be discharged by opening the lower carbon dioxide ventilation valve and the top vent valve; the ventilation valve can select the number of ventilations according to specific requirements. During the carbonization process, opening the two ventilation valves at the same time can ensure that the carbon dioxide concentration above and below the carbonization reactor is uniform, so that the fiber cement board is uniformly carbonized; the vent valve can be used for ventilation and collection of hot exhaust gas, and ventilation and venting can be used to discharge the air in the reactor simultaneously.

[0054] A temperature sensor is installed on the wall of the reactor shell to monitor the temperature changes inside the reactor in real time, and the internal temperature is controlled within the optimal temperature range of the carbonization reaction through ventilation. A CO2 concentration detector and a pressure gauge are installed on the wall of the reactor shell to monitor the stability of the CO2 atmosphere inside the reactor and control the CO2 concentration and pressure inside the reactor in real time.

[0055] The floor of the reactor shell is an arc-shaped floor with a high middle and low sides in the longitudinal direction, and guiding slopes connected to the arc-shaped floor at both ends in the transverse direction; drainage channels with valves are arranged on both longitudinal sides of the arc-shaped floor, and the arc-shaped design of the floor is conducive to the ground surface water generated during the carbonization process to flow to the drainage channels on both sides; the guiding slope is conducive to the fiber cement board entering the carbonization reactor, and the drainage channel valve ensures that the reactor has good airtightness; a hygrometer is arranged on the side wall of the reactor shell to monitor the humidity changes inside the reactor. The humidity is related to the valve of the drainage channel. When the humidity reaches a certain range and remains for more than 30 minutes, the valve is opened to discharge the accumulated water once.

[0056] In the present invention, unless otherwise specified, the raw materials used are all commercially available products in the art.

[0057] In order to further illustrate the ultra-high performance concrete shell material of the present invention, the material of the present invention is described in detail below in combination with embodiments and comparative examples, but they should not be construed as limiting the scope of protection of the present invention.

[0058] Example 1

[0059] According to the mass ratio of cement: mineral powder: silica fume: quartz sand: water reducer: fiber = 500:400:125:1150:25:20, the water-binder mass ratio is 0.18, and 6 groups of test pieces are cast and formed, numbered S1-1, S1-2, S1-3, S1-4, S1-5, S1-6, with 3 test pieces in each group. After 1 day of casting, demoulding is carried out, and 1 to 3 are placed under standard curing conditions for 3 days, 7 days and 28 days, with a curing temperature of 20℃±2℃ and a relative humidity of more than 95%; 4 to 6 are placed under carbonization curing conditions for 3 days, 7 days and 28 days, with a curing temperature of 40℃, a relative humidity of 50%, an air pressure of 0.1MPa, and a CO2 volume concentration of 99%, to obtain the carbonization reactor shell.

[0060] Comparative Example 1

[0061] According to the mass ratio of cement: quartz sand: water reducing agent: fiber = 1000: 1100: 25: 20, the water-binder mass ratio is 0.18, and 6 groups of test pieces are cast and formed, numbered D1-1, D1-2, D1-3, D1-4, D1-5, D1-6, with 3 test pieces in each group. The preparation method and curing process are the same as in Example 1.

[0062] Comparative Example 2

[0063] According to the mass ratio of cement: mineral powder: silica fume: quartz sand: water reducing agent: fiber = 750:200:75:1150:25:20, the water-binder mass ratio is 0.18, and 6 groups of test pieces are cast and formed, numbered D2-1, D2-2, D2-3, D2-4, D2-5, D2-6, with 3 test pieces in each group. The preparation method and curing process are the same as in Example 1.

[0064] Comparative Example 3

[0065] According to the mass ratio of cement: mineral powder: silica fume: quartz sand: water reducing agent: fiber = 225:600:200:1000:25:20, the water-binder mass ratio is 0.18, and 6 groups of test pieces are cast and formed, numbered D3-1, D3-2, D3-3, D3-4, D3-5, D3-6, with 3 test pieces in each group. The preparation method and curing process are the same as in Example 1.

[0066] The raw material mass ratios of the embodiments of the present invention and the comparative examples are shown in Table 1 below.

[0067] Table 1 Raw material mass ratio of the embodiments of the present invention and the comparative examples

[0068]

[0069]

[0070] The test was carried out in accordance with the relevant provisions of GB / T 50081-2019 "Standard for Test Methods for Physical and Mechanical Properties of Concrete", and each group of specimens was tested. The average value was taken as the test result of each group. The specific test results are shown in Table 2 below.

[0071] Table 2 Compressive strength of carbonization reactor shell under different curing conditions

[0072]

[0073] It can be seen from Example 1 and Comparative Examples 1 to 3 that, within a given formula range, the mechanical properties of ultra-high performance concrete during carbonation curing are higher than those during standard curing, and the addition of mineral powder and silica fume has higher later strength than when only cement is added as a cementitious material. If too much or too little mineral powder and silica fume are added, the strength is lower than that within the formula range; this shows that the present invention can produce a synergistic effect by casting and molding ultra-high performance concrete within a specific formula range in combination with carbonation curing conditions.

[0074] In order to further illustrate the inorganic coating material of the present invention, the material of the present invention is described in detail below in combination with examples and comparative examples, but they should not be construed as limiting the protection scope of the present invention.

[0075] Example 2

[0076] The coating slurry was prepared by mixing the gelling component: water: water reducing agent: organic admixture in a mass ratio of 66:28:2:4, and the coating slurry was sprayed on one side of the ultra-high performance concrete test block obtained in Example 1, and the coated concrete test block was placed in a CO2 atmosphere with a volume concentration of 99% and a pressure of 0.1 MPa for curing at room temperature for 1 day. There were 2 groups, numbered S2-1 and S2-2, with 3 specimens in each group. The first group was used to measure the bonding strength, and the second group was used to measure the ion permeability.

[0077] Example 3

[0078] The coating slurry was prepared by mixing the cementing component: water: water reducing agent: organic admixture in a mass ratio of 66:28:2:3, and the coating slurry was sprayed on one side of the ultra-high performance concrete test block obtained in Example 1, with a total of 2 groups, numbered S3-1 and S3-2, with 3 test pieces in each group. The preparation method and curing process were the same as in Example 2.

[0079] Example 4

[0080] The coating slurry was prepared by mixing the cementing component: water: water reducing agent: organic admixture in a mass ratio of 64:30:2:4, and the coating slurry was sprayed on one side of the ultra-high performance concrete test block obtained in Example 1, with a total of 2 groups, numbered S4-1 and S4-2, with 3 test pieces in each group. The preparation method and curing process were the same as in Example 2.

[0081] Comparative Example 4

[0082] The ultra-high performance concrete test blocks obtained in Example 1 were taken without spraying, and a total of 1 group, numbered D4, with 3 test pieces in each group. The preparation method and curing process were the same as in Example 2.

[0083] The test was carried out in accordance with the relevant provisions of JGJ 110-2017 "Test Standard for Bond Strength of Facing Tiles in Construction Engineering" and JCT 1086-2008 "Test Method for Chloride Ion Diffusion Coefficient of Cement". The test results are shown in Table 3 below.

[0084] Table 3 Coating bonding strength and chloride ion diffusion coefficient of carbonization reactor shell

[0085] serial number Bond strength / MPa <![CDATA[Chloride ion diffusion coefficient / m 2 ·s -1 > S2 4.03 <![CDATA[4.8×10 -13 <!-- 6 -->]]> S3 2.44 <![CDATA[7.4×10 -13 ]]> S4 1.85 <![CDATA[9.2×10 -13 ]]> D4 - <![CDATA[4.5×10 -12 ]]>

[0086] It can be seen from Examples 2-4 and Comparative Example 4 that, within a given formula range, the chloride ion diffusion coefficient of Examples 2-4 is one order of magnitude lower than that of Comparative Example 4, and the bonding strength is between 1.85 and 4.03 MPa, indicating that the inorganic coating has good bonding with the concrete. Spraying the inorganic coating on the surface of ultra-high performance concrete can improve the concrete's impermeability and durability.

[0087] Moreover, the bonding strength of the coating in Example 2 is higher than that in Examples 3-4, and the chloride ion diffusion coefficient is lower than that in Examples 3-4, indicating that there is a coordination effect between the coating ratios, especially the amount of cementitious material, water and organic admixture has a great influence on the performance of the obtained coating.

[0088] Compared with the prior art, the present invention provides a corrosion-resistant fiber cement board carbonization reactor and a manufacturing method; the fiber cement board carbonization reactor of the present invention is a reactor shell that is formed by casting ultra-high performance concrete and is connected in the transverse direction, and the inner surface of the reactor shell is attached with an inorganic coating to form a carbonization reactor; the upper part of the reactor is a triangular reactor top, the lower part is a rectangular reactor body, two ventilation valves are arranged on the upper and lower side walls, and a vent valve is arranged on the reactor top. The reactor body is provided with a temperature sensor, a hygrometer, a CO2 concentration detector and a pressure gauge, and the ground is an arc-shaped ground with a high middle and low sides in the longitudinal direction, and the two ends in the transverse direction are inclined surfaces connected to the arc-shaped ground, and drainage channels with valves are arranged on both sides of the longitudinal direction. Traditional metal carbonization reactors are very easy to rust in the high humidity and heat environment of carbonization, thereby affecting the life of the reactor and the performance of the carbonized product. The fiber cement board carbonization reactor provided by the present invention can avoid the rust problem, the wall and ground design is conducive to the discharge of moisture, and the carbonization process also makes the inner surface of the reactor more compact, thereby improving the strength and durability of the carbonization reactor.

[0089] The specific implementation of the present invention described above does not constitute a limitation on the protection scope of the present invention. Any other corresponding changes and modifications made based on the technical concept of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. A corrosion-resistant fiber cement board carbonization reactor, characterized in that: It includes a carbonization reactor shell and a coating arranged on the inner side wall of the carbonization reactor shell; The carbonization reactor shell is formed by casting concrete slurry; the raw materials of the concrete slurry include a first cementitious component, fine aggregate, a first water reducer and a reinforcing material in a mass ratio of (950-1100): (1100-1200): (20-30): (15-20); the first cementitious component includes cement, mineral powder and silica fume in a mass ratio of (450-500): (400-450): (100-150); the reinforcing material is PVA fiber; the water-cement mass ratio in the concrete slurry is 0.16-0.19; The raw materials of the coating include a second gelling component, water, a second water reducing agent and an organic admixture in a mass ratio of (64-68):(26-30):(2-2.5):(3-5), wherein the second gelling component is calcium silicate mineral powder and the organic admixture is styrene-butadiene emulsion.

2. The corrosion-resistant fiber cement board carbonization reactor according to claim 1, characterized in that: The fine aggregate includes one or more of quartz sand and river sand; the cement strength grade is PⅡ52.5, the grade of mineral powder is S105, and the particle size of silica fume is 0.1-0.3 μm.

3. The corrosion-resistant fiber cement board carbonization reactor according to claim 1, characterized in that: The first water reducer and the second water reducer are both polycarboxylate water reducers.

4. The corrosion-resistant fiber cement board carbonization reactor according to claim 1, characterized in that: The thickness of the carbonization reactor shell is 50 mm to 100 mm, and the thickness of the coating is 1 to 2 mm.

5. The corrosion-resistant fiber cement board carbonization reactor according to claim 1, characterized in that: The carbonization reactor shell comprises a bottom plate, two side walls, a reactor top and a movable door plate. The bottom plate, the side walls and the reactor top are connected to form a chamber with openings at both ends. The movable door plate is used to close the opening of the chamber.

6. The corrosion-resistant fiber cement board carbonization reactor according to claim 5, characterized in that: The chamber comprises a rectangular kettle body at the lower side and a triangular kettle top at the upper side; The bottom plate includes an arc-shaped ground surface and guiding inclined surfaces located at two ends of the arc-shaped ground surface, and the guiding inclined surfaces are located outside the opening of the chamber; The arc-shaped floor is a floor that is high in the middle and low on both sides, and the two lower sides are parallel to each other and connected to the bottom of the side wall; the two lower sides of the arc-shaped floor are provided with drainage channels with valves.

7. The corrosion-resistant fiber cement board carbonization reactor according to claim 6, characterized in that: The angle between the tangent line at the lowest point of the arc-shaped ground and the horizontal plane along the arc direction is 3°~5°; the angle between the guiding slope and the horizontal plane is 5°~10°.

8. The corrosion-resistant fiber cement board carbonization reactor according to claim 5, characterized in that: A plurality of vent valves are arranged on the side wall of the carbonization reactor shell, and a vent valve is arranged on the top of the reactor; a temperature control device, a humidity control device, a CO2 concentration detector and a pressure control device are arranged on the carbonization reactor shell.

9. The method for manufacturing a corrosion-resistant fiber cement board carbonization reactor according to any one of claims 1 to 8, characterized in that: The following steps are involved: (1) uniformly mixing the first cementitious component and fine aggregate to obtain a solid phase mixture; mixing the solid phase mixture with water, a first water reducing agent and a reinforcing material to obtain a concrete slurry, and demolding after casting to obtain a carbonization reactor shell; (2) uniformly mixing the second gelling component, water, the second water reducing agent and the organic admixture to obtain a coating slurry; The coating slurry is sprayed on the inner surface of the carbonization reactor shell, and then cured to obtain a corrosion-resistant fiber cement board carbonization reactor.