A method for recovering styrene from byproducts of propylene oxide produced by co-oxidation
Through distillation and alkali washing, impurities are removed, combined with the coordinated catalysis of solid acid catalysts and organic hydrochloride additives, the low economic benefits and equipment corrosion problems caused by impurities such as phenylethanol in co-oxidation method are solved, and efficient styrene recovery is achieved and product purity improvement.
Patent Information
- Application Number
- CN202310000489.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-01-03
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-01-03
AI Technical Summary
In the process of producing propylene oxide by co-oxidation, impurities such as phenylethanol contained in the by-product recombinant components lead to low economic benefits in the process, and traditional incineration treatment has low economic benefits and equipment corrosion risks.
Removal of heavy impurities by distillation, use NaOH aqueous solution to remove acidic impurities, and catalyze them in conjunction with solid acid catalyst and organic hydrochloride additives to carry out cracking and dehydration reaction to produce styrene and water, which improves conversion and selectivity and extends the catalyst life , reduce the impact of metal ions on the product.
It significantly improves the conversion rate and reaction selectivity of phenylethanol ether, extends the catalyst life, reduces the color number of the product and equipment corrosion risks, and improves the economic benefits of the process and product purity.
Abstract
Description
Technical Field
[0001] The invention relates to a method for recovering styrene from byproducts of producing propylene oxide by a co-oxidation method, and belongs to the field of styrene. Technical Background
[0002] Styrene is a chemical raw material with important application value. Its downstream derivatives are mainly synthetic resins. For example, general-grade polystyrene can be produced after modification to obtain high-impact polystyrene. It can be polymerized with butadiene to produce styrene-butadiene rubber and styrene-butadiene latex, polymerized with acrylonitrile to produce styrene-acrylonitrile copolymer resin, polymerized with butadiene and acrylonitrile to produce acrylonitrile-butadiene-styrene (ABS) resin, and polymerized with divinylbenzene to produce ion exchange resin, etc. It is widely used in coatings, medicine, pharmaceuticals, electronics, automobile industry, daily light industrial products and other industries.
[0003] The main methods for industrial production of styrene include ethylbenzene dehydrogenation, propylene oxide / styrene (PO / SM) co-oxidation, etc. Ethylbenzene dehydrogenation is the current mainstream production process of styrene, with advanced technology, mature and reliable, and high product quality. The PO / SM co-production method first oxidizes ethylbenzene into ethylbenzene hydroperoxide, and then reacts with propylene to produce propylene oxide and phenylethanol. The phenylethanol separation process successively removes heavy components and light component impurities in the system, and then the crude phenylethanol undergoes a dehydration reaction to produce styrene. The process is described in patent CN1310698A. The PO / SM co-production method has two products, relatively low investment, reduces the market risk of a single product, and has more advantages in building large-scale production equipment.
[0004] During the separation of phenylethanol in the PO / SM co-oxidation process, phenylethanol is removed from heavy oil impurities in a de-weighting tower before entering a dehydration reaction. In general processes, the heavy oil material is incinerated, which has low economic benefits.
[0005] Therefore, it is necessary to develop a process for recovering the heavy component of phenylethanol to improve the economic benefit of the device. Summary of the invention
[0006] In order to solve the above problems, the present invention provides a method for recovering styrene from the by-product of producing propylene oxide by a co-oxidation method. After the harmful heavy components and acidic impurities are removed from the waste oil in the bottom of the tower, a 1-phenylethanol solution containing an organic hydrochloride is added to the material as an auxiliary agent, which exerts a synergistic catalytic effect with the solid acid to catalyze the cracking and dehydration reaction to generate styrene and water, which can significantly improve the conversion rate and selectivity of the reaction, effectively prolong the life of the solid catalyst, and significantly reduce the influence of metal ions on the color of the product.
[0007] In order to achieve the above invention object, the technical solution of the present invention is as follows:
[0008] The present invention provides a method for recovering styrene from the byproduct of producing propylene oxide by co-oxidation, the steps comprising:
[0009] 1) using a by-product heavy component from the co-oxidation process to produce propylene oxide as a raw material, wherein the by-product heavy component comprises phenylethyl alcohol ether, removing the heavy component from the by-product heavy component by distillation, and collecting a light component comprising phenylethyl alcohol ether;
[0010] 2) mixing the light component of step 1) with a NaOH aqueous solution, removing acidic impurities by alkali washing, then standing for phase separation, and collecting the upper oil phase material;
[0011] 3) mixing the oil phase material of step 2) with a solid acid catalyst and an organic hydrochloride auxiliary agent to cause the phenylethyl alcohol ether therein to undergo a cracking and dehydration reaction to generate styrene and water;
[0012] 4) The reaction system of step 3) is subjected to oil-water separation and distillation to obtain styrene.
[0013] In the present invention, the by-product heavy components from the co-oxidation process for producing propylene oxide in step 1) include, by weight percentage, 40-60% of phenylethyl alcohol ether, preferably 40-50%, 1-3% of benzoic acid, 0-1% of acetophenone, 0-1% of phenylethyl alcohol, 1-2% of benzaldehyde and phenylacetic acid, and the rest are heavy component impurities (such as phenylethyl alcohol polymers, polymers produced in the upstream reaction and separation process, and other heavy components), and trace amounts of metal ions such as Fe, Cr, Ni ions, etc.; wherein, the effective component phenylethyl alcohol ether is generated by dehydration polymerization of two molecules of phenylethyl alcohol under high temperature conditions during the separation process of phenylethyl alcohol, and is also called phenylethyl alcohol dimer.
[0014] The by-product heavy components from the co-oxidation process for producing propylene oxide described in the present invention mainly come from the heavy oil in the bottom of the phenylethanol de-heavy tower, including phenylethanol ether, benzoic acid, acetophenone, phenylethanol, benzaldehyde, phenylacetic acid and phenylethanol polymers. This process is a prior art, and the present invention does not make specific requirements for its preparation method. As long as the by-product containing phenylethanol ether obtained by the process is applicable to the method of the present invention.
[0015] In the present invention, the distillation in step 1) has a pressure of 1-10 kPaA, preferably 1-5 kPaA; a temperature of 150-200°C, preferably 170-190°C; and a time of 10-60 min, preferably 20-30 min. The by-product heavy components can be distilled to remove heavy component impurities including phenylethanol polymers. The polymers will undergo competitive dehydration during the cracking and dehydration process of phenylethanol ether to generate other high molecular substances. Removing the heavy components before the reaction helps to improve the dehydration reaction effect and catalyst life.
[0016] In the present invention, the mass ratio of the light component of step 1) and the NaOH aqueous solution mixed in step 2) is 0.5-4:1, preferably 1-3:1;
[0017] The pH value of the NaOH aqueous solution is 12-14, preferably 13-13.5.
[0018] In the present invention, the alkali washing temperature in step 2) is 30-60°C, preferably 45-55°C; the time is 30-70min, preferably 30-50min. The alkali washing process can remove acidic impurities such as benzoic acid, benzaldehyde, and phenylacetic acid in the material, and their content can be reduced to ≤500ppm, so as to reduce the influence of the above impurities on the color number and purity of the styrene product.
[0019] In the present invention, the solid acid catalyst in step 3) is selected from one or more of a strongly acidic cation exchange resin or a supported solid acid catalyst, preferably a supported solid acid catalyst;
[0020] The strong acid cation exchange resin is selected from LX-67 acidic ion exchange resin of Lanxiao Technology or No. 732 strong acid cation exchange resin of Jinda Zhengtong.
[0021] The supported solid acid catalyst, the carrier is selected from one or more of activated carbon and SiO2, the supported acid is selected from one or more of benzenesulfonic acid and p-toluenesulfonic acid, preferably p-toluenesulfonic acid / SiO2 solid acid catalyst; preferably, the supported solid acid catalyst has an acid content of 20-40wt%, preferably 25-35wt%.
[0022] The supported solid acid catalyst selected in the present invention has multiple advantages over traditional liquid phase strong acid catalysts, such as sulfuric acid, p-toluenesulfonic acid, etc., which have the advantages of being not easy to corrode and being renewable. The solid acid catalyst described in the present invention has no special requirements on its source and can be purchased or homemade. For example, the strong acid cation exchange resin can be a commercially available product, and the supported solid acid catalyst can be homemade by conventional supported catalyst preparation methods such as impregnation method, etc., which are not specifically limited in the present invention.
[0023] In the present invention, the amount of the solid acid catalyst in step 3) is 2-6 wt %, preferably 2.5-4.5 wt %, of the mass of the oil phase material in step 2).
[0024] In the present invention, the organic hydrochloride auxiliary agent in step 3) is a 1-phenylethanol solution of organic hydrochloride, with a concentration of 1-10wt%, preferably 5-8wt%;
[0025] The organic hydrochloride is selected from one or more of triethylammonium hydrochloride and trimethylammonium hydrochloride;
[0026] The amount of the organic hydrochloride auxiliary agent, calculated as the organic hydrochloride therein, is 500-1000ppm, preferably 600-800ppm, of the oil phase material in step 2). During the distillation operation of step 1), most of the metal ions such as iron in the by-product heavy component raw material are also discharged from the system at the bottom of the tank with the heavy component, but a small amount of metal ions with a content of about 500ppm are still entrained in the evaporation gas phase and enter the alkali washing system with the light component. Under the high temperature reaction conditions, the organic hydrochloride auxiliary agent can react with metal ions such as Fe 2+ Cr 3+ 、Ni 2+ The acidic ionic liquid [Et3NH]Cl / MX (taking triethylammonium hydrochloride as an example) is generated by complexation. The ionic liquid has the characteristics of large density and uniform distribution of acid sites, high acid strength and good thermal stability. The L acid sites carried by the ionic liquid cooperate with the B acid sites of the solid acid catalyst to effectively improve the conversion rate and selectivity of the cracking reaction.
[0027] In the present invention, the cracking and dehydration reaction in step 3) is carried out at a temperature of 80-150°C, preferably 100-120°C; the residence time of the reaction liquid is 10-40min, preferably 20-30min. Phenylethyl alcohol ether undergoes cracking and dehydration reaction under the synergistic action of the catalyst and the auxiliary agent to generate styrene and water; the method of the present invention can maintain the reaction conversion rate of phenylethyl alcohol ether at 95-99%, and the reaction selectivity is 90-94%. Compared with the dehydration reaction of phenylethyl alcohol, the cracking and dehydration reaction of phenylethyl alcohol ether has lower requirements on the reaction temperature and the concentration of the acid catalyst, so there is no need to select liquid catalysts such as organic acids such as liquid benzenesulfonic acid or inorganic strong acids. The above-mentioned solid acid catalyst and the organic hydrochloride auxiliary agent synergistically catalyze, which not only has a good catalytic effect on the cracking and dehydration process of phenylethyl alcohol ether, but also greatly reduces the risk of equipment corrosion. In addition, the catalyst can be recovered and reused after regeneration, so that the investment of the recovery system is reduced.
[0028] In the present invention, the oil-water separation in step 3) is a conventional operation in the art, for example, a static stratification method can be used, the separation temperature is 5-20°C, preferably 10-20°C; the time is 0.5-2h, preferably 0.5-1h.
[0029] In the present invention, the distillation in step 3) is carried out in a distillation tower at a pressure of 1-10 kPaA, preferably 4-8 kPaA; the tower bottom temperature is 100-140° C., preferably 120-130° C.; the reflux ratio is 1-6; preferably 2-3; the heavy components in the cracking and dehydration products, such as phenylethanol, acetophenone, ionic liquid, etc., are further removed by the distillation operation, and the styrene product can be obtained from the top of the tower.
[0030] The styrene product obtained by the method of the invention has a purity of more than 99.95% and a color number lower than 10.
[0031] The technical solution of the present invention has the following advantages:
[0032] 1. The heavy oil in the benzene ethanol separation process is cracked to recover styrene, which is the resource utilization of waste oil in the production unit, which can effectively increase the styrene output of the unit, reduce material losses and improve economic benefits.
[0033] 2. The method of the present invention removes harmful impurities such as heavy components of phenylethanol polymer, benzoic acid, benzaldehyde, etc. during the pretreatment process, effectively improving the reaction effect of phenylethanol ether and extending the life of the catalyst; in addition, the removal of impurities such as benzaldehyde can reduce the color number of the styrene product and ensure that the indicators are qualified.
[0034] 3. The method of the present invention introduces an organic hydrochloride auxiliary agent in the reaction process, which can generate an ionic liquid with metal ions. The ionic liquid has the characteristics of large acid site density, uniform distribution, high acid strength, good thermal stability, etc., and synergistic catalysis with the solid acid catalyst, significantly improving the conversion rate and selectivity of the dehydration reaction, effectively extending the life of the solid catalyst, and significantly reducing the influence of metal ions on the product color.
[0035] 4. The dehydration reaction of the present invention uses a solid acid catalyst which is regenerable, has a low corrosion risk, a long catalyst life, has no strict requirements on the reactor material, and reduces the equipment investment of the recovery system. DETAILED DESCRIPTION
[0036] In order to make the technical solution and advantages of the present invention clearer, the present invention is further described in detail by examples below. The specific embodiments described here are only used to explain the present invention and are not used to limit the present invention.
[0037] The gas phase analysis conditions adopted in the embodiment of the present invention are: Agilent 7890B, chromatographic column HP-5ms, vaporization chamber temperature of 280°C, detector temperature of 280°C; programmed temperature rise: 50°C for 3 min; 40°C / min to 100°C for 4 min; heating to 200°C at 10°C / min, holding for 4 min; heating to 280°C at 40°C / min, holding for 5 min.
[0038] In the various embodiments and comparative examples of the present invention, the sources of the main raw materials are as follows. Unless otherwise specified, other raw materials and reagents are purchased through common commercial channels:
[0039] By-product heavy components: by-product heavy components from the PO / SM unit of Wanhua Chemical Group Co., Ltd., produced by the co-oxidation process to produce propylene oxide, namely, the bottom heavy oil produced in the oxidation reaction separation and phenylethanol refining process.
[0040] Triethylamine hydrochloride was purchased from Jinan Better New Materials Co., Ltd., CAS No. 554-68-7;
[0041] The supported solid acid catalyst is prepared by referring to the method disclosed in the document "Preparation of supported p-toluenesulfonic acid catalyst and study on its catalytic double esterification reaction [J]". Specifically, taking p-toluenesulfonic acid / SiO2 supported catalyst (acid loading 30wt%) as an example, the preparation method is as follows: first, SiO2 is dried at 120°C for 5h, and after cooling, 50wt% p-toluenesulfonic acid solution is added and immersed for 50h, then the p-toluenesulfonic acid solution is discharged, and the catalyst particles are dried for a second time at 120°C for 5h to obtain a solid acid catalyst with a p-toluenesulfonic acid loading of 30%.
[0042] Example 1
[0043] The by-product heavy component raw materials of the co-oxidation process for producing propylene oxide include: 49.7% phenylethyl ether, 1.6% benzoic acid, 0.2% acetophenone, 0.8% phenylethyl alcohol, 1.1% benzaldehyde and phenylacetic acid, and the rest are 46.6% heavy components produced by the upstream reaction separation process such as phenylethyl alcohol polymer, including trace amounts of metal ions such as Fe, Cr, Ni ions, etc.
[0044] The method for cracking and recovering styrene comprises the following steps:
[0045] 1) The above by-product heavy components are removed by distillation, the distillation pressure is 3 kPaA, the temperature is 180° C., and the time is 25 min, and the light components containing phenylethyl ether are collected.
[0046] 2) 810 kg of the light component from step 1) was mixed with 400 kg of a NaOH aqueous solution having a pH value of 13, and the acidic impurities were removed by alkali washing at a temperature of 50° C. for 40 min. The mixture was then allowed to stand for phase separation, and the upper oil phase material was collected, wherein the content of acidic impurities such as benzoic acid, benzaldehyde, and phenylacetic acid was reduced to 300 ppm, and the content of metal ions was 480 ppm.
[0047] 3) 805 kg of the oil phase material of step 2) was mixed with 25 kg of p-toluenesulfonic acid / SiO2 supported catalyst (acid loading 30 wt%) and 800 ppm of 5 wt% triethylamine hydrochloride 1-phenylethanol solution (calculated as triethylamine hydrochloride), and phenylethyl alcohol ether was subjected to cracking and dehydration reaction at a reaction temperature of 115° C. and a reaction residence time of 25 min to generate styrene and water.
[0048] 4) The reaction system of step 3) is subjected to static stratification to achieve oil-water separation at a separation temperature of 15° C. and a time of 0.8 h, and then transferred to a distillation tower for distillation at a distillation pressure of 6 kPaA, a bottom temperature of 120° C., and a reflux ratio of 3 to obtain styrene.
[0049] In this embodiment, the conversion rate of phenylethyl alcohol ether is 98.5%, the selectivity of styrene is 92.8%, the purity of styrene product is 99.97%; and the platinum cobalt color number is 8.7.
[0050] Example 2
[0051] The by-product heavy component raw materials of the co-oxidation process for producing propylene oxide include: 41.3% phenylethyl ether, 2.2% benzoic acid, 0.3% acetophenone, 0.9% phenylethyl alcohol, 1.5% benzaldehyde and phenylacetic acid, and the rest 53.8% heavy components by-products of the upstream reaction and separation process such as phenylethyl alcohol polymer, including trace amounts of metal ions such as Fe, Cr, Ni ions, etc.
[0052] The method for cracking and recovering styrene comprises the following steps:
[0053] 1) The above by-product heavy components are removed by distillation, the distillation pressure is 2 kPaA, the temperature is 150° C., and the time is 20 min, and the light components containing phenylethyl ether are collected.
[0054] 2) 730 kg of the light component from step 1) was mixed with 380 kg of a NaOH aqueous solution having a pH value of 13.5, and the acidic impurities were removed by alkali washing at a temperature of 55° C. for 50 min. The mixture was then allowed to stand for phase separation, and the upper oil phase material was collected, wherein the content of acidic impurities such as benzoic acid, benzaldehyde, and phenylacetic acid was reduced to 240 ppm, and the content of metal ions was 400 ppm.
[0055] 3) 725 kg of the oil phase material of step 2) was mixed with 30 kg of LX-67 acidic ion exchange resin of Lanxiao Technology and 750 ppm of 8 wt% 1-phenylethanol solution of triethylammonium sulfate (calculated as triethylammonium hydrochloride), and phenylethyl alcohol ether was subjected to cracking and dehydration reaction at a reaction temperature of 120° C. and a reaction residence time of 30 min to generate styrene and water.
[0056] 4) The reaction system of step 3) is subjected to static stratification to achieve oil-water separation at a separation temperature of 15° C. for 1 h, and then transferred to a distillation tower for distillation at a distillation pressure of 4 kPaA, a bottom temperature of 120° C., and a reflux ratio of 3 to obtain styrene.
[0057] In this embodiment, the conversion rate of phenylethyl alcohol ether is 98.9%, the selectivity of styrene is 91.2%, the purity of styrene product is 99.95%; and the platinum cobalt color number is 9.5.
[0058] Example 3
[0059] The by-product heavy component raw materials of the co-oxidation process for producing propylene oxide include: 44.9% phenylethyl ether, 1.2% benzoic acid, 0.4% acetophenone, 0.6% phenylethyl alcohol, 1.8% benzaldehyde and phenylacetic acid, and the rest are 51.1% heavy components produced by the upstream reaction and separation process such as phenylethyl alcohol polymer, including trace amounts of metal ions such as Fe, Cr, Ni ions, etc.
[0060] The method for cracking and recovering styrene comprises the following steps:
[0061] 1) The above by-product heavy components are removed by distillation, the distillation pressure is 5 kPaA, the temperature is 190° C., and the time is 20 min, and the light components containing phenylethyl ether are collected.
[0062] 2) 770 kg of the light component from step 1) was mixed with 290 kg of a NaOH aqueous solution having a pH value of 13.2, and the acidic impurities were removed by alkali washing at a temperature of 45° C. for 30 min. The mixture was then allowed to stand for phase separation, and the upper oil phase material was collected, wherein the content of acidic impurities such as benzoic acid, benzaldehyde, and phenylacetic acid was reduced to 350 ppm, and the content of metal ions was 500 ppm.
[0063] 3) 766 kg of the oil phase material of step 2) was mixed with 20 kg of benzenesulfonic acid / SiO2 catalyst (acid loading 30 wt%) and 550 ppm of 6 wt% trimethylamine hydrochloride 1-phenylethanol solution (calculated as trimethylamine hydrochloride), and phenylethyl alcohol ether was subjected to cracking and dehydration reaction at a reaction temperature of 100° C. and a reaction residence time of 22 min to generate styrene and water.
[0064] 4) The reaction system of step 3) is subjected to standing stratification to achieve oil-water separation at a separation temperature of 20° C. for 40 min, and then transferred to a distillation tower for distillation at a distillation pressure of 8 kPaA, a bottom temperature of 126° C., and a reflux ratio of 2 to obtain styrene.
[0065] In this embodiment, the conversion rate of phenylethyl alcohol ether is 96.8%, the selectivity of styrene is 93.3%, the purity of styrene product is 99.95%; and the platinum cobalt color number is 9.8.
[0066] Comparative Example 1
[0067] The method of Example 1 is referred to, except that the 1-phenylethanol solution of triethylamine hydrochloride is not added as an auxiliary agent, and other operations remain unchanged to obtain styrene.
[0068] In this comparative example, the conversion rate of phenylethyl alcohol ether was 83.6%, the selectivity of styrene was 88.6%, the purity of styrene product was 99.85%, and the platinum cobalt color number was 10.6.
[0069] Comparative Example 2
[0070] The preparation method according to Example 1 is different only in that triethylamine hydrochloride is replaced by triethylamine sulfate, and other operations remain unchanged to obtain styrene.
[0071] In this comparative example, the conversion rate of phenylethyl alcohol ether was 96.5%, the selectivity of styrene was 92.8%, the purity of styrene product was 99.95%, and the platinum cobalt color number was 8.8.
[0072] Comparative Example 3
[0073] The preparation method according to Example 1 is different only in that the step of removing heavy oil by evaporation is eliminated, the materials in the bottom of the tower are directly subjected to alkali washing and then reacted, and other operations remain unchanged to obtain styrene.
[0074] In this comparative example, the conversion rate of phenylethyl alcohol ether was 80.2%, the selectivity of styrene was 82.3%, the purity of styrene product was 93.6%, and the platinum cobalt color number was 13.1.
[0075] Comparative Example 4
[0076] The preparation method is described in Example 1, except that the alkali washing step after evaporation is eliminated and other operations remain unchanged to obtain styrene.
[0077] In this comparative example, the conversion rate of phenylethyl alcohol ether was 86.2%, the selectivity of styrene was 89.3%, the purity of styrene product was 98.9%, and the platinum cobalt color number was 12.9.
[0078] Comparative Example 5
[0079] The preparation method according to Example 1 is different only in that the solid acid catalyst is replaced by a homogeneous benzenesulfonic acid catalyst and other operations remain unchanged to obtain styrene.
[0080] In this comparative example, the conversion rate of phenylethyl alcohol ether was 94.2%, the selectivity of styrene was 85.3%, the purity of styrene product was 99.74%, and the platinum cobalt color number was 9.9.
Claims
1. A method for recovering styrene from the byproduct of propylene oxide produced by co-oxidation, It is characterized in that the steps include: 1) using a by-product heavy component from the co-oxidation process to produce propylene oxide as a raw material, wherein the by-product heavy component comprises phenylethyl alcohol ether, removing the heavy component from the by-product heavy component by distillation, and collecting a light component comprising phenylethyl alcohol ether; 2) mixing the light component of step 1) with a NaOH aqueous solution, removing acidic impurities by alkali washing, then standing for phase separation, and collecting the upper oil phase material; 3) mixing the oil phase material of step 2) with a solid acid catalyst and an organic hydrochloride auxiliary agent, so that the phenylethyl ether therein undergoes a cracking and dehydration reaction to generate styrene and water; the organic hydrochloride is selected from one or more of triethylamine hydrochloride and trimethylamine hydrochloride; 4) The reaction system of step 3) is subjected to oil-water separation and distillation to obtain styrene.
2. The method according to claim 1, It is characterized in that The by-product heavy components from the co-oxidation process for producing propylene oxide in step 1) include: 40-60% phenylethyl ether, 1-3% benzoic acid, 0-1% acetophenone, 0-1% phenylethyl alcohol, 1-2% benzaldehyde and phenylacetic acid, and the rest are heavy component impurities and trace amounts of metal ions.
3. The method according to claim 2, It is characterized in that The mass percentage of the phenylethyl alcohol ether is 40-50%.
4. The method according to claim 1, It is characterized in that In step 1), the distillation is carried out at a pressure of 1-10 kPaA, a temperature of 150-200° C. and a time of 10-60 min.
5. The method according to claim 4, It is characterized in that The distillation has a pressure of 1-5 kPaA, a temperature of 170-190° C., and a time of 20-30 min.
6. The method according to claim 1, It is characterized in that Step 2) The mass ratio of the light component in step 1) to the NaOH aqueous solution is 0.5-4:1; The pH value of the NaOH aqueous solution is 12-14; Step 2) The alkali washing temperature is 30-60°C and the time is 30-70 minutes.
7. The method according to claim 6, It is characterized in that The mass ratio of the light component in step 1) to the NaOH aqueous solution is 1-3:
1.
8. The method according to claim 6, It is characterized in that The pH value of the NaOH aqueous solution is 13-13.
5.
9. The method according to claim 6, It is characterized in that The alkali washing temperature is 45-55°C and the time is 30-50 minutes.
10. The method according to claim 1, It is characterized in that Step 3) the solid acid catalyst is selected from one or more of a strongly acidic cation exchange resin or a supported solid acid catalyst; The amount of the solid acid catalyst used is 2-6 wt % of the mass of the oil phase material in step 2).
11. The method according to claim 10, It is characterized in that The solid acid catalyst is selected from supported solid acid catalysts.
12. The method according to claim 10, It is characterized in that The amount of the solid acid catalyst used is 2.5-4.5 wt % of the mass of the oil phase material in step 2).
13. The method according to claim 10, It is characterized in that The strong acid cation exchange resin is selected from LX-67 acidic ion exchange resin of Lanxiao Technology or No. 732 strong acid cation exchange resin of Jinda Zhengtong.
14. The method according to claim 10, It is characterized in that The supported solid acid catalyst, the carrier is selected from activated carbon, SiO 2 One or more of the above, the loaded acid is selected from one or more of benzenesulfonic acid and p-toluenesulfonic acid.
15. The method according to claim 10, It is characterized in that The supported solid acid catalyst is selected from p-toluenesulfonic acid / SiO 2 Solid acid catalyst.
16. The method according to claim 10, It is characterized in that The supported solid acid catalyst has an acid content of 20-40 wt%.
17. The method according to claim 10, It is characterized in that The supported solid acid catalyst has an acid content of 25-35 wt%.
18. The method according to claim 1, It is characterized in that Step 3) the organic hydrochloride auxiliary agent is a 1-phenylethanol solution of organic hydrochloride with a concentration of 1-10wt%; The amount of the organic hydrochloride auxiliary agent, calculated as the organic hydrochloride therein, is 500-1000 ppm of the oil phase material in step 2).
19. The method according to claim 18, It is characterized in that The 1-phenylethanol solution of the organic hydrochloride has a concentration of 5-8 wt %.
20. The method according to claim 1, It is characterized in that The amount of the organic hydrochloride auxiliary agent used in step 3) is 600-800 ppm of the oil phase material in step 2) based on the organic hydrochloride therein.
21. The method according to claim 1, It is characterized in that In step 3), the cracking and dehydration reaction is carried out at a temperature of 80-150° C. and a residence time of the reaction solution of 10-40 min.
22. The method according to claim 21, It is characterized in that The cracking and dehydration reaction is carried out at a temperature of 100-120°C.
23. The method according to claim 21, It is characterized in that The residence time of the reaction solution is 20-30min.
24. The method according to claim 1, It is characterized in that Step 4) The oil-water separation is carried out by static stratification method, the separation temperature is 5-20°C, and the time is 0.5-2h; Step 4) The distillation is carried out in a distillation tower at a pressure of 1-10 kPaA; The bottom temperature of the tower is 100-140°C; the reflux ratio is 1-6.
25. The method according to claim 24, It is characterized in that The oil-water separation has a separation temperature of 10-20°C and a time of 0.5-1h.
26. The method according to claim 24, It is characterized in that The distillation pressure is 4-8 kPaA; The bottom temperature of the tower is 120-130°C; the reflux ratio is 2-3.