Process research on a new type of carbon and lithium doped ternary cathode precursor material

By using lithium carboxymethyl cellulose to form a stable slurry and processing it at high temperatures, the problem of high energy consumption and high pollution of residual alkali and carbon doping processes on the surface of the ternary cathode material is solved, and uniform carbon doping and lithium are achieved Doping improves the electrochemical performance and high-rate performance of the battery.

CN116495795BActive Publication Date: 2024-10-01GREEN ENERGY FIBER MATERIALS (SUZHOU) TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211237813.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-10-11
Publication Date
2024-10-01
Estimated Expiration
2042-10-11

AI Technical Summary

Technical Problem

The surface residual alkali problem of the ternary cathode material causes the battery to bulge and deform. The existing method of reducing the surface residual alkali increases the hardness and fine powder content of the material, and the carbon doping process has problems of high energy consumption, pollution and high cost.

Method used

Lithium carboxymethyl cellulose is used as the suspending agent, and a stable slurry is formed through high-speed stirring, and is processed and calcined in a rotary kiln at high temperature to form a uniform carbon-doped and lithium-doped ternary cathode composite material, using an inert atmosphere Protect carbonization and crushing, and control particle size distribution.

Benefits of technology

It improves the electrochemical performance of the ternary cathode material, reduces energy consumption and pollution, solves the problem of insufficient surface doping, and improves the battery's high rate, fast charge and discharge, and low temperature performance.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a process research of a novel carbon and lithium doped ternary positive electrode precursor material, specifically including the following steps: weighing raw materials, taking carboxymethyl cellulose lithium, adding it to deionized water and stirring and dissolving it at high speed in a reactor to form a slurry of carboxymethyl cellulose lithium, adding an appropriate amount of nickel source, cobalt source, manganese source and lithium source and dispersant auxiliary agent to the slurry for high-speed uniform stirring for synthesis, and then treating it in a rotary kiln at high temperature for 10-20h to obtain precursor particles, and then synthesizing it through high-temperature calcination to obtain a carbon-doped and lithium-doped ternary positive electrode composite material with relatively uniformity. The process research of the novel carbon and lithium doped ternary positive electrode precursor material disclosed by the invention has reduced the high energy consumption, high pollution and high cost of the current existing carbon doping process, and at the same time, it also solves the insufficient effect of additional lithium doping and lithium supplementation in the current lithium battery process, which only supplements lithium on the surface. Carboxymethyl cellulose salts (sodium salts, lithium salts, ammonium salts and other metal ion salts) have very good suspension and dispersion functions. They can suspend and disperse the precursor powder very well. When carbonized and coated, they will form a very uniform carbon coating (carbon doping) layer, and even form a lithium-doped carbonized layer, thereby improving the electrochemical performance of the material during application.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of lithium-ion batteries, and in particular to a process research on a novel carbon and lithium-doped ternary positive electrode precursor material. Background Art

[0002] Ternary cathode materials combine the advantages of LiCoO2, LiNiO2 and LiMnO2, and are one of the cathode materials with the greatest development potential. In particular, high-nickel ternary materials have become the application direction of high-energy-density power batteries in the future. In recent years, ternary cathode materials have gradually developed in the direction of high specific capacity, high compaction, high voltage and low cost, but the problem of residual alkali on the surface of ternary materials has always been a prominent problem affecting their practical application. The main reason is that the residual alkali on the surface (LiOH and Li2CO3) can easily react with the electrolyte to produce gas, causing the battery to swell and deform, creating safety hazards.

[0003] At present, the methods that can be used for industrialization to reduce the residual alkali on the surface of ternary materials are mainly carried out by increasing the sintering temperature and solvent washing. Increasing the sintering temperature can significantly reduce the residual alkali on the surface, but this method makes the primary particles of the material larger and the hardness increases. The post-processing process is likely to cause an increase in the amount of fine powder, making it difficult to obtain high-quality materials. At the same time, the increase in sintering temperature increases the degree of lithium-nickel mixing, resulting in a decrease in product capacity. The (solvent) washing method can also effectively reduce the residual alkali on the surface. The solvents used are usually: ethanol, deionized water, organic weak acid, non-aqueous organic solvent, boric acid, citric acid, etc. However, whether it is elution washing, slurry washing, or filter press washing, it increases the difficulty of industrial operation, and it is at the expense of the consistency and partial performance of the material.

[0004] In addition, the sintering of conventional ternary materials requires high temperatures and high hardness, and post-processing requires increased crushing strength in order to control the appropriate product particle size distribution. This not only causes certain damage to the particle morphology, but also makes it easier to produce fine powder. The current existing carbon doping process has the disadvantages of high energy consumption, high pollution and high cost. Summary of the invention

[0005] The present invention discloses a process research of a novel carbon and lithium doped ternary positive electrode precursor material, aiming to solve the technical problems proposed in the background technology that the conventional ternary material sintering has high temperature and high hardness, and the post-processing needs to improve the crushing strength to control the appropriate product particle size distribution, which not only causes certain damage to the particle morphology, but also makes it easier to produce fine powder. The current existing carbon doping process has the disadvantages of high energy consumption, high pollution and high cost.

[0006] In order to achieve the above object, the present invention adopts the following technical solutions:

[0007] A process study of a novel carbon and lithium doped ternary cathode precursor material specifically includes the following steps:

[0008] S1: weighing raw materials, taking 1-5 parts of lithium carboxymethyl cellulose, adding 50-100 parts of deionized water, stirring and dissolving at high speed in a reaction kettle to form a slurry of lithium carboxymethyl cellulose;

[0009] S2: adding appropriate amounts of nickel source, cobalt source, manganese source, lithium source and dispersant additive to the lithium carboxymethyl cellulose slurry obtained in step S1 and stirring at high speed for synthesis to form a stable slurry;

[0010] S3: treating in a rotary kiln at high temperature for 10-20 hours, the high temperature being 550°C-1000°C, to obtain precursor particles;

[0011] S4: Finally, the precursor particles obtained in step S3 are subjected to high-temperature calcination to obtain a ternary positive electrode composite material with relatively uniform carbon doping and lithium doping.

[0012] Generally, the higher the concentration of lithium carboxymethyl cellulose, the higher the carbon doping and lithium doping contents of the final product. Correspondingly, the carbon doping and lithium doping contents of the nickel-cobalt-manganese-lithium precursor or product will be high, the conductivity of the product will be better, the surface carbon coating of the nickel-cobalt-manganese-lithium precursor or product will be more uniform, and the lithium coating will also be more uniform.

[0013] In a preferred scheme, the steps S2-S4 need to be kept in an inert gas atmosphere and heated to 650-850°C under the protection of the inert gas atmosphere. During the carbonization process, it is noted that the particles of the precursor can be between 1-10 microns and adjusted according to the process conditions to finally obtain a relatively uniform carbon-coated and lithium-coated ternary positive electrode material. In an inert gas atmosphere, the mixture is first mixed in proportion to obtain a uniformly dispersed stable mixed slurry, the stable slurry is pre-coated at a certain temperature and within a certain time range, the pre-coated material is raised to a high temperature for carbonization and insulation, and after cooling, it is crushed and sieved by a jet mill for grading, the sieved material is subjected to high-temperature heat treatment, and cooled to obtain the required carbon-doped and lithium-doped ternary positive electrode materials of different particle sizes.

[0014] The carbon doping and lithium doping processes are not limited to various synthesis process routes of ternary positive electrode composite materials, including: solid phase method, liquid phase method, high temperature solid phase reaction method, carbon thermal reduction method, microwave synthesis method and deposition method, solution gel method, hydrothermal synthesis method, template method, precipitation method and solvent thermal synthesis method, etc., as long as the suspension and dispersion of carboxymethyl cellulose related products are used as the optimized process, the carbon doping or lithium doping process route can be carried out.

[0015] In a preferred embodiment, the nickel source is at least one of nickel sulfate, nickel acetate and nickel nitrate, the cobalt source is at least one of cobalt sulfate, cobalt acetate and cobalt nitrate, the manganese source is at least one of manganese sulfate, manganese acetate and manganese nitrate, the lithium source can also be mainly lithium carboxymethyl cellulose, with at least one of lithium carbonate, lithium acetate and lithium hydroxide, the stirring rate in step S1 is 10rpm to 1000rpm, and the control in the reactor is as follows: the pH of the prepared slurry is 8.0 to 12.0, and the slurry is 1 / 6 to 2 / 3 of the volume of the reactor; the temperature during the reaction is 55 to 75°C, the stirring rate during the reaction is 100 to 800rpm, and the oxygen content in the reactor is controlled by introducing an inert gas into the reactor.

[0016] In a preferred embodiment, the inert gas atmosphere is a combination of one or more of nitrogen, helium and argon, and the nickel-cobalt-manganese ternary precursor is NCM523 precursor material, and its molecular formula is: Ni 0.5Co0.2Mn0.3(OH)2.

[0017] As can be seen from the above, a process study on a novel carbon and lithium doped ternary positive electrode precursor material specifically includes the following steps: S1: weigh the raw materials, take 1-5 parts of lithium carboxymethyl cellulose, add them to 50-100 parts of deionized water, stir and dissolve them at high speed in a reactor to form a slurry of lithium carboxymethyl cellulose; S2: add an appropriate amount of nickel source, cobalt source, manganese source and lithium source and a dispersant aid to the lithium carboxymethyl cellulose slurry obtained in step S1, stir and synthesize them at high speed and evenly to form a stable slurry; S3: treat it in a rotary kiln at high temperature for 10-20h, the high temperature is 550℃-1000℃, to obtain precursor particles; S4: finally, the precursor particles obtained in step S3 are subjected to high-temperature calcination to obtain a ternary positive electrode composite material with relatively uniform carbon doping and lithium doping.

[0018] The process research of the novel carbon and lithium doped ternary positive electrode precursor material provided by the present invention has the following technical effects:

[0019] The carboxymethyl cellulose lithium used in the present invention has a very good suspension and dispersion effect. It can suspend and disperse the materials such as the ternary positive electrode material precursor very well, so that a relatively uniformly coated carboxymethyl cellulose lithium solution is formed around the ternary positive electrode material, thereby forming a relatively uniform carbon source and lithium source, and then calcined at high temperature to obtain a relatively uniform carbon-doped and lithium-doped ternary positive electrode material precursor. The carbon source on the surface of the ternary positive electrode material of the terminal product finally formed is evenly distributed, and the lithium source is evenly distributed, so as to improve the electrochemical performance of the ternary positive electrode material during the use of the lithium battery. The high energy consumption, high pollution and high cost of the current existing carbon doping process are reduced. At the same time, it also solves the shortcomings of the additional lithium doping and lithium supplementation in the current lithium battery process, which is only supplemented on the surface. In this way, the electrochemical performance in the new energy process can be greatly improved, the high rate can be improved, the fast charge and discharge can be improved, the first effect can be improved, the internal resistance can be reduced, the ion conductivity can be improved, the low temperature performance can be solved, and the rate performance can be improved. DETAILED DESCRIPTION

[0020] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0021] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] A process study of a novel carbon and lithium doped ternary cathode precursor material specifically includes the following steps:

[0023] S1: weighing raw materials, taking 1-5 parts of lithium carboxymethyl cellulose, adding 50-100 parts of deionized water, stirring and dissolving at high speed in a reaction kettle to form a slurry of lithium carboxymethyl cellulose;

[0024] S2: adding appropriate amounts of nickel source, cobalt source, manganese source, lithium source and dispersant additive to the lithium carboxymethyl cellulose slurry obtained in step S1 and stirring at high speed for synthesis to form a stable slurry;

[0025] S3: treating in a rotary kiln at high temperature for 10-20 hours, the high temperature being 550°C-1000°C, to obtain precursor particles;

[0026] S4: Finally, the precursor particles obtained in step S3 are subjected to high-temperature calcination to obtain a ternary positive electrode composite material with relatively uniform carbon doping and lithium doping.

[0027] In a preferred embodiment, the steps S2-S4 need to be kept in an inert gas atmosphere and heated to 650-850°C under the protection of the inert gas atmosphere. During the carbonization process, it is noted that the particles of the precursor can be between 1-10 microns and adjusted according to the process conditions. Finally, a ternary positive electrode material with relatively uniform carbon coating and lithium coating is obtained. In an inert gas atmosphere, it is first mixed according to the proportion to obtain a uniformly dispersed stable mixed slurry.

[0028] In a preferred embodiment, the nickel source is at least one of nickel sulfate, nickel acetate, and nickel nitrate, the cobalt source is at least one of cobalt sulfate, cobalt acetate, and cobalt nitrate, the manganese source is at least one of manganese sulfate, manganese acetate, and manganese nitrate, and the lithium source is at least one of lithium carbonate, lithium acetate, and lithium hydroxide.

[0029] In a preferred embodiment, the stirring rate in step S1 is 100 rpm to 1000 rpm.

[0030] In a preferred embodiment, the control in the reactor is as follows: the pH of the prepared slurry is 8.0-12.0, and the slurry is 1 / 6-2 / 3 of the volume of the reactor; the temperature during the reaction is 55-75°C, the stirring rate during the reaction is 100-800 rpm, and the oxygen content in the reactor is controlled by introducing inert gas into the reactor.

[0031] In a preferred embodiment, the inert gas atmosphere is a combination of one or more of nitrogen, helium and argon.

[0032] In a preferred embodiment, the stable slurry is pre-coated at a certain temperature and within a certain time range, the pre-coated material is raised to a high temperature for carbonization and heat preservation, and after cooling, it is crushed and sieved by a jet mill, and the sieved material is subjected to high-temperature heat treatment and cooled to obtain the required carbon-doped and lithium-doped ternary positive electrode materials of different particle sizes.

[0033] In a preferred embodiment, the nickel-cobalt-manganese ternary precursor is an NCM523 precursor material, and its molecular formula is: Ni 0.5Co 0.2Mn 0.3(OH)2.

[0034] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0035] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

[0036] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A new process for carbon and lithium doped ternary cathode precursor materials, It is characterized in that The specific steps include: S1: weighing raw materials, taking 1-5 parts of lithium carboxymethyl cellulose, adding 50-100 parts of deionized water, stirring and dissolving at high speed in a reaction kettle to form a slurry of lithium carboxymethyl cellulose; S2: adding appropriate amounts of nickel source, cobalt source, manganese source, lithium source and dispersant additive to the lithium carboxymethyl cellulose slurry obtained in step S1, and stirring at high speed for synthesis to form a stable slurry; S3: treating in a rotary kiln at high temperature for 10-20 hours, the high temperature being 550°C-1000°C, to obtain precursor particles; S4: Finally, the precursor particles obtained in step S3 are subjected to high-temperature calcination to obtain a ternary positive electrode composite material with relatively uniform carbon doping and lithium doping.

2. A process for preparing a novel carbon and lithium doped ternary cathode precursor material according to claim 1, It is characterized in that In steps S2-S4, it is necessary to keep it in an inert gas atmosphere and heat it to 650-850°C under the protection of the inert gas atmosphere. During the carbonization process, pay attention to the precursor particles between 1-100 microns, and adjust them according to the process conditions. Finally, a ternary positive electrode material with relatively uniform carbon coating and lithium coating is obtained. In an inert gas atmosphere, first mix them according to the proportion to obtain a uniformly dispersed stable mixed slurry.

3. A process for preparing a novel carbon and lithium doped ternary cathode precursor material according to claim 1, It is characterized in that The nickel source is at least one of nickel sulfate, nickel acetate, and nickel nitrate; the cobalt source is at least one of cobalt sulfate, cobalt acetate, and cobalt nitrate; the manganese source is at least one of manganese sulfate, manganese acetate, and manganese nitrate; and the lithium source is mainly lithium carboxymethyl cellulose, with at least one or more of lithium carbonate, lithium acetate, and lithium hydroxide as auxiliary.

4. A process for preparing a novel carbon and lithium doped ternary cathode precursor material according to claim 1, It is characterized in that The stirring rate in step S1 is 10 rpm to 1000 rpm.

5. A process for preparing a novel carbon and lithium doped ternary cathode precursor material according to claim 1, It is characterized in that The control in the reactor is as follows: the pH of the prepared slurry is 8.0-12.0, and the slurry is 1 / 6-2 / 3 of the volume of the reactor; the temperature during the reaction is 55-75°C, the stirring rate during the reaction is 100-800rpm, and the oxygen content in the reactor is controlled by introducing inert gas into the reactor.

6. A process for preparing a novel carbon and lithium doped ternary cathode precursor material according to claim 5, It is characterized in that The inert gas atmosphere is a combination of one or more of nitrogen, helium and argon.

7. The process of a novel carbon and lithium doped ternary cathode precursor material according to claim 1, It is characterized in that The stable slurry is pre-coated at a certain temperature and within a certain time range, the pre-coated material is raised to a high temperature for carbonization and heat preservation, and after cooling, it is crushed and sieved by a jet mill, and the sieved material is subjected to high-temperature heat treatment and cooled to obtain the required carbon-doped and lithium-doped ternary positive electrode materials of different particle sizes.

8. The process of a novel carbon and lithium doped ternary cathode precursor material according to claim 1, It is characterized in that The nickel-cobalt-manganese ternary precursor is a precursor material of NCM523, 622, 811 or 910 type.