A photodetection device and a method for preparing the same

By forming isolation walls and metal grids in the photodetection device, combined with 3D printing technology and microlens design, the problem of efficiency attenuation of traditional silicon-based short-wave infrared sensors after the 800nm ​​band is solved, the response time and resolution are improved, and the cost, achieving effective detection of short-wave infrared bands.

CN116845076BActive Publication Date: 2024-10-11RADIUM YOUXIN TECH (SUZHOU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310787255.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-29
Publication Date
2024-10-11
Estimated Expiration
2043-06-29

AI Technical Summary

Technical Problem

The quantum efficiency of traditional silicon-based short-wave infrared focal plane sensors is severely attenuated after the 800nm ​​band, resulting in high cost and poor reliability. It cannot effectively detect the short-wave infrared band, limiting its application in fields such as autonomous driving and night photography.

Method used

By forming isolation walls and metal grids in the photodetection device, using 3D printing technology to fill the photoelectric conversion layer, adding a transparent common electrode layer, and forming microlenses on the pixel unit, electron mobility and optical isolation are improved, and dark current is reduced. and cost.

Benefits of technology

It improves the response time and resolution of the photodetection device, reduces material usage and production costs, enhances the reliability and performance of the device, and achieves effective detection of the short-wave infrared band.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116845076B_ABST
    Figure CN116845076B_ABST
Patent Text Reader

Abstract

The present invention discloses a photodetection device and a preparation method thereof, comprising the steps of step S1: providing a substrate formed with a readout circuit array, wherein each readout circuit unit in the array corresponds to a pixel unit; step S2: forming an electron transport layer array on the readout circuit array of the substrate; step S3: forming an isolation wall between the pixel units; step S4: filling a photoelectric conversion layer array between the isolation walls; and step S5: forming a transparent common electrode layer array above the photoelectric conversion layer array, wherein the pixel walls are formed in advance and photoelectric pixel points are formed by a processing technique, thereby saving materials, reducing costs, and improving device performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of optoelectronic technology, and in particular to a light detection device and a preparation method thereof. Background Art

[0002] Since the 21st century, image sensing technology has rapidly developed with the continuous advancement of semiconductor technology. After nearly a decade of research and development, it has been found that most objects at room temperature radiate radiation in the infrared band. Consequently, infrared radiation imaging has become a new detection method. Infrared imaging technology uses infrared photoelectric systems to convert received infrared radiation into images perceptible to the human eye. Silicon-based imaging arrays have gradually improved in resolution, expanded in pixel size, and decreased in pixel size, reaching the billion-level. Survey statistics show that the market for silicon-based image sensors is growing annually. However, due to silicon's absorption capacity, silicon-based image sensors have a detection band of only 1.1μm and are in a blind spot beyond 1700nm, limiting their widespread application in areas such as autonomous driving and night photography.

[0003] The short-wave infrared (SWIR) range, between 900 and 2500 nm, occupies the electromagnetic spectrum above the near-infrared, significantly exceeding the capabilities of traditional silicon-based imaging sensors. Despite this, the SWIR band is increasingly used in machine vision, offering unique detection, classification, and quality control capabilities, as well as in ambient light applications such as surveillance and remote sensing. Because silicon's quantum efficiency rapidly decays beyond 800 nm, SWIR sensors rely on alternative chemistries such as indium gallium arsenide (InGaAs) or mercury cadmium telluride (MCT). Traditional SWIR focal plane sensors (FPSs) primarily utilize InGaAs materials. The fabricated detector arrays are interconnected to silicon-based readout circuitry via an indium pillar flip-chip bonding process. While these materials are more mature than other imaging methods, the high cost of semiconductor epitaxial growth and the low power efficiency of flip-chip bonding contribute to the high cost and poor device reliability of SWIR FPAs fabricated using InGaAs. Summary of the Invention

[0004] In order to solve the above-mentioned problem of the performance of the optical detection device, the present invention provides a optical detection device and a preparation method thereof, which improves the performance of the device by forming an isolation wall.

[0005] The method for preparing a light detection device of the present invention comprises:

[0006] Step S1: providing a substrate having a readout circuit array formed thereon, wherein each readout circuit unit in the array corresponds to a pixel unit;

[0007] Step S2: forming an electron transport layer array on the readout circuit array of the substrate;

[0008] Step S3: forming isolation walls between pixel units;

[0009] Step S4: filling the photoelectric conversion layer array between the isolation walls;

[0010] Step S5: forming a transparent common electrode layer array above the photoelectric conversion layer array.

[0011] The present invention also provides a light detection device, comprising: a substrate having a readout circuit array formed thereon, wherein each readout circuit unit in the array corresponds to a pixel unit;

[0012] an electron transport layer array located on the readout circuit array;

[0013] Isolation walls between pixel units;

[0014] A photoelectric conversion layer array filled between the isolation walls;

[0015] A transparent common electrode layer array is located above the photoelectric conversion layer array.

[0016] The light detection device and preparation method of the present invention forms a pixel wall in advance and then forms a photoelectric pixel point by using a processing technology (such as inkjet printing, etc.), thereby saving materials, reducing costs and improving device performance.

[0017] This solution provides a metal grid around the pixels, which significantly increases electron mobility and improves device response time. Furthermore, the metal grid provides optical isolation, blocking light from entering adjacent photodiodes and reducing optical interference between photoelectric pixels.

[0018] This solution forms a microlens above the photosensitive area of ​​the pixel. At this time, the photosensitive area is no longer determined by the area of ​​the photosensitive opening, but by the surface area of ​​the microlens. This can take into account the size of a single pixel while improving the sensitivity, thereby achieving high resolution. Through processing technology, ITO is engraved into a microlens, which not only saves costs but also improves the performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 A flow chart of an embodiment of a method for preparing a photodetector device according to the present invention;

[0020] Figures 2 to 6 is a schematic diagram of a first embodiment of a method for manufacturing a photodetecting device according to the present invention;

[0021] Figure 7 Schematic diagrams of the second and third embodiments of the method for manufacturing a photodetection device of the present invention. DETAILED DESCRIPTION

[0022] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention, so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more precise definition of the protection scope of the present invention. Obviously, the embodiments described in the present invention are only a part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. In addition, the technical features involved in the different implementation methods of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0023] The present invention provides a light detection device and a method for manufacturing the same. Figures 1 to 6 , the preparation method of the present application comprises:

[0024] Step S1 : providing a substrate 120 having a readout circuit array 110 formed thereon, wherein each readout circuit unit in the array corresponds to a pixel unit.

[0025] Specifically, the substrate includes a pixel unit area 130 and an isolation area 140. The pixel unit area 130 is used to form a pixel unit array. In this embodiment, the pixel unit 130 area has an array-distributed readout circuit array 110. A readout circuit (ROIC) is formed in each pixel unit in the pixel unit area. The readout circuit is responsible for providing a stable and reliable voltage bias for the pixel unit array, integrating the input current and converting it into a voltage signal, and converting it into a suitable output voltage after amplification and buffering for use by subsequent modules. In addition, the readout circuit will also be equipped with a digital control module to realize a variety of windowing and timing control functions. Therefore, the performance of the readout circuit determines the imaging quality of the infrared focal plane array. In traditional technology, there is dark current between different pixels, which results in poor performance of the circuit operation.

[0026] In some embodiments, the substrate 120 may include a semiconductor substrate, and the material of the substrate may be a semiconductor material such as Si, Ge, SiGe, SiC, SiGeC, SiO2, etc. The readout circuit array 110 is formed using a semiconductor substrate, and the readout circuit array may be a functional circuit formed using a conventional semiconductor process. The method may also include placing the substrate in a vacuum molybdenum chamber, introducing Ar gas to control the pressure in the chamber to be 1.0-3.0 Pa. Sputtering is performed at a power of 300-350W for 8-10 cycles, and then sputtering is performed at a power of 800-1000W at a pressure of 0.3-0.5Pa for 4-6 cycles, the Ar gas is turned off, and the substrate is taken out after cooling for 5-10 minutes to form the bottom electrode of the readout circuit array.

[0027] Step S2 : forming an electron transport layer array 150 on the readout circuit array 110 of the substrate 120 .

[0028] Specifically, in this embodiment, the step of preparing the electron transport layer on the readout circuit specifically includes the following steps:

[0029] A pattern layer is formed on the substrate 120, such as by first applying photoresist and using photolithography to form a pattern layer with groove openings, the openings exposing the readout circuit array. Of course, other conventional methods can also be used to form a pattern layer with openings above the readout circuit array.

[0030] Then, the electron transport layer material is formed. The electron transport layer material can be polysilicon or metal with n-type impurities, or polysilicon with p-type impurities. The metal includes aluminum, titanium, nickel or gold. The electron transport layer array 150 can be formed by physical vapor deposition or chemical vapor deposition methods such as magnetron sputtering and evaporation. For example, the substrate with the bottom electrode is placed in the MBE vacuum coating chamber, the vacuum degree is controlled to 2x10-5-5x10-5Pa, and a five-source simultaneous evaporation method is adopted. Cu, Zn, Cd, Sn, and Se are used as targets. The precursor is grown in a one-step method to form the electron transport layer array 150 in the groove opening. Specifically, the substrate is first heated to 120-130 degrees Celsius and stabilized. After the five source targets are preheated for 20 minutes, the baffle is opened, and the deposition is carried out simultaneously for 20-30 minutes. The baffle is closed and the material is removed to obtain an electron transport layer material with a thickness of about 1-2 μm. Of course, other processes, such as 3D printing or physical vapor deposition, may also be used to form the electron transport layer.

[0031] Since the electron transport layer material is only distributed above the readout circuit array, the electron transport layer array 150 is distributed in an array. Figure 3 As shown, a dielectric layer is formed between the electron transport layer arrays, and the dielectric layer can be a patterned layer formed before depositing the electron transport layer material.

[0032] Step S3: forming isolation walls 160 between pixel units.

[0033] Specifically, refer to Figure 4In this embodiment, a photoresist layer can be first deposited in the isolation region 140 between the pixel units. For example, the photoresist layer can be deposited on the surface of the substrate on which the electron transport layer is formed. The photoresist layer is then patterned to form a trench opening in the photoresist layer in the isolation region. A metal material is then deposited in the trench opening to form the isolation wall. The deposition is performed using physical or chemical vapor deposition, for example, using physical vapor deposition equipment, an aluminum target, argon as the sputtering gas, and a vacuum of less than 5*10-7 Torr. The metal material used can also be common semiconductor metals such as copper, tungsten, and gold. Finally, the photoresist layer is removed.

[0034] Step S4 : filling the photoelectric conversion layer array 170 between the isolation walls 160 .

[0035] Specifically, refer to Figure 5 3D printing can be used. The printing process uses high-resolution 3D printing technology to print test patterns and print material properties based on the printer calibration file. Appropriate printing parameters are selected, such as a printing speed of 50-100 mm / s; optoelectronic materials such as PbS use platform heating and infrared curing; and the platform heating temperature is 50-100°C. The optoelectronic material printing voltage is 5-20V, and the material thickness is 100-150nm. The optoelectronic conversion layer array can be composed of a stack of optoelectronic material layers and dielectric material layers. The dielectric material is cured using platform heating and UV curing.

[0036] In this embodiment, the colloidal quantum dot photoelectric conversion layer made of the photoelectric material PbS (lead sulfide) is suitable for absorbing visible light and short-wave infrared light. Therefore, it can improve the conversion efficiency of the colloidal quantum dot photoelectric conversion layer to visible light and short-wave infrared light, stimulate the colloidal quantum dot photoelectric conversion layer to generate more photogenerated carriers, and increase the current intensity formed by the directional movement of photogenerated carriers, thereby increasing the intensity of the electrical signal of the short-wave infrared focal plane sensor and improving the resolution of the short-wave infrared focal plane sensor.

[0037] The PI junction functions similarly to a PN junction, exhibiting unidirectional conductivity. However, unlike a PN junction, the semiconductors at both ends are different: one end is an intrinsic semiconductor, and the other is a P-type semiconductor. When light passes through the common electrode and irradiates the colloidal quantum dot photoelectric conversion layer, the layer generates photogenerated carriers. These carriers, under the influence of the electric field formed between the bias electrode and the common electrode, form a directional current. When this directional current meets certain conditions, the thin-film transistor turns on, transmitting this current signal through the drain electrode of the thin-film transistor to the imaging device. Therefore, dark current in the isolation region significantly impacts device performance.

[0038] In this embodiment, the isolation wall 160 is first formed, and then the photoelectric pixel point is formed by magnetron sputtering technology, which saves materials and reduces costs; the pixel wall can also achieve pixel isolation through design to reduce the dark current level and improve device performance.

[0039] Step S5: forming a transparent common electrode layer array 180 on the photoelectric conversion layer array.

[0040] Specifically, refer to Figure 6 A transparent common electrode layer 180 (ITO), such as an indium tin oxide semiconductor, is deposited above the photoelectric conversion layer. The ITO layer formation process parameters are: a vacuum of 10-5 × 10-4 Pa, a DC power of 100-300 W, an RF power of 300-500 W, and an argon gas flow rate of 50-150 sccm. The ITO thickness is 250-350 nm.

[0041] refer to Figure 7 In a second embodiment of the present invention, before forming the ITO layer, a metal layer 210 is formed above the isolation wall, thereby forming a metal grid around the pixel. This significantly improves electron mobility and device response time. Furthermore, the metal grid provides optical isolation, blocking light from entering adjacent photodiodes and improving optical interference between photoelectric pixels. Specifically, this metal grid can be formed using electroplating or physical vapor deposition.

[0042] Continue to refer Figure 7 In a third embodiment of the present invention, after forming the ITO layer, the method further includes forming a microlens 220 above the pixel photosensitive area corresponding to the ITO layer. In this case, the photosensitive area is no longer determined by the photosensitive opening area, but by the surface area of ​​the microlens. This can take into account the size of a single pixel while improving the sensitivity, thereby achieving high resolution. By using a processing technology, the ITO is engraved into a microlens, which not only saves costs but also improves the performance of the device.

[0043] In this embodiment, specifically, photoresist is coated on the ITO surface, and then the desired pattern and photoresist morphology are formed using a grayscale exposure process. The exposure parameter specifications are as follows: write head resolution: 1μm, write head direct writing rate: 150 (mm2 / min), laser band: 405nm, grayscale direct writing level: 256 levels, and autofocus accuracy: 100nm.

[0044] A dry etching process is used to retain the photoresist pattern on the arc surface above each unit of the transparent common electrode layer array to form a microlens. The specific dry etching process transfers the photolithography group onto the ITO. An ICP dry etching process is used: RF power is 100-300W, ICP power is 200-400W, gas pressure is 5-15mtorr, and the gas can be a mixed gas of chlorine 25-35sccm, C2H4 5-10sccm, and Ar 40-60sccm.

[0045] In addition, the present invention also provides a photodetection device formed by the above method, comprising: a substrate having a readout circuit array formed thereon, wherein each readout circuit unit in the array corresponds to a pixel unit; an electron transport layer array located on the readout circuit array; isolation walls located between the pixel units; a photoelectric conversion layer array filled between the isolation walls; and a transparent common electrode layer array located above the photoelectric conversion layer array.

[0046] In the second embodiment of the optical detection device, a metal grid is further provided above the isolation wall.

[0047] In the third embodiment of the photodetection device, a microlens is further formed above the transparent common electrode layer array corresponding to the photoelectric conversion layer array.

[0048] The above description is only a preferred embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made by using the contents of the present invention description and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the invention.

Claims

1. A method for preparing a photodetection device, characterized in that: include: Step S1: providing a substrate formed with a readout circuit array, wherein each readout circuit unit in the array corresponds to a pixel unit; Step S2: forming an electron transport layer array on the readout circuit array of the substrate; Step S3: forming a metal isolation wall between the pixel units; Step S4: filling the photoelectric conversion layer array between the isolation walls; Step S5: forming a transparent common electrode layer array above the photoelectric conversion layer array.

2. The method for preparing a photodetector device according to claim 1, characterized in that: The isolation wall is formed by physical vapor deposition, with a metal target of aluminum, copper, tungsten or gold, argon as a sputtering gas, and a vacuum of less than 5*10-7 torr.

3. The method for preparing a photodetector device according to claim 1, characterized in that: The method for filling the photoelectric conversion layer array is: 3D printing.

4. The method for preparing a photodetection device according to claim 3, characterized in that: The printing parameters of 3D printing are: printing speed is 50-100mm / s; optoelectronic material PbS, using platform heating and infrared curing; platform heating temperature is 50-100℃, optoelectronic material printing voltage is 5-20V, and material thickness is 100-150nm.

5. The method for preparing a photodetection device according to claim 1, characterized in that: The method further includes forming a metal layer on the isolation wall between steps S4 and S5, thereby forming a metal grid around the pixel.

6. The method for preparing a photodetection device according to claim 1, characterized in that: After forming the transparent common electrode layer array, the method further comprises the following steps: Applying photoresist on the surface of the transparent common electrode layer array; Using grayscale exposure process to form the desired pattern and photoresist morphology; A photoresist pattern with an arc surface is retained above each unit of the transparent common electrode layer array by a dry etching process to form a microlens.

7. The method for preparing a photodetection device according to claim 6, characterized in that: The dry etching adopts an ICP dry etching process: RF power is 100-300W, ICP power is 200-400W, gas pressure is 5-15mtorr, and the gas selected is a mixed gas of chlorine 25-35sccm, C2H45-10sccm, and Ar40-60sccm.

8. A light detection device, characterized in that: include: A substrate having a readout circuit array formed thereon, wherein each readout circuit unit in the array corresponds to a pixel unit; an electron transport layer array located on the readout circuit array; A metal isolation wall between pixel units; An array of photoelectric conversion layers filled between the isolation walls; A transparent common electrode layer array is located above the photoelectric conversion layer array.

9. The optical detection device according to claim 8, characterized in that: A metal grid is also included above the separation wall.

10. The optical detection device according to claim 8, characterized in that: A microlens is also formed above the transparent common electrode layer array corresponding to the photoelectric conversion layer array.