A method and system for penetrant detection and defect repair in titanium alloy casting processing

By combining mechanical scanning, image processing and ultrasonic cleaning technology, efficient and accurate penetration detection and defect repair of titanium alloy castings are achieved, and the problems of inaccurate and reliability of detection results in the existing technology are solved, and the intelligence of detection is improved and efficiency.

CN117110574BActive Publication Date: 2024-11-05PANXI VANADIUM & TITANIUM INSPECTION & TESTING INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310986173.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-08-07
Publication Date
2024-11-05
Estimated Expiration
2043-08-07

AI Technical Summary

Technical Problem

The existing permeability detection methods do not fully expose the fine defects on the surface of titanium alloy castings, and fine sand particles can easily block the defect openings, reducing the accuracy of the detection results and the brightness of the permeability, and affecting the detection reliability of titanium alloy castings.

Method used

Using the combination technology of mechanical scanning module, image acquisition module, image enhancement module, central control module, image transmission module, video surveillance module and ultrasonic cleaning module, we realize automated and intelligent penetration detection and defect repair process through image enhancement and Real-time monitoring to discover and repair defects, and use ultrasonic cleaning to remove surface impurities to ensure the accuracy of the detection results.

Benefits of technology

It improves the sensitivity and accuracy of penetration detection, enhances the detection reliability of titanium alloy castings, reduces human error and pollution risks, and improves detection efficiency and cost-effectiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117110574B_ABST
    Figure CN117110574B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of casting detection and repair, and discloses a method and system for penetration detection and defect repair in titanium alloy casting processing, wherein a mechanical scanning module is used to perform penetration detection on titanium alloy castings, and process image information and video image information of the penetration detection process are obtained; an image enhancement module is used to perform image enhancement on the process image information and video image information of the penetration detection process; a central control module is used to control the mechanical scanning module to perform penetration action and movement, and the process image information enhanced by the image enhancement module is received and transmitted to a video monitoring module; defects found in the detection are repaired by a defect repair module, and cleaned by an ultrasonic cleaning module, and penetration detection is performed again until the defects are repaired. The present invention has a high degree of intelligence, improved detection accuracy, more effective observation and recording, low construction period cost, and reduced personnel participation rate and pollution risk.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of casting detection and repair, and in particular relates to a penetration detection and defect repair method in titanium alloy casting processing. Background Art

[0002] As one of the five conventional non-destructive testing methods, penetrant testing is used to check for open defects on the surface of metal and non-metal materials and is widely used in the aerospace field. Penetrant testing has strict requirements on the surface condition of parts. After machining and other processes, there are many dirts on the surface of parts, such as dust, oil, metal processing debris and oxide scale. Due to the influence of these dirts, the detection rate of surface defects of parts during penetrant testing is low.

[0003] At present, heat treatment and sand blasting are commonly used as surface pretreatment methods for penetrant testing of titanium alloy castings at home and abroad. This process method does not fully expose small defects, and fine sand particles can easily block the defect openings and reduce the brightness of the penetrant liquid, affecting the accuracy of the detection conclusion.

[0004] The defects of the existing technology and the technical problems that need to be solved urgently are as follows:

[0005] 1. Influence of surface contaminants: After machining and other processes, titanium alloy castings will have various contaminants on their surfaces, such as dust, oil, metal processing debris, and oxide scale. These contaminants will adhere to the surface of the parts, resulting in a low defect detection rate during penetration testing, because they may cover or block the opening of the defect, making it difficult for the defect to be detected by the penetrant.

[0006] 2. Limitations of surface pretreatment: At present, heat treatment and sand blasting are commonly used as surface pretreatment methods for penetrant testing in China. However, this method does not fully expose small defects and cannot effectively remove residual pollutants. At the same time, fine sand particles can easily block defect openings, reduce the brightness of the penetrant liquid, and affect the accuracy of the penetrant test results.

[0007] Therefore, the technical issues that need to be solved at present include the development of more effective surface cleaning and pretreatment methods to thoroughly remove contaminants from the surface of parts and fully expose defect openings. This can improve the sensitivity and accuracy of penetrant testing, ensuring that defects in titanium alloy castings can be reliably detected. At the same time, it is also necessary to consider the optimization of the penetrant to improve its brightness and permeability to ensure that defects of various sizes and types can be effectively detected. The solution to these technical problems will improve the reliability and application scope of penetrant testing in the aerospace field, and provide better support for quality control and safety assurance. Summary of the invention

[0008] In view of the problems existing in the prior art, the present invention provides a method for penetration testing and defect repairing in titanium alloy casting processing.

[0009] The present invention is implemented as follows: a method for penetrant detection and defect repair in titanium alloy casting processing, the method specifically comprising:

[0010] S1: Use mechanical scanning module to perform penetration testing on titanium alloy castings;

[0011] S2: using an image acquisition module to acquire process image information and video image information of the penetration detection process;

[0012] S3: using an image enhancement module to enhance the process image information and video image information of the penetration detection process;

[0013] S4: Using the central control module to control the mechanical scanning module to perform penetration action and movement;

[0014] S5: using the image transmission module to receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module;

[0015] S6: Use the video monitoring module to monitor the penetration testing process of the titanium alloy casting, and use the defect repair module to repair the defects found in the test;

[0016] S7: Use the ultrasonic cleaning module to clean and perform penetration testing again until the defect is repaired.

[0017] Furthermore, the specific implementation method of S1 is:

[0018] A mechanical device with certain control capabilities, such as a mechanical arm or robot, is used to carry a penetrant detection probe to scan the surface of titanium alloy castings under a predetermined trajectory. This probe is usually made of sensitive penetrant detection materials, which can absorb penetrant liquid in the defect area and display the defect location through dyeing or fluorescence.

[0019] Furthermore, the specific implementation method of S2 is:

[0020] Install a camera or video equipment and synchronize it with the mechanical scanning module to capture images and video information of the penetration inspection process. The image acquisition module should have high resolution and the ability to adapt to different lighting conditions to ensure accurate inspection results.

[0021] Furthermore, the specific implementation method of S3 is:

[0022] The image enhancement module can use digital image processing techniques such as filtering, contrast enhancement, edge enhancement, etc. to improve image quality and clarity, which helps to better detect and repair defects.

[0023] Furthermore, the specific implementation method of S4 is:

[0024] The central control module is the core control unit of the method. It can use a single-chip microcomputer, embedded system or computer, etc., to control the action and motion trajectory of the mechanical scanning module through a preset program to achieve automated penetration detection.

[0025] Furthermore, the specific implementation method of S5 is:

[0026] The image transmission module can use wired or wireless transmission technology to transmit the data processed by the image enhancement module to the video monitoring module. In this way, the operator can observe the penetration detection process in real time and find defects in time.

[0027] Furthermore, the specific implementation method of S6 is:

[0028] The video monitoring module is used to display and record the real-time video of the penetration testing process. The operator can find the defects on the surface of the titanium alloy casting during the monitoring. Once the defects are found, they can switch to the defect repair module.

[0029] Furthermore, the specific implementation method of S7 is:

[0030] The ultrasonic cleaning module uses ultrasonic vibration to generate tiny bubbles, which are impacted and folded in the liquid to clean the surface of the titanium alloy casting. After cleaning, the penetration test needs to be repeated until no defects are found to ensure that the quality of the titanium alloy casting meets the requirements.

[0031] Further, the cleaning using the ultrasonic cleaning module specifically includes:

[0032] (1) Pre-cleaning the titanium alloy casting;

[0033] (2) The outer surface of the titanium alloy casting is rinsed with a cleaning liquid in a high-pressure nozzle. The cleaning liquid is mixed with cleaning balls. After the cleaning balls are sprayed under high pressure, they contact the outer surface of the titanium alloy casting and vibrate, thereby loosening impurities on the surface of the aluminum alloy;

[0034] (3) The titanium alloy casting after pre-cleaning is subjected to deep ultrasonic cleaning. The ultrasonic wave generated by the ultrasonic generator propagates in the cleaning liquid, causing the titanium alloy casting to vibrate together at the ultrasonic frequency, and the oil and impurities on the outer surface of the titanium alloy casting can fall off during the vibration;

[0035] (4) Perform the final cleaning of the titanium alloy castings, and use clean water to wash away the oil and debris retained on the surface of the titanium alloy castings.

[0036] Further, the cleaning using the ultrasonic cleaning module specifically includes:

[0037] (1) Pre-cleaning the titanium alloy casting;

[0038] (2) The outer surface of the titanium alloy casting is rinsed with a cleaning liquid in a high-pressure nozzle. The cleaning liquid is mixed with cleaning balls. After the cleaning balls are sprayed under high pressure, they contact the outer surface of the titanium alloy casting and vibrate, thereby loosening impurities on the surface of the aluminum alloy;

[0039] (3) The titanium alloy casting after pre-cleaning is subjected to deep ultrasonic cleaning. The ultrasonic wave generated by the ultrasonic generator propagates in the cleaning liquid, causing the titanium alloy casting to vibrate together at the ultrasonic frequency, and the oil and impurities on the outer surface of the titanium alloy casting can fall off during the vibration;

[0040] (4) Perform the final cleaning of the titanium alloy castings, and use clean water to wash away the oil and debris retained on the surface of the titanium alloy castings.

[0041] Furthermore, the cleaning balls and the cleaning liquid are uniformly mixed in a ratio of 1:5, and the outer surface hardness of the cleaning balls is less than the outer surface hardness of the titanium alloy casting.

[0042] Furthermore, the cleaning ball has a diameter of 50 micrometers to 100 micrometers.

[0043] Another object of the present invention is to provide a penetration detection and defect repair system for titanium alloy casting processing that implements the penetration detection and defect repair method for titanium alloy casting processing, characterized in that the system comprises:

[0044] Mechanical scanning module for penetrant testing of titanium alloy castings;

[0045] An image acquisition module is used to acquire process image information and video image information of the penetration detection process;

[0046] An image enhancement module is used to enhance the process image information and video image information of the penetration detection process;

[0047] Video monitoring module, used to monitor the penetration testing process of titanium alloy castings;

[0048] Defect repair module, used to repair defects found during detection;

[0049] Ultrasonic cleaning module, used to clean titanium alloy castings;

[0050] A central control module is connected to the image enhancement module, the mechanical scanning module, the video monitoring module, the defect repair module, the image acquisition module and the ultrasonic cleaning module, and is used to control the operation of each module, and receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module;

[0051] Another object of the present invention is to provide a computer device, characterized in that the computer device includes a memory and a processor, the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the penetration detection and defect repair method in the titanium alloy casting processing.

[0052] Another object of the present invention is to provide a computer-readable storage medium storing a computer program, which, when executed by a processor, enables the processor to perform the steps of the penetration detection and defect repair method in the titanium alloy casting processing.

[0053] In combination with the above technical solutions and the technical problems solved, the advantages and positive effects of the technical solutions to be protected by the present invention are as follows:

[0054] First, the present invention adopts the pretreatment process of corrosion, heat treatment and ultrasonic cleaning to provide a surface preparation method for penetrant testing, which provides a good surface condition for the titanium alloy casting when penetrant testing is performed during the forming process, thereby improving the efficiency of penetrant testing and the accuracy of the test results.

[0055] Second, the penetration detection and defect repair method in titanium alloy casting processing provided by the present invention has a high degree of intelligence, improved detection accuracy, more effective observation and recording, low construction period cost, and reduced personnel participation rate and pollution risk.

[0056] Third, in the method of penetration testing and defect repair in the titanium alloy casting processing, each step involves some technological progress. The following is a specific description of the significant technological progress achieved in each step:

[0057] S1: Use the mechanical scanning module to perform penetrant testing on titanium alloy castings.

[0058] Significant technological progress: Automation and precision of mechanical scanning modules. Compared with traditional manual operations, the use of automated devices such as robotic arms or robots for penetration testing can improve detection efficiency and accuracy, reduce human errors, and can also perform comprehensive scanning on the surface of complex castings, thereby increasing the coverage of detection.

[0059] S2: Use the image acquisition module to acquire process image information and video image information of the penetration detection process.

[0060] Significant technological progress: High-resolution image acquisition technology. The application of modern high-resolution cameras and video cameras can capture subtle defects and surface features, making the inspection results clearer and more accurate. At the same time, the fast transmission and processing capabilities of the image acquisition module make real-time monitoring and data recording possible.

[0061] S3: Use the image enhancement module to enhance the process image information and video image information of the penetration detection process.

[0062] Significant technological progress: Digital image processing and enhancement technology. With the help of computer vision and image processing algorithms, the acquired images are filtered, contrast enhanced, edge enhanced, etc., which can improve image quality, highlight defects and surface details, and make it easier for operators to find potential defects.

[0063] S4: Using the central control module to control the mechanical scanning module to perform penetration action and movement.

[0064] Significant technological progress: Intelligent control technology. The central control module can accurately control the movement trajectory and action of the mechanical scanning module through a preset program, realizing a fully automatic penetration detection process. In addition, it can be combined with sensor technology to achieve real-time monitoring and adaptive adjustment of the detection process, improving the intelligence level of the system.

[0065] S5: using the image transmission module to receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module.

[0066] Significant technological progress: Real-time image transmission technology. The application of the image transmission module enables image data to be transmitted to the video monitoring module in real time. Operators can remotely observe the entire penetration testing process and find defects in a timely manner, avoiding the limitation of real-time on-site observation and improving efficiency and convenience.

[0067] S6: Use the video monitoring module to monitor the penetration testing process of titanium alloy castings, and use the defect repair module to repair the defects found during the inspection.

[0068] Significant technological advancement: Integration of real-time monitoring and repair. Combining the video monitoring module with the defect repair module allows for immediate repair operations after defects are discovered, without the need for manual reconfirmation, saving time and resources, and ensuring the timeliness and accuracy of the repair process.

[0069] S7: Use the ultrasonic cleaning module to clean and perform penetration testing again until the defect is repaired.

[0070] Significant technological progress: Ultrasonic cleaning technology. The ultrasonic cleaning module can efficiently remove surface impurities and penetrants without damaging titanium alloy castings. It can also penetrate into minute defects to ensure thorough defect repair. This cleaning method is more efficient and environmentally friendly than traditional cleaning technology.

[0071] In general, the penetration testing and defect repair method in titanium alloy casting processing adopts automation, digitization and intelligent technology, fully utilizing the advantages of modern science and technology, improving the efficiency and accuracy of detection and repair, while also reducing the risks and costs brought by manual operation. BRIEF DESCRIPTION OF THE DRAWINGS

[0072] Figure 1 It is a flow chart of a method for penetration testing and defect repair in titanium alloy casting processing provided by an embodiment of the present invention;

[0073] Figure 2 It is a structural diagram of a penetration detection and defect repair system in titanium alloy casting processing provided by an embodiment of the present invention;

[0074] In the figure: 1. Mechanical scanning module; 2. Image enhancement module; 3. Video monitoring module; 4. Defect repair module; 5. Ultrasonic cleaning module; 6. Image acquisition module; 7. Central control module. DETAILED DESCRIPTION

[0075] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0076] like Figure 1 As shown, an embodiment of the present invention provides a method for penetration detection and defect repair in titanium alloy casting processing, the method specifically comprising:

[0077] S1: Use mechanical scanning module to perform penetration testing on titanium alloy castings;

[0078] S2: using an image acquisition module to acquire process image information and video image information of the penetration detection process;

[0079] S3: using an image enhancement module to enhance the process image information and video image information of the penetration detection process;

[0080] S4: using the central control module to control the mechanical scanning module to perform penetration action and movement;

[0081] S5: using the image transmission module to receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module;

[0082] S6: Use the video monitoring module to monitor the penetration testing process of the titanium alloy casting, and use the defect repair module to repair the defects found in the test;

[0083] S7: Use the ultrasonic cleaning module to clean and perform penetration testing again until the defect is repaired.

[0084] The steps of the penetration detection and defect repair method in the titanium alloy casting processing will be introduced step by step below:

[0085] S1: Use the mechanical scanning module to perform penetrant testing on titanium alloy castings.

[0086] Implementation: Use a mechanical device with certain control capabilities, such as a mechanical arm or robot, equipped with a penetrant detection probe to scan the surface of titanium alloy castings under a predetermined trajectory. This probe is usually made of sensitive penetrant detection materials, which can absorb penetrant liquid in the defect area and display the defect location through dyeing or fluorescence.

[0087] S2: Use the image acquisition module to acquire process image information and video image information of the penetration detection process.

[0088] Implementation: Install a camera or video equipment and synchronize it with the mechanical scanning module to capture images and video information of the penetration testing process. The image acquisition module should have high resolution and the ability to adapt to different lighting conditions to ensure accurate test results.

[0089] S3: Use the image enhancement module to enhance the process image information and video image information of the penetration detection process.

[0090] Implementation: The image enhancement module can use digital image processing techniques such as filtering, contrast enhancement, edge enhancement, etc. to improve image quality and clarity, which helps to better detect and repair defects.

[0091] S4: Using the central control module to control the mechanical scanning module to perform penetration action and movement.

[0092] Implementation plan: The central control module is the core control unit of this method. It can use a single-chip microcomputer, embedded system or computer, etc., to control the action and motion trajectory of the mechanical scanning module through a preset program to achieve automated penetration detection.

[0093] S5: using the image transmission module to receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module.

[0094] Implementation: The image transmission module can use wired or wireless transmission technology to transmit the data processed by the image enhancement module to the video monitoring module. In this way, the operator can observe the penetration detection process in real time and find defects in time.

[0095] S6: Use the video monitoring module to monitor the penetration testing process of titanium alloy castings, and use the defect repair module to repair the defects found during the inspection.

[0096] Implementation: The video monitoring module is used to display and record real-time video of the penetration testing process. Operators can find defects on the surface of titanium alloy castings during monitoring. Once defects are found, they can switch to the defect repair module.

[0097] S7: Use the ultrasonic cleaning module to clean and perform penetration testing again until the defect is repaired.

[0098] Implementation: The ultrasonic cleaning module uses ultrasonic vibration to generate tiny bubbles, which are impacted and folded in the liquid to clean the surface of the titanium alloy casting. After cleaning, the penetration test needs to be repeated until no defects are found to ensure that the quality of the titanium alloy casting meets the requirements.

[0099] The specific implementation steps of the penetration detection and defect repair method in titanium alloy casting processing can be adjusted and improved according to specific engineering requirements and technical conditions in practical applications.

[0100] In S1, using the mechanical scanning module to perform penetration testing on the titanium alloy casting specifically includes:

[0101] The castings formed by casting are subjected to hot isostatic pressing at a temperature of 900°C-1100°C. The castings subjected to hot isostatic pressing are subjected to penetration testing using conventional methods.

[0102] The image enhancement in S3 specifically includes:

[0103] 1) Providing an image composed of a plurality of pixels arranged in a matrix, and converting the image into a grayscale image;

[0104] 2) Calculate the absolute value Q1 of the difference between the grayscale values ​​of two adjacent rows of pixels in each column and the first grayscale value weight k1;

[0105] The calculation formula for the absolute value Q1 of the difference in grayscale values ​​between two adjacent rows of pixels in the same column is:

[0106] Q1=abs(Gray(i,j)-Gray(i+1,j));

[0107] The calculation formula of the first grayscale value weight k1 is:

[0108]

[0109] The absolute value Q1 of the difference between the grayscale values ​​of two adjacent rows of pixels in the same column ranges from 0 to 255, and n is a positive integer greater than 1;

[0110] The calculation formula is:

[0111]

[0112] Wherein, i and j are positive integers, representing the row and column numbers of the pixel, respectively; Gray(i,j) is the grayscale value of the pixel in the i-th row and j-th column; Gray(i+1,j) is the grayscale value of the pixel in the i+1-th row and j-th column; H1(a) is the number of pixels with grayscale value a; C1(X) is the sum of the number of pixels corresponding to each grayscale value from Gray(i,j) to Gray(i+1,j);

[0113] 3) Calculate the absolute value Q2 of the difference in grayscale values ​​between two adjacent columns of pixels in each row and the second grayscale value weight k2;

[0114] The calculation formula for the absolute value Q2 of the difference in grayscale values ​​between two adjacent columns of pixels in the same row is:

[0115] Q2=abs(Gray(i,j)-Gray(i,j+1));

[0116] The calculation formula of the second grayscale value weight k2 is:

[0117]

[0118] The absolute value Q2 of the difference in grayscale values ​​between two adjacent columns of pixels in the same row ranges from 0 to 255, and n is a positive integer greater than 1 and is the same as the value in step 2);

[0119] The second grayscale value weight k2 is cumulatively calculated with the grayscale values ​​of the pixels in the two adjacent columns in each row. The calculation formula is:

[0120]

[0121] Wherein, i and j are positive integers, representing the row and column numbers of the pixel, respectively; Gray(i,j) is the grayscale value of the pixel in the i-th row and j-th column; Gray(i,j+1) is the grayscale value of the pixel in the i-th row and j+1-th column; H3(a) is the number of pixels with grayscale value a; C3(X) is the sum of the number of pixels corresponding to each grayscale value from Gray(i,j) to Gray(i,j+1);

[0122] 4) Add C1(X) in step 2) and C3(x) in step 3) to obtain C(X);

[0123] C(X)=C1(X)+C3(X);

[0124] 5) Maximum value normalization, the calculation formula is:

[0125]

[0126] Then multiply N(X) by 255 to obtain the enhanced grayscale table out(X), and obtain the new output grayscale value out_gray(i,j) by looking up the table.

[0127] The repairing of the defects found in the detection by using the defect repair module specifically includes: grinding and repairing with a pneumatic grinding wheel; and corroding the repaired parts.

[0128] The use of an ultrasonic cleaning module for cleaning specifically includes:

[0129] (1) Pre-cleaning the titanium alloy casting;

[0130] (2) The outer surface of the titanium alloy casting is rinsed with a cleaning liquid in a high-pressure nozzle. The cleaning liquid is mixed with cleaning balls. After the cleaning balls are sprayed under high pressure, they contact the outer surface of the titanium alloy casting and vibrate, thereby loosening impurities on the surface of the aluminum alloy;

[0131] (3) The titanium alloy casting after pre-cleaning is subjected to deep ultrasonic cleaning. The ultrasonic wave generated by the ultrasonic generator propagates in the cleaning liquid, causing the titanium alloy casting to vibrate together at the ultrasonic frequency, and the oil and impurities on the outer surface of the titanium alloy casting can fall off during the vibration;

[0132] (4) Perform the final cleaning of the titanium alloy castings, and use clean water to wash away the oil and debris retained on the surface of the titanium alloy castings.

[0133] The cleaning balls and the cleaning liquid are uniformly mixed in a ratio of 1:5, and the outer surface hardness of the cleaning balls is less than the outer surface hardness of the titanium alloy casting.

[0134] The diameter of the cleaning ball is 50 microns to 100 microns.

[0135] like Figure 2 As shown, an embodiment of the present invention provides a penetration detection and defect repair system in titanium alloy casting processing for implementing the penetration detection and defect repair method in titanium alloy casting processing, characterized in that the system comprises:

[0136] The mechanical scanning module 1 is used for penetrant testing of titanium alloy castings; the image enhancement module 2 is used for image enhancement of process image information and video image information of the penetrant testing process;

[0137] Video monitoring module 3, used to monitor the penetration testing process of titanium alloy castings;

[0138] Defect repair module 4, used to repair defects found during detection;

[0139] Ultrasonic cleaning module 5, used for cleaning titanium alloy castings;

[0140] An image acquisition module 6 is used to acquire process image information and video image information of the penetration detection process;

[0141] The central control module 7 is connected with the image enhancement module 2, the mechanical scanning module 1, the video monitoring module 3, the defect repair module 4, the ultrasonic cleaning module 5 and the image acquisition module 6, and is used to control the operation of each module, and receive the process image information enhanced by the image enhancement module 2 and transmit it to the video monitoring module 3;

[0142] An embodiment of the present invention provides a computer device, characterized in that the computer device includes a memory and a processor, the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the penetration detection and defect repair method in the titanium alloy casting processing.

[0143] An embodiment of the present invention provides a computer-readable storage medium storing a computer program. When the computer program is executed by a processor, the processor executes the steps of the penetration detection and defect repair method in titanium alloy casting processing.

[0144] As an optimization solution of the embodiment of the present invention, a specific implementation solution is given for each step:

[0145] S1: Use the mechanical scanning module to perform penetrant testing on titanium alloy castings.

[0146] To scan using a robotic device, follow these steps:

[0147] 1. Design a mechanical scanning module: According to the shape and size of the titanium alloy casting, design a suitable robotic arm or robot to enable it to scan the surface.

[0148] 2. Install the penetrant detection probe: Install the penetrant detection probe at the end of the robotic arm or robot to ensure that the penetrant liquid can be applied to the entire casting surface.

[0149] 3. Program control: Write a program to control the movement path and speed of the mechanical scanning module to achieve comprehensive and accurate scanning.

[0150] 4. Perform scanning: According to the predetermined path, the mechanical scanning module begins to perform penetration testing on the surface of the titanium alloy casting.

[0151] S2: Use the image acquisition module to acquire process image information and video image information of the penetration detection process.

[0152] 1. Install camera or webcam: Install high-resolution camera or webcam at appropriate location to capture images and videos of the penetration testing process.

[0153] 2. Synchronization with the mechanical scanning module: Ensure that the operation of the camera or camera head is synchronized with the mechanical scanning module, that is, during the penetrant coating process, the camera or camera head records the corresponding image information.

[0154] 3. Image storage: Store the acquired image information in a computer or other data storage device for subsequent processing and analysis.

[0155] S3: Use the image enhancement module to enhance the process image information and video image information of the penetration detection process.

[0156] 1. Digital image processing: Use digital image processing technology to write algorithms to enhance images, such as filtering, contrast enhancement, edge enhancement, etc.

[0157] 2. Image enhancement operation: The collected image information is processed through the image enhancement module to improve image quality and highlight defects and surface details.

[0158] 3. Storage after image enhancement: Save the enhanced image information for subsequent real-time monitoring and further analysis.

[0159] S4: Using the central control module to control the mechanical scanning module to perform penetration action and movement.

[0160] 1. Central control unit: An embedded system or computer is used as the core of the central control module, which has the ability to control the mechanical scanning module.

[0161] 2. Program writing: Write the control program, preset the motion trajectory, speed and action of the mechanical scanning module, and realize fully automatic penetration detection.

[0162] 3. Motion control: The central control module communicates with the mechanical scanning module to transmit control instructions, thereby controlling the movement and action of the mechanical scanning module.

[0163] S5: using the image transmission module to receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module.

[0164] 1. Image transmission technology: Use wireless transmission technology, such as Wi-Fi or Bluetooth, to achieve the transmission of image information.

[0165] 2. Image receiving device: A receiving device is configured in the video monitoring module to receive image information from the image enhancement module.

[0166] 3. Real-time transmission: Ensure the real-time transmission of images so that operators can observe the penetration testing process in time and find defects.

[0167] S6: Use the video monitoring module to monitor the penetration testing process of titanium alloy castings, and use the defect repair module to repair the defects found during the inspection.

[0168] 1. Video surveillance equipment: Configure a video surveillance module so that operators can observe the penetration detection process in real time.

[0169] 2. Integration of detection and repair: Connect the video surveillance module with the defect repair module to ensure that operators can perform repair operations immediately after discovering defects.

[0170] 3. Defect repair: Based on the test results, the operator uses the defect repair module to repair the defects found in the titanium alloy castings.

[0171] S7: Use the ultrasonic cleaning module to clean and perform penetration testing again until the defect is repaired.

[0172] 1. Ultrasonic cleaning technology: Ultrasonic vibration is used to generate tiny bubbles, which are impacted and folded in the liquid to clean the surface of titanium alloy castings.

[0173] 2. Cleaning device: Equipped with ultrasonic cleaning module to ensure that the repaired area can be cleaned.

[0174] 3. Re-penetration test: After the repair is completed, the penetration test is performed again to confirm that the defect has been completely repaired. If new defects are found, the defects are completely repaired.

[0175] 1. Mechanical scanning module: A robotic device equipped with a penetration detection probe is used to conduct a comprehensive scan of the titanium alloy blades of aircraft engines through a pre-planned path.

[0176] 2. Image acquisition module: Equipped with high-resolution camera equipment, it works synchronously with the mechanical scanning module to capture images and video information of the blade surface.

[0177] 3. Image enhancement module: Use digital image processing algorithms to filter, enhance contrast and enhance edges of images and videos to highlight defect features.

[0178] 4. Central control module: The embedded system is used as the core control unit, and the detection path and parameters are preset to realize the automatic control of the mechanical scanning module.

[0179] 5. Image transmission module: uses wireless transmission technology to transmit image-enhanced data to the operator's monitoring display device.

[0180] 6. Video monitoring module: The operator uses the monitoring display device to observe the penetration detection process of the blade in real time, and proceed to the next step after discovering defects.

[0181] 7. Defect repair module: The operator repairs the defective area found based on the inspection results, which can be done by welding or other repair methods.

[0182] 8. Ultrasonic cleaning module: Use ultrasonic cleaning technology to clean the repaired area to ensure that the surface is clean and free of impurities.

[0183] 9. Re-penetration test: After the repair is completed, conduct penetration test again until it is confirmed that there are no defects.

[0184] Example 2: Penetration testing and defect repair of titanium alloy containers in nuclear power plants

[0185] 1. Mechanical scanning module: It uses a mechanical arm device equipped with a penetration detection probe, which can flexibly adapt to the complex shape and structure of the surface of the titanium alloy container of the nuclear power plant.

[0186] 2. Image acquisition module: Install high-resolution camera equipment, which works synchronously with the mechanical scanning module to capture image and video information of the container surface.

[0187] 3. Image enhancement module: Use digital image processing technology to enhance and clarify the acquired images to ensure that defects are visible.

[0188] 4. Central control module: Use a single-chip microcomputer control center to write programs to control the motion trajectory and actions of the robotic arm to achieve automated detection.

[0189] 5. Image transmission module: transmits the image enhanced data to the monitoring terminal via wired transmission.

[0190] 6. Video monitoring module: The operator observes the penetration inspection process of the nuclear power plant's titanium alloy container in real time on the monitoring terminal and can repair any defects found.

[0191] 7. Defect repair module: Based on the test results, the defects found in the container are repaired by using filling or other repair materials.

[0192] 8. Ultrasonic cleaning module: Use ultrasonic cleaning technology to thoroughly clean the repaired area and eliminate surface residues.

[0193] 9. Re-penetration test: After the repair is completed, the penetration test is carried out again to confirm that there are no defects on the surface of the container to ensure the safe operation of the nuclear power plant.

[0194] The above two embodiments are respectively for titanium alloy blades of aircraft engines and titanium alloy containers of nuclear power plants, and use technologies such as automation, digital image processing, intelligent control and ultrasonic cleaning to achieve efficient, accurate and safe penetration detection and defect repair. These technological advances have improved the efficiency and reliability of the entire process and brought important progress to related fields.

[0195] It should be noted that the embodiments of the present invention can be implemented by hardware, software, or a combination of software and hardware. The hardware part can be implemented using dedicated logic; the software part can be stored in a memory and executed by an appropriate instruction execution system, such as a microprocessor or dedicated design hardware. It will be understood by those skilled in the art that the above-mentioned devices and methods can be implemented using computer executable instructions and / or contained in processor control codes, such as such codes provided on carrier media such as disks, CDs or DVD-ROMs, programmable memories such as read-only memories (firmware), or data carriers such as optical or electronic signal carriers. The devices and modules of the present invention can be implemented by hardware circuits such as very large-scale integrated circuits or gate arrays, semiconductors such as logic chips, transistors, etc., or programmable hardware devices such as field programmable gate arrays, programmable logic devices, etc., can also be implemented by software executed by various types of processors, and can also be implemented by a combination of the above-mentioned hardware circuits and software, such as firmware.

[0196] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any modifications, equivalent substitutions and improvements made by any technician familiar with the technical field within the technical scope disclosed by the present invention and within the spirit and principle of the present invention should be covered by the protection scope of the present invention.

Claims

1. A method for penetrant testing and defect repair in titanium alloy casting processing, characterized in that: The method specifically includes: S1: Use mechanical scanning module to perform penetration testing on titanium alloy castings; S2: using an image acquisition module to acquire process image information and video image information of the penetration detection process; S3: using an image enhancement module to enhance the process image information and video image information of the penetration detection process; S4: Using the central control module to control the mechanical scanning module to perform penetration action and movement; S5: using the image transmission module to receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module; S6: Use the video monitoring module to monitor the penetration testing process of the titanium alloy casting, and use the defect repair module to repair the defects found in the test; S7: Use the ultrasonic cleaning module to clean and perform penetration testing again until the defect is repaired; The specific implementation method of S1 is: A mechanical device with certain control capability is used to scan the surface of titanium alloy castings under a predetermined trajectory. This probe is made of sensitive penetrant testing materials, which can absorb penetrant liquid in the defect area and display the defect location through dyeing or fluorescence; The specific implementation method of S2 is: Install a camera or video equipment and synchronize it with the mechanical scanning module to capture images and video information of the penetration testing process; the image acquisition module should have high resolution and the ability to adapt to different lighting conditions to ensure accurate test results; The specific implementation method of S3 is: The image enhancement module uses digital image processing technology to improve image quality and clarity, helping to better detect and repair defects; The specific implementation method of S4 is: The central control module is the core control unit of the method, which uses a single-chip microcomputer, an embedded system or a computer to control the action and motion trajectory of the mechanical scanning module through a preset program to achieve automated penetration detection; The specific implementation method of S5 is: The image transmission module uses wired or wireless transmission technology to transmit the data processed by the image enhancement module to the video monitoring module. The operator observes the penetration detection process in real time and finds defects in time. The specific implementation method of S6 is: The video monitoring module is used to display and record the real-time video of the penetration testing process. When the operator finds defects on the surface of the titanium alloy casting during monitoring, he switches to the defect repair module.

2. The method for penetrant testing and defect repair in titanium alloy casting processing as claimed in claim 1, characterized in that: The specific implementation method of S7 is: The ultrasonic cleaning module uses ultrasonic vibration to generate tiny bubbles, which clean the surface of titanium alloy castings through impact and folding in the liquid. After cleaning, penetration testing is required again until no defects are found to ensure that the quality of titanium alloy castings meets the requirements.

3. The method for penetrant testing and defect repair in titanium alloy casting processing as claimed in claim 1, characterized in that: The use of an ultrasonic cleaning module for cleaning specifically includes: (1) Pre-cleaning the titanium alloy casting; (2) The outer surface of the titanium alloy casting is rinsed with a cleaning liquid in a high-pressure nozzle. The cleaning liquid is mixed with cleaning balls. After the cleaning balls are sprayed under high pressure, they contact the outer surface of the titanium alloy casting and vibrate, thereby loosening impurities on the surface of the aluminum alloy; (3) The titanium alloy casting after pre-cleaning is subjected to deep ultrasonic cleaning. The ultrasonic wave generated by the ultrasonic generator propagates in the cleaning liquid, causing the titanium alloy casting to vibrate together at the ultrasonic frequency, and the oil and impurities on the outer surface of the titanium alloy casting can fall off during the vibration; (4) Perform the final cleaning of the titanium alloy castings, and use clean water to wash away the oil and debris retained on the surface of the titanium alloy castings.

4. A penetration detection and defect repair system in titanium alloy casting processing that implements the penetration detection and defect repair method in titanium alloy casting processing as described in any one of claims 1 to 3, characterized in that: The system includes: Mechanical scanning module for penetrant testing of titanium alloy castings; An image acquisition module is used to acquire process image information and video image information of the penetration detection process; An image enhancement module is used to enhance the process image information and video image information of the penetration detection process; Video monitoring module, used to monitor the penetration testing process of titanium alloy castings; Defect repair module, used to repair defects found during detection; Ultrasonic cleaning module, used to clean titanium alloy castings; The central control module is connected to the image enhancement module, the mechanical scanning module, the video monitoring module, the defect repair module, the image acquisition module and the ultrasonic cleaning module, and is used to control the operation of each module, and receive the process image information enhanced by the image enhancement module and transmit it to the video monitoring module.