A passivation film and method for improving flip chip reliability
By adopting a double-layer dielectric layer structure on the chip, a high-density first dielectric layer is retained at the step position, and a second dielectric layer with a micro-roughened structure is formed in other areas, which solves the problems caused by insufficient density and high stress of the existing passivation film. Electromigration and reliability issues, improving chip reliability and adhesion.
Patent Information
- Application Number
- CN202311497204.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-10
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2043-11-10
AI Technical Summary
The existing passivation film is not dense enough, which leads to electromigration problems at chip step locations, prone to strip breakage and poor reliability. High-density films are prone to stress and peeling off of the film layer.
A double-layer dielectric layer structure is adopted, in which the high-density first dielectric layer is retained at the step position, and the second dielectric layer with a micro-roughened structure is formed in other areas. The micro-roughened structure enhances the bonding force and releases stress, improving the durability of the passivation film. reliability.
It effectively solves the electromigration problem at the chip step position, avoids micro-cracks and micro-defects caused by stress, and improves the reliability and adhesion of the chip.
Smart Images

Figure CN117253957B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of chip packaging, in particular to a passivation film for improving the reliability of a flip chip. Background Art
[0002] As flip-chip LED chips are increasingly used in high-efficiency, high-power lighting, and Mini / Micro LED display fields, higher requirements are placed on the reliability and yield of flip-chip LEDs, especially in the micro-display field where a failure rate of ppm is required. Among them, electromigration is the main reliability issue affecting interconnect leads, and the geometric size and shape of the leads, as well as the grain structure inside the interconnect leads, all have an important influence on electromigration. In particular, the step position of the chip is not limited in the formation process, and the step coverage is poor, the thickness is reduced, and the current density increases here, which makes it easier to break the bar, resulting in poor chip reliability.
[0003] Covering a passivation layer on top of the metal film can reduce the probability of metal ions moving from the body to the surface and inhibit surface diffusion. However, the density of the existing passivation layer is not enough, and the use of high-density films will result in high stress and prone to problems such as film peeling. Summary of the invention
[0004] In order to solve the above problems, the present invention proposes a passivation film for improving the reliability of flip chip.
[0005] The main contents of the present invention include:
[0006] A passivation film for improving the reliability of a flip chip comprises a first region and a second region, wherein the first region is a region corresponding to a chip step position, and the remaining region is the second region; the first region and the second region both comprise a first dielectric layer deposited on a chip metal film and a second dielectric layer deposited on the first dielectric layer; the density of the first dielectric layer is greater than the density of the second dielectric layer; a micro-roughened structure is formed on a side of the first dielectric layer of the second region facing the second dielectric layer, and the first dielectric layer of the first region is not roughened.
[0007] Preferably, the hydrofluoric acid etching rate of the first dielectric layer is 1-10 μm / min; and the hydrofluoric acid etching rate of the second dielectric layer is 20-50 μm / min.
[0008] Preferably, the ratio of the thickness of the second dielectric layer to the thickness of the first dielectric layer is greater than 1 and less than 10.
[0009] Preferably, the remaining thickness of the first dielectric layer in the second region after the micro-roughened structure is formed is not less than 10-100 nm.
[0010] Preferably, the micro-roughened structure is formed by wet etching or dry etching.
[0011] Preferably, the first dielectric layer and the second dielectric layer are made of one or more of silicon oxide, aluminum oxide, silicon nitride and zirconium oxide.
[0012] The present invention also proposes a method for improving the reliability of a flip chip, comprising the following steps:
[0013] S1. Depositing a first dielectric layer on the metal film of the chip;
[0014] S2. Etching a micro-roughened structure on the first dielectric layer in the first region; the first region is a region corresponding to the step position of the chip;
[0015] S3. depositing a second dielectric layer on the first dielectric layer;
[0016] The density of the first dielectric layer is greater than that of the second dielectric layer; and the ratio of the thickness of the second dielectric layer to the thickness of the first dielectric layer is greater than 1 and less than 10.
[0017] Preferably, the specific steps in step S2 include:
[0018] S21. Coating a photoresist on the first dielectric layer;
[0019] S22. Opening the photoresist of the first dielectric layer in the second region according to a set pattern;
[0020] S23. Etch the first dielectric layer by wet etching or dry etching to obtain the micro-roughened structure.
[0021] Preferably, the roughness of the micro-roughened structure is 50-300nm; the pure hydrofluoric acid rate of the first dielectric layer is 1-10μm / min; the pure hydrofluoric acid rate of the second dielectric layer is 20-50μm / min; and the remaining thickness of the first dielectric layer in the second region after the micro-roughened structure is formed is not less than 10-100nm.
[0022] Preferably, the ratio of the refractive index of the second dielectric layer to the refractive index of the first dielectric layer is 0.94-0.99; the material of the first dielectric layer and the second dielectric layer is one or more of silicon oxide, aluminum oxide, silicon nitride and zirconium oxide.
[0023] Compared with the prior art, the present invention proposes a passivation film and method for improving the reliability of a flip chip, wherein a second dielectric layer with a lower density is deposited on a first dielectric layer with a higher density, and the first dielectric layer with a higher density is completely retained in the step position area of the chip, while a micro-roughened structure is formed on the first dielectric layer in other areas; the present invention deposits two dielectric layers with different densities, and the first dielectric layer with a higher density is micro-roughened in different areas to obtain a passivation film, which not only solves the problem of electromigration at the step position, but also improves the stress of the existing passivation film, avoids problems such as microcracks and microdefects caused by high stress, and thus improves the reliability of the chip. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a schematic diagram of the structure of the passivation film of the present invention;
[0025] Figure 2 A schematic diagram of the process for preparing the passivation film of the present invention;
[0026] 1-chip; 10-step position; 2-insulating layer; 3-lower metal film; 4-passivation film; 41-first dielectric layer; 410-remaining part after micro-roughening; 42-second dielectric layer; 43-micro-roughening structure; 5-upper metal film; 6-photoresist. DETAILED DESCRIPTION
[0027] The technical solution protected by the present invention is described in detail below with reference to the accompanying drawings.
[0028] The present invention proposes a new passivation film, which can improve the problem of micro cracks, micro defects and even film shedding caused by excessive stress during the growth of the existing passivation film, thereby affecting the reliability of the chip.
[0029] like Figure 1As shown, the passivation film proposed in the present invention includes a double-layer structure, and because the step position 10 of the chip 1 is more prone to the problem of metal electron migration, in order to ensure the reliability of the step position, different structural designs are adopted for the first area covering the step position 10 and the second area outside the step position. Specifically, the passivation film includes a first dielectric layer 41 and a second dielectric layer 42 arranged up and down; wherein, a micro-roughened structure is first formed on the first dielectric layer 41 in the second area after micro-roughening treatment, retaining a certain thickness, while the first dielectric layer 41 corresponding to the step position 10 does not undergo micro-roughening treatment and maintains the original surface, and then the second dielectric layer 42 is directly deposited on the first dielectric layer 41 after the micro-roughening treatment, so as to obtain the passivation film of the present invention, wherein the first dielectric layer 41 and the second dielectric layer 42 in the second area are connected by the micro-roughened structure, that is, the first dielectric layer 41 in the second area and the second dielectric layer 42 are connected by the micro-roughened structure. The contact portion of the dielectric layer is a micro-roughened structure 43, which can not only enhance the bonding force between the first dielectric layer 41 and the second dielectric layer 42, but also release the stress of the first dielectric layer 41, thereby avoiding micro-cracking caused by excessive stress. The contact portion of the first dielectric layer 41 and the second dielectric layer 42 in the first region (i.e., the step position 10) maintains the original high density, which can effectively solve the problem of metal electron electromigration at the wall step position 10. At the same time, the low-density second dielectric layer 42 deposited thereon can release the stress of the first dielectric layer 41 to a certain extent.
[0030] The surface of the first dielectric layer 41 in the second region facing the second dielectric layer 42 is etched to obtain a corresponding micro-roughened structure, so that the first region of the passivation film finally obtained, i.e., the step position 10 of the chip 1, has a complete first dielectric layer 41, and the first dielectric layer 41 in the second region is combined with the second dielectric layer 42 after roughening, so that the step position can have a better ability to resist metal migration, while ensuring the connection reliability between the first dielectric layer and the second dielectric layer; Figure 1 The micro-roughened structure in the figure is only for illustration, and the shape and size of the micro-roughened structure actually produced can be controlled by relevant preparation processes.
[0031] Since the dielectric layer with lower density has a loose structure, metal atoms are more likely to form short circuits and leakage failures through the loose structure. Therefore, in order to prevent electromigration of metal atoms and ensure the antistatic property of the chip, a dielectric layer with higher density is usually selected in this field. However, the first dielectric film with higher density is prone to short circuits between the upper metal film and the lower metal film due to microcracks and microdefects caused by stress growth, thereby causing chip failure. The present invention first selects a first dielectric film with higher density to be deposited on the metal film layer, and then improves the stress problem by covering the second dielectric layer with lower density on top of the first dielectric layer. Specifically, the first dielectric layer is corroded by pure hydrofluoric acid at a rate of 1-10μm / min; and the second dielectric layer is corroded by pure hydrofluoric acid at a rate of 20-50μm / min.
[0032] Furthermore, the ratio of the thickness of the second dielectric layer 42 to the thickness of the first dielectric layer 41 is greater than 1 and less than 10, and the thickness of the remaining portion 410 of the first dielectric layer after micro-roughening is retained to be no less than 10-100nm, that is, the thickness of the second dielectric layer 42 needs to be greater than the thickness of the first dielectric layer 41; and then the second dielectric layer 42 is deposited on the first dielectric layer 41, which can not only play a protective role, but also maintain stronger adhesion. In the prior art, the thickness of the passivation film at the step position 10 is usually less than the thickness of other parts, but the step position 10 is more prone to metal migration. The use of the passivation film of the present invention can also solve this problem in the prior art.
[0033] In one embodiment, the material of the first dielectric layer 41 and the second dielectric layer 42 are both selected from one of silicon oxide, aluminum oxide, silicon nitride, and zirconium oxide. The refractive index ratio of the second dielectric layer 42 to the first dielectric layer 41 is 0.94-0.99, and both have high transmittance in the visible light range, and the transmittance is greater than 95%.
[0034] See also Figure 2 , the following will describe in detail how to form the passivation film of the present invention on a chip to ensure the reliability of the chip.
[0035] First, a metal film is deposited on a chip structure having steps, wherein the chip structure includes an insulating layer 2, on which an upper metal film 3 is first deposited, and then a first dielectric layer 41 is formed on the upper metal film 3;
[0036] Then, a micro-roughened structure is formed on the first dielectric layer in the second region. Specifically, a photoresist 6 is coated on the first dielectric layer 41, and then a semiconductor photolithography technique is used to retain the photoresist in the first region (step position), such as Figure 2As shown, a hole is opened in the photoresist in the second area, and then the first dielectric layer is etched by a wet etching or dry etching process until the first dielectric layer retains a thickness of not less than 10-100 nm, thereby obtaining a first dielectric layer with a micro-roughened structure.
[0037] Subsequently, the second dielectric layer 42 is formed on the first dielectric layer 41 having the micro-roughened structure, thereby obtaining the passivation film of the present invention.
[0038] When performing photolithographic hole opening on the first dielectric layer, it is possible to choose to retain more photoresist within 10% of the periphery of the step position, that is, to retain the complete first dielectric layer within a certain range outside the step position, so as to further improve the ability to resist metal migration. The second area can be etched by ion etching, and the etching gas is generally a halogen element or compound containing F ions and Cl ions. The etching depth is regulated by controlling the process parameters such as etching power and time to ensure the thickness of the first dielectric layer after etching, so that the first dielectric layer can work together to improve the stress problem while maintaining a reliable connection with the second dielectric layer.
[0039] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A passivation film for improving the reliability of a flip chip, characterized in that: The flip chip includes an insulating layer and a conductive metal hole opened on the insulating layer; the conductive metal hole is a through hole that is wide at the top and narrow at the bottom; an upper metal film is deposited on the insulating layer and on the bottom and side walls of the through hole; the passivation film is deposited on the metal film; the passivation film includes a first area and a second area, the first area is the part of the passivation film deposited on the wall of the conductive metal hole, and the rest is the second area; the first area and the second area both include a first dielectric layer and a second dielectric layer deposited on the first dielectric layer; the density of the first dielectric layer is greater than the density of the second dielectric layer; a micro-roughened structure is formed on the side of the first dielectric layer of the second area facing the second dielectric layer, and the first dielectric layer of the first area is not roughened; the roughness of the micro-roughened structure is 50-300nm.
2. A passivation film for improving flip chip reliability according to claim 1, characterized in that: The hydrofluoric acid etching rate of the first dielectric layer is 1-10 μm / min; the hydrofluoric acid etching rate of the second dielectric layer is 20-50 μm / min.
3. A passivation film for improving flip chip reliability according to claim 1, characterized in that: A ratio of a thickness of the second dielectric layer to a thickness of the first dielectric layer is greater than 1 and less than 10.
4. A passivation film for improving flip chip reliability according to claim 2, characterized in that: The remaining thickness of the first dielectric layer in the second region after the micro-roughened structure is formed is not less than 10-100 nm.
5. A passivation film for improving flip chip reliability according to claim 1, characterized in that: The micro-roughened structure is formed by wet etching or dry etching.
6. A passivation film for improving flip chip reliability according to claim 1, characterized in that: The material of the first dielectric layer and the second dielectric layer is one or more of silicon oxide, aluminum oxide, silicon nitride and zirconium oxide.
7. A method for forming a passivation film for improving the reliability of a flip chip according to claim 1, characterized in that: The steps include: etching a micro-roughened structure on the first dielectric layer in the first region; depositing a second dielectric layer on the first dielectric layer; Wherein, the ratio of the thickness of the second dielectric layer to the thickness of the first dielectric layer is greater than 1 and less than 10.
8. The method for forming a passivation film for improving flip chip reliability according to claim 7, characterized in that: The specific steps of etching a micro-roughened structure on the first dielectric layer in the first region include: S21. Coating a photoresist on the first dielectric layer; S22. Opening the photoresist of the first dielectric layer in the second region according to a set pattern; S23. Etch the first dielectric layer by wet etching or dry etching to obtain the micro-roughened structure.
9. The method for forming a passivation film for improving flip chip reliability according to claim 8, characterized in that: The roughness of the micro-roughened structure is 50-300nm; the pure hydrofluoric acid rate of the first dielectric layer is 1-10μm / min; the pure hydrofluoric acid rate of the second dielectric layer is 20-50μm / min; the remaining thickness of the first dielectric layer in the second region after the micro-roughened structure is formed is not less than 10-100nm.
10. The method for forming a passivation film for improving flip chip reliability according to claim 7, characterized in that: The material of the first dielectric layer and the second dielectric layer is one or more of silicon oxide, aluminum oxide, silicon nitride and zirconium oxide.